Flexible dimming panel and preparation method thereof

By arranging a dye liquid crystal layer and frame sealing glue on the flexible dimming panel, and using laser cutting and tearing technology to remove excess parts, the problem of high cutting defect rate is solved, the reliability of the panel is improved and the cost is reduced.

CN113504667BActive Publication Date: 2024-10-22BEIJING BOE SENSOR TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110830819.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-07-22
Publication Date
2024-10-22
Estimated Expiration
2041-07-22

AI Technical Summary

Technical Problem

Flexible dimming panels have a high defect rate during the cutting process, which reduces their reliability and increases costs.

Method used

A preparation method is adopted, which includes setting a dye liquid crystal layer and a sealing glue on the dimming substrate, and using specific cutting lines and pad area designs to remove excess parts using laser cutting and tearing technology to ensure the integrity of the light-transmitting electrode layer. Isolated to avoid short circuits.

Benefits of technology

The yield rate of the flexible dimming panel is improved, its reliability is enhanced and the preparation cost is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113504667B_ABST
    Figure CN113504667B_ABST
Patent Text Reader

Abstract

The present disclosure provides a flexible dimming panel and a preparation method thereof, which belongs to the technical field of dimming panels. The preparation method of the flexible dimming panel disclosed in the present disclosure includes: providing a dimming substrate, the dimming substrate includes a first substrate and a second substrate arranged in a box; between the first substrate and the second substrate, the dimming substrate is provided with a dye liquid crystal layer and a frame sealant surrounding the dye liquid crystal layer; the first substrate has a first reserved area surrounded by a first cutting line, and the first reserved area has a first solder pad area extending to the outside of the frame sealant; the second substrate has a second reserved area surrounded by a second cutting line, and the second reserved area has a second solder pad area extending to the outside of the frame sealant; the first cutting line and the second cutting line both overlap with the frame sealant at least partially; the first substrate and the second substrate are cut along the first cutting line and the second cutting line, respectively. The preparation method of the flexible dimming panel provided in the present disclosure can improve the yield of the flexible dimming panel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the technical field of dimming panels, and in particular to a flexible dimming panel and a preparation method thereof. Background Art

[0002] Flexible dimming panels have the advantages of being thin, bendable, and intelligently interactive, which can greatly improve the driving comfort of users and bring a more intelligent interactive travel experience. Flexible dimming panels usually include two layers of substrates, a dye liquid crystal layer sandwiched between the substrates, and the overall contour is formed by cutting. However, the defective rate of flexible dimming panels is high during cutting, which reduces the reliability of flexible dimming panels and increases their cost.

[0003] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present disclosure, and therefore may include information that does not constitute the prior art known to ordinary technicians in the field. Summary of the invention

[0004] The purpose of the present disclosure is to overcome the above-mentioned deficiencies of the prior art and provide a flexible dimming panel and a preparation method thereof, so as to improve the yield rate of the flexible dimming panel.

[0005] According to one aspect of the present disclosure, a method for preparing a flexible dimming panel is provided, comprising:

[0006] A dimming substrate is provided, the dimming substrate comprising a first substrate and a second substrate arranged in a box; between the first substrate and the second substrate, the dimming substrate is provided with a dye liquid crystal layer and a frame sealant surrounding the dye liquid crystal layer; the first substrate comprises a first flexible substrate, a first light-transmitting electrode layer and a first orientation layer stacked in sequence from the outside to the inside; the second substrate comprises a second flexible substrate, a second light-transmitting electrode layer and a second orientation layer stacked in sequence from the outside to the inside; the first substrate has a first reserved area surrounded by a first cutting line, the first reserved area has a first pad area extending to the outside of the frame sealant; the second substrate has a second reserved area surrounded by a second cutting line, the second reserved area has a second pad area extending to the outside of the frame sealant; the first cutting line and the second cutting line both overlap at least partially with the frame sealant;

[0007] The first substrate and the second substrate are cut along the first cutting line and the second cutting line respectively.

[0008] According to an embodiment of the present disclosure, the portion where the first cutting line and the second cutting line overlap each other is an integral cutting line;

[0009] Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes:

[0010] removing the first light-transmitting electrode layer and / or the second light-transmitting electrode layer on the overall cutting line;

[0011] Cutting the first substrate and the second substrate along the overall cutting line by laser;

[0012] Cutting the first flexible substrate along a non-integral cutting line portion of the first cutting line, wherein the cutting depth does not exceed the thickness of the first flexible substrate;

[0013] tearing off a portion of the first substrate outside the first cutting line;

[0014] Cutting the second flexible substrate along the non-integral cutting line portion of the second cutting line, and the cutting depth does not exceed the thickness of the second flexible substrate;

[0015] A portion of the second substrate outside the second cutting line is removed.

[0016] According to an embodiment of the present disclosure, the overall cutting line overlaps with the frame sealing glue.

[0017] According to an embodiment of the present disclosure, the non-integral cutting line portion of the first cutting line is composed of a portion where the first cutting line overlaps with the second pad area and a portion of the first cutting line adjacent to the first pad area;

[0018] The non-integral cutting line portion of the second cutting line consists of a portion where the second cutting line overlaps the first pad area and a portion of the second cutting line adjacent to the second pad area.

[0019] According to an embodiment of the present disclosure, removing the first light-transmitting electrode layer on the overall cutting line includes:

[0020] Allowing laser to transmit from one side of the first flexible substrate to the first light-transmitting electrode layer, and fusing the first light-transmitting electrode layer along the overall cutting line;

[0021] Removing the second light-transmitting electrode layer on the overall cutting line includes:

[0022] The laser is transmitted from one side of the second flexible substrate to the second light-transmitting electrode layer, and the second light-transmitting electrode layer is melted along the integral cutting line.

[0023] According to an embodiment of the present disclosure, cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes:

[0024] Cutting the first flexible substrate along the first cutting line, wherein the cutting depth does not exceed the thickness of the first flexible substrate;

[0025] tearing off a portion of the first substrate outside the first cutting line;

[0026] Cutting the second flexible substrate along the second cutting line, wherein the cutting depth does not exceed the thickness of the second flexible substrate;

[0027] A portion of the second substrate outside the second cutting line is removed.

