Method for stirring liquid metal in electric arc furnace

By arranging multiple electromagnetic stirrers in the electric arc furnace and adjusting the direction of the electromagnetic field, the problem of insufficient temperature uniformization of liquid metal is solved, the melting and refining efficiency is improved, and the energy consumption and component life of the electric arc furnace are optimized.

CN114729781BActive Publication Date: 2024-10-15DANIELI & C OFFICINE MECCANICHE SPA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080078178.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-09-19
Filing Date
2020-09-15
Publication Date
2024-10-15
Estimated Expiration
2040-09-15

AI Technical Summary

Technical Problem

The temperature homogenization of liquid metal in existing electric arc furnaces is insufficient, resulting in uneven element concentrations, process parameter errors, local temperature peaks and premature component wear. Moreover, the role of the electromagnetic stirrer is not related to the steps of the melting cycle, limiting the liquid state. The best fusion of metals.

Method used

Arrange at least two electromagnetic stirrers in the electric arc furnace to generate electromagnetic fields that are inconsistent and consistent with each other to adjust the direction of the mixing force of the liquid metal in different steps, ensure uniform stirring and temperature homogenization of the steel, and optimize melting and refining in the furnace efficiency.

Benefits of technology

Through this method, the uniformity of the temperature and chemical composition of the liquid metal is achieved, the total energy consumption of the electric arc furnace is optimized and the cycle time is reduced, and the service life of the furnace components is extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114729781B_ABST
    Figure CN114729781B_ABST
Patent Text Reader

Abstract

A method for electromagnetically stirring liquid metal in a continuously charged electric arc furnace (10), wherein a first electromagnetic field is positioned along a first electromagnetic stirring axis (X1) and a second electromagnetic field is positioned along a second electromagnetic stirring axis (X2).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for electromagnetically stirring liquid metal in an electric arc furnace, which can be used in a process for melting metallic material with a substantially continuous charge. Background Art

[0002] Plants for melting metallic materials of the continuous charge type are known which comprise an electric arc furnace provided with at least one container or housing in which the metallic charge is melted.

[0003] The electric arc furnace also includes a covered roof with holes for the passage of electrodes, which enter the shell to allow the arc to be struck, allowing the metal charge to melt. The roof also has holes for extracting the fumes, and at the bottom or sides of the shell there are usually means for tapping the liquid metal.

[0004] The electric arc furnace is associated with a device for feeding the metallic material, which may be a continuous charging system.

[0005] The continuous charging type of solution usually uses a charging system with a hanging basket to perform the first startup charge with the furnace closed, so as to produce a large amount of metal material to be melted at the beginning of the cycle at the bottom of the furnace. Usually, when this material is completely melted, the process of continuously charging scrap into the furnace begins.

[0006] In the most common solution, the electric arc furnace has an eccentric tap hole at the bottom of the shell, called "eccentric bottom tap" or EBT, or, alternatively, a tap chute at the bottom of the shell for extracting molten metal from the shell during the tapping step.

[0007] The tapping step follows the refining step during which specific elements are introduced into the molten metal to improve its quality or to give it the desired properties, depending on the recipe of the steel to be obtained.

[0008] One of the most common drawbacks in this type of melting process is the homogenization of the molten metal temperature within the shell.

[0009] Lack of uniformity in the temperature of the molten metal mass may lead to problems such as unwanted concentrations of certain elements, incorrect measurement of process parameters, localized temperature peaks, premature wear of components, or other problems known in the art.

[0010] In order to solve these problems, it is known to use electromagnetic stirrers, which are usually arranged below the bottom of the furnace or at most associated with its side walls.

[0011] For example, document WO 2018 / 145754 describes an electric arc furnace having an electromagnetic stirrer located approximately centrally below the bottom of the shell and having an electromagnetic stirring axis intersecting a central vertical plane passing through the center of the shell and the discharge hole or discharge trough.

[0012] Document EP 2 616 560 B1 is also known, which describes an electric arc furnace provided with two electromagnetic stirrers lying opposite each other with respect to the central axis of the furnace.

[0013] US 3,409,726 is also known, which generally states that the direction of movement of the molten metal can be easily reversed by reversing the polarity of the direct current or the excitation current of the electromagnet passing through the molten metal. US'726 describes the use of a magnetic pole centered about the bottom of the housing, or in addition to the central magnetic pole, three magnetic poles arranged radially and equidistantly on the circumference of the electric furnace.

