Method for closing an injection molding mold using an anti-pinch strip
By placing shape-matched strips on the exposed surface of the fiber prefabricated parts, the problem of fiber prefabricated parts is solved during the mold closure process, avoiding the defect of "squeezing fibers" and ensuring the mechanical properties and surface quality of the gas turbine housing.
Patent Information
- Application Number
- CN202080064346.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-12
- Filing Date
- 2020-09-03
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-09-03
AI Technical Summary
When manufacturing gas turbine housing made of composite materials, in the prior art, the "extruded fiber" defects caused by the extrusion of the fiber prefabricated parts during the mold closure process, which affects the mechanical properties and surface quality.
Use strips to place strips on the exposed surface of the fiber preform to cover the angled fan joint area to prevent the fiber preform from being squeezed during mold closure, and use strips made of composite or metal materials to ensure that they are connected to the mold ring base The shape matches to prevent the blistering part from being pushed back and realizes mold closure without clamping.
It effectively avoids the defect of "extruded fiber" on finished parts, maintains mechanical properties and surface quality, and ensures the continuity and performance of the composite shell.
Smart Images

Figure CN114375251B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the general field of the manufacture of rotating components such as gas turbine casings. Background Art
[0002] In the aeronautical field, attempts are made to reduce the mass of engine components while maintaining their mechanical properties at a high level. For example, in aircraft turbines, the fan casing that defines the contours of the engine's inlet airflow path, and the rotor that supports the fan blades therein, are now made of composite materials.
[0003] The manufacture of a fan casing made of composite material begins with the mounting of a fiber reinforcement in a winding manner on a mandrel whose profile matches that of the casing to be produced. For example, the fiber reinforcement can be manufactured by three-dimensional or multilayer weaving, such as described in patent US 8 322 971. The fiber reinforcement is shaped so as to constitute a single piece comprising a tubular portion and a flange corresponding to the housing clamp. The manufacture continues with the densification of the fiber preform by a polymer matrix, consisting in impregnating the preform with a resin and polymerizing the latter to obtain the final component.
[0004] The invention relates more specifically to a manufacturing mode in which a fiber preform is impregnated by an injection molding process known as RTM (resin transfer molding). According to this process, the fiber preform is enclosed in a rigid mold of fixed geometry, comprising a mandrel or a drum on which the fiber preform is wound, and a counter-mold deposited on the fiber preform and having a shape corresponding to the part of revolution to be obtained; after the walls of the two mold parts are brought together and a vacuum is formed therein, if necessary, a pressurized, temperature-controlled resin is injected into the mold. After the resin has been injected, it is polymerized by heating the mold, and after injection and polymerization, the final part is demoulded, subsequently trimmed to remove excess resin, and the chamfers are machined to obtain the desired part, such as a housing.
[0005] Since the preform expands as it is wound on the mandrel, ie acquires an additional thickness compared to the theoretical thickness of the finished part, the closing of the mould ensures the function of final compaction of the preform so that it reaches its final thickness.
[0006] Figure 1 An RTM injection mold 300 is shown, consisting of a drum or mandrel 310, on which a fiber preform 30 is wound, and a counter-mold formed by a plurality of angular sectors 320. The mold closure is performed by the angular sectors 320, ensuring compaction of the preform. A method for closing such a mold is described in detail in the publication US 2018 / 370082.
[0007] However, closing the mold with such an angled sector is a delicate operation. Figure 2A As shown, one of the two sectors is placed first, each sector locally compressing the fiber preform. The fiber preform 30 has a foaming portion 31 near the end of each angular sector 320 because it is no longer compressed. Figure 2B and 2C As shown, the remaining angular sectors are positioned between the sectors already positioned to continue closing the mold. During the installation of these sectors, because the preform is displaced from the middle of the sectors due to compression, the blister 31 is pushed back to the edge of the sectors already positioned. In addition, the shape of the sectors and the direction of mold closing are such that there is space between the sectors until the last moment of mold closing. Subsequently, as Figure 2C As shown, part of the bubble 31 enters this space and ends up being sandwiched between the edges of adjacent sectors. The fibers of the preform are thus pinched, resulting in a defect called "pinched fibers" on the finished part. In fact, these pinched fibers eventually appear on the finished part, that is, in the form of bubbles on the outer surface of the part after the resin is injected into the preform and the latter is converted into a matrix. In order to obtain a satisfactory surface condition, the bubble is sanded, which will lead to the destruction of the continuity of the yarns or strands in the part, thus significantly reducing its mechanical properties. Summary of the invention
[0008] The object of the present invention is to propose a solution that avoids the above-mentioned drawbacks.