[0028] According to an embodiment of the present disclosure, the portion where the first cutting line and the second cutting line overlap each other is an integral cutting line;

[0029] Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes:

[0030] Punching the first substrate and the second substrate along the integral cutting line;

[0031] Cutting the first flexible substrate along a non-integral cutting line portion of the first cutting line, wherein the cutting depth does not exceed the thickness of the first flexible substrate;

[0032] tearing off a portion of the first substrate outside the first cutting line;

[0033] Cutting the second flexible substrate along the non-integral cutting line portion of the second cutting line, and the cutting depth does not exceed the thickness of the second flexible substrate;

[0034] A portion of the second substrate outside the second cutting line is removed.

[0035] According to an embodiment of the present disclosure, cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes:

[0036] inserting a blocking gasket between the first substrate and the second substrate, the blocking gasket at least overlapping the first pad area and the second pad area;

[0037] Punching the first substrate along the first cutting line;

[0038] The second substrate is punched along the second cutting line.

[0039] According to an embodiment of the present disclosure, a portion where the first cutting line overlaps with the second pad area is located outside the frame sealant; a portion where the second cutting line overlaps with the first pad area is located outside the frame sealant.

[0040] According to another aspect of the present disclosure, a flexible dimming panel is provided, comprising a first substrate and a second substrate arranged in a box; between the first substrate and the second substrate, the flexible dimming panel is provided with a dye liquid crystal layer and a frame sealant surrounding the dye liquid crystal layer; the first substrate comprises a first flexible substrate, a first light-transmitting electrode layer and a first alignment layer stacked in sequence from the outside to the inside; the second substrate comprises a second flexible substrate, a second light-transmitting electrode layer and a second alignment layer stacked in sequence from the outside to the inside; wherein the first substrate comprises a first solder pad located outside the frame sealant, and the second substrate comprises a second solder pad located outside the frame sealant;

[0041] The portion where the edge of the first substrate and the edge of the second substrate overlap each other is an integral edge; the non-integral edge portion of the edge of the first substrate is composed of the edge of the first pad and the overlapping portion of the edge of the first substrate and the second pad; at least one of the first light-transmitting electrode layer and the second light-transmitting electrode layer does not extend to the integral edge.

[0042] It is to be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] The accompanying drawings herein are incorporated into the specification and constitute a part of the specification, illustrate embodiments consistent with the present disclosure, and together with the specification are used to explain the principles of the present disclosure. Obviously, the accompanying drawings described below are only some embodiments of the present disclosure, and for ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without creative work.

[0044] Figure 1 The figure is a schematic diagram of a top view of a dimming substrate in one embodiment of the present disclosure.

[0045] Figure 2 The figure is a schematic diagram of the cross-sectional structure of a dimming substrate in one embodiment of the present disclosure.

[0046] Figure 3 for Figure 1 Schematic diagram of the cross-sectional structure of the dimming substrate at the MN position.

[0047] Figure 4 The figure is a schematic diagram of a top view of a flexible dimming panel in one embodiment of the present disclosure.

[0048] Figure 5 In one embodiment, Figure 4 Schematic diagram of the cross-sectional structure of the flexible dimming panel at the MN position.

[0049] Figure 6This is a structural schematic diagram of inserting a blocking gasket between a first substrate and a second substrate in one embodiment of the present disclosure.

[0050] Figure 7 In one embodiment, Figure 4 Schematic diagram of the cross-sectional structure of the flexible dimming panel at the MN position.

[0051] Figure 8 In one implementation, a schematic top view of the structure in which the first light-transmitting electrode layer and / or the first light-transmitting electrode layer of the dimming substrate is patterned.

[0052] Fig. 9 In one embodiment, Figure 8 Schematic diagram of the cross-sectional structure of the dimming substrate at the MN position shown in FIG.

[0053] Fig.10 In one embodiment, Figure 4 Schematic diagram of the cross-sectional structure of the flexible dimming panel at the MN position.

[0054] Fig.11 FIG. 4 is a schematic structural diagram of an incision formed when the first flexible substrate is cut in one embodiment.

[0055] Fig.12 FIG. 4 is a schematic structural diagram of an incision formed when the second flexible substrate is cut in one embodiment.

[0056] Fig.13 The figure is a schematic flow chart of a method for preparing a flexible dimming panel in one embodiment.

[0057] Description of reference numerals:

[0058] PNL, flexible dimming panel; PNL0, dimming substrate; 100, first substrate; 110, first flexible substrate; 120, first light-transmitting electrode layer; 130, first alignment layer; L100, first cutting line; L101, non-integral cutting line portion of first cutting line; L102, integral cutting line portion of first cutting line; A111, first pad area; E100, edge of first substrate; E101, non-integral edge portion of edge of first substrate; E102, integral edge portion of edge of first substrate; P100, first pad; 200, second substrate; 21 0, second flexible substrate; 220, second light-transmitting electrode layer; 230, second orientation layer; L200, second cutting line; L201, non-integral cutting line portion of the second cutting line; L202, integral cutting line portion of the second cutting line; A211, second pad area; E200, edge of the second substrate; E201, non-integral edge portion of the edge of the second substrate; E202, integral edge portion of the edge of the second substrate; P200, second pad; 300, dye liquid crystal layer; 400, frame sealing glue; 500, blocking gasket; LL, integral cutting line; EE, integral edge. DETAILED DESCRIPTION

[0059] Example embodiments will now be described more fully with reference to the accompanying drawings. However, the example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that the present disclosure will be comprehensive and complete and fully convey the concepts of the example embodiments to those skilled in the art. The same reference numerals in the figures represent the same or similar structures, and thus their detailed description will be omitted. In addition, the drawings are only schematic illustrations of the present disclosure and are not necessarily drawn to scale.

[0060] Although relative terms such as "upper" and "lower" are used in this specification to describe the relative relationship of one component of the illustration to another component, these terms are used in this specification only for convenience, such as according to the orientation of the examples described in the drawings. It is understood that if the device of the illustration is turned upside down, the component described as "upper" will become the component "lower". When a structure is "on" other structures, it may mean that the structure is formed integrally on the other structure, or that the structure is "directly" disposed on the other structure, or that the structure is "indirectly" disposed on the other structure through another structure.

