Semiconductor device and method for forming the same
By using a higher and partially overlapping hard mask layer structure in semiconductor devices, the problem of improving the electrical performance of multi-gate transistors is solved, the device size is reduced and the electrical performance is improved, and the stability and use range of the device are ensured.
Patent Information
- Application Number
- CN202010641641.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-07-06
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-07-06
AI Technical Summary
The electrical performance of multi-gate transistors in the existing technology still needs to be improved. Especially after the device size is reduced, the photolithography process constraints are difficult to overcome, making it difficult to achieve performance improvement.
By designing a specific hard mask layer structure in the semiconductor device, the top surface of the second hard mask layer is higher than the first hard mask layer and partially overlaps it to form the first and second interconnection layers to implement the gate. The reduction of the structure and the safe distance during electrical connection avoid short-circuit problems.
It effectively improves the electrical performance and stability of semiconductor devices, is suitable for manufacturing smaller-sized semiconductor devices, and expands its scope of use.
Smart Images

Figure CN113903803B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a semiconductor device and a method for forming the same. Background Art
[0002] Over the past several decades, the scaling of feature sizes in integrated circuits has been the driving force behind the growing semiconductor industry. Scaling to smaller and smaller feature sizes enables increased density of functional units on the limited substrate area of a semiconductor chip. For example, reducing transistor size allows an increased number of memory or logic devices to be included on a chip, resulting in the manufacture of products with increased capacity. But the drive for greater capacity is not without its problems. The necessity to optimize the performance of each device becomes increasingly apparent.
[0003] In the manufacture of integrated circuit devices, multi-gate transistors become more common as device dimensions continue to shrink. In conventional processes, multi-gate transistors are usually manufactured on a silicon substrate or a silicon-on-insulator substrate.
[0004] But shrinking the size of multi-gate transistors is not without its problems. As the size of these basic building blocks of microelectronic circuits decreases, and as the absolute number of basic building blocks manufactured in a given area increases, the constraints of the photolithography process used to form the building block patterns become difficult to overcome. The electrical performance of multi-gate transistors in the prior art still needs to be improved. Summary of the invention
[0005] The technical problem solved by the present invention is to provide a semiconductor device and a method for forming the same, which can effectively improve the performance of the finally formed semiconductor device.
[0006] To solve the above problems, the present invention provides a semiconductor device, comprising: a substrate; a gate structure located on the substrate; a source-drain doped layer located in the substrate on both sides of the gate structure; a conductive layer located on the source-drain doped layer; a first hard mask layer located on the top of the gate structure; a second hard mask layer located on the top surface of the conductive layer, the top surface of the second hard mask layer is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer.
[0007] Optionally, a top surface of the second hard mask layer is 3 nm to 10 nm higher than a top surface of the first hard mask layer.
[0008] Optionally, an angle between a sidewall of the second hard mask layer and a sidewall of the gate structure is 0° to 10°.
[0009] Optionally, the method further includes: a first interconnection layer located in the first hard mask layer and located on the top of the gate structure between the source and drain doping layers.
[0010] Optionally, the method further includes: a second interconnect layer located in the second hard mask layer and on top of the conductive layer.
[0011] Optionally, a first interlayer dielectric layer is further included, which is located on top of the first hard mask layer, and an etching rate of the first interlayer dielectric layer is greater than an etching rate of the first hard mask layer.
[0012] Optionally, a second interlayer dielectric layer is further included, located on top of the first interlayer dielectric layer and the second hard mask layer.
[0013] Correspondingly, the present invention also provides a method for forming a semiconductor device, comprising: providing a substrate, the substrate having a gate structure and a source-drain doped layer located in the substrate on both sides of the gate structure; forming a first hard mask layer on the top surface of the gate structure; forming a first interlayer dielectric layer on the substrate, the first interlayer dielectric layer covering the first hard mask layer; etching the first interlayer dielectric layer until the top surface of the source-drain doped layer is exposed to form a first opening; forming a conductive layer in part of the first opening, the top surface of the conductive layer is lower than the top surface of the first interlayer dielectric layer; forming a second hard mask layer on the conductive layer, the second hard mask layer fills the remaining first opening, the top surface of the second hard mask layer is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer.
[0014] Optionally, a top surface of the second hard mask layer is 3 nm to 10 nm higher than a top surface of the first hard mask layer.
[0015] Optionally, an angle between a sidewall of the second hard mask layer and a sidewall of the gate structure is 0° to 10°.
[0016] Optionally, a portion of the second hard mask layer is etched to form a second opening in the second hard mask layer, wherein the bottom of the second opening exposes the top surface of the conductive layer; a second interconnect layer is formed in the second opening; the first hard mask layer between the source and drain doping layers is etched to expose the top surface of the gate structure to form a third opening, and a first interconnect layer is formed in the third opening.
