A method for detecting GPC3 based on RGO-CMCS-Hemin / Pd NPs electrochemical sensor
By using RGO-CMCS-Hemin/Pd NPs nanocomposite to construct an electrochemical aptasensor, which hinders the redox reaction of Hemin when combined with GPC3, it solves the problems of high detection cost and low sensitivity of GPC3 in the existing technology, and achieves 9.898 The lowest detection limit of ng/mL and label-free detection provide a simple and economical detection method.
Patent Information
- Application Number
- CN202210450824.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-04-27
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-04-27
AI Technical Summary
The existing GPC3 detection technology has problems such as high cost, easy degradation, large batch-to-batch differences, and difficulty in storage and transportation. There is an urgent need to develop a new, convenient and sensitive detection method.
An electrochemical aptasensor was constructed using a nanocomposite material based on reduced graphene oxide-carboxymethyl chitosan-heme chloride/nano-palladium (RGO-CMCS-Hemin/Pd NPs), through Pd NPs and thiolated GPC3 The aptamer forms a coordination bond and blocks Hemin's redox reaction when combined with GPC3. Differential pulse voltammetry is used to record changes in current signals to detect GPC3.
Sensitive detection of GPC3 was achieved, with the lowest detection limit of 9.898 ng/mL, providing a simple and low-cost detection method, improving the sensitivity of the detection signal and achieving label-free detection.
Smart Images

Figure CN114813876B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of biological detection, and specifically relates to a method for detecting GPC3 based on aptamer-modified graphene nanocomposite materials. Background Art
[0002] Glypican-3 (GPC3) is a heparan sulfate (HS) glycoprotein on the cell membrane surface. Commonly used GPC3 detection technologies include enzyme-linked immunosorbent assay (ELISA), chemiluminescent immunoassay (CLIA), radioimmunoassay (RIA), and bioimmunosensors. The invention patent with publication number CN 107085109A relates to the use of a highly positively charged green fluorescent protein (ScGFP) in the preparation of a GPC3 kit for early diagnosis of liver cancer. It uses the specific recognition of antibodies and GPC3 proteins and the charge binding of ScGFP and the side chain to achieve the detection of GPC3. The invention patent with publication number CN 109580951A relates to a kit for detecting early liver cancer markers with multiple antibodies and its use method. It uses fluorescent microspheres coated with colored antibodies to capture markers, thereby diagnosing early liver cancer. The antibodies involved in these two patents themselves still have shortcomings, such as high cost, easy degradation, large batch differences, and difficulty in storage and transportation. Therefore, there is an urgent need to develop a new, convenient and sensitive GPC3 detection method. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a nanocomposite material based on reduced graphene oxide-carboxymethyl chitosan-hemin / nanopalladium (RGO-CMCS-Hemin / Pd NPs) to construct an electrochemical aptamer sensor to realize the detection of GPC3. The minimum detection limit of this method is 9.898 ng / mL.
[0004] The detection principle of the present invention is: utilizing the large specific surface area of RGO, the good biocompatibility of carboxymethyl chitosan (CMCS), the high conductivity of Pd NPs and the electroactive substance Hemin, the RGO-CMCS-Hemin / Pd NPs nanocomposite material is synthesized. The Pd NPs in the RGO-CMCS-Hemin / Pd NPs nanocomposite material react with the thiolated GPC3 aptamer (GPC3 Apt ) forms a coordination bond, making GPC3 Apt Firmly fixed on the electrode surface; when GPC3 is present, the single-chain GPC3 Apt The aptamer-protein complex specifically binds to GPC3 to form a stable spatial structure, which hinders the Hemin (Fe 2+) / Hemin(Fe 3+ ) causes the redox reaction between the two, resulting in a decrease in the current signal. The differential pulse voltammetry (DPV) technique in the electrochemical workstation is used to record the change in the current signal, thereby realizing the concentration determination of GPC3. On the one hand, the RGO-CMCS-Hemin / Pd NPs nanocomposite material can amplify the detection signal of the electrochemical aptamer sensor and improve the sensitivity of the sensor; on the other hand, the material can be used as an in-situ electroactive probe to indicate the current signal of the electrochemical aptamer sensor and realize label-free GPC3 detection.
