Semiconductor structure and method for manufacturing the same

By forming multi-layer structures and trenches on the semiconductor substrate, filling the word line structure and setting the source and drain electrodes, the problem of DRAM substrate leakage current is solved and the reliability of the semiconductor structure is improved.

CN114093818BActive Publication Date: 2024-10-25CHANGXIN MEMORY TECH INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202010855256.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-24
Publication Date
2024-10-25
Estimated Expiration
2040-08-24

Smart Images

  • Figure CN114093818B_ABST
    Figure CN114093818B_ABST
Patent Text Reader

Abstract

The present invention provides a semiconductor structure and a preparation method thereof, the preparation method comprising the following steps: providing a semiconductor substrate; forming a groove in the semiconductor substrate; forming a first insulating layer, the first insulating layer at least covering the inner wall of the groove; forming a channel layer, the channel layer at least covering the inner wall of the first insulating layer; forming a second insulating layer, the second insulating layer at least covering the inner wall of the channel layer; filling a word line structure in the groove; removing part of the semiconductor substrate, part of the first insulating layer and part of the channel layer, forming a recessed area on the outer wall of the second insulating layer; forming a source and drain in the recessed area, the source and drain being electrically connected to the channel layer. The advantage of the present invention is that the first insulating layer is used to isolate the channel layer from the semiconductor substrate, thereby avoiding the generation of substrate leakage current and improving the reliability of the semiconductor structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a preparation method thereof. Background Art

[0002] Dynamic Random Access Memory (DRAM) is a semiconductor device commonly used in electronic devices such as computers. It consists of a memory cell array for storing data and a peripheral circuit located outside the memory cell array. Each memory cell usually includes a transistor and a capacitor. The word line voltage on the transistor can control the opening and closing of the transistor, thereby reading the data information stored in the capacitor through the bit line, or writing the data information into the capacitor.

[0003] With the continuous development of process technology, the size of transistors is getting smaller, while the channel electric field strength of transistors is getting stronger. As the process node of DRAM reaches 20nm and below, the substrate leakage current problem of transistors is getting more and more serious, which will lead to reliability problems of devices. For example, device snapback breakdown, latch-up effect of CMOS circuits and reduction of device life.

[0004] Therefore, how to avoid substrate leakage current has become a problem that needs to be solved urgently. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a semiconductor structure and a preparation method thereof, which can avoid substrate leakage current and improve the reliability of the semiconductor structure.

[0006] In order to solve the above problems, the present invention provides a method for preparing a semiconductor structure, which includes the following steps: providing a semiconductor substrate; forming a groove on the semiconductor substrate; forming a first insulating layer, wherein the first insulating layer at least covers the inner wall of the groove; forming a channel layer, wherein the channel layer at least covers the inner wall of the first insulating layer; forming a second insulating layer, wherein the second insulating layer at least covers the inner wall of the channel layer; filling a word line structure in the groove; removing part of the semiconductor substrate, part of the first insulating layer and part of the channel layer, and forming a recessed area on the outer wall of the second insulating layer; forming a source and a drain in the recessed area, wherein the source and the drain are electrically connected to the channel layer.

[0007] Furthermore, the semiconductor substrate has a plurality of independent active regions, the active regions are isolated by shallow trench isolation structures, and the trenches are formed in the active regions.

[0008] Furthermore, the word line structure includes a conductive structure and a third insulating layer located on the conductive structure, and the conductive structure includes a barrier layer and a first conductive layer.

[0009] Furthermore, the step of forming the channel layer further includes: forming a semiconductor layer at least on the inner wall of the first insulating layer; and doping the semiconductor layer to form the channel layer.

[0010] Furthermore, the method for doping the semiconductor layer is to dope the semiconductor layer using an ion implantation process.

