Printed wiring board and method for manufacturing the same
By using high specific conductivity metal foil patterns and liquid crystal polymer dielectric layers in printed wiring boards, combined with laser processing and lamination processes, the problems of high-frequency signal transmission loss and mechanical stress are solved, and more stable signal transmission is achieved and mechanical properties.
Patent Information
- Application Number
- CN202110182256.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-03-05
- Filing Date
- 2021-02-08
- Publication Date
- 2024-09-27
- Estimated Expiration
- 2041-02-08
AI Technical Summary
Existing printed wiring boards have high transmission losses and mechanical stress in high-frequency signal transmission, leading to deterioration of signal transmission characteristics and the risk of signal line breakage, especially under bending conditions.
Using a metal foil pattern with high specific conductivity and a liquid crystal polymer dielectric layer, the conductive holes are formed through laser processing and filled with conductive paste. The lamination process and heating and pressing technology are combined to form a printed wiring with a three-layer strip line structure. The plate is designed symmetrically in the thickness direction to reduce stress.
It effectively reduces the transmission loss of high-frequency signals, improves the mechanical stability and signal transmission characteristics of printed wiring boards, prevents signal line breakage, and is suitable for signal transmission of high-frequency communications and electronic equipment.
Smart Images

Figure CN113365415B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application is based on Japanese Patent Application No. 2020-037868 filed with the Japan Patent Office on March 5, 2020, and all the contents of the Japanese Patent Application are hereby incorporated by reference. Technical Field
[0003] The present invention relates to a printed wiring board and a method for manufacturing the same. Background Art
[0004] In recent years, with the miniaturization and high speed of electronic devices including smartphones, laptops, digital cameras and game consoles, the amount of information processing performed by the electronic devices has increased dramatically. Therefore, there is a tendency for the signal transmission speed of printed wiring boards used to transmit high-frequency signals to become increasingly faster. For example, from 2019, portable communication terminals such as smartphones began to shift to the next-generation communication standard 5G. In the 5G standard, signals with frequencies from several GHz to 20 to 30 GHz are used. Furthermore, by around 2022, the frequency of signals sent and received by communication terminals is expected to increase to around 50 GHz.
[0005] Generally speaking, as the frequency increases, the signal transmission loss increases. Therefore, it is increasingly important to suppress the transmission loss of the signal line.
[0006] In order to reduce signal transmission loss, it is desirable to use materials with excellent dielectric properties, including dielectric constant and dielectric loss tangent, in the dielectric layer of a printed wiring board. For example, Japanese Patent Application Publication Nos. 2011-66293 and 2007-96121 describe printed wiring boards using liquid crystal polymers (LCP). Summary of the invention
[0007] A printed wiring board according to an embodiment of the present invention comprises: a first dielectric layer having a first main surface and a second main surface opposite to the first main surface; a first adhesive layer formed on the first main surface; a first metal foil pattern formed on the first adhesive layer and constituting a signal line; and a second metal foil pattern formed on the second main surface and constituting a ground layer, the first metal foil pattern having a specific conductivity greater than the specific conductivity of the second metal foil pattern. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 It is a top view of the high-frequency signal transmission component according to the present embodiment.
[0009] Figure 2It is a plan view showing the inner layer signal lines and ground lines in region R of the printed wiring board according to the present embodiment.
[0010] Figure 3 It is along Figure 1 and Figure 2 A cross-sectional view of a line II printed wiring board.
[0011] Figure 4 yes Figure 3 Magnified view of area S.
[0012] Fig.5A1 , Figure 5A2 as well as Figure 5A3 The present invention is a cross-sectional view of a process for explaining the method for manufacturing a wiring base material of a printed wiring board according to the present embodiment.
[0013] Figure 5B1 , Figure 5B2 and Figure 5B3 Then Figure 5A3 A cross-sectional view of a process for explaining a method for manufacturing a wiring substrate of a printed wiring board according to the present embodiment.
[0014] Fig.5C1 , Fig.5C2 and Fig.5C3 Then Figure 5B3 A cross-sectional view of a process for explaining a method for manufacturing a wiring substrate of a printed wiring board according to the present embodiment.
[0015] Fig.6A1 , Fig.6A2 and Figure 6A3 The present invention is a cross-sectional view of a process for explaining the method for manufacturing a wiring base material of a printed wiring board according to the present embodiment.
[0016] Fig.6B1 , Figure 6B2 and Figure 6B3 Then Figure 5A3 A cross-sectional view of a process for explaining a method for manufacturing a wiring substrate of a printed wiring board according to the present embodiment.
[0017] Fig. 7A and Figure 7B It is a process cross-sectional view for explaining the lamination process of the printed wiring board of this embodiment.
[0018] Fig. 8A , Figure 8B , Figure 8C and Fig.8D The present invention is a cross-sectional view of a process for explaining a method for manufacturing a wiring base material of a printed wiring board in a modified example of the present embodiment.
[0019] Fig. 9A and Fig. 9BThe present invention is a cross-sectional view of a process for explaining a method for manufacturing a wiring base material of a printed wiring board in a modified example of the present embodiment.
[0020] Fig.10A1 and Fig.10A2 It is a process cross-sectional view for explaining the lamination process of the printed wiring board in the modification of this embodiment.
[0021] Fig.10B1 and Fig.10B2 Then Fig.10A2 A process cross-sectional view for explaining a punching process of a printed wiring board in a modified example of the present embodiment.
[0022] Fig.10C1 and Fig.10C2 Then Fig.10B2 A process cross-sectional view for explaining an interlayer connection process of a printed wiring board in a modified example of the present embodiment.
[0023] Fig.11A1 and Fig.11A2 The diagram is a cross-sectional view of a process for explaining a method for manufacturing a printed wiring board in a comparative example.
[0024] Fig.11B1 and Fig.11B2 Then Fig.11A2 A cross-sectional view of a process for explaining a method for manufacturing a printed wiring board in a comparative example. DETAILED DESCRIPTION
[0025] In the detailed description below, for the purpose of illustration, in order to provide a thorough understanding of the disclosed embodiments, many specific details are set forth. However, it is apparent that one or more embodiments may be implemented without these specific details. In other cases, in order to simplify drawing, well-known structures and devices are schematically shown.
[0026] Reference Fig.11A1 , Fig.11A2 , Fig.11B1 and Fig.11B2 The following describes a method for producing a printed wiring board in the comparative example. In this method, three single-sided copper-clad laminates are used to produce a printed wiring board having a three-layer stripline structure.
[0027] like Fig.11A1As shown, three wiring substrates (lower side, center, upper side) are prepared. The wiring substrate on the lower side is a single-sided copper-clad laminate on which a dielectric layer 110 and a copper foil 120 are bonded, and an adhesive layer 130 and a protective film 140 are sequentially laminated. In the wiring substrate in the center, an adhesive layer 230 and a protective film 240 are sequentially laminated on the resin surface of a single-sided copper-clad laminate including a bonded dielectric layer 210 and a copper foil 220. In the wiring substrate on the upper side, an adhesive layer 330 and a protective film 340 are sequentially laminated on the resin surface of a single-sided copper-clad laminate including a bonded dielectric layer 310 and a copper foil 320. In addition, in order to ensure the bonding strength between the copper foils 120, 220, 320 and the dielectric layers 110, 210, 310, the back surface of each copper foil is roughened. In addition, the copper foils 120 and 320 are patterned by a known manufacturing method to have a ground layer. Likewise, the copper foil 220 is patterned to have a signal line layer and a ground wiring layer.
[0028] Then, if Fig.11A2 As shown, conductive paste 150, 250, 350 is filled into the predetermined portions of the three wiring substrates. Specifically, conductive holes are formed in the predetermined portions of the wiring substrates by laser processing. Then, screen printing is performed using the protective films 140, 240, 340 as masks, thereby filling the conductive holes with conductive paste.