[0005] The present invention is carried out according to the following steps:
[0006] Step 1: Preparation of RGO-CMCS-Hemin / Pd NPs nanocomposites
[0007] (1) Preparation of reduced graphene oxide (RGO): Graphene oxide (GO) was poured into water and ultrasonically crushed to obtain a GO suspension, which was then reduced by adding ascorbic acid (AA) to obtain an RGO suspension.
[0008] (2) Preparation of reduced graphene oxide-hemin (RGO-Hemin): Hemin was dissolved in ammonia water and added to the RGO solution. After mixing, the mixture was ultrasonically crushed to obtain a RGO-Hemin dispersion.
[0009] (3) Preparation of reduced graphene oxide-carboxymethyl chitosan-hemin (RGO-CMCS-Hemin): After dissolving carboxymethyl chitosan (CMCS) in acetic acid, the CMCS solution was added to the RGO-Hemin dispersion, mixed and ultrasonically crushed to obtain the RGO-CMCS-Hemin solution.
[0010] (4) Preparation of reduced graphene oxide-carboxymethyl chitosan-hemin / nanopalladium (RGO-CMCS-Hemin / Pd) composite material: Sodium hexachloropalladate solution and AA were added to the RGO-CMCS-Hemin solution, stirred, and centrifuged to remove the supernatant to obtain a RGO-CMCS-Hemin / Pd NPs solution.
[0011] Step 2: Electrode modification and sensing interface construction
[0012] (1) Preparation of Au NPs / SPE: The screen-printed electrode (SPE) was activated in a dilute H2SO4 solution; the activated SPE was placed in a solution containing chloroauric acid (HAuCl4) and subjected to constant potential deposition to obtain an Au NPs / SPE electrode.
[0013] (2) Preparation of RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE sensing interface: RGO-CMCS-Hemin / Pd NPs suspension was added dropwise onto Au NPs / SPE, incubated, soaked in activator of 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide hydrochloride / N-hydroxysuccinimide (EDC / NHS), and dried naturally to obtain RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE.
[0014] (3) GPC3 Apt Construction of / RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE electrochemical aptasensor: GPC3 Apt The prepared RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE sensing interface was added dropwise for incubation, washed with water and dried, and then blocked with bovine serum albumin (BSA) solution to obtain GPC3. Apt / RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE working electrode.
[0015] Step 3: Drawing of GPC3 working curve
[0016] (1) Place the working electrode in step 2 in a PBS buffer solution, scan using the DPV of an electrochemical workstation, and record the response current value of the sensor.
[0017] (2) Detect different concentrations of GPC3, record the current peak, and draw the GPC3 working curve based on the relationship between the difference between the response current peak at that concentration and the response current peak of the GPC3 blank group and the GPC3 concentration.
[0018] Step 4: Detection of GPC3 in actual serum samples
[0019] (1) The sample to be tested is mixed with GPC3 and added to the working electrode in step 2. After incubation for a period of time, the electrode is immersed in PBS buffer solution and scanned using DPV detection technology. At the same time, a blank group is set up to record the current response peak.
[0020] (2) Based on the working curve obtained in step 3, calculate the concentration of GPC3 in the sample to be tested.
[0021] Further, the concentration of the RGO-CMCS-Hemin / Pd NPs solution in step 1 is 1.0 mg / mL;
[0022] Further, in step 2, the concentration of the dilute H2SO4 solution is 0.5 mol / L, and the cyclic voltammetry (CV) scanning voltage is 0.4 V to 1.2 V;
[0023] Furthermore, in step 2, the concentration of HAuCl4 solution is 0.01%, the constant voltage is - 0.5 V, and the scanning time is 2 min;
[0024] Furthermore, in step 2, the incubation time of the nanocomposite material is 2 h, the incubation temperature is 25°C, the dosage is 3.0 μL, the concentration of the activator EDC / NHS is 10.0 mmol / L, the immersion time is 15 min, and the dosage is 4.0 μL;
[0025] Further, in step 2, GPC3 Apt The incubation time was 1 h, the dosage was 4.0 μL, the concentration of BSA solution was 0.5%, and the blocking time was 30 min;
[0026] Further, the concentration of the PBS buffer solution in step 3 is 0.2 mol / L;
[0027] Further, in the step 3 and step 4, the DPV scan has a voltage range of 0.2 V to 1.0 V;
[0028] Preferably, in step 3 and step 4, when the incubation temperature of the electrode is 25° C., the incubation time is 30 min, and the pH value of the PBS buffer is 6.5, the difference between the sensor response current and the blank control group response current is the largest.
