Fixing device and image forming device provided with the fixing device

By forming an alumina film layer on the surface of the heat-cooling component and filling a solid lubricant, the problem of deformation and wear of the coating material in the firing process is solved, and the stability of the heat-cooling component and the long-term good performance of the fixing device are achieved.

CN114830040BActive Publication Date: 2024-11-22RICOH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080086865.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-12-17
Filing Date
2020-11-17
Publication Date
2024-11-22
Estimated Expiration
2040-11-17

AI Technical Summary

Technical Problem

When using a heat-smoothing component containing a PTFE coating material, the heat-smoothing component may be deformed during the firing process, increasing the unit torque of the fixing device, and the aggregation of the coating surface causes the fixing belt to wear, affecting the fixing effect.

Method used

A homogenized component made of aluminum or aluminum alloy is used, and an alumina film layer is formed on its surface. A solid lubricant is filled with multiple micropores to ensure that the thickness of the alumina film layer is less than the thickness of the sliding layer to maintain homogenized heat. Performance and reduce sliding resistance.

Benefits of technology

Effectively prevent deformation of the heat-homogenized components, maintain good lubricity and heat-homogenized properties, reduce the sliding resistance of the fixing device, and improve the reliability and sustainability of the fixing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114830040B_ABST
    Figure CN114830040B_ABST
Patent Text Reader

Abstract

The fixing device includes a fixing component, a heat source, a pressure component, a clamping portion forming component, and a heat equalizing component. The heat equalizing component is configured to cover the surface of the clamping portion forming component facing the fixing component and transfer heat in the axial direction of the fixing component. The fixing component includes at least a cylindrical substrate made of metal, and a sliding layer made of a heat-resistant resin on the inner peripheral surface of the substrate. The heat equalizing component made of aluminum or an aluminum alloy has an aluminum oxide film layer on the surface facing the inner peripheral surface of the fixing component. A plurality of micropores in the aluminum oxide film layer are filled with a solid lubricant having a friction coefficient lower than that of the aluminum oxide film layer. The thickness of the aluminum oxide film layer is less than the thickness of the sliding layer of the fixing component.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present disclosure relate to a fixing device and an image forming apparatus provided with the fixing device. Background Art

[0002] In recent years, a fixing device has been proposed which achieves reliable fixing performance by a thin film-like endless belt having a low heat capacity and directly heated by a fixing heat source even when the fixing device is mounted in an image forming apparatus having high productivity.

[0003] In this fixing device, a rotating member disposed opposite to the outer peripheral surface of the endless fixing belt is pressed against a supporting member (or a nip forming member) fixed inside the fixing belt (or inside the ring formed by the fixing belt) through the fixing belt to form a fixing nip between the rotating member and the supporting member. The nip forming member may be provided with a heat-dissipating member made of a metal material with high thermal conductivity to uniformly heat the fixing belt, which can reduce the temperature increase of the end of the fixing belt during continuous conveyance of the recording medium.

[0004] The structure of such a fixing device is known, in which a sheet (or sliding sheet) made of a fiber such as polytetrafluoroethylene (PTFE) impregnated with a lubricant such as silicone grease is arranged on the surface of the nip forming member to reduce the sliding resistance (or torque) between the fixing belt and the nip forming member. However, the sliding sheet can be used as a heat insulating member, and there is a concern that the heat equalization effect of the fixing belt is hindered.

[0005] In order to solve this situation, a structure is also known in which a coating having sliding properties is directly applied to the surface of the heat-sinking member instead of a sliding sheet (for example, Patent Document 1 and Patent Document 2). In addition, a structure is also proposed in which appropriate surface roughness is formed on the surface of the coating to retain grease.

[0006] Citation List

[0007] Patent Literature

[0008] [Patent Document 1] Japanese Unexamined Patent Application Publication No. 2017-125922

[0009] [Patent Document 2] Japanese Unexamined Patent Application Publication No. H9-197880 Summary of the invention

[0010] Technical issues

[0011] When the surface of the heat spreader is coated with a coating material containing PTFE, for example, a sintering process may be performed to improve the adhesion and strength of the coating film. However, since the heat spreader is a thin plate, the heat spreader may be deformed by heat during the sintering process. In order to prevent such deformation of the heat spreader, the sintering process is performed at a temperature lower than the temperature at which the original coating film can exert its performance.

[0012] When agglomerates are generated in the coating material, minute protrusions are formed on the coating film surface. The protrusions promote wear of the inner surface of the fixing belt (or the inner surface of the sleeve), generating wear powder, and therefore, the unit torque of the fixing device may increase at an early stage.

[0013] In view of the above problems, a general object of the present invention is to provide a fixing device which can perform good fixing over time by maintaining reduced sliding resistance between the heat-equalizing member and the fixing member without impairing the reliability and heat-equalizing performance of the heat-equalizing member.

[0014] Solutions to the problem

[0015] In order to solve the above problems and achieve the above objects, a fixing device as described in the attached claims is provided. Advantageous embodiments are defined by dependent claims. Advantageously, the fixing device comprises: a rotatable annular fixing member, a heat source, a pressure member, a clamping portion forming member, and a heat equalizing member. The heat source is configured to heat the fixing member. The pressure member is arranged on the outside of the fixing member, facing the fixing member. The clamping portion forming member is arranged on the inside of the fixing member, and a clamping portion is formed between the fixing member and the pressure member. The heat equalizing member is configured to cover the surface of the clamping portion forming member facing the fixing member, and transfer heat along the axial direction of the fixing member. The fixing member comprises at least: a cylindrical substrate made of metal, and a sliding layer made of heat-resistant resin on the inner peripheral surface of the substrate. The heat equalizing member is made of aluminum or an aluminum alloy. The heat equalizing member has an aluminum oxide film layer on the surface facing the inner peripheral surface of the fixing member. The plurality of micropores in the aluminum oxide film layer are filled with a solid lubricant having a friction coefficient lower than that of the aluminum oxide film layer. The thickness of the aluminum oxide film layer is smaller than that of the sliding layer of the fixing member.