[0061] The terms "a", "an", "the", "said" and "at least one" are used to indicate the presence of one or more elements / components / etc.; the terms "including" and "having" are used to express an open-ended inclusive meaning and mean that additional elements / components / etc. may exist in addition to the listed elements / components / etc.; the terms "first", "second" and "third" etc. are used merely as labels and are not intended to limit the quantity of their objects.

[0062] The present disclosure provides a flexible dimming panel and a preparation method thereof, so as to improve the yield of the flexible dimming panel, thereby improving the reliability of the flexible dimming panel and reducing its preparation cost. Fig.13 The method for preparing the flexible dimming panel provided in the present disclosure includes:

[0063] Step S110, see Figure 1 and Figure 2 , providing a dimming substrate PNL0. The dimming substrate PNL0 includes a first substrate 100 and a second substrate 200 arranged in a box; between the first substrate 100 and the second substrate 200, the dimming substrate PNL0 is provided with a dye liquid crystal layer 300 and a frame sealant 400 surrounding the dye liquid crystal layer 300; the first substrate 100 includes a first flexible substrate 110, a first light-transmitting electrode layer 120 and a first alignment layer 130 stacked in sequence from the outside to the inside; the second substrate 200 includes a second flexible substrate 210, a second light-transmitting electrode layer 220 and a second alignment layer 230 stacked in sequence from the outside to the inside; the first substrate 100 has a first reserved area surrounded by a first cutting line L100, and the first reserved area has a first pad area A111 extending to the outside of the frame sealant 400; the second substrate 200 has a second reserved area surrounded by a second cutting line L200, and the second reserved area has a second pad area A211 extending to the outside of the frame sealant 400; see Figure 3 , the first cutting line L100 and the second cutting line L200 at least partially overlap with the frame sealing glue 400 .

[0064] Step S120, see Figure 4 The first substrate 100 and the second substrate 200 are cut along the first cutting line L100 and the second cutting line L200 respectively to form the required flexible dimming panel PNL.

[0065] In the method for preparing the flexible dimming panel PNL provided in the present disclosure, the first cutting line L100 and the second cutting line L200 both overlap at least partially with the sealant 400. Figure 5At the cutting position, at least part of the first light-transmitting electrode layer 120 and at least part of the second light-transmitting electrode layer 220 are isolated by the frame sealing glue 400, which can reduce the short circuit caused by the electrical connection between the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 at the cutting position, thereby improving the preparation yield of the flexible dimming panel PNL.

[0066] Below, the structure, principle and effect of the flexible dimming panel PNL and the preparation method thereof provided by the present disclosure are further explained and illustrated in conjunction with the accompanying drawings.

[0067] In step S110, a dimming substrate PNL0 to be cut may be provided. By cutting the dimming substrate PNL0, a desired flexible dimming panel PNL may be obtained.

[0068] See also Figure 2 The dimming substrate PNL0 includes a first substrate 100, a dye liquid crystal layer 300, and a second substrate 200 which are stacked in sequence, wherein a sealant 400 surrounding the dye liquid crystal layer 300 is further disposed between the first substrate 100 and the second substrate 200. The first substrate 100, the second substrate 200, and the sealant 400 form a liquid crystal box, and the dye liquid crystal is filled in the liquid crystal box to form the dye liquid crystal layer 300.

[0069] In some implementations, in order to ensure a good sealing effect and facilitate cutting, the width of the frame sealant 400 may be 4 to 10 mm. Of course, the width of the frame sealant 400 may also be adjusted according to actual needs.

[0070] In some embodiments, in order to maintain the thickness of the liquid crystal box, a spacer may be provided between the first substrate 100 and the second substrate 200. The spacer may be particles (such as plastic balls, etc.) independent of the first substrate 100 and the second substrate 200, or may be a support column formed on the first substrate 100 or the second substrate 200, and the present disclosure does not impose any special restrictions. In one embodiment of the present disclosure, the spacer between the first substrate 100 and the second substrate 200 may be a plastic ball, which may have a certain elasticity, and while supporting the first substrate 100 and the second substrate 200, it may also be deformed when the flexible dimming panel PNL is bent, thereby avoiding puncturing or damaging the first substrate 100 and the second substrate 200 due to excessive hardness.

[0071] In some implementations, spacers may be added to the frame sealant 400 , such as silicon balls, etc. In this way, the spacers in the frame sealant 400 may better maintain the distance between the first substrate 100 and the second substrate 200 .

[0072] In the present disclosure, the first substrate 100 includes a first flexible substrate 110, a first light-transmitting electrode layer 120, and a first alignment layer 130, which are sequentially stacked from the outside to the inside. The outside of the first substrate 100 refers to a side away from the dye liquid crystal layer 300; correspondingly, the inside of the first substrate 100 refers to a side close to the dye liquid crystal layer 300.

[0073] Optionally, the material of the first flexible substrate 110 may be a flexible organic transparent material, for example, it may be PET (polyethylene terephthalate), PI (polyimide), PEN (polyethylene naphthalate) or other flexible resins and other transparent organic polymers. Exemplarily, in one embodiment of the present disclosure, the first flexible substrate 110 is a PET layer. Of course, in other embodiments of the present disclosure, the first flexible substrate 110 may also include multiple flexible organic material layers and inorganic layers sandwiched between the flexible organic material layers, and these flexible organic material layers and inorganic layers are all made of light-transmitting materials.

[0074] The thickness of the first flexible substrate 110 can be determined according to design requirements, so that the first flexible substrate 110 meets the requirements in terms of light transmittance, mechanical properties, etc. Optionally, the thickness of the first flexible substrate 110 can be between 100 microns and 2000 microns, and in particular, between 300 microns and 600 microns.

[0075] Optionally, the material of the first light-transmitting electrode layer 120 may be an organic conductive material, an organic / inorganic conductive composite material, or an inorganic conductive material, and in particular, may be a conductive metal oxide, such as indium gallium zinc oxide (IGZO), indium gallium oxide (IGO), indium zinc oxide (IZO), indium tin zinc oxide (ITZO), tin oxide (SnO2), zinc oxide (ZnO), indium tin oxide (ITO), etc. Exemplarily, in one embodiment of the present disclosure, the first light-transmitting electrode layer 120 is an ITO layer.