[0029] Then, if Fig.11B1 As shown, the protective films 140, 240, and 340 are peeled off from the respective wiring base materials. In this way, the tops of the conductive pastes 150, 250, and 350 filled in the conduction holes protrude.
[0030] Then, if Fig.11B2 As shown in FIG. 1 , three wiring substrates are stacked after being aligned to form a laminate. Then, the laminate is integrated by heating and pressing. Thus, a printed wiring board having a three-layer stripline structure can be obtained.
[0031] In the printed wiring board manufactured by the method of the comparative example, the back surface of the copper foil 220 is rough. Therefore, it is difficult to reduce the transmission loss of the high-frequency signal flowing on the back surface of the copper foil 220 due to the skin effect.
[0032] It is expected that the transmission loss can be reduced by using a liquid crystal polymer in the dielectric layer as described above. However, even if the copper foil is directly pressed onto the liquid crystal polymer, it is difficult to obtain sufficient bonding strength. Therefore, it is necessary to roughen the surface of the copper foil. Alternatively, it is necessary to provide a back surface treatment film containing a magnetic metal such as nickel. The back surface treatment film also becomes the main cause of the increase in transmission loss caused by the skin effect.
[0033] In addition, if Fig.11B2As shown in FIG. 1 , the printed wiring board in the comparative example has an asymmetric structure in the thickness direction. Therefore, when the printed wiring board is bent to be inserted into the frame of the electronic device, or when the bent printed wiring board is placed in the frame, a large stress is applied to the signal line. Therefore, there is a possibility that the signal line is broken or the transmission characteristics are deteriorated.
[0034] Therefore, a first object of the present invention is to provide a printed wiring board and a method for manufacturing the same which can reduce the transmission loss of a high-frequency signal.
[0035] A second object of the present invention is to provide a printed wiring board capable of suppressing the application of a large stress to a signal line even when bent, and a method for manufacturing the same.
[0036] A printed wiring board according to a first aspect of the present invention is characterized by comprising:
[0037] A first dielectric layer having a first main surface and a second main surface opposite to the first main surface;
[0038] a first adhesive layer formed on the first main surface;
[0039] a first metal foil pattern formed on the first adhesive layer and constituting a signal line; and
[0040] A second metal foil pattern is formed on the second main surface and constitutes a ground layer,
[0041] The first metal foil pattern has a specific conductivity greater than a specific conductivity of the second metal foil pattern.
[0042] Furthermore, in the printed wiring board, the first dielectric layer may be made of a liquid crystal polymer.
[0043] In addition, in the printed wiring board, the printed wiring board may further include:
[0044] A second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface;
[0045] a second adhesive layer formed on the fourth main surface and bonded to the first adhesive layer; and
[0046] A third metal foil pattern is formed on the third main surface and constitutes a ground layer,
[0047] The first metal foil pattern has a specific conductivity greater than a specific conductivity of the third metal foil pattern.
[0048] Furthermore, in the printed wiring board,
[0049] The second adhesive layer is thicker than the first metal foil pattern.
[0050] The first metal foil pattern is embedded in an adhesive layer composed of the first adhesive layer and the second adhesive layer.
[0051] Furthermore, in the printed wiring board,
[0052] The first dielectric layer and the second dielectric layer have the same thickness,
[0053] The first adhesive layer and the second adhesive layer have the same thickness.
[0054] Furthermore, in the printed wiring board,
[0055] The first dielectric layer and the second dielectric layer have the same thickness,
[0056] The first adhesive layer is thinner than the second adhesive layer by an amount corresponding to the thickness of the first metal foil pattern.
[0057] Furthermore, in the printed wiring board,
[0058] The second dielectric layer is made of liquid crystal polymer.
[0059] Furthermore, in the printed wiring board,
[0060] The first metal foil pattern has a smaller surface roughness than the second metal foil pattern and the third metal foil pattern, and / or contains a small amount of magnetic metal.
[0061] Furthermore, in the printed wiring board,
[0062] The ten-point average roughness of the first metal foil pattern is 1.0 μm or less.
[0063] Furthermore, in the printed wiring board,
[0064] The printed wiring board further comprises:
[0065] a fourth metal foil pattern formed on the first adhesive layer, arranged in parallel with the signal line of the first metal foil pattern at a predetermined interval, and constituting a ground wiring;
[0066] a first grounding portion electrically connecting the second metal foil pattern and the fourth metal foil pattern; and
[0067] The second ground portion electrically connects the third metal foil pattern and the fourth metal foil pattern.
[0068] A printed wiring board according to a second aspect of the present invention is characterized by comprising:
[0069] A first dielectric layer having a first main surface and a second main surface opposite to the first main surface;
[0070] a first adhesive layer formed on the first main surface;
[0071] a first metal foil pattern formed on the first adhesive layer and constituting a signal line;
[0072] a second metal foil pattern formed on the second main surface and constituting a ground layer;
[0073] A second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface;
[0074] a second adhesive layer formed on the fourth main surface and bonded to the first adhesive layer; and
[0075] A third metal foil pattern is formed on the third main surface and constitutes a ground layer,
[0076] The second adhesive layer is thicker than the first metal foil pattern.
[0077] The first metal foil pattern is embedded in an adhesive layer composed of the first adhesive layer and the second adhesive layer.
[0078] A method for manufacturing a printed wiring board according to a first aspect of the present invention is characterized by comprising:
[0079] A first single-sided metal foil-clad laminate is prepared, the first single-sided metal foil-clad laminate comprising: a first dielectric layer having a first main surface and a second main surface opposite to the first main surface; and a first metal foil provided on the second main surface;
[0080] irradiating a predetermined portion of the first protective film laminated on the first main surface via the first adhesive layer with a laser to remove the first protective film, the first adhesive layer, and the first dielectric layer, thereby forming a first conduction hole so that the first metal foil is exposed at the bottom surface of the first conduction hole;
[0081] filling the first conductive hole with a first conductive paste;
[0082] peeling the first protective film from the first adhesive layer;
[0083] a laminating step of laminating a second metal foil having a lower specific conductivity than the first metal foil on the first adhesive layer; and
[0084] By patterning the second metal foil, a metal foil pattern constituting a signal line and a metal foil pattern constituting a ground wiring are formed.
[0085] A method for manufacturing a printed wiring board according to a second aspect of the present invention is characterized by comprising:
[0086] A first single-sided metal foil-clad laminate is prepared, the first single-sided metal foil-clad laminate comprising: a first dielectric layer having a first main surface and a second main surface opposite to the first main surface; and a first metal foil provided on the second main surface;
[0087] irradiating a predetermined portion of the first protective film laminated on the first main surface via the first adhesive layer with a laser to remove the first protective film, the first adhesive layer, and the first dielectric layer, thereby forming a first conduction hole so that the first metal foil is exposed at the bottom surface of the first conduction hole;
[0088] filling the first conductive hole with a first conductive paste;
[0089] peeling the first protective film from the first adhesive layer;
[0090] a laminating step of laminating a second metal foil having a lower specific conductivity than the first metal foil on the first adhesive layer; and
[0091] By patterning the second metal foil, a metal foil pattern constituting a signal line and a metal foil pattern constituting a ground wiring are formed to obtain a first wiring substrate;
[0092] preparing a second single-sided metal foil-clad laminate, the second single-sided metal foil-clad laminate comprising: a second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface; and a third metal foil provided on the third main surface;
[0093] irradiating a predetermined portion of the second protective film laminated on the fourth main surface via the second adhesive layer with a laser to remove the second protective film, the second adhesive layer, and the second dielectric layer, thereby forming a second conductive hole so that the third metal foil is exposed at the bottom surface of the second conductive hole;
[0094] A step of filling the second conductive paste in the second conductive hole;
[0095] peeling the second protective film from the second adhesive layer to obtain a second wiring substrate;
[0096] laminating the second wiring base material on the first wiring base material such that the second conductive paste protruding from the second adhesive layer is in contact with the metal foil pattern of the ground wiring; and
[0097] The stacked first wiring base material and the second wiring base material are integrated by heating and pressurizing them.
