Semiconductor device and method

By using protective masks and moderate etch selectivity in the MRAM cell manufacturing process, the problem of over-etching of dielectric features is solved, the reliability of the device and manufacturing yield are improved, and the integrity of the conductive features is ensured.

CN113140672BActive Publication Date: 2024-11-12TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110054250.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-01-17
Filing Date
2021-01-15
Publication Date
2024-11-12
Estimated Expiration
2041-01-15

AI Technical Summary

Technical Problem

In the prior art, when manufacturing magnetoresistive random access memory (MRAM) units, it is difficult to effectively prevent excessive etching of dielectric features, resulting in damage to conductive features, affecting the reliability of the device and manufacturing yield.

Method used

Protect the logical region during the ion beam etching (IBE) process using a protection mask to slow down the etching rate by forming a mask layer covering the portion, preventing over-etching of the logical region, and using moderate etching selectivity in the etching process to protect it Conductive characteristics.

Benefits of technology

Improves the reliability and manufacturing yield of the MRAM cell, prevents excessive etching and damage to the logic region, ensures the integrity of the conductive features and the high performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113140672B_ABST
    Figure CN113140672B_ABST
Patent Text Reader

Abstract

The present disclosure relates to semiconductor devices and methods. In one embodiment, a method includes: forming a first intermetallic dielectric (IMD) layer above a semiconductor substrate; forming a bottom electrode layer above the first IMD layer; forming a magnetic tunnel junction (MTJ) film stack above the bottom electrode layer; forming a first top electrode layer above the MTJ film stack; forming a protection mask covering a first region of the first top electrode layer, a second region of the first top electrode layer not covered by the protection mask; forming a second top electrode layer above the protection mask and the first top electrode layer; and patterning the second top electrode layer, the first top electrode layer, the MTJ film stack, the bottom electrode layer, and the first IMD layer using an ion beam etching (IBE) process to form an MRAM cell, wherein the protection mask is etched during the IBE process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to semiconductor devices and methods. Background Art

[0002] Semiconductor memory is used in integrated circuits of electronic devices, including, for example, radios, televisions, cellular phones, and personal computing devices. One type of semiconductor memory is magnetoresistive random access memory (MRAM), which involves spintronics that combines semiconductor technology with magnetic materials and devices. The spin of electrons is used to indicate bit values ​​through their magnetic moments. An MRAM cell typically includes a magnetic tunnel junction (MTJ) stack, which includes two ferromagnets separated by a thin insulator. Summary of the invention

[0003] According to one embodiment of the present disclosure, a method for manufacturing a semiconductor device is provided, comprising: forming a first intermetallic dielectric (IMD) layer above a semiconductor substrate; forming a bottom electrode layer above the first IMD layer; forming a magnetic tunnel junction (MTJ) film stack above the bottom electrode layer; forming a first top electrode layer above the MTJ film stack; forming a protection mask covering a first area of ​​the first top electrode layer, a second area of ​​the first top electrode layer not covered by the protection mask; forming a second top electrode layer above the protection mask and the first top electrode layer; and patterning the second top electrode layer, the first top electrode layer, the MTJ film stack, the bottom electrode layer and the first IMD layer using an ion beam etching (IBE) process to form an MRAM unit, wherein the protection mask is etched during the IBE process, the IBE process etches the protection mask at a first etching rate, the IBE process etches the first top electrode layer at a second etching rate, and the first etching rate is less than the second etching rate.

[0004] According to another embodiment of the present disclosure, a semiconductor device is provided, comprising: a semiconductor substrate including an active device; a first intermetallic dielectric (IMD) layer located above the semiconductor substrate; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode comprising: a first conductive layer located above the first MTJ stack; a dielectric layer located above the first conductive layer; and a second conductive layer located above the dielectric layer; a second IMD layer located above the first top electrode; and a second conductive feature extending through the second IMD layer, the second conductive feature contacting the first top electrode.

[0005] According to another embodiment of the present disclosure, a semiconductor device is provided, comprising: a semiconductor substrate including an active device; an interlayer dielectric (ILD) layer located above the semiconductor substrate; a first intermetallic dielectric (IMD) layer located above the ILD layer; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode comprising: a first conductive layer located above the first MTJ stack; and a second conductive layer located above the first conductive layer; a spacer disposed on sidewalls of the first conductive layer, the second conductive layer, the first MTJ stack, and the first bottom electrode; a second IMD layer having a first portion and a second portion, the first portion being located above the ILD layer, the second portion at least partially extending into the ILD layer; and a second conductive feature extending through the first portion of the second IMD layer, the second conductive feature being electrically connected to the active device. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] When read in conjunction with the accompanying drawings, various aspects of the present invention can be best understood from the following detailed description. It should be noted that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, for clarity of discussion, the size of the various features may be arbitrarily increased or reduced.

[0007] Figure 1 is a block diagram of a semiconductor device according to some embodiments.

[0008] Figure 2 is a cross-sectional view of a semiconductor device according to some embodiments.

[0009] Figures 3 to 15 are various views of intermediate stages in fabricating an interconnect structure for a semiconductor device according to some embodiments.

[0010] Fig.16 is a cross-sectional view of a semiconductor device according to some other embodiments.

[0011] Figures 17 to 19 are various views of intermediate stages in fabricating an interconnect structure for a semiconductor device according to some other embodiments.

[0012] Figure 20 to Figure 21 are various views of intermediate stages in fabricating an interconnect structure for a semiconductor device according to some other embodiments.

[0013] Fig. 22 is a detailed view of an MRAM cell according to some embodiments.

[0014] Fig.23 is a detailed view of an MRAM cell according to some other embodiments. DETAILED DESCRIPTION

[0015] The following disclosure provides many different embodiments or examples for implementing the different features of the present invention. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are merely examples and are not intended to limit the present disclosure. For example, in the following description, forming a first feature above or on a second feature may include an embodiment in which the first feature and the second feature are formed in direct contact, and may also include an embodiment in which additional features may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may repeat reference numerals and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself represent the relationship between the various embodiments and / or configurations discussed.

[0016] Additionally, spatially relative terms (e.g., "below," "beneath," "below," "above," "upper," etc.) may be used herein to facilitate describing the relationship of one element or feature shown in the figures relative to another element or feature(s). These spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should be interpreted accordingly.

[0017] According to some embodiments, an interconnect structure of an integrated circuit is formed, and an MTJ stack is formed in a memory region of the interconnect structure. The MTJ stack is used to form an MRAM cell in the interconnect structure. During the formation of the MTJ stack, a protection mask is formed over a logic region of the interconnect structure. The MTJ stack is patterned using the protection mask, for example, the patterning of the MTJ stack is performed while the protection mask covers the logic region. The use of the protection mask helps prevent over-etching of dielectric features when forming the MTJ stack, thereby preventing damage to the underlying conductive features of the interconnect structure.

[0018] Figure 15 is a block diagram of a semiconductor device 50 according to some embodiments. The semiconductor device 50 includes an MRAM array 52, a row decoder 54, and a column decoder 56. The MRAM array 52 includes MRAM cells 58 arranged in rows and columns. The row decoder 54 may be, for example, a static CMOS decoder, a pseudo-NMOS decoder, etc. During operation, the row decoder 54 selects a desired MRAM cell 58 in a row of the MRAM array 52 by activating a corresponding word line WL of the row. The column decoder 56 may be, for example, a static CMOS decoder, a pseudo-NMOS decoder, etc., and may include a writer driver, a sense amplifier, a combination thereof, etc. During operation, the column decoder 56 selects a bit line BL for a desired MRAM cell 58 from a column in a selected row of the MRAM array 52, and reads data from or writes data to the selected MRAM cell 58 using the bit line BL.

[0019] Figure 2 is a cross-sectional view of a semiconductor device 50 according to some embodiments. Figure 2 5 is a simplified view, and some features (discussed below) are omitted for clarity of illustration. Semiconductor device 50 includes a logic region 50L and a memory region 50M. Memory devices (e.g., MRAM) are formed in memory region 50M, and logic devices (e.g., logic circuits) are formed in logic region 50L. For example, MRAM array 52 (see Figure 1 ) may be formed in the memory region 50M, and the row decoder 54 and the column decoder 56 (see Figure 1 ) may be formed in the logic region 50L. The logic region 50L may occupy most of the area of ​​the semiconductor device 50. For example, the logic region 50L may occupy 95% to 99% of the area of ​​the semiconductor device 50, and the memory region 50M occupies the remaining area of ​​the semiconductor device 50. The memory region 50M may be disposed at an edge of the logic region 50L, or the logic region 50L may surround the memory region 50M.

