A core structure for an electric fusion bent pipe and a winding method for the core structure
By designing an intersecting and splicing core structure of the electrofusion bend pipe, using the characteristics of the stitching bend, positioning pins and limiting bumps, the problems of winding quality and fluid smoothness of the electrofusion bend pipe are solved, and stable and uniform winding is achieved. Wire density and high-quality resistive wire winding.
Patent Information
- Application Number
- CN202210331866.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-31
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-03-31
AI Technical Summary
The core structure of existing electromelting bevel pipes is difficult to ensure the quality of the winding, especially in terms of smooth fluid and tightness in the bevel pipes, and sharp edges can cause damage to the resistive wires.
A male and female die core structure that can be intersected and spliced together is designed. The male die core and female die are ensured by setting the aligned bevel and positioning pins, limit bumps and grooves at the splicing end. The core is coaxially connected and smoothly transition, thereby achieving stable and uniform winding density and avoiding contact between resistive lines and sharp edges.
High-quality winding of the electrofusion bend pipe is achieved, avoiding large deflection swings and damage to resistive wires, and improving winding efficiency and overall product quality.
Smart Images

Figure CN114669691B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of electric fusion pipe fitting moulds and relates to a core structure of an electric fusion bent pipe and a winding method of the core structure. Background Art
[0002] Electric fusion pipe fittings are plastic pipe fittings used for hot-melt connection of pipes. The structure of electric fusion pipe fittings mainly includes a plastic pipe body, a resistance wire arranged on the inner wall of the pipe body, and an electrode for electrifying the resistance wire. The welding principle is to melt the plastic material of the pipe fitting and the pipe to be connected by electrifying the resistance wire, and then the pipes are fused after connection. In addition to relying on the core and mold, the production of electric fusion pipe fittings also needs to consider the winding wiring of the resistance wire, and the wiring of electric fusion elbows is more difficult than that of traditional straight pipe heads.
[0003] A Chinese patent application with application publication number CN110056732A discloses a fully automatic electric fusion pipe wiring device, comprising a base plate, a pair of power ejector modules disposed opposite to each other on the base plate, a pair of core modules disposed opposite to each other fixed between the pair of power ejector modules disposed opposite to each other, a winding moving module disposed on the base plate, and a pair of stripping modules disposed on one side of the pair of core modules disposed opposite to each other. The enameled wire to be wound is evenly wound on the core module through the winding moving module, and the insulating layer of the end of the enameled wire is stripped by the stripping module.
[0004] The above structure can realize the winding and wiring of the right-angle electric fusion bend, but the winding is still achieved by winding the male mold core and the female mold core separately, which makes it difficult to ensure uniform and stable winding quality. In order to ensure the smooth flow of fluid in the bend and to ensure tight splicing, the outer periphery of the joint area of the male mold core and the female mold core is rounded and has sharp edges, just like the above mold core structure. The sharp edges of the non-intersecting male mold core and the female mold core will cause damage to the resistance wire wound to this area, affecting the winding quality. Summary of the invention
[0005] The present invention aims at the above problems existing in the prior art and provides a core structure for an electric fusion bent pipe. The technical problem to be solved by the present invention is: how to improve the winding quality of the electric fusion bent pipe.
[0006] The purpose of the present invention can be achieved by the following technical solutions:
[0007] A core structure for an electric fusion bent pipe comprises a male mold core and a female mold core that can intersect and splice, the splicing end of the male mold core having a splicing bevel 1, the splicing bevel 1 having a positioning pin arranged along the axial direction of the male mold core, the splicing end of the female mold core having a splicing bevel 2 and a positioning blind hole 1, when the positioning pin is inserted into the positioning blind hole 1 and the splicing bevel 1 and the splicing bevel 2 are made to fit together, the male mold core and the female mold core can form a bent pipe core, characterized in that the splicing end of the female mold core also has a positioning blind hole 2 arranged along the axial direction of the female mold core, when the male mold core and the female mold core are coaxially butt-jointed, the positioning pin can be inserted into the positioning blind hole 2 and the splicing bevel 1 and the splicing bevel 2 are made to fit together.