[0098] A method for manufacturing a printed wiring board according to a third aspect of the present invention is characterized by comprising:
[0099] A single-sided metal foil-clad laminate is prepared, the single-sided metal foil-clad laminate comprising: a dielectric layer having a first main surface and a second main surface opposite to the first main surface; and a first metal foil formed on the second main surface;
[0100] laminating an adhesive layer on the first main surface;
[0101] a laminating step of laminating a second metal foil having a lower specific conductivity than the first metal foil on the adhesive layer;
[0102] By patterning the second metal foil, a metal foil pattern constituting a signal line and a metal foil pattern constituting a ground wiring are formed;
[0103] Forming a conformal mask by patterning the first metal foil;
[0104] irradiating the conformal mask with a laser to remove the dielectric layer and the adhesive layer, thereby forming a conductive hole so that the metal foil pattern of the ground wiring is exposed at the bottom surface of the conductive hole; and
[0105] A metal plating layer is formed inside the conduction hole so as to electrically connect the metal foil pattern of the ground wiring and the first metal foil.
[0106] A method for manufacturing a printed wiring board according to a fourth aspect of the present invention is characterized by comprising:
[0107] A first single-sided metal foil-clad laminate is prepared, the first single-sided metal foil-clad laminate comprising: a first dielectric layer having a first main surface and a second main surface opposite to the first main surface; and a first metal foil formed on the second main surface;
[0108] laminating a first adhesive layer on the first main surface;
[0109] a laminating step of laminating a second metal foil having a lower specific conductivity than the first metal foil on the first adhesive layer;
[0110] By patterning the second metal foil, a metal foil pattern constituting a signal line and a metal foil pattern constituting a ground wiring are formed to obtain a first wiring substrate;
[0111] preparing a second single-sided metal foil-clad laminate, the second single-sided metal foil-clad laminate comprising: a second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface; and a third metal foil formed on the third main surface;
[0112] laminating a second adhesive layer on the fourth main surface to obtain a second wiring substrate;
[0113] stacking the first wiring base material and the second wiring base material in such a manner that the first adhesive layer and the second adhesive layer face each other;
[0114] integrating the stacked first wiring base material and the second wiring base material by heating and pressurizing them;
[0115] forming a first conformal mask by patterning the first metal foil;
[0116] forming a second conformal mask by patterning the third metal foil;
[0117] removing the first dielectric layer and the first adhesive layer by irradiating the first conformal mask with a laser, thereby forming a first conductive hole so that the metal foil pattern of the ground wiring is exposed at the bottom surface of the first conductive hole;
[0118] irradiating the second conformal mask with a laser to remove the second dielectric layer and the second adhesive layer, thereby forming a second conductive hole so that the metal foil pattern of the ground wiring is exposed at the bottom surface of the second conductive hole;
[0119] forming a metal plating layer inside the first conducting hole so as to electrically connect the metal foil pattern of the ground wiring to the first metal foil; and
[0120] A metal plating layer is formed inside the second conduction hole so as to electrically connect the metal foil pattern of the ground wiring and the third metal foil.
[0121] Hereinafter, embodiments of the present invention will be described with reference to the schematic drawings. In each figure, components having equivalent functions are marked with the same symbols. The relationship between the thickness and the plane size (aspect ratio) and the ratio of the thickness of each layer shown in the drawings may not be consistent with the actual ratio.
[0122] (High frequency signal transmission component 1)
[0123] First, refer to Figure 1 A high-frequency signal transmission component 1 according to this embodiment will be described. Figure 1 The figure shows a top view of a high-frequency signal transmission component 1. The high-frequency signal transmission component 1 is disposed in a housing of an information processing terminal including a smartphone and a tablet terminal. The high-frequency signal transmission component 1 electrically connects an antenna for transmitting and receiving wireless signals and a main body substrate on which a signal processing chip is mounted.
[0124] like Figure 1As shown, the high-frequency signal transmission component 1 includes a printed wiring board 2 constituting an elongated ribbon cable portion and a connector 3 provided at an end of the printed wiring board 2 .
[0125] The printed wiring board 2 is a flexible printed wiring board (FPC) having flexibility and has a three-layer strip line structure (see Figure 3 ).like Figure 2 As shown, in the printed wiring board 2, the metal foil pattern 17a constituting the signal line and the metal foil pattern 17b constituting the ground wiring form the inner wiring pattern. In the wiring pattern, the metal foil pattern 17a and the ground wiring arranged alternately are extended along the long side direction. For example, a high-frequency signal of several GHz to several tens of GHz is input to these signal lines. In addition, the number of signal lines is not limited to the number shown in the figure.
[0126] Connector 3 is provided at an end of printed wiring board 2 and electrically connected to, for example, a main body substrate or an antenna. Connector 3 has connection pins 3a electrically connected to metal foil pattern 17a of a signal line and connection pins 3b electrically connected to metal foil pattern 17b of a ground line.
[0127] In addition, the signal line of the printed wiring board can also be set as a differential line. In this case, the two signal lines are set in parallel without sandwiching the ground wiring. In addition, a pair of differential lines can also be set in multiple groups with the ground wiring separated. Alternatively, the transmission line and the differential line of the single-ended structure can also exist in a mixed state.
[0128] The planar shape of the metal foil patterns 17a and 17b of the signal line or the ground wiring is not limited to Figure 2 For example, the planar shape may be a shape described in Japanese Patent Publication No. 2019-106508.
[0129] (Printed wiring board 2)
[0130] Below, refer to Figure 3 as well as Figure 4 The printed wiring board 2 will be described in more detail. Figure 3 Indicates along Figure 1 as well as Figure 2 A cross-sectional view of the printed wiring board 2 taken along line II. Figure 4 yes Figure 3 Magnified view of area S.
[0131] like Figure 3As shown, the printed wiring board 2 includes dielectric layers 11, 21, a plurality of metal foil patterns (signal lines) 17a, a plurality of metal foil patterns (ground wirings) 17b, metal foil patterns 12a, 22a constituting a ground layer, filled through holes 16c, 26c, and an adhesive layer 33. Although not shown, the outer metal foil patterns 12a, 22a may be covered with an insulating protective film.
[0132] In more detail, from Figure 4 It can be seen that the printed wiring board 2 includes a dielectric layer 11, an adhesive layer 13 formed on the upper surface (first main surface) of the dielectric layer 11, metal foil patterns 17a, 17b formed on the adhesive layer 13, a metal foil pattern 12a formed on the lower surface (second main surface) of the dielectric layer 11, a dielectric layer 21, a metal foil pattern 22a formed on the upper surface (third main surface) of the dielectric layer 21, an adhesive layer 23 formed on the lower surface (fourth main surface) of the dielectric layer 21, and filled through holes 16c, 26c of the interlayer conductive path.
[0133] The dielectric layer 11 and the dielectric layer 21 are both flexible insulating resin films, and have an upper surface and a lower surface opposite to the upper surface. In the present embodiment, the dielectric layer 11 and the dielectric layer 21 have the same thickness (for example, each is 100 μm). In addition, in the present embodiment, the dielectric layers 11 and 21 are made of a liquid crystal polymer, which is one of the materials having the lowest dielectric constant and dielectric loss tangent.
[0134] In addition, the material of the dielectric layers 11 and 21 is not limited to LCP, and the material may be other insulating materials (polyimide, fluorine-based resin, etc.).
[0135] In the present embodiment, dielectric layer 11 and dielectric layer 21 are composed of a single layer. However, at least one of dielectric layer 11 and dielectric layer 21 may include a plurality of stacked thin films. In this case, the materials of the plurality of thin films may be the same or different.