[0016] Effects of the Invention

[0017] In a fixing device according to an embodiment of the present invention, an aluminum oxide film layer is formed on the surface of a heat spreader, and a solid lubricant is filled in a plurality of micropores in the aluminum oxide film layer, so that the fixing device maintains lubrication between the heat spreader and the fixing member. In addition, the thickness of the aluminum oxide film layer is less than the thickness of the sliding layer of the fixing member, so that the heat spread performance of the heat spreader is not impaired. Moreover, compared with a coating treatment, the aluminum oxide film treatment does not cause deformation or slight protrusion of the heat spreader, thereby improving the reliability of the heat spreader. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The accompanying drawings are intended to illustrate example embodiments of the present invention and should not be interpreted as limiting the scope thereof. Unless explicitly stated, the accompanying drawings should not be considered to be drawn to scale. Moreover, the same or similar reference numerals represent the same or similar components in several views.

[0019] Figure 1 is a schematic diagram of an imaging device according to an embodiment of the present disclosure.

[0020] Figure 2 is a schematic cross-sectional view of a fixing device according to an embodiment of the present disclosure.

[0021] Figure 3 is a cross-sectional view of a fixing belt according to an embodiment of the present disclosure.

[0022] Figure 4 yes Figure 2 Schematic perspective view of an axial end portion of the fixing device shown.

[0023] Figure 5 is an exploded perspective view of a clamping portion forming member, a supporting member, and a heat spreading member constituting a clamping portion forming unit according to an embodiment of the present disclosure.

[0024] Figure 6 is a perspective view of a heat spreader according to one embodiment of the present disclosure.

[0025] Figure 7 yes Figure 6 An enlarged cross-sectional view of the heat spreader is shown.

[0026] Figure 8 1 is a first diagram illustrating a method for manufacturing a heat spreader according to an embodiment of the present disclosure.

[0027] Fig. 9 FIG. 2 is a second diagram illustrating a method for manufacturing a heat spreader according to an embodiment of the present disclosure.

[0028] Fig.10 FIG. 3 is a third diagram illustrating a method for manufacturing a heat spreader according to an embodiment of the present disclosure.

[0029] Fig.11A is a cross-sectional view of a heat equalizing member and a fixing belt according to a comparative example, Fig. 11B is a cross-sectional view of a heat spreader and a fixing belt according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0030] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the present invention.As used herein, the singular forms "a", "an", and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise.

[0031] When describing the embodiments shown in the drawings, specific terms are used for clarity. However, the disclosure of this specification is not intended to be limited to the specific terms so selected, and it should be understood that each specific element includes all technical equivalents having similar functions, operating in a similar manner and achieving similar results.

[0032] Figure 1 1 is a schematic diagram of an image forming apparatus according to an embodiment of the present invention. The image forming apparatus 1 is a color laser printer, and four image forming units 4Y, 4C, 4M and 4K are arranged side by side in the center of the printer body of the image forming apparatus 1 along the direction in which the intermediate transfer belt 30 extends. The image forming units 4Y, 4C, 4M and 4K have the same structure and contain developers of different colors corresponding to the color separation components of the color image, namely yellow (Y), cyan (C), magenta (M) and black (K).

[0033] Specifically, each of the image forming units 4Y, 4C, 4M, and 4K serving as image stations includes, for example, a drum-shaped photoreceptor 5 as a latent image carrier, a charging device 6 for charging the surface of the photoreceptor 5, a developing device 7 for supplying toner to the surface of the photoreceptor 5, and a cleaning device 8 for cleaning the surface of the photoreceptor 5. Figure 1 In the figure, only the photoconductor 5, the charging device 6, the developing device 7 and the cleaning device 8 of the image forming unit 4K for forming a black toner image are denoted by symbolic numerals, while the symbolic numerals are omitted for the other image forming units 4Y, 4C and 4M.

[0034] An exposure device 9 is disposed below the imaging units 4Y, 4C, 4M and 4K for exposing the surface of the photoreceptor 5. The exposure device 9 includes, for example, a light source, a polygonal mirror, an f-θ lens and a reflecting mirror for irradiating the surface of each photoreceptor 5 with a laser beam according to image data.

[0035] The transfer device 3 is disposed above the image forming units 4Y, 4C, 4M and 4K, and includes an intermediate transfer belt 30 as a transfer body, four primary transfer rollers 31 as primary transfer devices, and a secondary transfer roller 36 as a secondary transfer device. The transfer device 3 also includes a secondary transfer support roller 32, a cleaning support roller 33, a tension roller 34, and a belt cleaning device 35.

[0036] The intermediate transfer belt 30 is an endless belt that is wound around a secondary transfer support roller 32, a cleaning support roller 33, and a tension roller 34. When the secondary transfer support roller 32 is driven to rotate, the intermediate transfer belt 30 moves along the Figure 1 The machine runs circumferentially (or rotates) in the direction indicated by the arrow.