[0009] This object is achieved in particular thanks to a method for closing an injection mold for producing a rotating component made of composite material, comprising:
[0010] a mandrel supporting the fiber preform obtained by winding a fiber web, the mandrel comprising an annular wall, the outer surface of which has a profile corresponding to the profile of the inner surface of the part to be manufactured,
[0011] a plurality of angular sectors comprising an annular base intended to come into contact with the fibrous tissue, the annular base extending in the axial direction between the first longitudinal edge and the second longitudinal edge and in the circumferential direction between the first lateral edge and the second lateral edge, the shape of the annular base of each sector corresponding to the shape of the part of revolution to be manufactured,
[0012] The method comprises successively positioning and fixing angle sectors on a mandrel, each sector pressing a ring-shaped base of a portion of the fiber preform being present oppositely, the side edge of the ring-shaped base of each angle sector being in contact with the side edge of the ring-shaped base of an adjacent sector,
[0013] It is characterized in that before the angular sectors are positioned and fixed on the mandrel, strips are placed on the exposed surface of the fiber preform, each strip covering such an area of the fiber preform that is positioned to face the joining area of the two side edges of the annular bases of two adjacent angular sectors, and the shape of each strip corresponds to the shape of the annular bases of the two adjacent angular sectors at the joining area.
[0014] Thus, according to the method of the invention, the fiber preform is protected during closing of the mold from any pinching between two adjacent angular sectors. In fact, the strips covering the preform in the area corresponding to the joining area between the sectors prevent the portion of the preform present at the blister from being pushed back to the side edges of the angular sectors, which allows to avoid any pinching of the preform between the side edges of two adjacent sectors. Thus, defects of the "pinch-fiber" type that appear on the finished part are avoided. Thus, it is possible to compact the preform with the various angular sectors without affecting the mechanical properties of the finished part.
[0015] According to a particular feature of the method for closing an injection mould according to the invention, the strips are made of a composite material comprising a fibre reinforcement densified by a matrix. The fibre reinforcement of each strip may comprise carbon fibres, glass fibres or a mixture of carbon fibres and glass fibres. The matrix may be obtained from a thermosetting or thermoplastic resin or material.
[0016] According to another particular feature of the method for closing an injection mould according to the invention, said strip is made of metallic material.
[0017] According to yet another particular feature of the method for closing an injection mould according to the invention, the thickness of each strip is less than or equal to 0.2 millimetres.
[0018] According to another specific feature of the method for closing an injection mold according to the present invention, the angular sectors are first positioned and fixed on the core shaft at a determined distance from each other to arrange a space between two angular sectors, and then the remaining angular sectors are positioned and fixed on the core shaft in the area arranged between the fixed angular sectors.
[0019] According to another specific feature of the method for closing an injection mold according to the present invention, each angular sector includes a first groove and a second groove, which are respectively present on a first side and a second side, and which extend axially; a seal, which is accommodated in a first groove on the first side of the angular sector and a second groove on the second side of an adjacent angular sector.
[0020] The invention also relates to a method for manufacturing a rotating component made of a composite material, the method comprising:
[0021] - Produce fiber tissue in the form of a net by three-dimensional or multi-layer weaving,
[0022] - overlapping and winding the fiber structure on the mandrel of the injection mold for several turns to form a fiber preform, the injection mold comprising a plurality of angular sectors,
[0023] - closing the injection mold according to the invention,
[0024] - densifying the fiber preform by means of a matrix to obtain a part of revolution made of a composite material comprising a fiber reinforcement densified by a matrix,
[0025] - De-moulding the composite part. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 is a schematic perspective view of an injection mold according to the prior art,
[0027] Figure 2A is a partial sectional view of a radial section showing a closed Figure 1 A step of the mold,
[0028] Figure 2B is a partial sectional view of a radial section showing a closed Figure 1 Another step of the mold,
[0029] Figure 2C is a partial sectional view of a radial section showing a closed Figure 1 Another step of the mold,
[0030] Figure 3 is a schematic perspective view of a fan housing made of composite material.
