Methods for interconnection schemes
By cutting metal lines in semiconductor integrated circuits to form metal islands and forming low dielectric layers and conical trenches therein, the gap problem of filling metal layers in small trenches is solved, and the formation quality and circuit performance of metal islands are improved .
Patent Information
- Application Number
- CN202110618776.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2015-07-20
- Filing Date
- 2015-11-30
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2035-11-30
AI Technical Summary
During the manufacturing process of semiconductor integrated circuits, when short-length metal wires (metal islands) are formed, there is a problem of gaps in the metal layer being filled in small trenches, resulting in high resistance and reliability problems, and it is difficult for existing methods to effectively reduce the dielectric layer. Damage to the process.
By forming the first and second trenches, the metal wires are cut to form metal islands and a low dielectric layer is formed therebetween, avoiding defects in filling the metal layer in the small trenches, exposing the metal wire portions using a patterned hard mask layer Etch, forming the second and third trenches of the tapered sidewalls, and finally a second dielectric layer is deposited within these trenches to provide electrical isolation.
The gap problem of filling the metal layer in small trenches is effectively avoided, the process damages to the low dielectric layer is reduced, and the formation quality and circuit performance of the metal island are improved.
Smart Images

Figure CN113314461B_ABST
Abstract
Description
[0001] Information about divisional applications
[0002] This application is a divisional application of an application with a filing date of November 30, 2015, application number “201510853081.4” and invention name “Method for interconnection scheme”. Technical Field
[0003] The present invention relates to a method and related apparatus for a semiconductor interconnection scheme. Background Art
[0004] The semiconductor integrated circuit (IC) industry has experienced a period of rapid growth. Technological advances in IC design and materials have produced several generations of semiconductor integrated circuits, each with smaller and more complex circuits than the previous generation. In the evolution of semiconductor integrated circuits, functional density (i.e., the number of interconnected devices per chip area) has generally increased, while geometric size (i.e., the smallest device (or line) that can be manufactured by the manufacturing process) has decreased.
[0005] Such scaling down processes have the benefit of increasing production efficiency and reducing associated costs. In addition, such scaling down processes also increase the complexity of IC processing and manufacturing. Similar developments are needed in IC processing and manufacturing to achieve these advanced processes. As semiconductor devices such as metal oxide semiconductor field effect transistors (MOSFETs) are reduced in size through various techniques, the dielectric materials associated with the interconnections between their wires and the wiring between transistors and other devices play a more important role in improving the performance of the IC. Although existing methods for manufacturing IC equipment have generally met their intended purposes, they are not completely satisfactory in all aspects. For example, forming metal lines with short lengths, or simply metal islands, faces great challenges. Summary of the invention
[0006] The present invention provides a method, which includes: forming a first dielectric layer on a substrate; forming a first trench in the first dielectric layer; forming a metal line in the first trench; removing a first portion of the metal line to form a second trench, and removing a second portion of the metal line to form a third trench, wherein the third portion of the metal line is disposed between the second trench and the third trench; and forming a second dielectric layer in the second trench and the third trench.
[0007] The present invention also provides a method, which includes: forming a first dielectric layer on a substrate; forming a metal line in the first dielectric layer; forming a patterned hard mask layer on the metal line, wherein the patterned hard mask layer has a first opening and a second opening exposing the metal line; removing the exposed portion of the metal line through the first opening and the second opening respectively to form a first trench and a second trench; and forming a second dielectric layer in the first trench and the second trench.
[0008] The present invention further provides a device comprising: a first metal line disposed on a substrate along a first direction; and a second metal line along the first direction and aligned to the first metal line, wherein the sidewall of the second metal line has a tapered sidewall profile along the first direction, wherein the bottom side of the second metal line along the first direction is wider than the top side of the second metal line.