[0029] In step 1, a RGO-CMCS-Hemin / Pd NPs composite material is prepared, which is the GPC in step 2. Apt The fixation of the RGO-CMCS-Hemin / Pd NPs provides a good biosensing interface and improves the conductivity of the entire system. At the same time, it acts as an in-situ electroactive probe, indicating the current signal of the electrochemical aptamer sensor in steps 3 and 4. Step 2 constructs a sensing interface that specifically recognizes GPC3 and uses the electroactive substance Hemin in the composite material to provide an electrochemical signal. The activator in step 2 (2) allows Pd and -SH to combine to form a coordination bond to provide a binding site for the aptamer, which is beneficial for the aptamer to be better fixed on the sensing interface, thereby increasing the binding rate of the aptamer and the protein. The construction of the biosensing interface in step 2 is an essential key step for the detection of GPC3 in steps 3 and 4. The working curve of GPC3 in step 3 provides a calculation basis for the determination of the GPC3 concentration in the actual sample in step 4. It can be seen that steps 1-4 support each other and work together to achieve the detection of GPC3 using the electrochemical aptamer sensor based on the RGO-CMCS-Hemin / Pd NPs composite material.
[0030] Compared with the prior art, the present invention has the following advantages:
[0031] The RGO-CMCS-Hemin / Pd NPs nanocomposite material formed by this patent has unique morphology and function. 2+ ) / Hemin(Fe 3+ ) caused the change of current signal, and the GPC3 aptamer sensor based on RGO-CMCS-Hemin / Pd NPs composite material was successfully prepared, which provided a simple and low-cost method for the detection of GPC3 with a minimum detection limit of 9.898 ng / mL. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 Schematic diagram of the electrochemical aptasensor based on RGO-CMCS-Hemin / Pd NPs composite for detecting GPC3.
[0033] Figure 2 Transmission electron microscopy images of RGO-Hemin (A), RGO-CMCS-Hemin (B) and RGO-CMCS-Hemin / Pd NPs (C) composites;
[0034] Figure 3 X-ray diffraction spectrum of RGO-CMCS-Hemin / Pd NPs;
[0035] Figure 4 SEM images of different modification processes on the electrode surface;
[0036] Figure 5 DPV working curve of the GPC3 aptamer sensor based on RGO-CMCS-Hemin / Pd NPs for detecting different concentrations of GPC3. DETAILED DESCRIPTION
[0037] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0038] A method for detecting GPC3 using an electrochemical aptamer sensor based on RGO-CMCS-Hemin / Pd NPs composite material. The detection principle is shown in Figure 1. The screen-printed electrode (SPE) was activated; Au NPs were electrodeposited on the SPE to enhance conductivity; the prepared RGO-CMCS-Hemin / Pd NPs nanocomposite was modified on the Au NPs / SPE; the nanocomposite made with RGO as the substrate was used to modify the electrode to maintain the activity of the loaded biomaterials, and Hemin is an electroactive substance that can serve as an electronic medium to provide signals for the sensor; at the same time, the addition of Hemin prevented RGO from agglomerating, which was beneficial to the subsequent combination of materials; CMCS has excellent biocompatibility and adhesion, which further enhanced the combination of the composite material, and the addition of metal Pd nanoparticles further enhanced the conductive properties of the nanocomposite. In addition, Pd in the nanocomposite combines with -SH to form a coordination bond for the subsequently added GPC3 Apt Provides binding sites, further increasing GPC3 Apt When GPC3 is present, the single-chain GPC3Apt specifically binds to GPC3 to form an aptamer-protein complex with a stable spatial structure, which hinders the binding of Hemin (Fe 2+ ) / Hemin(Fe 3+ ) causes the redox reaction between the two, resulting in a decrease in the current signal. The differential pulse voltammetry (DPV) technique in the electrochemical workstation is used to record the change in the current signal, thereby achieving the concentration determination of GPC3. The implementation steps are as follows:
[0039] Step 1: Preparation of RGO-CMCS-Hemin / Pd NPs composites
[0040] (1) Weigh 30.0 mg of single-layer graphene oxide GO and pour it into a beaker containing 30.0 mL of ultrapure water. Ultrasonicate for 2 h with a power of 70% and a speed of 5 sed. After the crushing, a GO suspension with a concentration of 1.0 mg / mL is obtained. Add 90.0 mg of AA to reduce the GO solution, and stir the solution evenly for 12 h to obtain an RGO suspension.