[0031] Figure 4 is a schematic perspective view of an injection mold according to an embodiment of the present invention,
[0032] Figure 5 It is shown Figure 4 A schematic three-dimensional view of the angled sectors of the mold,
[0033] Figure 6 It is shown Figure 4 Another schematic perspective view of an angular sector of the mold,
[0034] Figure 7 It is shown Figure 4 A schematic perspective view of a strip of a mold,
[0035] Figure 8 It is shown Figure 4 Another schematic perspective view of a strip of a mold,
[0036] Fig.9A is a partial sectional view of a radial section showing the closed Figure 4 During the process of mold making, the angle sector is positioned at the beginning.
[0037] Fig. 9B is a partial sectional view of a radial section showing the closed Figure 4 The mold,
[0038] Fig.10 yes Fig. 9B Radial and axial cross-sections of the mold. DETAILED DESCRIPTION
[0039] The present invention is generally applicable to any casing for a gas turbine made of an organic-based composite material.
[0040] The present invention will be described below in conjunction with its application to a fan case in an aviation gas turbine engine.
[0041] Figure 3 A perspective view of a fan casing 10 that can be made using the mold and method according to the invention is shown. This casing is centered on a longitudinal axis XX and comprises an annular wall 11, which is bounded upstream by an upstream clamp 12 and downstream by a downstream clamp 13 (upstream and downstream are defined according to the flow direction of the gas turbine) The inner surface 14 of the annular wall 11 is intended to define an inlet airflow path in the gas turbine and / or a support panel (acoustic attenuation, wear-resistant material, etc.).
[0042] Figure 4 is a schematic perspective view of a mold according to the present invention being closed. Such a mold can be used for impregnation by such a process, that is, a RTM (resin transfer molding) type process of a fiber preform to manufacture a fan case 10 as described above. The fiber preform can be made of a fiber organization three-dimensionally woven in the form of a mesh of fibers, such as carbon, glass, aramid or ceramic fibers, and the impregnation matrix can be made of a polymer, such as epoxide, bismaleimide or polyimide.
[0043] The mold 100 is rotatably mounted on a drive shaft (not shown) centered on an axis XX and comprises a mandrel 110. Subsequently, an axial direction D is defined according to the axis XX. A and radial direction D R , axial direction D A Parallel to the axis XX and radial direction D R Perpendicular to axis XX. Figure 4 As shown, reference will also be made to the circumferential direction D C , which corresponds to the direction tangent to any circle centered on the axis XX. This direction is perpendicular to the axial direction D A and radial direction DR Both.
[0044] The mandrel 110 comprises an annular wall 111 in the form of a handle, which supports the fiber preform 20 formed by winding the fiber web, and flanges 112 on both sides. The mandrel 110 is held on its drive shaft by a shaft 113 .
[0045] The flange 112 forms a bearing intended to receive the folded portion of the preform 20 wound onto the mandrel 110 and intended to form the upstream and downstream clamps 12 , 13 of the fan casing 10 .
[0046] The mold 100 also comprises a counter-mold consisting of several angular sectors 120 (here six) assembled in a sealed manner on a mandrel 110. In the example described here, the sectors are locked together in a sealed manner by means of locking keys 130 which maintain a flat seal between the sectors ( Figure 4 According to a variant, the sectors can be locked together directly by bolts using oblique screws. In this case, the seal between the sectors is achieved by pressing the seals housed in grooves on the side edges of the sectors, as described below.
[0047] The angular sectors 120 are assembled on the side flanges 112 by means of clamping screws 131 which pass through apertures 122 in the sectors 120 and are screwed into threaded holes 1120 on the side flanges 112. The screws 131 allow the sectors 120 to be assembled on the flanges 112, as well as the compression pressure applied to the fiber preform 20 to be adjusted.
[0048] In the example described here, the angular sectors 120 are locked together by clamping screws 141 which pass through orifices 132 in the locking keys 130 and are screwed into threaded holes 128 on the angular sectors 120 or into bolts integral with the tool. The keys 130 are fixed between two adjacent sectors 120 by two rows of screws 141 extending longitudinally on the end of each sector 120. Once the sectors 120 are assembled on the mandrel 110, the locking keys 130 are assembled radially from the outside. In this way, the keys ensure that the sectors 120 are clamped together circumferentially.
