All-solid-state lithium-ion secondary battery and leakage inspection method using the same

By pre-setting the concave-convex structure on the packaging film of the all-solid-state lithium-ion secondary battery, the problem of being unable to detect leaks under vacuum packaging is solved, enabling fast and simple leak inspection, improving detection accuracy and ensuring battery durability.

CN114639865BActive Publication Date: 2024-10-25HONDA MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111534391.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-12-16
Filing Date
2021-12-15
Publication Date
2024-10-25
Estimated Expiration
2041-12-15

AI Technical Summary

Technical Problem

It is difficult to quickly and simply perform leakage inspection of all-solid-state lithium-ion secondary batteries with the existing technology, especially when leakage cannot be detected under vacuum packaging conditions.

Method used

Pre-set concave and convex structures on the packaging film, and measure their displacement before and after vacuum packaging to determine the location for leakage inspection, thereby achieving fast and simple leakage detection.

Benefits of technology

The pre-set concave and convex structure can effectively detect the leakage of the battery packaging film, improving the detection accuracy and speed without affecting the durability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114639865B_ABST
    Figure CN114639865B_ABST
Patent Text Reader

Abstract

The problem to be solved by the present invention is to provide an all-solid-state lithium-ion secondary battery that can be quickly and easily inspected for leakage. In order to solve the above problem, the present invention provides an all-solid-state lithium-ion secondary battery, comprising: an electrode laminate, which is formed by alternating laminations of a positive electrode, a solid electrolyte layer, and a negative electrode; a tab cluster extending from the electrode; and a packaging film, which packages the electrode laminate and the tab cluster; and the electrode laminate and the tab cluster are vacuum-packaged by the packaging film. For example, there is an inspection recess formed by following the inspection recess formed on the surface of the electrode laminate side by the packaging film, and by measuring the displacement of the inspection recess, the all-solid-state lithium-ion secondary battery can be inspected for leakage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an all-solid-state lithium-ion secondary battery and a leakage inspection method using the all-solid-state lithium-ion secondary battery. Background Art

[0002] In the past, lithium-ion secondary batteries were widely used as secondary batteries with high energy density. Liquid lithium-ion secondary batteries have a battery cell structure in which a separator is present between the positive electrode and the negative electrode and a liquid electrolyte (electrolyte) is filled. In addition, in the case of an all-solid-state battery in which the electrolyte is solid, there is a battery cell structure in which a solid electrolyte is present between the positive electrode and the negative electrode. Multiple single battery cells are laminated to form a lithium-ion secondary battery. These single battery cells are all sealed and packaged by a packaging film (hereinafter, this state is also referred to as a laminated battery cell). The sealing degree of the laminated battery cell needs to be ensured by a leak check.

[0003] In a lithium-ion secondary battery with a liquid electrolyte, although it is sealed by a packaging film, the interior is not in a vacuum state. Therefore, by placing the packaged battery cells in a vacuum state, detecting the gas contained therein, or confirming whether the laminated battery cells have expanded in volume, a leak test can be performed, that is, the presence of cracks or pinholes in the packaging film can be detected (see Patent Document 1).

[0004] On the other hand, in the case of an all-solid lithium ion secondary battery, no gas is generated inside, and there is a problem that since the battery is vacuum packaged, the packaged battery cell is placed in a vacuum state and leakage inspection cannot be performed.

[0005] In this regard, it is also known to perform appearance inspection by capturing convexities or concavities generated on a battery packaging film as an image (see Patent Document 2).

[0006] [Prior technical literature]

[0007] (Patent Document)

[0008] Patent Document 1: Japanese Patent Application Publication No. 2019-039772

[0009] Patent Document 2: Japanese Patent Application Publication No. 2015-065178 Summary of the invention

[0010] [Problems to be solved by the invention]

[0011] The appearance inspection disclosed in Patent Document 2 requires image inspection of the entire battery cell without omission, which results in much wasted effort. Also, since bulges or depressions may not necessarily occur during leakage inspection, appearance inspection is not a suitable inspection method for leakage inspection.

[0012] The present invention has been made in view of the above, and an object of the present invention is to provide an all-solid-state lithium-ion secondary battery and a method for inspecting the battery for leakage that can be quickly and easily inspected.

[0013] The inventors found that by intentionally providing unevenness for leak detection on the packaging film and inspecting it before and after vacuum packaging, the leak detection location can be determined and leaks can be visually detected, thereby completing the present invention. That is, the present invention provides the following.