[0076] Optionally, the first light-transmitting electrode layer 120 may be a whole electrode layer without being hollowed out or having a specific pattern. Of course, in other embodiments of the present disclosure, the first light-transmitting electrode layer 120 may also be a hollow electrode, especially the portion overlapping with the dye liquid crystal layer 300 may be a hollow electrode.

[0077] The first alignment layer 130 is used to contact the dye liquid crystal layer 300 so that the liquid crystal molecules are arranged at a certain angle and direction. The first alignment layer 130 can be made of a flexible organic material, such as a polyimide material. In one embodiment of the present disclosure, the thickness of the first alignment layer 130 can be 20 to 100 nanometers, so that the liquid crystal molecules can be arranged at a predetermined angle and direction. Exemplarily, in one embodiment of the present disclosure, the thickness of the first alignment layer 130 can be in the range of 30 to 50 nanometers.

[0078] In the present disclosure, the second substrate 200 includes a second flexible substrate 210, a second light-transmitting electrode layer 220, and a second alignment layer 230, which are stacked in sequence from the outside to the inside. The outside of the second substrate 200 refers to the side away from the dye liquid crystal layer 300; correspondingly, the inside of the second substrate 200 refers to the side close to the dye liquid crystal layer 300.

[0079] Optionally, the material of the second flexible substrate 210 may be a flexible organic transparent material, for example, it may be PET (polyethylene terephthalate), PI (polyimide), PEN (polyethylene naphthalate) or other flexible resins and other transparent organic polymers. Exemplarily, in one embodiment of the present disclosure, the second flexible substrate 210 is a PET layer. Of course, in other embodiments of the present disclosure, the second flexible substrate 210 may also include multiple flexible organic material layers and inorganic layers sandwiched between the flexible organic material layers, and these flexible organic material layers and inorganic layers are all made of light-transmitting materials.

[0080] The thickness of the second flexible substrate 210 can be determined according to design requirements, so that the second flexible substrate 210 meets the requirements in terms of light transmittance, mechanical properties, etc. Optionally, the thickness of the second flexible substrate 210 can be between 100 microns and 2000 microns, especially between 300 microns and 600 microns.

[0081] In one embodiment of the present disclosure, the first flexible substrate 110 and the second flexible substrate 210 are identical in structure, thickness and material. In other words, the first flexible substrate 110 and the second flexible substrate 210 may be identical flexible substrates.

[0082] Optionally, the material of the second light-transmitting electrode layer 220 may be an organic conductive material, an organic / inorganic conductive composite material, or an inorganic conductive material, and in particular, may be a conductive metal oxide, such as indium gallium zinc oxide (IGZO), indium gallium oxide (IGO), indium zinc oxide (IZO), indium tin zinc oxide (ITZO), tin oxide (SnO2), zinc oxide (ZnO), indium tin oxide (ITO). Exemplarily, in one embodiment of the present disclosure, the second light-transmitting electrode layer 220 is an ITO layer.

[0083] Optionally, the second light-transmitting electrode layer 220 may be a whole electrode layer without being hollowed out or having a specific pattern. Of course, in other embodiments of the present disclosure, the second light-transmitting electrode layer 220 may also be a hollow electrode, especially the portion overlapping with the dye liquid crystal layer 300 may be a hollow electrode.

[0084] In one embodiment of the present disclosure, the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 are identical in structure, thickness and material. In other words, the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 may be the same light-transmitting electrode layer.

[0085] The second alignment layer 230 is used to contact the dye liquid crystal layer 300 so that the liquid crystal molecules are arranged at a certain angle and direction. The second alignment layer 230 can be made of a flexible organic material, such as a polyimide material. In one embodiment of the present disclosure, the thickness of the second alignment layer 230 can be 20 to 100 nanometers, so that the liquid crystal molecules can be arranged at a predetermined angle and direction. Exemplarily, in one embodiment of the present disclosure, the thickness of the second alignment layer 230 can be in the range of 30 to 50 nanometers.

[0086] In one embodiment of the present disclosure, the first alignment layer 130 and the second alignment layer 230 are identical in structure, thickness and material. In other words, the first alignment layer 130 and the second alignment layer 230 may be identical alignment layers.

[0087] In one embodiment of the present disclosure, the first substrate 100 and the second substrate 200 may be the same substrate.

[0088] In this disclosure, see Figure 1 to Figure 5 The dimming substrate PNL0 needs to be cut to form the required flexible dimming panel PNL. Specifically, the first substrate 100 and the second substrate 200 need to be cut to remove the redundant parts on the first substrate 100 and the second substrate 200, and to cut out pads on the first substrate 100 and the second substrate 200.

[0089] In the present disclosure, the trajectory of cutting the first substrate 100 is the first cutting line L100; after the first substrate 100 is cut along the first cutting line L100, the portion outside the first cutting line L100 is removed, and the portion inside the first cutting line L100 is retained as a reserved area of ​​the first substrate 100 (i.e., the first reserved area) to the flexible dimming panel. The first reserved area is the first substrate 100 of the flexible dimming panel PNL. After cutting, the first pad area A111 extends to the outside of the frame sealant 400 so as to serve as the first pad P100 on the first substrate 100. The first pad P100 can be bound and connected to the circuit board so that the circuit board supplies power to the first light-transmitting electrode layer 120. In one embodiment of the present disclosure, the circuit board has a plurality of first pins for binding and connecting with the first pad P100. These first pins are located at the first pad P100 and can pierce the first orientation layer 130 and the first light-transmitting electrode layer 120 and penetrate into the first flexible substrate 110, thereby achieving electrical connection with the first pad P100.

[0090] Correspondingly, in the present disclosure, the trajectory of cutting the second substrate 200 is the second cutting line L200; after the second substrate 200 is cut along the second cutting line L200, the portion outside the second cutting line L200 is removed, and the portion inside the second cutting line L200 is retained as the reserved area of ​​the second substrate 200 (i.e., the second reserved area) to the flexible dimming panel. The second reserved area is the second substrate 200 of the flexible dimming panel PNL. After cutting, the second pad area A211 extends to the outside of the frame sealant 400 so as to serve as the second pad P200 on the second substrate 200. The second pad P200 can be bound and connected to the circuit board so that the circuit board supplies power to the second light-transmitting electrode layer 220. In one embodiment of the present disclosure, the circuit board has a plurality of second pins for binding and connecting with the second pad P200. These second pins can pierce the second orientation layer 230 and the second light-transmitting electrode layer 220 and penetrate into the second flexible substrate 210 at the position of the second pad P200, thereby achieving electrical connection with the second pad P200.

