Method for manufacturing glass articles
By preforming thin-walled portions and thick-walled portions in the glass base material and extending them during the redraw forming process, the problem of poor handling properties of the glass plate is solved, the strength and dimensional accuracy of the glass items are improved, and breakage and dimensional accuracy are reduced. Risk of dirt adhesion.
Patent Information
- Application Number
- CN202080057743.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-30
- Filing Date
- 2020-06-04
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-06-04
AI Technical Summary
When using the redrawing method to manufacture miniaturized and thinned glass plates, there are problems with poor handling properties, including the problem that the thin-walled portion of the glass plate is easily damaged and dirt is difficult to clean.
By forming thin-walled portions and thick-walled portions in the width direction in the glass base material in advance, and extending them during the redraw forming process, a glass ribbon having a second thin-walled portion and a second thick-walled portion is formed, thereby improving the quality of the glass. The handling of items. The method includes forming a first thin-walled part and a first thick-walled part in a glass base material, and forming a second thin-walled part and a second thick-walled part by redrawing, ensuring that the supporting part is only in contact with the thick-walled part, Reduces the possibility of damage and dirt adhesion.
It improves the handleability of glass items, enhances their strength and surface quality, ensures that they are not prone to breakage and dirt adhesion during the manufacturing process, and the obtained glass items have excellent dimensional accuracy.
Smart Images

Figure CN114222719B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a glass article and a method for manufacturing the glass article. Background Art
[0002] As is well known, glass substrates for flat panel displays such as liquid crystal displays and organic EL displays are becoming larger and thinner, and therefore, the overflow down-draw method is widely used as a molding method thereof.
[0003] On the other hand, in glass sheets used for small devices, it is sometimes required to be thinner than glass substrates used for flat panel displays while being miniaturized. In this field, a redraw method is sometimes used as a method for forming a glass sheet (for example, Patent Document 1). The redraw method is a method of stretching a glass matrix while reheating it to form a very thin and long glass ribbon.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2015-44742 Summary of the invention
[0007] Problems to be solved by the invention
[0008] A glass plate obtained by miniaturization and thinning using the re-drawing method has a problem in that the handling properties in the device manufacturing process are poor.
[0009] That is, when the support part (such as a robot or a worker's finger) contacts a very thin wall portion of the glass plate, it may be easily damaged. In addition, there is also a problem that when dirt is attached to the thin wall portion of the glass plate due to contact with the support part, it is difficult to remove the dirt by cleaning.
[0010] An object of the present invention is to improve the handling properties of a glass article having a thin-walled portion.
[0011] Solutions to Solve Problems
[0012] The method for manufacturing a glass article of the present invention, which is made in order to solve the above-mentioned problems, is characterized in that the method for manufacturing a glass article comprises: a preparation step of preparing a glass mother material having a first thin-walled portion and a first thick-walled portion at different positions in a width direction; a forming step of extending the glass mother material downward while heating it using a re-drawing method to form a glass ribbon having a second thin-walled portion and a second thick-walled portion at different positions in the width direction; and an article forming step of obtaining a glass article from the glass ribbon.
[0013] In this way, the first thin-walled portion and the first thick-walled portion are formed in advance in the glass mother material, so the second thin-walled portion and the second thick-walled portion are reliably formed in the glass ribbon formed by the redrawing method. When a glass article (such as a glass plate, a glass roll, etc.) is obtained from the glass ribbon, the second thin-walled portion and the second thick-walled portion are also formed in the glass article. Therefore, since the second thick-walled portion having a larger thickness than the second thin-walled portion can be supported to handle the glass article, the handling property of the glass article becomes good.
[0014] In the above-mentioned structure, it is preferable that the glass base material has a first thin-walled portion in a center portion in a width direction and has first thick-walled portions at both ends in the width direction.
[0015] Thus, in the glass article obtained from the glass ribbon, the second thin-walled portion is formed in the middle portion in the width direction, and the second thick-walled portions are formed at both ends in the width direction. That is, the second thin-walled portion is sandwiched between the two second thick-walled portions, so that other components are less likely to contact the second thin-walled portion, and the handling of the glass article becomes better.
[0016] In the above-mentioned structure, it is preferable that, in the glass base material, on both surfaces in the thickness direction, the first thick portion protrudes more than the first thin portion.
