A method for preparing a photoelectric detector
By forming a gradient nanostructure inside the silicon substrate and adjusting the silicon band structure using laser processing, the problems of insufficient photoresponsiveness and poor process compatibility of the photodetector are solved, and the preparation of high-responsiveness and stability photodetectors are achieved.
Patent Information
- Application Number
- CN202210279169.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-21
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-03-21
AI Technical Summary
The photoresponsivity of the photodetector based on intrinsic crystal silicon is limited by the physical limit, and the process complexity increases after the introduction of defect energy levels on the silicon surface, reducing compatibility with the CMOS process and greatly affected by environmental factors.
By using physical focus of laser light inside the silicon substrate, the band structure of silicon is adjusted by adjusting the linear defect area to prepare a high-responsive photodetector. Specific methods include using femtosecond laser to treat the silicon substrate, setting the laser wavelength between 1100 nanometers and 1500 nanometers, energy density between 400 microwatts and 800 microwatts, and scanning the upper surface of the silicon substrate to form a uniform gradient nanostructure, and finally The source electrode and the drain electrode were prepared on a silicon substrate.
It realizes the improvement of the photodetector's photoresponse, while ensuring the compatibility of surface flatness and CMOS process, reducing the pollution of silicon material components, and improving the stability and success rate of the processing process.
Smart Images

Figure CN114678431B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of optoelectronic technology, and in particular to a method for preparing a photoelectric detector. Background Art
[0002] Crystalline silicon has a wide range of applications in the field of photodetectors. However, photodetectors based on intrinsic crystalline silicon have physical limits in terms of light responsivity, which limits further improvements in their photodetection performance. Therefore, other materials or surface microstructures are usually introduced on the silicon surface to improve its photoelectric properties.
[0003] At present, introducing defect energy levels in silicon crystals can effectively modify the energy band structure of silicon, thereby realizing the generation of high-performance photodetector devices. However, after introducing defect energy levels on the silicon surface, other elements will increase the complexity of the process, reduce the compatibility of silicon wafers with complementary metal oxide semiconductor (CMOS) processes, and be greatly affected by environmental factors such as air humidity and surface cleanliness during processing, affecting product performance. Summary of the invention
[0004] The object of the present invention is to provide a method for preparing a photoelectric detector, which improves the light response of the photoelectric detector by adjusting the silicon energy band structure in a silicon substrate.
[0005] To achieve the above objectives, in a first aspect, the present invention provides a method for preparing a photodetector, comprising: providing a silicon substrate; forming a gradient nanostructure inside the silicon substrate using a physical focusing method of a laser, wherein the gradient nanostructure has a linear defect region, and the lattice mismatch formed by the linear defect region is used to adjust the energy band structure within the silicon substrate; and preparing a source electrode and a drain electrode on top of the silicon substrate.
[0006] The beneficial effect of the present invention is that a gradient nanostructure is formed inside the silicon substrate, and the gradient nanostructure has a linear defect region. The lattice mismatch formed by the linear defect region is used to adjust the energy band structure within the silicon substrate, so that the silicon substrate has a high photoelectric response effect, thereby ultimately forming a photodetector with high responsiveness.
[0007] Optionally, the formation of the gradient nanostructure inside the silicon substrate by physical focusing of the laser includes: using a femtosecond laser to process the internal structure of the silicon substrate to form the gradient nanostructure; wherein the laser wavelength emitted by the femtosecond laser is between 1100 nanometers and 1500 nanometers. The beneficial effect is that by setting the laser wavelength of the femtosecond laser to between 1100 nanometers and 1500 nanometers, the gradient nanostructure is directly formed inside the silicon substrate, the surface flatness of the silicon substrate is ensured, and the silicon defect state is introduced, the silicon band structure is effectively regulated, and the surface structure of the silicon substrate is avoided from being damaged.
[0008] Optionally, the laser energy density emitted by the femtosecond laser is between 400 microwatts and 800 microwatts. The beneficial effect is that by setting the laser energy density emitted by the femtosecond laser between 400 microwatts and 800 microwatts, the reliability of forming the gradient nanostructure in the silicon substrate is ensured.
[0009] Optionally, the femtosecond laser is disposed on the upper surface of the silicon substrate, and the scanning speed of the femtosecond laser is 1 mm / s-10 mm / s. The beneficial effect is that by disposing the femtosecond laser on the upper surface of the silicon substrate and setting the scanning speed of the femtosecond laser to 1 mm / s-10 mm / s, the upper surface of the silicon substrate is uniformly scanned, thereby improving the uniformity and processing efficiency of forming the gradient nanostructure.
[0010] Optionally, the spot size of the femtosecond laser is between 10 μm and 1000 μm. The beneficial effect is that by setting the spot size of the femtosecond laser between 10 μm and 1000 μm, the processing efficiency is improved and the uniformity of the gradient nanostructure is ensured.
[0011] Optionally, preparing the source electrode and the drain electrode on the top of the silicon substrate includes: preparing the source electrode and the drain electrode on the upper surface of the silicon substrate by photolithography and electron beam evaporation. The beneficial effect is that: the source electrode and the drain electrode are prepared on the silicon substrate, and finally a photodetector with high responsiveness is formed. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 A flow chart of a method for preparing a photoelectric detector according to an embodiment of the present invention;
[0013] Figure 2 A schematic diagram of the structure of a silicon substrate according to an embodiment of the present invention;
[0014] Figure 3 A schematic diagram of the structure of an embodiment provided by the present invention after a silicon substrate is processed by a femtosecond laser;
[0015] Figure 4 This is a schematic diagram of the structure of an electrical detector according to an embodiment of the present invention. DETAILED DESCRIPTION
[0016] In order to make the purpose, technical solutions and advantages of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with general skills in the field to which the present invention belongs. "Including" and similar words used in this article mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects.