[0091] See also Figure 1 , the first pad area A111 and the second pad area A211 do not overlap each other. Figure 4 The first pad P100 and the second pad P200 of the flexible dimming panel PNL do not overlap, so that the first pin and the second pin are respectively bound and connected to the first pad P100 and the second pad P200.

[0092] See also Figure 1 and Figure 3, the first cutting line L100 and the second cutting line L200 partially overlap, so as to facilitate the cutting of the dimming substrate PNL0 and make the flexible dimming panel PNL have a relatively flat edge. In the present disclosure, the part where the first cutting line L100 and the second cutting line L200 overlap each other is defined as the overall cutting line LL. At the overall cutting line LL, the first substrate 100 and the second substrate 200 can be cut at the same time or separately. In the flexible dimming panel PNL formed by cutting, see Figure 1 and Figure 4 The edge formed at the overall cutting line LL can be defined as the overall edge EE. It can be understood that in the flexible dimming panel PNL, the portion where the edge of the first substrate 100 and the edge of the second substrate 200 overlap each other is the overall edge EE of the flexible dimming panel PNL.

[0093] See also Figure 1 and Figure 3 , the portion of the first cutting line L100 that does not overlap with the second cutting line L200 can be used as the non-integral cutting line portion L101 of the first cutting line L100. The non-integral cutting line portion L101 of the first cutting line L100 and the integral cutting line portion L102 of the first cutting line L100 complement each other to form a closed track. The portion of the second cutting line L200 that does not overlap with the first cutting line L100 can be used as the non-integral cutting line portion L201 of the second cutting line L200. The non-integral cutting line portion L201 of the second cutting line L200 and the integral cutting line portion L202 of the second cutting line L200 complement each other to form a closed track.

[0094] Accordingly, see Figure 4 For the flexible dimming panel PNL formed by cutting, the portion of the edge E100 of the first substrate 100 that does not overlap with the edge E200 of the second substrate 200 can be used as the non-integral edge portion E101 of the first substrate 100. The non-integral edge portion E101 of the first substrate 100 and the integral edge portion E102 of the first substrate 100 complement each other to form a closed edge. For the flexible dimming panel PNL formed by cutting, the portion of the edge E200 of the second substrate 200 that does not overlap with the edge E100 of the first substrate 100 can be used as the non-integral edge portion E201 of the second substrate 200. The non-integral edge portion E201 of the second substrate 200 and the integral edge portion E202 of the second substrate 200 complement each other to form a closed edge.

[0095] In one embodiment of the present disclosure, see Figure 1The non-integrated cutting portion L101 of the first cutting line L100 is composed of the overlapping portion of the first cutting line L100 and the second pad area A211 and the portion of the first cutting line L100 adjacent to the first pad area A111. Figure 4 The non-integral edge portion E101 of the first substrate 100 is composed of the overlapping portion of the edge E100 of the first substrate 100 and the second pad P200, and the edge of the first pad P100.

[0096] In one embodiment of the present disclosure, the non-integral cutting line portion L201 of the second cutting line L200 is composed of the portion where the second cutting line L200 overlaps with the first pad area A111 and the portion where the second cutting line L200 is adjacent to the second pad area A211. Thus, in the formed flexible dimming panel PNL, the non-integral edge portion E201 of the second substrate 200 is composed of the portion where the edge E200 of the second substrate 200 overlaps with the first pad P100 and the edge of the second pad P200.

[0097] In one embodiment of the present disclosure, see Figure 3 , the overall cutting line LL overlaps with the frame sealant 400. In this way, at the overall cutting line LL, when the first substrate 100 and the second substrate 200 are cut at the same time, the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 can be isolated by the frame sealant 400, thereby preventing the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 of the flexible dimming panel PNL from being electrically connected to each other at the overall edge EE portion, thereby preventing a short circuit defect.

[0098] In step S120, the first substrate 100 and the second substrate 200 may be cut along the first cutting line L100 and the second cutting line L200, respectively. In this way, the remaining portion of the dimming substrate PNL0 may be used as the flexible dimming panel PNL of the present disclosure.

[0099] According to the preparation method disclosed in the present invention, see Figure 5The formed flexible dimming panel PNL includes a first substrate 100 and a second substrate 200 arranged in a box; between the first substrate 100 and the second substrate 200, the flexible dimming panel PNL is provided with a dye liquid crystal layer 300 and a sealant 400 surrounding the dye liquid crystal layer 300; the first substrate 100 includes a first flexible substrate 110, a first light-transmitting electrode layer 120 and a first orientation layer 130 stacked in sequence from the outside to the inside; the second substrate 200 includes a second flexible substrate 210, a second light-transmitting electrode layer 220 and a second orientation layer 230 stacked in sequence from the outside to the inside; wherein the first substrate 100 includes a first pad P100 located outside the sealant 400, and the second substrate 200 includes a second pad P200 located outside the sealant 400. wherein at least part of the edge of the first substrate 100 is flush with the edge of the sealant 400; and at least part of the edge of the second substrate 200 is flush with the edge of the sealant 400.

[0100] In the present disclosure, step S120 can be implemented by a variety of different methods, so as to further reduce defects generated during the cutting process and improve the yield of the flexible dimming panel PNL.

[0101] In the first implementation of the present disclosure, step S120 may be implemented by the method shown in steps S210 to S260.

[0102] Step S210, see Figure 8 , remove the first light-transmitting electrode layer 120 and / or the second light-transmitting electrode layer 220 on the overall cutting line LL; Figure 8 In the figure, the area where the light-transmitting electrode layer (the first light-transmitting electrode layer 120 and / or the second light-transmitting electrode layer 220) is removed is indicated by the oblique line filling area DD, and the position where the frame sealant 400 is removed is indicated by the dot filling area.

[0103] Step S220, see Fig. 9 , cutting the first substrate 100 and the second substrate 200 by laser along the overall cutting line LL;

[0104] Step S230, see Fig. 9 , the first flexible substrate 110 is cut along the non-integral cutting line portion L101 of the first cutting line L100, and the cutting depth does not exceed the thickness of the first flexible substrate 110. Fig.11 , the cut CC formed by cutting the first flexible substrate 110 does not cut off the first flexible substrate 110 .