[0017] Compared with the prior art, the technical solution of the present invention has the following advantages:
[0018] In the semiconductor device of the present invention, the process of subsequently forming the first interconnection layer and the second interconnection layer is simple. Since the top surface of the second hard mask layer is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer, on the one hand, the first interconnection layer is formed in the first hard mask layer, and is located on the top of the gate structure between the source and drain doping layers, and is electrically connected to the gate structure, which helps to reduce the size of the gate structure, thereby adapting to the manufacture of smaller semiconductor device sizes; on the other hand, the top surface of the first hard mask layer located on the top of the gate structure is lower than the top surface of the second hard mask layer located on the top surface of the conductive layer, and the second hard mask layer partially overlaps with the first hard mask layer, so that when the second interconnection layer is formed on the top of the conductive layer, a safe distance is provided between the second interconnection layer and the gate structure, thereby avoiding bridging and short circuit between the second interconnection layer and the gate structure; at the same time, when the first interconnection layer is formed on the gate structure, a safe distance is ensured between the first interconnection layer and the conductive layer, thereby avoiding the short circuit problem between the first interconnection layer and the conductive layer, thereby improving the electrical performance and stability of the formed semiconductor device.
[0019] In the formation method of the present invention, after forming a gate structure on a substrate, source-drain doped layers are formed in the substrate on both sides of the gate structure, a conductive layer is formed on the source-drain doped layers, a first hard mask layer is formed on the top surface of the gate structure, and a second hard mask layer is formed on the top of the conductive layer. The top surface of the second hard mask layer is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer. In this way, on the one hand, a first interconnection layer located on the top of the gate structure is subsequently formed in the first hard mask layer, and the first interconnection layer is located on the gate structure between the source-drain doped layers. Not only does the first interconnection layer form on the gate structure in the source region (active), but also the size of the gate structure is reduced, making it suitable for smaller sizes. The invention relates to the manufacture of semiconductor devices. Moreover, due to the partial overlap between the first hard mask layer and the second hard mask layer, the distance between the first interconnection layer and the conductive layer formed in the first hard mask layer is increased, thereby avoiding the short circuit problem between the first interconnection layer and the conductive layer. On the other hand, due to the height of the second hard mask layer being higher than the height of the first hard mask layer, when the second interconnection layer is subsequently formed in the second hard mask layer to realize the electrical connection with the conductive layer, the existence of the second hard mask layer increases the distance between the second interconnection layer and the gate structure, thereby avoiding the short circuit between the gate structure and the second interconnection layer, thereby improving the electrical performance and stability of the finally formed semiconductor device and expanding the use range of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 to Figure 2 is a cross-sectional view of a semiconductor structure in one embodiment;
[0021] Figure 3 to Figure 4is a cross-sectional view of a semiconductor structure in another embodiment;
[0022] Figures 5 to 22 It is a structural schematic diagram of a formation process of a semiconductor device according to an embodiment of the present invention. DETAILED DESCRIPTION
[0023] The electrical performance of the COAG structure MOSFET in the prior art still needs to be improved.
[0024] Figure 1 to Figure 2 is a cross-sectional view of a semiconductor structure in one embodiment.
[0025] Figure 1 for Figure 2 A top view of Figure 2 yes Figure 1 Section view at section line AA.
[0026] Please refer to Figure 1 to Figure 2 , a substrate 100; a fin 101, located on the substrate 100; a gate structure 102, spanning the fin 101; a sidewall 103, located on the sidewall of the gate structure 102; a source-drain doped layer 104, located in the fin 101 on both sides of the gate structure 102; a conductive layer 105, located on the top of the source-drain doped layer 104; a first hard mask layer 106, located on the top surface of the gate structure 102; a second hard mask layer 107, located on the top of the conductive layer 105, and the second hard mask layer 107 is located on the top of the sidewall 103; a dielectric layer 108, located on the first hard mask layer 106 and the second hard mask layer 107; a second interconnect layer 109, located in the second hard mask layer 107 and on the top of the conductive layer 105.
[0027] In the above embodiment, from Figure 2 It can be seen that after the second interconnect layer 109 is formed, since the distance between the second interconnect layer 109 and the gate structure 102 is small (the dotted circle part in the figure), a short circuit is likely to occur between the second interconnect layer 109 and the gate structure 102 during the electrical connection process, thereby affecting the usability of the semiconductor device.
[0028] Another method for forming a semiconductor structure will be described in detail below with reference to the accompanying drawings.
[0029] Figure 3 to Figure 4 is a cross-sectional view of a semiconductor structure in another embodiment.
[0030] Figure 3 for Figure 4 A top view of Figure 4 yes Figure 3 Section view at section line AA.
[0031] Please refer to Figure 3 and Figure 4 , substrate 200; fin 201, located on the substrate 200; gate structure 202, spanning the fin 201; sidewall 203, located on the sidewall of the gate structure 202; source-drain doped layer 204, located in the fin 201 on both sides of the gate structure 202; conductive layer 205, located on the top of the source-drain doped layer 204; a first hard mask layer 206, located on the top surface of the gate structure 202; a second hard mask layer 207, located on the top of the conductive layer 205 and not covering the top of the sidewall 203; a dielectric layer 208, located on the first hard mask layer 206 and the second hard mask layer 207; a first interconnect layer 209, located in the first hard mask layer 206 and located on the top of the gate structure 202 between the source-drain doped layer 204.
[0032] In the above embodiment, from Figure 4 It can be seen that after the first interconnection layer 209 is formed, due to the small distance between the first interconnection layer 209 and the conductive layer 205, a short circuit (the dotted circle part in the figure) is likely to occur between the first interconnection layer 209 and the conductive layer 205 during the electrical connection process, which affects the usability of the semiconductor device.