[0037] Each of the four primary transfer rollers 31 sandwiches the intermediate transfer belt 30 with the corresponding photoconductor 5, thereby forming a primary transfer nip between the intermediate transfer belt 30 and the corresponding photoconductor 5. The primary transfer rollers 31 are connected to a power source of the printer body, and the power source applies at least one of a predetermined direct current (DC) voltage and a predetermined alternating current (AC) voltage to the primary transfer rollers 31.

[0038] The secondary transfer roller 36 and the secondary transfer backup roller 32 sandwich the intermediate transfer belt 30, thereby forming a secondary transfer nip between the secondary transfer roller 36 and the intermediate transfer belt 30. Similar to the primary transfer roller 31, the secondary transfer roller 36 is connected to a power source of the printer body, and the power source applies at least one of a predetermined DC voltage and a predetermined AC voltage to the secondary transfer roller 36.

[0039] The belt cleaning device 35 includes a cleaning brush and a cleaning blade, which are arranged to contact the intermediate transfer belt 30. The bottle housing portion 2 is provided at the upper portion of the printer body, and four toner bottles 2Y, 2C, 2M, and 2K that contain new toner are detachably mounted in the bottle housing portion 2. Toner supply pipes are provided between the toner bottles 2Y, 2C, 2M, and 2K and the corresponding developing devices 7. The new toner is supplied from each of the toner bottles 2Y, 2C, 2M, and 2K to the corresponding developing devices 7 through the corresponding toner supply pipes.

[0040] At the lower part of the printer body, there are provided, for example, a paper feed tray 10 for accommodating a plurality of sheets of paper P as recording media and a paper feed roller 11 for feeding the plurality of sheets of paper P one at a time from the paper feed tray 10. Examples of recording media include, but are not limited to, plain paper, thick paper, postcards, envelopes, thin paper, coated paper, coated paper, tracing paper, and overlay (OHP) transparent sheets. The image forming device 1 may include a bypass feeder that inputs such recording media placed on the bypass feeder into the image forming device 1.

[0041] Inside the printer body, a conveying path R is formed by internal components of the image forming device 1, along which the paper P is conveyed from the paper supply tray 10 through the secondary transfer nip and discharged to the outside of the image forming device 1. Along the conveying path R, in the paper conveying direction in which the paper P is conveyed, a registration roller pair 12 is provided upstream of the position of the secondary transfer roller 36, and the registration roller pair 12 is a conveying device that conveys the paper P to the secondary transfer nip.

[0042] Furthermore, the fixing device 20 is provided downstream of the position of the secondary transfer roller 36 in the paper conveying direction, and the fixing device 20 fixes the unfixed image transferred onto the paper P onto the paper P. Furthermore, the paper discharge roller pair 13 is provided downstream of the fixing device 20 in the paper conveying direction along the conveying path R, and the paper discharge roller pair 13 discharges the paper P to the outside of the image forming apparatus 1. An output tray 14 is provided on the upper surface of the printer body, and a plurality of sheets of paper P discharged one sheet at a time to the outside of the image forming apparatus 1 are stacked on the output tray 14.

[0043] The basic operation of the printer according to the present embodiment will now be described. When the image forming operation starts, the photosensitive body 5 is driven in each of the image forming units 4Y, 4C, 4M, and 4K. Figure 1 Rotating clockwise, the charging device 6 uniformly charges the surface of the photoreceptor 5 to a predetermined polarity, and the exposure device 9 irradiates the charged surface of the photoreceptor 5 with a laser beam to form an electrostatic latent image on the surface of the photoreceptor 5. The image data exposed on the photoreceptor 5 is a monochrome image data obtained by decomposing a desired full-color image into respective color components of yellow, cyan, magenta, and black, and the developing device 7 supplies toner to the electrostatic latent image thus formed on the photoreceptor 5 to make the electrostatic latent image visible as a toner image.

[0044] At the same time, when the image forming operation starts, the secondary transfer back-up roller 32 is driven to rotate counterclockwise ( Figure 1 ), and along Figure 1 The intermediate transfer belt 30 rotates in the direction indicated by the middle arrow. A constant voltage or a constant current control voltage having a polarity opposite to that of the charged toner is supplied to each primary transfer roller 31, and thus a transfer electric field is generated at the primary transfer nip between each primary transfer roller 31 and the corresponding photoreceptor 5.

[0045] When the toner images of different colors formed on the photoreceptors 5 reach the primary transfer nips due to the rotation of the photoreceptors 5, the toner images are transferred from the photoreceptors 5 to the intermediate transfer belt 30 by the transfer electric fields generated at the primary transfer nips, so that the toner images are sequentially superimposed one by one on the intermediate transfer belt 30, thereby forming a full-color toner image on the surface of the intermediate transfer belt 30. The cleaning device 8 removes residual toner from the photoreceptors 5, which in this case is toner that has not been transferred to the intermediate transfer belt 30 and therefore remains on the photoreceptors 5. Then, the discharger discharges the surface of the photoreceptors 5 so that the surface potential of the photoreceptors 5 is initialized.

[0046] At the lower part of the image forming apparatus 1, the paper supply roller 11 starts to rotate to convey the paper P from the paper supply tray 10 to the conveying path R. The registration roller pair 12 conveys the paper P conveyed to the conveying path R to the secondary transfer nip between the secondary transfer roller 36 and the secondary transfer backup roller 32 at an appropriate time. At this time, the secondary transfer roller 36 is supplied with a transfer voltage having a polarity opposite to that of the charged toner contained in the full-color toner image formed on the intermediate transfer belt 30, thereby generating a transfer electric field at the secondary transfer nip.