[0017] Thus, in the glass article obtained from the glass ribbon, the second thick portion protrudes more than the second thin portion on both surfaces in the thickness direction, so that other members are less likely to come into contact with the second thin portion, and the glass article is more easily handled.
[0018] In the above-mentioned structure, it is preferable that the first thin-walled portion is formed by grinding or etching the glass base material.
[0019] In this way, the first thin-walled portion thinner than the first thick-walled portion can be easily and reliably formed in the glass mother material. In addition, since the processing accuracy and surface quality of the first thin-walled portion of the glass mother material are improved, the quality of the second thin-walled portion of the glass ribbon or glass article is also stable.
[0020] In the above-mentioned structure, in the article forming step, the glass ribbon is wound into a roll.
[0021] In this way, a glass roll in which the glass ribbon is wound in a roll shape is formed as a glass article.
[0022] In the above-described configuration, in the forming step, a stretching roller in contact with the glass ribbon is provided to stretch the glass base material, and the stretching roller is preferably in contact with only the second thick portion of the glass ribbon.
[0023] In this manner, since the stretching roller does not come into contact with the second thin-walled portion of the glass ribbon, it is difficult for the second thin-walled portion of the glass ribbon or the glass article to be damaged or contaminants to adhere thereto.
[0024] In the above-described configuration, preferably, in the forming step, a support portion for supporting the glass base material is provided, and the support portion is in contact with only the first thick portion of the glass base material.
[0025] Thus, the support portion does not contact the first thin-walled portion of the glass mother material, so it is difficult to damage or stain the first thin-walled portion of the glass mother material. In other words, it is difficult to damage or stain the second thin-walled portion of the glass ribbon or glass component obtained from the glass mother material.
[0026] In the above-mentioned structure, it is preferable that (the thickness of the first thick-walled portion) / (the thickness of the first thin-walled portion) is 1.1-25.
[0027] In this way, a glass article having excellent dimensional accuracy can be obtained stably.
[0028] In the above-mentioned structure, it is preferable that (full width of the glass base material) / (thickness of the first thick portion) is 25 to 4000.
[0029] In this way, a glass article having excellent dimensional accuracy can be obtained stably.
[0030] In the above-mentioned structure, it is preferable that (width of the first thick portion) / (width of the first thin portion) is 0.02 to 40,000.
[0031] In this way, a glass article having excellent dimensional accuracy can be obtained stably.
[0032] The glass article of the present invention, which is made to solve the above-mentioned problems, is characterized in that it has a thin-walled portion and a thick-walled portion at different positions in the width direction, the thickness of the thick-walled portion is at least 1.1 times the thickness of the thin-walled portion, and the surfaces of the thin-walled portion and the thick-walled portion are composed of forged surfaces.
[0033] In this way, the glass component can be handled by supporting the thick wall portion which is thicker than the thin wall portion, so the handling property of the glass article becomes good. In addition, if the surface of the thin wall portion and the thick wall portion is a forged surface, it is difficult to form defects (such as micro cracks) that cause breakage, and the corners formed on the surface in the process of forming the forged surface are rounded. Therefore, the strength of the glass article is improved.
[0034] In the above structure, preferably, the thin-walled portion is formed in the center portion in the width direction, and the thick-walled portions are formed in both ends in the width direction, and the surface of the thin-walled portion is composed of a flat surface and / or a concave curved surface.
[0035] Thus, thick-walled portions are formed on both sides of the thin-walled portion in the width direction, so that other components are more difficult to contact the thin-walled portion, and the handling property of the glass article becomes better. In addition, the surface of the thin-walled portion is configured as a flat surface and / or a concave curved surface, so it is also easy to ensure the strength of the thin-walled portion.
[0036] In the above-mentioned structure, it is preferable that the thick-walled portion protrudes more than the thin-walled portion on both surfaces in the thickness direction.
[0037] This makes it more difficult for other members to come into contact with the thin-walled portion, and the glass article can be handled more easily.
[0038] In the above-mentioned structure, it is preferable that (full width of the glass article) / (thickness of the thick wall portion) is 1.1-25.
[0039] In the above-mentioned structure, it is preferable that (width of the thick wall portion) / (width of the thin wall portion) is 0.02 to 40,000.
[0040] In the above-mentioned structure, preferably, the thickness of the thin-walled portion is 10 μm or less, and the full width of the glass article (maximum width of the glass article) is 0.5 to 40 mm.