[0014] (1) An all-solid-state lithium-ion battery comprising:

[0015] A solid-state battery comprises an electrode laminate formed by alternately laminating a positive electrode, a solid electrolyte layer and a negative electrode, and a tab bundle portion extending from one end of each electrode and bundling a plurality of extending portions; and

[0016] A packaging film for housing the solid-state battery; and

[0017] The solid-state battery is vacuum-packed by the packaging film.

[0018] On the surface of the packaging film, one or both of the following parts are formed:

[0019] an inspection recess of the packaging film formed by the packaging film following the recess formed on the surface side of the solid-state battery;

[0020] The remaining portion of the packaging film is folded back in a ring shape with respect to the front surface side of the solid-state battery to form a rib-shaped inspection protrusion.

[0021] According to the invention of (1), by checking the displacement of the inspection concave portion or the inspection convex portion provided in advance before and after vacuum packaging, leakage inspection can be performed simply and quickly.

[0022] (2) The all-solid lithium ion secondary battery according to (1), wherein the inspection recess and / or the inspection protrusion are formed at a position covering the tab gathering portion.

[0023] According to the invention of (2), since the space at the position covering the tab cluster is larger than other positions, the displacement of the inspection recess or inspection convex portion is larger, so it is more preferred. In addition, since it is a position that does not affect the restraint of the laminated battery cell, it does not affect the durability of the battery, so it is preferably used.

[0024] (3) The all-solid lithium ion secondary battery according to (1) or (2), wherein a plurality of the inspection recesses and / or the inspection protrusions are provided.

[0025] According to the invention of (3), by installing the device at multiple locations, the inspection accuracy can be improved.

[0026] (4) The all-solid-state lithium-ion secondary battery according to any one of (1) to (3), wherein the electrode includes a current collector composed of a metal porous body,

[0027] The inspection recessed portion and / or the inspection convex portion are formed along the recessed portion and / or convex portion formed in the current collector.

[0028] According to the invention of (4), the porous metal body can easily form a concave portion for inspection or a convex portion for inspection due to its three-dimensional structure and elasticity.

[0029] (5) The all-solid lithium ion secondary battery according to any one of (1) to (4), wherein a protection member is formed between the inspection recess and / or the inspection projection and the tab gathering portion.

[0030] According to the invention of (5), by providing the protective member as the intermediate layer, it is possible to prevent the current collector foil or the packaging film from being damaged due to displacement of the unevenness of the packaging film.

[0031] (6) The all-solid lithium ion secondary battery according to (5), wherein recessed portions and / or projecting portions are formed on a surface of the protection member.

[0032] According to the invention of (6), the position of the inspection concave portion or the inspection convex portion can be clearly identified in advance.

[0033] (7) The all-solid lithium ion secondary battery according to (6), wherein the elastic modulus of the protective member is smaller than the elastic modulus of the surface of the electrode laminate.

[0034] According to the invention of (7), by reducing the elastic modulus of the protective member, that is, by increasing the deformation of the protective member and softening it, it is possible to prevent the collector foil or the packaging film from being damaged.

[0035] (8) A method for detecting leakage of an all-solid-state lithium-ion secondary battery, for determining whether there is leakage during vacuum packaging, comprising:

[0036] The first step is to vacuum-pack the solid-state battery using a packaging film, wherein the solid-state battery comprises an electrode laminate formed by alternately laminating a positive electrode, a solid electrolyte layer and a negative electrode, and a tab bundling portion extending from one end of each electrode and bundling a plurality of extending portions; and

[0037] At least one of the following first inspection step and second inspection step,

[0038] The first inspection step is to form a recessed portion on the surface side of the solid-state battery before the first step, and in the first step, the packaging film follows the recessed portion, and after the first step, the release degree of the packaging film following the recessed portion is measured as the displacement of the inspection recessed portion;

[0039] The second inspection step is to form a spatial rib having a space inside on the surface side of the solid-state battery by folding back the remaining part of the packaging film before the first step, and in the first step, the packaging film forms an inspection convex portion by reducing the space, and after the first step, the displacement of the inspection convex portion is measured.

[0040] According to the invention of (8), by measuring the displacement of the inspection concave portion or the inspection convex portion provided in advance before and after vacuum packaging, leakage inspection can be performed simply and quickly. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 It is a partial cross-sectional schematic diagram of one embodiment of the lithium ion secondary battery of the present invention using a foamed metal current collector.

[0042] Figure 2 In the first embodiment Figure 1 An enlarged cross-sectional view of the vicinity of the lug clustering portion.

[0043] Figure 3 In the second embodiment Figure 1 An enlarged cross-sectional view of the vicinity of the lug clustering portion.

[0044] Figure 4 It is an enlarged cross-sectional view showing a first modification example.

[0045] Figure 5 It is an enlarged cross-sectional view showing a second modification example.