[0011] Furthermore, the first insulating layer also covers the area above the semiconductor substrate, the channel layer also covers the surface of the first insulating layer located above the semiconductor substrate, and the second insulating layer also covers the surface of the channel layer located above the semiconductor substrate. The step of filling the word line structure in the groove further includes the following steps: forming the barrier layer on the surface of the second insulating layer, and the barrier layer also covers the surface of the second insulating layer above the semiconductor substrate; forming a first conductive layer on the surface of the barrier layer, and the first conductive layer fills the groove; etching back the first conductive layer and the barrier layer so that the top surfaces of the first conductive layer and the barrier layer are lower than the top surface of the semiconductor substrate, and removing the film layer above the semiconductor substrate, using the first insulating layer as an etching stop layer; forming the third insulating layer, and the third insulating layer fills the groove and covers the area above the semiconductor substrate; removing the film layer above the semiconductor substrate, using the semiconductor substrate as an etching stop layer.

[0012] Furthermore, the first insulating layer and the third insulating layer are made of different materials.

[0013] Furthermore, the step of forming source and drain electrodes in the recessed area further includes: depositing a second conductive layer, the second conductive layer filling the recessed area and covering the surface of the semiconductor substrate; etching the second conductive layer and stopping at the third insulating layer to form the source and drain electrodes.

[0014] Furthermore, the step of depositing a second conductive layer further includes the following steps: depositing a semiconductor layer, the semiconductor layer filling the recessed area and covering the surface of the semiconductor substrate; and performing plasma implantation or ion doping on the semiconductor layer to enhance the conductivity of the semiconductor layer.

[0015] The present invention also provides a semiconductor structure, which includes: a semiconductor substrate having a groove; a first insulating layer covering the inner wall of the groove; a channel layer covering the inner wall of the first insulating layer; a second insulating layer covering the inner wall of the channel layer; a word line structure filled in the groove; and a source and drain arranged on the outer wall of the second insulating layer and electrically connected to the channel layer.

[0016] Furthermore, the semiconductor substrate has a plurality of independent active regions, the active regions are isolated by shallow trench isolation structures, and the trenches are formed in the active regions.

[0017] Furthermore, the depth of the groove is 50-300 nm, and the width of the groove is 20-100 nm.

[0018] Furthermore, the thickness of the first insulating layer is 1-30 nm.

[0019] Furthermore, the thickness of the channel layer is 3-30 nm.

[0020] Furthermore, a top surface of the first insulating layer is lower than a top surface of the channel layer, and a top surface of the channel layer is lower than a top surface of the second insulating layer.

[0021] Furthermore, the upper surface of the source and drain is flush with the upper surface of the word line structure.

[0022] Furthermore, the upper surface of the source and drain is flush with the upper surface of the shallow trench isolation structure.

[0023] The advantage of the present invention is that the first insulating layer is used to isolate the channel layer from the semiconductor substrate, thereby avoiding the generation of substrate leakage current and improving the reliability of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 is a schematic diagram of steps of an embodiment of a method for preparing a semiconductor structure of the present invention;

[0025] Figure 2 to Figure 14 It is a process flow chart of an embodiment of a method for preparing a semiconductor structure of the present invention. DETAILED DESCRIPTION

[0026] The specific implementation manner of the semiconductor structure and the preparation method thereof provided by the present invention is described in detail below with reference to the accompanying drawings.

[0027] Figure 1 FIG. 1 is a schematic diagram of the steps of an embodiment of a method for preparing a semiconductor structure of the present invention. Figure 1 The preparation method of the semiconductor structure includes the following steps: providing a semiconductor substrate; forming a groove in the semiconductor substrate; forming a first insulating layer, wherein the first insulating layer at least covers the inner wall of the groove; forming a channel layer, wherein the channel layer at least covers the inner wall of the first insulating layer; forming a second insulating layer, wherein the second insulating layer at least covers the inner wall of the channel layer; filling a word line structure in the groove; removing part of the semiconductor substrate, part of the first insulating layer and part of the channel layer, and forming a recessed area on the outer wall of the second insulating layer; forming a source and a drain in the recessed area, wherein the source and the drain are electrically connected to the channel layer.

[0028] Figure 2 to Figure 14 It is a process flow chart of an embodiment of a method for preparing a semiconductor structure of the present invention.

[0029] See also Figure 2 , provide a semiconductor substrate 200. The semiconductor substrate 200 may be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP or other III / V compound semiconductors, including a multilayer structure of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI). As an example, in this embodiment, the constituent material of the semiconductor substrate 200 is selected from single crystal silicon.