[0033] In order to overcome the above problems, the present invention utilizes a second hard mask layer whose top surface is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer. Thus, on the one hand, a first interconnection layer located at the top of the gate structure is formed in the first hard mask layer, and the first interconnection layer is located on the gate structure between the source and drain doping layers. Not only is the first interconnection layer formed on the gate structure in the source region (active), so that the size of the gate structure is reduced and suitable for the manufacture of semiconductor devices of smaller sizes, but also, due to the partial overlap between the first hard mask layer and the second hard mask layer, the distance between the first interconnection layer formed in the first hard mask layer and the conductive layer is increased, thereby avoiding the short circuit problem between the first interconnection layer and the conductive layer. On the other hand, since the height of the second hard mask layer is higher than the height of the first hard mask layer, when the second interconnection layer is formed in the second hard mask layer to realize electrical connection with the conductive layer, due to the existence of the second hard mask layer, the distance between the second interconnection layer and the gate structure is increased, thereby avoiding the short circuit between the gate structure and the second interconnection layer, thereby improving the electrical performance and stability of the finally formed semiconductor device, and expanding the use range of the semiconductor device.
[0034] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0035] Figures 5 to 22It is a structural schematic diagram of a formation process of a semiconductor device according to an embodiment of the present invention.
[0036] Please refer to Figure 5 , providing a substrate 300.
[0037] In this embodiment, the base 300 includes a substrate 301 and a plurality of discretely arranged fins 302 located on the substrate 301 , and the fins 302 extend along the second direction X.
[0038] In other embodiments, the fin 302 may not be formed on the substrate 301 .
[0039] In this embodiment, the material used for the substrate 301 is single crystal silicon.
[0040] In other embodiments, the substrate 301 may also be polycrystalline silicon or amorphous silicon. The substrate 301 may also be made of semiconductor materials such as germanium, silicon germanium, gallium arsenide, silicon on insulator (SOI), and germanium on insulator (GOI).
[0041] In this embodiment, the material of the fin 302 is silicon; in other embodiments, the material of the fin 302 may also be a semiconductor material such as silicon germanium.
[0042] In this embodiment, the method for forming the fin 302 includes: forming a fin material film (not shown) on the substrate 301; forming a patterned layer (not shown) on the fin material film; etching the fin material film using the patterned layer as a mask until the surface of the substrate 301 is exposed to form the fin 302.
[0043] In this embodiment, an isolation structure 303 is further formed on the substrate 301 , and the isolation structure 303 covers a portion of the sidewall of the fin 302 .
[0044] In this embodiment, the isolation structure 303 is made of silicon nitride.
[0045] In other embodiments, the material of the isolation structure 303 may also include one or more combinations of materials such as silicon nitride (SiN), silicon oxynitride (SiON), silicon carbide (SiC), silicon oxycarbide (SiOC), silicon carbon nitride (SiCN), silicon oxycarbonitride (SiOCN), and silicon carbon boron nitride (SiCBN).
[0046] In this embodiment, the isolation structure 303 functions to form electrical isolation.
[0047] The method for forming the isolation structure 303 includes: forming an isolation structure film (not shown) covering the fin structure 302 on the substrate 301 ; and etching back the isolation structure film to form the isolation structure 303 .
[0048] The process for forming the isolation structure film is a deposition process, such as a fluid chemical vapor deposition process. The isolation structure film is formed by the fluid chemical vapor deposition process, so that the filling performance of the isolation structure film is better.
[0049] The steps of the fluid chemical vapor deposition process used to form the isolation structure film include: forming an isolation fluid layer on the substrate 301; and performing water vapor annealing to form the isolation structure film from the isolation fluid layer.
[0050] The parameters of the water vapor annealing include: the gases used include oxygen, ozone and gaseous water, and the annealing temperature is 350 degrees Celsius to 750 degrees Celsius.
[0051] Please refer to Figures 6 to 11 A gate structure is formed on the substrate 300, and source-drain doping layers are provided in the substrate on both sides of the gate structure.
[0052] Please refer to Figure 6 and Figure 7 , Figure 6 yes Figure 7 A top view of Figure 7 yes Figure 6 In the cross-sectional view taken along line AA, a dummy gate structure 304 is formed on the substrate 300 .
[0053] In this embodiment, a dummy gate structure 304 is formed on the substrate 301 and crosses the fin 302 .
[0054] In this embodiment, the dummy gate structure 304 includes: a dummy gate dielectric layer 305 located on the fin 302 , a dummy gate layer 306 located on the dummy gate dielectric layer 305 , and a protection layer 307 located on the dummy gate layer 306 .
[0055] In this embodiment, the material of the dummy gate dielectric layer 305 is silicon oxide.
[0056] In this embodiment, the material of the dummy gate layer 306 is polysilicon.
[0057] In this embodiment, the material of the protective layer 307 includes: silicon nitride or silicon oxide; in other embodiments, the material of the protective layer 307 can also be one or more combinations of materials such as silicon carbide (SiC), silicon oxynitride (SiON), silicon oxycarbide (SiOC), silicon carbonitride (SiCN), silicon oxycarbonitride (SiOCN), and silicon carbon boron nitride (SiCBN).
[0058] In this embodiment, the protection layer 307 protects the dummy gate layer 306 during the subsequent process of forming the source-drain doping layer, and also serves as a stop layer for the subsequent planarization of the dielectric layer.
[0059] In this embodiment, a spacer 308 is further formed on the sidewalls of the dummy gate layer 306 and the protection layer 307 .
