Method and device for forming three-dimensional microstructure

Through the oblique scanning technology of the light dot array without a mask exposure machine and the polygonal micro-cap array, combined with the digital micro-reflector and micro-lens array, the problems of low manufacturing efficiency and complex design of three-dimensional microstructures in the existing technology are solved. Achieve high-precision and low-cost three-dimensional microstructure production.

CN113835294BActive Publication Date: 2024-12-06李永春
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202110579299.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-06-23
Filing Date
2021-05-26
Publication Date
2024-12-06
Estimated Expiration
2041-05-26

AI Technical Summary

Technical Problem

It is difficult for the prior art to efficiently manufacture high-precision, multi-scale three-dimensional microstructures, especially in electronic products such as liquid crystal display backlight modules, traditional methods have problems such as easy tool, long manufacturing cycle, and complex design.

Method used

Adopt the oblique scanning technology of a high-precision mask-free exposure machine, combined with the polygonal micro-capsule array, and the oblique scanning of the mask array and the substrate covered by the photoresist, and use digital micro-reflectors and micro-lens arrays to perform beam shaping. , dynamically adjust the intensity and direction of light to form a high-precision three-dimensional microstructure.

Benefits of technology

It realizes high-precision, low-cost and rapid production of three-dimensional microstructures, solves the problems of low manufacturing efficiency and complex design in traditional methods, and is suitable for large-area and high-yield three-dimensional microstructure manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113835294B_ABST
    Figure CN113835294B_ABST
Patent Text Reader

Abstract

The present invention provides a method and apparatus for forming three-dimensional microstructures on, for example, a light guide plate or an integrated circuit. On one hand, the present invention allows a mask array having one or more special profile masks and a substrate covered by a photoresist layer to move relative to each other, and on the other hand, allows each light beam projected through the mask array to be adjusted individually and dynamically, thereby exposing the photoresist layer to form a patterned photoresist layer with different portions corresponding to different three-dimensional microstructures. In particular, the relative movement direction between the mask array and the substrate intersects with both the row direction and the column direction of the mask array. By adjusting this relative movement direction, it is possible to at least adjust how the photoresist layer is patterned and the corresponding profiles and distribution of each three-dimensional microstructure formed on the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention claims priority to U.S. Provisional Application No. 63 / 042,608, filed on June 23, 2020, the entire contents of which are incorporated herein by reference.

[0002] The present invention relates to a method and apparatus for forming a three-dimensional microstructure, and more particularly to a method and apparatus for forming a three-dimensional microstructure by using oblique scanning between a mask array and a substrate covered by a photoresist and elastically transferring the mask array pattern to the photoresist. Background Art

[0003] In modern electronic products and modern electronic product manufacturing processes, the importance of three-dimensional microstructures is increasing day by day. For example, in flat panel displays, it is often necessary to form a plurality of three-dimensional microstructures on a light guide plate (LGP), and by changing the propagation direction and propagation intensity of light passing through any three-dimensional microstructure, the uniformity and light extraction efficiency of the entire LGP can be changed. For example, in integrated circuits, with the increasing popularity of non-planar components such as fin transistors (Fin Field Effect Transistors), it is often inevitable to use three-dimensional microstructures in semiconductor manufacturing processes to form non-planar transistors, etc., or even directly form three-dimensional microstructures that are part of non-planar components. Therefore, there is a strong need to continuously develop new methods and devices to form the required three-dimensional microstructures. Summary of the invention

[0004] The present invention proposes a method based on the oblique scanning technology of the light spot array of a high-precision maskless exposure machine, combined with a polygonal micro mask array, to achieve the goal of three-dimensional microstructure processing by dragging the mask array. This new exposure processing principle is to inherit the oblique scanning of the UV light spot array, use the digital micromirror device (DMD) and the UV light source module to control the digital image, and use the microlens array, with the arbitrary polygon mask array as a spatial filter and UV beam shaping, to obtain a three-dimensional microstructure with the highest precision and the smallest line width; the most important invention of this patent is to use a "UV beam shaping" processing method, with the above-mentioned UV mask array oblique scanning, this microstructure processing method is applied to the mold manufacturing of the display backlight module, with the advantages of high yield, large area, design flexibility, etc., can be used to replace the traditional use of mechanical ultra-precision processing machines, the problems of easy damage to the tool, long mold manufacturing cycle, and difficult integration of the design process end, and is applied to the LCD backlight module (LCDbacklight module). le) industry.