[0030] Furthermore, in this embodiment, the semiconductor substrate 200 has a plurality of independent active regions 201, and the active regions 201 are isolated by shallow trench isolation structures 202. The material of the shallow trench isolation structure may be an insulating material such as oxide.

[0031] See also Figure 3 , a trench 210 is formed in the semiconductor substrate 200 .

[0032] In this embodiment, the trench 210 is formed in the active region 201. Figure 3 As shown, two trenches 210 are formed in one of the active regions 201 .

[0033] The method for forming the groove may be to form a patterned hard mask layer 300 on the semiconductor substrate 200; and to transfer the pattern of the hard mask layer 300 to the semiconductor substrate 200 by photolithography and etching processes to form the groove 210. The depth of the groove 210 may be 50 to 300 nm, and the width may be 20 to 100 nm, so as to provide sufficient space for the structure formed in the subsequent process. After this step, the hard mask layer is not removed, so as to protect the semiconductor substrate 200 in the subsequent process.

[0034] See also Figure 4, forming a first insulating layer 220, the first insulating layer 220 at least covers the inner wall of the groove 210. Among them, the first insulating layer 220 can be formed by an atomic layer deposition (ALD) process. The first insulating layer 220 formed by this process has a dense structure and a strong blocking effect. In this embodiment, the first insulating layer 220 is a nitride, such as silicon nitride. In other embodiments of the present invention, the first insulating layer 220 can also be other insulating materials, such as oxides. The thickness of the first insulating layer 220 ranges from 1 to 30 nm, so that it can not only effectively block leakage current, but also avoid occupying too much space in the active area 202, thereby affecting the performance of the semiconductor device.

[0035] Furthermore, the first insulating layer 220 not only covers the inner wall of the trench 210, but also covers the surface of the semiconductor substrate 200. Specifically, in this embodiment, since the surface of the semiconductor substrate 200 has a hard mask layer 300, the first insulating layer 220 not only covers the inner wall of the trench 210, but also covers the hard mask layer 300 on the surface of the semiconductor substrate 200.

[0036] See also Figure 5 , forming a channel layer 230, the channel layer 230 at least covers the inner wall of the first insulating layer 220. Further, the channel layer 230 not only covers the inner wall of the first insulating layer 220, but also covers the upper surface of the first insulating layer 220 above the semiconductor substrate 200.

[0037] The method of forming the channel layer 230 is:

[0038] A semiconductor layer is formed at least on the inner wall of the first insulating layer 220. In one embodiment, the semiconductor layer not only covers the inner wall of the first insulating layer 220, but also covers the upper surface of the first insulating layer 220 above the semiconductor substrate 200. The semiconductor layer can be formed by low pressure chemical vapor deposition (LPCVD) or by low pressure chemical vapor deposition and epitaxial process. The semiconductor layer includes but is not limited to silicon, germanium and other structural layers.

[0039] The semiconductor layer is doped to form the channel layer 230. The method of doping the semiconductor layer is to dope the semiconductor layer using an ion implantation process. Specifically, in this embodiment, the semiconductor layer is doped with boron (B) using an ion implantation process to form the channel layer 230.

[0040] Furthermore, after the channel layer 230 is formed, a rapid thermal process (RTP) is performed on the channel layer 230 to repair lattice damage of the channel layer 230 , increase carrier mobility of the channel layer 230 , and ensure the performance of the semiconductor device.

[0041] Furthermore, the thickness of the channel layer 230 is 3-30 nm, so that the channel layer 230 can meet the requirements of semiconductor devices while avoiding occupying the active area space and affecting the formation of subsequent word line structures.

[0042] See also Figure 6 , forming a second insulating layer 240, the second insulating layer 240 at least covers the inner wall of the channel layer 230. The second insulating layer 240 serves as an insulating layer between the subsequent word line structure and the channel layer. The thickness of the second insulating layer 240 can be 15 to 40 angstroms. If it is too thin, it will not play the role of insulating between the word line structure and the channel layer. If it is too thick, it will increase the threshold voltage of the semiconductor device and affect the performance of the semiconductor device.