[0060] In this embodiment, the material of the side wall 308 is silicon oxide; in other embodiments, the material of the side wall 308 can also be one or more combinations of materials such as silicon nitride (SiN), silicon carbide (SiC), silicon oxynitride (SiON), silicon oxycarbide (SiOC), silicon carbonitride (SiCN), silicon oxycarbonitride (SiOCN), and silicon boron carbonitride (SiCBN).
[0061] The sidewall spacer 308 is used to define the position of the subsequently formed source and drain doping layer, and the sidewall spacer 308 is used to protect the sidewall of the dummy gate layer 306 to prevent the subsequently formed gate layer from having morphological defects that affect the electrical performance of the semiconductor structure.
[0062] The method for forming the sidewall 308 includes: forming a sidewall material layer (not shown) on the top surface of the pseudo gate dielectric layer 305, the sidewall of the pseudo gate layer 306, and the sidewall and top surface of the protective layer 307; and etching back the sidewall material layer until the protective layer 307 and the top surface of the fin 302 are exposed to form the sidewall 308.
[0063] The formation process of the sidewall material layer is one or more combinations of a chemical vapor deposition process, a physical vapor deposition process or an atomic layer deposition process.
[0064] The process of back-etching the side wall material layer is anisotropic dry etching, and the process parameters of the dry etching are: using fluorine-containing gas (such as CH3F, CH2F2 or CHF3), argon and oxygen, the etching power is 200W~400W, the pressure of the etching chamber is 30mTorr~200mTorr, and the etching temperature is 40℃~60℃.
[0065] Please refer to Figure 6 In the present embodiment, the pseudo gate structure 304 has only the first region I. This is because in the subsequent process of forming the first interconnection layer on the gate structure, the first interconnection layer is formed on the top of the gate structure between the source and drain doping layers, thereby shortening the length of the gate structure finally formed, thereby improving the integration of the semiconductor device and preparing for the manufacture of semiconductor devices with higher integration.
[0066] Please refer to Figure 8 , Figure 8 and Figure 7In accordance with the viewing direction, the source-drain doping layer 309 is formed in the substrate 200 on both sides of the dummy gate structure 304.
[0067] In this embodiment, the fins 302 on both sides of the dummy gate structure 304 are etched to form the source-drain doped layer 309 in the fins 302 .
[0068] The source-drain doping layer 309 has source-drain doping ions.
[0069] The process of forming the source-drain doping layer 309 includes an epitaxial growth process; the process of doping source-drain doping ions in the source-drain doping layer 309 is an in-situ doping process.
[0070] When the semiconductor device is a P-type device, the material of the source-drain doping layer 309 includes: silicon, germanium or silicon germanium; the source-drain doping ions are P-type ions, including boron ions, BF 2- ions or indium ions; when the semiconductor device is an N-type device, the material of the source and drain doping layer 309 includes: silicon, gallium arsenide or indium gallium arsenic; the source and drain doping ions are N-type ions, including phosphorus ions or arsenic ions.
[0071] In this embodiment, the semiconductor device is a P-type device, the material of the source-drain doping layer 309 is silicon, and the source-drain doping ions are boron ions. In other embodiments, the semiconductor device is an N-type device, the material of the source-drain doping layer 309 is silicon, and the source-drain doping ions are phosphorus ions.
[0072] In this embodiment, the process of etching the fin 302 is an anisotropic dry etching process, and the parameters of the dry etching process include: the etching gases used include HBr and Ar, wherein the gas flow rate of HBr is 10 sccm to 1000 sccm, and the gas flow rate of Ar is 10 sccm to 1000 sccm.
[0073] Please refer to Fig. 9 A dielectric layer 310 is formed on the substrate 300 and the source-drain doped layer 309 , and the dielectric layer 310 exposes the top surface of the dummy gate structure 304 .
[0074] In this embodiment, the dielectric layer 310 is formed on the substrate 301 and the source-drain doping layer 309 , and the dielectric layer 310 covers the sidewalls of the dummy gate structure 304 and exposes the top surface of the protection layer 307 .
[0075] In this embodiment, the method for forming the dielectric layer 310 includes: forming a dielectric layer material layer on the substrate 301 and the source-drain doping layer 309, the dielectric layer material layer covering the top surface of the pseudo gate structure 304, and planarizing the dielectric layer material layer until the top surface of the protective layer 307 is exposed to form the dielectric layer 310.
[0076] In this embodiment, the material of the dielectric layer 310 is silicon oxide; in other embodiments, the material of the dielectric layer 310 can also be a low-k dielectric material (low-k dielectric material refers to a dielectric material with a relative dielectric constant lower than 3.9) or an ultra-low-k dielectric material (ultra-low-k dielectric material refers to a dielectric material with a relative dielectric constant lower than 2.5).
[0077] In this embodiment, the dielectric layer 310 is formed by a chemical vapor deposition process; in other embodiments, the dielectric layer 310 may be formed by a chemical vapor deposition process, a physical vapor deposition process or an atomic layer deposition process or a combination of the two.
[0078] Please refer to Fig.10 , the dummy gate structure 304 is removed by etching until the surface of the substrate 300 is exposed, thereby forming a gate opening 311 .
[0079] In this embodiment, the dummy gate layer 306 and the dummy gate dielectric layer 305 are removed, and the gate opening 311 is formed between the sidewalls 2308 .
