A method for detecting airtightness of semiconductor device
The dyeing solution of the upconverting material excitation by infrared light is detected in semiconductor devices, and the problem of inaccurate resolution of the penetration position and depth in the prior art is solved, and efficient and interference-free airtight detection is achieved, which significantly improves the detection accuracy and efficiency.
Patent Information
- Application Number
- CN202111368064.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-18
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2041-11-18
AI Technical Summary
The existing methods of airtight detection of semiconductor devices cannot effectively distinguish the penetration position and depth. Especially for fluorescent white LEDs, ultraviolet excitation will cause interference and the leakage position cannot be accurately judged.
The upconverting material dyeing solution excitated by infrared light is used for detection. The infrared excitation light source with a wavelength range of 700-1200nm is irradiated. The upconverting material is used to output green, yellow, blue and red light under infrared light, which clearly shows its existence area. Avoid interference, combine vacuum or high-pressure environment and circulation treatment to improve detection accuracy.
It realizes the interference-free resolution of the hollow position and depth of the semiconductor device, significantly improves the airtightness detection efficiency, and can more accurately reflect the sealing properties and moisture resistance of the device.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a method for detecting the air tightness of a semiconductor device. Background Art
[0002] At present, the detection of airtightness of semiconductor devices is extremely important.
[0003] CN103454049A discloses a method for detecting the sealing of LED packaging glue, the method comprising the following steps: (1) uniformly mixing glue A and glue B, removing bubbles, filling glue, and heating and curing; (2) soaking the cured lamp beads in red ink and boiling them, and then observing the dipping of the red ink under a microscope. The method has high precision and is simple to operate, and is suitable for detecting the sealing of LED packaging glue.
[0004] The red ink dyeing test method is commonly used to test the ability of plastic packaged microelectronic devices to resist moisture ingress and detect cracks in packaging materials for LEDs or non-sealed semiconductor devices. The dye in the red ink is an organic material with a large particle size. It often cannot penetrate into the tiny leakage channels on the device. Its inspection ability is limited and cannot well reflect the sealing and moisture resistance of the device. There are also existing technical solutions that use yellow phosphor as a dye to generate fluorescence through ultraviolet light excitation to judge the sealing of the device. However, for fluorescent white light LEDs, ultraviolet light will excite the phosphor in the device, making it impossible to distinguish the leakage location.
[0005] In summary, it is crucial to develop a method to efficiently, quickly and accurately detect the airtightness of semiconductor devices. Summary of the invention
[0006] In view of the deficiencies in the prior art, an object of the present invention is to provide a method for detecting the airtightness of a semiconductor device, which can conveniently and without interference distinguish the penetration position and penetration depth of the semiconductor device and has high airtightness detection efficiency.
[0007] To achieve this object, the present invention adopts the following technical solutions:
[0008] The present invention provides a method for detecting the airtightness of a semiconductor device, the method comprising the following steps:
[0009] The semiconductor device is placed in an upconversion material dye solution excited by infrared light, left to stand in a vacuum or high-pressure environment and then restored to normal pressure, and irradiated with an infrared excitation light source with a wavelength range of 700-1200nm (e.g. 800nm, 900nm, 1000nm, 1100nm, etc.) to complete the airtightness test of the semiconductor device.
[0010] The present invention adopts an up-conversion material excited by infrared light to form a dyeing solution to perform airtightness detection of semiconductor devices. The up-conversion material can realize green, yellow, blue and red light output under the excitation of infrared light, so as to clearly show the existence area of the up-conversion material in the semiconductor device, avoid the traditional ultraviolet light excitation of fluorescent powder in the white light LED device to emit fluorescence, thereby generating interference, and can conveniently and non-interferencely distinguish the location and depth of the cavity of the semiconductor device, and the airtightness detection efficiency is high.
[0011] Preferably, the particle size of the up-conversion material is 20 nm-5 μm, for example, 40 nm, 60 nm, 100 nm, 200 nm, 400 nm, 600 nm, 800 nm, 1 μm, 2 μm, 3 μm, 4 μm, etc.
[0012] The particle size of the up-conversion material of the present invention is within a relatively small range of 20 nm-5 μm. The up-conversion material can penetrate into tiny cavities of semiconductor devices, thereby better detecting the air tightness of the device.
[0013] Preferably, the up-conversion material comprises any one of rare earth ion-doped fluorides, rare earth ion-doped oxyfluorides, rare earth ion-doped oxyhalides, rare earth ion-doped oxides or rare earth ion-doped sulfides, or a combination of at least two thereof, wherein typical but non-limiting combinations include: a combination of rare earth ion-doped fluorides and rare earth ion-doped oxyfluorides, a combination of rare earth ion-doped oxides, rare earth ion-doped oxyfluorides and rare earth ion-doped sulfides, a combination of rare earth ion-doped oxyhalides, rare earth ion-doped fluorides, rare earth ion-doped oxyfluorides or rare earth ion-doped sulfides, etc.