[0009] The present invention provides a method for forming small metal islands. The method uses cutting metal lines to form metal islands to avoid small gap filling defects. The method uses a scheme that includes first forming metal lines, including metal islands, and then forming a low-k dielectric layer to minimize process-induced damage on the low-k dielectric layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] To assist the reader in achieving the best understanding, it is recommended that the present invention be read in conjunction with the accompanying drawings and the following detailed description. It should be noted that, in accordance with standard practice in the industry, the features are not drawn to scale. In fact, for the sake of clarity of discussion, the dimensions of the features may be arbitrarily enlarged or reduced.
[0011] Figure 1 Flowchart of an example method for manufacturing a semiconductor device constructed according to some embodiments.
[0012] Figure 2A , 3A , 4A, 4C, 5A, 6A, 6C, and 7A are top views of example semiconductor devices according to some embodiments.
[0013] Figure 2B For example semiconductor devices according to some embodiments, Figure 2A Cross-sectional view along line AA.
[0014] Figure 3B For example semiconductor devices according to some embodiments, Figure 3A Cross-sectional view along line BB in FIG.
[0015] Figure 4B For example semiconductor devices according to some embodiments, Figure 4A Cross-sectional view along line BB in FIG.
[0016] Figure 4D For example semiconductor devices according to some embodiments, Figure 4C Cross-sectional view along line BB in FIG.
[0017] Figure 5B For example semiconductor devices according to some embodiments, Figure 5A Cross-sectional view along line AA.
[0018] Figure 6B For example semiconductor devices according to some embodiments, Fig. 6A Cross-sectional view along line AA.
[0019] Fig.6D For example semiconductor devices according to some embodiments, Figure 6C Cross-sectional view along line AA.
[0020] Figure 7B and Figure 7C For example semiconductor devices according to some embodiments, Fig. 7A Cross-sectional view along line AA. DETAILED DESCRIPTION
[0021] The following disclosure provides several different embodiments or examples for implementing different features of the provided subject matter. To simplify the present disclosure, specific examples of various devices and layouts are described below. Of course, these are merely examples and are not intended to be limiting. For example, the first feature in this description is based on the second feature, and the formation of the second feature following the second feature may include some embodiments in which the first feature and the second feature are formed in direct contact; it may also include some embodiments in which additional features are formed between the first feature and the second feature so that the first feature and the second feature are formed in indirect contact. In addition, the present disclosure may repeat reference values and / or letters in various examples. This repetition is for the purpose of simplicity and clarity and does not itself indicate the relationship between the various embodiments and / or arrangements discussed.
[0022] Additionally, to facilitate the description herein, spatially relative terms, such as "below," "below," "above," "upper," etc., are used herein. The terms are used to describe one element, or a relationship of one feature to another element(s), or feature(s) depicted in a figure. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should be interpreted accordingly.
[0023] Figure 11 is a flow chart of a method 100 for fabricating one or more semiconductor devices according to some embodiments. Figure 2A to 2B , Figures 3A to 3B , Figures 4A to 4D , Figures 5A to 5B , Figures 6A to 6D and Figures 7A to 7C The method 100 is discussed in detail below with reference to the semiconductor device 200 shown in FIG.
[0024] Figure 1 1 is a flow chart of an embodiment of a method 100 for fabricating one or more semiconductor devices according to aspects of the present disclosure. Figures 2A to 7B The method 100 is discussed in detail below by taking the semiconductor device 200 shown in FIG. 1 as an example.
[0025] See also Figure 1 and Figure 2A to 2B , the method 100 begins with providing a substrate 210 in step 102. The substrate 210 can be a bulk silicon substrate. Alternatively, the substrate 210 can include: an elemental semiconductor, such as silicon or germanium in a crystal structure; a compound semiconductor, such as silicon germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide and / or indium antimonide; or a combination of the above. Other possible substrates 210 also include silicon-on-insulator (SOI) substrates. SOI substrates are manufactured using separation by implantation of oxygen (SIMOX), wafer bonding and / or other suitable methods.
[0026] Some examples of the substrate 210 further include an insulating layer. The insulating layer includes any suitable material, including silicon oxide, sapphire, and / or combinations thereof. An example of an insulating layer is a buried oxide layer (BOX). The insulating layer may be formed by any suitable process, such as implantation (e.g., SIMOX), oxidation, deposition, and / or other suitable processes. In some examples of the semiconductor device 200, the insulating layer is a component (e.g., layer) of a silicon-on-insulator substrate.