[0080] In this embodiment, the process for removing the dummy gate structure 304 is a wet etching process, and specifically, tetramethylammonium hydroxide (TMAH) is used as an etching solution.
[0081] In other embodiments, the process of removing the dummy gate structure 304 may also be a dry etching process.
[0082] Please refer to Fig.11 , a gate structure 312 is formed in the gate opening 311 , and a top surface of the gate structure 312 is lower than a top surface of the dielectric layer 310 .
[0083] In this embodiment, the gate structure 312 includes a gate dielectric layer (not shown in the figure) and a gate layer (not shown in the figure) located on the gate dielectric layer.
[0084] In this embodiment, the material of the gate dielectric layer includes a high-K dielectric material, such as oxides - Al2O3, HfO2, Ta2O5, TiO2, ZrO2, etc.
[0085] In other embodiments, the material of the gate dielectric layer may further include other dielectric materials with a dielectric constant higher than 3.9.
[0086] In this embodiment, the material of the gate layer is metal, and the metal material includes one or more combinations of copper, tungsten, nickel, chromium, titanium, tantalum and aluminum.
[0087] In this embodiment, the method for forming the gate structure 312 includes: forming the gate dielectric layer on the sidewalls and bottom of the gate opening 311, forming an initial gate material layer on the gate dielectric layer, and flattening the initial gate material layer until the top surface of the gate material layer is lower than the top of the dielectric layer 310, thereby forming the gate layer 312.
[0088] In this embodiment, the gate structure 312 fills approximately two-thirds of the gate opening 311 , and the remaining space is used to subsequently form a first hard mask layer on the top surface of the gate structure 312 .
[0089] Please refer to Fig.12 A first hard mask layer 313 is formed on the top surface of the gate structure 312 , and the top surface of the first hard mask layer 313 is flush with the top surface of the dielectric layer 310 .
[0090] In this embodiment, the material of the first hard mask layer 313 is silicon nitride.
[0091] In other embodiments, the material of the first hard mask layer 313 may also be one or more combinations of silicon carbide (SiC), silicon oxynitride (SiON), silicon oxycarbide (SiOC), silicon carbonitride (SiCN), silicon oxycarbonitride (SiOCN), silicon carbon boron nitride (SiCBN) and the like.
[0092] In this embodiment, the step of forming the first hard mask layer 313 includes: forming an initial first hard mask layer material on the gate structure 312 and the dielectric layer 310, flattening the initial first hard mask layer material to expose the top surface of the dielectric layer 310, and forming a first hard mask layer 313 on the top surface of the gate structure 312.
[0093] In this embodiment, the process of forming the first hard mask layer 313 is a chemical vapor deposition process; in other embodiments, the process of forming the first hard mask layer 313 may also be a physical vapor deposition process or an atomic layer deposition process.
[0094] Please refer to Fig.13 , a first interlayer dielectric layer 314 is formed on the substrate 300 , and the first interlayer dielectric layer 314 covers the first hard mask layer 313 .
[0095] In this embodiment, a first dielectric layer 314 is formed on the first hard mask layer 313 , the dielectric layer 310 , and the top surface of the spacer 308 .
[0096] The material of the first interlayer dielectric layer 314 is a material with a dielectric constant less than 2.5.
[0097] In this embodiment, the material of the first interlayer dielectric layer 314 is silicon oxide; in other embodiments, the material of the first interlayer dielectric layer 314 may also be black diamond, carbon silicon oxyhydride (SiCOH), fluorine-doped silicon dioxide (FSG), boron-doped silicon dioxide (BSG), phosphorus-doped silicon dioxide (PSG), boron-phosphorus-doped silicon dioxide (BPSG), hydrogenated silsesquioxane or methyl silsesquioxane, etc.
[0098] In this embodiment, the process of forming the first interlayer dielectric layer 314 is a chemical vapor deposition process; in other embodiments, the process of forming the first interlayer dielectric layer 314 may also be a physical vapor deposition process or an atomic layer deposition process.
[0099] Please refer to Fig.14 , the first interlayer dielectric layer 314 is etched until the top surface of the source / drain doped layer 309 is exposed, thereby forming a first opening 315 .
[0100] In this embodiment, during the etching of the first interlayer dielectric layer 314 , the dielectric layer 310 on the source / drain doped layer 309 is also etched until the top surface of the source / drain doped layer 309 is exposed to form the first opening 315 .
[0101] In this embodiment, the first opening 315 provides space for subsequently forming a conductive layer and a second hard mask layer.
[0102] In this embodiment, the process of forming the first opening 315 is a wet etching process; in other embodiments, the first opening 315 may also be formed by a dry etching process.
[0103] In this embodiment, the etching rate of the first interlayer dielectric layer 314 is greater than the etching rate of the first hard mask layer 313, so the use of wet etching can avoid damaging the surface quality of the first hard mask layer 313 during the process of removing the first interlayer dielectric layer 314, thereby improving the quality of the finally formed semiconductor device.
[0104] Please refer to Fig.15 , a conductive layer 316 is formed in a portion of the first opening 315 , and a top surface of the conductive layer 316 is lower than a top surface of the first interlayer dielectric layer 314 .
[0105] In this embodiment, the top surface of the conductive layer 316 is lower than the top surface of the first hard mask layer 313 , in order to provide space for the subsequent formation of the second hard mask layer.
[0106] In this embodiment, the conductive layer 316 is made of metal, including copper, tungsten or aluminum.