[0020] The logic region 50L and the memory region 50M are formed over the same semiconductor substrate 60. The semiconductor substrate 60 may be doped or undoped silicon, or an active layer of a semiconductor on insulator (SOI) substrate. The semiconductor substrate 60 may include other semiconductor materials, such as germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, gallium nitride, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or combinations thereof. Other substrates, such as multilayer or gradient substrates, may also be used.

[0021] Devices 62 are formed at the active surface of semiconductor substrate 60. Devices 62 may be active devices or passive devices. For example, devices 62 may be transistors, diodes, capacitors, resistors, etc. formed by any suitable formation method. Devices 62 are interconnected to form memory devices and logic devices of semiconductor device 50. For example, some of devices 62 may be access transistors.

[0022] One or more interlayer dielectric (ILD) layers 64 are formed on the semiconductor substrate 60, and conductive features such as contact plugs 66 are formed to be electrically connected to the device 62. The ILD layer(s) 64 may be formed of any suitable dielectric material, for example, nitrides such as silicon nitride; oxides such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), etc.; etc. The ILD layer(s) may be formed by any acceptable deposition process, such as spin coating, physical vapor deposition (PVD), chemical vapor deposition (CVD), etc., or a combination thereof. The conductive features in the ILD layer(s) may be formed by any suitable process, such as deposition, damascene (e.g., single damascene, dual damascene, etc.), etc., or a combination thereof.

[0023] An interconnect structure 68 is formed above the semiconductor substrate 60. The interconnect structure 68 interconnects the devices 62 to form an integrated circuit in each of the logic region 50L and the memory region 50M. The interconnect structure 68 includes a plurality of metallization layers M1-M6. Although six metallization layers are shown in the figure, it should be understood that more or fewer metallization layers may be included. Each of the metallization layers M1-M6 includes a metallization pattern in a dielectric layer. The metallization pattern is electrically coupled to the device 62 of the semiconductor substrate 60, and includes metal lines L1-L6 and vias V1-V6 formed in one or more intermetallic dielectric (IMD) layers, respectively. The interconnect structure 68 can be formed by a damascene process (e.g., a single damascene process, a dual damascene process, etc.). In some embodiments, the contact plug 66 is also a part of the metallization pattern, such as a part of the bottommost layer of the metal via V1. Figure 2 Some reference numerals are also indicated and will be further described below.

[0024] The MRAM cell 58 is formed in the interconnect structure 68. The MRAM cell 58 can be formed in any of the metallization layers M1-M6 and is shown as being formed in the middle metallization layer M5. Each MRAM cell 58 includes a conductive via 72, a bottom electrode 74 on the conductive via 72, an MTJ stack 76 on the bottom electrode 74, and a top electrode 78 on the MTJ stack 76. An additional IMD layer 80 can be formed around the MRAM cell 58, wherein the conductive via 72 extends through the IMD layer 80. Spacers 82 can also be formed around the MRAM cell 58. The IMD layer 80 and / or the spacer 82 surround and protect the components of the MRAM cell 58. The resistance of the MTJ stack 76 is programmable and can be set to a high resistance (R ap ) ) and a low resistance (R p ) (which may represent, for example, a value of "0"). Thus, a value may be written to the MRAM cell 58 by programming the resistance of its MTJ stack 76 with its corresponding access transistor, and the value may be read from the MRAM cell 58 by measuring the resistance of the MTJ stack 76 with the access transistor.

[0025] The MRAM cells 58 are electrically connected to the device 62. The conductive via 72 is physically and electrically coupled to the underlying metallization pattern, such as to the metal line L4 in the example shown. The top electrode 78 is physically and electrically coupled to the overlying metallization pattern, such as to the metal via V6 in the example shown. The MRAM cells 58 are arranged in an MRAM array having memory rows and columns. The metallization pattern includes access lines (e.g., word lines and bit lines) of the MRAM array. For example, the underlying metallization pattern may include word lines arranged along the rows of the MRAM array, and the overlying metallization pattern may include bit lines arranged along the columns of the MRAM array.

[0026] Figures 3 to 20 5 is a diagram showing various intermediate stages in the fabrication of an interconnect structure of a semiconductor device 50 according to some embodiments. The interconnect structure includes an MRAM array of MRAM cells. As discussed further below, a protection mask is formed over the logic region 50L during the process of the memory region 50M, which can help protect the logic region 50L from excessive etching damage during the process.

[0027] exist Figure 3 In the metallization layer of the interconnect structure (e.g., M4, see Figure 2 ) is formed. The metallization layer includes an IMD layer 102 and a conductive feature 104 (which may correspond to a metal line L4, see Figure 2). The IMD layer 102 is formed over the (one or more) ILD layers 64. The IMD layer 102 may be formed of any suitable dielectric material, for example, a nitride, such as silicon nitride; an oxide, such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), etc.; etc. The IMD layer 102 may be formed by any acceptable deposition process, such as spin coating, physical vapor deposition (PVD), chemical vapor deposition (CVD), etc., or a combination thereof. The IMD layer 102 may be a layer formed of a low-k dielectric material having a k value of less than about 3.0. The IMD layer 102 may be a layer formed of an ultra-low-k (ELK) dielectric material having a k value of less than 2.5.

[0028] Conductive feature 104 is formed in IMD layer 102 and is electrically connected to device 62. According to some embodiments, conductive feature 104 includes a diffusion barrier layer and a conductive material above the diffusion barrier layer. An opening is formed in IMD layer 102 using, for example, an etching process. The opening exposes the conductive feature below, such as a metal via below. The diffusion barrier layer may be formed of TaN, Ta, TiN, Ti, CoW, etc., and may be formed in the opening by a deposition process (e.g., atomic layer deposition (ALD) or the like). The conductive material may include copper, aluminum, tungsten, silver, and combinations thereof, etc., and may be formed above the diffusion barrier layer in the opening by an electrochemical plating process, CVD, ALD, PVD, etc., or a combination thereof. In one embodiment, the conductive material is copper, and the diffusion barrier layer is a thin barrier layer that prevents copper from diffusing into IMD layer 102. After forming the diffusion barrier layer and the conductive material, the excess diffusion barrier layer and the conductive material may be removed by, for example, a planarization process (e.g., a chemical mechanical polishing (CMP) process). In some embodiments, conductive feature 104 is a metal line.

[0029] The etch stop layer 106 is formed on the conductive features 104 and the IMD layer 102. The etch stop layer 106 may be formed of a dielectric material (e.g., aluminum nitride, aluminum oxide, silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, combinations thereof, etc.). The etch stop layer 106 may be formed by chemical vapor deposition (CVD), physical vapor deposition (PVD), ALD, a spin-on dielectric process, etc., or a combination thereof. The etch stop layer 106 may also be a composite layer formed of a plurality of dielectric sublayers. For example, the etch stop layer 106 may include a silicon carbide sublayer and an aluminum oxide sublayer formed on the silicon carbide sublayer, wherein the thickness of the aluminum oxide sublayer is about 100 Å. to about and the thickness of the silicon carbide sublayer is about to about The silicon carbide sublayer is used as a glue layer to improve the adhesion between the underlying layer and the aluminum oxide sublayer.

[0030] The IMD layer 108 is formed on the etch stop layer 106. In some embodiments, the IMD layer 108 is formed of tetraethyl orthosilicate (TEOS) oxide (e.g., silicon oxide deposited using, for example, a chemical vapor deposition (CVD) process with TEOS as a precursor). In some embodiments, the IMD layer 108 may be formed using PSG, BSG, BPSG, undoped silicate glass (USG), fluorosilicate glass (FSG), SiOCH, flowable oxide, porous oxide, etc., or a combination thereof. For example, the IMD layer 108 may also be formed of a low-k dielectric material having a k value of less than about 3.0. The IMD layer 108 may be formed at about to about The thickness is within the range of .

[0031] The conductive via 110 is formed to extend through the IMD layer 108 and the etch stop layer 106. The conductive via 110 may also be referred to as a bottom via. In some embodiments, the conductive via 110 includes a conductive region 112 and a conductive barrier layer 114, which lines the sidewalls and bottom surface of the conductive region 112. The conductive barrier layer 114 may be formed of titanium, titanium nitride, tantalum, tantalum nitride, cobalt, combinations thereof, and the like. The conductive region 112 may be formed of a metal (e.g., copper, aluminum, tungsten, cobalt, alloys thereof, and the like). The formation of the conductive via 110 may include: etching the IMD layer 108 and the etch stop layer 106 to form a via opening; forming a blanket conductive barrier layer extending into the via opening; depositing a metal material over the blanket conductive barrier layer; and performing a planarization process (e.g., a CMP process or a mechanical grinding process) to remove excess portions of the blanket conductive barrier layer and the metal material.