[0041] In the above configuration, the glass article may be a glass roll obtained by winding a glass ribbon having a thick portion and a thin portion in a roll shape.
[0042] In the case of a glass roll, it is preferable that a protection sheet is interposed between glass ribbons facing each other in the radial direction, and the protection sheet is in contact with only the thick portion on at least one surface in the thickness direction of the glass ribbon.
[0043] In this manner, since at least one surface of the protection sheet in the thickness direction of the glass ribbon does not contact the thin-walled portion, it is possible to suppress the thin-walled portion from being scratched or contaminants from being attached due to contact with the protection sheet.
[0044] Effects of the Invention
[0045] According to the present invention, the handleability of a glass article having a thin-walled portion can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 This is a side view showing the method for producing the glass article according to the first embodiment.
[0047] Figure 2 It is shown Figure 1 Stereoscopic image of glass mother material.
[0048] Figure 3 It is shown Figure 1 Cross-sectional view of the glass mother material.
[0049] Figure 4 It is shown Figure 1 A cross-sectional view of a glass ribbon.
[0050] Figure 5 yes Figure 1 AA section view.
[0051] Figure 6 yes Figure 1 BB cross-sectional view.
[0052] Figure 7 yes Figure 1 CC cross-sectional view.
[0053] Figure 8 This is a side view showing a method for producing a glass article according to a second embodiment.
[0054] Fig. 9 It is a cross-sectional view showing a modified example of the glass base material.
[0055] Fig.10 It is a cross-sectional view showing a modified example of the glass base material.
[0056] Fig.11 It is a cross-sectional view showing a modified example of the glass base material.
[0057] Fig.12 It is a cross-sectional view showing a modified example of the glass base material.
[0058] Fig.13 It is a cross-sectional view showing a modified example of the glass base material.
[0059] Fig.14 It is a cross-sectional view showing a modified example of the glass base material. DETAILED DESCRIPTION
[0060] Hereinafter, the glass article and the manufacturing method thereof according to the embodiment of the present invention will be described with reference to the accompanying drawings. It should be noted that XYZ in the drawings is an orthogonal coordinate system. The X direction and the Y direction are horizontal directions, and the Z direction is a vertical direction.
[0061] (First Embodiment)
[0062] like Figure 1 to Figure 3 As shown, the manufacturing method of the glass article of the first embodiment includes: a preparation step (refer to Figure 2 as well as Figure 3 ), prepare glass matrix 1; forming process (refer to Figure 1 ), using a re-drawing method to extend the glass base material 1 downward while heating to form a glass ribbon 2; and an article forming step (refer to Figure 1 ), a glass roll 3 as a glass article is obtained from the glass ribbon 2.
[0063] like Figure 2 as well as Figure 3 As shown, in the preparation step, the glass base material 1 having the first thin-walled portion 1 a and the first thick-walled portion 1 b at different positions in the width direction (Y direction) is prepared.
[0064] Specifically, the glass base material 1 has a first thin portion 1a in the widthwise center and first thick portions 1b at both widthwise ends. In this embodiment, each of the first thin portion 1a and the first thick portion 1b has a planar portion with a constant thickness.
[0065] Furthermore, the first thick portion 1b protrudes more than the first thin portion 1a on both surfaces in the thickness direction (X direction) of the glass mother material 1. In other words, recesses 1c are formed on both surfaces in the thickness direction of the glass mother material 1 at positions corresponding to the first thin portion 1a.
[0066] It should be noted that, in the present embodiment, the cross section of the glass mother material 1 on the XY plane is line symmetric with respect to the thickness direction center line P passing through the center in the thickness direction and the width direction center line Q passing through the center in the width direction. Of course, the cross-sectional shape of the glass mother material 1 is not limited to the case of having such symmetry.