[0047] Thereafter, when the toner image on the intermediate transfer belt 30 reaches the secondary transfer nip as the intermediate transfer belt 30 rotates, the transfer electric field generated at the secondary transfer nip transfers the toner image from the intermediate transfer belt 30 onto the paper P in one piece. The belt cleaning device 35 removes residual toner from the intermediate transfer belt 30, which in this case is toner that has not been transferred onto the paper P and therefore remains on the intermediate transfer belt 30, and the removed toner is conveyed and collected in a waste toner container provided inside the printer body.

[0048] Thereafter, the paper P is conveyed to the fixing device 20 , and the fixing device 20 fixes the toner image on the paper P to the paper P. The paper discharge roller pair 13 discharges the paper P to the outside of the image forming apparatus 1 , so that a plurality of papers P are stacked on the output tray 14 .

[0049] The image forming device 1 can form a monochrome image using any one of the image forming units 4Y, 4C, 4M and 4K, or can form a two-color image using two of the image forming units 4Y, 4C, 4M and 4K, or can form a three-color image using three of the image forming units 4Y, 4C, 4M and 4K.

[0050] like Figure 2 As shown, the fixing device 20 includes a fixing belt 21 formed in an endless shape, a pressure roller 22, a temperature sensor 29, a separation component 40, and various components such as heaters 23A and 23B, a clamping portion forming component 24, a support component 25, a heat equalization component 27, and reflection components 28A and 28B arranged in the loop formed by the fixing belt 21. The fixing belt 21 and the components arranged in the loop formed by the fixing belt 21 constitute a belt unit 21U that is detachably connected to the pressure roller 22. The fixing belt 21 is a thin, bendable endless belt as a cylindrical fixing component. The pressure roller 22 is a pressure component that contacts the outer peripheral surface of the fixing belt 21. The fixing belt 21 is heated by radiant heat of heaters 23A and 23B as a plurality of heat sources (or fixing heat sources) arranged in the fixing belt 21 (or in the loop formed). The heaters 23A and 23B as heat sources generally use halogen heaters. Alternatively the heat source may be, for example, an induction heating device, a resistive heating generator or a carbon heater.

[0051] A nip forming member 24 and a support member 25 are provided inside the fixing belt 21. The nip forming member 24 forms a fixing nip N between the fixing belt 21 and the pressure roller 22, and the support member 25 (as a support member) supports the nip forming member 24, and the support member 25 fixes and supports the nip forming member 24 arranged in the axial direction (width direction) of the fixing belt 21, thereby preventing the nip forming member 24 from being bent due to the pressure on the nip forming member 24 from the pressure roller 22. Therefore, the fixing nip N maintains a uniform width in the axial direction (i.e., longitudinal direction) of the pressure roller 22.

[0052] like Figure 3 As shown, the fixing belt 21 includes a cylindrical base 21a made of metal or heat-resistant resin, a release layer 21b made of heat-resistant resin and provided on the outer peripheral surface of the base 21a, and a sliding layer 21c made of resin and provided on the inner peripheral surface of the base 21a.

[0053] The thickness of the substrate 21a ranges from 20 μm to 50 μm. The substrate 21a is made of a metal material such as nickel or steel (SUS) using stainless steel, or a resin material such as polyimide (PI) or polyamide-imide (PAI).

[0054] The layer thickness of the release layer 21b ranges from 10 μm to 50 μm. The release layer 21b is made of a material such as tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA) or polytetrafluoroethylene (PTFE). The release layer 21b ensures the releasability of the fixing belt 21 relative to the toner image on the paper P, wherein "releasability" refers to the peeling of an object from another object attached to the object, and "releasability" refers to the ease with which objects can be separated from each other.

[0055] In addition, an elastic layer 21d made of silicone rubber or the like may be provided between the base material 21a and the release layer 21b. In the case where the fixing belt 21 is not provided with the elastic layer 21d, although the fixing belt 21 has the advantages of small heat capacity and improved fixability, since the fixing belt 21 and the pressure roller 22 sandwich and press the unfixed image on the paper P in the fixing nip portion N, the slight surface roughness of the fixing belt 21 may be transferred to the toner image of the paper P, resulting in an orange peel image with uneven gloss similar to orange peel appearing in the solid image portion of the image, where the orange peel image refers to an image with slight surface roughness. In order to solve this problem, the thickness of the elastic layer 21d made of silicone rubber is preferably not less than 100 μm, and the deformation of the elastic layer 21d absorbs the slight surface roughness in the fixing belt 21, thereby preventing the appearance of the orange peel image.

[0056] As the sliding layer 21c, for example, PAI or fluororesin having heat resistance and sliding properties is preferred. As the fluororesin, PTFE or PFA is preferred. When the sliding layer 21c is made of a mixed coating material of fluororesin and PAI, the sliding layer 21c has a reduced dynamic friction coefficient and improves adhesion with the substrate 21a.

[0057] The sliding layer 21c is applied to the inner peripheral surface of the base material 21a of the fixing belt 21 by spraying to have a thickness of about 15 μm. However, if the thickness is less than 15 μm, particularly less than 10 μm, coating unevenness (i.e., local unevenness in color in the coating film) may occur.

[0058] The sliding layer 21c thus formed has a dynamic friction coefficient of not more than 0.1 and a tensile elastic modulus of not more than 5000 MPa.

[0059] In order to reduce the heat capacity, the fixing belt 21 has a total thickness of not more than 1 mm and a ring diameter of 20 mm to 40 mm. In order to further reduce the heat capacity, the fixing belt 21 preferably has a total thickness of not more than 0.2 mm, more preferably not more than 0.16 mm, and the ring diameter of the optimal fixing belt 21 is not more than 30 mm.