[0027] The substrate 210 may also include various doped regions. The doped regions may be doped with p-type dopants, such as boron or boron difluoride (BF 2 ); n-type dopant, such as phosphorus or arsenic; or a combination of the above. The doped region can be formed directly on the substrate 210 in a P-well structure, an N-well structure, a double-well structure, or a raised structure. The substrate 210 may further include various active regions, such as a region arranged for an N-type metal oxide semiconductor transistor device and a region arranged for a P-type metal oxide semiconductor transistor device.
[0028] The substrate 210 may also include various isolation features. The isolation features separate various device regions in the substrate 210. The isolation features include different structures formed using different processing techniques. For example, the isolation features may include shallow trench isolation (STI) features. The formation of STI may include etching trenches in the substrate 210 and filling the trenches with an insulator material such as silicon oxide, silicon nitride, or silicon oxynitride. The filled trenches may have a multi-layer structure, such as a thermal oxide liner layer with a silicon nitride filled trench. Chemical mechanical polishing (CMP) may be performed to polish back the excess insulating material and planarize the top surface of the isolation features.
[0029] The substrate 210 may also include a gate stack, which is formed by a dielectric layer and an electrode layer. The dielectric layer may include an interfacial layer (IL) and a high-k (HK) dielectric layer, and the high-k dielectric layer is deposited by a suitable technique, such as chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), thermal oxidation, a combination of the above or other suitable techniques. The electrode layer may include a single layer or multiple layers formed by ALD, PVD, CVD or other suitable processes, such as a metal layer, a liner layer, a wetting layer and an adhesion layer.
[0030] The substrate 210 may also include source / drain (S / D) features separated by the gate stack. The S / D features may include germanium (Ge), silicon (Si), gallium arsenide (GaAs), aluminum gallium arsenide (AlGaAs), silicon germanium (SiGe), gallium arsenide phosphide (GaAsP), gallium antimony (GaSb), indium antimony (InSb), indium gallium arsenide (InGaAs), indium arsenide (InAs), and / or other suitable materials. The S / D features may be formed by epitaxial growth processes such as CVD, VPE and / or UHV-CVD, molecular beam epitaxy, and / or other suitable processes.
[0031] The substrate 210 may also include conductive features. The conductive features may include electrodes, capacitors, resistors, or portions of resistors. The conductive features may also include portions of an interconnect scheme, a portion of which includes a multi-layer interconnect (MLI) structure and an interlevel dielectric (ILD) layer integrated with the MLI structure, the interconnect scheme providing electrical wiring to couple various devices in the substrate 210 to input / output power and signals. The interconnect scheme includes various metal lines, contacts, and via features (or via plugs). The metal lines provide horizontal electrical wiring. The contacts provide vertical connections between the silicon substrate and the metal lines, while the via features provide vertical connections between metal lines in different metal layers. The conductive features may be formed by a process including photolithography, etching, and deposition.
[0032] In the present embodiment, the substrate 210 includes a first dielectric layer 220. The first dielectric layer 220 may include silicon oxide, a dielectric material having a dielectric constant (k) less than that of thermal silicon oxide, and therefore referred to as a low-k dielectric material layer, such as tetraethylorthosilicate (TEOS) oxide, undoped silicate glass or doped silicon oxide, such as borophosphosilicate glass (BPSG), fused silica glass (FSG), phosphosilicate glass (PSG), boron doped silicon glass (BSG) and / or other suitable dielectric materials. The first dielectric layer 220 may include a single layer or multiple layers. The first dielectric layer 220 may be deposited by CVD, ALD or spin coating.