[0032] One or more bottom electrode layers 116 are formed on the conductive vias 110 and the IMD layer 108. In some embodiments, the bottom electrode layer(s) 116 are formed as a blanket layer and may be formed using CVD, physical vapor deposition (PVD), electrochemical plating (ECP), chemical plating, etc. The bottom electrode layer(s) 116 may be formed of a conductive material (e.g., Cu, Al, Ti, Ta, W, Pt, Ni, Cr, Ru, TiN, TaN, combinations thereof, multiple layers thereof, etc.). For example, the bottom electrode layer(s) 116 may include a first bottom electrode layer 116A and a second bottom electrode layer 116B above the first bottom electrode layer 116A. The first bottom electrode layer 116A may be made of a first conductive material (e.g., TaN), and the second bottom electrode layer 116B may be made of a second conductive material (e.g., TiN). In some embodiments, the thickness of the first bottom electrode layer 116A is about to about In some embodiments, the second bottom electrode layer 116B has a thickness of up to about In some embodiments, such as embodiments where a single bottom electrode layer 116 is formed, the second bottom electrode layer 116B is omitted.

[0033] exist Figure 4 In the embodiment, the MTJ film stack 118 is formed on the bottom electrode layer(s) 116. The MTJ film stack 118 is a multilayer including an antiferromagnetic layer 118A, a pinned layer 118B on the antiferromagnetic layer 118A, a tunnel barrier layer 118C on the pinned layer 118B, and a free layer 118D on the tunnel barrier layer 118C. The total thickness of the MTJ film stack 118 is about 1000 Å. to about Each layer of the MTJ thin film stack 118 may be deposited using one or more deposition methods (eg, CVD, PVD, ALD, a combination thereof, etc.).

[0034] The antiferromagnetic layer 118A may be formed of a metal alloy including manganese (Mn) and one or more other metals (e.g., platinum (Pt), iridium (Ir), rhodium (Rh), nickel (Ni), palladium (Pd), iron (Fe), osmium (Os), etc.). For example, the antiferromagnetic layer 118A may be formed of PtMn, IrMn, RhMn, NiMn, PdPtMn, FeMn, OsMn, etc. The thickness of the antiferromagnetic layer 118A may be about 1000 nm. to about within the range.

[0035] The fixed layer 118B may be formed of a ferromagnetic material having a larger coercive field than the free layer 118D, such as cobalt iron (CoFe), cobalt iron boron (CoFeB), a combination thereof, etc. The thickness of the fixed layer 118B may be about 1000 nm. to about In some embodiments, the fixed layer 118B has a synthetic ferromagnetic (SFM) structure, in which the coupling between the magnetic layers is ferromagnetic coupling. The fixed layer 118B may also adopt a synthetic antiferromagnetic (SAF) structure, which includes multiple magnetic metal layers separated by multiple non-magnetic spacer layers. The magnetic metal layer may be formed of Co, Fe, Ni, etc. The non-magnetic spacer layer may be formed of Cu, Ru, Ir, Pt, W, Ta, Mg, etc. For example, the fixed layer 118B may have a Co layer and a repeated (Pt / Co) x Layer, where x represents the number of repeats, which can be any integer equal to or greater than 1, such as an integer in the range of about 3 to about 20.

[0036] The tunnel barrier layer 118C may be formed of a dielectric material (eg, MgO, AlO, AlN, combinations thereof, etc.). The thickness of the tunnel barrier layer 118C may be in the range of about 1 nm to about 10 nm. The tunnel barrier layer 118C is thicker than other layers of the MTJ thin film stack 118.

[0037] The free layer 118D can be formed of a suitable ferromagnetic material (e.g., CoFe, NiFe, CoFeB, CoFeBW, combinations thereof, etc.). The free layer 118D can also adopt a synthetic ferromagnetic structure similar to the SAF structure, in which the thickness of the non-magnetic spacer layer is adjusted to achieve ferromagnetic coupling between separated magnetic metals, such as coupling the magnetic moments in the same direction. The magnetic moment of the free layer 118D is programmable, and the resistance of the resulting MTJ stack is therefore programmable. Specifically, the free layer 118D can be programmed at a high resistance (R ap ) and low resistance (R p ) between the 118C and 119C layers. Thus, the MTJ stack may also be referred to as a programmable resistance element or a programmable resistor. The thickness of the tunnel barrier layer 118C contributes to the R of the MTJ stack. ap and R p .

[0038] It should be understood that the material and structure of the MTJ film stack 118 can have many variations, which are also within the scope of the present disclosure. For example, the layers 118A, 118B, 118C, and 118D can be formed in the reverse order of the above order. Therefore, the free layer 118D can be the bottom layer of the MTJ film stack 118, and the antiferromagnetic layer 118A can be the top layer of the MTJ film stack 118.

[0039] The first top electrode layer 120 is formed on the MTJ thin film stack 118. In some embodiments, the first top electrode layer 120 is formed as a blanket layer and can be formed using CVD, PVD, ECP, chemical plating, etc. The first top electrode layer 120 is a conductive layer and can include a metal (e.g., titanium, tantalum, tungsten, aluminum, copper, alloys thereof, multilayers thereof, etc.). For example, the first top electrode layer 120 can be formed of TiN, Ta, TaN, Ti, Ru, W, WC, multilayers thereof, etc. In some embodiments, the first top electrode layer 120 is formed of titanium nitride. In some embodiments, the thickness of the first top electrode layer 120 is about to about In some embodiments, the thickness of the first top electrode layer 120 is greater than the combined thickness of the bottom electrode layer(s) 116. The first top electrode layer 120 is used as a hard mask in the subsequent patterning of the MTJ thin film stack 118.

[0040] The mask layer 121 is formed on the first top electrode layer 120. In some embodiments, the mask layer 121 is formed of silicon oxide. In other embodiments, the mask layer 121 may be formed using PSG, BSG, BPSG, USG, FSG, SiOCH, flowable oxide, porous oxide, etc. or a combination thereof. For example, the mask layer 121 may also be formed of a low-k dielectric material having a k value of less than about 3.0. The mask layer 121 may be formed to a thickness of about to about In some embodiments, the mask layer 121 is formed using materials and methods similar to those of the IMD layer 108. For example, both the mask layer 121 and the IMD layer 108 may be formed of silicon oxide.

[0041] exist Figure 5 , the mask layer 121 is patterned to expose a portion of the first top electrode layer 120 outside the logic region 50L. The patterning process forms a protection mask 122, which includes the remaining portion of the mask layer 121. In the illustrated embodiment, the protection mask 122 covers all of the logic region 50L and a portion of the memory region 50M. For example, the protection mask 122 may cover up to about 1% of the memory region 50M. Specifically, the protection mask 122 may cover all of the logic region 50L and a row / column of the conductive vias 110 at the interface of the logic region 50L and the memory region 50M (e.g., a row / column of the MRAM cell 58, see Figure 8 ). In other embodiments (discussed further below), the protective mask 122 covers a portion of the logic region 50L and exposes all of the memory region 50M. The patterning process can be performed by appropriate photolithography and etching processes. For example, a mask (e.g., photoresist) covering the logic region 50L can be patterned, the mask can be used to form the protective mask 122, and then the mask can be removed.

[0042] After the protective mask 122 is patterned, the exposed portion of the first top electrode layer 120 may have a reduced thickness, for example, about to about Alternatively, the thickness of the first top electrode layer 120 may be substantially unchanged by patterning.

[0043] exist Figure 6In the embodiment, the second top electrode layer 124 is formed on the protective mask 122 and the exposed portion of the first top electrode layer 120. In some embodiments, the second top electrode layer 124 is formed as a blanket layer and can be formed using CVD, PVD, ECP, chemical plating, etc. The second top electrode layer 124 is a conductive layer and can include a metal (e.g., titanium, tantalum, tungsten, aluminum, copper, alloys thereof, multilayers thereof, etc.). For example, the second top electrode layer 124 can be formed of TiN, Ta, TaN, Ti, Ru, W, WC, multilayers thereof, etc. In some embodiments, the second top electrode layer 124 is formed using materials and methods similar to those of the first top electrode layer 120. For example, both the first top electrode layer 120 and the second top electrode layer 124 can be titanium nitride. In other embodiments, the first top electrode layer 120 and the second top electrode layer 124 can be different materials. In some embodiments, the thickness of the second top electrode layer 124 is about to about The thickness of the second top electrode layer 124 may be greater than the thickness of the first top electrode layer 120. The second top electrode layer 124 is used as a hard mask in the subsequent patterning of the MTJ thin film stack 118.