[0105] Step S240, tearing off the portion of the first substrate 100 outside the first cutting line L100;

[0106] Step S250, see Fig. 9, the second flexible substrate 210 is cut along the non-integral cutting line portion L201 of the second cutting line L200, and the cutting depth does not exceed the thickness of the second flexible substrate 210; see Fig.12 , the cut CC formed by cutting the second flexible substrate 210 does not cut off the second flexible substrate 210 .

[0107] Step S260 , tearing off the portion of the second substrate 200 outside the second cutting line L200 .

[0108] Among them, in step S210, the first light-transmitting electrode layer 120 on the overall cutting line LL can be removed separately, and the second light-transmitting electrode layer 220 on the overall cutting line LL can also be removed separately. Of course, the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 on the overall cutting line LL can also be removed. In this way, there are no two light-transmitting electrode layers located on two substrates (the first substrate 100 or the second substrate 200) on the overall cutting line LL; that is, there is at most one light-transmitting electrode layer on the overall cutting line LL. In step S220, when the first substrate 100 and the second substrate 200 are cut simultaneously along the overall cutting line LL by using a laser, the two layers of light-transmitting electrode layers will not be connected to each other after melting and short-circuited, further reducing the risk of short-circuit defects. Specifically, if there is no light-transmitting conductive layer on the overall cutting line LL, no conductive material will be melted during the cutting process. If there is only one transparent electrode layer on the overall cutting line LL, even if the transparent conductive layer melts and forms punctures during laser cutting, it will not cause a short circuit between the two transparent electrode layers. Fig.10 In the formed flexible dimming panel PNL, at least one of the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 does not extend to the entire edge EE.

[0109] In a feasible manner, the first light-transmitting electrode layer 120 on the overall cutting line LL can be removed by the following method: the laser is transmitted from one side of the first flexible substrate 110 to the first light-transmitting electrode layer 120, and the first light-transmitting electrode layer 120 is melted along the overall cutting line LL. In this manner, by utilizing the difference in materials between the first light-transmitting electrode layer 120 and the first flexible substrate 110, the laser parameters (such as wavelength, power, etc.) are adjusted so that the laser is selectively irradiated onto the first light-transmitting electrode layer 120. In this way, the patterning of the first light-transmitting electrode layer 120 is achieved without damaging or cutting the first flexible substrate 110.

[0110] In a feasible manner, the second light-transmitting electrode layer 220 on the overall cutting line LL can be removed by the following method: the laser is transmitted from one side of the second flexible substrate 210 to the second light-transmitting electrode layer 220, and the second light-transmitting electrode layer 220 is melted along the overall cutting line LL. In this manner, by utilizing the difference in materials between the second light-transmitting electrode layer 220 and the second flexible substrate 210, the laser parameters (such as wavelength, power, etc.) are adjusted so that the laser is selectively irradiated onto the second light-transmitting electrode layer 220. In this way, the patterning of the second light-transmitting electrode layer 220 is achieved without damaging or cutting the second flexible substrate 210.

[0111] In step S230, the first flexible substrate 110 can be cut from the outside of the first substrate 100, and the first flexible substrate 110 can be cut to avoid damaging the first light-transmitting electrode layer 120. In some feasible ways, laser cutting can be used. By adjusting the parameters of the laser (such as wavelength, power, etc.), the laser is selectively irradiated onto the first flexible substrate 110, and the first flexible substrate 110 is melted from the outside to the inside in sequence, so as to achieve cutting of the first flexible substrate 110. By controlling the laser power and irradiation time, etc., the cutting depth can be controlled to avoid completely cutting the first flexible substrate 110 and damaging the first light-transmitting electrode layer 120.

[0112] In step S240, the portion of the first substrate 100 outside the first cutting line L100 (the portion to be removed) can be grasped and torn to separate it from the first reserved area of ​​the first substrate 100. For example, the portion to be removed can be grasped by a cutting staff to be torn off, or a tearing mechanism specially provided for the cutting equipment can be used to clamp the portion to be removed and tear it off.

[0113] In step S250, the second flexible substrate 210 can be cut from the outside of the second substrate 200, and the second flexible substrate 210 can be cut to avoid damaging the second light-transmitting electrode layer 220 by cutting off the second flexible substrate 210. In some feasible ways, laser cutting can be used. By adjusting the parameters of the laser (such as wavelength, power, etc.), the laser is selectively irradiated onto the second flexible substrate 210, and the second flexible substrate 210 is melted from the outside to the inside in sequence, so as to achieve cutting of the second flexible substrate 210. By controlling the laser power and irradiation time, etc., the cutting depth can be controlled to avoid completely cutting off the second flexible substrate 210 and damaging the second light-transmitting electrode layer 220.

[0114] In step S260, the portion of the second substrate 200 outside the second cutting line L200 (the portion to be removed) can be grasped and torn to separate it from the second reserved area of ​​the second substrate 200. For example, the portion to be removed can be grasped by the cutting personnel to be torn off, or the portion to be removed can be clamped and torn off by a tearing mechanism specially provided for the cutting equipment.

[0115] In a feasible manner, after completing step S230 and step S250, step S240 and step S260 may be performed simultaneously. Specifically, the portion to be removed of the first substrate 100 and the portion to be removed of the second substrate 200 may be clamped at the same time, and then the portion to be removed of the first substrate 100 and the portion to be removed of the second substrate 200 may be removed simultaneously by tearing.

[0116] In a second embodiment of the present disclosure, step S120 may be implemented by the method shown in steps S310 to S340.

[0117] Step S310, cutting the first flexible substrate 110 along the first cutting line L100, and the cutting depth does not exceed the thickness of the first flexible substrate 110; see Fig.11 , the cut CC formed by cutting the first flexible substrate 110 does not cut off the first flexible substrate 110 .

[0118] Step S320 , tearing off the portion of the first substrate 100 outside the first cutting line L100 .

[0119] Step S330, cutting the second flexible substrate 210 along the second cutting line L200, and the cutting depth does not exceed the thickness of the second flexible substrate 210; see Fig.12 , the cut CC formed by cutting the second flexible substrate 210 does not cut off the second flexible substrate 210 .