[0033] Multilayer interconnects are typically formed on a substrate 210 to connect various devices (transistors, resistors, capacitors, etc.) to form an integrated circuit. In a typical interconnect scheme, metal wires (e.g., copper wires) are laid in a first dielectric layer 220 and connected from one layer to another through vias. Copper wires and vias are typically made using a single damascene process or a dual damascene process. In such a process, the first dielectric layer 220 is patterned to form a groove, then the groove is filled with excess copper, and chemical-mechanical planarization (CMP) is used to remove excess copper, thereby forming copper wires in the groove. Subsequently, another dielectric layer is formed on the dielectric layer below it, and the above process is repeated to form vias and upper copper wires.
[0034] The need for metal lines of various lengths is very common, especially as devices are scaled down. Generally, metal lines are first formed by forming trenches of various lengths and then filling these trenches with metal layers. However, as the size of the trenches becomes smaller, the gap filling ability of the metal material is limited, and the quality and reliability of the gap filling are also challenged. This results in the formation of voids in the metal lines, which can cause high resistance problems and device reliability issues. In the process of forming metal lines, minimizing process-induced damage to the dielectric layer is also faced with challenges. In the present embodiment, the method 100 provides for forming metal lines (or islands) while avoiding many of the challenges of filling metal layers in small trenches.
[0035] See also Figure 1 and Figures 3A to 3B , the method 100 proceeds to step 104, where a first trench 310 is formed in the first dielectric layer 220. The first trench 310 is formed along Figure 3A . In some embodiments, the first trench 310 is formed by forming a patterned photoresist layer on the first dielectric layer 220 and then etching the first dielectric layer through the patterned photoresist layer. An example of a photolithography process may include forming a photoresist layer, exposing the photoresist layer through a photolithography exposure process, performing a post-exposure baking process, and developing the photoresist layer to form a patterned photoresist layer. In another embodiment, the first trench 310 is formed by depositing a HM layer on the second dielectric layer 220, depositing a photoresist layer on the HM layer, patterning the photoresist layer, then etching the HM layer through the patterned photoresist layer to pattern it, and then etching the dielectric layer 220 through the patterned HM layer.
[0036] The etching process may include selective wet etching, selective dry etching, and / or a combination thereof. For example, the etching process includes a plasma dry etching process using a fluorine-based chemistry, such as CF 4 , SF 6 , CH 2 F 2 , CH 2 F 2 and / or C 2 F 6 Etc. The respective etching processes may adjust various etching parameters, such as the etchant used, etching temperature, etching solution concentration, etching pressure, etchant flow rate, and / or other suitable parameters.
[0037] After forming the first trench 310, the patterned HM is removed by a suitable etching process. In an example, the patterned HM is a photoresist pattern, and the patterned HM is removed by wet stripping and / or plasma ashing.
[0038] See also Figure 1 and FIG. 4A to FIG. 4B , the method 100 proceeds to step 106, forming a metal layer 405 in the first groove 310. In the present embodiment, the metal layer 405 is deposited in the first groove 310. The metal layer 405 may include copper (Cu), tin (Sn), silver (Ag), gold (Au), palladium (Pd), platinum (Pt), rhenium (Re), iridium (Ir), ruthenium (Ru), osmium (Os), copper manganese (CuMn), copper aluminum (CuAl), copper titanium (CuTi), copper vanadium (CuV), copper chromium (CuCr), copper silicon (CuSi), copper niobium (CuNb) or other suitable metals. The metal layer 405 may be deposited by PVD, CVD, ALD, electrochemical plating (Electrochemical plating, ECP) or other appropriate treatments. In an embodiment, the metal layer 405 includes a copper layer deposited by PVD. In an embodiment, the metal layer 405 includes a copper seed layer deposited by PVD and a bulk copper layer by electroplating. In various other examples, copper deposition may be achieved by other techniques, such as CVD or MOCVD. A copper reflow process may additionally be used to enhance the copper fill profile.
[0039] In some embodiments, an electrical metal diffusion barrier layer (not shown) is first deposited in the first trench 310, and the metal layer 405 is deposited on the barrier layer. The barrier layer may include tantalum (Ta) or tantalum nitride (TaN) and a metal conductor, which may be copper (Cu), aluminum (Al), tungsten (W), cobalt (Co) or other suitable metals. In an embodiment, the barrier layer includes one or more layers of materials. The barrier layer is deposited by PVD, MOCVD or other suitable techniques.
