Semiconductor devices
By forming a specific recessed structure on the peripheral edge of the radiator bottom surface of the semiconductor device and filling the packaging resin, the problem of peeling the interface between the packaging resin and the radiator is solved, and protection of insulation characteristics and long-term stability of the device are achieved.
Patent Information
- Application Number
- CN202111031125.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-03
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-09-03
AI Technical Summary
The existing semiconductor devices are prone to peeling the interface between the packaging resin and the radiator at high temperatures, resulting in deterioration of insulation characteristics, especially when the stress at the corners of the bottom step portion of the radiator is concentrated.
The first recess is formed in the peripheral edge of the bottom surface of the radiator, and the second recess is sunk downwardly, and the first recess is filled with encapsulation resin to suppress the development of peeling of the interface, while preventing peeling from the insulating layer through the second recess. The interface development with the radiator.
It effectively suppresses excessive warping of the radiator and interface peeling between the packaging resin and the radiator, extends the service life of the semiconductor device, and improves the interface stability between the insulating layer and the radiator.
Smart Images

Figure CN114242666B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor device having a heat sink. Background Art
[0002] A semiconductor device includes a heat sink, a semiconductor element, and a sealing resin that seals the heat sink and the semiconductor element in a state where the bottom surface of the heat sink is exposed. In such a semiconductor device, a step portion is provided on the bottom surface of the heat sink.
[0003] For example, Patent Document 1 discloses a technique for preventing a heat sink from falling off from the encapsulation resin by solidifying the encapsulation resin that has been bent around the step portion to form a resin hook. The resin hook is a structure in which the solidified resin is hooked on the unevenness of a component like a hook to prevent the component from falling off. Generally, the heat sink is formed using a material having good heat dissipation properties such as Al or Cu.
[0004] Patent Document 1: Japanese Patent Application Publication No. 2003-7933
[0005] However, in conventional semiconductor devices, when thermal stress or the like is applied to the corner of the step portion provided on the bottom surface of the heat sink, stress is easily concentrated, which easily becomes the starting point of peeling at the interface between the encapsulation resin and the heat sink. When the peeling progresses along the side surface of the heat sink toward the interface between the insulating layer provided on the upper surface of the heat sink and the heat sink, there is a problem of deterioration of the insulation characteristics of the semiconductor device. Summary of the invention
[0006] Therefore, an object of the present invention is to provide a technology capable of suppressing the delamination at the interface between a sealing resin and a heat sink from advancing to the interface between an insulating layer provided on the upper surface of the heat sink and the heat sink in a semiconductor device having a heat sink.
[0007] The semiconductor device of the present invention comprises: a heat sink; an insulating layer, which is arranged on the upper surface of the heat sink; a lead frame, which is fixed to the upper surface of the insulating layer; a semiconductor element, which is mounted on the upper surface of the lead frame; and a packaging resin, which packages the heat sink and the semiconductor element in a state where the bottom surface of the heat sink is exposed, a bottom surface step portion that is recessed in a step shape is formed on the peripheral portion of the bottom surface of the heat sink, a first recessed portion that is recessed upward and not exposed from the packaging resin is formed on the bottom surface step portion, and a second recessed portion that is recessed downward is formed on the upper surface of the heat sink.
[0008] Effects of the Invention
[0009] According to the present invention, at high temperature, the sealing resin filled in the first recess can suppress excessive warping of the heat sink, so that the peeling of the interface between the sealing resin and the heat sink can be suppressed from progressing from the corner of the bottom step portion. Furthermore, even if the peeling of the interface between the sealing resin and the heat sink progresses, the second recess can suppress the peeling of the interface between the sealing resin and the heat sink from progressing to the interface between the insulating layer and the heat sink. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 This is a cross-sectional view of the semiconductor device according to the first embodiment.
[0011] Figure 2 It is a bottom view of the heat sink included in the semiconductor device according to the first embodiment.
[0012] Figure 3 It is a bottom view of a heat sink included in the semiconductor device according to the second embodiment.
[0013] Figure 4 It is a bottom view of a heat sink included in a semiconductor device according to Modification 1 of Embodiment 2.
[0014] Figure 5 It is a bottom view of a heat sink included in a semiconductor device according to a second variation of the second embodiment.
[0015] Figure 6 This is an enlarged cross-sectional view of a semiconductor device according to a third embodiment.
[0016] Figure 7 This is a cross-sectional view showing the warpage of the semiconductor device when no recess is formed in the bottom step portion. DETAILED DESCRIPTION
[0017] <Implementation method 1>
[0018] Hereinafter, Embodiment 1 will be described using the drawings. Figure 1 It is a cross-sectional view of the semiconductor device 100 according to the first embodiment. Figure 2 It is a bottom view of the heat sink 5 included in the semiconductor device 100 .