[0067] The first thin-walled portion 1a (recess 1c) is formed, for example, by grinding or etching the glass mother material 1 in the shape of a rectangular parallelepiped. In particular, in the case of etching, it is preferred to adopt the following method: using photolithography or the like, a mask is generated on the main surface of the glass mother material 1 in the shape of a rectangular parallelepiped before the first thin-walled portion 1a (recess 1c) is formed, and wet etching or dry etching is used to obtain the desired first thin-walled portion 1a. The glass mother material 1 in the shape of a rectangular parallelepiped before the first thin-walled portion 1a is formed can be formed, for example, by a down-drawing method such as an overflow down-drawing method, a slit down-drawing method, a re-drawing method, a float method, and the like. As the glass mother material 1, for example, alkali-free glass (for example, Type-D manufactured by Nippon Electric Glass Co., Ltd.) is used. It should be noted that the method for forming the first thin-walled portion 1a of the glass mother material 1 is not particularly limited, and other methods such as mold forming can also be used.
[0068] like Figure 1 As shown in the figure, in the forming process, the upper end of the glass mother material 1 is supported by the support part 4, and the glass mother material 1 is supplied to the inside of the heating furnace 5 while the support part 4 is lowered. Inside the heating furnace 5, the glass mother material 1 is heated by the heater 5a and softened. A pair of stretching rollers 6 are provided below the heating furnace 5 to contact both surfaces of the glass ribbon 2 continuous with the softened glass mother material 1. The softened glass mother material 1 is stretched by pulling the glass ribbon 2 downward by the pair of stretching rollers 6. Thus, a glass ribbon 2 with a relatively thin thickness is formed from the glass mother material 1.
[0069] like Figure 4As shown in FIG. 1 , the glass ribbon 2 has a second thin-walled portion 2a corresponding to the first thin-walled portion 1a of the glass mother material 1 and a second thick-walled portion 2b corresponding to the first thick-walled portion 1b of the glass mother material 1. That is, the glass ribbon 2 has the second thin-walled portion 2a in the central portion in the width direction and the second thick-walled portion 2b at both ends in the width direction. In the example shown in the figure, the surface of the second thin-walled portion 2b is composed of a flat surface extending in the width direction, but for example, the surface of the second thin-walled portion 2b may be composed of a concave curved surface or a flat surface and a concave curved surface. Moreover, in the glass ribbon 2, on both surfaces in the thickness direction, the second thick-walled portion 2b protrudes more than the second thin-walled portion 2a. In other words, in the glass ribbon 2, on both surfaces in the thickness direction, a concave portion 2c is formed at a position corresponding to the second thin-walled portion 2a. The glass mother material 1 extends in such a manner that the thickness t6 of the second thin-walled portion 2a of the glass ribbon 2 is, for example, 1 to 50 μm (preferably 1 to 30 μm).
[0070] like Figure 5 As shown in FIG. 1 , the support surface of the support portion 4 is a flat surface, and the support portion 4 is in contact with only the first thick wall portion 1b of the glass base material 1 and is not in contact with the first thin wall portion 1a. Figure 6 As shown, the pair of stretching rollers 6 are rod-shaped rollers with a constant diameter, and the pair of stretching rollers 6 only contact the second thick wall portion 2b of the glass ribbon 2, and do not contact the second thin wall portion 2a. Therefore, it is possible to suppress the first thin wall portion 1a of the glass mother material 1 and the second thin wall portion 2a of the glass ribbon 2 from being damaged or dirt from being attached. It should be noted that the support portion 4 and / or the stretching rollers 6 may also contact the thin wall portions 1a and 2a.
[0071] like Figure 3 As shown, (thickness t3 of first thick wall portion 1b of glass mother material 1) / (thickness t2 of first thin wall portion 1a of glass mother material 1) is preferably 1.1-25, more preferably 1.5-12.5, further preferably 2-12.5, and most preferably 2-5.
[0072] (Full width w1 of glass base material 1) / (thickness t3 of first thick portion 1b of glass base material 1) is preferably 25 to 4000, and more preferably 500 to 3000.
[0073] The ratio of (the width w3 of the first thick portion 1b of the glass base material 1) / (the width w2 of the first thin portion 1a of the glass base material 1) is preferably 0.02 to 40,000.
[0074] like Figure 4 As shown, (the thickness t6 of the second thick portion 2b of the glass ribbon 2) / (the thickness t5 of the second thin portion 2a of the glass ribbon 2) is preferably 1.1 or more, more preferably 1.5 to 12.5, further preferably 2 to 12.5, and most preferably 2 to 5.
[0075] (The total width w4 of the glass ribbon 2) / (The thickness t6 of the second thick portion 2b of the glass ribbon 2) is preferably 1.1-25, more preferably 1.5-12.5, and most preferably 2-5.
