A wet heat aging test device

By designing the drying, smoothing and anti-pull mechanisms of the moist heat aging test device, the problem of surface roughness and wrinkles of thermoplastic resin products during thermal aging is solved, the efficient drying and smoothing of the film is achieved, and the efficiency of the aging test and the product are improved. stability.

CN115015091BActive Publication Date: 2024-10-01GUANGZHOU METROLOGY & TESTING TECH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202210232730.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-10
Publication Date
2024-10-01
Estimated Expiration
2042-03-10

AI Technical Summary

Technical Problem

Existing thermoplastic resin products are prone to surface roughness and wrinkles during the thermal aging process, and are inconvenient to store and store after aging, which reduces the efficiency of the aging test.

Method used

A humid heat aging test device is designed, including a drying mechanism, a smoothing mechanism and an anti-tension mechanism. By adjusting the movement path of the thermoplastic resin film, using dense copper balls for point pressing, and elastic tension springs to absorb instant tension, Eliminates wrinkles and improves membrane stability.

Benefits of technology

It effectively eliminates the moisture problem of the thermoplastic resin film, facilitates storage, eliminates wrinkle rebound, improves the efficiency of aging tests and product stability, and avoids tearing and positional deviation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115015091B_ABST
    Figure CN115015091B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of wet heat aging test, and in particular to a wet heat aging test device. The wet heat aging test device comprises a truss; a winding assembly, located at the tail end of the truss; a drying mechanism, located in the middle of the truss, and the drying mechanism controls the drying time of the thermoplastic resin film by adjusting the movement stroke of the thermoplastic resin film; a smoothing mechanism, located on the truss between the drying mechanism and the winding assembly, and the smoothing mechanism eliminates the wrinkles of the thermoplastic resin film by point pressing. When the thermoplastic resin films on both sides of the anti-tension mechanism of the wet heat aging test device provided by the present invention are subjected to an instantaneous upward (or downward) pulling force, the rotating frame deflects upward (or downward), so that the tension spring on the connecting plate is compressed (or stretched), thereby eliminating the problem of the thermoplastic resin film being torn or damaged due to the instantaneous excessive internal stress pulling force.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of damp heat aging test, and in particular to a damp heat aging test device. Background Art

[0002] Aging test mainly refers to the thermal oxygen aging test for rubber, plastic products, electrical insulation materials and other materials; or ventilation aging test for electronic parts and plastic products. There are two methods for aging test products: 1. Aging box; mainly for plastic products, and it is more practical for products that are not large in quantity and volume; 2. Aging cabinet or aging room; mainly for high-performance electronic products (such as: computer machines, monitors, terminals, automotive electronic products, power supplies, motherboards, monitors, switching chargers, etc.) to simulate a high temperature and harsh environment test equipment, which is an important test equipment to improve product stability and reliability, and an important production process for various manufacturers to improve product quality and competitiveness. The equipment is widely used in power electronics, computers, communications, biopharmaceuticals and other fields.

[0003] Existing thermoplastic resin products undergo stretching, electron irradiation and wet heat treatment during thermal aging, resulting in rough and wrinkled product surfaces. In addition, they are not easy to store and preserve after aging, which reduces the efficiency of aging tests.

[0004] Therefore, it is necessary to provide a wet heat aging test device to solve the above technical problems. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a damp heat aging test to solve the above technical problems.

[0006] The wet heat aging test device provided by the present invention comprises:

[0007] truss;

[0008] A winding assembly is located at the rear end of the truss, and the winding assembly is used to wind up the thermoplastic resin film and provide source power for the thermoplastic resin film to pass through various mechanisms; and further includes:

[0009] A drying mechanism is located in the middle of the truss, and the drying mechanism controls the drying time of the thermoplastic resin film by adjusting the movement stroke of the thermoplastic resin film;

[0010] A smoothing mechanism is located on the truss between the drying mechanism and the winding assembly, and the smoothing mechanism eliminates wrinkles of the thermoplastic resin film by point pressing;

[0011] The drying mechanism includes a mounting frame, on which three lower guide rollers are horizontally distributed and equidistantly arranged, and the lower guide rollers are rotatably connected to the mounting frame, and two hot air blowers are mounted on the mounting frame below the lower guide rollers, and sliding rods are fixedly installed on the trusses on both sides of the mounting frame, and each of the sliding rods is sleeved with a sliding sheet in a slidable connection, the upper surface of the sliding sheet is fixedly connected to the output section of the hydraulic cylinder, and the hydraulic cylinder is fixedly installed on the inner top wall of the truss, and a V-shaped frame is fixedly installed between the two sliding sheets, specifically, the V-shaped frame opens downward, and rotatably connected upper guide rollers are installed on both sides of the V-shaped frame.