[0136] like Figure 4 As shown in FIG. 1 , the adhesive layer 13 and the adhesive layer 23 are bonded to each other to form an adhesive layer 33. Here, the adhesive layer 23 is thicker than the metal foil pattern 17a. In addition, the metal foil patterns 17a and 17b are embedded in the adhesive layer 33. In this way, the signal line, that is, the metal foil pattern 17a, is embedded in the adhesive layer 33. Therefore, even when the printed wiring board 2 is bent, it is easy to maintain the mechanical stability of the signal line. Therefore, it is possible to suppress the deterioration of the transmission quality.
[0137] In the present embodiment, adhesive layers 13 and 23 have dielectric properties equal to or lower than those of dielectric layers 11 and 21. Alternatively, adhesive layers having better dielectric properties than dielectric layers 11 and 21 may be used as adhesive layers 13 and 23.
[0138] The metal foil patterns 17a and 17b are coated on the dielectric layer 11 via the adhesive layer 13. The metal foil pattern 17a constitutes a signal line, and the metal foil pattern 17b constitutes a ground line.
[0139] The metal foil patterns 17a and 17b are formed by patterning a sheet of metal foil. The details will be described later in the section related to the method for manufacturing a printed wiring board. The metal foil patterns 17a and 17b are formed by patterning a metal foil (copper foil, etc.) attached to the upper surface of the adhesive layer 13. Therefore, it is possible to use a type of metal foil (for example, a low-roughness copper foil with a rough surface) that cannot obtain sufficient bonding strength between the dielectric layer 11 such as LCP to form the metal foil pattern 17a. In contrast, the metal foil patterns 12a and 22a are formed by patterning a metal foil (for example, a copper foil with a large roughness) of a single-sided metal foil laminate.
[0140] The filled through-holes 16c and 26c are interlayer conductive paths that electrically connect the inner layer ground wiring (metal foil pattern 17b) and the outer layer ground layer (metal foil pattern 12a and 22a). The filled through-hole 16c electrically connects the metal foil pattern 17b and the metal foil pattern 12a. The filled through-hole 26c electrically connects the metal foil pattern 17b and the metal foil pattern 22a. As described in detail later, the filled through-holes 16c and 26c are formed by curing the conductive paste filled in the through-holes that penetrate the dielectric layers 11 and 21 in the thickness direction.
[0141] In this way, the filled through hole is used as the interlayer connection portion (grounding portion) between the outer ground layer and the inner ground wiring. As a result, a liquid crystal polymer having a larger thermal expansion coefficient in the thickness direction than conventional insulating materials such as polyimide can be applied to the dielectric layer. In this case, sufficient connection reliability against temperature cycles can be ensured.
[0142] Here, the characteristics of the metal foil pattern 17a (17b) will be described in more detail.
[0143] The metal foil pattern 17a has a greater specific conductivity than the metal foil pattern 12a and the metal foil pattern 22a. Here, the specific conductivity (σr) represents the conductivity at a predetermined frequency relative to the conductivity of an ideal metal surface. The specific conductivity (σr) is calculated by equation (1).
[0144]
[0145] Where, μ0: vacuum magnetic permeability, f0: resonant frequency, σ0: conductivity of international standard annealed copper (58×10 6 S / m), R s : Surface resistance.
[0146] The resonance frequency f0 is the TE of a MIC (Microwave Integrated Circuits) type dielectric cylindrical resonator (see, for example, http: / / sumtec.biz / whatis_rod.html). 01δ The resonant frequency of the mode. Surface resistance R s It is the surface resistance based on the dual dielectric resonator method. Surface resistance R s The measurement is performed by the method defined in standards such as JIS H7307 (2005) and IEC 61788-7 (2002).
[0147] The smaller the surface roughness (roughness) of a metal foil such as copper foil, the larger the value of the specific conductivity. In addition, the more magnetic metals (such as nickel) with high magnetic permeability the metal foil contains, the smaller the value of the specific conductivity. For example, in order to improve the bonding strength between the copper foil and the dielectric, a back surface treatment film containing nickel and cobalt is provided on the back of the copper foil after the roughening treatment. In this case, the specific conductivity of the copper foil becomes lower. In the presence of such a back surface treatment film, high-frequency transmission is hindered.
[0148] In this embodiment, if Figure 4 As schematically shown in FIG. 1 , the surface roughness of the back side of the metal foil pattern 17a (i.e., the side in contact with the adhesive layer 13) is smaller than the surface roughness of the back side of the metal foil patterns 12a and 22a (i.e., the side in contact with the dielectric layers 11 and 21). Therefore, the transmission loss of the high-frequency signal flowing in the metal foil pattern 17a can be reduced (the specific values are described later in Table 1).
[0149] The surface roughness mentioned here is the roughness of the surface of the metal foil after the surface is roughened for the purpose of obtaining an anchoring effect, etc. The surface roughness is, for example, the ten-point average roughness (Rzjis) specified by standards such as JIS B0601-2001 and ISO 4287-1997. The ten-point average roughness of the metal foil pattern 17a is preferably less than 1.0 μm. As a result, as shown in Table 1 described later, the transmission loss of high-frequency signals above 20 GHz can be greatly reduced.
[0150] In addition, the metal foil pattern 17a may also have a content of magnetic metal (Ni, Co, etc.) less than that of the metal foil patterns 12a and 22a. For example, a back surface treatment film may not be provided on the back surface of the metal foil pattern 17a. In contrast, in order to improve the bonding strength with the dielectric layers 11 and 21, a back surface treatment film is provided on the back surface of the metal foil patterns 12a and 22a. In this way, the magnetic metal content of the metal foil pattern 17a is less than that of the metal foil patterns 12a and 22a. In this case, the transmission loss of the high-frequency signal flowing in the metal foil pattern 17a can also be reduced.
[0151] (Effect)
[0152] As described above, in the printed wiring board 2 of the present embodiment, the specific conductivity of the metal foil pattern 17a is greater than the specific conductivity of the metal foil pattern 12a and the metal foil pattern 22a. In contrast, in the comparative example, the specific conductivity of the metal foil pattern 17a is the same as the specific conductivity of the metal foil patterns 12a and 22a. Therefore, according to the printed wiring board 2 of the present embodiment, the transmission loss of the high-frequency signal flowing in the metal foil pattern 17a can be further reduced compared with the comparative example.
[0153] In addition, the surface roughness of the metal foil patterns 12a and 22a is coarse. Therefore, even if the dielectric layers 11 and 21 are made of soft and difficult-to-bond resin materials such as liquid crystal polymers, metal foils with high bonding strength can be applied. Therefore, a printed wiring board with strong bending resistance is provided.
[0154] Furthermore, in the printed wiring board 2 of the present embodiment, the thickness of the dielectric layer 11 and the dielectric layer 21 are substantially the same. Furthermore, the thickness of the adhesive layer 13 and the adhesive layer 23 are also substantially the same. Figure 3 and Figure 4 As shown in FIG. 1 , the printed wiring board 2 is formed into a structure that is approximately symmetrical in the thickness direction with the metal foil pattern 17a (signal line) as the center. Therefore, when the printed wiring board 2 is bent in order to assemble the high-frequency signal transmission component 1 into the frame of the electronic device, the stress applied to the metal foil pattern (signal line) 17a can be reduced. As a result, it is possible to prevent the signal line from breaking and other undesirable situations. At the same time, it is possible to ensure good signal transmission characteristics.
[0155] In order to further improve the symmetry of the printed wiring board 2, the thickness of the adhesive layer 13 may be thinner than the adhesive layer 23 by the thickness of the metal foil pattern 17a. Thus, the distance from the surface (upper surface) of the metal foil pattern 17a to the metal foil pattern 22a is equal to the distance from the back surface (lower surface) of the metal foil pattern 17a to the metal foil pattern 12a. As a result, the stress applied to the metal foil pattern 17a when the printed wiring board 2 is bent can be further reduced.