[0046] Figure 6 1 is a schematic cross-sectional view showing a third modified example.

[0047] Figure 7 yes Figure 6 An enlarged cross-sectional view of the vicinity of the lug clustering portion.

[0048] Figure 8 It is a schematic cross-sectional view showing a fourth modification example. DETAILED DESCRIPTION

[0049] Hereinafter, one embodiment of the present invention will be described with reference to the drawings. The content of the present invention is not limited to the description of the following embodiment.

[0050] [First embodiment]

[0051] <Overall structure of lithium-ion secondary battery>

[0052] like Figure 1 As shown, the present embodiment Figure 1 The lithium-ion secondary battery 100 is an all-solid-state battery, and includes an electrode laminate 50 in which positive electrodes 10 , solid electrolyte layers 30 , and negative electrodes 20 are alternately laminated.

[0053] The electrode tab bundling part 65 is included. The electrode tab bundling part 65 is led out from one end of the current collector of each electrode of the electrode laminate 50 and is reduced in diameter, and then a plurality of extensions are bundled. The electrode laminate 50 and the electrode tab bundling part 65 are taken as a whole to form a solid-state battery 80. Figure 1 As shown, the tab clustering portion 65 is a portion where multiple tabs 60 extending from one end of the current collector are overlapped to form a bundle so as to be joined to the lead tab 90. The lead tab 90 is electrically connected to one end of the tab clustering portion 65. In this embodiment, the tab 60 only needs to be led out from each electrode current collector. That is, the tab clustering portion 65 can be a component extending from each current collector, or a component different from the current collector. The material that can be used for the tab clustering portion 65 is not particularly limited, and the same material as the existing component used for secondary batteries can be used.

[0054] In the present invention, the electrode current collector may be a current collector foil or a current collector using a porous metal body. In the following embodiments, an example in which a porous metal body is used as the electrode current collector will be described.

[0055] After the electrode laminate 50 and the tab assembly 65 are housed in a bag-shaped packaging film 70 made of a laminate film, the opening 75 is heat-sealed and sealed using a conventional well-known vacuum packaging method (see Figure 1 In addition, Figure 1 The left end of the electrode laminate 50 is actually sealed by the packaging film 70. Figure 1 Omitted in .

[0056] The components constituting these are described below.

[0057] <Positive and negative electrodes>

[0058] In this embodiment, the positive electrode 10 and the negative electrode 20 are each composed of a metal porous body having mutually continuous pores (interconnected pores), and include a first current collector 11 and a second current collector 21 .

[0059] The holes of the first current collector 11 and the second current collector 21 are filled with an electrode composite material (positive electrode composite material) and an electrode composite material (negative electrode composite material) containing an electrode active material, respectively. In contrast, the tab clustering portion 65 and the lead tab 90 are unfilled areas where the electrode composite material is not filled.

[0060] (Current Collector)

[0061] The first current collector 11 constituting the positive electrode current collector and the second current collector 21 constituting the negative electrode current collector are composed of a metal porous body having mutually continuous pores. Since the first current collector 11 and the second current collector 21 have mutually continuous pores, the positive electrode composite material and the negative electrode composite material containing the electrode active material can be filled inside the pores, thereby increasing the amount of electrode active material per unit area of ​​the electrode layer. As the above-mentioned metal porous body, there is no particular limitation as long as it has mutually continuous pores, and examples thereof include foamed metal, metal mesh, expanded metal, punched metal, metal non-woven fabric, etc. having pores formed by foaming.

[0062] As the metal used in the metal porous body, as long as it has conductivity, there is no particular limitation, and examples thereof include nickel, aluminum, stainless steel, titanium, copper, silver, etc. Among these, foamed aluminum, foamed nickel, and foamed stainless steel are preferred as the current collector constituting the positive electrode, and foamed copper and foamed stainless steel can be preferably used as the current collector constituting the negative electrode.

[0063] By using the first current collector 11 and the second current collector 21, the amount of active material per unit area of ​​the electrode can be increased, and as a result, the volume energy density of the lithium-ion secondary battery can be improved. In addition, since the fixation of the positive electrode composite material and the negative electrode composite material becomes easy, unlike the electrode using the existing metal foil as the collector, when the electrode composite material layer is thickened, it is not necessary to thicken the coating slurry forming the electrode composite material layer. Therefore, the binder of the organic polymer compound required for thickening can be reduced. Therefore, the capacity per unit area of ​​the electrode can be increased, and the high capacity of the lithium-ion secondary battery can be achieved.