[0040] Next, see Figure 4C to Figure 4D A CMP process is performed to planarize the top surface of the device 200 to remove the excess metal layer 405 on the first dielectric layer 220. The metal layer 405 remains in the first trench 310 to form the metal line 410. As a result of the CMP process, the top surface of the dielectric layer 220 and the top surface of the metal line 410 can form a substantially coplanar structure.
[0041] The metal lines 410 may be coupled to active and / or passive elements in the substrate 210 through other underlying interconnect schemes or through terminals (eg, source, drain, and gate contacts) of the active and / or passive elements.
[0042] See also Figure 1 and FIG. 5A to FIG. 5B , the method 100 proceeds to step 108, forming a hard mask 510 (or cutting a hard mask) and a dielectric layer 220 on the metal line 410. The hard mask 510 has a first opening 520 and a second opening 525 to expose a first portion and a second portion of the metal line 410, respectively, which are marked with reference numerals 410A and 410B, respectively. In this embodiment, the first opening 520 is away from the second opening 525 along the direction of the AA line by a distance, and the distance is selected as a target length L of the future metal island, as described below. In some embodiments, the hard mask 510 defines the first opening 520 and the second opening 525 that are wider than the metal line 410, and a portion of the first dielectric layer 220 is also exposed in the first opening 520 and the second opening 525, which are marked with reference numerals 220A. In other embodiments, the first opening 520 and the second opening 525 have a larger width so that they extend adjacent to the first dielectric layer 220A to have more benefits.
[0043] In some embodiments, the hard mask 510 is a patterned photoresist layer. In another embodiment, the hard mask 510 is formed by a process comprising depositing a hard mask layer, forming a patterned photoresist layer on the hard mask layer, and etching the hard mask layer using the patterned photoresist layer as an etching mask.
[0044] See also Figure 1 and FIG. 6A to FIG. 6B, the method 100 proceeds to step 110, which removes the exposed first portion 410A and the second portion 410B of the metal line 410 through the first opening 520 and the second opening 525, respectively, to form a second trench 610 and a third trench 620, respectively. The third portion of the metal line 410 located between the first opening 520 and the second opening 525 is protected by the hard mask 520 during the etching process. The etching process may include wet etching, dry etching and / or a combination of the above. In some embodiments, the metal line 410 is a copper line, and the copper etching gas used in reactive ion etching (RIE) includes CxHy, CxFy, CxHyFz or a combination of the above. The value of the subscript x, y or z is greater than 0 and less than 6. In some embodiments, the copper etching gas used in reactive ion etching (RIE) further includes carbon monoxide (CO) and oxygen (O 2 ), and nitrogen (N 2 ) and argon (Ar). In a further example, the etching temperature (substrate temperature) ranges from about 20°C to about 120°C. In another example, the etching temperature ranges from about 20°C to about 80°C.
[0045] In some embodiments, the second trench 610 and the third trench 620 are both formed with a tapered sidewall profile so that along the direction of line AA, the second trench 610 and the third trench 620 have a first width w1 greater than a second width w2, and the second width w2 is the width of the bottom opening of the second trench 610 and the third trench 620.
[0046] In some embodiments, a wet etching process may be used instead of or in addition to remove the exposed first portion 410A and the second portion 410B. The corresponding etchant includes HCl, FeCl 3 and H 2 In another embodiment, when the metal line 410 includes other suitable metals, such as aluminum or tungsten, other etching gases may also be used.
[0047] In some embodiments, the metal line 410 includes a barrier layer surrounding the metal line 410A. In this case, the etching process further includes etching the barrier layer. In an embodiment, the etching process to remove the exposed metal line 410A includes: a first etching sub-step as described above to etch the metal layer 405; and a second etching sub-step to etch the barrier layer, such as dry etching and / or wet etching. For example, the second etching sub-step to etch the barrier layer includes using a CxFx, N 2 (or Ar), CxHy, and Cl 2In another embodiment, wet etching is used to etch the barrier layer, and the corresponding etchant contains NH 4 OH, H 2 O 2 and H 2 O's standard cleaning solution (SC1).