[0008] The male mold core and the female mold core can intersect and splice to form a bent tube core, which can be used in conjunction with the mold to achieve bent tube injection molding. At this time, the splicing bevel one and the splicing bevel two are aligned to make the outer circumference of the male mold core and the female mold core smoothly transition to ensure the quality of the pipe fittings. The locating pin on the splicing bevel one is plugged into the locating blind hole one at the splicing end of the female mold core. The setting direction of the locating blind hole one intersects with the axis of the female mold core and is related to the angle of the bent tube to be formed, ensuring that the female mold core and the male mold core will not separate along the axial direction of the female mold core after they are spliced. By setting a second positioning blind hole arranged along the axial direction of the female mold core at the splicing end of the female mold core, the positioning pin can be inserted into the second positioning blind hole when the male mold core and the female mold core are coaxially connected, and the splicing bevel one and the splicing bevel two are also fitted together. When the male mold core and the female mold core are wound in this state, it is beneficial for the winding device to complete the winding operation at one time, and ensure that the winding density of the male mold core and the female mold core is uniform and consistent; at the same time, the joint ends of the male mold core and the female mold core are limited to each other in the radial direction through the limit pin and the positioning blind hole two, ensuring that the male mold core and the female mold core can still ensure stable coaxial rotation under the traction force of the resistance wire during the winding process, avoiding large deflection swing and affecting the winding effect; and when the splicing bevel one and the splicing bevel two are fitted together, there will be a smooth transition area at the junction of the edges of the two, which is beneficial to the design that the resistance wire passing through this place will not be cut by the sharp edges of the splicing bevel one or the splicing bevel two, thereby ensuring the winding quality.
[0009] In the core structure of the above-mentioned electric fusion bending pipe, the first splicing inclined surface has a limiting convex block, the positioning pin is located on the limiting convex block, the second splicing inclined surface has a limiting groove, the first positioning blind hole and the second positioning blind hole are both located on the inner side wall of the limiting groove, and when the male mold core and the female mold core are coaxially docked, the limiting convex block is inserted into the limiting groove and is positioned and matched along the circumferential direction of the male mold core. In this way, the limiting convex block cooperates with the limiting groove to limit the relative rotation of the male mold core and the female mold core during the winding process, avoiding axial runout between the male mold core and the female mold core when the two ends of the male mold core are not firmly positioned, thereby affecting the winding effect.
[0010] In the core structure of the above-mentioned electric fusion bent pipe, the male mold core includes a winding segment 1 and a forming segment 1 arranged in sequence axially, and the splicing slope 1 is located on the forming segment 1. The female mold core includes a winding segment 2 and a forming segment 2 arranged in sequence axially, and the splicing slope 2 is located on the forming segment 2. The radial dimension of the forming segment 1 is smaller than the radial dimension of the winding segment 1, and an annular step surface 1 is formed between the forming segment 1 and the winding segment 1. The radial dimension of the forming segment 2 is smaller than the radial dimension of the winding segment 2, and an annular step surface 2 is formed between the forming segment 2 and the winding segment 2. The winding segment 1 and the winding segment 2 are high-density winding areas of the resistance wire, and the forming segment 1 and the forming segment 2 are mainly involved in the forming of the inner cavity of the pipe fitting. In this way, the corresponding setting of different radial dimensions is conducive to distinguishing and judging the winding modes of different areas, and ensuring the winding effect.
[0011] In the core structure of the above-mentioned electric fusion bending pipe, the annular step surface 1 has a slot 1 arranged along the length direction of the winding segment 1, the position of the slot 1 is opposite to the position of the splicing slope 1 closest to the annular step surface 1, and a wire clamping pin 1 is inserted in the slot 1; the annular step surface 2 has a slot 2 arranged along the length direction of the winding segment 2, the position of the slot 2 is opposite to the position of the splicing slope 2 closest to the annular step surface 2, and a wire clamping pin 2 is inserted in the slot 2. This is conducive to designing that the resistance wire on the forming segment 1 and the forming segment 2 starts to be wound from the position corresponding to the slot 1 or the slot 2. At this time, the winding direction of the resistance wire can be adapted to the edge extension direction of the splicing slope 1 or the splicing slope 2 to the greatest extent, reducing the probability of the resistance wire contacting the sharp edge and improving the winding quality. The wire clamping pin 1 and the wire clamping pin 2 installed later can ensure that the resistance wire on the winding segment 1 and the winding segment 2 will not be loosened during splicing and adjustment, thereby ensuring the winding quality of the product.
