IGBT wafer processing technology with back-bonded glass substrate

By performing gentle slope treatment and polyimide coating on the backside of the IGBT wafer, combined with glass carrier bonding and subsequent removal, the problem of fragmentation caused by high temperatures in the backside process and the backside tempering temperature limit are solved, achieving stress buffering and The stability of the metal coating ensures the integrity and cutting accuracy of the wafer.

CN114093815BActive Publication Date: 2024-10-18SHAOXING TONGXINCHENG INTEGRATED CIRCUIT CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202111341009.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-12
Publication Date
2024-10-18
Estimated Expiration
2041-11-12

AI Technical Summary

Technical Problem

In the current high-temperature step of the backside process of the existing IGBT wafer production process, the adhesive cannot withstand the high temperature, causing the wafer to be easily broken or damaged, and the backside tempering temperature is strictly limited, making it difficult to achieve effective edge processing and metal coating applications.

Method used

The back side of the wafer is treated with a gentle slope and coated with polyimide to provide stress support and buffering to overcome the back tempering temperature limit. The glass carrier is bonded to buffer the stress in the front metal thick film and electroplating process. After debonding Remove polyimide to prevent warping and damage.

Benefits of technology

It effectively avoids fragments and edge cracks during backside processing, overcomes backside tempering temperature limitations, ensures that thin wafers are not warped and damaged after thick metal coating, and improves scribe line alignment and metal layer cutting accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114093815B_ABST
    Figure CN114093815B_ABST
Patent Text Reader

Abstract

The present invention discloses an IGBT wafer processing technology with a back-bonded glass carrier, comprising the following steps: S1, completing the process before the metal process on the front side of the wafer; S2, etching the back side of the wafer to form a gentle slope; S3, completing the back side process of the wafer; S4, coating polyimide on the back side and bonding the glass carrier; S5, making the front side metal process; S6, coating polyimide on the front side, exposing the cutting path after developing, curing and etching; S7, completing cutting by etching and laser, and removing the polyimide on the front side; S8, attaching to the cutting mold frame, debonding and removing the glass carrier, and removing the adhesive; S9, removing the back side polyimide to separate the grains. The present invention makes a gentle slope treatment on the back side of the wafer to provide stress support at the edge, overcomes the limitation of the back side tempering temperature, and at the same time, the back side of the wafer of the present invention is coated with polyimide and bonded with the glass carrier, which can buffer the stress of the metal thick film and ensure that the thin wafer will not be warped and damaged after the thick metal coating.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of semiconductor processing, and in particular to an IGBT wafer processing technology with a back-bonded glass carrier. Background Art

[0002] IGBT is a composite fully controlled voltage-driven power semiconductor device composed of BJT (bipolar transistor) and MOS (insulated gate field effect transistor). It has the advantages of high input impedance of MOSFET (metal-oxide semiconductor field effect transistor) and low conduction voltage drop of GTR (power transistor). GTR has low saturation voltage drop and large current density, but large driving current; MOSFET has very low driving power and fast switching speed, but large conduction voltage drop and low current density. IGBT combines the advantages of the above two devices, with low driving power and low saturation voltage drop. It is very suitable for use in converter systems with DC voltage of 600V and above, such as AC motors, inverters, switching power supplies, lighting circuits, traction drives and other fields.

[0003] The current IGBT wafer production process is to complete the front side process of the wafer first, then bond the front side to a glass substrate, and then thin the back side and complete the subsequent wafer back side process. However, due to the high temperature steps involved in the back side process, the adhesive is a polymer material that can only withstand a maximum heating temperature of 350°C, and the metal process has been completed on the front side. AI or Cu can only withstand a maximum heating temperature of 560°C. Therefore, it cannot be implemented on wafers bonded to a glass substrate, but the wafer after debonding is prone to breakage and damage. Summary of the invention

[0004] In order to solve the deficiencies mentioned in the above-mentioned background technology, the purpose of the present invention is to provide an IGBT wafer processing technology with a back-bonded glass carrier. The present invention makes a gentle slope treatment on the back of the wafer to provide stress support at the edge after the wafer is thinned, so as not to cause breakage or local cracks on the edge, and overcomes the limitation of the back annealing temperature. At the same time, the back of the wafer of the present invention is coated with polyimide and then bonded to the glass carrier, which can buffer the stress generated by the front metal thick film and the electroplating and chemical plating processes. After debonding, the back polyimide is removed to ensure that the thin wafer will not warp or be damaged after the thick metal coating.