[0005] Some embodiments of the present invention implement beam shaping by using a plurality of digital micro-mirrors and an arbitrary polygonal mask array, which can not only directly expose the photoresist but also adjust the exposure dose and exposure position. Based on the characteristic that the exposure dose can be arbitrarily adjusted, these embodiments can flexibly adjust the exposure result of the photoresist, thereby forming the required three-dimensional microstructure on the substrate covered by the photoresist. Depending on actual needs, such as three-dimensional microstructures of different sizes that need to be exposed, one digital micro-mirror can correspond to one polygonal mask array, or any plurality of digital micro-mirrors can correspond to one polygonal mask array, so as to select the best combination of digital micro-mirrors and polygonal masks according to the size and morphology of the three-dimensional microstructure to be formed.

[0006] Some embodiments of the present invention are based on a digital micro-mirror array, with a polygonal mask array, and achieve the goal of three-dimensional microstructure processing by oblique scanning motion of the mask array. These embodiments are regulated by a digital micro-mirror device (DMD) and a light source module, with an arbitrary polygonal mask arranged in an array, to achieve light beam shaping, thereby obtaining a three-dimensional microstructure with high precision and small line width on a substrate covered by a photoresist. Since micro-mirror devices and micro-lenses are already commercial products, such as those disclosed on the Texas Instruments website https: / / www.mouser.com / new / texas-instruments / ti-dlp470tp-dmd / , there are no technical difficulties in the specific implementation of these embodiments.

[0007] In the present invention, the main feature of the mask array is the mask with a special profile, where the special profile can be equal to the profile of the three-dimensional microstructure to be formed, or can be a profile similar to the three-dimensional microstructure profile calculated based on the properties of the photoresist, etc. In the present invention, the relative movement path between the mask array and the substrate covered by the photoresist, that is, the scanning line, intersects with the arrangement direction of the masks on the mask array, that is, when the masks are arranged in the row direction and the column direction to form a two-dimensional array, or the scanning line intersects with both the row direction and the column direction, or the mask array is rotated at an angle relative to the scanning line, that is, the mask array and the substrate are obliquely scanned. In the present invention, the main feature of the digital micro-mirror array (or light spot array) composed of the digital micro-mirror device and the light source module is that different parts thereof can be turned on or off or adjusted individually, so that the light projected onto the photoresist on the substrate can come from different parts thereof at different times, and even the light intensity and / or direction from different parts at different times can be different.

[0008] In the present invention, the projection position and projection profile of each mask in the mask array on the photoresist can be adjusted by changing the angle between the scan line and the row direction and the column direction of the mask array, or in other words, by adjusting the angle of rotation of the mask array relative to the scan line. In the present invention, during the relative movement between the mask array and the substrate covered by the photoresist, the same light or different light can be projected through the mask array at different times and reach different parts of the photoresist layer. In this way, the present invention can flexibly adjust the profile of the exposed photoresist, thereby adjusting the three-dimensional microstructure formed on the substrate covered by the exposed photoresist in the subsequent process.

[0009] It must be emphasized that the present invention does not need to be limited to specific details. For example, ultraviolet light can be used, but other wavelengths of light can also be used. A digital micromirror device (DMD) can be used in combination with a mask array, but other hardware can also be used in combination with the mask array to transfer different mask patterns to the photoresist layer at different times. For example, each mask possessed by the mask array usually has the same profile (size / shape) and the same arrangement direction, but can also have individual variations if necessary. For example, the angle of oblique scanning, or the angle between the mask array and the scan line, often depends on how many masks there are in the mask array along the scan line direction when the angle between the mask array and the scan line is zero, that is, it depends on the number of masks possessed by the mask array or the number of mask projections that will appear in the direction perpendicular to the scan line during oblique scanning, but it can also depend on other factors, such as the distribution density, shape, plane size and three-dimensional depth of each three-dimensional structure that needs to be formed on the substrate.

[0010] In short, the present invention provides a method and device for forming a three-dimensional microstructure. This method allows an oblique scan to be performed between a mask array and a substrate covered by a photoresist layer, that is, the scanning line between the two and the arrangement direction of the mask array are intersected, and on the other hand, during the oblique scanning, light is flexibly projected through the mask array as needed to reach the photoresist layer on the substrate, thereby forming a patterned photoresist layer corresponding to the required three-dimensional microstructure, so that the subsequent process can use this patterned photoresist layer to form the required three-dimensional microstructure on the substrate. This device has at least a light spot array (such as a digital micro-mirror array) that can flexibly provide light, a mask array with a special contour mask, and a drive assembly that can drive the mask array and the substrate covered by the photoresist layer to perform oblique scanning, so that under the control of a computer or a microprocessor, the photoresist layer is exposed to become a patterned photoresist layer corresponding to the required three-dimensional microstructure. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 is a schematic diagram of a summary of existing photoresist patterning process technology.