[0012] Preferably, the two upper guide rollers on the V-shaped frame and the three lower guide rollers on the mounting frame are in an "M" shape, and the two hot air blowers correspond to the two upper guide rollers, and the air outlet of the hot air blower is in a fan shape.

[0013] Preferably, the smoothing mechanism includes a mounting column, on which a lower platen is fixedly mounted, and the lower platen is mounted with an upper platen via a plurality of sets of connecting parts, the inner plate surfaces of the lower platen and the upper platen are provided with a plurality of evenly distributed arc-shaped interlocking cavities, and a rolling copper ball is interlocked in each of the arc-shaped interlocking cavities, the spherical body of the copper ball extends out of the arc-shaped interlocking cavity by one third, and pressing parts are installed on the inner plate surfaces of the lower platen and the upper platen near the winding assembly.

[0014] Preferably, the connecting member includes a threaded rod, which is fixedly engaged at the corners of the lower platen and passes through a through hole opened in the upper platen. A threaded adjusting nut is sleeved on the threaded rod below the upper platen, and a threaded limiting nut is sleeved on the threaded rod above the upper platen.

[0015] Preferably, the pressing part comprises a rubber pressing plate, the inner plate wall of the rubber pressing plate is elastically connected to the mounting cavity opened on the inner wall of the table plate through a plurality of springs with the same elastic coefficient, and the rubber pressing plates in the lower table plate and the upper table plate are against each other.

[0016] Preferably, the head end of the truss is equipped with an anti-pull mechanism, and the anti-pull mechanism includes a mounting plate, a rotating frame is installed on the lower plate surface of the mounting plate, and a double-axis roller frame is installed at the bottom of the rotating frame, two guide rollers arranged parallel to each other are installed on the double-axis roller frame, and a connecting plate is fixedly installed on the top of the double-axis roller frame, the connecting plate is elastically connected to the mounting plate by a number of tension springs with the same elastic coefficient, and the mounting plate is fixedly installed on the inner top wall of the truss end by screws.

[0017] Preferably, a limited slip component is installed on the truss behind the anti-pulling mechanism, and the limited slip component includes a U-shaped frame, a rotatably connected lead screw is installed in the U-shaped frame, and one end of the lead screw is fixedly connected to the output end of a driving motor mounted on the side wall of the U-shaped frame, two opposite threaded sections are arranged on the lead screw, and a threaded connecting plate is threadedly installed on each threaded section, and a U-shaped clamp is installed at the bottom of each threaded connecting plate. Specifically, the openings of the two U-shaped clamps are arranged opposite to each other, and the upper and lower inner surfaces of the U-shaped clamps are both equipped with rotatably connected rotating rods, a limiting rod parallel to the lead screw is fixedly installed in the U-shaped frame, and the limiting rod passes through the two threaded connecting plates and is slidably connected to the threaded connecting plates.

[0018] Preferably, the winding assembly comprises a reel, the reel is rotatably mounted on the truss via a bracket, and a rotating motor for driving the reel to rotate is mounted on the bracket.

[0019] Compared with the related art, the wet heat aging test device provided by the present invention has the following beneficial effects:

[0020] 1. The drying mechanism designed in the present invention can flexibly adjust the path of the thermoplastic resin film rolling there, so that the path can be reasonably adjusted according to whether the thermoplastic resin film needs to be dried or the degree of drying, so that the efficiency of the thermoplastic resin film rolling can be flexibly set. The drying treatment of the thermoplastic resin film can eliminate the moisture problem on the film surface during wet heat aging, and the rolling treatment can facilitate the storage of the product after the aging test;

[0021] 2. The smoothing mechanism designed in the present invention is provided with dense copper balls to perform point pressing on the thermoplastic resin film, thereby more effectively eliminating wrinkles on the thermoplastic resin film and making it less likely for the thermoplastic resin film to rebound after being flattened;