[0049] An O-ring (not shown) located on the flange 112 ensures a seal between the sectors 120 and the mandrel 110 .
[0050] Figure 5 and 6 Angular sectors 120 are shown. Each angular sector 120 comprises an annular base 121 for contacting the fibrous tissue 20. The annular base extends in the radial direction D between the first longitudinal edge 122 and the second longitudinal edge 123. A The first side edge 124 and the second side edge 125 extend along the circumferential direction DC The first side edge 124 of the annular base 121 of the angular sector 120 contacts the second side edge 125 of the annular base of the adjacent angular sector ( Fig. 9B ).
[0051] The annular base 121 has a shape corresponding to the shape of the rotating component to be manufactured. In the example described here, the annular base 121 has a shape in the axial direction D A More specifically, the annular base 121 comprises a recessed portion 1212 which corresponds to the shape of the additional thickness 22 on the preform 20 and is intended to form a retention area ( Fig.10 ). The concave portion is along the circumferential direction D C Extends over the entire length of the annular base 121 .
[0052] The first side edge 124 of the annular base 121 of each angular sector 120 comprises a lower portion 1240 . The second side edge 125 of the annular base 121 of each angular sector 120 comprises a lower portion 1250 .
[0053] Each angular sector 120 further includes a first side surface 1241 and a second side surface 1251. The first side surface 1241 is parallel to the radial direction D R The second side surface 1251 is parallel to the radial direction D and exists in the extension portion of the first side edge 124 of the annular base 121. R And it is present in the extension of the second side edge 125 of the annular base 121. This helps to fix the sector 120 on the mandrel 110.
[0054] In addition, the first groove 1242 and the second groove 1252 may exist on the first side surface 1241 and the second side surface 1251, respectively, and these grooves are arranged along the axial direction D A The seal 150 is housed in a first groove 1242 of a first side 1241 of an angular sector and in a second groove 1252 of a second side 1251 of an adjacent angular sector. This allows a seal to be obtained between sectors and the sectors are locked together directly without the use of a clamping key and the flat seals described above.
[0055] According to the invention, before the injection mold 100 is closed by the angular sectors 120, the strips 200 are positioned on the exposed surface of the fiber preform 20. More specifically, the strips 200 are placed at each location of the exposed surface of the preform 20 that is intended to face the junction area ( Figure 4 ). Each strip 200 has a size that can cover the area. In the example described here, each strip 200 is axially oriented in the direction DA The width l200 is at least equal to the width 1121 of the annular base 121 of each angular sector 120, along the axial direction D A The length L200 allows the strip 200 to be moved along the circumferential direction D C Extending beyond the side edges 124 and 125 of two adjacent angular sectors ( Figure 4 , 7 and 8). When there is no risk of pinching over the entire width of the preform, the length of the strips may be less than the width of the fiber preform. According to a variant, some of the strips may be arranged in the axial direction D A Adjacently set.
[0056] like Figure 7 and 8 As shown, the shape of each strip 200 corresponds to the shape of the annular bases of two adjacent angular sectors in the joining area. More specifically, the outer surface 202 of each strip, which is intended to be in contact with the annular bases of two adjacent angular sectors, comprises a raised portion 2020 whose shape exactly matches the recessed portion 1212 present on the annular base 121 of each angular sector 120. Correspondingly, the inner surface 201 of each strip 200 comprises a recessed portion 2010, which reproduces the shape of the recessed portion 1212 present on the annular base 121 of each angular sector 120. The portions 2010 and 2020 are connected along the circumferential direction D C Extends the entire length of each strip.
[0057] According to one aspect of the invention, the strip 200 is made of a composite material from a fiber reinforcement densified by a matrix. Various types of composite materials and manufacturing methods can be used. The strip can be made from a preform made by:
[0058] - Overlaying in carbon fibers, glass fibers or a mixture of carbon fibers and glass fibers as unidirectional or bidirectional layers, each layer being pre-impregnated with a matrix precursor, such as epoxy resin.
[0059] - impregnation of the dried fiber structure with epoxy resin, which is obtained by overmolding, for example, with unidirectional or bidirectional layers,
[0060] - Overlay formed in unidirectional or bidirectional layers in carbon fiber, glass fiber or a mixture of carbon fiber and glass fiber, each layer is pre-impregnated with a resin or thermoplastic material such as polyetheretherketone (PEEK), polyetherketoneketone (PEKK), polyaryletherketone (PAEK), polyetherimide (PEI).