[0012] Figure 2 FIG. 1 is a summary showing the oblique scanning used in the present invention.

[0013] Figure 3 The present invention provides a method for forming a three-dimensional microstructure.

[0014] Figure 4 The invention provides a device for forming a three-dimensional microstructure.

[0015] Figure 5 It shows how a single mask of different shapes will form patterns on the photoresist layer after relative motion and exposure.

[0016] Figure 6 These are some embodiments of the device for forming a three-dimensional microstructure proposed by the present invention.

[0017] Fig. 7A 7H to 7H are embodiments of the exposure method of the digital micromirror device of the present invention.

[0018] Fig. 8A to Figure 8B The graphs respectively show the characteristic curves of the commonly used photoresist materials showing an exponential distribution and the relationship between the exposure dose and the structure depth corrected by the present invention.

[0019] Fig. 9 Qualitatively demonstrate the basic mathematical properties of some equations used to calculate the actual characteristic curves of exposure dose and development depth of photoresist materials.

[0020] Fig.10 The optical power distribution per unit area is calculated by surface fitting and assuming energy distribution.

[0021] Fig.11A The structure depth-exposure dose curve for the single-sided slope structure and the designed d-frontal mask pattern obtained according to the above calculation are shown.

[0022] Fig. 11B to Fig. 11C The cross sections of two target structures and the designed mask patterns obtained according to the above calculations are shown respectively.

[0023] Fig.12 Display the target of 3D microstructure processing and calculate the corresponding 3D exposure dose distribution and the 3D structure depth after development. DETAILED DESCRIPTION

[0024] The present invention improves the existing photoresist patterning process. Figure 1 The schematic diagram of the conventional photoresist patterning process technology is shown, along the Z axis, the substrate 110 is covered by the photoresist layer 120, and the mask 130 and the light source 140 are arranged in sequence and separated from each other and the photoresist layer 110. The substrate 110 and the photoresist layer 120 can move along the X axis and the mask 130 (and even the light source 140) can move along the Y axis. By controlling the respective movements, the photoresist layer 120 can be converted into a patterned photoresist layer with a specific pattern 150, so that the specific pattern 150 can be transferred to the substrate 110 in the subsequent etching process to form the desired three-dimensional microstructure.

[0025] The present invention has at least the following improvements over the existing photoresist patterning process. First, oblique scanning is used, that is, when a plurality of masks are arranged into a two-dimensional mask array, the mask array is rotated at an angle relative to the scanning line between the mask array and the substrate, or when the mask array is located on a two-dimensional plane, the scanning line and the row and column directions of the two-dimensional mask array are intersected with each other. By adjusting the angle between each other, the profile (size, dimension and direction) of each mask projection along the direction perpendicular to the scanning line and the distribution (density, position) of all mask projections can be adjusted, thereby changing the special pattern of the patterned photoresist layer and adjusting the three-dimensional microstructure subsequently formed on the substrate 110. Second, the light projected onto the photoresist layer can be dynamically and flexibly adjusted, so that during the relative movement between the mask array and the substrate, light can be projected or not projected onto different parts of the mask array at different times to transfer different mask patterns, or even light of different intensities can be projected onto the same or different parts of the mask array at different times to fully or partially transfer the patterns of the same or different parts of the mask array, so that a certain special pattern as required can be formed on different parts of the photoresist layer 120, or even different special patterns as required can be formed separately.

[0026] The oblique scanning used in the present invention can be summarized as follows: Figure 2 As shown, a plurality of masks with the same profile are arranged into a mask array 201 with M rows and N columns. Any mask itself corresponds to m and n light spots in the row direction and column direction respectively. The scanning direction 202 between the substrate (not shown) and the mask array 201 intersects with the column direction of the mask array 201 to form an angle θ. The light direction of the light from the light source (not shown) also intersects with the scanning direction, so that each mask has a mask projection 203 in the scanning direction, and the distance between adjacent mask projections 203 along the scanning direction 202 is smaller than the distance between adjacent masks along the row direction or column direction of the mask array 201. Figure 2 As shown, the difference between the distance between adjacent mask projections 202 and the distance between adjacent masks depends on the angle between the scanning direction and the row direction (or column direction) of the two-dimensional array.