[0022] 3. The anti-pull mechanism designed by the present invention, when the thermoplastic resin films on both sides of the anti-pull mechanism are subjected to an instantaneous upward (or downward) pulling force, the rotating frame deflects upward (or downward), so that the tension spring on the connecting plate is compressed (or stretched), thereby eliminating the problem of the thermoplastic resin film being torn or damaged due to the instantaneous excessive internal stress tension. At the same time, when the film source of the thermoplastic resin film is vibrated, the tension spring on the connecting plate can absorb part of the fluctuation transmitted by the thermoplastic resin film, thereby improving the stability of the subsequent travel of the thermoplastic resin film. In addition, after the aging test, the film product is repaired when the instantaneous tension is stretched, thereby improving the efficiency of the aging test;

[0023] 4. The limited slip assembly designed in the present invention effectively avoids the phenomenon of positional deviation when the thermoplastic resin film is subsequently rolled up, and serves the purpose of correcting the position of the thermoplastic resin film when it is rolled up. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention.

[0025] Figure 1 A schematic structural diagram of a preferred embodiment of the wet heat aging test device provided by the present invention;

[0026] Figure 2 for Figure 1 A schematic structural diagram of the movement path of the thermoplastic resin film shown;

[0027] Figure 3 for Figure 1 The structural schematic diagram of the anti-pull mechanism shown;

[0028] Figure 4 for Figure 1 A schematic diagram of the structure of the limited slip assembly shown;

[0029] Figure 5 for Figure 1 The structural schematic diagram of the drying mechanism shown;

[0030] Figure 6 for Figure 1 The structural schematic diagram of the smoothing mechanism shown;

[0031] Figure 7 for Figure 6 A schematic diagram of the planar structure of the smoothing mechanism shown;

[0032] Figure 8 for Figure 6 Schematic diagram of the structure of the pressed parts shown.

[0033] Numbers in the figure: 1, truss; 2, winding assembly; 3, anti-pull mechanism; 31, mounting plate; 32, rotating frame; 33, double-axis roller frame; 34, guide roller; 35, connecting plate; 36, tension spring; 4, limited slip assembly; 41, U-shaped frame; 42, lead screw; 43, driving motor; 44, threaded connecting plate; 45, U-shaped clamp; 46, rotating rod; 47, limit rod; 5, drying mechanism; 51, mounting frame; 52, lower guide Roller; 53, hot air blower; 54, sliding rod; 55, sliding plate; 56, V-frame; 57, upper guide roller; 58, hydraulic cylinder; 6, smoothing mechanism; 61, mounting column; 62, lower platen; 63, upper platen; 64, connecting piece; 641, threaded rod; 642, adjusting nut; 643, limiting nut; 65, copper ball; 66, arc-shaped interlocking cavity; 67, pressing piece; 671, rubber pressing plate; 672 spring. DETAILED DESCRIPTION

[0034] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments; based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0035] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0036] The specific implementation of the present invention is described in detail below in conjunction with specific embodiments.

[0037] See also Figures 1 to 8 A device for testing wet heat aging provided by an embodiment of the present invention comprises: a truss 1, a winding assembly 2, a drying mechanism 5 and a smoothing mechanism 6. The winding assembly 2 is located at the rear end of the truss 1, and the winding assembly 2 winds up the thermoplastic resin film and provides source power for the thermoplastic resin film to pass through various mechanisms. The winding assembly 2 comprises a reel, which is rotatably mounted on the truss 1 through a bracket, and a rotating motor for driving the reel to rotate is installed on the bracket. The rotating motor is turned on to drive the reel to rotate, so that the reel winds up the thermoplastic resin film.

[0038] It should be noted that: the drying mechanism 5 can flexibly adjust the rolling path of the thermoplastic resin film at that location, so that the path can be reasonably adjusted according to whether the thermoplastic resin film needs to be dried or the degree of drying, so that the efficiency of the thermoplastic resin film winding can be flexibly set; and the smoothing mechanism 6 is provided with dense copper balls 65, so as to perform point pressing on the thermoplastic resin film, thereby more effectively eliminating the wrinkles of the thermoplastic resin film and making it less likely for the thermoplastic resin film to rebound after being flattened.