[0043] The material of the second insulating layer 240 may be an oxide or a high-K dielectric material. For example, the oxide may be silicon oxide, and the high-K dielectric material may be HfO 2 , HfSiO, HfSiON, HfTaO, HfTiO, HfZrO, Al 2 O 3 ,La 2 O 3 、ZrO 2 , LaAlO or Ta 2 O 5 Furthermore, the material of the second insulating layer 240 is different from that of the first insulating layer 210, so that in the subsequent process, under the same etching conditions, the second insulating layer 240 and the first insulating layer 220 have different etching rates, thereby enabling selective etching.

[0044] Furthermore, in this embodiment, the second insulating layer 240 not only covers the inner wall of the channel layer 230 , but also covers the upper surface of the channel layer 230 above the semiconductor substrate 200 .

[0045] See also Figure 7 to Figure 11, a word line structure 250 is filled in the trench 210, and the word line structure 250 includes a conductive structure 251 and a third insulating layer 252 located on the conductive structure 251. The conductive structure 251 includes a barrier layer 251A and a first conductive layer 251B. The material of the third insulating layer 252 is different from that of the first insulating layer 220, so that in the subsequent etching process, under the same etching conditions, the third insulating layer 252 and the first insulating layer 220 have different etching rates, thereby enabling selective etching.

[0046] Specifically, in this embodiment, the method of filling the word line structure 250 in the trench 210 includes the following steps:

[0047] See also Figure 7 A barrier layer 251A is formed on the surface of the second insulating layer 240, and the barrier layer 251A also covers the upper surface of the second insulating layer 240 above the semiconductor substrate 200. The barrier layer 251A may be a TiN layer or a composite layer of Ti and TiN. The thickness of the barrier layer 251A may be 2-7 nm.

[0048] See also Figure 8 , a first conductive layer 251B is formed on the barrier layer 251A, the first conductive layer 251B fills the groove 210 and covers the upper surface of the barrier layer 251A above the semiconductor substrate 200. The first conductive layer 251B may be a metal tungsten layer. In this embodiment, the first conductive layer 251B is formed by chemical vapor deposition (CVD), and chemical mechanical polishing is performed to make the surface of the first conductive layer 251B flat. In other embodiments of the present invention, other deposition methods may be used to form the first conductive layer 251B, for example, physical vapor deposition (PVD).

[0049] See also Fig. 9 , the first conductive layer 251B and the barrier layer 251A are etched back by dry etching, so that the top surfaces of the first conductive layer 251B and the barrier layer 251A are lower than the top surface of the semiconductor substrate 200. After this step, a part of the trench 210 is filled with the conductive structure 251, and a part of the sidewall of the second insulating layer 240 is exposed. The distance from the upper surface of the first conductive layer 251B to the top surface of the semiconductor substrate 200 may be 20 to 150 nm.

[0050] Further, the film layer above the semiconductor substrate 200 is removed, and the first insulating layer 220 is used as an etching stop layer. Specifically, the first conductive layer 251B, the barrier layer 251A, the second insulating layer 240 and the channel layer 230 located above the semiconductor substrate 200 are removed, and the first insulating layer 220 is retained.

[0051] Furthermore, after dry etching, wet etching is performed to remove the barrier layer 251A remaining on the sidewall of the second insulating layer 240 .

[0052] See also Fig.10 , forming a third insulating layer 252, the third insulating layer 252 fills the trench 210 and covers the area above the semiconductor substrate 200. Specifically, in this embodiment, the third insulating layer 252 fills the trench 210 and covers the surface of the first insulating layer 220 located above the semiconductor substrate 200. The material of the third insulating layer 252 can be SiON.

[0053] See also Fig.11 , remove the film layer above the semiconductor substrate 200, and use the semiconductor substrate 200 as an etching stop layer. In this embodiment, dry etching is used to remove the third insulating layer 252, the first insulating layer 220 and the hard mask layer 300 above the semiconductor substrate 200 to expose the semiconductor substrate 200. After this step, the top surfaces of the first insulating layer 220, the channel layer 230, the second insulating layer 240 and the third insulating layer 252 are flush with the top surface of the semiconductor substrate 200.