[0027] In brief, the present invention provides a method for forming a three-dimensional microstructure, such as Figure 3First, as shown in step block 301, the mask array and the substrate covered by the photoresist layer are allowed to move relative to each other along the scanning line, wherein the mask array has at least one mask with a special profile arranged in an array, and the scanning line intersects with the arrangement direction of the mask array. Second, as shown in step block 302, during the relative movement of the mask array and the substrate, the projected light passes through the mask array and reaches the photoresist layer, thereby forming a patterned photoresist layer having a profile corresponding to the three-dimensional microstructure to be formed. Of course, although not in Figure 3 It is shown that the method can also perform an etching process after the relative movement ends and the patterned photoresist layer is formed to form a three-dimensional microstructure on the substrate.

[0028] In brief, the present invention provides a device for forming a three-dimensional microstructure, such as Figure 4 As shown, there is a mask array 401, a light spot array (such as a digital micro-mirror array) 402, and a driving assembly 403. Here, the mask array 401 is configured to have at least one mask with a special contour arranged in an array, the light spot array 402 is configured to have at least one light spot that can be individually operated and arranged in an array (such as a digital micro-mirror array composed of at least one digital micro-mirror that can be individually operated and arranged in an array), and the driving assembly 403 is configured to allow the mask array 401 and the substrate 4042 covered by the photoresist layer 4041 to move relative to each other along the scanning line 405. Here, the scanning line 405 intersects with the arrangement direction of the mask array 401, and the light spot array 402 (such as a digital micro-mirror array) provides light during the relative movement of the mask array 401 and the substrate 4042, so as to form a patterned photoresist layer having a contour corresponding to the three-dimensional microstructure to be formed. Although not shown in Figure 4 It is shown that the device may further include an etching assembly, which is configured to perform an etching process to form a three-dimensional microstructure on the substrate 4042 after the relative movement ends and the photoresist layer is patterned.

[0029] It must be emphasized that the present invention does not require many restrictions on hardware details and process details. For example, as long as oblique scanning can be achieved, it does not matter how the mask array is rotated or how the rotation angle is adjusted. After all, the key is to rotate the mask array to an angle relative to the scan line so as to adjust how the photoresist layer is patterned accordingly. For example, as long as relative movement can be achieved along the scan line (or the relative movement direction), it does not matter whether only the mask array is moved, only the substrate is moved, or both the mask array and the substrate are moved, and it does not matter whether the mask array and the substrate move relative to each other along the scan line at a fixed rate. For example, as long as light can be transmitted to the photoresist layer through the mask array to form the required special pattern when needed, it does not matter how the light spot array (such as a digital micro-mirror array), the mask array and the substrate are relatively moved. For example, depending on the contour of the special pattern to be formed (or the three-dimensional microstructure to be formed), ultraviolet light, deep ultraviolet light, yellow light or light with other wavelengths can be used. For example, in order to dynamically transfer patterns from different parts of the mask array to different parts of the photoresist layer, different digital micro-mirrors (i.e., different light spots) can be individually turned on or off, and the intensity of the light generated can be individually adjusted. In addition, at different first moments and second moments during the relative movement of the mask array and the substrate, light from a first light spot group (such as the first digital micro-mirror group) and light from a second light spot group (such as the second digital micro-mirror group) can be allowed to pass through the mask array and reach the photoresist layer, respectively, wherein one or more light spots (or one or more digital micro-mirrors) included in the first light spot group are different from one or more light spots (or one or more digital micro-mirrors) included in the second light spot group. Here, the light spot array may be a combination of a large light source and a plurality of digital micro-mirrors (i.e., a digital micro-mirror array), so as to dynamically provide light through different parts of the mask array by dynamically adjusting whether each digital micro-mirror reflects light from the large light source to the mask array, or may be a plurality of tiny light sources arranged in a two-dimensional array, so as to dynamically provide light through different parts of the mask by dynamically adjusting the turning on or off of each tiny light source. For example, each mask in the mask array usually has the same shape, the same size, and the same arrangement direction, but at least two masks may have different shapes, different sizes, and / or different arrangement directions as needed.

[0030] It must be emphasized that the present invention does not need to be limited to what the three-dimensional microstructure is formed, that is, the present invention can be applied to many modern electronic products and modern electronic product processes. For example, the present invention can be applied to the production of light guide plates in backlight modules used in liquid crystal displays, etc. The present invention can arbitrarily adjust the characteristics of the exposure dose. In addition to having greater flexibility in design and production, it can also improve the production efficiency of the entire light guide plate mold, thereby improving the existing light guide plate process chemical etching, ultra-precision machining, photolithography and internal diffusion, and other methods, which are generally faced with the shortcomings of slow processing rate, low yield, difficult to control microstructure morphology, and difficult large-scale production. For example, the present invention can be used to make components such as memory and / or integrated circuits. For example, the well-known yellow light lithography process has been widely used, and the present invention can further optimize the existing lithography process by using oblique scanning between the mask and the substrate and a light source that can output light with different spatial distributions at different times. Even if the hardware used is not significantly improved, the required three-dimensional microstructure can be made more efficiently and flexibly.