[0039] It is worth noting that the travel path of the thermoplastic resin film in the roll-forming device is as follows: Figure 2 As shown, specifically, after the thermoplastic resin film passes through the gap between the two guide rollers 34 in the anti-pull mechanism 3, the thermoplastic resin film extends to the slip limiting assembly 4, and after the two side edges of the thermoplastic resin film pass through the two U-shaped frames 41 in the slip limiting assembly 4 respectively, the thermoplastic resin film passes through the guide rollers in the drying mechanism 5, and the stroke is "M" shaped. Subsequently, the thermoplastic resin film passes through the gap between the upper platen 63 and the lower platen 62 in the smoothing mechanism 6, and is finally wound onto the reel in the winding assembly 2.

[0040] In the embodiments of the present invention, please refer to Figure 1 and Figure 3The head end of the truss 1 is equipped with an anti-pull mechanism 3, and the anti-pull mechanism 3 includes a mounting plate 31, a rotating frame 32 is installed on the lower plate surface of the mounting plate 31, and a double-axis roller frame 33 is installed at the bottom of the rotating frame 32, two guide rollers 34 arranged parallel to each other are installed on the double-axis roller frame 33, and a connecting plate 35 is fixedly installed on the top of the double-axis roller frame 33, the connecting plate 35 is elastically connected to the mounting plate 31 by a plurality of tension springs 36 with the same elastic coefficient, and the mounting plate 31 is fixedly installed on the inner top wall of the end of the truss 1 by screws.

[0041] It should be noted that: after the thermoplastic resin film passes through the gap between the two guide rollers 34 in the anti-tension mechanism 3, when the thermoplastic resin films on both sides of the anti-tension mechanism 3 are subjected to an instantaneous upward (or downward) pulling force, the rotating frame 32 deflects upward (or downward), so that the tension spring 36 on the connecting plate 35 is compressed (or stretched), thereby eliminating the problem of the thermoplastic resin film being torn or damaged due to the instantaneous excessive internal stress tension. At the same time, when the film source of the thermoplastic resin film is vibrated, the tension spring 36 on the connecting plate 35 can absorb part of the fluctuation transmitted by the thermoplastic resin film, thereby improving the stability of the subsequent travel of the thermoplastic resin film.

[0042] In the embodiments of the present invention, please refer to Figure 1 and Figure 4 The slip limiting assembly 4 is installed on the truss 1 behind the anti-tension mechanism 3, and the slip limiting assembly 4 includes a U-shaped frame 41, a rotatably connected lead screw 42 is installed in the U-shaped frame 41, and one end of the lead screw 42 is fixedly connected to the output end of a driving motor 43 mounted on the side wall of the U-shaped frame 41, and two opposite threaded sections are arranged on the lead screw 42, and a threaded connecting plate 44 with a thread connection is installed on each threaded section, and a U-shaped clamp 45 is installed at the bottom of each threaded connecting plate 44, specifically, the openings of the two U-shaped clamps 45 are arranged opposite to each other, and the upper and lower inner surfaces of the U-shaped clamp 45 are both installed with a rotatably connected rotating rod 46, a limiting rod 47 parallel to the lead screw 42 is fixedly installed in the U-shaped frame 41, and the limiting rod 47 passes through the two threaded connecting plates 44 and is slidably connected to the threaded connecting plates 44.

[0043] It should be noted that: the two U-shaped clips 45 are adjusted according to the width of the rolled thermoplastic resin film, and the driving motor 43 is turned on to drive the lead screw 42 to rotate, so that the two U-shaped clips 45 move toward (or away from) each other along with the two threaded connecting plates 44 on the lead screw 42 until the two U-shaped clips 45 cover both sides of the thermoplastic resin film, which effectively avoids the position deviation of the thermoplastic resin film during subsequent rolling, and serves the purpose of correcting the position of the rolled thermoplastic resin film;

[0044] It should also be noted that the limiting rod 47 installed in the U-shaped frame 41 limits the two U-shaped clips 45 to prevent the two U-shaped clips 45 from swinging as the lead screw 42 rotates.