[0017] In view of the problems existing in the prior art, an embodiment of the present invention provides a method for preparing a photoelectric detector. Figure 1 As shown, the method includes:
[0018] S101: Provide a silicon substrate.
[0019] In this step, refer to Figure 2 As shown, the silicon substrate 100 needs to be cleaned in advance to reduce the pollution of the environment or impurity elements to the silicon substrate 100.
[0020] S102: forming a gradient nanostructure inside the silicon substrate by means of physical focusing of laser, wherein the gradient nanostructure has a linear defect region, and the lattice mismatch formed by the linear defect region is used to adjust the energy band structure inside the silicon substrate.
[0021] In this step, refer to Figure 3 As shown, a laser beam 200 emitted by a femtosecond laser is used to process the internal structure of the silicon substrate 100. By adjusting the parameters of the femtosecond laser, the laser wavelength emitted by the femtosecond laser is set to be between 1100 nanometers and 1500 nanometers, and the laser energy density emitted by the femtosecond laser is set to be between 400 microwatts and 800 microwatts. The internal three-dimensional processing of the silicon substrate 100 material is performed by focusing the objective lens, thereby forming the gradient nanostructure 101, which improves the processing efficiency and ensures the uniformity of the gradient nanostructure 101.
[0022] In addition, it should be noted that the femtosecond laser is movably arranged on the upper surface of the silicon substrate 100, and the scanning speed of the femtosecond laser on the silicon substrate 100 is 1 mm / s-10 mm / s. By setting the scanning speed of the femtosecond laser to 1 mm / s-10 mm / s, the upper surface of the silicon substrate 100 is uniformly scanned, thereby improving the uniformity and processing efficiency of forming the gradient nanostructure 101.
[0023] In this embodiment, the laser wavelength of the femtosecond laser is 1300 nanometers, the laser energy density is 600 microwatts, and the scanning speed is 5 mm / s. In some embodiments, the parameters of the femtosecond laser can be adjusted according to the size of the silicon substrate 100, so that the laser wavelength is 1100 nanometers or 1500 nanometers, the laser energy density is 400 microwatts or 800 microwatts, and the scanning speed is 1 mm / s or 10 mm / s.
[0024] S103: preparing a source electrode and a drain electrode on the top of the silicon substrate.
[0025] In this step, refer to Figure 4 As shown, a photoresist is first coated on the silicon substrate 100, and then a source electrode groove and a drain electrode groove are set on the photoresist. Then, a conductive metal is formed in the source electrode groove and the drain electrode groove by electron beam evaporation. Finally, the photoresist is removed to form the source electrode 103 and the drain electrode 104.
[0026] In this embodiment, by forming a gradient nanostructure 101 on the silicon substrate, the gradient nanostructure 101 has a linear defect region, and the lattice mismatch formed by the linear defect region is used to adjust the band structure in the silicon substrate 100, so that the silicon substrate 100 has a high photoelectric response effect, thereby finally forming a photodetector with high responsiveness. In addition, the method can effectively ensure the integrity and flatness of the surface of the silicon substrate 100 after processing, can effectively guarantee the compatibility of subsequent CMOS processes, and effectively reduce the contamination of silicon material components after processing, ensure the stability of the product processing process, and improve the success rate of preparation.
[0027] The above is only a specific implementation of the embodiment of the present application, but the protection scope of the embodiment of the present application is not limited thereto, and any changes or replacements within the technical scope disclosed in the embodiment of the present application should be included in the protection scope of the embodiment of the present application. Therefore, the protection scope of the embodiment of the present application should be based on the protection scope of the claims.
Claims
1. A method for preparing a photoelectric detector, characterized in that: include: providing a silicon substrate; A gradient nanostructure is formed inside the silicon substrate by a physical focusing method of a laser, wherein the gradient nanostructure has a line defect region, and the lattice mismatch formed by the line defect region is used to adjust the energy band structure inside the silicon substrate; Preparing a source electrode and a drain electrode on the top of the silicon substrate; The method of forming a gradient nanostructure inside the silicon substrate by using a physical focusing method of a laser includes: The internal structure of the silicon substrate is processed by a femtosecond laser to form the gradient nanostructure; wherein the laser energy density emitted by the femtosecond laser is between 400 microwatts and 800 microwatts.
2. The method according to claim 1, characterized in that: The method of forming a gradient nanostructure inside the silicon substrate by using a physical focusing method of a laser includes: The internal structure of the silicon substrate is processed by femtosecond laser to form the gradient nanostructure; wherein, The wavelength of the laser emitted by the femtosecond laser is between 1100 nanometers and 1500 nanometers.
3. The method according to claim 1, characterized in that The femtosecond laser is actively arranged on the upper surface of the silicon substrate, and the scanning speed of the femtosecond laser is 1 mm / s-10 mm / s.
4. The method according to claim 3, characterized in that The spot size of the femtosecond laser is between 10 μm and 1000 μm.
5. The method according to claim 4, characterized in that A source electrode and a drain electrode are prepared on the top of the silicon substrate, comprising: The source electrode and the drain electrode are prepared on the upper surface of the silicon substrate by using photolithography and electron beam evaporation.