Iridium-containing complex and preparation method thereof

By reacting the iridium compound with triphenylphosphine and formaldehyde in a solvent, and heating it with acetylacetone, a high-purity iridium complex [Ir(acac)(CO)(TPP)] was prepared, and the prior art was solved. The problems of complex preparation methods and high impurity content have achieved simple and efficient processes and high purity products.

CN114437133BActive Publication Date: 2024-11-19CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011204691.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-11-02
Publication Date
2024-11-19
Estimated Expiration
2040-11-02

AI Technical Summary

Technical Problem

In the prior art, the preparation method of iridium compounds is complex, the conditions are harsh and impurities are easily introduced, resulting in a unclear process and a high product impurity content.

Method used

In the first solvent, the iridium compound is contacted with triphenylphosphine to form a triphenylphosphine halide of iridium, and then react with formaldehyde in the presence of hydrochloric acid to obtain a triphenylphosphine carbonyl halide of iridium, followed by a second solvent Heating reaction with acetylacetone was performed to prepare an iridium-containing complex [Ir(acac)(CO)(TPP)].

Benefits of technology

This method simplifies the preparation process, shortens the synthesis time, improves production efficiency, the product purity reaches more than 99%, the weight content of chlorine is less than 0.02%, and does not require further purification. It is suitable for laboratory and industrial production.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to the field of preparation of precious metal compounds, and in particular, to a method for preparing an iridium-containing complex and a method for preparing the same. The present invention discloses a method for preparing an iridium-containing complex, comprising the following steps: (1) contacting an iridium compound containing a halogen atom with triphenylphosphine in the presence of a first solvent to obtain an iridium triphenylphosphine halide; (2) reacting formaldehyde with the iridium triphenylphosphine halide in the presence of hydrochloric acid to obtain an iridium triphenylphosphine carbonyl halide; (3) heating acetylacetone with the iridium triphenylphosphine carbonyl halide in the presence of a second solvent. The method for preparing an iridium-containing complex provided by the present invention has the advantages of simple process, mild conditions and low impurity content in the product, and has broad application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of preparation of precious metal compounds, and in particular to an iridium-containing complex and a preparation method thereof. Background Art

[0002] Due to their unique physical and chemical properties, platinum group metals are widely used in various fields such as chemical industry, medicine, materials, and military industry. Among them, acetylacetonate complexes of platinum group metals have attracted much attention in recent years. In addition to using vapor deposition technology to prepare metal coatings, carrier catalysts, and thin film catalysts, they have great application value in the synthesis of homogeneous and heterogeneous catalysts, fuel cell catalysts, and new nanomaterials. In the carbonyl synthesis of butyl octanol, acetylacetonate triphenylphosphine carbonyl rhodium is usually used as a catalyst. In addition to traditional rhodium-based catalysts, compounds such as acetylacetonate dicarbonyl iridium [Ir(acac)(CO)2] and tri(triphenylphosphine) carbonyl hydride iridium [HIr(CO)(TPP)3] also show good catalytic performance. The price of iridium is much lower than that of rhodium, so the research on iridium compounds has greater application value. However, there are not many studies on the preparation methods of iridium-containing compounds. CN104230999A discloses a method for preparing iridium dicarbonyl acetylacetonate, using hydrated iridium trichloride and 1,5-cyclooctadiene as starting materials, and obtaining the target product through the (1,5-cyclooctadiene) iridium chloride dimer intermediate. The method needs to be carried out under an argon atmosphere, and uses cyclooctadiene and tetrahydrofuran, which makes the preparation process more complicated and is likely to introduce more impurities.

[0003] Therefore, it is necessary to seek a method for preparing iridium-containing complexes with simple process, mild conditions and low impurity content. Summary of the invention

[0004] The purpose of the present invention is to overcome the technical problems of the prior art, such as the complex preparation process, harsh conditions, and the introduction of impurities during the preparation process, and to provide an iridium-containing complex and a preparation method thereof. The method provided by the present invention has the advantages of simple preparation process, mild conditions, and low impurity content in the product.