[0005] The purpose of the present invention can be achieved through the following technical solutions:

[0006] A back-bonded glass carrier IGBT wafer processing process comprises the following steps:

[0007] S1, complete the process before the metal process on the front side of the wafer;

[0008] S2, adhering a grinding tape to the front side of the wafer, and then forming a gentle slope or step-shaped wafer structure at the edge of the back side of the wafer, and removing the grinding tape;

[0009] S3, remove the grinding tape and complete the wafer backside process;

[0010] S4, coating polyimide on the gentle slope of the back side of the wafer to make the back side flat, and then bonding the back side of the wafer to the glass carrier;

[0011] S5, flipping the wafer to the front side and making the front side metal process;

[0012] S6, coating polyimide on the front side of the wafer, and exposing the cutting path after developing, curing, and etching;

[0013] S7, cutting the path to the back metal layer by plasma etching, cutting the back metal by laser, and then removing the polyimide on the front side;

[0014] S8, turning over the cut wafer so that the front side is attached to the first cutting mold frame, removing the glass carrier on the back side of the wafer by laser debonding, and removing the adhesive;

[0015] S9, removing the polyimide at the gentle slope of the back side by oxygen plasma;

[0016] S10, removing the surrounding gentle slope edges, and then attaching the back of the wafer to the second cutting mold frame, turning over the first cutting mold frame, the wafer and the second cutting mold frame as a whole, removing the stickiness of the first cutting film frame by ultraviolet light irradiation, and removing the first cutting mold frame.

[0017] Further preferably, the processes before the front metal process in step S1 include trench, ILD and contact hole processes.

[0018] Further preferably, in step S2, a gentle slope or stepped wafer structure is formed on the back edge of the wafer by grinding and edge air ring or protective liquid etching, and the wafer thickness after thinning is 40-150 um.

[0019] Further preferably, the back metal process in step S3 includes photolithography, ion implantation, tempering and back metal process.

[0020] Beneficial effects of the present invention:

[0021] The present invention performs gentle slope treatment on the back side of the wafer. Although it is an ultra-thin wafer, the edge can still contact the contact point or edge of the mechanical transmission arm of the heating and metal-related process equipment, so as not to cause fragments or local cracks on the edge, and at the same time overcome the limitation of the back side tempering temperature; the present invention coats polyimide on the back side of the wafer and then bonds it to the glass carrier, which can buffer the stress generated by the front side metal thick film and electroplating and chemical plating processes, and removes the back side polyimide after debonding to ensure that the thin wafer will not be warped and damaged after the thick metal coating; the present invention coats polyimide on the front side, then develops, cures, and etches to expose the cutting path, which can be automatically aligned on the front side, etches the cutting path first, and then laser cuts off the back side metal, which overcomes the problem of difficult alignment in traditional wafer back side cutting. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The present invention will be further described below in conjunction with the accompanying drawings.

[0023] Figure 1 It is a schematic diagram of the molding process step S1 of the present invention;

[0024] Figure 2 It is a schematic diagram of the molding process step S2 of the present invention;

[0025] Figure 3 It is a schematic diagram of the molding process step S3 of the present invention;

[0026] Figure 4 It is a schematic diagram of the molding process step S4 of the present invention;

[0027] Figure 5 It is a schematic diagram of the molding process step S5 of the present invention;

[0028] Figure 6 It is a schematic diagram of the molding process step S6 of the present invention;

[0029] Figure 7 It is a schematic diagram of the molding process step S7 of the present invention;