[0014] JP 62-73591 describes a magnetic stirring device for an electric arc furnace. The device comprises an electromagnetic stirrer which can be moved below the furnace to assume variable positions according to the different steps of the melting cycle.

[0015] The use of a stirrer to stir the molten metal within a furnace generally does not provide correlation between the action of the stirrer itself and the steps of the melting cycle.

[0016] This can result in excessive wear of the inner wall of the housing, where the liquid metal has a higher velocity, and define dead zones where the liquid metal tends to stagnate, rather than optimally merging with the surrounding liquid metal.

[0017] Therefore, there is a need to improve a method for electromagnetically stirring liquid metal in an electric arc furnace that can overcome the shortcomings of the prior art.

[0018] In particular, an object of the present invention is to perfect a method for electromagnetically stirring liquid metal in an electric arc furnace that prevents problems of differential wear of the furnace walls and the furnace bottom, makes the temperature of the entire liquid metal mass uniform and improves the efficiency of the melting and refining steps in the furnace.

[0019] The Applicant has devised, tested and embodied the present invention to overcome the shortcomings of the state of the art and to obtain these and other purposes and advantages. Summary of the invention

[0020] The invention is set forth and characterized in the independent claims. The dependent claims describe other characteristics of the invention or variants to the main inventive idea.

[0021] According to the above objectives, the present invention relates to a method for electromagnetic stirring of liquid metal associated with a melting phase in an electric arc furnace, the method providing at least a charging step during which a metal charge is introduced into the furnace, a melting step in the electric arc furnace and a step of refining the liquid metal.

[0022] According to one embodiment of the present invention, this electromagnetic stirring is applied in a continuously charged electric arc furnace, wherein at least one first electromagnetic field along a first electromagnetic stirring axis and at least one second electromagnetic field along a second electromagnetic stirring axis are generated by at least two electromagnetic stirrers arranged at the furnace bottom or below the bottom of the furnace.

[0023] According to one aspect of the invention, in at least the first step of the furnace cycle, the first electromagnetic field and the second electromagnetic field generate mixed forces on the liquid metal having directions inconsistent with each other, and in at least the second step of the furnace cycle, the electromagnetic fields generate forces on the liquid metal having directions consistent with each other.

[0024] In the description here and below, the term "inconsistent" means that the axis of the mixing force generated by the first electromagnetic stirrer has an opposite direction relative to the axis of the mixing force generated by the second electromagnetic stirrer; on the other hand, the term "consistent" means that the axes of the mixing forces generated by the two electromagnetic stirrers have the same direction, that is, they have the same direction.

[0025] In this way, when the directions of the axes of force are not coincident (or opposite), the agitation of the steel is generally towards the entire periphery of the shell, the steel performing a substantially circular and tangential movement relative to the refractory wall of the shell.

[0026] On the other hand, when the axes of the electromagnetic forces have a consistent orientation, the two stirrers force the steel to move toward the same peripheral region of the furnace, and the steel rebounds at the periphery and returns to the center.

[0027] Differentiating the mixing effects associated with the steps of the melting process makes it possible to optimize the overall energy consumption of the electric arc furnace and reduce the overall cycle time, in addition to obtaining a liquid metal with very homogeneous thermophysical and chemical composition characteristics. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] These and other aspects, features and advantages of the invention will become apparent from the following description of some embodiments, which are given as non-limiting examples with reference to the accompanying drawings, in which:

[0029] - Figure 1 is a cross-sectional schematic diagram of an electric arc furnace to which the electromagnetic stirring method of the present invention is applicable;

[0030] - Figure 2 and Figure 3 They are schematic diagrams of the stirring method according to the present invention;

[0031] - Figures 4a-4f is a schematic diagram of a possible alternative arrangement of an electromagnetic stirrer in an electric arc furnace to which the electromagnetic stirring method of the present invention is applicable.

[0032] To facilitate understanding, where possible, the same reference numerals have been used to designate the same common elements in the drawings. It should be understood that elements and features of one embodiment may be conveniently incorporated in other embodiments without further clarification. DETAILED DESCRIPTION

[0033] We will now refer in detail to possible embodiments of the present invention, one or more examples of which are shown in the accompanying drawings. Each example is provided as an illustration of the present invention and should not be construed as limiting thereof. For example, features shown or described, as long as they are part of one embodiment, may be changed or adopted on other embodiments, or associated with other embodiments to produce other embodiments. It should be understood that the present invention shall include all such modifications and variations.