[0012] In the core structure of the above-mentioned electric fusion bending pipe, the forming section 1 is coaxially arranged with the winding section, and the forming section 2 is coaxially arranged with the winding section 2. This is conducive to ensuring the coaxiality of the male mold core and the female mold core after coaxial docking, reducing the eccentric load and position deviation during the rotation process, and ensuring the winding effect.
[0013] In the core structure of the above-mentioned electric fusion bending pipe, the end edge of the positioning pin, the edge of the limiting protrusion and the open edge of the limiting groove are all processed with rounded corners, which can improve the smoothness and convenience of the operation when the male mold core and the female mold core are connected and spliced.
[0014] A winding method for an electric fusion bending tube core structure comprises the following steps:
[0015] Step 1: Coaxially connect the male mold core and the female mold core, so that the positioning pin is plugged into the second positioning blind hole and the first and second splicing bevels are aligned;
[0016] Step 2: Place the male mold core and the female mold core that are coaxially connected on the rotating device of the winding equipment, and clamp the axial ends of the male mold core and the female mold core.
[0017] Step 3, wind one end of the resistance wire onto the winding segment 1 or the winding segment 2, control the male mold core and the female mold core to rotate coaxially, and at the same time control the mobile pay-off device of the winding equipment to move along the axial direction of the male mold core and the female mold core;
[0018] Step 4: When the resistance wire is wound to the area where the forming section 1 and the forming section 2 are located, the moving speed of the mobile pay-off device is increased or the rotating speed of the rotating device is reduced;
[0019] Step 5: After the male mold core and the female mold core are wound, the resistance wires on the winding section 1 and the winding section 2 are hot pressed by a hot head device;
[0020] Step 6: Insert the clamping pin 1 and the clamping pin 2 into the slot 1 and the slot 2 respectively to clamp the resistance wires in the corresponding areas, and take out the male mold core and the female mold core;
[0021] Step 7: Split the male mold core and the female mold core axially, rotate the male mold core or the female mold core in the opposite direction of the winding of the resistance wire and swing toward the intersection state at the same time, and finally intersect and splice the male mold core with the female mold core.
[0022] In this way, the male mold core and the female mold core are pre-axially butted together to form an axially and circumferentially stable whole. The winding operation is completed at one time through the winding device, which improves the efficiency and consistency of the winding quality. At the same time, the winding density is reduced in the non-working area, and the resistance wire margin during splitting can be guaranteed, so that the splicing operation after winding is smooth and reliable.
[0023] In the winding method of the above-mentioned electric fusion bending tube core structure, in the fourth step, the number of winding turns of the resistor wire in the forming section 1 and the forming section 2 is 1.5 turns, and the resistor wire is wound from the position on the forming section 1 opposite to the slot 1 to the position on the forming section 2 opposite to the slot 2. In this way, it can be ensured that when the resistor wire passes through the joint of the splicing inclined surface 1 and the splicing inclined surface 2, it is just a smooth transition area without being affected by sharp edges, thereby improving the winding quality.
[0024] Compared with the prior art, the advantages of the present invention are as follows:
[0025] The core structure of the electric fusion bent pipe is provided with a second positioning blind hole arranged along the axial direction of the female mold core at the splicing end of the female mold core, so that when the male mold core and the female mold core are coaxially connected, the positioning pin can be inserted into the second positioning blind hole and the splicing inclined surface 1 and the splicing inclined surface 2 can also be fitted. This is conducive to the winding device to complete the winding operation at one time, ensuring that the winding density of the male mold core and the female mold core is uniform; at the same time, it is avoided that large deflection swing affects the winding effect; and it is conducive to designing the resistance wire so that it is not cut by the sharp edges of the splicing inclined surface 1 or the splicing inclined surface 2, thereby ensuring the winding quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 Schematic diagram of the three-dimensional structure of the male mold core in this embodiment.