[0048] As mentioned above FIG. 5A to FIG. 5B As discussed, in some embodiments, a portion of the dielectric layer 220A is exposed within the first opening 520 and the second opening 525. In this case, the etching process is appropriately selected to etch the exposed first portion 410A and the second portion 410B without substantially etching the exposed dielectric layer 220A. In this embodiment, the exposed portion of the dielectric layer 220A within the first opening 520 and the second opening 525 acts as a sub-etching mask during the etching process. With appropriate etching selectivity, the self-aligned characteristic is used to remove the exposed first portion 410A and the second portion 410B, which can reduce the limitation of the etching process.
[0049] See also Figure 6C and Fig.6D After removing the exposed first portion 410A and the second portion 410B, the hard mask 510 is removed by etching. In an example, the hard mask 510 is a photoresist pattern, and the hard mask 510 is removed by moisture and / or plasma ashing. As shown in the figure, the metal line 410 is divided into a plurality of sub-metal lines, which include a metal island 410I, and the metal island 410I is a third portion of the metal line 410 between the first opening 520 and the second opening 525. Figure 5A and 5B As shown in the figure, the first portion 410A of the metal line 410 defines a first sidewall 615 of the second trench 610, the metal island 410I defines a second sidewall 616 of the second trench 610, and a third sidewall 625 of the third trench 620. The second portion 410B of the metal line 410 defines a fourth sidewall 626 of the third trench 620.
[0050] As mentioned above FIG. 5A to FIG. 5B As discussed, in some embodiments, the second trench 610 and the third trench 620 have tapered sidewall profiles. In this case, the metal island 410I has a top length L along the line AA. T , the top length L T Less than its bottom length L BAt the same time, each of the metal lines 410 located on each side of the metal island 410I has a length L greater than its top. D Bottom length L C .
[0051] In this embodiment, the metal island 410I is formed by cutting the metal line 410, rather than filling a metal layer in a small trench to form a metal island. This method avoids gap filling problems, such as forming a gap in the metal island 410I, or using a poor metal filling step to cover the sidewalls and bottom of the trench.
[0052] See also Figure 1 and Figures 7A to 7B , the method 100 proceeds to step 112, by depositing a second dielectric layer 710 on the first dielectric layer 220, the metal island 410I and the metal line 410, including filling the second trench 610 and the third trench 620 to provide electrical isolation between the metal island 410I and the metal line 410. The metal island 410I is embedded in the second dielectric layer 710. In an embodiment, the second dielectric material layer 710 has a similar composition to the first dielectric material layer 220. For example, the second dielectric layer 710 includes a low-k dielectric material, silicon oxide or other suitable dielectric material layer. The second dielectric layer 710 has a material with a dielectric constant (k) lower than the dielectric constant of silicon dioxide to reduce the capacitance component and the crosstalk between the metal lines to minimize time delay and power consumption. The second dielectric layer 710 can be deposited by CVD, ALD or spin coating.
[0053] like Figures 7A to 7B As shown, the second dielectric layer 710 substantially fills the second trench 610 and the third trench 620. As shown in the example, the second dielectric layer 710 is deposited by a spin-on dielectric (SOD) process to substantially fill the second trench 610 and the third trench 620.
[0054] In another embodiment, the second dielectric layer 710 is disposed in the second trench 610 and the third trench 620, which includes a gap (or air gap) 715 to further reduce the average dielectric constant and improve the isolation efficiency. Figure 7C As shown. The air gap 715 can be formed by selecting and adjusting an appropriate deposition process to form the second dielectric layer 710. In an embodiment, the second dielectric layer 710 is deposited by CVD, and the CVD deposition is adjusted to form the air gap 715. For example, when the CVD deposition rate is adjusted to be higher so that the second dielectric layer 710 is closed before the second trench 610 and the third trench 620 are completely filled, the air gap 715 is formed.