[0107] In this embodiment, the process of forming the conductive layer 316 includes a physical vapor deposition process or an electroplating process.
[0108] In this embodiment, the conductive layer 316 is used to subsequently realize electrical connection between the source-drain doped layer 309 and the outside.
[0109] Please refer to Fig.16 , a second hard mask layer 317 is formed on the conductive layer 316, the second hard mask layer 317 fills the remaining first opening 315, the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, and the second hard mask layer 317 partially overlaps with the first hard mask layer 313.
[0110] In this embodiment, the top surface of the second hard mask layer 317 is 3nm to 10nm higher than the top surface of the first hard mask layer 313. When the height of the top surface of the second hard mask layer 317 is less than 3nm higher than the top surface of the first hard mask layer 313, the height of the second hard mask layer 317 formed at this time is too low and cannot play an isolation role; when the height of the top surface of the second hard mask layer 317 is greater than 10nm higher than the top surface of the first hard mask layer 313, the volume of the second hard mask layer 317 formed at this time is too large, resulting in a large resistance, which affects the performance of the semiconductor device finally formed.
[0111] In this embodiment, an angle θ between the sidewall of the second hard mask layer 317 and the sidewall of the gate structure 312 is 0° to 10°.
[0112] In this embodiment, the angle between the side wall of the second hard mask layer 317 and the side wall of the side wall 308 is 0°~10°. The angle between the side wall of the second hard mask layer 317 and the side wall of the side wall 308 is 0°~10°. In the process of forming the second hard mask layer 317, the second hard mask layer 317 will partially overlap with the first hard mask layer 313.
[0113] In this embodiment, the second hard mask layer 317 partially overlaps with the first hard mask layer 313 along the extension direction X of the fin 301 .
[0114] In this embodiment, the material of the second hard mask layer 317 is silicon carbide.
[0115] In other embodiments, the material of the second hard mask layer 317 may also be one or more combinations of materials such as silicon nitride (SiN), silicon oxynitride (SiON), silicon oxycarbide (SiOC), silicon carbonitride (SiCN), silicon oxycarbonitride (SiOCN), and silicon carbon boron nitride (SiCBN).
[0116] In this embodiment, the step of forming the second hard mask layer 317 includes: forming an initial second hard mask layer material (not shown in the figure) on the first interlayer dielectric layer 314 / on the conductive layer 316, planarizing the initial second hard mask layer material until the top surface of the first interlayer dielectric layer 314 is exposed, and forming the second hard mask layer 317 on the conductive layer 316.
[0117] In this embodiment, the formation process of the initial second hard mask layer material is a chemical vapor deposition process, and the specific process parameters include: the gases used include hydrogen, HCl gas, SiH2Cl2 and PH3, the flow rate of hydrogen is 2000sccm~20000sccm, the flow rate of HCl gas is 30sccm~150sccm, the flow rate of SiH2Cl2 is 50sccm~1000sccm, the flow rate of PH3 is 10sccm~2000sccm, the chamber pressure is 10torr~600torr, and the temperature is 650 degrees Celsius~850 degrees Celsius.
[0118] In this embodiment, the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, and the second hard mask layer 317 partially overlaps with the first hard mask layer 313 (i.e., at Fig.16 In the embodiment of the present invention, the first hard mask layer 317 is formed in the first hard mask layer 313, and the first interconnection layer 317 is located on the top of the gate structure 312 between the source-drain doping layer 309. The spacing between the first interconnection layer and the conductive layer 316 is increased, thereby avoiding the short circuit problem between the first interconnection layer and the conductive layer 316. In addition, since the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, and the second hard mask layer 317 partially overlaps with the first hard mask layer 313, the distance between the second interconnection layer located on the conductive layer 316 and the gate structure 312 is increased, and it is also ensured that there will be no short circuit problem between the second interconnection layer and the gate structure 312, thereby improving the electrical performance and stability of the finally formed semiconductor device.
[0119] Please refer to Fig.17 , a second interlayer dielectric layer 318 is formed on the first interlayer dielectric layer 314 and the second hard mask layer 317 .
[0120] In this embodiment, the material of the second interlayer dielectric layer 318 is the same as that of the first interlayer dielectric layer 314 .
[0121] In this embodiment, the material of the second interlayer dielectric layer 318 is silicon oxide; in other embodiments, the material of the second interlayer dielectric layer 318 may also be black diamond, carbon silicon oxyhydride (SiCOH), fluorine-doped silicon dioxide (FSG), boron-doped silicon dioxide (BSG), phosphorus-doped silicon dioxide (PSG), boron-phosphorus-doped silicon dioxide (BPSG), hydrogenated silsesquioxane or methyl silsesquioxane, etc.
[0122] Please refer to Figure 18 to Figure 19 , a portion of the second interlayer dielectric layer 318 is etched to form a second opening 319 in the second interlayer dielectric layer 318 , and the bottom of the second opening 319 exposes the top surface of the conductive layer 316 .
[0123] Fig.18 yes Fig.19 In the AA section, Fig.19 yes Fig.18 Top view of the .
[0124] In this embodiment, the process of forming the second opening 319 is a dry etching process; in other embodiments, the second opening 319 may also be formed by a wet etching process.
[0125] In this embodiment, during the etching of the second interlayer dielectric layer 318 , the second hard mask layer 317 is simultaneously etched away until the top surface of the conductive layer 316 is exposed.