[0027] Figure 2 It is a schematic diagram of the three-dimensional structure of the female mold core in this embodiment.
[0028] Figure 3 It is a schematic diagram of the three-dimensional structure of the male mold core and the female mold core intersecting and splicing in this embodiment.
[0029] Figure 4 It is a schematic diagram of the three-dimensional structure of the coaxial docking of the male mold core and the female mold core in this embodiment.
[0030] Figure 5 It is a schematic cross-sectional structure diagram of the coaxial docking of the male mold core and the female mold core in this embodiment.
[0031] Figure 6 yes Figure 5 Enlarged view of part A in .
[0032] In the figure, 1, male mold core; 11, joint inclined surface 1; 111, positioning pin; 112, limiting protrusion; 12, winding section 1; 13, forming section 1; 14, annular step surface 1; 141, slot 1;
[0033] 2. Female mold core; 21. Splicing inclined surface 2; 211. Positioning blind hole 1; 212. Positioning blind hole 2; 213. Limiting groove; 22. Winding segment 2; 23. Forming segment 2; 24. Annular step surface 2; 241. Slot 2;
[0034] 3. Wire clamp pin one; 4. Wire clamp pin two. DETAILED DESCRIPTION
[0035] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0036] Embodiment 1:
[0037] like Figure 1-6As shown, the core structure of the electric fusion bent pipe comprises a male mold core 1 and a female mold core 2 which can be vertically spliced. The spliced end of the male mold core 1 has a spliced inclined surface 11, and the angle between the spliced inclined surface 11 and the axis of the male mold core 1 is 45 degrees. The spliced inclined surface 11 has a positioning pin 111 arranged along the axial direction of the male mold core 1. The spliced end of the female mold core 2 has a spliced inclined surface 21 and a positioning blind hole 211. The setting direction of the positioning blind hole 211 is perpendicular to the axial direction of the female mold core 2. The spliced inclined surface 21 and the positioning blind hole 211 are perpendicular to the axial direction of the female mold core 2. The axial angle of the female mold core 2 is also 45 degrees. When the positioning pin 111 is inserted into the positioning blind hole 1 211 and the splicing bevel 1 1 and the splicing bevel 2 21 are fitted together, the male mold core 1 and the female mold core 2 can form a bent tube core. The splicing end of the female mold core 2 also has a positioning blind hole 212 arranged axially along the female mold core 2. When the male mold core 1 and the female mold core 2 are coaxially connected, the positioning pin 111 can be inserted into the positioning blind hole 212 and the splicing bevel 1 1 and the splicing bevel 2 21 are fitted together. The male mold core 1 and the female mold core 2 can be vertically assembled to form a bent tube core, which can be used in conjunction with the mold to achieve bent tube injection molding. At this time, the splicing bevel 11 and the splicing bevel 21 are aligned to make the outer circumference of the male mold core 1 and the female mold core 2 smoothly transition to ensure the quality of the pipe fittings. The locating pin 111 on the splicing bevel 11 is plugged into the locating blind hole 211 at the splicing end of the female mold core 2 to ensure that the female mold core 2 and the male mold core 1 will not separate axially along the female mold core 2 after they are assembled. By setting a second positioning blind hole 212 arranged axially along the female mold core 2 at the splicing end of the female mold core 2, the positioning pin 111 can be inserted into the second positioning blind hole 212 when the male mold core 1 and the female mold core 2 are coaxially connected, and the splicing inclined surface 11 and the splicing inclined surface 21 are also fitted together. When the male mold core 1 and the female mold core 2 are wound in this state, it is beneficial for the winding device to complete the winding operation at one time, ensuring that the winding density of the male mold core 1 and the female mold core 2 is uniform; at the same time, the joint end of the male mold core 1 and the female mold core 2 is connected The limit pin and the second positioning blind hole 212 cooperate to form a limit with each other in the radial direction, ensuring that during the winding process, the male mold core 1 and the female mold core 2 can still ensure stable coaxial rotation due to the traction force of the resistance wire, avoiding large deflection swing and affecting the winding effect; and when the splicing