[0044] After forming the second top electrode layer 124, one or more masks are formed over the second top electrode layer 124. In some embodiments, the one or more masks may include one or more hard masks, a three-layer mask, a combination thereof, and the like. For example, a hard mask layer 126 may be formed over the second top electrode layer 124, and a photosensitive mask 128 may be formed over the hard mask layer 126. In some embodiments, the hard mask layer 126 is formed of an oxide (e.g., titanium oxide, silicon oxide, a combination thereof, and the like). In some embodiments, the thickness of the hard mask layer 126 is about 1000 Å. to about The photosensitive mask 128 may be a photoresist, such as a single-layer photoresist, a double-layer photoresist, a triple-layer photoresist, etc. The photosensitive mask 128 is formed in the memory region 50M, wherein a pattern of the photosensitive mask 128 corresponds to a pattern of a subsequently formed MRAM cell.

[0045] exist Figure 7 In the embodiment of the present invention, the photosensitive mask 128 is used as an etching mask to etch and pattern the hard mask layer 126, the second top electrode layer 124, and the exposed portion of the first top electrode layer 120. The etching method may include a plasma etching method, such as ion beam etching (IBE). Etching may be achieved using glow discharge plasma (GDP), capacitively coupled plasma (CCP), inductively coupled plasma (ICP), etc. The photosensitive mask 128 may be consumed in the etching process.

[0046] After the etching process, the exposed portion of the protective mask 122 may have a reduced thickness, for example, at about to about Alternatively, the thickness of the protective mask 122 may be substantially unchanged by the etching process. After the etching process, both the protective mask 122 and the MTJ thin film stack 118 may be exposed.

[0047] exist Figure 8 , the patterned hard mask layer 126 and the second top electrode layer 124 are used together as an etching mask to etch and pattern the protective mask 122, the first top electrode layer 120, the MTJ thin film stack 118 and the (one or more) bottom electrode layers 116. Patterning may include one or more etching processes, and a groove 130 is formed in the IMD layer 108. The etching method may include a plasma etching method, such as ion beam etching (IBE). Etching may be achieved using glow discharge plasma (GDP), capacitively coupled plasma (CCP), inductively coupled plasma (ICP), etc. For example, when the etching method is an IBE process, etching may be performed using an etchant (e.g., Ar, He, Ne, Xe, O2, N2, methanol (CH3OH, i.e., MeOH), CO, ammonia (NH3), etc., or a combination thereof), at a pressure in the range of about 0.05 mTorr to about 0.7 mTorr and at a temperature in the range of about 10°C to about 60°C. The patterned hard mask layer 126 may be consumed during the etching process.

[0048] The etching process forms the bottom electrode 132, the MTJ stack 134, and the top electrode 136 (including the top electrodes 136A and 136B), which together form the MRAM cell 58. Each MRAM cell 58 includes the bottom electrode 132, the MTJ stack 134, and the top electrode 136. The bottom electrode 132 includes the remaining portion of the bottom electrode layer (one or more) 116. The MTJ stack 134 includes the remaining portion of the MTJ film stack 118. The top electrode 136 includes the remaining portion of the first top electrode layer 120 and the second top electrode layer 124. As discussed further below, the first subset of the top electrodes 136A also includes the remaining portion of the protective mask 122, but the second subset of the top electrodes 136B does not include the remaining portion of the protective mask 122. In some embodiments, the etching process partially etches the IMD layer 108 and the conductive via 110. In such an embodiment, the remaining portion of the IMD layer 108 has a sloped sidewall and has a trapezoidal shape in the cross-section shown. The MTJ stack 134 and the bottom electrode 132 also have sloped sidewalls and have a trapezoidal shape in the cross-section shown. In addition, the top electrode 136 has a hemispherical top surface.

[0049] As described above, the etching process may include using a plasma etching method, such as an IBE process. IBE provides a high level of precision (e.g., high anisotropy), which can help control the profile of the MTJ stack 134. However, re-deposition may occur during IBE, and specifically, metal elements etched by IBE may be re-sputtered on the sidewalls of the MTJ stack 134. The presence of etching residues (e.g., from the MTJ thin film stack 118 or (one or more) bottom electrode layers 116) on the sidewalls of the MTJ stack 134 may change the resistance of the MTJ stack 134, thereby causing the resulting MRAM cell 58 to have an undesirably high resistance (R ap ) and low resistance (R p ) value. For example, the presence of the conductive etching residues may short-circuit various layers of the MTJ stack 134, thereby reducing the expected resistance value of the MTJ stack 134. The amount of etching residues may be reduced by performing the IBE process for a long duration (e.g., a duration in a range of about 100 seconds to about 600 seconds), which helps to increase the consumption of the etching residues.

[0050] As described above, the second top electrode layer 124 may be formed using materials and methods similar to the first top electrode layer 120, and the protection mask 122 may be formed using materials and methods similar to the IMD layer 108. For example, the first top electrode layer 120 and the second top electrode layer 124 may be formed of the same conductive electrode material (e.g., titanium nitride), and the protection mask 122 and the IMD layer 108 may be formed of the same dielectric isolation material (e.g., silicon oxide). The electrode material and the isolation material have a moderate etching selectivity relative to the IBE process. For example, the ratio of the etching rate of the isolation material to the etching rate of the electrode material relative to the IBE process may be in the range of about 1:1 to about 1:2.5. In an embodiment where the first top electrode layer 120 is multi-layered, at least the topmost sub-layer of the first top electrode layer 120 has a moderate etching selectivity to the isolation material relative to the IBE process. The moderate etching selectivity between the electrode material and the isolation material helps protect the logic region 50L from damage by over-etching during the IBE process. Specifically, the moderate etch selectivity slows down but does not stop the IBE process in the logic region 50L, which can help prevent the IBE process from completely etching through the IMD layer 108 in the logic region 50L. Therefore, sandwiching the protection mask 122 between the first top electrode layer 120 and the second top electrode layer 124 can help protect the conductive features 104 from over-etching, which would otherwise occur due to the long duration of the IBE process and the pattern loading effect in the memory region 50M.

[0051] As described above, in this embodiment, the protective mask 122 (see Figure 5) covers all of the logic region 50L and a portion of the memory region 50M. In this way, before the IBE process, at least some of the MTJ stack 134 is covered by the protection mask 122. Therefore, the MRAM cell 58 has two different types of top electrodes 136. The top electrode 136A is an electrode near the interface of the memory region 50M and the logic region 50L, which corresponds to the MRAM cell 58 covered by the protection mask 122. As a result, the top electrode 136A may include a portion of the patterned protection mask 122. The top electrode 136B is an electrode inside the memory region 50M, which corresponds to the MRAM cell 58 not covered by the protection mask 122. As described above, the protection mask 122 is a dielectric material. Therefore, the top electrode 136A has a greater resistance than the top electrode 136B. In this way, the MRAM cell 58 with the top electrode 136A therefore has an increased high resistance (R ap ) and low resistance (R p ) value. In addition, the top electrode 136A has a greater thickness than the top electrode 136B. For example, the thickness of the top electrodes 136A and 136B can be about to about and the top electrode 136A may be thicker than the top electrode 136B by the thickness of the protective mask 122, for example, in the range of about to about In addition, due to the difference in etching selectivity, the portion of the IMD layer 108 covered by the protective mask 122 is less recessed than the portion of the IMD layer 108 not covered by the protective mask 122. Specifically, the grooves 130 differ in depth by a distance D1, which may be approximately to about within the range.

[0052] exist Fig. 9 In the embodiment, the passivation layer 138 is blanket formed over the MRAM cell 58 and in the recess 130 (see Figure 8 In some embodiments, the passivation layer 138 may include silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, silicon carbonitride, combinations thereof, and the like, and may be formed using CVD, plasma enhanced chemical vapor deposition (PECVD), ALD, plasma enhanced atomic layer deposition (PEALD), PVD, combinations thereof, and the like. In some embodiments, the passivation layer 138 may reduce or prevent moisture (e.g., H2O) from diffusing into the MRAM cell 58 during subsequent processes. In some embodiments, the thickness of the passivation layer 138 may be about 1000 nm. to about within the range.