[0126] In this embodiment, the purpose of forming the second opening 319 is to provide space for forming a second interconnection layer.
[0127] Please refer to Fig. 20 , a second interconnection layer 320 is formed in the second opening 319 .
[0128] Fig. 20 The viewing direction and Fig.18 The viewing direction is the same.
[0129] In this embodiment, the material of the second interconnect layer 320 is metal, including aluminum, copper, nickel, etc.
[0130] In this embodiment, the second interconnection layer 320 is used to connect different devices together to form a circuit, and can also transmit external electrical signals to different parts inside the semiconductor device, thereby forming a semiconductor device with certain functions.
[0131] In this embodiment, the process for forming the second interconnection layer 320 is an electroplating process, because the electroplating process can form the second interconnection layer 320 with good density and high uniformity.
[0132] In this embodiment, since the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, and the second hard mask layer 317 partially overlaps with the first hard mask layer 313, the distance (D) between the second interconnect layer 320 and the gate structure 312 is increased, ensuring that there will be no short circuit problem between the second interconnect layer 320 and the gate structure 312, thereby improving the electrical performance and stability of the semiconductor device finally formed.
[0133] Please refer to Figure 21 to Figure 22 , the first hard mask layer 313 between the source and drain doping layers 309 is etched until the top surface of the gate structure 312 is exposed to form a third opening, and a first interconnection layer 321 is formed in the third opening.
[0134] Fig.21 yes Fig. 22 In the AA section, Fig. 22 yes Fig.21 Top view of the .
[0135] In this embodiment, a portion of the second interlayer dielectric layer 318 and the first hard mask layer 313 between the source-drain doping layer 309 are etched to expose the top surface of the gate structure 312 to form a third opening, and a first interconnection layer 321 is formed in the third opening.
[0136] In this embodiment, a self-aligned etching process is adopted. Since the etching rate of the second dielectric layer 318 is greater than that of the first hard mask layer 313 and the sidewall spacer 308 , it is ensured that the sidewall spacer 308 is not damaged.
[0137] In this embodiment, the material of the first interconnect layer 321 is metal, including aluminum, copper, nickel, etc.
[0138] In this embodiment, the first interconnection layer 321 is used to connect different devices together to form a circuit, and can also transmit external electrical signals to different parts inside the semiconductor device, thereby forming a semiconductor device with certain functions.
[0139] In this embodiment, the process for forming the first interconnection layer 321 is an electroplating process, because the electroplating process can form the first interconnection layer 321 with good density and high uniformity.
[0140] In this embodiment, since the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, the second hard mask layer 317 partially overlaps with the first hard mask layer 313. At the same time, in the process of etching the second dielectric layer 318 to form the first interconnection layer 321, since the etching rate of the second dielectric layer 318 is greater than that of the first hard mask layer 313 and the side wall 308, it is ensured that the side wall 308 is not damaged, so that the distance (d) between the first interconnection layer 321 and the conductive layer 316 is increased, thereby avoiding the short circuit problem between the first interconnection layer 321 and the conductive layer 316, and improving the electrical performance of the formed semiconductor device.
[0141] In this embodiment, the second interlayer dielectric layer 318 and the first hard mask layer 313 between the source-drain doping layer 309 are etched until the top surface of the gate structure 312 is exposed to form a third opening, and a first interconnection layer 321 is formed in the third opening.
[0142] Correspondingly, the present invention also provides a semiconductor device, including: a substrate 300; a gate structure 312, located on the substrate 300; a source-drain doped layer 309, located in the substrate 300 on both sides of the gate structure 312; a conductive layer 316, located on the source-drain doped layer 309; a first hard mask layer 313, located on the top of the gate structure 312; a second hard mask layer 317, located on the top surface of the conductive layer 316, the top surface of the second hard mask layer 317 is higher than the top surface of the first hard mask layer 313, and the second hard mask layer 317 partially overlaps with the first hard mask layer 313.
[0143] In this embodiment, the first interconnect layer 321 is located in the first hard mask layer 313 and on the top of the gate structure 312 between the source and drain doping layers 309 .
[0144] In this embodiment, the second interconnect layer 320 is located in the second hard mask layer 317 and on top of the conductive layer 316 .
[0145] In this embodiment, on the one hand, the first interconnection layer 321 is formed in the first hard mask layer 313 and is located on the top of the gate structure 312 between the source and drain doping layers 309 to achieve electrical connection with the gate structure 312, which helps to reduce the size of the gate structure 312, thereby adapting to the manufacture of smaller semiconductor devices. On the other hand, the top surface of the first hard mask layer 313 located on the top of the gate structure 312 is lower than the top surface of the second hard mask layer 317 located on the top surface of the conductive layer 316, and the second hard mask layer 317 is connected to the first hard mask layer 313. The film layer 313 is partially overlapped, so that when the second interconnection layer 320 is formed on the top of the conductive layer 316, a safe distance is provided between the second interconnection layer 320 and the gate structure 312, thereby avoiding bridging and short circuit between the second interconnection layer 320 and the gate structure 312; at the same time, when the first interconnection layer 321 is formed on the gate structure 312, a safe distance is ensured between the first interconnection layer 321 and the conductive layer 316, thereby avoiding the short circuit problem between the first interconnection layer 321 and the conductive layer 316, thereby improving the electrical performance and stability of the formed semiconductor device.