bevel 11 and the splicing bevel 21 are fitted together, there will be a smooth transition area at the junction of the edges of the two, which is conducive to the design that the resistance wire passing through this place will not be cut by the sharp edges of the splicing bevel 11 or the splicing bevel 21, thereby ensuring the winding quality. Furthermore, the splicing bevel 11 has a limiting protrusion 112 in the shape of a right-angled triangular prism, the positioning pin 111 is located on the limiting protrusion 112, the splicing bevel 21 has a limiting groove 213, the positioning blind hole 1 211 and the positioning blind hole 212 are both located on the inner side wall of the limiting groove 213, and when the male mold core 1 and the female mold core 2 are coaxially connected, the limiting protrusion 112 and the limiting groove 213 are matched along the circumferential limiting direction of the male mold core 1.In this way, the limiting protrusion 112 cooperates with the limiting groove 213 to limit the relative rotation of the male mold core 1 and the female mold core 2 during the winding process, avoiding axial jump between the male mold core 1 and the female mold core 2 when the two ends are not firmly positioned, thereby affecting the winding effect. The end edge of the positioning pin 111, the edge of the limiting protrusion 112 and the open edge of the limiting groove 213 are all processed with rounded corners. This can improve the smoothness and convenience of the operation when the male mold core 1 and the female mold core 2 are docked and assembled.
[0038] like Figure 1-6 As shown, the male mold core 1 includes a winding segment 12 and a molding segment 13 arranged in sequence in the axial direction, and the splicing slope 11 is located on the molding segment 13. The female mold core 2 includes a winding segment 22 and a molding segment 23 arranged in sequence in the axial direction, and the splicing slope 21 is located on the molding segment 23. The radial dimension of the molding segment 13 is smaller than the radial dimension of the winding segment 12, and an annular step surface 14 is formed between the molding segment 13 and the winding segment 12. The radial dimension of the molding segment 23 is smaller than the radial dimension of the winding segment 22, and an annular step surface 24 is formed between the molding segment 23 and the winding segment 22. The winding segment 12 and the winding segment 22 are high-density winding areas of the resistance wire, and the molding segment 13 and the molding segment 23 are mainly involved in the molding of the inner cavity of the pipe fitting. In this way, the corresponding setting of different radial dimensions is conducive to distinguishing and judging the winding modes of different areas, and ensuring the winding effect. Specifically, the annular step surface 14 has a slot 141 arranged along the length direction of the winding segment 12, the position of the slot 141 is opposite to the position where the splicing inclined surface 11 is closest to the annular step surface 14, and a wire clamping pin 3 is inserted in the slot 141; the annular step surface 24 has a slot 241 arranged along the length direction of the winding segment 22, the position of the slot 241 is opposite to the position where the splicing inclined surface 21 is closest to the annular step surface 24, and a wire clamping pin 24 is inserted in the slot 241. This is conducive to designing the resistance wire on the forming section 1 13 and the forming section 2 23 to start winding from the position corresponding to the slot 1 141 or the slot 2 241. At this time, the winding direction of the resistance wire can be adapted to the edge extension direction of the splicing slope 1 11 or the splicing slope 2 21 to the greatest extent, reducing the probability of the resistance wire contacting the sharp edge and improving the winding quality. The clamping pin 1 3 and the clamping pin 2 4 installed later can ensure that the resistance wire on the winding section 1 12 and the winding section 2 22 will not get loose during the splicing adjustment, thereby ensuring the winding quality of the product. The forming section 1 13 is coaxially arranged with the winding section 1 12, and the forming section 2 23 is coaxially arranged with the winding section 2 22. This is conducive to ensuring the coaxiality of the male mold core 1 and the female mold core 2 after coaxial docking, reducing the eccentric load and position offset during the rotation process, and ensuring the winding effect.