[0053] exist Fig.10In the embodiment of the present invention, the passivation layer 138 is patterned to expose the top portion of the top electrode 136. In some embodiments, the patterning is a dry etching process, such as an anisotropic etching process. The patterning removes the horizontal portion of the passivation layer 138. Subsequently, another passivation layer 140 is formed over the passivation layer 138, and an oxide layer 142 is formed over the passivation layer 140. In some embodiments, the passivation layer 140 is formed of one of the candidate materials and methods for the passivation layer 138, but is formed of a different material from the passivation layer 138. For example, the passivation layer 138 may be formed of an oxide such as silicon oxide, and the passivation layer 140 may be formed of a nitride such as silicon nitride. In some embodiments, the oxide layer 142 may include silicon oxide, etc., and may be formed using CVD, PECVD, ALD, PEALD, a combination thereof, etc. Subsequently, one or more dry etching processes are performed to etch the passivation layer 140 and the oxide layer 142 and expose the top portion of the top electrode 136, such as the top portion of the second top electrode layer 124. In some embodiments, the one or more dry etching processes are anisotropic etching processes and remove horizontal portions of the passivation layer 140 and the oxide layer 142. The remaining portions of the passivation layer 138, the passivation layer 140, and the oxide layer 142 form spacers 144, which are disposed on the sidewalls of the MRAM cell 58. After the spacers 144 are patterned, the IMD layer 108 in the logic region 50L is exposed.

[0054] exist Fig.11 In the embodiment of the present invention, an IMD layer 146 is formed over the spacer 144, the MRAM cell 58, and the IMD layer 108. In some embodiments, the IMD layer 146 is formed using materials and methods similar to those of the IMD layer 108. Then, an anti-reflective layer 148 is formed on the IMD layer 146. The anti-reflective layer 148 may be a nitrogen-free anti-reflective layer (NFARL) and may be formed of a nitrogen-free dielectric material (e.g., silicon oxycarbide). During subsequent processes of the logic region 50L, the IMD layer 146 and the anti-reflective layer 148 will be used to protect the memory region 50M.

[0055] exist Fig.12 In the embodiment of the present invention, the anti-reflective layer 148, the IMD layer 146 and the IMD layer 108 are patterned to expose the etch stop layer 106 in the logic region 50L. In some embodiments, the patterning process may include suitable photolithography and etching processes. After the patterning process, the anti-reflective layer 148 and the IMD layer 146 are retained in the memory region 50M.

[0056] exist Fig.13, an IMD layer 150 is formed over the etch stop layer 106, the patterned IMD layer 146, and the patterned anti-reflective layer 148. In some embodiments, the IMD layer 150 is formed using materials and methods similar to those of the IMD layer 108. An anti-reflective layer 152 is then formed over the IMD layer 150. In some embodiments, the anti-reflective layer 152 is formed using materials and methods similar to those of the anti-reflective layer 148.

[0057] exist Fig.14 , a conductive feature 154 is formed in the IMD layer 150 and the etch stop layer 106. The conductive feature 154 may include a conductive line 154L and a conductive via 154V, and is formed in the logic region 50L. The memory region 50M may not have the conductive feature 154. The conductive feature 154 may be formed by a suitable method (e.g., a damascene process). Exemplary damascene processes include a single damascene process, a dual damascene process, and the like. In some embodiments, the conductive feature opening is formed by a via-first process. In other embodiments, the conductive feature opening is formed by a trench-first process. Subsequently, the conductive feature opening is filled with a suitable conductive material, such as copper, aluminum, a combination thereof, and the like. Next, a planarization process (e.g., a CMP process) is performed to remove excess material above the memory region 50M and expose the topmost surface of the top electrode 136. In some embodiments, after planarization, the topmost surface of the top electrode 136 (e.g., the second top electrode layer 124) is planar with the topmost surface of the conductive feature 154. In some embodiments, the planarization process completely removes the anti-reflective layer 152 (see Fig.13 ). After the planarization process, the top electrode 136 has a uniform thickness, for example, the combined thickness of the constituents of the top electrode 136A is equal to the combined thickness of the constituents of the top electrode 136B. Although each conductive via 154V and corresponding conductive line 154L are shown as separate elements, it should be understood that they can be continuous conductive features, such as in embodiments where they are formed by a dual damascene process.

[0058] exist Fig.15 In the embodiment, another metallization layer of the interconnect structure is formed (e.g., M6, see Figure 2 ). The metallization layer includes an etch stop layer 156, an IMD layer 158, and a conductive feature 160. The conductive feature 160 includes a conductive via 160V (which may correspond to a metal via V6, see Figure 2 ) and conductive line 160L (which may correspond to metal line L6, see Figure 2), and is formed in both the logic region 50L and the memory region 50M. In some embodiments, the etch stop layer 156 is formed using materials and methods similar to the etch stop layer 106. In some embodiments, the IMD layer 158 is formed using materials and methods similar to the IMD layer 150. In some embodiments, the conductive feature 160 is formed using materials and methods similar to the conductive feature 154. The conductive feature 160 is electrically connected to the memory device (e.g., MRAM) formed in the memory region 50M and the logic device (e.g., logic circuit) formed in the memory region 50L. Specifically, the conductive feature 160 is physically and electrically connected to the conductive feature 154 and the top electrode 136. In some embodiments, the conductive feature 160 electrically connects the memory device to the logic device. For example, the conductive feature 160 can be used to connect some of the conductive features 154 to some of the top electrodes 136. Although each conductive via 160V and the corresponding conductive line 160L are shown as separate elements, it should be understood that they can be continuous conductive features, such as in embodiments in which they are formed by a dual damascene process.

[0059] Fig.16 is a cross-sectional view of a semiconductor device 50 according to some other embodiments. In this embodiment, the protective mask 122 is patterned to be Figure 5 The embodiment further extends to the memory region 50M. For example, the protection mask 122 can cover from 0.1% to 1% of the memory region 50M. Specifically, the protection mask 122 can cover all of the logic region 50L, and from about 10 to about 30 rows / columns of the MRAM cells 58 at the interface of the logic region 50L and the memory region 50M. In this way, multiple rows / columns of the MRAM cells 58 near the interface of the memory region 50M and the logic region 50L have top electrodes 136A that include portions of the protection mask 122. Lithographic shift may occur during patterning of the protection mask 122. The amount of overlap between the protection mask 122 and the memory region 50M can vary depending on the degree of shift during patterning.

[0060] Figures 17 to 19 is a cross-sectional view of an intermediate stage in the fabrication of a conductor device 50 according to some other embodiments. Figures 17 to 19 Some of the process steps of the embodiment are Figures 3 to 15 The process steps of the embodiment of FIG. 5 are similar, and therefore only the differences between the process steps are described. In this embodiment, the protection mask 122 is patterned to cover only a portion of the logic region 50L and expose all of the memory region 50M.

[0061] Fig.17 Shows that Figure 7The semiconductor device 50 is shown in a similar state of process, for example, after patterning the first top electrode layer 120. The protection mask 122 is patterned so that a portion of the logic region 50L adjacent to the memory region 50M is exposed. As a result, the protection mask 122 covers most but not all of the logic region 50L. For example, the protection mask 122 may cover from 90% to 99.9% of the logic region 50L. The exact amount of the logic region 50L exposed may be controlled by forming an etching mask for patterning the protection mask 122 (see Figure 5 ). Note that the mask is selected such that the conductive features 104 in the logic region 50L are covered by the protective mask 122 and the exposed portions of the logic region 50L are free of the conductive features 104 .

[0062] Fig.18 Shows that Figure 8 Semiconductor device 50 in a similar process state, for example after patterning MRAM cell 58. After patterning, recess 130 may still differ in depth by a distance D1. However, some over-etching during the IBE process discussed above may occur in the uncovered portion of logic region 50L. Over-etching forms recess 162 in IMD layer 108, which may also extend into etch stop layer 106 and IMD layer 102. Recess 162 may have a rounded bottom surface. Although recess 162 is shown in a portion of logic region 50L, it should be understood that recess 162 may be formed in all areas between memory cell 58 and the covered portion of logic region 50L. Because conductive features 104 in logic region 50L remain protected by protective mask 122, recess 162 does not expose or damage conductive features 104. Advantageously, protective mask 122 is formed to expose a portion of logic region 50L, thereby allowing all protective mask 122 to be removed during the IBE process for patterning MRAM cell 58.

[0063] Fig.19 Shows that Fig.15 The semiconductor device 50 is similar to the state of the art. The IMD layer 150 fills the recess 162, and thus the bottommost surface of the IMD layer 150 can be located below the bottommost surface of the etch stop layer 106. Advantageously, removing all of the protective mask 122 during the formation of the MRAM cell 58 allows all of the resulting MRAM cells 58 to have a top electrode 136B that is free of the remaining portion of the protective mask 122. By avoiding the formation of the top electrode 136A (see Figure 8 ), all resulting MRAM cells 58 may have similar high resistance (R ap ) and low resistance (R p )value.