[0005] In order to achieve the above object, the first aspect of the present invention provides a method for preparing an iridium-containing complex, characterized in that it comprises the following steps:

[0006] (1) contacting an iridium compound containing a halogen atom with triphenylphosphine in the presence of a first solvent to obtain a triphenylphosphine halide of iridium;

[0007] (2) reacting formaldehyde with the iridium triphenylphosphine halide in the presence of hydrochloric acid to obtain iridium triphenylphosphine carbonyl halide;

[0008] (3) In the presence of a second solvent, acetylacetone and the iridium triphenylphosphine carbonyl halide are subjected to a heating reaction.

[0009] The second aspect of the present invention provides an iridium-containing complex, characterized in that the structure of the iridium-containing complex is as follows:

[0010] [Ir(acac)(CO)(TPP)].

[0011] Compared with the prior art, the method for preparing the iridium-containing complex of the present invention has a short synthesis time, a simple process, greatly improved production efficiency, and a high product purity, which can reach more than 99%, and the weight content of the chlorine element is less than 0.02%, and no further purification is required, and it can be directly used in the catalytic reaction. The method provided by the present invention has easy control of process conditions, is not only suitable for laboratories, but also conducive to industrialization. DETAILED DESCRIPTION

[0012] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0013] The first aspect of the present invention provides a method for preparing an iridium-containing complex, the method comprising the following steps:

[0014] (1) contacting an iridium compound containing a halogen atom with triphenylphosphine in the presence of a first solvent to obtain a triphenylphosphine halide of iridium;

[0015] (2) reacting formaldehyde with the iridium triphenylphosphine halide in the presence of hydrochloric acid to obtain iridium triphenylphosphine carbonyl halide;

[0016] (3) In the presence of a second solvent, acetylacetone and the iridium triphenylphosphine carbonyl halide are subjected to a heating reaction.

[0017] According to some embodiments of the present invention, in step (1), the iridium compound containing halogen atoms can be selected from soluble iridium compounds, that is, compounds soluble in the first solvent, preferably selected from at least one of iridium chloride, iridium tetrachloride, iridium iodide, iridium bromide, iridium chloride hydrate, iridium tetrachloride hydrate, iridium iodide hydrate and iridium bromide hydrate, more preferably selected from iridium chloride and / or iridium chloride hydrate.

[0018] In the present invention, there is no particular limitation on the number of water of crystallization in hydrated iridium chloride (IrCl3·nH2O), hydrated iridium tetrachloride (IrCl4·nH2O), hydrated iridium iodide (IrI3·nH2O) and hydrated iridium bromide (IrBr3·nH2O), and can be 3-6, preferably 3 and / or 6, that is, there is no particular limitation on the value of n in IrCl3·nH2O, IrCl4·nH2O, IrI3·nH2O and IrBr3·nH2O, and can be 3-6, preferably 3 and / or 6.

[0019] According to some embodiments of the present invention, preferably, in step (1), the molar ratio of triphenylphosphine to the iridium compound containing halogen atoms can be (1-20):1, more preferably (2-10):1, and the molar amount of the iridium compound containing halogen atoms is calculated as iridium element.

[0020] According to some embodiments of the present invention, preferably, in step (1), the contact conditions may include: temperature of 40-120°C, pressure of 0.05-5MPa, and time of 0.2-10h; more preferably, temperature of 50-80°C, pressure of 0.1-1MPa, and time of 0.5-5h.

[0021] According to some embodiments of the present invention, the contacting is preferably carried out under an inert atmosphere, and the inert atmosphere can be provided by replacing the air with an inert gas, wherein, relative to 50 g of the iridium compound containing halogen atoms to be reacted, the flow rate of the inert gas replacing the air can be 50-2500 mL / min, preferably 80-500 mL / min.

[0022] In the present invention, there is no particular limitation on the method of replacing air with the inert gas, as long as an inert atmosphere can be provided for the contact. For example, the inert gas may be introduced into the first solvent.