[0076] It is preferable that (the width w6 of the second thick portion 2b of the glass ribbon 2) / (the width w5 of the second thin portion 2a of the glass ribbon 2) is 0.02 to 40,000.
[0077] The thickness t6 of the second thin-walled portion 2a of the glass ribbon 2 is preferably 10 μm or less, and the full width w4 of the glass ribbon 2 (maximum width of the glass article) is preferably 0.5 to 40 mm.
[0078] The surface of the glass ribbon 2 is formed by a forged surface. That is, the surfaces of the second thin-walled portion 2a and the second thick-walled portion 2b are formed by a forged surface. Here, the forged surface means an unpolished surface that solidifies without contacting other components such as rollers after the glass is melted. If it is a forged surface, in addition to being difficult to form defects (such as microcracks) that may cause breakage, the corners formed on the surface are also rounded during the melting process, and become chamfered. Therefore, if it is a forged surface, the strength (especially bending strength) of the glass ribbon 2 is improved.
[0079] like Figure 1 As shown in FIG. 1 , in the article forming step, the glass ribbon 2 is wound around a winding roller 7 as a winding core to form a glass roll 3 as a glass article. In this embodiment, a protective sheet roll 8 is arranged near the winding roller 7. The protective sheet 9 unwound from the protective sheet roll 8 overlaps with the glass ribbon 2 and is wound around the winding roller 7 together with the glass ribbon 2. That is, as shown in FIG. Figure 7 As shown, the glass ribbon 2 and the protection sheets 9 are alternately stacked in the radial direction of the glass roll 3. In order to suppress damage and contamination of the glass ribbon 2, the innermost and outermost layers of the glass roll 3 are preferably formed of the protection sheets 9.
[0080] The glass ribbon 2 has a second thin-walled portion 2a in the center in the width direction, and has second thick-walled portions 2b at both ends in the width direction, and has recessed portions 2c formed at positions corresponding to the second thin-walled portion 2a on both surfaces in the thickness direction. Therefore, on both surfaces in the thickness direction of the glass ribbon 2, the protective sheet 9 contacts only the second thick-walled portion 2b of the glass ribbon 2, and does not contact the second thin-walled portion 2a. Therefore, it is possible to suppress the formation of damage or adhesion of dirt on both surfaces in the thickness direction of the second thin-walled portion 2a of the glass ribbon 2 due to contact with the protective sheet 9. It should be noted that the protective sheet 9 may also contact the second thin-walled portion 2a. For example, when the recessed portion 2c is formed at a position corresponding to the second thin-walled portion 2a on only one surface in the thickness direction of the glass ribbon 2, the protective sheet 9 contacts the second thin-walled portion 2a on the other surface in the thickness direction of the glass ribbon 2 (the surface on the side where the recessed portion 2c is not formed).
[0081] The glass ribbon 2 included in the glass roll 3 is cut into a predetermined length to form a glass plate, and is assembled to a device. Since the glass ribbon 2 or glass plate has a second thin-walled portion 2a and a second thick-walled portion 2b having a shape based on the glass mother material 1, the second thick-walled portion 2b having a larger thickness than the second thin-walled portion 2a can be supported in the manufacturing process of the device, thereby handling the glass ribbon 2 or glass plate. Therefore, the handling property of the glass ribbon 2 or glass plate becomes good. It should be noted that the second thick-walled portion 2b may be cut off and removed after the predetermined process included in the manufacturing process of the device, and only the second thin-walled portion 2a may be assembled to the device. Alternatively, the second thick-walled portion 2b may not be cut off and removed in the manufacturing process of the device, but may be assembled to the device together with the second thin-walled portion 2a. The second thick-walled portion 2b may be easily broken and removed, for example, by applying bending stress.
[0082] As devices to which the glass ribbon 2 included in the glass roll 3 is applied, for example, there may be mentioned a membrane device, a biofilter, a nanopore sensor, a glass sheet specimen, other sample containers, a sample cover, and the like.
[0083] The diaphragm device is a device that controls fluid by using deformation of a diaphragm, and the diaphragm is a glass plate obtained by cutting the glass ribbon 2. Typical examples of the diaphragm device include a diaphragm valve that opens and closes a flow path by using a diaphragm, and a diaphragm pump that pressurizes a fluid.