[0064] Figure 20 to Figure 21 is a cross-sectional view of an intermediate stage in the fabrication of a semiconductor device 50 according to some other embodiments. Figure 20 to Figure 21 Some of the process steps of the embodiment are Figures 3 to 15 The process steps of the embodiment of the present invention are similar, and therefore only the differences between the process steps are described. In this embodiment, the protection mask 122 is patterned to cover a portion of the logic region 50L and expose all of the memory region 50M. In addition, the resistor 164 is formed in the logic region 50L. Although only one resistor 164 is shown, it should be understood that a plurality of resistors 164 may be formed.

[0065] Fig. 20 Shows that Figure 8 The semiconductor device 50 is similarly processed, for example, after patterning the MRAM cell 58. Figure 8 ), some portions of the bottom electrode layer(s) 116 and the MTJ film stack 118 in the logic region 50L are masked. Some of the masked portions of the bottom electrode layer(s) 116 and the MTJ film stack 118 thus remain in the logic region 50L and form portions that will become the resistor 164. As an example of forming the resistor 164, the photosensitive mask 128 (see Figure 6 ) can be formed with a pattern in the logic region 50L and used in a subsequent patterning process (eg, Figure 7 and Figure 8 The resistor 164 is patterned in the patterning process described in the foregoing. After patterning, the grooves 130 may still differ in depth by a distance D1. To help protect the bottom electrode layer(s) 116 and ensure the formation of the resistor 164, the thickness of the protective mask 122 may be greater in this embodiment, for example, about 1000 Å. to about within the range.

[0066] Fig.21 Shows that Fig.15 Semiconductor device 50 of similar process state. Some of the conductive features 154 are physically and electrically coupled to resistor 164, for example, coupled to the topmost surface of resistor 164. Some portions of the topmost surface of resistor 164 may also be contacted by IMD layer 146. Advantageously, forming resistor 164 in logic region 50L from a portion of MTJ film stack 118 allows forming a high impedance resistor 164 for a logic device. For example, resistor 164 may have an impedance in the range of about 0.5 kΩ to about 5 kΩ.

[0067] Fig. 22is a detailed view of an MRAM cell 58 according to some other embodiments. During the formation of the MRAM cell 58, an interfacial oxide layer 166 can be formed in the top electrode 136B, between the first top electrode layer 120 and the second top electrode layer 124. Before forming the second top electrode layer 124, the interfacial oxide layer 166 can be formed by oxidizing the first top electrode layer 120. For example, the first top electrode layer 120 and the second top electrode layer 124 can be formed in different processes, and the vacuum in the process chamber can be broken between the processes so that the first top electrode layer 120 is exposed to an oxygen-containing environment. The thickness of the interfacial oxide layer 166 can be controlled by changing the duration of exposure to the environment. In some embodiments, the thickness can be further controlled by optionally etching the interfacial oxide layer 166. For example, the interfacial oxide layer 166 can be formed before forming the second top electrode layer 124 (see Figure 6 ) is performed before performing a wet etch using dHF to reduce the interface oxide layer 166 to a desired thickness. The amount of remaining interface oxide layer 166 may affect the high resistance (R ap ) and low resistance (R p ) value, where a thicker interface oxide layer 166 produces a higher resistance value. In other words, the high resistance (R) of the MRAM cell 58 can be adjusted by forming the interface oxide layer 166 to a desired thickness. ap ) value and low resistance (R p Thus, in some embodiments, some of the top electrodes 136 (e.g., top electrode 136A) may have a first dielectric layer (e.g., protective mask 122) of a first thickness, and some of the top electrodes 136 (e.g., top electrode 136B) may have a second dielectric layer (e.g., interfacial oxide layer 166) of a smaller second thickness.

[0068] Fig.23 is a detailed view of an MRAM cell 58 according to some other embodiments. During the formation of the MRAM cell 58, an insulating feature 168 can be formed in the top electrode 136B, between the first top electrode layer 120 and the second top electrode layer 124. The insulating feature 168 can be formed by patterning the protective mask 122 to partially cover some of the MRAM cells 58 so that residues from the protective mask 122 remain in some of the top electrodes 136B. An interfacial oxide layer 166 can also be formed between the second top electrode layer 124 and the insulating feature 168. Therefore, the interfacial oxide layer 166 can have an uneven (e.g., non-flat) interface with the underlying features. As described above, a cleaning process can be performed to try and control the thickness of the interfacial oxide layer 166. The amount of remaining interfacial oxide layer 166 and insulating features 168 can affect the high resistance (R ap ) and low resistance (R p) values, where thicker interfacial oxide layer 166 and larger insulating features 168 produce higher resistance values.

[0069] It should be understood that due to process variations, the semiconductor device 50 may have many of the features discussed herein. For example, the semiconductor device 50 may have the following: an MRAM cell 58 having a flat interface oxide layer 166, an MRAM cell 58 having an uneven interface oxide layer 166, and an MRAM cell 58 having no interface oxide layer 166. In addition, the recess 162 (see Fig.18 ) may be formed in some areas of the logic region 50L, but not formed in other areas of the logic region 50L. Finally, the resistor 164 (see Fig.21 ) may be formed in some areas of the logic region 50L, but not formed in other areas of the logic region 50L. For example, both grooves 162 may be formed in some areas of the logic region 50L, and the resistor 164 may be formed in other areas of the logic region 50L.

[0070] Embodiments can achieve advantages. A protective mask 122 is formed at least partially over the logic region 50L (see Figure 5 ) helps during the IBE process for patterning the MTJ stack 134 (see Figure 8 ) protects the logic region 50L from over-etching damage. Specifically, the protection mask 122 slows down the IBE process in the logic region 50L, thereby preventing the IBE process from damaging the underlying conductive features 104. Therefore, the reliability of the resulting MRAM cell 58 can be improved, and the manufacturing yield of the semiconductor device 50 can also be improved.

[0071] In one embodiment, a method includes: forming a first intermetal dielectric (IMD) layer over a semiconductor substrate; forming a bottom electrode layer over the first IMD layer; forming a magnetic tunnel junction (MTJ) film stack over the bottom electrode layer; forming a first top electrode layer over the MTJ film stack; forming a protection mask covering a first region of the first top electrode layer, a second region of the first top electrode layer not covered by the protection mask; forming a second top electrode layer over the protection mask and the first top electrode layer; and patterning the second top electrode layer, the first top electrode layer, the MTJ film stack, the bottom electrode layer, and the first IMD layer using an ion beam etching (IBE) process to form an MRAM cell, wherein the protection mask is etched during the IBE process, the IBE process etches the protection mask at a first etching rate, the IBE process etches the first top electrode layer at a second etching rate, and the first etching rate is less than the second etching rate.

[0072] In some embodiments of the method, forming the protective mask includes: depositing a mask layer on a first region and a second region of the first top electrode layer using a chemical vapor deposition process using tetraethyl orthosilicate (TEOS) as a precursor; and patterning the mask layer to remove a portion of the mask layer above the second region of the first top electrode layer. In some embodiments of the method, an MRAM cell is formed by a first region of the first top electrode layer, and the MRAM cell includes: a bottom electrode including a portion of the bottom electrode layer remaining after an IBE process; an MTJ stack including a portion of the MTJ thin film stack remaining after the IBE process; and a top electrode including a portion of the first top electrode layer and a portion of the second top electrode layer remaining after the IBE process, wherein the IBE process removes all of the protective mask. In some embodiments of the method, an MRAM cell is formed by a second region of the first top electrode layer, and the MRAM cell includes: a bottom electrode including a portion of the bottom electrode layer remaining after the IBE process; an MTJ stack including a portion of the MTJ thin film stack remaining after the IBE process; and a top electrode including a portion of the first top electrode layer, a second top electrode layer, and a portion of the protective mask remaining after the IBE process. In some embodiments, the method further comprises: patterning a first groove and a second groove in the first IMD layer using an IBE process, the first groove being in a portion of the first IMD layer located below the first region of the first top electrode layer, the second groove being in a portion of the first IMD layer located below the second region of the first top electrode layer, the second groove being deeper than the first groove. In some embodiments, the method further comprises: patterning a third groove in the first IMD layer using an IBE process, the third groove being disposed below the second region of the first top electrode layer, the third groove being deeper than the first groove and the second groove. In some embodiments, the method further comprises: patterning the MTJ film stack, the bottom electrode layer, and the first IMD layer using an IBE process to form a resistor; forming a second IMD layer above the resistor; and forming a conductive feature extending through the second IMD layer to contact the resistor. In some embodiments of the method, a ratio of the first etching rate to the second etching rate is in a range of 1:1 to 1:2.5. In some embodiments of the method, the duration of performing the IBE process is in a range of 100 seconds to 600 seconds. In some embodiments of the method, the first region occupies 95% to 99% of the area of ​​the first top electrode layer.