[0120] Step S340 , tearing off the portion of the second substrate 200 outside the second cutting line L200 .

[0121] In step S310, the first flexible substrate 110 can be cut from the outside of the first substrate 100, and the first flexible substrate 110 can be cut to avoid damaging the first light-transmitting electrode layer 120 by cutting off the first flexible substrate 110. Among them, in some feasible methods, laser cutting can be used. By adjusting the parameters of the laser (such as wavelength, power, etc.), the laser is selectively irradiated onto the first flexible substrate 110, and the first flexible substrate 110 is melted from the outside to the inside in sequence, so as to achieve the cutting of the first flexible substrate 110. By controlling the laser power and irradiation time, etc., the cutting depth is controlled to avoid completely cutting off the first flexible substrate 110 and damaging the first light-transmitting electrode layer 120. Of course, in other embodiments of the present disclosure, other methods can also be used to cut the first flexible substrate 110, for example, a cutter wheel can be used to cut the first flexible substrate 110 from the outside of the first flexible substrate 110.

[0122] In step S320, the portion of the first substrate 100 outside the first cutting line L100 (the portion to be removed) can be grasped and torn to separate it from the first reserved area of ​​the first substrate 100. For example, the portion to be removed can be grasped by a cutting staff to be torn off, or a tearing mechanism specially provided for the cutting equipment can be used to clamp the portion to be removed and tear it off.

[0123] In step S330, the second flexible substrate 210 can be cut from the outside of the second substrate 200, and the second flexible substrate 210 can be cut to avoid damaging the second light-transmitting electrode layer 220 by cutting off the second flexible substrate 210. Among them, in some feasible methods, laser cutting can be used. By adjusting the parameters of the laser (such as wavelength, power, etc.), the laser is selectively irradiated onto the second flexible substrate 210, and the second flexible substrate 210 is melted from the outside to the inside in sequence, so as to achieve the cutting of the second flexible substrate 210. By controlling the laser power and irradiation time, etc., the cutting depth is controlled to avoid completely cutting off the second flexible substrate 210 and damaging the second light-transmitting electrode layer 220. Of course, in other embodiments of the present disclosure, other methods can also be used to cut the second flexible substrate 210, for example, a cutter wheel can be used to cut the second flexible substrate 210 from the outside of the second flexible substrate 210.

[0124] In step S340, the portion of the second substrate 200 outside the second cutting line L200 (the portion to be removed) can be grasped and torn to separate it from the second reserved area of ​​the second substrate 200. For example, the portion to be removed can be grasped by the cutting personnel to be torn off, or the portion to be removed can be clamped and torn off by a tearing mechanism specially provided for the cutting equipment.

[0125] In the second embodiment, the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 are torn off at the first cutting line L100 and the second cutting line L200 respectively, and the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 will not be melted and electrically contacted, thereby further reducing the risk of short circuit failure.

[0126] In a feasible manner, after completing step S310 and step S330, step S320 and step S340 may be performed simultaneously. Specifically, the portion to be removed of the first substrate 100 and the portion to be removed of the second substrate 200 may be clamped at the same time, and then the portion to be removed of the first substrate 100 and the portion to be removed of the second substrate 200 may be removed simultaneously by tearing.

[0127] In a third implementation of the present disclosure, step S120 may be implemented by the method shown in steps S410 to S450.

[0128] Step S410, punching the first substrate 100 and the second substrate 200 along the overall cutting line LL;

[0129] Step S420, cutting the first flexible substrate 110 along the non-integral cutting line portion L101 of the first cutting line L100, and the cutting depth does not exceed the thickness of the first flexible substrate 110; see Fig.11 , the cut CC formed by cutting the first flexible substrate 110 does not cut off the first flexible substrate 110 .

[0130] Step S430, tearing off the portion of the first substrate 100 outside the first cutting line L100;

[0131] Step S440 , cutting the second flexible substrate 210 along the non-integral cutting line portion L201 of the second cutting line L200 , and the cutting depth does not exceed the thickness of the second flexible substrate 210 ;

[0132] Step S450 , tearing off the portion of the second substrate 200 outside the second cutting line L200 .

[0133] In the third embodiment, quick cutting can be achieved by punching in step S410. In step S410, since there is no need to perform laser melting on the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220, the punching process will not cause the first light-transmitting electrode layer 120 and the second light-transmitting electrode layer 220 to be electrically connected at this position, thereby further reducing the risk of short circuit failure.

[0134] In a feasible manner, steps S420 to S450 may be performed with reference to the method shown in steps S230 to S460, and the present disclosure will not elaborate on them here.

[0135] In a fourth implementation of the present disclosure, step S120 may be implemented by the method shown in steps S510 to S530.

[0136] Step S510, see Figure 6 , a blocking gasket 500 is inserted between the first substrate 100 and the second substrate 200, and the blocking gasket 500 at least overlaps with the first pad area A111 and the second pad area A211;

[0137] Step S520, punching the first substrate 100 along the first cutting line L100;

[0138] Step S530 , punching the second substrate 200 along the second cutting line L200 .

[0139] Among them, in step S510, the blocking gasket 500 can be inserted between the first substrate 100 and the second substrate 200. In this way, when punching, if punching is performed at the position of the gasket, the substrate (the first substrate 100 or the second substrate 200) below the gasket will not be damaged. In this way, in step S520, the blocking gasket 500 will provide protection for the second pad area A211 to prevent the second light-transmitting electrode layer 220 of the second pad area A211 from being damaged by punching. Correspondingly, in step S530, the blocking gasket 500 will provide protection for the first pad area A111 to prevent the first light-transmitting electrode layer 120 of the first pad area A111 from being damaged by punching.

[0140] In this embodiment, the first substrate 100 and the second substrate 200 are cut by punching, which avoids the first light-transmitting electrode layer 120 and the second electrode layer from melting and causing a short circuit, and further reduces the risk of a short circuit defect.

[0141] In a feasible implementation, the blocking gasket 500 may overlap only the first pad area A111 and the second pad area A211. In this way, the blocking gasket 500 can specifically protect the first pad P100 and the second pad P200 of the flexible dimming panel PNL. Exemplarily, the number of the blocking gaskets 500 is two, and the two blocking gaskets 500 overlap the first pad area A111 and the second pad area A211, respectively.