[0031] Furthermore, when the present invention uses oblique scanning, basically, the projections of the masks on the mask array in the direction perpendicular to the scanning line are usually uniformly distributed, and / or the projections of at least M masks on the mask array in the direction perpendicular to the scanning line are overlapped, where M is a positive integer greater than 1. In particular, a commonly used option is to rotate the mask array relative to the scanning line by an angle Here N is the number of masks along the scan line when the rotation angle is zero. When a mask in the mask array is illuminated by light from a light spot array (such as a digital micro-mirror array) that has m and n light spots in each row and column respectively, and the length and width dimensions of each light spot (such as each digital micro-mirror) are Δ, the mask pattern will form an energy distribution in the exposed part of the photoresist layer, and then accumulate into a three-dimensional energy distribution along the scan line with the relative movement between the mask array and the substrate. Here, if the scan line is parallel to the y-axis, there will be different mask opening sizes at different x-coordinates in the direction perpendicular to the scan line. Where k is a constant coefficient to be determined, and the size of the mask opening will determine the exposure dose accumulation along the scan line after the relative motion and exposure of the photoresist layer. Obviously, as long as the value of m and / or Δ increases, a three-dimensional photoresist structure with high spatial resolution can be exposed over a large area, thereby forming a three-dimensional microstructure with high spatial resolution on the substrate after a subsequent etching process. For example, in a certain embodiment, 64 digital micromirrors with a length and width of 13.68 μm are arranged in an array of 8 rows and 8 columns as a subunit of the digital micromirror array, and a mask array with a row number and a column number between 128 and 1024 and between 96 and 768, respectively, is used. At this time, the constant coefficient k ranges from 0.1 to 5, and the angle θ ranges from 0.010416 to 0.001302 (rad / radian). As an example, Figure 5 A number of different shapes of single masks are shown ( Figure 5 Left side) after relative motion and exposure ( Figure 5 What kind of pattern will be formed on the photoresist layer (middle) Figure 5 On the right side), the black part represents the light being blocked, the white part represents the light being completely penetrated, and the gray part represents the slope band where the dose gradually accumulates. Obviously, when the contour of the three-dimensional microstructure to be formed is different, the pattern to be formed on the photoresist layer will be different, thus requiring a single mask of different shapes. That is, the pattern of each mask in the mask array is designed separately for the contour of the three-dimensional microstructure to be formed. Figure 1 The shape of the opening of the middle mask 130 for allowing light to pass through is a diamond shape, which is a mask specially designed for the special pattern 150 that needs to be transferred to the photoresist layer 120.

[0032] Some embodiments of the device for forming a three-dimensional microstructure according to the present invention can be summarized as follows: Figure 6Here, a digital micro-mirror array 601 is used as a light point array, which includes an ultraviolet light-emitting diode light source (UltraViol et Light-Emitting Diode Light Source) 6011 that can provide ultraviolet light, a reflector (Refl ect ion Mirror) 6012 that can change the direction of ultraviolet light, a reverse total internal reflection mirror (Reverse Total Internal Refl ect ion) 6013 whose opposite surfaces can respectively allow ultraviolet light to be refracted and reflected, a digital micro-mirror device (Digital Micromirror Device) 6014 having one or more digital micro-mirrors that can reflect ultraviolet light and change the reflection direction, and a first and a second imaging lens group (Projection Lens) 6015 / 6016 that can be used to adjust the uniformity of the ultraviolet light beam passing through. Here, the mask array 602 includes a spatial filter array (Micro lens Pinhole Array) 6021 and is located between two imaging lens groups 6015 / 6016, and the driving assembly 603 includes a motion platform 6031 and can move the substrate 605 covered by the photoresist layer 604. Obviously, in this embodiment, only the substrate 605 moves, but the digital micro-mirror array 601 and the mask array 602 are fixed, and the number of digital micro-mirrors of the digital micro-mirror device 6014 can be adjusted. By means of the programming of the computer 6061 and the motion controller 6062, it is possible to specify which digital micro-mirrors in the digital micro-mirror device 6014 are turned on at different moments during the relative movement between the mask array 602 and the substrate 605 so as to reflect back the ultraviolet light from the reflector 6012 through the inverted internal total reflection mirror 6013. That is, it is possible to control which parts of the mask array 602 (or which masks of the mask array 602 will be illuminated) the ultraviolet light from the digital micro-mirror device 6014 through the inverted internal total reflection mirror 6013 will pass through. That is, it is possible to generate a beam shaping effect (or change the profile of the ultraviolet light beam that will reach the photoresist layer 604) after the ultraviolet light passes through the mask array 602. Thus, it is possible to arbitrarily control how the pattern of the mask array 602 is transferred to the photoresist layer 604 at different times, such as transferring the entire pattern of the entire mask array 602 at a specific time or only transferring a specific part of the pattern of the mask array 602 at a specific time, that is, different patterns can be transferred to the photoresist layer 604 at different parts of the scan line.That is, since the relative movement between the two-dimensional mask array 602 and the substrate 605 can generate a three-dimensional energy accumulation distribution in the photoresist layer 604 along the scanning line, and the digital micro-mirror device 6014 can be controlled to be turned on or off at a specific position, these embodiments can be used to produce a patterned photoresist layer 604 with a special pattern having an arbitrary position distribution, variable length and three-dimensional morphology corresponding to the three-dimensional microstructure that needs to be formed on the substrate 605.