[0014] Preferably, the ambient pressure of the vacuum or high-pressure environment is 20Pa-304KPa, for example, 500Pa, 1KPa, 50KPa, 100KPa, 200KPa, 300KPa, etc.
[0015] Preferably, the standing time is 5-120 min, for example, 10 min, 20 min, 40 min, 60 min, 80 min, 100 min, etc.
[0016] Preferably, the number of cycles of standing in a vacuum or high-pressure environment and then restoring to normal pressure is 1-20 times, for example, 4 times, 6 times, 8 times, 10 times, 15 times, 18 times, etc.
[0017] Preferably, the cycle is maintained for 10-60 minutes after completion, such as 20 minutes, 30 minutes, 40 minutes, 50 minutes, 60 minutes, etc.
[0018] Preferably, before determining the penetration depth of the infrared-excited up-conversion material dyeing solution in the semiconductor device, the step further includes drying the semiconductor device.
[0019] Preferably, the drying method is baking;
[0020] The baking temperature is 50-100°C, such as 60°C, 70°C, 80°C, 90°C, etc.;
[0021] The baking time is 0.5-1 h, such as 0.6 h, 0.7 h, 0.8 h, 0.9 h, etc.
[0022] Preferably, the temperature of the up-conversion material dyeing solution is 25-150°C, for example, 40°C, 60°C, 80°C, 100°C, 120°C, 140°C, etc.
[0023] Preferably, the infrared light detection object may be the surface of a device being directly irradiated, a cross section of a device, or a chip, packaging glue, or a bracket after the device is mechanically opened.
[0024] Preferably, the semiconductor device comprises a light emitting diode, such as a visible light LED or an ultraviolet UV LED.
[0025] Preferably, the semiconductor device includes a semiconductor power device, such as a diode, a triode, a transistor, a capacitor, an inductor, a rectifier, a MOS tube, a discrete device or a power device.
[0026] Preferably, the semiconductor device comprises a semiconductor device module, such as a display module or a sensor module.
[0027] Preferably, the infrared light detection device comprises a microscope with an adjustable magnification and an infrared light excitation light source lens.
[0028] Preferably, the infrared light detection device comprises a fluorescence spectrometer and an infrared light excitation light source to test the fluorescence emission peak of the upconversion material on the surface or inside of the test sample to determine whether the device has leakage.
[0029] Preferably, the detection method can be to observe the luminescence by infrared light excitation in a dark room and record it with a CCD digital camera with a thermal filter. In the present invention, the thermal filter is a filter that prevents infrared or near-infrared radiation from passing through.
[0030] As a preferred technical solution, the detection method comprises the following steps:
[0031] Step 1, placing the semiconductor device in a 25-250° C. upconversion material dyeing solution excited by infrared light;
[0032] Step 2, stand in a vacuum or high pressure environment with an ambient pressure of 20Pa-304 KPa for 5-120 minutes and then return to normal pressure, cycle 1-20 times, and maintain for 10-60 minutes;
[0033] Step 3: After drying the semiconductor device to be tested at 50-100° C. for 0.5-1 h, irradiate it with an infrared excitation light source with a wavelength range of 700-1200 nm to complete the airtightness test of the semiconductor device.
[0034] Compared with the prior art, the present invention has the following beneficial effects:
[0035] The detection method of the present invention can conveniently and without interference distinguish the location and depth of the cavity of the semiconductor device, and has high airtightness detection efficiency. DETAILED DESCRIPTION
[0036] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0037] Example 1
[0038] This embodiment provides a method for detecting the airtightness of a semiconductor device, the method comprising the following steps:
[0039] Step 1, placing the semiconductor device diode in an infrared excited up-conversion material (with a particle size of 800 nm, fluoride doped with rare earth ions, NaYF4) dyeing solution at a temperature of 125°C;
[0040] Step 2: Place the mixture in a vacuum environment at an ambient pressure of 80 Pa for 60 minutes and then return to normal pressure. After 10 cycles, maintain the mixture for 30 minutes.
[0041] Step 3: After drying the semiconductor device to be tested at 80° C. for 0.8 h, irradiate it with an infrared excitation light source with a wavelength range of 800 nm to determine the penetration depth of the infrared excited upconversion material dyeing solution in the semiconductor device, thereby completing the airtightness test of the semiconductor device.
[0042] Example 2
[0043] This embodiment provides a method for detecting the airtightness of a semiconductor device, the method comprising the following steps:
[0044] Step 1: Place the semiconductor device rectifier tube in an infrared-excited upconversion material (particle size 20nm, Er fluoride doped with rare earth ions) at a temperature of 25°C. 3+ :CaF) staining solution;
[0045] Step 2: Place the mixture in a high-pressure environment with an ambient pressure of 200 KPa for 5 minutes and then return to normal pressure. After 20 cycles, keep the mixture for 60 minutes.
[0046] Step 3: After the semiconductor device to be tested is dried at 50° C. for 1 hour, the penetration depth of the infrared-excited upconversion material dyeing solution in the semiconductor device is determined, and the airtightness test of the semiconductor device is completed by irradiating the semiconductor device with an infrared excitation light source with a wavelength range of 700 nm.