[0142] In some other embodiments, the blocking gasket 500 may not only overlap the first pad area A111 and the second pad area A211, but may also extend to the area between the first pad area A111 and the second pad area A211; further, the blocking gasket 500 may also extend in the direction of the first pad area A111 away from the second pad area A211, and in the direction of the second pad area A211 away from the first pad area A111. In this way, the range that the blocking gasket 500 can protect is larger than the first pad area A111 and the second pad area A211, which can reduce the alignment requirements of the blocking gasket 500 when inserted and increase the process window for inserting the blocking gasket 500.

[0143] In one possible mode of the fourth embodiment, see Figure 6 , the blocking gasket 500 can be inserted between the first substrate 100 and the second substrate 200, and is not inserted into the sealant 400. The portion where the first cutting line L100 overlaps with the second pad area A211 is located outside the sealant 400; the portion where the second cutting line L200 overlaps with the first pad area A111 is located outside the sealant 400. In this way, the blocking gasket 500 can provide protection for the first pad area A111 and the second pad area A211. Accordingly, see Figure 7 In the formed flexible dimming panel PNL, the portion of the non-integral edge portion E101 of the first substrate overlapping with the second pad P200 can extend to the outside of the sealant 400. Correspondingly, the portion of the non-integral edge portion E201 of the second substrate overlapping with the first pad P100 can extend to the outside of the sealant 400.

[0144] It should be noted that, although the steps of the method for preparing the flexible dimming panel in the present disclosure are described in a specific order in the accompanying drawings, this does not require or imply that the steps must be performed in this specific order, or that all the steps shown must be performed to achieve the desired results. Additionally or alternatively, some steps may be omitted, multiple steps may be combined into one step, and / or one step may be decomposed into multiple steps, etc.

[0145] Those skilled in the art will readily appreciate other embodiments of the present disclosure after considering the specification and practicing the invention disclosed herein. This application is intended to cover any modification, use or adaptation of the present disclosure, which follows the general principles of the present disclosure and includes common knowledge or customary techniques in the art that are not disclosed in the present disclosure. The specification and examples are intended to be exemplary only, and the true scope and spirit of the present disclosure are indicated by the appended claims.

Claims

1. A method for preparing a flexible dimming panel, characterized in that: include: A dimming substrate is provided, the dimming substrate comprising a first substrate and a second substrate arranged in a box; between the first substrate and the second substrate, the dimming substrate is provided with a dye liquid crystal layer and a frame sealant surrounding the dye liquid crystal layer; the first substrate comprises a first flexible substrate, a first light-transmitting electrode layer and a first orientation layer stacked in sequence from the outside to the inside; the second substrate comprises a second flexible substrate, a second light-transmitting electrode layer and a second orientation layer stacked in sequence from the outside to the inside; the first substrate has a first reserved area surrounded by a first cutting line, the first reserved area has a first pad area extending to the outside of the frame sealant; the second substrate has a second reserved area surrounded by a second cutting line, the second reserved area has a second pad area extending to the outside of the frame sealant; the first cutting line and the second cutting line both overlap at least partially with the frame sealant; Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively; The part where the first cutting line and the second cutting line overlap each other is the whole cutting line; Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes: removing the first light-transmitting electrode layer and / or the second light-transmitting electrode layer on the overall cutting line; Cutting the first substrate and the second substrate along the overall cutting line by laser; Cutting the first flexible substrate along a non-integral cutting line portion of the first cutting line, wherein the cutting depth does not exceed the thickness of the first flexible substrate; tearing off a portion of the first substrate outside the first cutting line; Cutting the second flexible substrate along the non-integral cutting line portion of the second cutting line, and the cutting depth does not exceed the thickness of the second flexible substrate; A portion of the second substrate outside the second cutting line is removed.

2. The method for preparing the flexible dimming panel according to claim 1, characterized in that: The overall cutting line overlaps with the frame sealing adhesive.

3. The method for preparing the flexible dimming panel according to claim 1, characterized in that: The non-integral cutting line portion of the first cutting line is composed of a portion where the first cutting line overlaps with the second pad area and a portion of the first cutting line adjacent to the first pad area; The non-integral cutting line portion of the second cutting line consists of a portion where the second cutting line overlaps the first pad area and a portion of the second cutting line adjacent to the second pad area.

4. The method for preparing the flexible dimming panel according to claim 1, characterized in that: Removing the first light-transmitting electrode layer on the overall cutting line includes: Allowing laser to transmit from one side of the first flexible substrate to the first light-transmitting electrode layer, and fusing the first light-transmitting electrode layer along the overall cutting line; Removing the second light-transmitting electrode layer on the overall cutting line includes: The laser is transmitted from one side of the second flexible substrate to the second light-transmitting electrode layer, and the second light-transmitting electrode layer is melted along the integral cutting line.

5. A method for preparing a flexible dimming panel, characterized in that: include: A dimming substrate is provided, the dimming substrate comprising a first substrate and a second substrate arranged in a box; between the first substrate and the second substrate, the dimming substrate is provided with a dye liquid crystal layer and a frame sealant surrounding the dye liquid crystal layer; the first substrate comprises a first flexible substrate, a first light-transmitting electrode layer and a first orientation layer stacked in sequence from the outside to the inside; the second substrate comprises a second flexible substrate, a second light-transmitting electrode layer and a second orientation layer stacked in sequence from the outside to the inside; the first substrate has a first reserved area surrounded by a first cutting line, the first reserved area has a first pad area extending to the outside of the frame sealant; the second substrate has a second reserved area surrounded by a second cutting line, the second reserved area has a second pad area extending to the outside of the frame sealant; the first cutting line and the second cutting line both overlap at least partially with the frame sealant; Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively; Cutting the first substrate and the second substrate along the first cutting line and the second cutting line respectively includes: Cutting the first flexible substrate along the first cutting line, wherein the cutting depth does not exceed the thickness of the first flexible substrate; tearing off a portion of the first substrate outside the first cutting line; Cutting the second flexible substrate along the second cutting line, wherein the cutting depth does not exceed the thickness of the second flexible substrate; A portion of the second substrate outside the second cutting line is removed.