[0061] The strip preform is then shaped and heat treated to convert the resin or thermosetting (polymerized) or thermoplastic (heated and then cooled) material into a matrix.
[0062] The shaping of the strip preform may advantageously be performed by moulding on the annular base 121 of the angular sectors 120, which ensures that the strip will perfectly match the shape of the annular base during closing of the mould.
[0063] The stiffness of the strip is adjusted so that it is flexible enough not to break during the deformation imposed by the first fixed angular sectors as described below.
[0064] The strip can also be made from a metallic material, in particular by pressing or additive manufacturing of sheet metal (for example by electroplating nickel), in a shape identical to that of the annular base of the angular sector.
[0065] The thickness Ep200 of each composite or metallic material is less than or equal to 0.2 mm, in particular in order not to form cavities that are too large in the fiber preform during closing of the mold.
[0066] Fig.9A and 9B The positioning of the angular sectors during closing of the mold 100 is shown. More specifically, during Fig.9A , the last angular sector 1206 is positioned between the two angular sectors 1201 and 1205 that have already been positioned to finally close the mold 100. According to one feature of the method for closing the mold of the present invention, one of the two angular sectors is first placed and fixed, and then the closing is completed by closing the free space between the two angular sectors with the remaining sector. However, other mold closing configurations are also conceivable.
[0067] exist Fig.9A In the embodiment, the fiber preform 20 has a bubble portion 21 near the side edge 125 of the angle sector 1205 and the side edge 124 of the angle sector 1201 due to the compression of these angle sectors. According to the present invention, the strip 200 exists on the exposed surface of the preform 20 at each bubble portion 21. In the mold closing step, the strip 200 is formed by the already positioned angle sectors ( Fig.9A Under the compressive force applied by the fans 1205 and 1201 in the strip 200, the strip 200 is deformed at the bubble portion 21.
[0068] like Fig. 9BAs shown, the mold closing continues with the positioning and fixing of the last angular sector 1206. During the installation of this sector, the blister 21 cannot enter the space existing between the angular sectors due to the presence of the strip 200. The strip 200 prevents the portion of the preform present at the blister 21 from being pushed back to the side edges of the sectors 1205 and 1201, which avoids any pinching of the preform between the side edges of two adjacent sectors.
[0069] from Fig.10 As can be seen in FIG. 1 , once the mold is closed, each strip 200 completely follows the shape of the annular base 121 of each angular sector 120 of the mold 100. In the example described here, each strip 200 is axially oriented in the direction D A The shape of the strip 200 is identical to the shape of the profile of the annular base 121 of the adjacent angular sectors between them. In particular, each strip 200 comprises on its outer surface a curved portion 2020 whose shape is adapted to the shape of the recessed portion 1212 present on the annular base 121 of each angular sector 120 and corresponds to the shape of the additional thickness 22 present on the preform 20 and is intended to form a retention area in the final shell.
[0070] Using the strip according to the invention, it is possible to avoid defects of the “squeezed fibers” type on the finished part. It is therefore possible to use each of these angular sectors 120 to compact the preform 20 without affecting the mechanical properties of the finished part.
[0071] Figure 3 The manufacture of the shell 10 shown starts with a fiber structure produced by three-dimensional weaving between warp yarns and weft yarns. "Three-dimensional weaving" or "3D weaving" here refers to a weaving pattern by which at least some of the weft yarns bind the warp yarns to several layers of warp yarns, and vice versa. The fiber structure can have an interlocking weave. "Interlocking weaving" here is a weaving method in which each layer of the weft yarns binds several layers of the warp yarns, and all yarns of the same weft yarn column have the same movement within the weaving plane. Other weavings can also be envisioned. The yarn used can especially be a yarn made of carbon, glass or silicon carbide fiber. The fiber structure has the form of a mesh that is wound around the mandrel 110 of the mold 100 for several turns to form a fiber preform 20.
[0072] Subsequently, the mold 200 is closed by means of the above-mentioned angular sectors 120 , which also carry out the compaction of the preform 20 .