[0034] Before describing these embodiments, we must also clarify that the present description is not limited in its application to the details of construction and arrangement of components described in the following description using the accompanying drawings. The present description may provide other embodiments and may be obtained or carried out in various other ways. We must also clarify that the phraseology and terminology used herein is for descriptive purposes only and is not to be regarded as limiting.

[0035] The embodiment depicted in the drawing relates to an electric arc furnace, which is designated as a whole by reference numeral 10 , in which liquid metal L is mixed according to the electromagnetic stirring method according to the invention.

[0036] The electric arc furnace 10 can be of the type powered by alternating current AC, characterized by the presence of three or more electrodes 14 between which the arc strikes to ignite and / or continue the melting process, or powered by direct current DC, characterized by the presence of one or two electrodes 14 arranged in the center, which perform the function of a cathode that cooperates with an anode located at the bottom of the electric arc furnace 10 to generate an arc.

[0037] Although in the figures described herein we refer to an electric arc furnace 10 of the type powered by alternating current AC, it is clear that the concepts described below are also applicable to an electric arc furnace 10 of the type powered by direct current DC.

[0038] according to Figure 1 In the illustrated embodiment, the electric arc furnace 10 comprises in its essential parts a container or shell 11 and a covering element or roof 12 arranged above and covering the shell 11 .

[0039] For the electric arc furnace 10 there are associated means 13 for continuously feeding a metal charge 25 which may comprise scrap S, for example.

[0040] The feeding device 13 is suitable for moving the metal charge 25 according to a determined feeding axis Z.

[0041] According to some embodiments, the supply device 13 can be arranged horizontally. Figure 1-3 , to introduce the metal charge 25 relative to the side of the electric arc furnace 10, or at the top, to introduce the metal charge 25 from a hole formed in the roof 12.

[0042] The metal charge 25 is positioned on the feed device 13 in a known manner and can have certain dimensions which can even be highly variable.

[0043] Holes for receiving and / or positioning electrodes 14 are formed in the top portion 12 , which holes are suitable for generating an electric arc to melt a metal charge present in the housing 11 .

[0044] The top 12 and the electrode 14 are associated with lifting and rotating means suitable for lifting the top 12 and the electrode 14, even independently of each other.

[0045] The housing 11 is provided with a bottom or furnace floor 15, and side walls 16 at least partially made of refractory material to withstand the high temperatures and highly reactive environment reached during the melting step.

[0046] The bottom 15 may be provided with an eccentric tapping hole 17 , also called “eccentric bottom tap” EBT, or, alternatively or additionally, with a tapping chute for extracting molten metal from the housing 11 during a tapping step.

[0047] The housing 11 is mounted on a support which is not visible in the drawings and actuating means are usually provided to rotate the housing 11 itself around a determined axis of rotation.

[0048] The furnace 10 further comprises a lining 18 provided with a lower edge 19 arranged to rest on the upper edge of the outer shell 11 .

[0049] A lining 18 , usually consisting of a cooling plate, extends substantially along the wall of the housing 11 , and the roof 12 is arranged above it so as to be arranged to close the latter.

[0050] The liner 18 is provided with a first hole 20 through which the feeding device 13 is positioned to feed the metal charge 25 and a second hole through which the slag tapping operation can be performed.

[0051] Inside the housing 11 , below the first opening 20 , there is a charging zone 28 , in which the newly introduced metal charge 25 accumulates.

[0052] The charging zone 28 is located in a peripheral position relative to a central area of ​​the electric arc furnace 10 where the electrodes 14 are present.

[0053] The second hole can be selectively accessible / inaccessible by means of a slag discharge door 22, which is usually located opposite to the discharge hole 17. Figure 2-3 .

[0054] According to some embodiments, Figure 2 and Figure 3 As shown, the electric arc furnace 10 is provided with two electromagnetic stirrers 23 , 24 below the housing 11 , which are configured to generate mixing forces F1 , F2 in the liquid metal L within the housing 11 during the smelting process.

[0055] As can be seen from the drawings, the electromagnetic stirrers 23 , 24 may be arranged in an opposing and mirror-symmetrical manner to form a pair of electromagnetic stirrers relative to the central plane P.

[0056] The electric arc furnace 10 includes a power supply device 26 configured to supply power to the electromagnetic stirrers 23 , 24 , and a control unit 27 operatively connected to the power supply device 26 to control driving of the electromagnetic stirrers 23 , 24 .