[0045] In the embodiments of the present invention, please refer to Figure 1 and Figure 5 , the drying mechanism 5 is located in the middle of the truss 1, and the drying mechanism 5 controls the drying time of the thermoplastic resin film by adjusting the movement stroke of the thermoplastic resin film, and the drying mechanism 5 includes a mounting frame 51, on which three lower guide rollers 52 are horizontally distributed and equidistantly arranged, and the lower guide rollers 52 are rotatably connected to the mounting frame 51, and two hot air blowers 53 are mounted on the mounting frame 51 below the lower guide rollers 52, and sliding rods 54 are fixedly installed on the trusses 1 on both sides of the mounting frame 51, and each of the sliding rods 54 is sleeved with a sliding sheet 55 that is slidably connected, and the upper surface of the sliding sheet 55 is fixedly connected to the output section of the hydraulic cylinder 58, and the hydraulic cylinder 58 is fixedly installed on the inner top wall of the truss 1, and a V-shaped frame 56 is fixedly mounted between the two sliding sheets 55, specifically, the V-shaped frame 56 opens downward, and both sides of the V-shaped frame 56 are equipped with rotatably connected upper guide rollers 57;

[0046] The two upper guide rollers 57 on the V-shaped frame 56 and the three lower guide rollers 52 on the mounting frame 51 are in an "M" shape, and the two hot air blowers 53 correspond to the two upper guide rollers 57, and the air outlet of the hot air blower 53 is fan-shaped.

[0047] It should be noted that: after the thermoplastic resin film passes through the lower guide roller 52, the upper guide roller 57, the lower guide roller 52, the upper guide roller 57 and the lower guide roller 52 in the drying mechanism 5 in sequence, so that the thermoplastic resin film is in an "M" shape at this location, the hot air blower 53 is turned on to effectively dry the "M"-shaped thermoplastic resin film;

[0048] If the thermoplastic resin film needs to be dried or strongly dried, the hydraulic cylinder 58 is turned on to recycle the output end, so that the V-shaped frame 56 slides up along the sliding rod 54 along with the sliding sheet 55, so that the rolling path of the thermoplastic resin film at this location is extended, and the time for the hot air blower 53 to dry the thermoplastic resin film is prolonged, so as to improve the drying degree of the thermoplastic resin film. The specific time can be determined by adjusting the length of the return stroke of the output end of the hydraulic cylinder 58;

[0049] If the thermoplastic resin film does not need to be dried, the hydraulic cylinder 58 is turned on to push down the sliding piece 55 at its output end and slide down along the sliding rod 54, so that the top of the upper guide roller 57 and the bottom of the lower guide roller 52 are in a parallel state. At this time, the rolling path of the thermoplastic resin film at this point is the shortest, thereby reducing the stroke of the thermoplastic resin film winding, thereby increasing the winding rate of the thermoplastic resin film.

[0050] In the embodiments of the present invention, please refer to Figure 6 , Figure 7 and Figure 8 The smoothing mechanism 6 is located on the truss 1 between the drying mechanism 5 and the winding assembly 2, and the smoothing mechanism 6 eliminates the wrinkles of the thermoplastic resin film by point pressing, and the smoothing mechanism 6 includes a mounting column 61, a lower platen 62 is fixedly mounted on the mounting column 61, and the lower platen 62 is mounted with an upper platen 63 through a plurality of groups of connecting members 64, the inner plate surfaces of the lower platen 62 and the upper platen 63 are both provided with a plurality of evenly distributed arc-shaped interlocking cavities 66, and each of the arc-shaped interlocking cavities 66 is interlocked with a rolling copper ball 65, and the sphere of the copper ball 65 extends one third of the arc-shaped interlocking cavity 66, and a pressing member 67 is installed on the inner plate surface of the lower platen 62 and the upper platen 63 close to the winding assembly 2;

[0051] The connecting member 64 includes a threaded rod 641, which is fixedly engaged at the corner of the lower platen 62 and passes through a through hole provided in the upper platen 63. An adjusting nut 642 is threadedly sleeved on the threaded rod 641 below the upper platen 63, and a limiting nut 643 is threadedly sleeved on the threaded rod 641 above the upper platen 63.

[0052] Among them, the pressing part 67 includes a rubber pressing plate 671, the inner plate wall of the rubber pressing plate 671 is elastically connected to the installation cavity opened on the inner wall of the table through a plurality of springs 672 with the same elastic coefficient, and the rubber pressing plates 671 in the lower table 62 and the upper table 63 are against each other.