[0023] In the present invention, the inert gas may be nitrogen.

[0024] According to some embodiments of the present invention, in step (1), the first solvent may be a mixture of alcohol and water.

[0025] Preferably, the weight percentage of alcohol in the second solvent may be 50-99%, more preferably 70-95%.

[0026] According to a preferred embodiment of the present invention, the alcohol may be selected from C1-C4 monohydric alcohols, more preferably at least one selected from methanol, ethanol, n-propanol and isopropanol, and further preferably ethanol.

[0027] According to a preferred embodiment of the present invention, the amount of the first solvent used is 2-50 mL, more preferably 5-25 mL, per gram of the iridium compound containing halogen atoms.

[0028] According to some embodiments of the present invention, preferably, the contacting conditions may further include: being carried out in the presence of an acid, more preferably, the acid may be selected from formic acid and / or oxalic acid, further preferably oxalic acid.

[0029] According to some embodiments of the present invention, in order to achieve a better reduction effect, there are certain requirements on the amount of acid used. Preferably, the molar ratio of the acid to the iridium compound containing halogen atoms can be (0.1-3):1, preferably (0.1-1.5):1, and the molar amount of the iridium compound containing halogen atoms is calculated as iridium element.

[0030] In the present invention, according to a particularly preferred embodiment, in step (1), the contacting of the iridium compound containing halogen atoms with triphenylphosphine can be carried out in the following manner:

[0031] The iridium compound containing halogen atoms is dissolved in the first solvent to prepare a 0.01-1 mol / L iridium compound solution containing halogen atoms, heated to 50-80°C, stirred for 20-40min, fully dissolved and mixed to obtain a first mixture. Subsequently, an inert gas (normal pressure) is continuously introduced into the first mixture at a flow rate of 100-150mL / min to replace the air therein to form an inert atmosphere, and then, under an inert atmosphere, oxalic acid is added to the first mixture, and stirring is continued at 50-80°C for 0.5-2h to obtain a second mixture. After that, triphenylphosphine is dissolved in the first solvent to prepare a 0.01-1 mol / L triphenylphosphine solution, and after the triphenylphosphine is completely dissolved, it is added to the above-mentioned second mixture, and stirred at 50-80°C for 0.5-2h under an inert atmosphere to obtain iridium triphenylphosphine halide. Among them, the amount of oxalic acid added is such that the molar ratio of oxalic acid to the iridium compound containing halogen atoms is (0.1-1.5):1, and the amount of triphenylphosphine added is such that the molar ratio of triphenylphosphine to the iridium compound containing halogen atoms is (2-10):1, and the molar amount of the iridium compound containing halogen atoms is calculated based on the iridium element.

[0032] In the present invention, preferably, the iridium triphenylphosphine halide obtained in step (1) can be directly used in step (2).

[0033] According to some embodiments of the present invention, preferably, in step (2), the molar ratio of formaldehyde to iridium triphenylphosphine halide can be (10-200):1, more preferably (50-100):1, and the molar amount of the iridium triphenylphosphine halide is calculated as iridium element.

[0034] In the present invention, preferably, formaldehyde can participate in the reaction in step (2) in the form of a formaldehyde solution. More preferably, the formaldehyde solution is an aqueous solution of formaldehyde.

[0035] In the present invention, preferably, the concentration of formaldehyde in the solution may be 20-50% by weight, more preferably 40% by weight.

[0036] According to some embodiments of the present invention, in step (2), the molar ratio of hydrochloric acid to iridium triphenylphosphine halide can be (2-50):1, preferably (5-10):1, and the molar amount of the iridium triphenylphosphine halide is calculated as iridium element.

[0037] In the present invention, preferably, hydrochloric acid can participate in the reaction in step (2) in the form of a hydrochloric acid solution. More preferably, the hydrochloric acid solution is an ethanol solution of hydrochloric acid with a concentration of 1-5M.

[0038] According to some embodiments of the present invention, preferably, the reaction conditions in step (2) may include: temperature of 40-120°C, pressure of 0.05-5MPa, and time of 0.5-10h; more preferably, temperature of 50-80°C, pressure of 0.1-1MPa, and time of 0.5-5h.