[0041] (2) Take 10.0 mL of 1.0 mg / mL RGO suspension, add 10.0 mL of Hemin solution, mix the two evenly, and then use a cell disruptor to ultrasonically disrupt for 30 min with the power set to 50% and the speed set to 3 sed to obtain RGO-Hemin dispersion. Figure 2 A is the TEM image of RGO-Hemin, which is wrinkled and dark in color. 10.0 mL of carboxymethyl chitosan CMCS solution was added to the RGO-Hemin dispersion, mixed well, and then crushed with a cell crusher for 30 min. Figure 2B is the TEM image of RGO-CMCS-Hemin, which shows a flat film-like morphology.
[0042] (3) Take 2.0mL of 20.0mmol / L sodium hexachloropalladate solution and add it to 10.0mL RGO-CMCS-Hemin solution; add 10.0mg ascorbic acid AA while stirring, place it on a magnetic stirrer and stir for 16 hours before taking it out. Centrifuge the obtained dispersion at a speed of 8000 r / min for 15 minutes. After centrifugation, remove the supernatant with a pipette, wash the black precipitate, and dry it to obtain RGO-CMCS-Hemin / Pd NPs, such as Figure 2 C is the TEM of RGO-CMCS-Hemin / Pd NPs. It can be seen that there are many small particles with dark colors, unique morphology, and clearer overall appearance, indicating that the RGO-CMCS-Hemin / Pd NPs composite material was successfully prepared.
[0043] X-ray diffraction of RGO-CMCS-Hemin / Pd NPs composite (solid) was performed, as shown in Figure 3 As shown in the figure, the diffraction peak at 2θ = 25.62° corresponds to the C (002) crystal plane. Metal palladium belongs to the platinum group of metals, and has diffraction peaks (111) and (220) at 2θ = 40.11° and 68.11°, respectively, indicating that Pd NPs have been successfully attached to the graphene composite material, once again proving that the RGO-CMCS-Hemin / Pd NPs composite material was successfully prepared.
[0044] Step 2: Electrode modification and biosensing interface construction
[0045] (1) The bare SPE was activated in a 0.5 mol / L dilute sulfuric acid solution, and CV scanning was performed at 0.4 V to 1.2 V, with 20 cycles at 0.5 V / s. After activation, a small beaker containing 0.01% HAuCl4 solution was placed on a magnetic stirrer, and it was scanned at a constant voltage of -0.5 V for 2 min. The SPE was washed three times with ultrapure water and dried to obtain Au NPs / SPE.
[0046] (2) Add 3.0 μL of RGO-CMCS-Hemin / Pd NPs suspension onto Au NPs / SPE, incubate the electrode at 25 °C for 2 h, add 4.0 μL of 10.0 mmol / L EDC / NHS onto the electrode and soak it for 15 min, and dry it naturally to obtain the RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE sensing interface.
[0047] (3) Add 3.0 μL of thiolated GPC to the constructed RGO-CMCS-Hemin / PdNPs / Au NPs / SPE sensing interface. Apt After incubation at 25 °C for 1 h, the aptamers not fixed on the sensing interface were washed away with pure water, and then 4.0 μL 0.5% BSA was used to block the nonspecific binding sites of the aptamers. The mixture was incubated for 30 min, washed and dried to obtain GPC Apt / RGO-CMCS-Hemin / PdNPs / AuNPs / SPE sensing interface.