[0053] It should be noted that: after the thermoplastic resin film passes through the gap between the upper platen 63 and the lower platen 62 in the smoothing mechanism 6, the gap between the upper platen 63 and the lower platen 62 is adjusted according to the thickness of the thermoplastic resin film, and the adjusting nut 642 is loosened to make the upper platen 63 slide down along the threaded rod 641 until the copper ball 65 in the upper platen 63 abuts against the upper surface of the thermoplastic resin film. Therefore, when the thermoplastic resin film slides over the upper platen 63 and the lower platen 62, the copper ball 65 in the upper platen 63 and the lower platen 62 rolls with the friction of the thermoplastic resin film. Therefore, the wrinkled thermoplastic resin film is flattened by the rotation of the rolling copper ball 65. Since the copper ball 65 in the upper platen 63 and the lower platen 62 are densely distributed, the thermoplastic resin film is point-pressed to eliminate the wrinkles of the thermoplastic resin film, and the flattened thermoplastic resin film is not prone to wrinkle rebound.

[0054] It should also be noted that: under the elastic force of the spring 672, the rubber pressing plate 671 in the lower platen 62 presses against the lower film surface of the thermoplastic resin film, while the rubber pressing plate 671 in the upper platen 63 presses against the upper film surface of the thermoplastic resin film. Therefore, after the copper ball 65 rolls and smoothes the thermoplastic resin film, the two rubber pressing plates 671 perform a secondary wrinkle removal treatment, thereby further improving the flatness of the thermoplastic resin film.

[0055] The working principle of the wet heat aging test device provided by the present invention is as follows:

[0056] After the thermoplastic resin film passes through the gap between the two guide rollers 34 in the anti-tension mechanism 3, when the thermoplastic resin films on both sides of the anti-tension mechanism 3 are subjected to an instantaneous upward (or downward) pulling force, the rotating frame 32 deflects upward (or downward), so that the tension spring 36 on the connecting plate 35 is compressed (or stretched), thereby eliminating the problem of the thermoplastic resin film being torn or damaged due to the instantaneous excessive internal stress tension. At the same time, when the film source of the thermoplastic resin film is vibrated, the tension spring 36 on the connecting plate 35 can absorb part of the fluctuation transmitted by the thermoplastic resin film, thereby improving the stability of the subsequent travel of the thermoplastic resin film. In addition, after the aging test, the film product is repaired when the instantaneous tension is stretched, thereby improving the efficiency of the aging test.

[0057] The two U-shaped clips 45 are adjusted according to the width of the rolled thermoplastic resin film, and the driving motor 43 is turned on to drive the lead screw 42 to rotate, so that the two U-shaped clips 45 move toward (or away from) each other along with the two threaded connecting plates 44 on the lead screw 42 until the two U-shaped clips 45 cover both sides of the thermoplastic resin film, effectively avoiding the position deviation of the thermoplastic resin film during subsequent rolling, and achieving the purpose of correcting the position of the rolled thermoplastic resin film;

[0058] After the thermoplastic resin film passes through the lower guide roller 52, the upper guide roller 57, the lower guide roller 52, the upper guide roller 57 and the lower guide roller 52 in the drying mechanism 5 in sequence, the thermoplastic resin film is in an "M" shape at this location, and the hot air blower 53 is turned on to effectively dry the "M"-shaped thermoplastic resin film; if the thermoplastic resin film needs to be dried or strongly dried, the hydraulic cylinder 58 is turned on to recover the output end, so that the V-shaped frame 56 slides up along the sliding rod 54 along with the sliding sheet 55, so that the rolling path of the thermoplastic resin film at this location is extended, and the time for the hot air blower 53 to dry the thermoplastic resin film is lengthened, so as to improve the drying degree of the thermoplastic resin film. The specific time can be adjusted by adjusting the length of the return stroke of the output end of the hydraulic cylinder 58. If the thermoplastic resin film does not need to be dried, the hydraulic cylinder 58 is turned on to push the sliding piece 55 down along the sliding rod 54 at its output end, so that the top of the upper guide roller 57 and the bottom of the lower guide roller 52 are in a parallel state. At this time, the rolling path of the thermoplastic resin film at this point is the shortest, thereby reducing the stroke of the thermoplastic resin film winding, thereby increasing the winding rate of the thermoplastic resin film; thus, the drying mechanism 5 can flexibly adjust the rolling path of the thermoplastic resin film at this point, so that the path can be reasonably adjusted according to whether the thermoplastic resin film needs to be dried or the degree of drying, and the efficiency of the thermoplastic resin film winding can be flexibly set. The drying treatment of the thermoplastic resin film can eliminate the moisture problem on the film surface during wet heat aging;