[0156] In the printed wiring board 2 of the present embodiment, ground layers are provided on both sides of the signal line. However, this is not limiting, and in the printed wiring board of the present embodiment, a ground layer may be provided on only one side. A printed wiring board having a ground layer provided on only one side has Figure 4 The illustrated structure is a structure in which the dielectric layer 21, the metal foil pattern 22a, the adhesive layer 23, and the filled via 26c are removed.
[0157] (Method of Manufacturing Printed Wiring Board 2)
[0158] Below, refer to Figure 5A1 to Figure 7B An example of a method for manufacturing the printed wiring board 2 according to the embodiment will be described. Figure 5A1 to Figure 7B express Figure 4 The area S shown is around the ground wiring (metal foil pattern 17b).
[0159] First, if Fig.5A1 As shown, a single-sided metal foil laminate 10 is prepared, which has a dielectric layer 11 and a metal foil 12 provided on one side of the dielectric layer 11. The dielectric layer 11 is, for example, a 100 μm thick liquid crystal polymer film. The metal foil 12 is, for example, a 12 μm thick copper foil. In addition, the metal foil 12 may also be formed of a metal other than copper (silver, aluminum, etc.).
[0160] Then, if Figure 5A2 As shown, the metal foil 12 of the single-sided metal foil-clad laminate 10 is patterned by a known photolithography method to form a metal foil pattern 12a. The metal foil pattern 12a includes a ground layer.
[0161] Then, if Figure 5A3 As shown, an adhesive layer 13 is laminated on the upper surface of the dielectric layer 11. Furthermore, a protective film 14 is laminated on the upper surface of the adhesive layer 13. The thickness of the adhesive layer 13 is, for example, 25 μm. The thickness of the protective film 14 is, for example, 15 μm. In this embodiment, the material used for the adhesive layer 13 can ensure the bonding strength with the liquid crystal polymer film and has dielectric properties that are equal to or less than the dielectric properties of the dielectric layer 11. For example, a film formed of polyethylene terephthalate (PET) can be used as the protective film 14.
[0162] In addition, the thickness of the protective film 14 determines the protrusion amount of the conductive paste 16 described later. When the protective film 14 is too thick, the protrusion amount of the conductive paste 16 becomes too large. Therefore, in the lamination process described later, the unevenness cannot be completely absorbed by the adhesive layer 2. As a result, the flatness of the printed wiring board 2 may be impaired. On the other hand, when the protective film 14 is too thin, the protrusion amount of the conductive paste 16 becomes too small. As a result, the connection reliability between the conductive paste 16 and the metal foil pattern 17b may not be fully ensured. Therefore, the thickness of the protective film 14 is preferably in the range of 15±10μm.
[0163] Alternatively, a protective film with an adhesive layer (not shown) including an adhesive layer 13 applied on one side of the protective film 14 may be used. In this case, by attaching the protective film with an adhesive layer to the dielectric layer 11 side of the single-sided metal foil-clad laminate 10, it is possible to achieve Figure 5A3 The composition shown.
[0164] Then, if Figure 5B1 As shown in FIG. 1 , the protective film 14, the adhesive layer 13, and the dielectric layer 11 are removed by irradiating a predetermined portion of the protective film 14 with laser light. In this way, a conductive hole H1 is formed. The metal foil pattern 12a is exposed at the bottom of the conductive hole H1. More specifically, after the hole is perforated by irradiation with laser pulses, a deslagging process is performed. Thus, the resin residue at the boundary between the dielectric layer 11 and the metal foil pattern 12a and the back surface treatment film (Ni / Cr film, etc.) of the metal foil pattern 12a are removed.
[0165] The diameter of the conductive hole H1 is, for example, φ150μm to 200μm. Examples of lasers used for laser processing include infrared lasers such as carbon dioxide lasers and UV-YAG lasers. When using a carbon dioxide laser, the beam diameter is adjusted to the diameter of the conductive hole H1. As an applicable laser processing machine, a carbon dioxide laser processing machine (ML605GTXIII-5100U2) manufactured by Mitsubishi Electric Corporation can be cited. By adjusting the beam diameter to 150μm using a specified aperture, the pulse width can be adjusted to 10μSec, the energy of each pulse to 5mJ, and 5 pulses emitted to irradiate each location.
[0166] Then, if Figure 5B2 As shown, the conductive hole H1 is filled with conductive paste 16. More specifically, the conductive hole H1 is filled with conductive paste 16 by a printing method such as screen printing, using protective film 14 as a printing mask. Here, conductive paste 16 is prepared by dispersing metal particles in a paste-like thermosetting resin, that is, a resin binder.
[0167] In addition, in order to suppress the mixing of voids in the conductive hole H1 during the printing process of the conductive paste, it is preferable to print the conductive paste 16 in a vacuum environment. For example, it is preferable to use a vacuum printer for screen printing. Thus, even if voids are generated in the conductive hole H1 during the printing of the conductive paste, when the vacuum is released, the voids will be crushed by the atmospheric pressure and disappear.
[0168] Then, if Figure 5B3 As shown, the protective film 14 is peeled off from the adhesive layer 13 . As a result, a part of the conductive paste 16 filled in the conduction hole H1 protrudes from the adhesive layer 13 .
[0169] Then, if Fig.5C1 as well as Fig.5C2 As shown, metal foil 17 is laminated on adhesive layer 13 (lamination step). Metal foil 17 may have a lower specific conductivity than metal foil 12 (e.g., low-roughness copper foil or copper foil without back surface treatment film). The thickness of metal foil 17 is, for example, 12 μm.
[0170] The details of this lamination process are described below. First, the metal foil 17 is placed on the adhesive layer 13 in a manner that it contacts the conductive paste 16 protruding from the adhesive layer 13. In the case where it is difficult to handle the metal foil 17 alone, first, the metal foil 17 that is bonded to a resin film (carrier, not shown) such as PET in a releasable manner can be placed on the adhesive layer 13. Thereafter, the carrier can be removed.
[0171] The metal foil 17 is patterned in a later step. Therefore, it is not particularly necessary to position the metal foil 17 when it is placed on the adhesive layer 13. In addition, guide holes and the like may be formed in the metal foil 17 as necessary.
[0172] As described above, after the metal foil 17 is placed on the adhesive layer 13, the single-sided metal foil-clad laminate 10 (laminated body) including the placed metal foil 17 is heated and pressurized using a vacuum pressing device or a vacuum laminating device. For example, the laminate is heated to about 200° C. and pressurized at a pressure of about several MPa. In addition, the heating temperature is preferably set to a temperature sufficiently lower than the softening temperature of the liquid crystal polymer constituting the dielectric layer 11 (for example, 50° C. or more).
[0173] When a vacuum press is used, the laminate is held under the above-mentioned heating and pressurizing conditions for, for example, about 30 to 60 minutes, thereby completing the thermal curing of the adhesive layer 13 and the thermal curing of the binder resin of the conductive paste 16 .
[0174] When a vacuum laminating device is used, the heating and pressurizing time is about several minutes. However, the thermal curing reaction is not completed at the end of the heating and pressurizing reaction. Therefore, the laminated body transferred from the vacuum laminating device to the oven device is subjected to post-curing treatment. In the post-curing treatment, for example, the laminated body is heated at a temperature of about 200° C. for about 60 minutes. Thus, the thermal curing of the adhesive layer 13 and the thermal curing of the binder resin of the conductive paste 16 are completed.
[0175] When using either the vacuum pressing device or the vacuum laminating device, the metal particles contained in the conductive paste 16 are metal-bonded to each other by heating at a predetermined temperature. At the same time, a part of the metal particles is metal-bonded to the metal foil pattern 12a and the metal foil 17. Fig.5C2 As shown, a filled through hole 16c for interlayer connection is formed. Furthermore, by this heating, the thermal curing reaction of the resin binder contained in the conductive paste 16 and the thermal curing reaction of the adhesive layer 13 are substantially completed.