[0064] (Electrode Composite Materials)

[0065] The positive electrode composite material and the negative electrode composite material are respectively disposed in the pores formed inside the first current collector 11 and the second current collector 21. The positive electrode composite material and the negative electrode composite material must contain a positive electrode active material and a negative electrode active material, respectively.

[0066] (Electrode Active Material)

[0067] The positive electrode active material is not particularly limited as long as it can absorb and release lithium ions, and examples thereof include LiCoO2, Li(Ni5 / 10 Co 2 / 10 Mn 3 / 10 )O2、Li(Ni 6 / 10 Co 2 / 10 Mn 2 / 10 )O2、Li(Ni 8 / 10 Co 1 / 10 Mn 1 / 10 )O2、Li(Ni 0.8 Co 0.15 Al 0.05 )O2、Li(Ni 1 / 6 Co 4 / 6 Mn 1 / 6 )O2、Li(Ni 1 / 3 Co 1 / 3 Mn 1 / 3 )O2, LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, sulfur, etc.

[0068] The negative electrode active material is not particularly limited as long as it can absorb and release lithium ions, and examples thereof include metallic lithium, lithium alloys, metal oxides, metal sulfides, metal nitrides, Si, SiO, and carbon materials such as artificial graphite, natural graphite, hard carbon, and soft carbon.

[0069] (Other ingredients)

[0070] The electrode composite material may also arbitrarily include other components other than the electrode active material and the ion conductive particles. As other components, there is no particular limitation, as long as they are components that can be used when making lithium ion secondary batteries. For example, conductive aids, binders, etc. can be listed. As conductive aids for the positive electrode, acetylene black, etc. can be exemplified, and as binders for the positive electrode, polyvinylidene fluoride, etc. can be exemplified. As binders for the negative electrode, sodium carboxymethylcellulose, styrene butadiene rubber, sodium polyacrylate, etc. can be exemplified.

[0071] (Method for manufacturing positive electrode and negative electrode)

[0072] The positive electrode 10 and the negative electrode 20 are obtained by filling the electrode composite material in the pores of a metal porous body having mutually continuous pores as a current collector. First, the electrode active material, and a binder and an auxiliary agent as required are uniformly mixed by a conventionally known method to obtain an electrode composite material composition adjusted to a specified viscosity, preferably in a slurry state.

[0073] Then, the electrode composite material composition is used as an electrode composite material and filled into the pores of the metal porous body as a current collector. The method of filling the current collector with the electrode composite material is not particularly limited, and the following method can be cited, for example: using a plunger die coater, applying pressure, and filling the pores of the current collector with a slurry containing the electrode composite material. In addition to the above, the ion conductor layer can also be impregnated into the interior of the metal porous body by impregnation.

[0074] In the present invention, the current collector is not limited to the metal porous body, and a conventionally known metal foil etc. can be used. The metal used for the metal foil can be the same as that for the above-mentioned metal porous body.

[0075] <Solid electrolyte layer>

[0076] like Figure 1 As shown, in the present invention, a solid electrolyte layer 30 is preferably formed between the positive electrode 1 and the reference electrode 3 and / or between the reference electrode 3 and the negative electrode 20 .

[0077] The solid electrolyte constituting the solid electrolyte layer 30 is not particularly limited, and examples thereof include: sulfide-based solid electrolyte materials, oxide-based solid electrolyte materials, nitride-based solid electrolyte materials, and halide-based solid electrolyte materials. As sulfide-based solid electrolyte materials, for example, if it is a lithium-ion battery, LPS-based halogens (Cl, Br, I), and Li2S-P2S5, Li2S-P2S5-LiI, etc. can be listed. In addition, the above-mentioned "Li2S-P2S5" refers to a sulfide-based solid electrolyte material made using a raw material composition containing Li2S and P2S5, and other records are the same. As oxide-based solid electrolyte materials, for example, if it is a lithium-ion battery, sodium superionic conductor (Na superionicconductor, NASICON) type oxides, garnet-type oxides, perovskite-type oxides, etc. can be listed. As NASICON-type oxides, for example, oxides containing Li, Al, Ti, P and O (such as Li 1.5 Al 0.5 Ti 1.5 (PO4)3). Examples of garnet-type oxides include oxides containing Li, La, Zr, and O (e.g., Li7La3Zr2O 12 ). Examples of perovskite-type oxides include oxides containing Li, La, Ti, and O (eg, LiLaTiO 3 ).

[0078] <Packaging film>

[0079] The packaging film 70 is a packaging body that is closely attached to the electrode laminate 50 by vacuum packaging and houses the electrode laminate 50 and the tab assembly 65. By hermetically housing the solid-state battery 80, it is possible to prevent atmospheric air from entering the solid-state battery 80.