[0039] According to a preferred embodiment of the present invention, in step (2), the reaction is carried out under an inert atmosphere, and the inert atmosphere can be provided by nitrogen.

[0040] According to some embodiments of the present invention, preferably, in step (3), the conditions for the heating reaction may include: temperature of 90-200°C, pressure of 0.05-5MPa, and time of 2-30h; more preferably, temperature of 120-180°C, pressure of 0.1-1MPa, and time of 5-15h.

[0041] According to some embodiments of the present invention, preferably, the heating reaction is carried out under an inert atmosphere, and the inert atmosphere can be provided by nitrogen.

[0042] According to some embodiments of the present invention, preferably, in step (3), the amount of acetylacetone used can be 1-20 mL, more preferably 5-10 mL, per gram of triphenylphosphine carbonyl halide of iridium calculated as iridium element.

[0043] According to some embodiments of the present invention, preferably, in step (3), the amount of the second solvent used can be 5-200 mL, preferably 20-100 mL, per gram of the iridium triphenylphosphine carbonyl halide. More preferably, the second solvent is acetone.

[0044] According to a preferred embodiment of the present invention, in step (3), the heating reaction can also be carried out in the presence of N,N-dimethylformamide. Preferably, the amount of N,N-dimethylformamide used is 0.5-20 mL, preferably 2-10 mL, per gram of the iridium triphenylphosphine carbonyl halide.

[0045] In the present invention, preferably, before step (3), the process may further include filtering (solid-liquid separation) the material after the reaction in step (2) to obtain iridium triphenylphosphine carbonyl halide.

[0046] In the present invention, preferably, before obtaining the iridium-containing complex, step (3) may further include post-treatment of the material after the heating reaction. The present invention has no particular limitation on the operation of post-treatment of the material after the heating reaction, and may refer to conventional operations in the art; for example, the material after the reduction reaction may be filtered (solid-liquid separation), the filtrate may be discarded to obtain a filter cake, and then the filter cake may be washed with distilled water and ethanol in sequence, and dried at 60-80° C. for 5-24 hours.

[0047] In the present invention, normal pressure generally refers to "0.1 MPa" unless otherwise specified.

[0048] The second aspect of the present invention provides an iridium-containing complex, the structure of which is shown below:

[0049] [Ir(acac)(CO)(TPP)].

[0050] The present invention will be described in detail below through examples.

[0051] In the following examples, the yield of the iridium-containing complex is calculated based on the mole of metallic iridium in the iridium-containing complex by the following formula: Iridium yield (iridium-containing complex yield) = (W0 / W1)*100%,

[0052] W0—the weight of iridium in the raw material chloroiridic acid (g), W1—the weight of iridium in the product (g).

[0053] The element contents were measured by ICP.

[0054] Example 1

[0055] (1) In a 500 mL three-necked flask, 2.112 g of IrCl3·3H2O was dissolved in 50 mL of 95% by weight ethanol aqueous solution, heated to 80° C., stirred for 30 min, fully dissolved and mixed to obtain a first mixture. Subsequently, nitrogen (normal pressure) was continuously introduced into the first mixture at a flow rate of 100 mL / min to replace the air therein to form an inert atmosphere. Subsequently, 0.419 g of oxalic acid was added to the first mixture under an inert atmosphere, and the mixture was stirred at 80° C. for 30 min to obtain a second mixture. Afterwards, 3.856 g of triphenylphosphine was weighed and dissolved in 50 mL of 95% by weight ethanol aqueous solution, and then added to the second mixture, and reacted for 60 min under a nitrogen atmosphere at 80° C. to obtain a material containing triphenylphosphine iridium chloride.

[0056] (2) To the system after the reaction in step (1), 30 mL of 2M hydrochloric acid-ethanol solution and 4.5 g of 40 wt % formaldehyde solution were added in sequence, and the mixture was reacted at 80° C. for 30 min under stirring, and a precipitate was gradually generated in the solution to obtain a material containing triphenylphosphinecarbonyliridium chloride.