[0060] Back to Figure 2 , and continue to describe other components. The clamping portion forming member 24 is made of a heat-resistant material having good mechanical strength and heat resistance of not less than 200°C, and is particularly made of a heat-resistant resin such as PI or polyetheretherketone (PEEK) or a heat-resistant resin reinforced with glass fiber. Therefore, the clamping portion forming member 24 does not undergo thermal deformation at a temperature within the fixing temperature range for fixing the toner image to the paper P, thereby maintaining a stable state of the fixing clamping portion N and maintaining stable output image quality. The opposite longitudinal ends of the support member 25 and the opposite longitudinal ends of the heaters 23A and 23B are fixed and supported on a pair of side plates of the fixing device 20 or a pair of brackets provided separately.

[0061] The heat-equalizing member 27 is a heat-transfer auxiliary member that promotes heat transfer in the axial direction of the fixing belt 21, and covers the surface of the clamping portion forming member 24 that faces the inner circumference of the fixing belt 21. The heat-equalizing member 27 actively transfers heat in the axial direction (width direction) of the fixing belt 21, that is, in the longitudinal direction of the heat-equalizing member 27, thereby preventing heat from staying in the opposite axial end regions of the fixing belt 21 when the small-sized paper P is conveyed on the fixing belt 21, and eliminating temperature unevenness in the axial direction of the fixing belt 21. The heat-equalizing member 27 of this embodiment is made of aluminum or an aluminum alloy material, which has a high thermal conductivity, so that heat can be transferred in a short time.

[0062] The heat equalizing member 27 has a belt sliding surface that is in direct contact with the inner peripheral surface of the fixing belt 21, and serves as a nip forming surface. Figure 2In the embodiment, the belt sliding surface is flat, or the belt sliding surface can be made into a concave shape or other suitable shapes. For example, when the paper P is discharged from the fixing nip N, the leading edge of the paper P is guided to the pressure roller 22, thereby facilitating the separation of the paper P from the fixing belt 21 and preventing paper jams.

[0063] In order to reduce the wear of the fixing belt 21 and the heat equalizing member 27, the inner peripheral surface of the fixing belt 21 may be coated with fluorine oil or fluorine grease containing fluorine compounds as a lubricant. The lubricant may be fluorine grease or silicone grease containing fluorine particles as a thickener.

[0064] The support member 25 has a T-shaped cross section and includes an arm 25a extending from the fixing nip N. The arm 25a is inserted between the heaters 23A and 23B as fixed heat sources to separate the heaters 23A and 23B from each other. One of the heaters 23A and 23B has a heating area in the longitudinal center portion to heat the toner image on the small-sized paper P passing through the fixing nip N, and the other of the heaters 23A and 23B has heating areas in the longitudinal both end portions to heat the toner image on the large-sized paper P passing through the fixing nip N.

[0065] The power supply located inside the printer body supplies power to the heaters 23A and 23B so that the heaters 23A and 23B generate heat. Specifically, the controller (e.g., a processor) is operably connected to the power supply and the temperature sensor 29. The power supply to the heaters 23A and 23B is controlled according to the temperature of the outer peripheral surface of the fixing belt 21 detected by the temperature sensor 29 disposed opposite to the outer peripheral surface of the fixing belt 21. In this way, the heating control of the heaters 23A and 23B adjusts the temperature of the fixing belt 21 to the desired fixing temperature.

[0066] The reflecting member 28A is disposed between the heater 23A and the support member 25, and the reflecting member 28B is disposed between the heater 23B and the support member 25. The reflecting members 28A and 28B reflect the heat from the heaters 23A and 23B onto the fixing belt 21, thereby improving the heating efficiency of the heaters 23A and 23B to heat the fixing belt 21. In addition, the reflecting members 28A and 28B prevent the radiant heat from the heaters 23A and 23B from heating the support member 25, thereby reducing the waste of energy. Alternatively, instead of the reflecting members 28A and 28B, the respective heater side surfaces of the support member 25 facing the heaters 23A and 23B can be subjected to insulation treatment or mirror polishing to improve the heating efficiency of the heaters 23A and 23B and reduce the waste of energy.

[0067] The pressure roller 22 is composed of a core, an elastic layer made of, for example, silicone rubber foam or fluororubber foam provided on the surface of the core, and a release layer made of, for example, PFA or PTFE provided on the surface of the elastic layer. When the pressure roller 22 is pressed against the fixing belt 21 by a pressure device such as a spring, the elastic layer of the pressure roller 22 is deformed, thereby forming a fixing nip N having a predetermined width in a pressure contact area between the fixing belt 21 and the pressure roller 22.

[0068] The pressure roller 22 is driven to rotate by a driving source such as a motor provided inside the printer body. When the driving source drives the pressure roller 22 to rotate, the driving force of the driving source is transmitted from the pressure roller 22 to the fixing belt 21 at the fixing nip N, thereby rotating the fixing belt 21. When the fixing belt 21 rotates, the fixing belt 21 located at the fixing nip N is sandwiched between the pressure roller 22 and the heat equalizing member 27. On the other hand, the circumferential width of the fixing belt 21 except for the nip width is guided by flanges fixed to a pair of side plates located at opposite axial ends of the fixing belt 21.

[0069] In the present embodiment, the pressure roller 22 is a solid roller, but it may be a hollow roller, that is, a tube. In the case where the pressure roller 22 is a hollow roller, a heat source such as a halogen heater may be provided inside the pressure roller 22. The elastic layer of the pressure roller 22 is made of solid rubber, and in the case where there is no heat source inside the pressure roller 22, the elastic layer may also be made of sponge rubber. Because sponge rubber has higher thermal insulation, it absorbs less heat from the fixing belt 21.