[0054] See also Fig.12 , remove part of the semiconductor substrate 200, part of the first insulating layer 220 and part of the channel layer 230, and form a recessed area 260 on the outer wall of the second insulating layer 240. In this step, a dry etching process is used for etching. Among them, an etching material with a low etching rate for the third insulating layer 252 and the second insulating layer 240 can be selected to etch to avoid the removal of the third insulating layer 252 and the second insulating layer 240. In this embodiment, the etching rate of the etching material on the first insulating layer 220 is greater than the etching rate of the semiconductor substrate 200 and the channel layer 230, and the etching rate of the semiconductor substrate 200 and the channel layer 230 is greater than the etching rate of the second insulating layer 240 and the third insulating layer 252, thereby forming a recessed area 260 on the outer wall of the second insulating layer 240.

[0055] For example, in one embodiment, after forming the recessed area, the etching depth of the first insulating layer 220 is 10-80 nm, the etching depth of the semiconductor substrate 200 and the channel layer 230 is 5-60 nm, and the remaining thickness of the third insulating layer 252 is 50-80 nm.

[0056] See also Fig.13 and Fig.14, forming source and drain electrodes 270 in the recessed region 260, and the source and drain electrodes 270 are electrically connected to the channel layer 230. The source and drain electrodes 270 are made of a conductive material, which fills the recessed region 260. The material of the source and drain electrodes 270 includes but is not limited to polysilicon.

[0057] Furthermore, the method of forming the source and drain electrodes 270 in the recessed region 260 includes the following steps:

[0058] See also Fig.13 , depositing a semiconductor layer 400, the semiconductor layer 400 fills the recessed area 260 and covers the surface of the semiconductor substrate 200. The semiconductor layer 400 may be deposited by a chemical vapor deposition (CVD) process, and the material of the semiconductor layer 400 includes but is not limited to polysilicon, germanium, etc. In this embodiment, the material of the semiconductor layer 400 is polysilicon.

[0059] Furthermore, after the step of depositing the semiconductor layer 400, the semiconductor layer 400 is plasma implanted or ion doped to enhance the conductivity of the semiconductor layer 400 and form a second conductive layer. The plasma implantation may use one or more of P ions and As ions.

[0060] Furthermore, the second conductive layer may be subjected to annealing treatment to repair lattice damage and improve device performance.

[0061] Furthermore, after doping, the second conductive layer is planarized to make its surface flat. The planarization process may be chemical mechanical polishing (CMP).

[0062] See also Fig.14 , the second conductive layer is etched until the third insulating layer 252 is reached to form the source and drain electrodes 270 . In this step, only the second conductive layer in the recessed area 260 is retained as the source and drain electrodes 270 .

[0063] The semiconductor structure formed by the preparation method of the present invention uses the retained second conductive layer as the source and drain 270 of the transistor, the word line structure 250 as the gate of the transistor, and the second insulating layer 240 as the gate insulating layer. The first insulating layer 220 isolates the channel layer 230 from the semiconductor substrate 200, thereby avoiding the generation of substrate leakage current and improving the reliability of the semiconductor structure.

[0064] The present invention also provides a semiconductor structure prepared by the above method. Fig.14In one embodiment of the semiconductor structure of the present invention, the semiconductor structure includes a semiconductor substrate 200 , a first insulating layer 220 , a channel layer 230 , a second insulating layer 240 , a word line structure 250 and a source and drain 270 .

[0065] The semiconductor substrate 200 has a groove 210. In this embodiment, the semiconductor substrate 200 has a plurality of independent active regions 201, the active regions 201 are isolated by shallow trench isolation structures 202, and the grooves 210 are formed in the active regions 201. The depth of the grooves 210 is 50 to 300 nm, and the width is 20 to 100 nm, so as to provide sufficient space for the semiconductor structure formed in the grooves 210. The semiconductor substrate 200 includes a plurality of the grooves 210. For example, Fig.14 As shown, two trenches 210 are formed in one of the active regions 201 .

[0066] The first insulating layer 220 covers the inner wall of the trench 210. In this embodiment, the first insulating layer 220 is a nitride, such as silicon nitride. In other embodiments of the present invention, the first insulating layer 220 may also be other insulating materials, such as oxides. The thickness of the first insulating layer 220 is 1 to 30 nm, so that it can effectively block leakage current and avoid occupying too much space in the active area 202, thereby affecting the performance of the semiconductor device.