[0033] The present invention proposes two exposure methods of the digital micro-mirror device. The first method is to project a corresponding polygonal mask array using a digital micro-mirror. Fig. 7A and Figure 7B , and the second is that any number of (8x8=64 in the figure) digital micro-mirrors project a corresponding polygonal mask array, such as Figure 7C and Fig.7D The difference between the two architectures is that they can expose three-dimensional microstructures of different sizes, so users can choose the best digital micromirror / pinhole mask combination according to the size and morphology of the microstructure.

[0034] Arbitrary polygonal mask arrays made by semiconductor yellow light lithography process, such as Fig. 7E , and a digital micromirror device (DMD) produced by Texas Instruments (TI), the reflected ultraviolet light is projected through the first imaging lens group to form an image, such as Figure 7F Each ultraviolet light reflection unit is projected onto the surface of the mask array and the corresponding mask array is individually lit. Figure 7G The digital micro-mirror device and the first imaging lens group provide a uniform illumination ultraviolet light source for the mask array. After the light source passes through the mask array, a "beam shaping" effect is produced. After the second imaging lens group forms an image, the polygonal mask pattern is projected onto the exposure processing imaging surface. With the unidirectional dragging motion of the motion platform, Figure 7H The direction of the middle arrow is the scanning direction, so the energy of this two-dimensional polygonal mask array produces a three-dimensional energy cumulative distribution along the scanning line direction. At this time, if the digital micro-mirror device is controlled to turn on or off at a specific position, a three-dimensional microstructure with arbitrary spatial distribution can be produced on the processing surface.