[0070] The temperature sensor 29 is provided at an appropriate position relative to the outer peripheral surface of the fixing belt 21, for example, upstream of the fixing nip N in the rotation direction of the fixing belt 21, to detect the temperature of the fixing belt 21. The separation member 40 is provided at a downstream position in the paper conveying direction of the fixing device 20 to separate the paper P from the fixing belt 21. The pressure device can release the pressure of the pressure roller 22 on the fixing belt 21.

[0071] Figure 4 yes Figure 2 The figure is a schematic perspective view of the axial end portions of the fixing device 20. A flange 45 is arranged at each axial end portion of the fixing belt 21. Figure 4 Indicates one axial end portion of the fixing belt 21 .

[0072] The flange 45 is hollow and open on both axial sides of the flange 45. The flange 45 includes a receiving portion 46 extending in the axial direction of the flange 45 and a jaw portion 47 protruding radially from the receiving portion 46. The receiving portion 46 is partially cylindrical or cylindrical. In a circumferential partial area of ​​the receiving portion 46, there is a cutout 48. The clamping portion forming member 24 and the heat-dissipating member 27 are inserted into the space defined by the cutout 48.

[0073] If the fixing belt 21 moves or tilts in the axial direction of the fixing belt 21 as the fixing belt 21 rotates, the axial end of the fixing belt 21 contacts the receiving portion 46, restricting the axial movement of the fixing belt 21. The jaw portion 47 is fixed to the side plate of the fixing device 20. Alternatively, an annular plate made of a material having good sliding properties relative to the fixing belt 21 may be inserted between the receiving portion 46 and the axial end of the fixing belt 21.

[0074] Figure 5 is an exploded perspective view of a clamping portion forming member, a supporting member, and a heat spreading member constituting a clamping portion forming unit according to an embodiment of the present disclosure.

[0075] like Figure 5 As shown, the heat-equalizing member 27 provided on the fixing nip side of the nip forming member 24 is joined to the nip forming member 24 having a substantially rectangular shape so that the heat-equalizing member 27 covers the nip side surface 24c of the nip forming member 24 facing the inner peripheral surface of the fixing belt 21, thereby joining the heat-equalizing member 27 to the nip forming member 24. The heat-equalizing member 27 may be joined to the nip forming member 24 by, for example, a protrusion that is joined to the nip forming member 24, or may be joined to the nip forming member 24 by, for example, an adhesive that is joined to the nip forming member 24.

[0076] The heat equalizing member 27 includes a belt sliding contact surface 27a facing the inner peripheral surface of the fixing belt 21. The clamping portion forming member 24 includes a support side surface on the opposite side to the fixing clamping portion side surface 24c. The support member 25 includes a clamping portion side surface facing the fixing clamping portion N. The clamping portion side surface of the support member 25 supports the support side surface of the clamping portion forming member 24. Preferably, the support side surface of the clamping portion forming member 24 and the clamping portion side surface of the support member 25 that are in contact with each other may respectively form a recess and a protrusion (e.g., a boss and a pin), for example, to reduce the contact area between the clamping portion forming member 24 and the support member 25.

[0077] Next, characteristic configurations of embodiments according to the present disclosure will be described.

[0078] Figure 6 is a perspective view of a heat spreader according to an embodiment of the present disclosure, Figure 7 yes Figure 6 An enlarged cross-sectional view of the heat sink is shown. Figure 6 and Figure 7 , the structure of the heat equalizing component 27 is described in detail.

[0079] like Figure 6 As shown, according to the present embodiment, the heat spreader 27 made of aluminum or aluminum alloy includes an aluminum oxide film (hereinafter referred to as an aluminum oxide film 54) on the surface of the heat spreader 27 (specifically, the surface opposite to the inner peripheral surface of the fixing belt 21). Figure 7As shown, molybdenum disulfide (MoS2) 56 used as a solid lubricant fills a plurality of micropores 54a regularly arranged in an aluminum oxide film layer 54 (located on an aluminum substrate 52).

[0080] The aluminum oxide film layer 54 is very hard and has good wear resistance, especially against abrasive wear. On the other hand, the molybdenum disulfide 56 is a solid lubricant, and its friction coefficient is lower than that of the aluminum oxide film layer 54. With this structure, the heat spreader 27 of this embodiment serves as a sliding member having both wear resistance and lubricity to the inner peripheral surface of the fixing belt 21.

[0081] Figures 8 to 10 The method for manufacturing a heat spreader according to an embodiment of the present invention is described. Figure 8 As shown, an aluminum substrate 52 is electrolyzed once by a known anodizing method to form an aluminum oxide film layer 54 on the surface of the aluminum substrate 52. In the aluminum oxide film layer 54, countless (multiple) micropores 54a arranged regularly are generated.

[0082] The thickness t of the aluminum oxide film layer 54 can be adjusted according to the amount of charge used for electrolysis (=current×time). Since the thermal conductivity of the aluminum oxide film layer 54 is lower than that of the aluminum substrate 52, it is preferable that the aluminum substrate 52 is as thin as possible. The aluminum oxide film layer 54 and the sliding layer 21c (see FIG. 2 ) of the fixing belt 21 sliding thereon are Figure 3 ) compared to other materials, it has very hard properties.

[0083] For example, when compared with Martens hardness, the value of the sliding layer 21c of the fixing belt 21 is 100 N / mm 2 Up to 300N / mm 2 , and the value of the aluminum oxide film layer 54 is about 3000N / mm 2 .