[0080] The packaging body is formed by forming the packaging film 70 into a bag shape. The packaging film 70 is preferably a film that can provide airtightness as the packaging body. The packaging film 70 may be a single-layer film or a laminate composed of a plurality of layers.

[0081] The packaging film 70 preferably includes a barrier layer made of, for example, a metal foil such as aluminum, a metal thin film such as aluminum, an inorganic oxide thin film such as silicon oxide or aluminum oxide, etc. The packaging film 70 including the barrier layer can provide airtightness as a packaging body.

[0082] The packaging film 70 preferably includes a sealing layer made of a thermoplastic resin such as a polyethylene resin or a polypropylene resin. The films can be joined together by making the sealing layers laminated on the films face each other and welded. Therefore, there is no need for a step of applying an adhesive. In addition, the packaging film 70 may not include a sealing layer. The packaging body may also be formed by joining the films together using an adhesive.

[0083] As the packaging film 70, a laminated body formed by laminating a base layer made of polyethylene terephthalate, polyethylene naphthalate, nylon, polypropylene, etc., the barrier layer, and the sealant layer can be exemplified. These layers can be laminated via a conventionally known adhesive or by extrusion coating.

[0084] The preferred thickness of the packaging film 70 varies depending on the material used for the film, but is preferably 50 μm or more, and more preferably 100 μm or more. The preferred thickness of the packaging film 70 is preferably 700 μm or less, and more preferably 200 μm or less. Within this range, film strength and flexibility can be achieved, and the inspection concave portion 71, the inspection convex portion 72, and the inspection convex compressed portion 52 of the packaging film 70 described below can be easily formed.

[0085] Next, the inspection recess 71 of the packaging film 70 which is a feature of the present invention will be described. Figure 2 In the first embodiment Figure 1 An enlarged cross-sectional view of the vicinity of the lug clustering portion. Figure 2 (a) is the state of correct vacuum packaging, that is, the state of qualified products. Figure 2 (b) is a state where the vacuum degree is low and leakage occurs, that is, a defective product state.

[0086] A plurality of recesses 61 are formed in advance on the tab 60 of the tab clustering portion 65, two recesses in this embodiment. The recesses 61 can be formed, for example, by shaping the current collector made of the above-mentioned porous metal body.

[0087] In this embodiment, the concave portion 61 and the convex portion 62 described below refer to the surface concave and convex portions formed on the tab 60 of the tab clustering portion 65. On the other hand, the inspection concave portion 71 and the inspection convex portion 72 described below refer to the surface concave and convex portions viewed from the packaging film 70 side, and the two should be distinguished.

[0088] The size of the inspection recess 71 is preferably Figure 2 In the state of closely following (a), the diameter when converted into a circle in a plan view is 0.1 mm to 10 mm, and the depth from the deepest part of the depression is preferably 0.01 mm to 1 mm.

[0089] The actual leakage inspection method will be described in detail below in order. First, as described above, in the solid-state battery 80 , the recessed portion 61 is formed in advance on the surface of the tab 60 of the tab clustering portion 65 .

[0090] Next, the packaging film 70 is formed into a bag shape having an opening 75 by heat sealing or the like to produce a packaging body (packaging bag). Then, the solid-state battery 80 is housed in the packaging body. Figure 2 As shown in (b), the packaging film 70 is flat and does not follow and fit tightly into the concave portion 61. Figure 2 In (b), the pre-inspection flat surface portion 71a is formed, but the defect inspection recessed portion 71a is formed later.

[0091] Next, in the first step, the opening 75 is sealed and packaged by heat sealing or the like in a vacuum state to obtain a vacuum package. The vacuum packaging can be performed using an existing well-known vacuum packaging machine. At this time, the interior of the package body formed by the packaging film 70 is vacuum, such as Figure 2 As shown in (a), when vacuum packaging is correctly performed, the packaging film 70 follows and adheres to the recess 61, thereby forming an inspection recess 71. And if the vacuum state can be maintained, the following is also maintained after exposure to the atmosphere. That is, the lithium ion secondary battery 100 has an inspection recess 71 on the surface of the packaging film 70 covering the vicinity of the tab clustering portion 65. This is the state of a qualified product.

[0092] Here, if there is a defect such as a pinhole in the packaging film 70 or any of its packaging bodies, the vacuum state cannot be maintained when it is exposed to the atmosphere after vacuum packaging, and then it is released and restored to its original state. Figure 2 (b) shows a flat state of the defect inspection recess 71a, that is, a state where the defect inspection recess 71a does not follow the close contact.