[0019] like Figure 1 As shown, the semiconductor device 100 includes a heat sink 5 , an insulating layer 4 , a sealing resin 6 , a plurality of lead frames 1 , and a plurality of semiconductor elements 2 .
[0020] The heat sink 5 is formed using a material having good heat dissipation properties such as Al or Cu. The insulating layer 4 is provided on the entire upper surface of the heat sink 5. The lead frame 1 is fixed to the upper surface of the insulating layer 4. The semiconductor element 2 is fixed to the upper surface of the lead frame 1 using a bonding material 3 such as solder. In addition, the semiconductor element 2 is connected to the lead frame 1 or other semiconductor elements 2 using a metal wire 14.
[0021] The sealing resin 6 seals the heat sink 5 and the semiconductor element 2 in a state where the bottom surface 10 of the heat sink 5 is exposed. The insulating layer 4 and the sealing resin 6 are made of a resin with good insulation properties such as epoxy resin or phenolic resin and an additive.
[0022] Next, the structure of the radiator 5 will be described. Figure 1 and Figure 2 As shown, a bottom step portion 7 is continuously formed along the peripheral edge of the bottom surface 10 of the heat sink 5. A groove-shaped recessed portion 11 is continuously formed along the outer periphery of the bottom step portion 7 and is recessed upward as a first recessed portion.
[0023] The recess 11 is filled with the sealing resin 6, and the recess 11 is not exposed from the sealing resin 6. By forming the recess 11 at the outer peripheral portion of the bottom step portion 7, that is, around the corner of the bottom step portion 7, the sealing resin 6 filled in the recess 11 can suppress excessive warping of the heat sink 5 at high temperature. As a result, the delamination of the interface between the sealing resin 6 and the heat sink 5 can be suppressed.
[0024] In addition, the recessed portion 11 is formed by stamping. When the recessed portion 11 is formed by stamping, the outer peripheral portion of the bottom step portion 7 is subjected to stamping, so that the peripheral portion of the side surface 9 subjected to the stamping is partially plastically deformed and deformed in an expanding manner. When the side surface 9 is smooth, the peeling generated at the corner of the bottom step portion 7 is easy to develop along the smooth side surface 9, but in the first embodiment, since the shape of the side surface 9 is distorted, it becomes difficult to develop.
[0025] On the upper surface of the heat sink 5, a groove-shaped recessed portion 12 is continuously formed along the outer periphery of the upper surface as a second recessed portion that is recessed downward. In addition, a portion of the insulating layer 4 that is opposite to the recessed portion 12 is formed into a convex shape that protrudes downward in a manner corresponding to the recessed portion 12. By forming the recessed portion 12 on the upper surface of the heat sink 5, when peeling of the interface between the encapsulating resin 6 and the heat sink 5 progresses, it is possible to suppress the peeling of the interface between the encapsulating resin 6 and the heat sink 5 from progressing toward the insulating layer 4. That is, before the peeling of the interface between the encapsulating resin 6 and the heat sink 5 progresses along the side surface 9 of the heat sink 5 and then connects to the peeling of the interface between the insulating layer 4 and the heat sink 5, it is possible to suppress the peeling of the interface between the encapsulating resin 6 and the heat sink 5 from progressing toward the insulating layer 4.
[0026] The recessed portion 12 may not be continuous but may be formed discontinuously in a plurality. In addition, when the recessed portion 12 is formed in the outer peripheral portion rather than the central portion of the upper surface of the heat sink 5, the effect of suppressing the development of separation is greater.
[0027] Next, the operation and effects of the semiconductor device 100 will be described in comparison with a case where the recess 11 is not formed in the bottom surface step portion 7 . Figure 7 It is a cross-sectional view showing the warpage of the semiconductor device 101 when the recessed portion 11 is not formed in the bottom surface step portion 7 .
[0028] Generally, the linear thermal expansion coefficient of the heat sink 5 is larger than that of the encapsulating resin 6. Figure 7 As shown, the entire semiconductor device 101 is warped so that the bottom surface 10 of the heat sink 5 becomes convex.
[0029] In contrast, the semiconductor device 100 according to the first embodiment comprises: a heat sink 5; an insulating layer 4 disposed on the upper surface of the heat sink 5; a lead frame 1 fixed to the upper surface of the insulating layer 4; a semiconductor element 2 mounted on the upper surface of the lead frame 1; and a packaging resin 6 that packages the heat sink 5 and the semiconductor element 2 in a state where the bottom surface 10 of the heat sink 5 is exposed, a bottom surface step portion 7 that is recessed in a step-like shape is formed on the peripheral portion of the bottom surface 10 of the heat sink 5, a recess 11 that is recessed upward and not exposed from the packaging resin 6 is formed on the bottom surface step portion 7, and a recess 12 that is recessed downward is formed on the upper surface of the heat sink 5.