[0039] Embodiment 2:
[0040] The winding method of the electric fusion bending tube core structure comprises the following steps:
[0041] Step 1: coaxially dock the male mold core 1 and the female mold core 2, so that the positioning pin 111 is plugged into the second positioning blind hole 212 and the first splicing inclined surface 11 is fitted with the second splicing inclined surface 21;
[0042] Step 2: Place the coaxially connected male mold core 1 and female mold core 2 on the rotating device of the winding equipment, and clamp the axial ends of the male mold core 1 and the female mold core 2.
[0043] Step 3, wind one end of the resistance wire onto the winding segment 1 12 or the winding segment 2 22, control the male mold core 1 and the female mold core 2 to rotate coaxially, and control the mobile pay-off device of the winding equipment to move along the axial direction of the male mold core 1 and the female mold core 2;
[0044] Step 4: When the resistance wire is wound to the area where the forming section 1 13 and the forming section 2 23 are located, the moving speed of the mobile pay-off device is increased or the speed of the rotating device is reduced. The number of windings of the resistance wire in the area of the forming section 1 13 and the forming section 2 23 is 1.5 turns, and the resistance wire is wound from the position on the forming section 1 13 opposite to the slot 1 141 to the position on the forming section 2 23 opposite to the slot 2 241;
[0045] Step 5: After the winding of the male mold core 1 and the female mold core 2 is completed, the resistance wires on the winding segment 1 12 and the winding segment 2 22 are hot pressed by a hot head device;
[0046] Step 6: insert the clamping pin 1 3 and the clamping pin 2 4 into the slot 1 141 and the slot 2 241 respectively to clamp the resistance wires in the corresponding areas, and take out the male mold core 1 and the female mold core 2;
[0047] Step 7, axially split the male mold core 1 and the female mold core 2, rotate the male mold core 1 or the female mold core 2 in the opposite direction of the winding of the resistance wire and swing toward the intersection state at the same time, and finally the male mold core 1 and the female mold core 2 are intersected and spliced.
[0048] In this way, the male mold core 1 and the female mold core 2 are pre-axially butted to form an axially and circumferentially stable whole, and the winding operation is completed at one time through the winding device, which improves the efficiency and consistency of the winding quality. At the same time, the winding density is reduced in the non-working area, and the resistance wire margin during the splitting can be ensured, so that the splicing operation after the winding is smooth and reliable. In this way, it can be ensured that when the resistance wire passes through the joint of the splicing inclined plane 11 and the splicing inclined plane 21, it is just a smooth transition area without being affected by sharp edges, thereby improving the winding quality.
[0049] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
Claims
1. A core structure for an electric fusion pipe bending, comprising a male mold core (1) and a female mold core (2) that can intersect and splice, wherein the splicing end of the male mold core (1) has a splicing inclined surface 1 (11), and the splicing inclined surface 1 (11) has a positioning pin (111) arranged along the axial direction of the male mold core (1), and the splicing end of the female mold core (2) has a splicing inclined surface 2 (21) and a positioning blind hole 1 (211), and when the positioning pin (111) is inserted into the positioning blind hole 1 (211) and the splicing inclined surface 1 (11) and the splicing inclined surface 2 (21) are abutted, the male mold core (1) and the female mold core (2) can form a pipe bending core, characterized in that: The splicing end of the female mold core (2) also has a second positioning blind hole (212) arranged axially along the female mold core (2). When the male mold core (1) and the female mold core (2) are coaxially connected, the positioning pin (111) can be inserted into the second positioning blind hole (212) and make the splicing inclined surface (11) and the splicing inclined surface (21) fit together. After the male mold core (1) and the female mold core (2) are axially separated, the male mold core (1) or the female mold core (2) is rotated in the opposite direction of the winding of the resistance wire and simultaneously moves toward the opposite direction. The male mold core (1) and the female mold core (2) are swung in an intersecting state, and can eventually make the male mold core (1) and the female mold core (2) intersect and splice; the male mold core (1) comprises a winding segment 1 (12) and a forming segment 1 (13) arranged in sequence axially, the splicing inclined surface 1 (11) is located on the forming segment 1 (13), and the female mold core (2) comprises a winding segment 2 (22) and a forming segment 2 (23) arranged in sequence axially, the splicing inclined surface 2 (21) is located on the forming segment 2 (23), and the radial dimension of the forming segment 1 (13) is smaller than The first winding segment (12) is a first winding segment (12), and an annular step surface (14) is formed between the first forming segment (13) and the first winding segment (12). The radial dimension of the second forming segment (23) is smaller than the radial dimension of the second winding segment (22), and an annular step surface (24) is formed between the second forming segment (23) and the second winding segment (22). The first annular step surface (14) has a slot (141) arranged along the length direction of the first winding segment (12). The slot (141) is located The slot 1 (141) is arranged opposite to the position of the splicing inclined surface 1 (11) closest to the annular step surface 1 (14), and a wire clamping pin 1 (3) is inserted into the slot 1 (141); the annular step surface 2 (24) has a slot 2 (241) arranged along the length direction of the winding segment 2 (22), the position of the slot 2 (241) is opposite to the position of the splicing inclined surface 2 (21) closest to the annular step surface 2 (24), and a wire clamping pin 2 (4) is inserted into the slot 2 (241).