[0057] According to some embodiments, each electromagnetic stirrer 23, 24 comprises a body made of magnetic material around which a coil of conductive material is wound. The coil is configured to be powered with current by a power supply device 26 to generate a magnetic field in the direction of the axis of electromagnetic stirring of the electromagnetic stirrer 23, 24.

[0058] According to some embodiments, the control unit 27 may also be operatively associated with the power supply device 13 and the electrodes 14 .

[0059] The first electromagnetic stirrer 23 is energized to generate a first electromagnetic field along the first electromagnetic stirring axis X1 .

[0060] The second electromagnetic stirrer 24 is energized to generate a second electromagnetic field of force along the second electromagnetic stirring axis X2.

[0061] According to another embodiment, Figures 4a-4f As shown, there may be a number greater than two electromagnetic stirrers 123 , 124 in order to generate a corresponding number of electromagnetic fields along the electromagnetic stirring axis X.

[0062] According to some embodiments, the electromagnetic stirrers 123, 124 may be arranged to form a pair of electromagnetic stirrers, for example two pairs ( Figure 4a , 4d ) or more, such as three pairs ( Figure 4e ).

[0063] Alternative embodiments may provide an offset relative to the center plane P ( Figure 4d ) or align( Figure 4e ) are arranged in pairs of opposing electromagnetic stirrers 123.

[0064] According to other embodiments, the pair of electromagnetic stirrers 123, 124 may be positioned at different distances relative to the center plane P ( Figure 4d ).

[0065] In other embodiments, different pairs of electromagnetic stirrers 123, 124 may have different distances from the center plane P ( Figure 4a ).

[0066] Other embodiments may provide an odd number of electromagnetic stirrers 123, 124, such as 3 or 5 ( Figure 4b , 4c ).

[0067] In an embodiment where an odd number of electromagnetic stirrers 123, 124 are provided, at least two stirrers may be arranged in opposite pairs relative to the center plane P. Figure 4b ).

[0068] According to some embodiments, one or more electromagnetic stirrers 123, 124 may be arranged substantially in line with the central plane P ( Figure 4b , 4c ).

[0069] Some embodiments may provide a center plane P ( Figure 4c ).

[0070] In other embodiments, the electromagnetic stirrers 123, 124 may be arranged such that their stirring axes X are inclined relative to the central plane P, for example, orthogonal ( Figure 4f ).

[0071] According to further embodiments not shown here, the arc furnace 10 can be provided with electromagnetic stirrers 123 , 124 , the stirring axes X of which are oriented differently relative to one another.

[0072] According to some embodiments, the electromagnetic stirrers 123 , 124 may be appropriately sized relative to the size and / or desired arrangement of the housing 11 .

[0073] Some embodiments not shown here may provide an electric arc furnace 10 provided with electromagnetic stirrers 123 , 124 of different sizes relative to each other.

[0074] According to some embodiments, the first electromagnetic stirring axis X1 and the second electromagnetic stirring axis X2 are parallel to each other relative to the central plane P.

[0075] The center plane P is vertical and passes through the center of the bottom 15 of the housing 11 and through the tap hole 17, or alternatively through the tap slot.

[0076] The center plane P may be a plane of symmetry at least for the housing 11 .

[0077] According to some embodiments, the housing 11 has a top planar cross-section, which may have a curved shape, for example defined by connecting one or more curves appropriately selected from the group consisting of a circle, a parabola, an ellipse, a straight line.

[0078] According to some embodiments, the housing 11 has an elongated curved shape in the direction of the discharge hole 17 , and thus the discharge hole 17 is located very far from the center of the housing 11 .

[0079] Reference by example Figure 2-3 , a method for electromagnetically stirring liquid metal L in an electric arc furnace 10 is described.

[0080] A melting process is carried out in the electric arc furnace 10 , which comprises at least one charging step, during which a metal charge 25 is introduced and melted, which is added to the previously melted liquid metal L, followed by a step of refining the liquid metal L in the electric arc furnace 10 .

[0081] In the method for electromagnetically stirring liquid metal in a continuously charged electric arc furnace 10 according to the present invention, a first electromagnetic field along a first electromagnetic stirring axis X1 and a second electromagnetic field along a second electromagnetic stirring axis X2 are generated.

[0082] According to one embodiment of the present invention, in a first step, the first electromagnetic field and the second electromagnetic field generate mixed forces F1 and F2 on the liquid metal L having directions inconsistent with each other, and in a second step, these electromagnetic fields generate forces F1 and F2 on the liquid metal L having directions consistent with each other.