[0084] Biofilters and nanopore sensors are devices for selectively extracting specific fine matter such as DNA and protein from an object to be inspected. The biofilter has a filter section that selectively extracts specific fine matter (such as exosomes from cancer) from an object to be inspected (such as blood), and as the filter section, a glass plate obtained by cutting a glass ribbon 2 is used. In addition to the filter section, the nanopore sensor also has a sensor for detecting (or detecting and analyzing) the selectively extracted fine matter. Fine holes are formed in the glass plate used as a filter section. In the case of a biofilter, the fine holes of the glass plate are, for example, circular openings with a diameter of 1 to 50 μm, and in the case of a nanopore sensor, for example, circular openings with a diameter of 100 to 1000 nm. The fine holes can be formed in the state of the glass ribbon 2 or in the state of the glass plate obtained by cutting the glass ribbon 2. The processing method of the fine holes is not particularly limited, but for example, mechanical processing based on a drill bit, laser processing, ultrasonic processing, FIB (ion beam) processing, etc. can be used. When the fine holes are nanometer-sized, it is preferable to use FIB processing.
[0085] (Second Embodiment)
[0086] like Figure 8As shown, the method for producing a glass article according to the second embodiment is different from the method for producing a glass article according to the first embodiment in that the stretching roll 6 is arranged on only one surface side of the glass ribbon 2 continuous with the glass base material 1 .
[0087] That is, the glass ribbon 2 is wound around a part of the circumferential region of the outer peripheral surface of one stretching roller 6, and the posture of the glass ribbon 2 is changed from a longitudinal posture (e.g., a vertical posture) to a transverse posture (e.g., a horizontal posture). In the process of this posture change, the glass ribbon 2 is pulled downward by the one stretching roller 6, and the glass mother material 1 softened in the heating furnace 5 is stretched. Thus, a glass ribbon 2 with a relatively thin thickness is formed from the glass mother material 1.
[0088] It should be noted that the contact angle α of the stretching roll 6 is preferably 90 degrees or more, and more preferably 90 to 225 degrees.
[0089] The other structures of this embodiment are the same as those of the first embodiment. In this embodiment, the same reference numerals are used to indicate the same components as those of the first embodiment.
[0090] It should be noted that the present invention is not limited to the configuration of the above-described embodiment, and is not limited to the above-described effects. The present invention can be modified in various ways without departing from the gist of the present invention.
[0091] In the above embodiment, the glass article is exemplified as a glass roll 3, but the glass article may be a glass sheet obtained by cutting the glass ribbon 2 into a predetermined length on the downstream side of the stretching roll 6. Even when the glass article is a glass sheet, the same manufacturing process exemplified in the above embodiment can be applied.
[0092] In the above-mentioned embodiment, the glass mother material 1 and the glass ribbon 2 (or glass article) are described as having thin-walled portions 1a and 2a in the center in the width direction, thick-walled portions 1b and 2b at both ends in the width direction, and the thick-walled portions 1b and 2b protrude more than the thin-walled portions 1a and 2a at mutually symmetrical positions on both surfaces in the thickness direction, but the shapes of the glass mother material 1 and the glass ribbon 2 are not limited thereto. That is, by changing the position and size of the first thick-walled portion 1b and the first thin-walled portion 1a of the glass mother material 1, it is possible to form a glass ribbon 2 (or glass article) of various shapes based on the shape of the glass mother material 1. The following is an example of a modification of the glass mother material 1 and the glass ribbon 2.
[0093] like Fig. 9As shown, the glass mother material 1 may have a first thin-walled portion 1a in the center in the width direction, and may have first thick-walled portions 1b at both ends in the width direction, and the first thick-walled portion 1b may protrude more than the first thin-walled portion 1a at different positions on both surfaces in the thickness direction. In other words, the width-direction position of the recess 1c may be slightly different on both surfaces in the thickness direction. However, if the cross-sectional shape of the glass mother material 1 is not linearly symmetrical with respect to a thickness-direction center line passing through the center in the thickness direction and a width-direction center line passing through the center in the width direction, warping may occur in the glass ribbon 2 during the forming process. Therefore, the cross-sectional shape of the glass mother material 1 is preferably linearly symmetrical with respect to at least one of a thickness-direction center line passing through the center in the thickness direction and a width-direction center line passing through the center in the width direction.