2. The core structure of the electric fusion bending pipe according to claim 1 is characterized in that: The first splicing inclined surface (11) has a limiting protrusion (112), the positioning pin (111) is located on the limiting protrusion (112), the second splicing inclined surface (21) has a limiting groove (213), the first positioning blind hole (211) and the second positioning blind hole (212) are both located on the inner side wall of the limiting groove (213), and when the male mold core (1) and the female mold core (2) are coaxially connected, the limiting protrusion (112) and the limiting groove (213) are matched along the circumferential limiting direction of the male mold core (1).
3. The core structure of the electric fusion pipe bending according to claim 1 is characterized in that: The first forming section (13) is coaxially arranged with the first winding section (12), and the second forming section (23) is coaxially arranged with the second winding section (22).
4. The core structure of the electric fusion pipe bending according to claim 2 is characterized in that: The end edge of the positioning pin (111), the edge of the limiting protrusion (112) and the open edge of the limiting groove (213) are all subjected to rounded transition processing.
5. A winding method for an electric fusion bending tube core structure, characterized in that: The following steps are involved: Step 1: coaxially connect the male mold core (1) and the female mold core (2), so that the positioning pin (111) is plugged into the second positioning blind hole (212) and the first splicing bevel (11) and the second splicing bevel (21) are in contact with each other; Step 2: placing the male mold core (1) and the female mold core (2) that have been coaxially butt-jointed on a rotating device of a winding device, and clamping the male mold core (1) and the female mold core (2) at both axial ends; Step 3, winding one end of the resistance wire onto the winding segment 1 (12) or the winding segment 2 (22), controlling the male mold core (1) and the female mold core (2) to rotate coaxially, and at the same time controlling the moving wire-releasing device of the winding device to move along the axial direction of the male mold core (1) and the female mold core (2); Step 4: When the resistance wire is wound to the area where the forming section 1 (13) and the forming section 2 (23) are located, the moving speed of the mobile pay-off device is increased or the rotating speed of the rotating device is reduced; Step 5: After the male mold core (1) and the female mold core (2) are wound, the resistance wires on the winding section 1 (12) and the winding section 2 (22) are hot pressed by a hot head device; Step 6: insert the first clamping pin (3) and the second clamping pin (4) into the slot 1 (141) and the slot 2 (241) respectively to clamp the resistance wires in the corresponding areas, and take out the male mold core (1) and the female mold core (2); Step 7: Axially separate the male mold core (1) and the female mold core (2), rotate the male mold core (1) or the female mold core (2) in the opposite direction of the winding of the resistance wire and swing toward the intersection state, and finally the male mold core (1) and the female mold core (2) are intersected and spliced.
6. The winding method of the electric fusion bending tube core structure according to claim 5, characterized in that: In the fourth step, the number of turns of the resistance wire in the forming section 1 (13) and the forming section 2 (23) is 1.5 turns, and the resistance wire is wound from the position on the forming section 1 (13) opposite to the slot 1 (141) to the position on the forming section 2 (23) opposite to the slot 2 (241).