[0057] (3) Filter the reacted material in step (2), discard the filtrate, and collect the filter cake. Dissolve the filter cake in 100 mL of acetone to obtain an acetone solution of triphenylphosphine carbonyl halide, and introduce nitrogen into the above solution to replace the air (normal pressure) therein to form an inert atmosphere. Then, add 5.8 mL of N,N-dimethylformamide and 6.5 mL of acetylacetone to the above solution, heat to reflux, and react for 10 hours. Remove the solvent by filtration under reduced pressure while hot, wash the filter cake with 200 mL of distilled water and 100 mL of ethanol in turn, and vacuum dry at 70°C for 5 hours to obtain 1.936 g of iridium complex.

[0058] The elemental analysis results show that the yield of the iridium complex is 55.4% based on the iridium element, and the weight content of the chlorine element is 178 ppm.

[0059] Example 2

[0060] (1) In a 1L three-necked flask, 2.615g of H2IrCl6·6H2O was dissolved in 50mL of 90% by weight ethanol aqueous solution, heated to 60°C, fully dissolved, and mixed to obtain a first mixture. Then, nitrogen (normal pressure) was continuously introduced into the first mixture at a flow rate of 100mL / min to replace the air therein to form an inert atmosphere. Then, under an inert atmosphere, 0.305g of oxalic acid was added to the first mixture, and stirring was continued at 60°C for 30min to obtain a second mixture. Afterwards, 2.078g of triphenylphosphine was weighed and dissolved in 50mL of 90% by weight ethanol aqueous solution, and then added to the second mixture, and reacted for 60min under nitrogen atmosphere and stirring at 60°C to obtain a material containing triphenylphosphine iridium chloride.

[0061] (2) To the system after the reaction in step (1), 50 mL of 2M hydrochloric acid-ethanol solution and 4.2 g of 40 wt % formaldehyde solution were added in sequence, and the mixture was reacted at 80° C. for 30 min under stirring, and a precipitate was gradually generated in the solution to obtain a material containing triphenylphosphinecarbonyliridium chloride.

[0062] (3) Filter the reacted material in step (2), discard the filtrate, and collect the filter cake. Dissolve the filter cake in 100 mL of acetone to obtain an acetone solution of triphenylphosphine carbonyl halide, and introduce nitrogen into the above solution to replace the air (normal pressure) therein to form an inert atmosphere. Then, add 3.2 mL of N,N-dimethylformamide and 4.6 mL of acetylacetone to the above solution, heat to reflux, and react for 10 hours. Remove the solvent by filtration under reduced pressure while hot, wash the filter cake with 200 mL of distilled water and 100 mL of ethanol in turn, and vacuum dry at 70°C for 7 hours to obtain 1.457 g of iridium complex.

[0063] The elemental analysis results show that the yield of the iridium complex is 49.3% based on the iridium element, and the weight content of the chlorine element is 166 ppm.

[0064] Example 3

[0065] (1) In a 2L three-necked flask, 50.365g of IrCl3·3H2O was dissolved in 500mL of 95% by weight ethanol aqueous solution, heated to 80°C, fully dissolved, and mixed to obtain a first mixture. Then, nitrogen (normal pressure) was continuously introduced into the first mixture at a flow rate of 150mL / min to replace the air therein to form an inert atmosphere. Then, under an inert atmosphere, 8.005g of oxalic acid was added to the first mixture, and stirring was continued at 80°C for 30min to obtain a second mixture. Afterwards, 50.798g of triphenylphosphine was weighed and dissolved in 1000mL of 95% by weight ethanol aqueous solution, and then added to the second mixture, and reacted for 60min under nitrogen atmosphere and stirring at 80°C to obtain a material containing triphenylphosphine iridium chloride.