[0055] In this embodiment, the second dielectric layer 710 is deposited after the metal islands 410I and the metal lines 410 are formed. This advantageously prevents the second dielectric layer 710 from experiencing plasma damage. During the formation of the metal layer 405 and the subsequent etching of the metal lines 410, the plasma damage may occur to the second dielectric 710. The plasma damage reduces the low-K dielectric constant value and causes poor capacitance performance of the circuit. The deposition of the second dielectric layer 710 is also accompanied by the ability to self-form air voids in the second trench 610, as described above. Figure 7C The content discussed.
[0056] Other steps are provided before or during the method 100 , and some of the steps described may be replaced, eliminated, or moved for other embodiments of the method 100 .
[0057] The semiconductor device 200 described may include additional features that may be formed by subsequent processing. For example, various vias or lines and multi-layer interconnect functions (e.g., metal layers and interlayer dielectrics) are formed on the substrate 210. For example, the multi-layer interconnects include vertical interconnects, such as conventional vias or lines; and horizontal interconnects, such as metal lines. The various interconnect features may implement various conductive materials, including copper, tungsten, and / or silicide. In an example, a copper-related multi-layer interconnect scheme is formed using single damascene and / or dual damascene processes.
[0058] Based on the above, it can be concluded that the present invention provides a method for forming small metal islands. The method uses cutting metal lines to form metal islands to avoid small gap filling defects. The method uses a scheme that includes first forming metal lines, including metal islands, and then forming a low-k dielectric layer to minimize the damage caused by the process on the low-k dielectric layer.
[0059] The present disclosure provides a plurality of different embodiments for manufacturing semiconductor devices, which provide one or more improvements over existing methods. In an embodiment, a method for manufacturing a semiconductor device includes: forming a first dielectric layer on a substrate; forming a first trench in the first dielectric layer; forming a metal line in the first trench; removing a first portion of the metal line to form a second trench, and removing a second portion of the metal line to form a third trench. The third portion of the metal line is disposed between the second trench and the third trench. The method also includes forming a second dielectric layer in the second trench and the third trench.
[0060] In another embodiment, a method includes forming a first dielectric layer on a substrate; forming a metal line in the first dielectric layer; and forming a patterned hard mask layer on the metal line. The patterned hard mask layer has a first opening and a second opening exposing the metal line. The method also includes: removing the exposed portion of the metal line through the first opening and the second opening, respectively, to form a first trench and a second trench; and forming a second dielectric layer in the first trench and the second trench.
[0061] In another embodiment, a semiconductor device includes: a first metal line disposed on a substrate along a first direction; and a second metal line along the first direction and aligned to the first metal line. A sidewall of the second metal line has a tapered sidewall profile along the first direction. A bottom side of the second metal line along the first direction is wider than a top side of the second metal line.
[0062] The foregoing summarizes the features of several embodiments so that those skilled in the art can better understand the various aspects of the present invention. Those skilled in the art will appreciate that they can easily use the present invention as a basis for designing or modifying other processes and structures for achieving the same purpose and / or achieving the same advantages of the embodiments described herein. Those skilled in the art will also appreciate that such equivalent constructions do not depart from the spirit and scope of the present invention, and they can make various changes, substitutions and modifications without departing from the spirit and scope of the present invention.
Claims
1. A method for an interconnection scheme, comprising: forming a first dielectric layer on the substrate; forming a first trench in the first dielectric layer; forming a metal line in the first trench; forming a hard mask having a first opening and a second opening on the metal line to expose a first portion and a second portion of the metal line, respectively, wherein a portion of the first dielectric layer is exposed in the first opening and the second opening; removing the first portion of the metal line to form a second trench, and removing the second portion of the metal line to form a third trench, wherein the third portion of the metal line is disposed between the second trench and the third trench, wherein the portion of the first dielectric layer is not substantially etched during the removal of the first portion and the second portion of the metal line; as well as A second dielectric layer is formed in the second trench and the third trench and on the third portion of the metal line.