[0146] The top surface of the second hard mask layer 317 is 3nm to 10nm higher than the top surface of the first hard mask layer 313; when the top surface of the second hard mask layer 317 is less than 3nm higher than the top surface of the first hard mask layer 313, the height of the second hard mask layer 317 formed at this time is too low and cannot play an isolation role; when the top surface of the second hard mask layer 317 is greater than 10nm higher than the top surface of the first hard mask layer 313, the volume of the second hard mask layer 317 formed at this time is too large, resulting in a large resistance, which affects the performance of the semiconductor device finally formed.
[0147] The angle between the side wall of the second mask layer 317 and the side wall of the gate structure 312 is 0°~10°, that is, the angle between the side wall of the second mask layer 317 and the side wall of the side wall 308 is 0°~10°, so that in the process of forming the second hard mask layer 317, the second hard mask layer 317 will partially overlap with the first hard mask layer 313.
[0148] The first interlayer dielectric layer 314 is also included and is located on the top of the first hard mask layer 313 . The etching rate of the first interlayer dielectric layer 314 is greater than the etching rate of the first hard mask layer 313 .
[0149] In this embodiment, the etching rate of the first interlayer dielectric layer 314 is greater than the etching rate of the first hard mask layer 313, so the use of wet etching can avoid damaging the surface quality of the first hard mask layer 313 during the process of removing the first interlayer dielectric layer 314, thereby improving the quality of the finally formed semiconductor device.
[0150] The structure further includes a second interlayer dielectric layer 318 located on top of the first interlayer dielectric layer 314 and the second hard mask layer 317 .
[0151] In this embodiment, the material of the second interlayer dielectric layer 318 is the same as that of the first interlayer dielectric layer 314 .
[0152] In this embodiment, the material of the second interlayer dielectric layer 318 is silicon oxide; in other embodiments, the material of the second interlayer dielectric layer 318 may also be black diamond, carbon silicon oxyhydride (SiCOH), fluorine-doped silicon dioxide (FSG), boron-doped silicon dioxide (BSG), phosphorus-doped silicon dioxide (PSG), boron-phosphorus-doped silicon dioxide (BPSG), hydrogenated silsesquioxane or methyl silsesquioxane, etc.
[0153] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A semiconductor device, characterized in that: include: substrate; A gate structure, located on the substrate; Source-drain doped layers, located in the substrate on both sides of the gate structure; A first opening, exposing a top surface of the source-drain doped layer; A conductive layer, located on the source-drain doped layer and in a portion of the first opening; A first hard mask layer, located on the top of the gate structure, wherein the top surface of the conductive layer is lower than the top surface of the first hard mask layer; A second hard mask layer is located on the top surface of the conductive layer and fills the remaining first opening. The top surface of the second hard mask layer is higher than the top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer.
2. The semiconductor device according to claim 1, wherein A top surface of the second hard mask layer is 3 nm to 10 nm higher than a top surface of the first hard mask layer.
3. The semiconductor device according to claim 1, wherein The angle between the sidewall of the second hard mask layer and the sidewall of the gate structure is 0° to 10°.
4. The semiconductor device according to claim 1, wherein Also includes: The first interconnection layer is located in the first hard mask layer and on the top of the gate structure between the source and drain doping layers.
5. The semiconductor device according to claim 1, wherein: Also includes: The second interconnect layer is located in the second hard mask layer and on top of the conductive layer.
6. The semiconductor device according to claim 1, wherein The method further comprises a first interlayer dielectric layer located on top of the first hard mask layer, wherein an etching rate of the first interlayer dielectric layer is greater than an etching rate of the first hard mask layer.
7. The semiconductor device according to claim 6, wherein: The invention also includes a second interlayer dielectric layer located on top of the first interlayer dielectric layer and the second hard mask layer.
8. A method for forming a semiconductor device, characterized in that: include: Providing a substrate, wherein the substrate has a gate structure and source-drain doping layers in the substrate located on both sides of the gate structure; forming a first hard mask layer on a top surface of the gate structure; forming a first interlayer dielectric layer on the substrate, wherein the first interlayer dielectric layer covers the first hard mask layer; Etching the first interlayer dielectric layer until the top surface of the source / drain doped layer is exposed to form a first opening; forming a conductive layer in a portion of the first opening, wherein a top surface of the conductive layer is lower than a top surface of the first interlayer dielectric layer; A second hard mask layer is formed on the conductive layer, the second hard mask layer fills the remaining first opening, a top surface of the second hard mask layer is higher than a top surface of the first hard mask layer, and the second hard mask layer partially overlaps with the first hard mask layer.
9. The method for forming a semiconductor device according to claim 8, wherein: A top surface of the second hard mask layer is 3 nm to 10 nm higher than a top surface of the first hard mask layer.
10. The method for forming a semiconductor device according to claim 8, wherein: The angle between the sidewall of the second hard mask layer and the sidewall of the gate structure is 0° to 10°.
11. The method for forming a semiconductor device according to claim 8, wherein: Also includes: etching a portion of the second hard mask layer to form a second opening in the second hard mask layer, wherein a bottom of the second opening exposes a top surface of the conductive layer; forming a second interconnect layer in the second opening; The first hard mask layer between the source and drain doping layers is etched until the top surface of the gate structure is exposed to form a third opening, and a first interconnection layer is formed in the third opening.