[0083] In an advantageous solution, the first step is a charging step and the second step is a refining step.

[0084] According to some embodiments, Figure 2-3 As shown, during at least one charging step and during the refining step, the first electromagnetic stirring axis X1 and the second electromagnetic stirring axis X2 are parallel to each other relative to a central vertical plane P passing through the center of the arc furnace 10 and through the discharge hole 17 of the arc furnace 10.

[0085] According to some embodiments, during at least one charging step, the mixing forces F1, F2 determine the flow of the liquid metal L in a counterclockwise peripheral direction, see Figure 2 .

[0086] In other words, during the above charging step, the axes of generation of the mixing forces F1, F2 of the first electromagnetic stirrer 23 and the second electromagnetic stirrer 24 are oriented in opposite (or inconsistent) directions to each other. Figure 2 In the figure, the opposite directions of the generated forces are indicated by F3 for the electromagnetic stirrer 23 and by F4 for the electromagnetic stirrer 24.

[0087] In this way, the agitation of the steel is mainly towards the entire periphery of the shell 11 and the movement of the liquid metal L is substantially circular and tangential to the refractory wall of the shell 11 .

[0088] In other embodiments, the mixing forces F1 , F2 determine the flow of the liquid metal L in a clockwise peripheral direction (not shown).

[0089] The position of the magnetic stirrers 23, 24 and the opposite and inconsistent directions of their stirring action, defined by the respective electromagnetic stirring axes X1, X2, allow to achieve in an optimal way the introduction of the metal charge 25 and its accumulation in the corresponding charging zone 28. Due to the direction of the stirring forces, the new metal charge 25 introduced gradually merges into the previous one, thus promoting the homogeneity of the temperature, as well as the area corresponding to the discharge opening 17 located further away from the center of the electric arc furnace 10.

[0090] Furthermore, this configuration and actuation mode of the electromagnetic stirrers 23 , 24 allows obtaining a more uniform velocity distribution, preventing eddies and / or instabilities in the liquid metal L flow.

[0091] In this case, the flow of liquid metal L, because it is substantially circular and tangential to the side wall 16 of the housing 11, has a reduced radial component of momentum. This helps to limit the erosive effects on the side wall 16 and thus reduce the need for frequent maintenance and repair interventions.

[0092] According to some embodiments, during the refining step, the mixing forces F1, F2 have a consistent direction, i.e. the electromagnetic stirrers 23 and 24 are powered so that the axis of the generated electromagnetic force (at Figure 3 The electromagnetic stirrer 23 is indicated by arrow F5, and the electromagnetic stirrer 24 is indicated by arrow F4) has the same direction and orientation.

[0093] In this case, the agitators 23 and 24 both promote the liquid metal L to move to the same peripheral area of ​​the furnace 10, in particular, to the eccentric discharge hole 17, and then the liquid metal L rebounds at the periphery and returns to the center, moving in the direction of the slag discharge door 22. Figure 3 .

[0094] This also allows the temperature in the central region of the housing 11 to be homogenized, the flow of liquid metal L moving at a faster speed corresponding to the side walls 16 of the housing 11 during the charging step, with little mixing occurring.

[0095] According to some embodiments, during at least one charging step and refining step, the control unit 27 sends a control signal to the power supply device 26, which powers the first electromagnetic stirrer 23 with a first current and powers the second electromagnetic stirrer 24 with a second current to generate the above-mentioned first electromagnetic field and second electromagnetic field, respectively, which are appropriately oriented in inconsistent (or opposite) directions or in consistent directions (i.e., having the same direction) according to one or the other of the steps.

[0096] According to some embodiments, the control unit 27 may receive a charging signal proportional to the amount of metal charge 25 introduced into the arc furnace 10 from the supply device 13 and send an operation signal to the power supply device 26 to limit the first current and the second current based on the amount of metal charge 25 introduced.

[0097] The greater the amount of metal charge 25 introduced, the greater the intensity of the current, since the respective mixing forces F1 , F2 have to stir a greater amount of liquid metal L.

[0098] This allows the stirring action of the electromagnetic stirrers 23 , 24 to be adjusted automatically, always obtaining a perfect and homogeneous mixing of the liquid metal L.

[0099] According to some embodiments, during at least one of the charging step and the refining step, the first current and the second current may have the same intensity.

[0100] According to further embodiments, during at least one of the charging step and the refining step, the first current and the second current may have different intensities.

[0101] In particular, during the charging step, an electric current having a greater intensity than the electric current during the refining step may be provided.