[0047] Example 3
[0048] This embodiment provides a method for detecting the airtightness of a semiconductor device, the method comprising the following steps:
[0049] Step 1: Place the semiconductor device UV LED in an up-conversion material (5 μm in particle size, sulfide doped with rare earth ions, Er) at a temperature of 150°C under infrared excitation. 3+ / Yb 3+ Co-doped Ga2S3:La2O3) dyeing solution;
[0050] Step 2: After standing for 120 minutes in a high-pressure environment with an ambient pressure of 500 Pa, return to normal pressure and maintain for 10 minutes;
[0051] Step 3: Dry the semiconductor device to be tested at 100°C for 0.5h, make a cross-section and take a cross-section photo under the irradiation of an infrared excitation light source with a wavelength range of 1200nm to determine the penetration depth of the infrared-excited upconversion material dyeing solution in the semiconductor device and complete the airtightness test of the semiconductor device.
[0052] Example 4
[0053] The difference between this embodiment and embodiment 1 is that the particle size of the up-conversion material is 6 μm, and the rest is the same as embodiment 1.
[0054] Comparative Example 1
[0055] The difference between this comparative example and Example 1 is that the infrared excited up-conversion material dyeing solution is replaced with red ink, and the rest is the same as Example 1.
[0056] Detection Summary
[0057] In Examples 1-3, the infrared light detection equipment includes a microscope with an infrared light excitation light source lens with adjustable magnification or a combination of an infrared light excitation light source and a fluorescence spectrometer. The fluorescence spectrometer tests the fluorescence emission peak of the upconversion material on the surface or inside the test sample to determine whether the device has leakage. The specific detection method includes: observing the luminescence with a microscope with an infrared light excitation light source lens with adjustable magnification in a dark room, and recording it with a CCD digital camera with a thermal filter, or irradiating the test sample with an infrared light excitation light source in a dark room, and using a fluorescence spectrometer to collect the fluorescence emission peak of the upconversion material, or using a fluorescence spectrometer with an infrared light excitation light source in a dark room to test the fluorescence emission peak of the upconversion material.
[0058] In Examples 1-3, the detection method can clearly distinguish the penetration position and penetration depth of the infrared excitation up-conversion material dye solution in the semiconductor device, thereby quickly completing the airtightness detection of the device.
[0059] In Example 4, relative to Example 1, it can be seen from the semiconductor device after inspection that there are still local tiny voids that have not been penetrated. This is because the particle size of the upconversion material is relatively large and cannot penetrate into the tiny voids of the device, proving that the upconversion material can achieve more accurate airtightness detection only within a smaller range.
[0060] In Comparative Example 1, compared with Example 1, it can be seen from the semiconductor device after inspection that there are still a large number of penetration channels that have not been penetrated by the red ink, and its inspection ability is limited, which cannot well reflect the sealing and moisture resistance of the device.
[0061] The present invention illustrates the detailed method of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed method, that is, it does not mean that the present invention must rely on the above-mentioned detailed method to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
Claims
1. A method for detecting the airtightness of a semiconductor device, characterized in that: The detection method comprises the following steps: The semiconductor device is placed in an up-conversion material dyeing solution at 25-150°C excited by infrared light, and then allowed to stand in a vacuum environment at an ambient pressure of 20Pa-100 KPa for 5-120 min and then restored to normal pressure, and after 1-20 cycles, maintained for 10-60 min, the semiconductor device to be tested is dried at 50-100°C for 0.5-1h, and then the surface of the semiconductor device is irradiated with an infrared excitation light source with a wavelength range of 700-1200 nm to achieve green, yellow, blue and red light output, distinguish the location and depth of the cavity in the semiconductor device, and complete the detection of the airtightness of the semiconductor device; the particle size of the up-conversion material is 20 nm-5 μm; The semiconductor device is a fluorescent white light LED device; The detection method adopts an infrared light detection device, and the infrared light detection device is a microscope with an adjustable magnification and an infrared light excitation light source lens.
2. The method for detecting the airtightness of a semiconductor device according to claim 1, characterized in that: The up-conversion material includes any one of fluorides doped with rare earth ions, fluorine oxides doped with rare earth ions, halides doped with rare earth ions, oxides doped with rare earth ions, or sulfides doped with rare earth ions, or a combination of at least two of these.
3. The method for detecting the airtightness of a semiconductor device according to claim 1, characterized in that: The drying method is baking.
Citation Information
Patent Citations
Method for detecting sealing performance of LED packing glue
CN103454049A
Multi-band fluorescent infrared up-conversion material based on sensitizer substrate
CN101225304A
Method for testing semiconductor device and method for manufacturing semiconductor device
CN111247409A
Infrared-to-visible up-conversion material, and infrared light identification elements comprising same
EP0569257A1
Method and apparatus for hermeticity determination and leak detection in semiconductor packaging