[0035] In addition, in practical applications, different photoresist materials often have different characteristic curves of exposure dose and development depth, and the commonly used photoresist materials have characteristic curves showing an exponential distribution. Fig. 8AAs shown in FIG. 1 , the normalized exposure dose reaches a dose threshold of 22% or more, which is sufficient to cause sufficient chemical reaction after the photoresist is developed to peel off (positive photoresist) or leave (negative photoresist), thereby forming a structure. If the photoresist is to be completely peeled off or left, the exposure dose needs to be increased to make the depth of the structure after development increase or decrease exponentially. Therefore, the present invention can consider the exposure dose and structure depth curve again, using Figure 8B The relationship between exposure dose and structure depth is calculated using a modified exponential distribution as shown in the figure. Where h(x,y) represents the structure depth h after the exposure intensity of the accumulated dose I(x,y) on the Karlsruhe coordinates (x,y) obtained by photoresist development, and h max is the thickness of the photoresist layer before exposure, I0 is the cumulative exposure dose threshold, and A and B are coefficients to be determined. In some embodiments, h and h max The range of is between 1 and 50 μm, the range of I0 is between 1 and 100 mJ / cm2 (millijoules / square centimeter) (this is the property of general photoresist materials), and the range of both A and B is between 0 and 50. In the case of negative photoresist, when the accumulated exposure dose I(x, y) is large enough, the depth of the structure after development approaches the thickness of the photoresist coating, that is, Based on the photoresist characteristic curve processed by this correction index analysis, the relationship between the mask array pattern, exposure dose and three-dimensional micro-dose morphology can be calculated. Fig. 9 By using surface fitting and assuming that the energy distribution can be approximated by a two-dimensional Gaussian distribution function, the optical power distribution per unit area can be calculated. for C and σ x ,σ y is the undetermined coefficient. In some embodiments, the undetermined coefficient C is greater than 0 but less than 1000, and the other two undetermined coefficients are both greater than 0.01 but less than 100. Next, considering the two-dimensional image convolution, the scanning speed, the exposure start point (x1, y1) and the exposure end point (x2, y2), the three-dimensional cumulative energy distribution can be obtained. Where ** is the two-dimensional image convolution operator, I(x, y) is the accumulated energy and its unit is mJ (millijoule), N is the number of steps of the motion platform used to push the substrate covered by the photoresist layer during exposure scanning, and δ(x+(x1-k△x), y+(y1-k△y)) is the Dirac delta function with the offset in space being (x1+k△x, y1+k△y), △x and △y are the small steps along the scanning direction on the XY plane, and △t is the dose accumulation time factor representing the time spent from the start point of exposure to the end point of exposure, which can also be expressed as Therefore, starting from the convolution of the two-dimensional image, we can know Among them, ξ,η are dummy variables, with a range of -∞<ξ,η<∞, which are used to prevent variable conflicts when mathematically calculating two-dimensional convolution and variable transformation. Finally, substitute the above results into the exposure dose and structure depth equation Then we can get the complete corrected version of the equation: According to this equation, as long as the coefficients A and B of the relationship between exposure dose and structure depth are measured and calculated, and the scanning exposure path (x1, y1)→(x2, y2), step (△x, △y) and speed v are determined, as well as the three-dimensional energy distribution equation e(x, y) of the mask array aperture, the three-dimensional structure morphology equation after exposure and development can be calculated. In addition, when the light power distribution is axisymmetric and the exposure scan is along the +x direction, e(x, y) can be simplified to And δ(x+(x1-k△x),y+(y1-k△y)) is simplified to δ(x+(x1-k△x)), so the accumulated energy distribution I(x,y) can be simplified to I(x), that is

[0036]

[0037] Here, Fig.10 Qualitatively demonstrate the basic mathematical properties of some of the above equations used to calculate the actual characteristic curves of exposure dose and development depth of photoresist materials. In addition, Fig.11A The structure depth-exposure dose curve for the single-sided slope structure and the designed mask pattern obtained according to the above calculation are shown. Fig. 11B and Fig. 11C The cross sections of the two target structures and the designed mask patterns obtained according to the above calculations are shown respectively.

[0038] The present invention proposes a light spot array oblique scanning technology using a high-precision maskless exposure machine, combined with a polygonal micro mask array, to achieve the goal of three-dimensional microstructure processing by dragging the mask array, and calculate the corresponding three-dimensional exposure dose distribution and the three-dimensional structure depth after development, such as Fig.12 .

[0039] Obviously, according to the description in the above embodiments, the present invention may have many modifications and differences. Therefore, it is necessary to understand that within the scope of patent protection of the claims, in addition to the above detailed description, the present invention can also be widely implemented in other embodiments. The above is only a preferred embodiment of the present invention, and is not intended to limit the scope of patent protection of the present invention; any other equivalent changes or modifications that are completed without departing from the spirit disclosed by the present invention should be included in the scope of protection of this patent.

Claims

1. A method for forming a three-dimensional microstructure, comprising: Allowing a mask array and a substrate covered by a photoresist layer to move relative to each other along a scanning line, wherein the mask array has at least one mask with a special profile arranged in an array, and the scanning line is obliquely crossed with the arrangement direction of the mask array; During the relative movement between the mask array and the substrate, a light spot array is used to project light through the mask array to reach the photoresist layer, thereby forming a patterned photoresist layer having a contour corresponding to the three-dimensional microstructure to be formed; After the relative movement ends and the patterned photoresist layer is formed, an etching process is performed to form a three-dimensional microstructure on the substrate; and At least according to the profile of the three-dimensional microstructure to be formed and the material of the photoresist, the profile of each mask in the mask array is set, and the following three-dimensional structure morphology equation is used to reversely infer how to form the required patterned photoresist layer according to the required profile of the three-dimensional microstructure: Here, h(x,y) is the structural depth of the photoresist after development after exposure intensity of cumulative dose I(x,y) at the Cartesian coordinate (x,y), hmax is the thickness of the photoresist layer, I 0 is the cumulative exposure dose threshold, A, B and k are three coefficients, (x 1 ,y 1 ) and (x 2 ,y 2 ) are the Cartesian coordinates of the start and end points of the scan line, (Δx, Δy) are the small steps along the scan line, and v is the relative movement speed of the mask array and the substrate along the scan line.