[0102] In fact, the presence of a partially molten and / or solid metal charge 25 requires mixing forces F1 , F2 greater than those required to stir the liquid metal L at the end of the melting process and during the refining step.

[0103] Varying the intensity of the electric current in connection with the above-described charging and refining steps and / or as a function of the amount of introduced metallic charge 25 allows optimizing the overall energy consumption of the electric arc furnace 10 .

[0104] Obviously, modifications and / or additional steps may be made to the method for electromagnetic stirring of liquid metal in an electric arc furnace described above without departing from the field and scope of the present invention.

[0105] It is also clear that, although the invention has been described with reference to some specific examples, a person skilled in the art will certainly be able to realize many other equivalent forms of the method for electromagnetic stirring of liquid metal in an electric arc furnace, which, since they have the characteristics described in the claims, are all within the scope of protection defined by the claims.

[0106] In the following claims, the sole purpose of reference signs in parentheses is to facilitate reading: they shall not be regarded as limiting factors with respect to the field of protection claimed in a particular claim.

Claims

1. A method for melting a metal material using a continuously charged electric arc furnace (10) associated with a supply device (13) for continuously supplying a metal charge (25), the method comprising a cycle of the continuously charged electric arc furnace (10), the cycle comprising a charging step of continuously supplying a metal charge (25) by the supply device (13), a melting step and a refining step, the method further comprising a method of electromagnetically stirring liquid metal in the continuously charged electric arc furnace (10), wherein at least one first electromagnetic field along a first electromagnetic stirring axis (X1) and at least one second electromagnetic field along a second electromagnetic stirring axis (X2) are generated by an electromagnetic stirrer (23, 24; 123, 124), and in the charging step of the furnace cycle, the first electromagnetic field and the second electromagnetic field are The electromagnetic field generates mixing forces (F1, F2) on the liquid metal (L), the respective generation axes (F4, F3) of the mixing forces (F1, F2) having opposite directions that are inconsistent with each other, and in the refining step of the furnace cycle, the electromagnetic field generates mixing forces (F1, F2) on the liquid metal (L), the respective generation axes (F4, F5) of the mixing forces (F1, F2) having the same directions that are consistent with each other, in the charging step, the electromagnetic stirrer (23, 24; 123, 124) is configured to promote stirring of the liquid metal towards the entire periphery of the shell (11) of the electric arc furnace (10), the movement of the liquid metal (L) is substantially circular and tangential to the refractory wall of the shell (11) of the electric arc furnace (10), and Features In the refining step, the electromagnetic stirrer (23, 24; 123, 124) is configured to promote the movement of liquid metal toward the eccentric discharge hole (17), and then the liquid metal (L) rebounds at the periphery and returns to the center, moving in the direction of the slag discharge door (22).

2. The method according to claim 1, Features During the at least one charging step and during the refining step, the first electromagnetic stirring axis (X1) and the second electromagnetic stirring axis (X2) are parallel to each other relative to a vertical center plane (P), which passes through the center of the electric arc furnace (10) and through the discharge hole (17) of the electric arc furnace (10).

3. The method according to any one of claims 1 or 2, Features During said at least one charging step, said mixing forces (F1, F2) determine a flow of liquid metal (L) in a counterclockwise peripheral direction.

4. The method according to any one of claims 1 or 2, Features During said at least one charging step, said mixing forces (F1, F2) determine a flow of liquid metal (L) in a clockwise peripheral direction.

5. The method according to claim 1, Features During the at least one charging step and the refining step, a control unit (27) sends an operating signal to a power supply device (26), which supplies power to at least one first electromagnetic stirrer (23) with a first current and supplies power to at least one second electromagnetic stirrer (24) with a second current, so as to generate the first electromagnetic field and the second electromagnetic field, respectively, which are appropriately oriented according to one or the other of the steps.

6. The method according to claim 5, Features The control unit (27) receives a charging signal proportional to the amount of metal charge (25) introduced into the electric arc furnace (10) from the supply device (13), and sends the operation signal to the power supply device (26), so that the first current and the second current have intensities proportional to the amount of the introduced metal charge (25).

7. The method according to claim 5 or 6, Features During said at least one charging step and said refining step, said first current and said second current have the same intensity.

8. The method according to claim 5 or 6, Features During said at least one charging step and said refining step, said first current and said second current have different intensities.

9. The method according to claim 8, Features In the at least one charging step, the first and second electric currents have a greater intensity than the first and second electric currents in the refining step.