[0067] The channel layer 230 covers the inner wall of the first insulating layer 220. The channel layer 230 may be made of boron-doped silicon material. The thickness of the channel layer 230 is 3-30 nm, so that the channel layer 230 can meet the needs of semiconductor devices while avoiding occupying the active area space and affecting the formation of subsequent word line structures.

[0068] The second insulating layer 240 covers the inner wall of the channel layer 230. The second insulating layer 240 serves as an insulating layer between the word line structure 250 and the channel layer 230. The thickness of the second insulating layer 240 may be 15 to 40 angstroms. If it is too thin, it will not play the role of insulating between the word line structure and the channel layer. If it is too thick, it will increase the threshold voltage of the semiconductor device and affect the performance of the semiconductor device.

[0069] The material of the second insulating layer 240 may be an oxide or a high-K dielectric material. For example, the oxide may be silicon oxide, and the high-K dielectric material may be HfO 2 , HfSiO, HfSiON, HfTaO, HfTiO, HfZrO, Al 2 O 3 ,La 2 O 3 、ZrO 2, LaAlO or Ta 2 O 5 Furthermore, the material of the second insulating layer 240 is different from that of the first insulating layer 210, so that in the subsequent process, under the same etching conditions, the second insulating layer 240 and the first insulating layer 220 have different etching rates, thereby enabling selective etching.

[0070] The word line structure 250 is filled in the trench 210. The word line structure 250 includes a conductive structure 251 and a third insulating layer 252 located on the conductive structure 251. The conductive structure 251 includes a barrier layer 251A and a first conductive layer 251B. The barrier layer 251A may be a TiN layer or a composite layer of Ti and TiN. The thickness of the barrier layer 251A may be 2 to 7 nm. The first conductive layer 251B may be a metal tungsten layer. The top surfaces of the first conductive layer 251B and the barrier layer 251A are lower than the top surface of the semiconductor substrate 200. The distance from the first conductive layer 251B to the top surface of the semiconductor substrate 200 may be 20 to 150 nm.

[0071] The material of the third insulating layer 252 may be SiON. The material of the third insulating layer 252 is different from that of the first insulating layer 220, so that in the etching process, under the same etching conditions, the third insulating layer 252 and the first insulating layer 220 have different etching rates, thereby enabling selective etching.

[0072] The source and drain electrodes 270 are disposed on the outer sidewalls of the second insulating layer 240 and are electrically connected to the channel layer 230. The source and drain electrodes 270 are made of a conductive material, including but not limited to polysilicon.

[0073] Furthermore, the top surface of the first insulating layer 220 is lower than the top surface of the channel layer 230 to increase the contact area between the source and drain 270 and the channel layer 230. The top surface of the channel layer 230 is lower than the top surface of the second insulating layer 240 to prevent the word line structure 250 from contacting the channel layer 230.

[0074] The word line structure 250, the source and drain 270 and the channel layer 230 constitute a transistor, wherein the word line structure 250 serves as a gate of the transistor and the second insulating layer 240 serves as a gate insulating layer. The first insulating layer 220 isolates the channel layer 230 from the semiconductor substrate 200, thereby avoiding the generation of substrate leakage current and improving the reliability of the semiconductor structure.

[0075] The above is only a preferred embodiment of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for preparing a semiconductor structure, characterized in that: The steps include: providing a semiconductor substrate; forming a trench in the semiconductor substrate; forming a first insulating layer, wherein the first insulating layer at least covers the inner wall of the groove; forming a channel layer, wherein the channel layer at least covers an inner wall of the first insulating layer; forming a second insulating layer, wherein the second insulating layer at least covers an inner wall of the channel layer; filling a word line structure in the trench; Removing a portion of the semiconductor substrate, a portion of the first insulating layer and a portion of the channel layer to form a recessed area on an outer sidewall of the second insulating layer; A source and a drain are formed in the recessed area, and the source and the drain are electrically connected to the channel layer.

2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The semiconductor substrate has a plurality of independent active regions, the active regions are isolated by shallow trench isolation structures, and the trenches are formed in the active regions.

3. The method for preparing a semiconductor structure according to claim 1, characterized in that: The word line structure includes a conductive structure and a third insulating layer located on the conductive structure, wherein the conductive structure includes a barrier layer and a first conductive layer.