[0030] Figure 8 It is a schematic diagram of the molding process step S8 of the present invention;

[0031] Fig. 9 It is a schematic diagram of the molding process step S9 of the present invention;

[0032] Fig.10 It is a forming schematic diagram of the process step S10 of the present invention. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] like Figure 1-10 As shown, a back-side bonded glass carrier IGBT wafer processing process includes the following steps:

[0035] S1. Complete the process before the metal process on the front side of the wafer, including trench, ILD and contact hole processes;

[0036] S2, adhere the grinding tape to the front side of the wafer, and then use grinding and edge air ring or protective liquid etching to form a gentle slope or step-shaped wafer structure on the back edge of the wafer. The wafer thickness after thinning is 40-150um;

[0037] S3, remove the grinding tape and complete the wafer backside process, including photolithography, ion implantation, tempering and backside metal process;

[0038] S4, coating polyimide on the gentle slope of the back side of the wafer to make the back side flat, and then bonding the back side of the wafer to the glass carrier;

[0039] S5, flipping the wafer to the front side and making the front side metal process;

[0040] S6, coating polyimide on the front side of the wafer, and exposing the cutting path after developing, curing, and etching;

[0041] S7, cutting the path to the back metal layer by plasma etching, cutting the back metal by laser, and then removing the polyimide on the front side;

[0042] S8, turning over the cut wafer so that the front side is attached to the first cutting mold frame, removing the glass carrier on the back side of the wafer by laser debonding, and removing the adhesive;

[0043] S9, removing the polyimide at the gentle slope of the back side by oxygen plasma;

[0044] S10, removing the surrounding gentle slope edges, and then attaching the back of the wafer to the second cutting mold frame, turning over the first cutting mold frame, the wafer and the second cutting mold frame as a whole, removing the stickiness of the first cutting film frame by ultraviolet light irradiation, and removing the first cutting mold frame.

[0045] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0046] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, and these changes and improvements all fall within the scope of the present invention to be protected.

Claims

1. A back-bonded glass carrier IGBT wafer processing process, characterized in that: The following steps are involved: S1, complete the process before the metal process on the front side of the wafer; S2, sticking a grinding tape on the front side of the wafer, and then etching the back side of the wafer to form a gently sloped wafer structure at the edge; S3, remove the grinding tape and complete the wafer backside process; S4, coating polyimide on the gentle slope of the back side of the wafer to make the back side flat, and then bonding the back side of the wafer to the glass carrier; S5, flipping the wafer to the front side and making the front side metal process; S6, coating polyimide on the front side of the wafer, and exposing the cutting path after developing, curing, and etching; S7, cutting the path to the back metal layer by plasma etching, then cutting the back metal by laser, and then removing the polyimide on the front side; S8, turning over the cut wafer so that the front side is attached to the first cutting mold frame, removing the glass carrier on the back side of the wafer by laser debonding, and removing the adhesive; S9, removing the polyimide at the gentle slope of the back side by oxygen plasma; S10, removing the surrounding gentle slope edges, and then attaching the back of the wafer to the second cutting mold frame, turning over the first cutting mold frame, the wafer and the second cutting mold frame as a whole, removing the stickiness of the first cutting film frame by ultraviolet light irradiation, and removing the first cutting mold frame.

2. The IGBT wafer processing process with back-bonded glass carrier according to claim 1, characterized in that: The processes before the front metal process include trench, ILD and contact hole processes.

3. The IGBT wafer processing process with back-side bonding glass carrier according to claim 1, characterized in that: In the step S2, a gently sloped wafer structure is formed at the back edge of the wafer by means of grinding and edge air ring or protective liquid etching, and the wafer thickness after thinning is 40-150 um.

4. The IGBT wafer processing process with back-bonded glass carrier according to claim 1, characterized in that: The backside metal process includes photolithography, ion implantation, annealing and backside metal process.

Citation Information

Patent Citations

  • Susceptor and epitaxial growth device

    CN107851561A

  • Process for electroplating copper thick films on two sides of ultrathin wafer

    CN111799178A