[0066] (2) To the system after the reaction in step (1), 350 mL of 5 M hydrochloric acid-ethanol solution and 110 g of 40 wt % formaldehyde solution were added in sequence, and the mixture was reacted at 80° C. for 60 min under stirring, and a precipitate was gradually generated in the solution to obtain a material containing triphenylphosphinecarbonyliridium chloride.

[0067] (3) Filter the reacted material in step (2), discard the filtrate, and collect the filter cake. Dissolve the filter cake in 1000 mL of acetone to obtain an acetone solution of triphenylphosphine carbonyl halide, and introduce nitrogen into the above solution to replace the air (normal pressure) therein to form an inert atmosphere. Then, add 150 mL of N,N-dimethylformamide and 175 mL of acetylacetone to the above solution, heat to reflux, and react for 15 hours. Remove the solvent by filtration under reduced pressure while hot, wash the filter cake with 2000 mL of distilled water and 1000 mL of ethanol in turn, and vacuum dry at 80°C for 5 hours to obtain 29.03 g of iridium complex.

[0068] The elemental analysis results show that the yield of the iridium complex is 51% based on the iridium element, and the weight content of the chlorine element is 182 ppm.

[0069] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for preparing an iridium-containing complex, characterized in that: The steps include: (1) contacting an iridium compound containing a halogen atom with triphenylphosphine in the presence of a first solvent to obtain a triphenylphosphine halide of iridium; (2) reacting formaldehyde with the iridium triphenylphosphine halide in the presence of hydrochloric acid to obtain iridium triphenylphosphine carbonyl halide; (3) in the presence of a second solvent, heating acetylacetone and the iridium triphenylphosphine carbonyl halide to react; Wherein, in step (1), the iridium compound containing halogen atoms is selected from at least one of iridium chloride, iridium tetrachloride, iridium iodide, iridium bromide, iridium chloride hydrate, iridium tetrachloride hydrate, iridium iodide hydrate and iridium bromide hydrate; Wherein, in step (1), the contacting conditions further include: being carried out in the presence of an acid, wherein the acid is selected from formic acid and / or oxalic acid; The molar ratio of the acid to the iridium compound containing halogen atoms is (0.1-1.5): 1, and the molar amount of the iridium compound containing halogen atoms is calculated based on iridium element.

2. The method according to claim 1, wherein: In step (1), the iridium compound containing halogen atoms is selected from iridium chloride and / or iridium chloride hydrate.

3. The method according to claim 1 or 2, wherein: In step (1), the molar ratio of triphenylphosphine to the iridium compound containing halogen atoms is (1-20): 1, and the molar amount of the iridium compound containing halogen atoms is calculated based on iridium element.

4. The method according to claim 3, wherein: In step (1), the molar ratio of triphenylphosphine to the iridium compound containing halogen atoms is (2-10): 1, and the molar amount of the iridium compound containing halogen atoms is calculated based on iridium element.

5. The method according to any one of claims 1, 2 and 4, wherein: In step (1), the contacting conditions include: a temperature of 40-120° C., a pressure of 0.05-5 MPa, and a time of 0.2-10 h; and / or the contacting is carried out under an inert atmosphere, and the inert atmosphere is provided by replacing air with an inert gas, wherein the flow rate of the inert gas replacing air is 50-2500 mL / min relative to 50 g of the iridium compound containing halogen atoms to be reacted.

6. The method according to claim 5, wherein: In step (1), the contacting conditions include: temperature of 50-80°C, pressure of 0.1-1 MPa, and time of 0.5-5 h; And / or, the contacting is carried out under an inert atmosphere, and the inert atmosphere is provided by replacing air with an inert gas, wherein the flow rate of the inert gas replacing air is 80-500 mL / min relative to 50 g of the iridium compound containing halogen atoms to be reacted.

7. The method according to any one of claims 1, 2, 4 and 6, wherein: In step (1), the first solvent is a mixture of alcohol and water, Wherein, the weight percentage of alcohol in the first solvent is 50-99%; Wherein, the alcohol is selected from C1-C4 monohydric alcohol; Wherein, the usage amount of the first solvent is 2-50 mL relative to each gram of the iridium compound containing halogen atoms.