[0073] Subsequently, the fiber preform is densified, which consists in filling the pores of the latter with the material constituting the matrix. To this end, a liquid matrix precursor, such as a resin, is injected into the entire preform present in the mould. The conversion of the precursor into an organic matrix, i.e. its polymerization, is carried out by a thermal treatment, usually by heating the mould, and after removal of any solvent and crosslinking of the polymer, the preform remains in the mould in a shape corresponding to that of the part to be manufactured. The organic matrix can be obtained in particular from an epoxy resin, such as a commercially available high-performance epoxy resin, or from a liquid precursor of a carbon or ceramic matrix.
[0074] Densification of the fiber preform can be carried out by a well-known transfer molding process called RTM (resin transfer molding), which consists of injecting a thermosetting resin into the internal space of a mold containing the fiber preform, and a pressure gradient is usually established in the internal space between the resin injection point and the discharge orifice to monitor and optimize the impregnation of the preform with the resin. Once the resin is injected into the entire preform, it is polymerized by heat treatment according to the RTM process.
[0075] After injection and polymerization, the part is demoulded.
[0076] Finally the part is trimmed to remove excess resin and machine the chamfers to obtain Figure 3 The housing 10 shown has a shape of revolution.
Claims
1. A method for closing an injection mold, the mold (100) being used to manufacture a rotating part made of a composite material, the mold include: - a mandrel (110) supporting a fiber preform (20) obtained by winding a fiber web, the mandrel comprising an annular wall (111) having an outer surface whose profile corresponds to the profile of the inner surface (14) of the part to be manufactured, - a plurality of angular sectors (120), said plurality of angular sectors (120) comprising an annular base (121) for contacting the fiber preform (20), said annular base extending in the axial direction (D) between the first longitudinal edge and the second longitudinal edge (122, 123) A ) and extends along a circumferential direction (D) between the first side edge and the second side edge (124, 125) C ) extends, the shape of the annular base of each sector corresponds to the shape of the rotating part to be manufactured, The method comprises continuously positioning and fixing the angular sectors (120) on the mandrel (110), each sector pressing the annular base (121) of the fiber preform being relatively present, the side edge of the annular base (121) of each angular sector (120) being in contact with the side edge of the annular base (121) of the adjacent sector, It is characterized in that before the angular sectors are positioned and fixed on the core shaft, a strip (200) is placed on the exposed surface of the fiber preform (20), the strip (200) covers each area of the fiber preform, each of the areas is positioned to face the joint area between the two side edges of the annular bases (121) of two adjacent angular sectors (120), and the shape of each strip corresponds to the shape of the annular bases of the two adjacent angular sectors at the joint area.
2. The method according to claim 1, It is characterized in that The strip (200) is made of a composite material comprising a fiber reinforcement densified by a matrix.
3. The method according to claim 2, It is characterized in that The fiber reinforcement of each of the strips includes carbon fibers, glass fibers, or a mixture of carbon fibers and glass fibers.
4. The method according to claim 2 or 3, It is characterized in that The matrix is obtained from a thermosetting or thermoplastic resin or material.
5. The method according to claim 1, It is characterized in that The strip is made of a metallic material.
6. The method according to claim 2 or 3, It is characterized in that The thickness of each strip (200) is less than or equal to 0.2 mm.
7. The method according to claim 1, It is characterized in that The angular sectors (120) are first positioned and fixed on the mandrel (110) at a determined distance from each other to arrange a space between two of the angular sectors, and then the remaining angular sectors (120) are positioned and fixed on the mandrel (110) in the area arranged between the fixed angular sectors.
8. The method according to claim 1, It is characterized in that Each of the angular sectors (120) comprises a first groove and a second groove (1242, 1252), wherein the first groove and the second groove are respectively present on a first side surface and a second side surface (1241, 1251), and the first groove and the second groove are arranged along the axial direction (D A )extend; A seal (150) is received in a first groove (1242) on a first side of the angular sector and in a second groove (1252) on a second side of an adjacent angular sector.
9. A method for manufacturing a rotating component made of a composite material (30), the method include: - Producing fiber tissue in the form of a mesh by three-dimensional or multi-layer weaving, - overlapping and winding the fiber structure on a core shaft (110) of an injection mold (100) for a plurality of turns to form a fiber preform (20), wherein the injection mold comprises a plurality of angular sectors (120), - closing the injection mold (100) according to any one of claims 1 to 8, - densifying the fiber preform (20) by means of a matrix to obtain a part of revolution made of a composite material (30) comprising a fiber reinforcement densified by a matrix, - demoulding the composite part.