4. The method for preparing a semiconductor structure according to claim 1, characterized in that: The step of forming the channel layer further includes: forming a semiconductor layer at least on the inner wall of the first insulating layer; The semiconductor layer is doped to form the channel layer.

5. The method for preparing a semiconductor structure according to claim 4, characterized in that: The method for doping the semiconductor layer is to dope the semiconductor layer using an ion implantation process.

6. The method for preparing a semiconductor structure according to claim 3, characterized in that: The first insulating layer also covers the area above the semiconductor substrate, the channel layer also covers the surface of the first insulating layer above the semiconductor substrate, and the second insulating layer also covers the surface of the channel layer above the semiconductor substrate; The step of filling the word line structure in the trench further comprises the following steps: forming the barrier layer on the surface of the second insulating layer, wherein the barrier layer also covers the surface of the second insulating layer above the semiconductor substrate; Forming the first conductive layer on the surface of the barrier layer, and the first conductive layer fills the groove; etching back the first conductive layer and the barrier layer, so that the top surfaces of the first conductive layer and the barrier layer are lower than the top surface of the semiconductor substrate, removing the film layer above the semiconductor substrate, and using the first insulating layer as an etching stop layer; forming the third insulating layer, wherein the third insulating layer fills the trench and covers the area above the semiconductor substrate; The film layer above the semiconductor substrate is removed, and the semiconductor substrate is used as an etching stop layer.

7. The method for preparing a semiconductor structure according to claim 3, characterized in that: The first insulating layer and the third insulating layer are made of different materials.

8. The method for preparing a semiconductor structure according to claim 3, characterized in that: The step of forming a source and a drain in the recessed area further comprises: Depositing a second conductive layer, wherein the second conductive layer fills the recessed area and covers the surface of the semiconductor substrate; The second conductive layer is etched until the third insulating layer is reached to form the source and drain electrodes.

9. The method for preparing a semiconductor structure according to claim 8, characterized in that: The step of depositing a second conductive layer further comprises the following steps: Depositing a semiconductor layer, wherein the semiconductor layer fills the recessed area and covers the surface of the semiconductor substrate; Plasma implantation or ion doping is performed on the semiconductor layer to enhance the conductivity of the semiconductor layer.

10. A semiconductor structure, characterized in that: include: A semiconductor substrate having a trench; A first insulating layer covering the inner wall of the groove; A channel layer, covering an inner wall of the first insulating layer; a second insulating layer, covering an inner wall of the channel layer; A word line structure filled in the trench; A recessed area, wherein a portion of the semiconductor substrate, a portion of the first insulating layer and a portion of the channel layer are removed to form the recessed area on an outer sidewall of the second insulating layer; The source and drain electrodes are arranged in the recessed area and are electrically connected to the channel layer.

11. The semiconductor structure according to claim 10, characterized in that: The semiconductor substrate has a plurality of independent active regions, the active regions are isolated by shallow trench isolation structures, and the trenches are formed in the active regions.

12. The semiconductor structure according to claim 10, characterized in that The depth of the groove is 50-300 nm, and the width of the groove is 20-100 nm.

13. The semiconductor structure according to claim 10, characterized in that: The thickness of the first insulating layer is 1-30 nm.

14. The semiconductor structure according to claim 10, characterized in that The thickness of the channel layer is 3-30 nm.

15. The semiconductor structure according to claim 10, characterized in that A top surface of the first insulating layer is lower than a top surface of the channel layer, and a top surface of the channel layer is lower than a top surface of the second insulating layer.

16. The semiconductor structure according to claim 10, characterized in that The upper surface of the source and drain is flush with the upper surface of the word line structure.

17. The semiconductor structure according to claim 11, characterized in that The upper surface of the source and drain is flush with the upper surface of the shallow trench isolation structure.

Citation Information

Patent Citations

  • Semiconductor device

    CN109427789A

  • Memory transistor, word line structure of memory transistor and word line preparing method

    CN110610940A

  • Semiconductor storage device and manufacturing method thereof

    CN114597175A

  • Vertical double-channel silicon-on-insulator transistor and method of manufacturing the same

    US20050017289A1

  • Recessed-gate thin-film transistor with self-aligned lightly doped drain

    US20080057649A1