[0093] Here, in the first inspection step, by measuring the displacement of the inspection recess 71 of the packaging film 70, specifically, by measuring the displacement from the inspection recess 71 to the defect inspection recess 71a, the leakage inspection of the lithium ion secondary battery 100 can be simply and quickly performed. If the displacement is 0 or smaller, it is a qualified product, and if the displacement is larger, it is a defective product.

[0094] The displacement can be measured by the height of the depression, the size (area) of the depression, the slope of the depression, or a combination of these or image processing. In the present invention, since the inspection recess 71 is a predetermined position, leakage determination can be performed only by measuring the inspection point.

[0095] In addition, the measurement in the present invention includes not only measurement by instruments such as images or lasers, but also determination by visual inspection. Furthermore, in the pass / fail determination criteria of the displacement amount, in addition to the presence or absence of depression, the value of a predetermined depression amount can also be used as a threshold value for the pass / fail determination criteria.

[0096] The inspection recess 71 and the inspection convex portion 72 described below in the present invention are "the surface side of the solid-state battery", so it means that in addition to being formed on the tab clustering portion 65 as in the present embodiment, it can also be formed on the surface of the electrode laminate 50, and can also be formed on the surface of the protective member 80 described below, but it is preferably formed on the surface of the packaging film 70 covering the tab clustering portion 65. At the position covering the tab clustering portion, the space inside the tab clustering portion 65 is larger than other parts, so the displacement of the inspection recess or the inspection convex portion is larger, so it is more preferred. In addition, since it is a position that does not affect the constraint of the laminated battery cell, it does not affect the durability of the battery, so it is preferably adopted.

[0097] It is preferable to provide a plurality of inspection recesses 71 and inspection protrusions 72 described below. Inspection accuracy can be improved by providing them at a plurality of locations.

[0098] The inspection recesses 71 and the inspection protrusions 72 described below are preferably formed in the recesses 61 or protrusions 62 on the surface of the current collector made of a porous metal body. The porous metal body can easily form inspection recesses or inspection protrusions due to its three-dimensional structure and elasticity.

[0099] [Second embodiment]

[0100] Figure 3 In the second embodiment Figure 1 This embodiment is an example in which a protruding portion 72 for inspection is formed instead of a recessed portion 71 for inspection. Hereinafter, the same reference numerals are attached to the same configurations as those in the first embodiment and their description is omitted.

[0101] Figure 3 In the second embodiment Figure 1 An enlarged cross-sectional view of the vicinity of the lug clustering portion. Figure 3 (a) is the state of correct vacuum packaging, that is, the state of qualified products. Figure 3 (b) is a state where the vacuum degree is low and leakage occurs, that is, a defective product state.

[0102] The actual leakage inspection method is described in detail below in order. In this embodiment, in the solid-state battery 80, the concave and convex parts are not formed in advance on the tab 60 of the tab clustering part 65. Figure 3 The planned inspection portion 74 in (b) is composed of a flat portion.

[0103] Next, the packaging film 70 is formed into a bag shape having an opening 75 by heat sealing or the like to produce a packaging body (packaging bag). Then, the solid-state battery 80 is housed in the packaging body. Figure 3 As shown in (b), a rib-shaped inspection front protrusion 72a (later detected as a defective inspection protrusion 72) is pre-formed on the inspection scheduled portion 74 which is a part of the surface of the tab 60 of the solid-state battery 80. The inspection front protrusion 72a is formed by folding the remaining portion of the packaging film 70 back into a substantially triangular shape and having a space 73a inside. The inspection front protrusion 72a may be pre-formed on the packaging film 70 by embossing or the like, or may be formed when the packaging film 70 is stored.

[0104] Next, in the first step, the opening 75 is sealed and packaged by heat sealing or the like under vacuum to obtain a vacuum package. At this time, in the inspection front convex portion 72a, the interior of the package formed by the packaging film 70 is vacuum, as shown in FIG. Figure 3 As shown in (a), the space 73a is shrunk by vacuuming to form the unbonded close-fitting portion 73, and the remaining portion of the packaging film 70 is folded back into a ring to form a rib-shaped inspection convex portion 72. And if the vacuum state can be maintained, the inspection convex portion 72 can also be maintained after being exposed to the atmosphere. That is, the lithium-ion secondary battery 100 has the inspection convex portion 72 on the surface of the packaging film 70 covering the vicinity of the tab clustering portion 65. This is the state of a qualified product.

[0105] Here, if there is a defect such as a pinhole in the packaging film 70 or its packaging body, the vacuum state cannot be maintained when it is exposed to the atmosphere after vacuum packaging, and the unbonded close contact portion 73 is released and restored. Figure 3 (b) is the state of the defect inspection protrusion 72a.