[0094] like Fig.10 As shown, the glass mother material 1 may have a first thick-walled portion 1b only at one end in the width direction and a first thin-walled portion 1a in the remaining portion in the width direction, and the first thick-walled portion 1b protrudes more than the first thin-walled portion 1a at mutually symmetrical positions on both surfaces in the thickness direction.
[0095] like Fig.11 As shown, the glass mother material 1 may have a first thick wall portion 1b in the center in the width direction and first thin wall portions 1a at both ends in the width direction, and the first thick wall portions 1b protrude more than the first thin wall portions 1a at mutually symmetrical positions on both surfaces in the thickness direction.
[0096] like Fig.12 As shown, the glass mother material 1 may have a first thin-walled portion 1a in the central portion in the width direction, and first thick-walled portions 1b at both ends in the width direction, and the first thick-walled portion 1b may protrude more than the first thin-walled portion 1a only on one surface in the thickness direction. In other words, the recessed portion 1c may be formed only on one surface in the thickness direction of the glass mother material 1.
[0097] like Fig.13 As shown, the glass mother material 1 may have the first thick portion 1b only at one end in the width direction and the first thin portion 1a in the remaining portion in the width direction, and the first thick portion 1b may protrude more than the first thin portion 1a only on one surface in the thickness direction.
[0098] like Fig.14 As shown, the glass mother material 1 may have a first thick portion 1b in the center in the width direction and first thin portions 1a at both ends in the width direction, and the first thick portion 1b may protrude more than the first thin portion 1a only on one surface in the thickness direction.
[0099] Description of Reference Numerals
[0100] 1Glass base material
[0101] 1a First thin-walled portion
[0102] 1b First thick wall part
[0103] 1c concave part
[0104] 2 Glass belt
[0105] 2a Second thin-walled portion
[0106] 2b Second thick wall part
[0107] 2c concave part
[0108] 3 Glass rolls
[0109] 4 Supporting part
[0110] 5Heating furnace
[0111] 6 extension rollers
[0112] 7 Winding roller
[0113] 8 protective film rolls
[0114] 9 Protective sheet.
Claims
1. A method for manufacturing a glass article, characterized in that: The manufacturing method of the glass article comprises: A preparation step of preparing a glass base material having a first thin-walled portion in a central portion in the width direction and having first thick-walled portions having a thickness greater than that of the first thin-walled portion at both ends in the width direction including the end faces in the width direction; a forming step of extending the glass base material while softening it in a heating furnace by a re-drawing method to form a glass ribbon having a second thin-walled portion with a thickness of 10 μm or less in a central portion in the width direction and second thick-walled portions with a thickness greater than that of the second thin-walled portion at both ends in the width direction including the end faces in the width direction; and an article forming step of obtaining a glass article from the glass ribbon, In the forming step, a stretching roller for pulling the glass ribbon downward is provided below the outer side of the heating furnace in order to stretch the softened glass base material, and the stretching roller is in contact with only the second thick portion of the glass ribbon.
2. The method for manufacturing a glass article according to claim 1, wherein: In the glass base material, the first thick portion protrudes more than the first thin portion on both surfaces in the thickness direction.
3. The method for manufacturing a glass article according to claim 1 or 2, wherein: The first thin-walled portion is formed by grinding or etching the glass base material.
4. The method for manufacturing a glass article according to claim 1 or 2, wherein: In the article forming step, the glass ribbon is rolled into a roll.
5. The method for manufacturing a glass article according to claim 1 or 2, wherein: In the forming step, a support portion for supporting the glass base material is provided, and the support portion is in contact with only the first thick portion of the glass base material.
6. The method for manufacturing a glass article according to claim 1 or 2, wherein: (The maximum thickness of the glass mother material) / (the minimum thickness of the glass mother material) is 1.1 to 25.
7. The method for manufacturing a glass article according to claim 1 or 2, wherein: (Full width of the glass mother material) / (maximum thickness of the glass mother material) is 25 to 4,000.
8. The method for manufacturing a glass article according to claim 1 or 2, wherein: The first thin-walled portion is composed of a thin-walled planar portion having a constant thickness. The first thick-walled portion is composed of a thick-walled plane portion having a greater thickness than the thin-walled plane portion and having a constant thickness. (The width of each of the first thick-walled portions) / (The width of the first thin-walled portion) is 0.02 to 40,000.