[0176] Then, if Fig.5C3 As shown, the metal foil 17 on the adhesive layer 13 is patterned by a known manufacturing method. In this way, a metal foil pattern 17a constituting a signal line and a metal foil pattern 17b constituting a ground wiring are formed. In addition, a portion of the metal foil pattern 17b becomes a receiving pad for the conductive paste 26 described later. The wiring substrate 100 is obtained through the steps so far.
[0177] In addition, in the case of a printed wiring board in which a ground layer is provided only on one side of the signal line, after obtaining the wiring substrate 100, surface treatment of the wiring layer (signal line, ground wiring) exposed to the outside, formation of a surface protective film, and outer shape processing are performed as needed to complete the printed wiring board.
[0178] Next, the production of the other wiring substrate 200 will be described.
[0179] First, if Fig.6A1 As shown, a single-sided metal foil laminate 20 is prepared, which includes a dielectric layer 21 and a metal foil 22 provided on one side of the dielectric layer 21. The dielectric layer 21 is, for example, a 100 μm thick liquid crystal polymer film. The metal foil 22 is, for example, a 12 μm thick copper foil. In addition, the metal foil 22 may also be formed of a metal other than copper (silver, aluminum, etc.).
[0180] Then, if Fig.6A2 As shown, the metal foil 22 of the single-sided metal foil-clad laminate 20 is patterned by a known photolithography method to form a metal foil pattern 22a. The metal foil pattern 22a includes a ground layer.
[0181] Then, if Figure 6A3As shown, an adhesive layer 23 is laminated on the lower surface of the dielectric layer 21 (the resin surface of the single-sided metal foil laminate 20). Furthermore, a protective film 24 made of PET or the like is laminated on the adhesive layer 23. The thickness of the adhesive layer 23 is, for example, 25 μm. The thickness of the protective film 24 is, for example, 15 μm. In this embodiment, the material used for the adhesive layer 23 can ensure the bonding strength with the liquid crystal polymer film and has dielectric properties that are equal to or less than the dielectric properties of the dielectric layer 21.
[0182] The thickness of the protective film 24 determines the amount of protrusion of the conductive paste 26 described later. As in the case of the protective film 14, the thickness of the protective film 24 is preferably within the range of 15±10 μm.
[0183] Alternatively, a protective film with an adhesive layer (not shown) including an adhesive layer 23 applied on one side of the protective film 24 may be used. In this case, by attaching the protective film with an adhesive layer to the dielectric layer 21 side of the single-sided metal foil-clad laminate 20, it is possible to achieve Figure 6A3 The composition shown.
[0184] Then, if Fig.6B1 As shown, by irradiating a predetermined portion of the protective film 24 with laser, the protective film 24, the adhesive layer 23, and the dielectric layer 21 are removed. In this way, the conductive hole H2 is formed. The metal foil pattern 22a is exposed on the bottom surface of the conductive hole H2. The diameter of the conductive hole H2 is, for example, φ150μm to 200μm. This process is the same as the process for forming the conductive hole H1 already described. Therefore, a detailed description is omitted.
[0185] Then, if Figure 6B2 As shown in FIG. 1 , the conductive hole H2 is filled with the conductive paste 26. This step is the same as the step of filling the conductive hole H1 with the conductive paste 16, which has been described above. Therefore, detailed description is omitted.
[0186] Then, if Figure 6B3 As shown, the protective film 24 is peeled off from the adhesive layer 23. Thus, the wiring substrate 200 is obtained.
[0187] The two wiring substrates 100 and 200 produced as described above are stacked on each other after being aligned. Then, the wiring substrates 100 and 200 are integrated by heating and pressing. Thus, the printed wiring board 2 is obtained. The detailed process is as follows.
[0188] First, if Fig. 7A as well as Figure 7B As shown, the wiring base material 100 and the wiring base material 200 are stacked so that the conductive paste 26 protruding from the adhesive layer 23 is in contact with the metal foil pattern 17b of the ground wiring (stacking step).
[0189] After that, the stacked wiring substrates 100 and 200 are integrated by heating and pressurizing (integration step). The heating in this step completes the thermal curing of the binder resin of the conductive paste 26. This step is performed in the same manner as the heating and pressurizing step of the single-sided metal foil-clad laminate 10 including the mounted metal foil 17.
[0190] In the case of using either the vacuum pressing device or the vacuum laminating device, the metal particles contained in the conductive paste 26 are metal-bonded to each other by heating at a predetermined temperature (lamination processing temperature). At the same time, a part of the metal particles is metal-bonded to the metal foil pattern 22a and the metal foil pattern 17b. Figure 7B As shown, a filled through hole 26c for interlayer connection is formed. Furthermore, by this heating, the thermal curing reaction of the resin binder contained in the conductive paste 26 and the thermal curing reaction of the adhesive layer 23 are substantially completed.
[0191] In addition, in the integration process, the metal particles contained in the conductive pastes 16 and 26 are metallically bonded to each other by heating at a lamination processing temperature (e.g., about 200° C.). For this reason, it is preferred that the melting point of the metal particles is below the lamination processing temperature. As such low melting point metals, In, SnIn, and SnBi can be cited. Therefore, it is preferred that the conductive pastes 16 and 26 used contain metal particles formed of any of these low melting point metals.
[0192] In addition, when the metal foil 12, 17, 22 is a copper foil, the conductive paste 16, 26 used preferably contains metal particles formed of Sn, Zn, Al, Ag, Ni, Cu or an alloy thereof. Thus, by heating at a lamination processing temperature (e.g., about 200° C.), the metal particles contained in the conductive paste 16, 26 form an alloy layer and are metal-bonded with the copper foil.
[0193] After the integration step, surface treatment of the wiring layer exposed to the outside, formation of a surface protection film, outer shape processing, etc. are performed as necessary.
[0194] The printed wiring board 2 is obtained through the above steps. According to the method for manufacturing a printed wiring board of this embodiment, the metal foil pattern (signal line) 17a can be formed by a metal foil having high specific conductivity despite weak bonding strength with the dielectric layer 11. Thus, a printed wiring board capable of reducing transmission loss of high-frequency signals can be manufactured.
[0195] Furthermore, according to the method for manufacturing a printed wiring board of the present embodiment, a printed wiring board having a three-layer stripline structure can be manufactured from two single-sided metal foil-clad laminates 10 and 20. Therefore, compared with the method of the comparative example using three single-sided metal foil-clad laminates, the printed wiring board can be manufactured more easily. As a result, the manufacturing efficiency can be improved.
[0196] Furthermore, according to the manufacturing method of the printed wiring board of the present embodiment, the same single-sided metal foil-clad laminate including dielectric layers having the same thickness can be used as a starting material to manufacture the printed wiring board. The printed wiring board has a substantially symmetrical structure in its thickness direction. That is, a printed wiring board with excellent bending characteristics can be manufactured by a relatively simple method.
[0197] In addition, in the manufacturing method of the printed wiring board 2, before the wiring substrate 100 and the wiring substrate 200 are stacked and integrated, the metal foil 12 and the metal foil 22 are patterned to form a pattern of a ground layer or the like. However, the present embodiment is not limited to this. That is, the metal foil 12 and the metal foil 22 may be patterned to form a pattern of a ground layer or the like after the integration process. Thus, the metal foils 12 and 22 can be patterned in a state of being aligned with the metal foil patterns 17a and 17b. This method is also effective when the shrinkage deviation of the dimensions of the wiring substrates 100 and 200 in the integration process is large.
[0198] In addition, when the metal foils 12 and 22 are patterned after the integration process, the metal foils 12 and 22 may be patterned simultaneously by exposing both sides simultaneously. Thus, the metal foil pattern 12a and the metal foil pattern 22a can be aligned with a higher accuracy than the alignment accuracy (lamination accuracy) when laminating the wiring substrate 100 and the wiring substrate 200. Specifically, the alignment accuracy within ±10 μm can be relatively easily achieved.