2. The method according to claim 1, It is characterized in that Also includes one of the following: Allow the mask array and the substrate to move relative to each other along the scanning line at a fixed rate; Only move the mask array along the scan line; and Only move the substrate along the scan line.

3. The method according to claim 1, It is characterized in that Further includes at least one of the following: The projections of the masks on the mask array in the direction perpendicular to the scanning line are evenly distributed; The projections of at least M masks on the mask array in a direction perpendicular to the scanning line overlap each other, where M is a positive integer greater than 1; and Rotate the mask array by an angle relative to the scan line Here, N is the number of masks that the mask array has along the scanning line direction when the rotation angle is zero.

4. The method according to claim 1, It is characterized in that The method further comprises allowing light from a first light spot group and a second light spot group of the light spot array to pass through the mask array and reach the photoresist layer at different first and second moments during the relative movement of the mask array and the substrate, respectively, wherein one or more light spots included in the first light spot group are different from one or more light spots included in the second light spot group, and the operation of the light spot array comprises one of the following: Different light spots can be turned on or off individually; and The intensity of the light generated by different light points can be adjusted individually.

5. The method according to claim 4, It is characterized in that The method further comprises using a digital micro-mirror array having at least one digital micro-mirror as the light spot array, wherein different digital micro-mirrors can be individually turned on, turned off and / or the intensity of the light generated can be adjusted.

6. A device for forming a three-dimensional microstructure, It is characterized in that Include: a mask array configured to have at least one mask with a specific profile arranged in an array; A driving assembly is configured to allow the mask array and a substrate covered by a photoresist layer to move relative to each other along a scanning line, where the scanning line is obliquely intersecting with the arrangement direction of the mask array; A light spot array is configured to have at least one light spot that can be operated individually and arranged in an array; Here, when the mask array and the substrate are in relative motion, the light spot array provides light to form a patterned photoresist layer having a contour corresponding to the three-dimensional microstructure to be formed; An etching assembly is configured to perform an etching process to form a three-dimensional microstructure on the substrate after the relative movement ends and the patterned photoresist layer is formed; as well as A control assembly is configured to perform the following operations: Controlling the operation of the light spot array, the light mask array and the drive assembly; and At least according to the profile of the three-dimensional microstructure to be formed and the material of the photoresist, the profile of each mask in the mask array is set, wherein the control assembly uses the following three-dimensional structure morphology equation to reversely infer how to form the required patterned photoresist layer according to the required profile of the three-dimensional microstructure: Here, h(x,y) is the structural depth of the photoresist after development after exposure intensity of cumulative dose I(x,y) at the Cartesian coordinate (x,y), hmax is the thickness of the photoresist layer, I 0 is the cumulative exposure dose threshold, A, B and k are three coefficients, (x 1 ,y 1 ) and (x 2 ,y 2 ) are the Cartesian coordinates of the start and end points of the scan line, (Δx, Δy) are the small steps along the scan line, and v is the relative movement speed of the mask array and the substrate along the scan line.

7. The device according to claim 6, It is characterized in that Also includes one of the following: The drive assembly allows the mask array and the substrate to move relative to each other along the scan line at a fixed rate; The drive assembly only moves the mask array along the scan line; The drive assembly moves the substrate only along the scan line; and Each array in the mask array has the same shape, the same size and the same arrangement direction; The driving assembly allows the projections of the masks on the mask array in a direction perpendicular to the scanning line to be evenly distributed; The driving assembly allows projections of at least M masks on the mask array in a direction perpendicular to the scanning line to overlap each other, where M is a positive integer greater than 1; and The drive assembly rotates the mask array at an angle relative to the scan line. Here, N is the number of masks that the mask array has along the scanning line direction when the rotation angle is zero.

8. The device according to claim 6, It is characterized in that It further includes allowing light from the first light spot group and from the second light spot group to pass through the mask array from the light spot array to reach the photoresist layer at a first moment and a second moment different during the relative movement of the light spot array and the substrate, respectively, wherein one or more light spots included in the first light spot group are different from one or more light spots included in the second light spot group.

9. The device according to claim 6, It is characterized in that The operation of this light spot array includes one of the following: Different light spots can be turned on or off individually; and The intensity of the light generated by different light points can be adjusted individually.

10. The device according to claim 9, It is characterized in that The operation of the light spot array includes: when a digital micro-mirror array having at least one digital micro-mirror is used as the light spot array, different digital micro-mirrors can be individually turned on, turned off and / or the intensity of the light generated can be adjusted.

Citation Information

Patent Citations

  • 3D gray exposure method for inclined high-speed scanning based on DMD

    CN116819899A