[0106] Here, in the second inspection step, by measuring the displacement of the inspection protrusion 72 of the packaging film 70, specifically, by measuring the displacement from the inspection protrusion 72 to the defect inspection protrusion 71a, the leakage inspection of the lithium ion secondary battery 100 can be simply and quickly performed. If the displacement is 0 or smaller, it is a qualified product, and if the displacement is larger, it is a defective product.

[0107] The displacement can be measured by the height of the convex portion, the extension (area) of the convex portion in the top view, the slope of the convex portion, or a combination of these or image processing. Among them, since the displacement of the convex area is large and easy to detect, it is more preferred. In the present invention, since the inspection convex portion 72 is a predetermined position, leakage determination can be performed only by measuring the inspection point.

[0108] exist Figure 3 In the state (a), the size of the inspection projection 72 is preferably such that the height of the projection is not less than 0.05 mm and not more than 5 mm.

[0109] [First Modification]

[0110] Figure 4 The following is an example: Figure 3 (b) The space 73a is not a complete space, and a convex portion 62 is formed on the surface of the current collector as a metal porous body at the position of the space 73a. Figure 4 (a) shows the inspection convex portion 76. In this case, Figure 4 As shown in (b), when there is a leak, the close contact of the packaging film 70 is loosened, resulting in the formation of a defect inspection convex portion 76a. In this embodiment, the position of the inspection convex portion is pre-defined, so it is more preferred. The convex portion 62 can be easily formed by embossing the surface of the collector.

[0111] In this case, Figure 4 In the state (a), the size of the inspection projection 76 is preferably such that the height of the projection is not less than 0.05 mm and not more than 10 mm.

[0112] [Second Modification]

[0113] Figure 5 In the first embodiment Figure 2 In the modification of (a), in this embodiment, a protective member 95 is provided as an intermediate layer between the packaging film 70 and the tab 60 .

[0114] At this time, if Figure 5As shown in FIG. 1 , when vacuum packaging is correctly performed, the packaging film 70 follows and is closely attached to the concave portion 91 of the protective member 95, thereby forming the inspection concave portion 71. In this embodiment, the position of the inspection convex portion is also predetermined, so it is more preferred. In addition, in this embodiment, the concave portion is formed on the surface of the protective member, but it is not limited to this, and a convex portion may also be formed.

[0115] Thus, by configuring the protective member 95 as an intermediate layer, it is possible to prevent the collector foil or the packaging film from being damaged due to displacement of the unevenness of the packaging film. In addition, when the collector is a porous metal body, it has a buffering effect itself, so the protective member 95 is particularly preferably used when the collector is a foil.

[0116] The elastic modulus of the protective member is preferably smaller than the elastic modulus of the electrode laminate surface. By reducing the elastic modulus of the protective member, that is, increasing the deformation of the protective member and softening it, it is possible to prevent the collector foil or packaging film from being damaged. As specific examples of the protective member, resins such as elastomers can be cited. The protective member can be formed not only as a formed member, but also by a coating. At this time, compared with a formed product, it can be configured more simply and the softness of the collector can be maintained.

[0117] [Third Modification]

[0118] Figure 6 The lithium ion secondary battery 100a is an example in which the above-mentioned metal porous body for the current collector is used as the protective member 95a. Figure 7 yes Figure 6 An enlarged view of the region V in . The recess 95b is a recess provided on the surface of the protective member 95a, which is the same as the recess 61 or the recess 91 described above. The metal porous body constituting the protective member 95a has a buffering effect on the external force applied to the lithium-ion secondary battery, so it is more preferred. In addition, when a metal porous body is also used in the collector, the surface concave-convex anchoring effect of the two laminated metal porous bodies can effectively prevent the lamination from being misaligned. Resin or the like can also be filled in the metal porous body of the protective member 95a. Thus, the strength can be improved.

[0119] In addition, the recessed portion 95b may be configured as a convex portion like the convex portion 62 of the first modification. Furthermore, in this embodiment, the current collector is not limited to a porous metal body, and a metal foil may be used.

[0120] [Fourth Modification]

[0121] Figure 8 The lithium-ion secondary battery 100b of the embodiment 1 is different from the first embodiment in that the current collector is not a metal porous body but is made of metal foil. Figure 8In the embodiment, the negative electrode composite material 21 a is disposed on both surfaces of the current collector foil 60 of the negative electrode, and the positive electrode composite material 11 a is disposed on both surfaces of the current collector foil 60 of the positive electrode.

[0122] In this embodiment, one end of the current collector foil 60 extends directly to form the tab 60, and a plurality of tabs 60 are stacked to form the tab assembly 65. As described above, the current collector in the present invention is not limited to a porous metal body, but may also be a metal foil.