[0199] (Verification results)
[0200] The results of measuring the transmission loss of the printed wiring board 2 of the embodiment and the printed wiring board of the comparative example are described with reference to Table 1. Here, the transmission loss was measured in the two embodiments 1 and 2 and the two comparative examples 1 and 2. In addition, the length of the signal line of the measured printed wiring board was 100 mm. The width of the signal line was 0.15 mm.
[0201] In Example 1 and Example 2, the types of copper foil constituting the signal line are different. In Example 1, a copper foil with an Rzjis of 0.1 μm is used, and in Example 2, a copper foil with an Rzjis of 1.0 μm is used. No back surface treatment film is provided for either type of copper foil (i.e., it does not contain magnetic metals such as nickel). As copper foil B of Example 1, NC-WS foil manufactured by Furukawa Electric Co., Ltd. is used. As copper foil C of Example 2, T49-DS-HD2 foil manufactured by Fukuda Metal Foil Powder Co., Ltd. is used.
[0202] As the copper foil constituting the ground layer, the same copper foil A was used in Examples 1 and 2. As the copper foil A, TP4S foil (Rzjis=1.3 μm) manufactured by Fukuda Metal Foil & Powder Co., Ltd. was used.
[0203] In contrast, in Comparative Example 1, the outer layer (GND) and the inner layer (signal line) use the copper foil A. In Comparative Example 2, the outer layer (GND) and the inner layer (signal line) use copper foil D (Furukawa Electric Co., Ltd. F2WS foil, Rzjis = 1.8 μm) having a roughness greater than that of copper foil A.
[0204] A back surface treatment film containing nickel is formed on copper foil A and copper foil D. A back surface treatment film is not formed on copper foil B and copper foil C.
[0205] In any of Examples 1 and 2 and Comparative Examples 1 and 2, the same material was used for the dielectric layers 11 and 21 and the adhesive layers 13 and 23. Specifically, a liquid crystal polymer film (RF-700S, 100 μm thick) manufactured by Panasonic Corporation was used for the dielectric layers 11 and 21. SAFY (25 μm thick) manufactured by Nikon Industries, Ltd. was used for the adhesive layers 13 and 23.
[0206] (Table 1)
[0207]
[0208] As can be seen from Table 1, in Example 1 in which copper foil B is applied to the signal line and in Example 2 in which copper foil C is applied to the signal line, the transmission loss is significantly smaller in the high frequency band above 20 GHz that is attracting attention in the fields of 5G communication and millimeter wave radar than in Comparative Examples 1 and 2. On the other hand, when a copper foil with large roughness is applied to the signal line, as in the case of copper foil D of Comparative Example 2, the transmission loss is large even at 5 GHz.
[0209] As described above, in the printed wiring board of the present embodiment, the metal foil pattern 17a is adhered to the dielectric layer 11 via the adhesive layer 13. Therefore, even when an insulating resin film such as a liquid crystal polymer, which is difficult to ensure adhesion strength, is used as the dielectric layer 11, a metal foil having a large specific conductivity such as a low-roughness copper foil or a copper foil without a back surface treatment film can be used as a signal line important for the transmission of high-frequency signals. Thus, the transmission loss of high-frequency signals can be reduced.
[0210] Furthermore, the printed wiring board of this embodiment has a structure that is roughly symmetrical in its thickness direction with the metal foil pattern 17a of the signal line as the center. Therefore, even if the printed wiring board 2 is bent in order to assemble the high-frequency signal transmission component 1 into a smartphone frame or the like, or even if the bent printed wiring board 2 is set in the frame, it is possible to prevent the signal line from breaking and other undesirable situations. At the same time, it is possible to maintain good signal transmission characteristics.
[0211] (Manufacturing method of printed wiring board (modification example))
[0212] Secondly, refer to Figure 8A to Figure 10C2 An example of a method for manufacturing a printed wiring board according to a modified example is described. In the printed wiring board according to this modified example, the interlayer connection portion (grounding portion) is formed by a metal plating layer. Figure 8A to Figure 10C2 express Figure 4 The surrounding of the ground wiring in the region S. In addition, in each figure, the same reference numerals are attached to the same configurations as those in the embodiment.
[0213] This modification example will be described below, with parts overlapping with the embodiment being omitted as appropriate.
[0214] First, if Fig. 8A As shown, a single-sided metal foil-clad laminate 10 including a dielectric layer 11 and a metal foil 12 provided on one side of the dielectric layer 11 is prepared.
[0215] Then, if Figure 8B As shown, an adhesive layer 13 is laminated on the upper surface of the dielectric layer 11 (the resin surface of the single-sided metal foil-clad laminate 10 ).
[0216] Then, if Figure 8C As shown in the figure, the metal foil 17 is attached to the adhesive layer 13. Specifically, first, the metal foil 17 is placed on the adhesive layer 13. Then, the single-sided metal foil-clad laminate 10 having the placed metal foil 17 is heated and pressurized using a vacuum pressing device or a vacuum laminating device. The conditions of heating and pressurizing are the same as those in the above-mentioned embodiment. Thus, the thermal curing of the adhesive layer 13 is completed.
[0217] Then, if Fig.8DAs shown, the metal foil 17 on the adhesive layer 13 is patterned by a known manufacturing method to form a metal foil pattern 17a constituting a signal line and a metal foil pattern 17b constituting a ground line. The wiring substrate 100A is obtained through the steps so far.
[0218] Next, the production of the other wiring substrate 200A will be described.
[0219] First, if Fig. 9A As shown, a single-sided metal foil-clad laminate 20 including a dielectric layer 21 and a metal foil 22 provided on one side of the dielectric layer 21 is prepared.
[0220] Then, if Fig. 9B As shown, adhesive layer 23 is laminated on the lower surface of dielectric layer 21 (resin surface of single-sided metal foil-clad laminate 20). Wiring substrate 200A is obtained through the steps thus far.
[0221] Then, if Fig.10A1 and Fig.10A2 As shown, wiring substrate 100A and wiring substrate 200A are aligned and stacked in a manner such that adhesive layer 13 and adhesive layer 23 face each other (stacking step). Then, stacked wiring substrate 100A and wiring substrate 200A are integrated by heating and pressurizing (integration step). Thus, adhesive layers 13 and 23 are cured.
[0222] Then, if Fig.10B1 As shown, the metal foil 12 is patterned by a known manufacturing method to form a conformal mask M1. Furthermore, the metal foil 22 is patterned to form a conformal mask M2.
[0223] Then, if Fig.10B2 As shown, the dielectric layer 11 and the adhesive layer 13 are removed by laser irradiation through the conformal mask M1. In this way, the conductive hole H1A is formed. The metal foil pattern 17b of the ground wiring is exposed on the bottom surface of the conductive hole H1A. Similarly, the dielectric layer 21 and the adhesive layer 23 are removed by laser irradiation through the conformal mask M2. In this way, the conductive hole H2A is formed. The metal foil pattern 17b of the ground wiring is exposed on the bottom surface of the conductive hole H2A.
[0224] In addition, in this process, for example, the carbon dioxide laser processing machine is used. More specifically, after the perforation is performed by irradiation with laser pulses, a deslagging process is performed. Thus, the resin residue at the boundary between the adhesive layer 13 and the metal foil pattern 17b is removed. In the case of using the metal foil 17 formed with a back surface treatment film, the back surface treatment film of the metal foil pattern 17b is removed by the deslagging process. In this way, the conductive hole H1A is formed. The same is true for the conductive hole H2A.
[0225] Then, if Fig.10C1 As shown, a metal plating layer 31 is formed inside the conductive hole H1A to electrically connect the metal foil pattern 17b to the metal foil 12. Similarly, a metal plating layer 32 is formed inside the conductive hole H2A to electrically connect the metal foil pattern 17b to the metal foil 22. The metal plating layers 31 and 32 are formed, for example, by electrolytic copper plating after a conductive treatment such as chemical plating. Alternatively, the metal plating layers 31 and 32 may be formed simultaneously by electroplating on both sides. Fig.10C1 As shown, the metal plating layers 31 and 32 are formed not only on the inner walls of the conducting holes H1A and H2A but also on the outer metal foils 12 and 22 .