[0073] In one embodiment, a device includes: a semiconductor substrate including an active device; a first intermetal dielectric (IMD) layer located above the semiconductor substrate; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode, the first top electrode including: a first conductive layer located above the first MTJ stack, a dielectric layer located above the first conductive layer, and a second conductive layer located above the dielectric layer; a second IMD layer located above the first top electrode; and a second conductive feature extending through the second IMD layer, the second conductive feature contacting the first top electrode.

[0074] In some embodiments, the device further comprises: a third conductive feature extending through the first IMD layer; a second bottom electrode located above the third conductive feature; a second MTJ stack located above the second bottom electrode; a second top electrode, the second top electrode comprising: a third conductive layer located above the second MTJ stack, and a fourth conductive layer located above the third conductive layer; and a fourth conductive feature extending through the second IMD layer, the fourth conductive feature contacting the second top electrode, wherein the second IMD layer is located above the second top electrode, and wherein the combined thickness of the third conductive layer and the fourth conductive layer is equal to the combined thickness of the first conductive layer, the dielectric layer, and the second conductive layer. In some embodiments, the device further comprises: a spacer disposed on the sidewalls of the first conductive layer, the second conductive layer, the third conductive layer, the fourth conductive layer, the dielectric layer, the first MTJ stack, the second MTJ stack, the first bottom electrode, and the second bottom electrode. In some embodiments, the device further comprises: an interfacial oxide layer located at the interface of the third conductive layer and the fourth conductive layer, the interfacial oxide layer being flat. In some embodiments, the device further comprises: an interfacial oxide layer located at the interface of the third conductive layer and the fourth conductive layer, the interfacial oxide layer being uneven. In some embodiments, the device also includes: a third IMD layer located above the semiconductor substrate, the third IMD layer being adjacent to the first IMD layer; a third conductive feature extending through the third IMD layer, the third conductive feature being electrically connected to the active device; and a fourth conductive feature extending through the second IMD layer, the fourth conductive feature contacting the third conductive feature.

[0075] In one embodiment, a device includes: a semiconductor substrate including an active device; an interlayer dielectric (ILD) layer located above the semiconductor substrate; a first intermetallic dielectric (IMD) layer located above the ILD layer; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode, the first top electrode including: a first conductive layer located above the first MTJ stack, and a second conductive layer located above the first conductive layer; a spacer disposed on sidewalls of the first conductive layer, the second conductive layer, the first MTJ stack, and the first bottom electrode; a second IMD layer having a first portion and a second portion, the first portion being located above the ILD layer, the second portion extending at least partially into the ILD layer; and a second conductive feature extending through the first portion of the second IMD layer, the second conductive feature being electrically connected to the active device.

[0076] In some embodiments of the device, the second portion of the second IMD layer has a rounded bottom surface. In some embodiments, the device further comprises: a resistor located on a portion of the first IMD layer, the second IMD layer contacting a top surface of the resistor; and a third conductive feature extending through the first portion of the second IMD layer, the third conductive feature contacting the top surface of the resistor. In some embodiments of the device, the first top electrode further comprises: a dielectric feature disposed between a portion of the first conductive layer and a portion of the second conductive layer; and an interfacial oxide layer located at an interface of the first conductive layer and the second conductive layer.

[0077] The features of several embodiments are discussed above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis to design or change other processes and structures for achieving the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also be aware that such equivalent structures do not deviate from the spirit and scope of the present disclosure, and that they can make various changes, substitutions and modifications herein without departing from the spirit and scope of the present disclosure.

[0078] Example 1. A method for manufacturing a semiconductor device, comprising: forming a first intermetallic dielectric (IMD) layer above a semiconductor substrate; forming a bottom electrode layer above the first IMD layer; forming a magnetic tunnel junction (MTJ) film stack above the bottom electrode layer; forming a first top electrode layer above the MTJ film stack; forming a protection mask covering a first area of ​​the first top electrode layer, a second area of ​​the first top electrode layer not covered by the protection mask; forming a second top electrode layer above the protection mask and the first top electrode layer; and patterning the second top electrode layer, the first top electrode layer, the MTJ film stack, the bottom electrode layer and the first IMD layer using an ion beam etching (IBE) process to form an MRAM unit, wherein the protection mask is etched during the IBE process, the IBE process etches the protection mask at a first etching rate, the IBE process etches the first top electrode layer at a second etching rate, and the first etching rate is less than the second etching rate.

[0079] Example 2. A method according to Example 1, wherein forming the protective mask includes: depositing a mask layer on the first region and the second region of the first top electrode layer using a chemical vapor deposition process using tetraethyl orthosilicate (TEOS) as a precursor; and patterning the mask layer to remove a portion of the mask layer above the second region of the first top electrode layer.

[0080] Example 3. A method according to Example 1, wherein the MRAM cell is formed by the first region of the first top electrode layer, and the MRAM cell includes: a bottom electrode, including a portion of the bottom electrode layer that remains after the IBE process; an MTJ stack, including a portion of the MTJ film stack that remains after the IBE process; and a top electrode, including portions of the first top electrode layer and the second top electrode layer that remain after the IBE process, wherein the IBE process removes all of the protective masks.

[0081] Example 4. A method according to Example 1, wherein the MRAM cell is formed by the second region of the first top electrode layer, and the MRAM cell includes: a bottom electrode, including a portion of the bottom electrode layer that remains after the IBE process; an MTJ stack, including a portion of the MTJ thin film stack that remains after the IBE process; and a top electrode, including the first top electrode layer, the second top electrode layer, and a portion of the protective mask that remains after the IBE process.

[0082] Example 5. The method according to Example 1 further includes: patterning a first groove and a second groove in the first IMD layer using the IBE process, wherein the first groove is in a portion of the first IMD layer below the first region of the first top electrode layer, and the second groove is in a portion of the first IMD layer below the second region of the first top electrode layer, and the second groove is deeper than the first groove.

[0083] Example 6. The method according to Example 5 further includes: patterning a third groove in the first IMD layer using the IBE process, the third groove is arranged below the second region of the first top electrode layer, and the third groove is deeper than the first groove and the second groove.

[0084] Example 7. The method according to Example 1 also includes: patterning the MTJ film stack, the bottom electrode layer and the first IMD layer using the IBE process to form a resistor; forming a second IMD layer above the resistor; and forming a conductive feature that extends through the second IMD layer to contact the resistor.

[0085] Example 8. The method of Example 1, wherein a ratio of the first etching rate to the second etching rate is in a range of 1:1 to 1:2.5.

[0086] Example 9. The method of Example 1, wherein the duration of performing the IBE process is in the range of 100 seconds to 600 seconds.

[0087] Example 10. The method of Example 1, wherein the first region occupies 95% to 99% of an area of ​​the first top electrode layer.

[0088] Example 11. A semiconductor device comprising: a semiconductor substrate including an active device; a first intermetallic dielectric (IMD) layer located above the semiconductor substrate; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode comprising: a first conductive layer located above the first MTJ stack; a dielectric layer located above the first conductive layer; and a second conductive layer located above the dielectric layer; a second IMD layer located above the first top electrode; and a second conductive feature extending through the second IMD layer, the second conductive feature contacting the first top electrode.

[0089] Example 12. The device according to Example 11 further includes: a third conductive feature extending through the first IMD layer; a second bottom electrode located above the third conductive feature; a second MTJ stack located above the second bottom electrode; a second top electrode, including: a third conductive layer located above the second MTJ stack; and a fourth conductive layer located above the third conductive layer; and a fourth conductive feature extending through the second IMD layer, the fourth conductive feature contacting the second top electrode, wherein the second IMD layer is located above the second top electrode, and wherein the combined thickness of the third conductive layer and the fourth conductive layer is equal to the combined thickness of the first conductive layer, the dielectric layer and the second conductive layer.

[0090] Example 13. The device according to Example 12 further includes: a spacer disposed on the side walls of the first conductive layer, the second conductive layer, the third conductive layer, the fourth conductive layer, the dielectric layer, the first MTJ stack, the second MTJ stack, the first bottom electrode and the second bottom electrode.

[0091] Example 14. The device according to Example 12 further includes: an interface oxide layer located at the interface between the third conductive layer and the fourth conductive layer, the interface oxide layer being flat.

[0092] Example 15. The device according to Example 12 further includes: an interface oxide layer located at the interface between the third conductive layer and the fourth conductive layer, the interface oxide layer being uneven.

[0093] Example 16. The device according to Example 11 further includes: a third IMD layer located above the semiconductor substrate, the third IMD layer being adjacent to the first IMD layer; a third conductive feature extending through the third IMD layer, the third conductive feature being electrically connected to the active device; and a fourth conductive feature extending through the second IMD layer, the fourth conductive feature contacting the third conductive feature.