[0123] As mentioned above, although the preferred embodiment of the present invention was described, the content of the present invention is not limited to the above-mentioned embodiment, and appropriate changes can be made.

[0124] Reference numerals

[0125] 10: Positive electrode

[0126] 11: First current collector (positive electrode current collector)

[0127] 11a: Positive electrode composite material

[0128] 20: Negative electrode

[0129] 21: Second current collector (positive electrode current collector)

[0130] 21a: Negative electrode composite material

[0131] 30: Solid electrolyte layer

[0132] 50: Electrode laminate

[0133] 60: Tab (current collector foil)

[0134] 61: concave part

[0135] 62: convex part

[0136] 65: Tab clustering unit

[0137] 70: Packaging film 70

[0138] 71: Inspection concave portion 71a: Fault inspection concave portion (inspection front flat portion) 72: Inspection convex portion 72a: Fault inspection convex portion (inspection front convex portion) 73: Unjoined close contact portion

[0139] 73a: Space

[0140] 74: Check the reservation department

[0141] 75: Opening

[0142] 76: Inspection convex portion 76a: Fault inspection convex portion (inspection front convex portion) 80: Solid-state battery

[0143] 90: Lead ear

[0144] 95, 95a: Protective components

[0145] 95b: concave part

[0146] 100, 100a, 100b: lithium ion secondary battery V: region

Claims

1. An all-solid-state lithium-ion battery having: A solid-state battery comprises an electrode laminate formed by alternately laminating a positive electrode, a solid electrolyte layer and a negative electrode, and a tab bundle portion extending from one end of each electrode and bundling a plurality of extending portions; and A packaging film for housing the solid-state battery; and The solid-state battery is vacuum-packed by the packaging film. The aforementioned all-solid-state lithium-ion battery is exposed to the atmosphere. On the surface of the packaging film, one or both of the following parts are formed: During vacuum packaging, a recessed portion for inspection of the packaging film for measuring displacement when exposed to the atmosphere is formed at a predetermined position by the packaging film following the recessed portion formed on the surface side of the solid-state battery; During vacuum packaging, the remaining portion of the packaging film is folded back into a ring shape relative to the surface side of the solid-state battery at a predetermined position to form a rib-shaped inspection protrusion for measuring displacement when exposed to the atmosphere. The displacement of the inspection concave portion and the inspection convex portion when exposed to the atmosphere after vacuum packaging is 0.

2. The all-solid-state lithium-ion secondary battery according to claim 1, wherein: The inspection recess and / or the inspection protrusion are formed at positions covering the tab clustering portion.

3. The all-solid-state lithium-ion secondary battery according to claim 1, wherein: A plurality of the inspection recesses and / or the inspection protrusions are provided.

4. The all-solid-state lithium-ion secondary battery according to claim 1, wherein: The electrode comprises a current collector composed of a porous metal body. The inspection recessed portion and / or the inspection convex portion are formed along the recessed portion and / or convex portion formed in the current collector.

5. The all-solid-state lithium-ion secondary battery according to claim 1, wherein: A protection member is formed between the inspection recess and / or the inspection projection and the tab gathering portion.

6. The all-solid-state lithium-ion secondary battery according to claim 5, wherein: Concave portions and / or convex portions are formed on the surface of the protection member.

7. The all-solid-state lithium-ion secondary battery according to claim 5, wherein: The protective member has an elastic modulus smaller than an elastic modulus of a surface of the electrode laminate.

8. A method for detecting leakage of an all-solid-state lithium-ion secondary battery, for determining whether there is leakage during vacuum packaging, comprising: The first step is to vacuum-pack the solid-state battery using a packaging film, wherein the solid-state battery comprises an electrode laminate formed by alternately laminating a positive electrode, a solid electrolyte layer and a negative electrode, and a tab bundling portion extending from one end of each electrode and bundling a plurality of extending portions; and At least one of the following first inspection step and second inspection step, The first inspection step is to form a recess on the surface side of the solid-state battery at a predetermined position before the first step, to form an inspection recess by making the packaging film follow the recess in the first step, and to measure the degree of release of the packaging film in the inspection recess when exposed to the atmosphere as the displacement of the inspection recess after the first step. The second inspection step is to form a spatial rib having a space inside by folding back the remaining part of the aforementioned packaging film at a predetermined position on the surface side of the aforementioned solid-state battery before the aforementioned first step, wherein in the aforementioned first step, the aforementioned packaging film forms an inspection protrusion by reducing the aforementioned space, and after the aforementioned first step, the displacement of the aforementioned inspection protrusion when exposed to the atmosphere is measured.