8. The method according to claim 7, wherein: In step (1), the first solvent is a mixture of alcohol and water, Wherein, the weight percentage of alcohol in the first solvent is 70-95%; Wherein, the alcohol is selected from at least one of methanol, ethanol, n-propanol and isopropanol; Wherein, the amount of the first solvent used is 5-25 mL relative to each gram of the iridium compound containing halogen atoms.

9. The method according to claim 8, wherein: In step (1), the alcohol is ethanol.

10. The method according to any one of claims 1, 2, 4, 6, 8 and 9, wherein: The acid is oxalic acid.

11. The method according to any one of claims 1, 2, 4, 6, 8 and 9, wherein: In step (2), the molar ratio of formaldehyde to iridium triphenylphosphine halide is (10-200): 1, the molar amount of iridium triphenylphosphine halide is calculated as iridium element; And / or, the molar ratio of hydrochloric acid to iridium triphenylphosphine halide is (2-50): 1, and the molar amount of the iridium triphenylphosphine halide is calculated based on iridium element.

12. The method according to claim 11, wherein: In step (2), the molar ratio of formaldehyde to iridium triphenylphosphine halide is (50-100): 1, the molar amount of iridium triphenylphosphine halide is calculated as iridium element; And / or, the molar ratio of hydrochloric acid to iridium triphenylphosphine halide is (5-10): 1, and the molar amount of iridium triphenylphosphine halide is calculated based on iridium element.

13. The method according to any one of claims 1, 2, 4, 6, 8, 9 and 12, wherein: The reaction conditions in step (2) include: temperature of 40-120° C., pressure of 0.05-5 MPa, and time of 0.5-10 h; And / or, in step (2), the reaction is carried out under an inert atmosphere, and the inert atmosphere is provided by nitrogen.

14. The method according to claim 13, wherein: The reaction conditions in step (2) include: temperature of 50-80°C, pressure of 0.1-1 MPa, and time of 0.5-5 h; And / or, in step (2), the reaction is carried out under an inert atmosphere, and the inert atmosphere is provided by nitrogen.

15. The method according to any one of claims 1, 2, 4, 6, 8, 9, 12 and 14, wherein: In step (3), the conditions of the heating reaction include: temperature of 90-200° C., pressure of 0.05-5 MPa, and time of 2-30 h; And / or, the heating reaction is carried out under an inert atmosphere, and the inert atmosphere is provided by nitrogen.

16. The method according to claim 15, wherein: In step (3), the conditions of the heating reaction include: temperature of 120-180° C., pressure of 0.1-1 MPa, and time of 5-15 h; And / or, the heating reaction is carried out under an inert atmosphere, and the inert atmosphere is provided by nitrogen.

17. The method according to any one of claims 1, 2, 4, 6, 8, 9, 12, 14 and 16, wherein: In step (3), the amount of acetylacetone used is 1-20 mL per gram of iridium triphenylphosphine carbonyl halide calculated as iridium element.

18. The method according to claim 17, wherein: In step (3), the amount of acetylacetone used is 5-10 mL per gram of iridium triphenylphosphine carbonyl halide calculated as iridium element.

19. The method according to any one of claims 1, 2, 4, 6, 8, 9, 12, 14, 16 and 18, wherein: In step (3), the amount of the second solvent can be 5-200 mL per gram of the iridium triphenylphosphine carbonyl halide; And / or, the heating reaction may also be carried out in the presence of N,N-dimethylformamide, with the amount of N,N-dimethylformamide being 0.5-20 mL per gram of the iridium triphenylphosphine carbonyl halide.

20. The method according to claim 19, wherein: In step (3), the amount of the second solvent can be 20-100 mL per gram of the iridium triphenylphosphine carbonyl halide, wherein the second solvent is acetone; And / or, the heating reaction may also be carried out in the presence of N,N-dimethylformamide, with the amount of N,N-dimethylformamide being 2-10 mL per gram of the iridium triphenylphosphine carbonyl halide.