[0048] (4) Scanning electron microscopy (SEM) was used to characterize the electrode surface after different modification processes, such as Figure 4 As shown, Figure 4 A is a bare SPE that has only been activated, and the overall surface of the electrode is darker; Figure 4 B is Au NPs / SPE, which is brighter overall, and there are a large number of bright spots scattered on the electrode, indicating that Au NPs are successfully deposited on the SPE; Figure 4 C is the RGO-CMCS-Hemin / Pd NPs / AuNPs / SPE sensing interface. The brighter clusters in the center are due to the film-forming property of CMCS. The convex and brighter center can be judged to be palladium nanoparticles. The darker color between the clusters is due to the black graphene composite material, indicating that the RGO-CMCS-Hemin / Pd NPs composite material has been attached to the sensing interface. Figure 4 D is for GPC Apt / RGO-CMCS-Hemin / PdNPs / AuNPs / SPE presents a wrinkled packaging morphology, and the surface morphology is obviously different from Figure 4 C, and the dispersion is uneven, which is because the addition of the aptamer makes the electrode surface thick and thin. Figure 4 E is GPC3 / GPC3 Apt / RGO- CMCS-Hemin / Pd NPs / Au NPs / SPE has a raised bright spot, which is the nano-palladium particle. There is a small block in the middle left, which may be the exposed SPE. GPC3 specifically binds to the aptamer to form a more obvious wrapping state, indicating that the sensor was successfully prepared.
[0049] Step 3: Drawing of GPC3 working curve
[0050] (1) In GPC3 Apt3.0 μL of different concentrations of GPC3 (10.0 ng / mL, 25.0 ng / mL, 50.0 ng / mL, 65.0 ng / mL, 85.0 ng / mL, 100.0 ng / mL) were dropped onto the sensing interface of / RGO-CMCS-Hemin / PdNPs / AuNPs / SPE, respectively, and incubated in an incubator at 25 °C for 30 min, and a GPC3 blank group was set.
[0051] (2) The working electrode obtained above was placed in a 0.2 mol / L PBS buffer solution (pH = 6.5), and the DPV scanning was performed by a CHI660E electrochemical workstation to record the current peak. The DPV curves of different GPC3 concentrations are shown in Figure 5 When the GPC3 concentration was between 10.0 and 100 ng / mL, the difference between the peak value of the response current at this concentration and the peak value of the response current of the GPC3 blank group (Y) was linear with the GPC3 concentration (X). The linear equation was Y = 0.0551 X + 0.7297, and the correlation coefficient R 2 = 0.9814. According to formula C LOD = 3.0 Sb / b (Sb represents the standard deviation of six GPC blank groups, b represents the slope of the standard curve), and the minimum detection limit is calculated to be 9.898 ng / mL.
[0052] Step 4: Detection of GPC3 in actual serum samples
[0053] The spiked method was used to detect human serum samples containing different concentrations of GPC3. Serum with AFP concentrations of 3.53 ng / mL, 34.97 ng / mL, and greater than 500.0 ng / mL and three different concentrations of GPC3 solutions (25.0 ng / mL, 65.0 ng / mL, and 85.0 ng / mL) were mixed in a 1:1 ratio by shaking for 5 min, and 3.0 μL of GPC3 was added dropwise. Apt / RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE, incubated at 25 °C for 30 min, set up a serum blank control group, placed the electrode in 0.2 mol / L PBS buffer solution (pH = 6.5), used DPV scanning to record the current response peak, and recorded the difference between the current peak corresponding to the mixed solution of different concentrations and the current peak of the blank control group. According to the working curve Y = 0.0551 X + 0.7297 obtained in step 3, the concentration of GPC3 in the corresponding actual serum sample can be calculated, and the test results are shown in Table 1. It can be concluded that the recovery rate of the sensor is 93.73 ~ 118.83%, and the RSD is between 1.45 ~ 14.27%. The sensor has good application prospects.
[0054] Table 1 Detection results of GPC3 in actual serum samples
[0055] .
[0056] (Note: The serum sample was provided by the 924th Hospital of the Joint Logistics Support Force of the People's Liberation Army of China).