[0084] Therefore, in the present embodiment, the thickness t of the aluminum oxide film 54 is at least smaller than the thickness of the sliding layer 21c of the fixing belt 21. As described above, the thickness of the sliding layer 21c of the fixing belt 21 is about 15 μm, and no uneven coating occurs. Therefore, in the present embodiment, the thickness t of the aluminum oxide film 54 is about 5 μm, which is about one-third of the thickness of the sliding layer 21c of the fixing belt 21. The thickness t of the aluminum oxide film 54 is an example, but is not limited thereto.

[0085] The pore diameter d of the micropore 54a varies depending on the treatment liquid used for the anodizing treatment, but is approximately The number of micropores 54a is such that the micropores 54a occupy 5% to 40% of the surface area of ​​the heat spreader 27. The above-mentioned pore diameter d and the number of micropores 54a are examples, but are not limited thereto.

[0086] Next, in an aqueous solution containing thiomolybdate as a main component, the aluminum substrate 52 on which the aluminum oxide film layer 54 is formed is used as an anode for secondary electrolysis. Fig. 9 As shown, molybdenum sulfide (i.e., molybdenum disulfide 56) is precipitated and fixed in the plurality of micropores 54a. The precipitation starts from the base 54b of the plurality of micropores 54a and advances toward the inlet (or outermost layer) of the plurality of micropores 54a as the electrolysis time passes.

[0087] Now, it is explained why molybdenum sulfide (i.e., molybdenum disulfide 56) is precipitated from the base 54b. The thiomolybdate in the secondary electrolyte is decomposed into thiomolybdate ions. Since these ions are negatively charged, they are attracted to the anode and enter the micropores 54a by electrophoresis or diffusion. Since the size of these ions is much smaller than that of the micropores 54a, these ions reach the deep part of the micropores 54a. Therefore, molybdenum sulfide (i.e., molybdenum disulfide 56) is precipitated from the base 54b of the plurality of micropores 54a.

[0088] When the above-precipitated molybdenum sulfide (i.e., molybdenum disulfide 56) is heat-treated after the secondary electrolysis, crystals having a graphite structure are formed. As a result, Fig.10 As shown, the plurality of micropores 54a in the aluminum oxide film layer 54 are filled with the molybdenum disulfide 56 from the base 54b of the plurality of micropores 54a to the outermost surface layer of the plurality of micropores 54a.

[0089] The heat equalizing member 27 of this embodiment has an aluminum oxide film layer 54 on the surface opposite to the inner peripheral surface of the fixing belt 21, and the plurality of micropores 54a in the aluminum oxide film layer 54 are filled with molybdenum disulfide 56 from the base 54b to the outermost layer of the plurality of micropores 54a. Since the aluminum oxide film layer 54 is formed by modifying the aluminum substrate 52, foreign matter is not mixed in when the aluminum oxide film layer 54 is formed. In addition, a tiny convex shape caused by uneven coating is not generated. Therefore, local wear of the inner surface of the fixing belt 21 can be prevented.

[0090] Furthermore, the molybdenum disulfide 56 fills the entire area in the depth direction of the aluminum oxide film layer 54. Therefore, even if the aluminum oxide film layer 54 is worn, as long as the aluminum oxide film layer 54 exists, the heat spreader 27 can provide the fixing belt 21 with good sliding properties, which are not changed from the initial stage.

[0091] In addition, in the present embodiment, the heat-scaling member 27 reduces the surface roughness of the surface opposite to the inner peripheral surface of the fixing belt 21. This is because the surface roughness for retaining grease is not particularly required. By reducing the surface roughness in this way, when the fixing belt 21 slides on the belt sliding contact surface 27a, the heat-scaling member 27 prevents damage to the inner peripheral surface of the fixing belt 21, thereby obtaining a further advantage. In the present embodiment, the arithmetic mean roughness Ra of the aluminum oxide film layer 54 is approximately 0.2 μm to 0.3 μm.

[0092] (Variation Example)

[0093] In the above embodiment, molybdenum disulfide is used as the solid lubricant, but the solid lubricant is not limited to molybdenum disulfide, and PTFE or fluorine grease may be impregnated and filled into the plurality of micropores 54a in the aluminum oxide film layer 54.

[0094] From the viewpoint of rigidity, the hardness (for example, Martens hardness) of the aluminum oxide film layer 54 is preferably greater than the hardness of the sliding layer 21c of the fixing belt 21. The hardness of the aluminum oxide film layer 54 is particularly preferably about 3 times, more preferably about 5 to 10 times, that of the sliding layer 21c of the fixing belt 21.

[0095] Next, the heat equalizing performance of the heat equalizing member according to the present embodiment will be described.

[0096] Fig.11A and Fig. 11B They are cross-sectional views of the heat-saturating component and the fixing belt, respectively. Specifically, Fig.11A As a comparative structure, the structures of the heat equalizing member 127 and the fixing belt 121 are shown. Fig. 11B The structures of the heat equalizing member 27 and the fixing belt 21 according to the embodiment of the present invention are shown.

[0097] Table 1 shows the comparison of the comparative structure of the fixing belt and the heat equalizing member and the structure of this embodiment.

[0098] Table 1

[0099]

[0100] like Fig.11A As shown, in the comparative structure, the sliding layers 121c and 53 are sandwiched between the aluminum base material 152 of the heat spreader 127 and the base material 121a of the fixing belt 121 to prevent mutual wear, and the sliding layer 53 is a well-known resin-based coating material such as a polyimide resin or a fluorine resin. An interface 60 exists between the aluminum base material 152 of the heat spreader 127 and the sliding layer 53. The total thickness of the sliding layers 121c and 53 is about 30μm.