2. The method of claim 1 , wherein after removing the first portion of the metal line to form the second trench, the first portion of the metal line defines a first sidewall of the second trench and the third portion of the metal line defines a second sidewall of the second trench, After the second portion of the metal line is removed to form the third trench, the second portion of the metal line defines a third sidewall of the second trench and the third portion of the metal line defines a fourth sidewall of the third trench.
3. The method according to claim 1, wherein the method of removing the first portion of the metal line to form the second trench and removing the second portion of the metal line to form the third trench comprises: The hard mask is removed. 4 . The method of claim 1 , wherein forming the second dielectric layer in the second trench and the third trench comprises forming air voids in the second dielectric layer. 5 . The method of claim 1 , wherein the forming the metal line comprises forming a metal line comprising copper, the metal line comprising copper being selected from the group consisting of copper, copper manganese, copper aluminum, copper silicon, and combinations thereof.
6. The method of claim 5 , wherein removing the first portion and the second portion of the metal line comprises performing a plasma etching process, the plasma etching process comprising at least one of a hydrocarbon, a fluorocarbon, and a fluoroalkane, one of carbon monoxide and oxygen, and one of nitrogen and argon. 7 . The method of claim 1 , wherein the third portion of the metal line includes a top portion having a first width and a bottom portion having a second width different from the first width. The method of claim 7 , wherein the second width is greater than the first width.
9. A method for an interconnection scheme, comprising: forming a first dielectric layer on the substrate; forming a metal line in the first dielectric layer; forming a patterned hard mask layer on the metal line, wherein the patterned hard mask layer has a first opening and a second opening exposing the metal line, wherein a portion of the first dielectric layer is exposed in the first opening and the second opening; removing exposed portions of the metal line through the first opening and the second opening, respectively, to form a first trench, a second trench, and a metal island between the first trench and the second trench, wherein the portion of the first dielectric layer is not substantially etched during the removal of the exposed portions of the metal line; as well as A second dielectric layer is formed in the first trench, the second trench and on the metal island.
10. The method of claim 9, wherein forming the metal line in the first dielectric layer comprises: forming a first trench in the first dielectric layer; filling the first trench with a metal layer; as well as The metal layer is planarized.
11. The method of claim 9, wherein forming the metal line in the first dielectric layer comprises forming a metal line comprising copper, the metal line comprising copper being selected from the group consisting of copper, copper manganese, copper aluminum, copper silicon, and combinations thereof. 12 . The method of claim 9 , wherein each of the first dielectric layer and the second dielectric layer comprises a low dielectric constant dielectric material. 13 . The method of claim 9 , wherein forming the second dielectric layer in the first trench and the second trench comprises forming air voids in the second dielectric layer.
14. The method of claim 9, wherein the metal island comprises a top portion having a first width and a bottom portion having a second width different from the first width. The method of claim 14 , wherein the second width is greater than the first width.
16. A method for an interconnect scheme, comprising: forming a first dielectric layer on the substrate; forming a first trench in the first dielectric layer; forming a metal line in the first trench; forming a patterned hard mask layer on the metal line to expose a portion of the metal line and a portion of the first dielectric layer; etching the portion of the metal line to form a second trench, wherein the portion of the first dielectric layer is not substantially etched during etching the portion of the metal line; as well as A second dielectric layer is formed in the second trench.
17. The method of claim 16, wherein forming the second trench comprises etching the portion of the metal line, the etching comprising at least one of a hydrocarbon, a fluorocarbon, and a fluoroalkane, one of carbon monoxide and oxygen, and one of nitrogen and argon.
18. The method of claim 16, wherein the first dielectric layer and the second dielectric layer comprise a low dielectric constant dielectric material.
19. The method of claim 16, wherein forming the second dielectric layer in the second trench comprises forming air voids in the second dielectric layer.
20. The method of claim 16, wherein the forming the metal line comprises forming a metal line comprising copper, the metal line comprising copper being selected from the group consisting of copper, copper manganese, copper aluminum, copper silicon, and combinations thereof.