Claims
1. A method for detecting GPC3 using an electrochemical aptamer sensor based on a composite material of reduced graphene oxide-carboxymethyl chitosan-hemin / nanopalladium RGO-CMCS- Hemin / Pd NPs for non-diagnostic purposes, comprising the following steps: Step 1: Preparation of RGO-CMCS-Hemin / Pd NPs composites (1) Preparation of reduced graphene oxide RGO: 30.0 mg of graphene oxide GO was dispersed in 30.0 mL of distilled water, ultrasonically crushed for 2 h, and 90.0 mg of ascorbic acid AA was added for reduction to obtain a 1.0 mg / mL RGO suspension; (2) Preparation of reduced graphene oxide-hemin RGO-Hemin: Weigh 10.0 mg of hemin Hemin, add 20.0 µL of ammonia water, and then add 10.0 mL of distilled water to obtain a 1.0 mg / mL Hemin solution; take 10.0 mL of 1.0 mg / mL RGO suspension, add 10.0 mL of Hemin solution, mix well, and then ultrasonically crush to obtain a 1.0 mg / mL RGO-Hemin suspension; (3) Preparation of reduced graphene oxide-carboxymethyl chitosan-hemin RGO-CMCS-Hemin: Weigh 50.0 mg of carboxymethyl chitosan CMCS and add it to 1.0% acetic acid solution, stir evenly to obtain a 1.0 mg / mL CMCS solution, take 10.0 mL of CMCS solution and add it to the RGO-Hemin solution, ultrasonically crush it, and obtain a 1.0 mg / mL RGO-CMCS-Hemin solution; (4) Preparation of reduced graphene oxide-carboxymethyl chitosan-hemin chloride / nanopalladium RGO-CMCS-Hemin / Pd NPs composite materials: 2.0 mL of 20.0 mmol / L sodium hexachloropalladate solution and 10.0 mg AA were added to 10.0 mL of RGO-CMCS-Hemin solution; stirred for 16 h and then taken out; centrifuged at 8000 r / min for 15 min; after centrifugation, the supernatant was removed with a pipette, the black precipitate was scraped, washed and dissolved with ultrapure water to obtain 1.0 mg / mL of RGO-CMCS-Hemin / Pd NPs solution; Step 2: Electrode modification and biosensing interface construction (1) The screen-printed electrode SPE was immersed in a dilute sulfuric acid solution with a concentration of 0.5 mol / L and cyclically scanned 20 times in the voltage range of 0.4 V to 1.2 V by electrochemical method; (2) Immerse the activated SPE electrode in 5.0 mL of 0.01% HAuCl 4 In the solution, Au NPs / SPE was obtained by electrochemical constant potential electrodeposition at - 0.5 V for 2 min; (3) The RGO-CMCS-Hemin / Pd NPs suspension was dropped onto the surface of Au NPs / SPE, incubated at 25 °C for 2 h, washed and dried to obtain RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE; (4) GP3 Apt The surface of RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE was added dropwise, incubated at 25 °C for 1 h, blocked with 0.5% BSA, washed and dried to obtain the biosensor interface GPC3. Apt / RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE; Step 3: Drawing of GPC3 working curve (1) GPC3 solutions of different concentrations were added dropwise to the obtained biosensor interface, incubated at 25 °C for 30 min, washed and dried to obtain GPC3 / GPC3 Apt / RGO-CMCS-Hemin / Pd NPs / Au NPs / SPE working electrode; (2) The obtained working electrode was immersed in a 0.2 mol / L PBS buffer solution and DPV scanning was performed with a scanning range of 0.2 V to 1.0 V and a scanning rate of 0.01 V / s; the peak current response was recorded; (3) Based on the relationship between the difference between the peak value of the response current and the peak value of the response current of the GPC3 blank group and the GPC3 concentration, a working curve was drawn. The linear equation obtained was Y = 0.0551 X + 0.7297, and the minimum detection limit was calculated to be 9.898 ng / mL; Step 4: Detection of GPC3 in real samples (1) The actual serum sample and GPC3 were mixed evenly and added dropwise to the biosensor interface obtained in step 2, and the working electrode was obtained after incubation at a constant temperature of 25°C for 30 min; (2) The obtained working electrode was immersed in a 0.2 mol / L PBS buffer solution and scanned using the DPV of an electrochemical workstation with a scanning range of 0.2 V to 1.0 V and a scanning rate of 0.01 V / s, and the response current value of the sensor was recorded; (3) According to the linear regression equation of the working curve obtained in step 3, the concentration of GPC3 in the actual sample to be tested is calculated.
Citation Information
Patent Citations
Application of high-positive-charge green fluorescent protein in preparing liver cancer early diagnostic kit
CN107085109A
Multi-antibody combined detection kit for early liver cancer markers and use method thereof
CN109580951A
Method for detecting GPC3 based on RGO-CS-Hemin / Au NPs nano composite material
CN111413384A
Method for detecting GPC3 based on RGO-CS-Fc / Pt-Pd NPs nano composite material
CN111413385A
Method for detecting GPC3 based on RGO-Hemin / Au NPs nano composite material
CN111505077A