[0101] As described above, the thickness of each of the sliding layers 121c and 53 is 15 μm for coating without causing coating unevenness.

[0102] In contrast, Fig. 11B As shown, in the structure of this embodiment, the sliding layer 21c and the aluminum oxide film layer 54 are sandwiched between the aluminum substrate 52 of the heat equalizing member 27 and the substrate 21a of the fixing belt 21, but there is no interface between the aluminum substrate 52 of the heat equalizing member 27 and the aluminum oxide film layer 54. The total thickness of the sliding layer 21c and the aluminum oxide film layer 54 is about 20 μm.

[0103] Since the distance between the aluminum substrate 52 of the heat spreader 27 and the substrate 21a of the fixing belt 21 is smaller than the distance between the aluminum substrate 152 of the heat spreader 127 and the substrate 121a of the fixing belt 121, the heat spreader 27 of this embodiment has improved thermal conductivity. In addition, since there is no obvious interface between the aluminum oxide film layer 54 and the aluminum substrate 52, the heat spreader 27 of this embodiment is conducive to heat conduction. Therefore, the heat spreader 27 of this embodiment has improved heat spread performance compared with the heat spreader of the comparative example.

[0104] With the above structure, a fixing device capable of performing good fixing even over time can be realized. An image forming apparatus provided with the fixing device can be used as a product capable of preventing the torque of the fixing unit from increasing for a long period of time.

[0105] For example, in the above-described embodiment, the gripper forming member 24 and the heat spreading member 27 are separate members, or the heat spreading member may have a role (or function) as the gripper forming member and be an integrated member.

[0106] The above embodiments are illustrative and do not limit the present invention. Therefore, based on the above teachings, many additional modifications and variations are possible. For example, within the scope of the present invention, elements and / or features of different illustrative embodiments may be combined with each other and / or replaced with each other.

[0107] This patent application is based on and claims the benefit of priority from Japanese Patent Application No. 2019-227137 filed in the Japan Patent Office on December 17, 2019, the disclosure of which is incorporated herein by reference in its entirety.

[0108] Reference numerals list

[0109] 1 Image forming device

[0110] 2 Bottle storage area

[0111] 2C, 2K, 2M, 2Y Toner Bottles

[0112] 3 Transfer device

[0113] 4 4C, 4K, 4M, 4Y imaging units

[0114] 5 Photoreceptor

[0115] 6 Charging device

[0116] 7 Development device

[0117] 8 Cleaning device

[0118] 9 Exposure device

[0119] 10 Paper supply tray

[0120] 11 Paper feed roller

[0121] 12 Positioning roller pairs

[0122] 13 Paper ejection roller pair

[0123] 14 Output Tray

[0124] 20 Fixing device

[0125] 21 Fusing belt

[0126] 21a Substrate

[0127] 21b Release layer

[0128] 21c Sliding layer

[0129] 21d Elastic layer

[0130] 22 Pressure roller

[0131] 23A, 23B Heater

[0132] 24 Clamping portion forming component

[0133] 25 pillar parts

[0134] 25a Arm

[0135] 27 Heat distribution components

[0136] 27a With sliding contact surface

[0137] 28A, 28B Reflective components

[0138] 29 Temperature sensor

[0139] 30 Intermediate transfer belt

[0140] 31 Primary transfer roller

[0141] 32 Secondary transfer backing roller

[0142] 33 Cleaning the support roller

[0143] 34 Tension roller

[0144] 35 with cleaning device

[0145] 36 Secondary transfer roller

[0146] 40 Separation parts

[0147] 45 Flange

[0148] 46 Receiving Department

[0149] 47 Jaw

[0150] 48 incision

[0151] 52 Aluminum substrate

[0152] 53 Sliding layer

[0153] 54 Aluminum oxide film

[0154] 54a Micropore

[0155] 54b Base

[0156] 56 Molybdenum disulfide

[0157] 60 Interface

[0158] N Fixing nip

[0159] P paper

Claims

1. A fixing device, comprising: A rotatable annular fixing member; a heat source configured to heat the fixing member; A pressure component, arranged outside the fixing component and facing the fixing component; a clamping portion forming member, disposed inside the fixing member, and forming a clamping portion between the fixing member and the pressing member; as well as a heat-dissipating member configured to cover the surface of the clamping portion forming member facing the fixing member and transfer heat in the axial direction of the fixing member, The fixing component at least comprises: A cylindrical substrate made of metal; as well as A sliding layer made of a heat-resistant resin is formed on the inner peripheral surface of the substrate, The heat-saturating component is made of aluminum or aluminum alloy. The heat equalizing member has an aluminum oxide film layer on a surface facing the inner peripheral surface of the fixing member. A solid lubricant having a graphite structure is filled in the plurality of micropores in the aluminum oxide film layer from the bottom of the plurality of micropores to the outermost layer of the plurality of micropores, and the friction coefficient of the solid lubricant is lower than the friction coefficient of the aluminum oxide film layer. The aluminum oxide film layer has a thickness smaller than that of the sliding layer of the fixing member.

2. The fixing device according to claim 1, in, The solid lubricant is molybdenum disulfide.

3. The fixing device according to claim 1, in, The solid lubricant is polytetrafluoroethylene (PTFE) or fluorine grease.

4. The fixing device according to any one of claims 1 to 3, in, The aluminum oxide film layer has a thickness less than 10 μm.