[0030] Therefore, at high temperatures, the encapsulation resin 6 filled in the recess 11 can suppress excessive warping of the heat sink 5, so that the delamination of the interface between the encapsulation resin 6 and the heat sink 5 can be suppressed from progressing from the corner of the bottom step 7. Furthermore, even if the delamination of the interface between the encapsulation resin 6 and the heat sink 5 progresses, the recess 12 can suppress the delamination of the interface between the encapsulation resin 6 and the heat sink 5 from progressing to the interface between the insulating layer 4 and the heat sink 5. Thus, the semiconductor device 100 can be used for a long time.
[0031] Furthermore, since the recessed portion 12 is formed in the outer peripheral portion of the upper surface of the heat sink 5 , the effect of suppressing the development of the peeling is increased.
[0032] Furthermore, since the recessed portion 11 is formed along the outer periphery of the bottom surface step portion 7 , it is possible to suppress the occurrence of peeling in the entire outer periphery of the bottom surface step portion 7 .
[0033] <Implementation method 2>
[0034] Next, a semiconductor device 100 according to a second embodiment will be described. Figure 3 It is a bottom view of the heat sink 5 included in the semiconductor device 100 according to the second embodiment. Figure 4 It is a bottom view of the heat sink 5 included in the semiconductor device 100 according to the first modification of the second embodiment. Figure 5 It is a bottom view of the heat sink 5 included in the semiconductor device 100 according to the modification 2 of the embodiment 2. In the embodiment 2, the same components as those described in the embodiment 1 are denoted by the same reference numerals, and the description thereof is omitted.
[0035] like Figure 3 As shown, in Embodiment 2, the recessed portion 11 is formed discontinuously. Specifically, the groove-shaped recessed portion 11 is formed only at the four corners of the bottom surface step portion 7 .
[0036] In addition, if Figure 4 As shown, the recessed portion 11 may be formed in a circular shape when viewed from below, and may be formed in plurality at intervals along the outer periphery of the bottom surface step portion 7 .
[0037] In addition, if Figure 5 As shown, the circular recessed portions 11 may be provided only at the four corners of the bottom surface step portion 7 .
[0038] As described above, in the second embodiment, since the recessed portion 11 is formed discontinuously, the effect of suppressing the progress of separation can be obtained, and the processing efficiency when forming the recessed portion 11 is improved compared with the case of the first embodiment.
[0039] <Implementation method 3>
[0040] Next, a semiconductor device 100 according to a third embodiment will be described. Figure 6 It is an enlarged cross-sectional view of the semiconductor device 100 according to the third embodiment. In the third embodiment, the same components as those described in the first and second embodiments are denoted by the same reference numerals, and the description thereof is omitted.
[0041] like Figure 6 As shown, in the third embodiment, the recess 11 is not formed in the bottom step 7, but instead, the recess 13 is formed in the side 9 of the heat sink 5. The recess 13 is formed along the circumferential direction of the side 9 in a manner recessed toward the inner circumference of the side 9, and is not exposed from the encapsulation resin 6.
[0042] As described above, in the third embodiment, since the recess 13 is formed on the side surface 9 of the heat sink 5, the peeling generated from the corner of the bottom step 7 can be prevented from advancing along the side surface 9. Thus, the peeling can be prevented from advancing to the interface between the insulating layer 4 and the heat sink 5.
[0043] In the third embodiment, the recessed portion 12 may be provided on the upper surface of the heat sink 5. This can suppress the delamination from progressing to the interface between the insulating layer 4 and the heat sink 5, compared with the case where the recessed portion 12 is not provided.
[0044] In addition, the various embodiments can be freely combined, or the various embodiments can be appropriately modified or omitted.
[0045] Description of the label
[0046] 1 lead frame, 2 semiconductor element, 4 insulating layer, 5 heat sink, 6 packaging resin, 7 bottom surface step portion, 11 recessed portion, 12 recessed portion, 13 recessed portion, 100 semiconductor device.
Claims
1. A semiconductor device comprising: heat sink; an insulating layer, which is disposed on the upper surface of the radiator; A lead frame fixed to the upper surface of the insulating layer; a semiconductor element mounted on the upper surface of the lead frame; as well as a sealing resin that seals the heat sink and the semiconductor element in a state where the bottom surface of the heat sink is exposed, A bottom surface step portion that is recessed in a step shape is formed on the peripheral edge of the bottom surface of the heat sink. A first recessed portion is formed on the bottom step portion, the first recessed portion being recessed upward and not exposed from the sealing resin. A second recessed portion recessed downward is formed on the upper surface of the heat sink. The first recessed portion is discontinuously formed only at four corners of the bottom surface step portion.
2. The semiconductor device according to claim 1, wherein The second recessed portion is formed on an outer peripheral portion of an upper surface of the heat sink.
Citation Information
Patent Citations
Resin-sealing semiconductor device
JP2003007933A
Resin-sealed semiconductor device
JP2008311366A
Semiconductor device cooler
JP2011258814A