[0094] Example 17. A semiconductor device comprising: a semiconductor substrate including an active device; an interlayer dielectric (ILD) layer located above the semiconductor substrate; a first intermetallic dielectric (IMD) layer located above the ILD layer; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode located above the first conductive feature; a first magnetic tunnel junction (MTJ) stack located above the first bottom electrode; a first top electrode comprising: a first conductive layer located above the first MTJ stack; and a second conductive layer located above the first conductive layer; a spacer disposed on sidewalls of the first conductive layer, the second conductive layer, the first MTJ stack, and the first bottom electrode; a second IMD layer having a first portion and a second portion, the first portion being located above the ILD layer, the second portion extending at least partially into the ILD layer; and a second conductive feature extending through the first portion of the second IMD layer, the second conductive feature being electrically connected to the active device.

[0095] Example 18. The device of Example 17, wherein the second portion of the second IMD layer has a rounded bottom surface.

[0096] Example 19. The device of Example 17 further includes: a resistor located on a portion of the first IMD layer, the second IMD layer contacting a top surface of the resistor; and a third conductive feature extending through the first portion of the second IMD layer, the third conductive feature contacting the top surface of the resistor.

[0097] Example 20. A device according to Example 17, wherein the first top electrode further includes: a dielectric feature disposed between a portion of the first conductive layer and a portion of the second conductive layer; and an interfacial oxide layer located at an interface between the first conductive layer and the second conductive layer.

Claims

1. A method for manufacturing a semiconductor device, comprising: forming a first intermetal dielectric (IMD) layer over the semiconductor substrate; forming a bottom electrode layer above the first IMD layer; forming a magnetic tunnel junction MTJ thin film stack above the bottom electrode layer; forming a first top electrode layer over the MTJ thin film stack; forming a protection mask covering a first region of the first top electrode layer, wherein a second region of the first top electrode layer is not covered by the protection mask; forming a second top electrode layer over the protection mask and the first top electrode layer; as well as The second top electrode layer, the first top electrode layer, the MTJ film stack, the bottom electrode layer and the first IMD layer are patterned using an ion beam etching (IBE) process to form a magnetoresistive random access memory (MRAM) cell, wherein the protection mask is etched during the IBE process, the IBE process etches the protection mask at a first etching rate, and the IBE process etches the first top electrode layer at a second etching rate, and the first etching rate is less than the second etching rate.

2. The method according to claim 1, wherein: Forming the protection mask comprises: depositing a mask layer on the first region and the second region of the first top electrode layer using a chemical vapor deposition process using tetraethyl orthosilicate (TEOS) as a precursor; and The mask layer is patterned to remove a portion of the mask layer above the second region of the first top electrode layer.

3. The method according to claim 1, wherein: The MRAM cell is formed by the first region of the first top electrode layer, and the MRAM cell comprises: A bottom electrode comprising a portion of the bottom electrode layer remaining after the IBE process; an MTJ stack, including a portion of the MTJ thin film stack remaining after the IBE process; and A top electrode comprising portions of the first top electrode layer and the second top electrode layer remaining after the IBE process, wherein the IBE process removes all of the protective mask.

4. The method according to claim 1, wherein: The MRAM cell is formed by the second region of the first top electrode layer, and the MRAM cell comprises: A bottom electrode comprising a portion of the bottom electrode layer remaining after the IBE process; an MTJ stack, including a portion of the MTJ thin film stack remaining after the IBE process; and A top electrode includes the first top electrode layer, the second top electrode layer, and a portion of the protection mask remaining after the IBE process.

5. The method according to claim 1, further comprising: The IBE process is used to pattern a first groove and a second groove in the first IMD layer, wherein the first groove is in a portion of the first IMD layer below the first region of the first top electrode layer, and the second groove is in a portion of the first IMD layer below the second region of the first top electrode layer, and the second groove is deeper than the first groove.

6. The method according to claim 5, further comprising: A third groove is patterned in the first IMD layer by using the IBE process, wherein the third groove is disposed below the second region of the first top electrode layer, and the third groove is deeper than the first groove and the second groove.

7. The method according to claim 1, further comprising: patterning the MTJ thin film stack, the bottom electrode layer, and the first IMD layer using the IBE process to form a resistor; forming a second IMD layer over the resistor; as well as A conductive feature is formed that extends through the second IMD layer to contact the resistor.

8. The method according to claim 1, wherein: A ratio of the first etching rate to the second etching rate is in a range of 1:1 to 1:2.

5.

9. The method according to claim 1, wherein: The duration of performing the IBE process is in the range of 100 seconds to 600 seconds.

10. The method according to claim 1, wherein: The first region occupies 95% to 99% of the area of ​​the first top electrode layer.

11. A semiconductor device comprising: Semiconductor substrates, including active devices; A first intermetallic dielectric (IMD) layer, located above the semiconductor substrate; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode disposed over the first conductive feature; A first magnetic tunnel junction MTJ stack, located above the first bottom electrode; A first top electrode comprising: A first conductive layer, located above the first MTJ stack; a dielectric layer located above the first conductive layer; and a second conductive layer, located above the dielectric layer; a second IMD layer located above the first top electrode; and a second conductive feature extending through the second IMD layer, the second conductive feature contacting the first top electrode, a third conductive feature extending through the first IMD layer; a second bottom electrode disposed over the third conductive feature; a second MTJ stack located above the second bottom electrode; The second top electrode comprises: A third conductive layer located above the second MTJ stack; and a fourth conductive layer, located above the third conductive layer; and a fourth conductive feature extending through the second IMD layer, the fourth conductive feature contacting the second top electrode, wherein the second IMD layer is located above the second top electrode, and The combined thickness of the third conductive layer and the fourth conductive layer is equal to the combined thickness of the first conductive layer, the dielectric layer and the second conductive layer.

12. The device according to claim 11, further comprising: A spacer is disposed on sidewalls of the first conductive layer, the second conductive layer, the third conductive layer, the fourth conductive layer, the dielectric layer, the first MTJ stack, the second MTJ stack, the first bottom electrode, and the second bottom electrode.

13. The device according to claim 11, further comprising: An interface oxide layer is located at the interface between the third conductive layer and the fourth conductive layer, and the interface oxide layer is flat.

14. The device according to claim 11, further comprising: An interface oxide layer is located at the interface between the third conductive layer and the fourth conductive layer, and the interface oxide layer is uneven.

15. The device according to claim 11, further comprising: A third IMD layer, located above the semiconductor substrate, the third IMD layer being adjacent to the first IMD layer; a third conductive feature extending through the third IMD layer, the third conductive feature being electrically connected to the active device; and A fourth conductive feature extends through the second IMD layer, the fourth conductive feature contacting the third conductive feature.

16. A semiconductor device comprising: Semiconductor substrates, including active devices; An interlayer dielectric ILD layer, located above the semiconductor substrate; A first intermetal dielectric IMD layer, located above the ILD layer; a first conductive feature extending through the first IMD layer, the first conductive feature being electrically connected to the active device; a first bottom electrode disposed over the first conductive feature; A first magnetic tunnel junction MTJ stack, located above the first bottom electrode; A first top electrode comprising: A first conductive layer located above the first MTJ stack; and a second conductive layer, located above the first conductive layer; a spacer disposed on sidewalls of the first conductive layer, the second conductive layer, the first MTJ stack, and the first bottom electrode; a second IMD layer having a first portion and a second portion, the first portion being located above the ILD layer and the second portion extending at least partially into the ILD layer; and a second conductive feature extending through the first portion of the second IMD layer, the second conductive feature being electrically connected to the active device; a third conductive feature extending through the first IMD layer; a second bottom electrode disposed over the third conductive feature; a second MTJ stack located above the second bottom electrode; The second top electrode comprises: a third conductive layer, located above the second MTJ stack; a dielectric layer, located above the third conductive layer; a fourth conductive layer located above the dielectric layer; and The combined thickness of the first conductive layer and the second conductive layer is equal to the combined thickness of the third conductive layer, the dielectric, and the fourth conductive layer.

17. The device according to claim 16, wherein The second portion of the second IMD layer has a rounded bottom surface.

18. The device according to claim 16, further comprising: a resistor disposed on a portion of the first IMD layer, the second IMD layer contacting a top surface of the resistor; as well as A fourth conductive feature extends through the first portion of the second IMD layer, the fourth conductive feature contacting the top surface of the resistor.

19. The device according to claim 16, wherein The first top electrode further comprises: a dielectric feature disposed between a portion of the first conductive layer and a portion of the second conductive layer; and An interface oxide layer is located at the interface between the first conductive layer and the second conductive layer.