[0226] Then, if Fig.10C2 As shown, the laminated film including the metal foil 12 and the metal plating layer 31 is patterned by photolithography to form a laminated film including the metal foil pattern 12a including the ground layer and the metal plating pattern 31a. Similarly, the laminated film including the metal foil 22 and the metal plating layer 32 is patterned to form a laminated film including the metal foil pattern 22a including the ground layer and the metal plating pattern 32a.
[0227] Thereafter, surface treatment of the wiring layer exposed to the outside, formation of a surface protective film, outer shape processing, etc. are performed as necessary.
[0228] Through the above steps, a printed wiring board according to a modified example is obtained.
[0229] In addition, even when the grounding portion is a metal plating layer as in the modified example, it is possible to manufacture a printed wiring board in which a grounding layer is provided only on one side of the signal line. Fig.8D ), the metal foil 12 is patterned to form a conformal mask M1. Then, the dielectric layer 11 and the adhesive layer 13 are removed by laser irradiation of the conformal mask M1. In this way, the conductive hole H1A is formed. The metal foil pattern 17b of the ground wiring is exposed on the bottom surface of the conductive hole H1A. Thereafter, a metal plating layer 31 is formed inside the conductive hole H1A to electrically connect the metal foil pattern 17b to the metal foil 12. In this way, a printed wiring board including a ground layer provided only on one side of the signal line and connected between layers by the metal plating layer can be manufactured.
[0230] The printed wiring board described above is not limited to application to the high-frequency signal transmission component 1. It is of course also applicable to other wiring components, substrates, etc. that transmit high-frequency signals.
[0231] Based on the above description, those skilled in the art can think of additional effects and various modifications of this embodiment. This embodiment is not limited to the above embodiment, and also includes additional effects and various modifications. Additions, changes and partial deletions of various implementation components can be used within the scope of the conceptual ideas and purposes of this embodiment derived from the subject matter of the invention specified in the claims and its equivalents.
[0232] The detailed description has been given for the purpose of example and illustration. Based on the teachings of the above surface, many variations and changes are possible. The detailed description is not exclusive of or intended to limit the subject matter described herein. Although the subject matter has been described in words with unique structural features and / or method processes, it should be understood that the subject matter defined in the claims is not necessarily limited to the specific features or specific processes described. More specifically, the specific features and specific processes are described as examples of implementing the claims.
Claims
1. A printed wiring board, characterized in that have: A first dielectric layer having a first main surface and a second main surface opposite to the first main surface; a first adhesive layer formed on the first main surface; a first metal foil pattern formed on the first adhesive layer and constituting a signal line; as well as A second metal foil pattern is formed on the second main surface and constitutes a ground layer, the first metal foil pattern has a specific conductivity greater than a specific conductivity of the second metal foil pattern, The surface roughness of the surface of the first metal foil pattern in contact with the first adhesive layer is smaller than the surface roughness of the surface of the second metal foil pattern in contact with the first dielectric layer.
2. The printed wiring board according to claim 1, wherein The first dielectric layer is made of liquid crystal polymer.
3. The printed wiring board according to claim 1 or 2, characterized in that: The printed wiring board further comprises: A second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface; a second adhesive layer formed on the fourth main surface and bonded to the first adhesive layer; as well as A third metal foil pattern is formed on the third main surface and constitutes a ground layer, The first metal foil pattern has a specific conductivity greater than a specific conductivity of the third metal foil pattern.
4. The printed wiring board according to claim 3, wherein The second adhesive layer is thicker than the first metal foil pattern. The first metal foil pattern is embedded in an adhesive layer composed of the first adhesive layer and the second adhesive layer.
5. The printed wiring board according to claim 4, wherein The first dielectric layer and the second dielectric layer have the same thickness, The first adhesive layer and the second adhesive layer have the same thickness.
6. The printed wiring board according to claim 4, wherein The first dielectric layer and the second dielectric layer have the same thickness, The first adhesive layer is thinner than the second adhesive layer by an amount corresponding to the thickness of the first metal foil pattern.
7. The printed wiring board according to claim 3, wherein: The second dielectric layer is made of liquid crystal polymer.
8. The printed wiring board according to claim 3, wherein The first metal foil pattern has a smaller surface roughness than the second metal foil pattern and the third metal foil pattern, and / or contains a small amount of magnetic metal.
9. The printed wiring board according to claim 8, wherein: The ten-point average roughness of the first metal foil pattern is 1.0 μm or less.
10. The printed wiring board according to claim 3, wherein The printed wiring board further comprises: a fourth metal foil pattern formed on the first adhesive layer, arranged in parallel with the signal line of the first metal foil pattern at a predetermined interval, and constituting a ground wiring; a first grounding portion electrically connecting the second metal foil pattern and the fourth metal foil pattern; as well as The second ground portion electrically connects the third metal foil pattern and the fourth metal foil pattern.
11. The printed wiring board according to claim 10, wherein The first grounding portion is formed by a through hole that penetrates the first dielectric layer in the thickness direction and is filled with a cured conductive paste. The second ground portion is formed by a through hole that penetrates the second dielectric layer in a thickness direction and is filled with a cured conductive paste.
12. The printed wiring board according to claim 10, wherein The first grounding portion is formed of a metal plating layer formed in a through hole penetrating the first dielectric layer in the thickness direction. The second ground portion is formed of a metal plating layer formed in a through hole penetrating the second dielectric layer in the thickness direction.
13. A printed wiring board, characterized in that: have: A first dielectric layer having a first main surface and a second main surface opposite to the first main surface; a first adhesive layer formed on the first main surface; a first metal foil pattern formed on the first adhesive layer and constituting a signal line; a second metal foil pattern formed on the second main surface and constituting a ground layer; A second dielectric layer having a third main surface and a fourth main surface opposite to the third main surface; a second adhesive layer formed on the fourth main surface and bonded to the first adhesive layer; as well as A third metal foil pattern is formed on the third main surface and constitutes a ground layer, The second adhesive layer is thicker than the first metal foil pattern. The first metal foil pattern is embedded in an adhesive layer composed of the first adhesive layer and the second adhesive layer. The surface roughness of the first metal foil pattern in contact with the first adhesive layer is smaller than the surface roughness of the second metal foil pattern in contact with the first dielectric layer and smaller than the surface roughness of the third metal foil pattern in contact with the second dielectric layer.
14. A method for manufacturing a printed wiring board, characterized in that: include: A first single-sided metal foil-clad laminate is prepared, the first single-sided metal foil-clad laminate comprising: a first dielectric layer having a first main surface and a second main surface opposite to the first main surface; and a first metal foil provided on the second main surface; irradiating a predetermined portion of the first protective film laminated on the first main surface via the first adhesive layer with a laser to remove the first protective film, the first adhesive layer, and the first dielectric layer, thereby forming a first conduction hole so that the first metal foil is exposed at the bottom surface of the first conduction hole; filling the first conductive hole with a first conductive paste; peeling the first protective film from the first adhesive layer; a laminating step of laminating a second metal foil having a lower specific conductivity than the first metal foil on the first adhesive layer; and By patterning the second metal foil, a metal foil pattern constituting a signal line and a metal foil pattern constituting a ground wiring are formed. The surface roughness of the surface of the first metal foil pattern in contact with the first adhesive layer is smaller than the surface roughness of the surface of the second metal foil pattern in contact with the first dielectric layer.
15. The method for manufacturing a printed wiring board according to claim 14, wherein: The lamination process comprises: placing the second metal foil on the first adhesive layer; and a heating step of heating the first conductive paste and the first adhesive layer at a predetermined temperature; In the heating step, the metal particles contained in the first conductive paste are metallically bonded to each other and to the first metal foil and the second metal foil, and at the same time, the thermal curing reaction of the resin binder contained in the first conductive paste and the first adhesive layer is completed.