[0059] After the thermoplastic resin film passes through the gap between the upper platen 63 and the lower platen 62 in the smoothing mechanism 6, the gap between the upper platen 63 and the lower platen 62 is adjusted according to the thickness of the thermoplastic resin film, and the adjusting nut 642 is loosened to make the upper platen 63 slide down along the threaded rod 641 until the copper ball 65 in the upper platen 63 abuts against the upper surface of the thermoplastic resin film. Therefore, when the thermoplastic resin film slides over the upper platen 63 and the lower platen 62, the copper ball 65 in the upper platen 63 and the lower platen 62 rolls with the friction of the thermoplastic resin film. Therefore, the wrinkled thermoplastic resin film is flattened by the rotation of the rolling copper ball 65. The copper balls 65 in the plate 62 are densely distributed, so the thermoplastic resin film is point-pressed to eliminate the wrinkles of the thermoplastic resin film and make the thermoplastic resin film less prone to wrinkle rebound after being flattened. Under the elastic force of the spring 672, the rubber pressing plate 671 in the lower platen 62 presses against the lower film surface of the thermoplastic resin film, and the rubber pressing plate 671 in the upper platen 63 presses against the upper film surface of the thermoplastic resin film. Therefore, after the copper balls 65 are rolled and smoothed, the thermoplastic resin film is subjected to a secondary wrinkle removal treatment by the two rubber pressing plates 671, thereby further improving the flatness of the thermoplastic resin film.

[0060] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0061] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A wet heat aging test device, characterized in that: include: Truss (1); A winding assembly (2) is located at the rear end of the truss (1), and the winding assembly (2) performs winding processing on the thermoplastic resin film and provides source power for the thermoplastic resin film to pass through various mechanisms; It also includes: a drying mechanism (5) located in the middle of the truss (1), and the drying mechanism (5) controls the drying time of the thermoplastic resin film by adjusting the movement stroke of the thermoplastic resin film; A smoothing mechanism (6) is located on the truss (1) between the drying mechanism (5) and the winding assembly (2), and the smoothing mechanism (6) eliminates wrinkles of the thermoplastic resin film by point pressing; The drying mechanism (5) comprises a mounting frame (51), on which three lower guide rollers (52) are arranged horizontally and equidistantly, and the lower guide rollers (52) are rotatably connected to the mounting frame (51); two hot air blowers (53) are mounted on the mounting frame (51) below the lower guide rollers (52); sliding rods (54) are fixedly mounted on the trusses (1) on both sides of the mounting frame (51), and each of the sliding rods (54) is sleeved with a sliding sheet (55) in a slidable connection, the upper surface of the sliding sheet (55) is fixedly connected to the output section of the hydraulic cylinder (58), and the hydraulic cylinder (58) is fixedly mounted on the inner top wall of the truss (1); a V-shaped frame (56) is fixedly mounted between the two sliding sheets (55), the V-shaped frame (56) is opened downward, and rotatably connected upper guide rollers (57) are installed on both sides of the V-shaped frame (56); The two upper guide rollers (57) on the V-shaped frame (56) and the three lower guide rollers (52) on the mounting frame (51) are in an "M" shape, and the two hot air blowers (53) correspond to the two upper guide rollers (57), and the air outlet of the hot air blower (53) is in a fan shape; The smoothing mechanism (6) comprises a mounting column (61), a lower platen (62) is fixedly mounted on the mounting column (61), and an upper platen (63) is mounted on the lower platen (62) via a plurality of connecting pieces (64), the inner plate surfaces of the lower platen (62) and the upper platen (63) are provided with a plurality of evenly distributed arc-shaped interlocking cavities (66), and a rolling copper ball (65) is interlocked in each of the arc-shaped interlocking cavities (66), the sphere of the copper ball (65) extends out of one third of the arc-shaped interlocking cavity (66), and a pressing piece (67) is mounted on the inner plate surfaces of the lower platen (62) and the upper platen (63) close to the winding assembly (2); The connecting member (64) comprises a threaded rod (641), the threaded rod (641) being fixedly engaged at the corner of the lower platen (62) and passing through a through hole provided in the upper platen (63); a threaded adjustment nut (642) is sleeved on the threaded rod (641) below the upper platen (63), and a threaded limit nut (643) is sleeved on the threaded rod (641) above the upper platen (63); The pressing member (67) comprises a rubber pressing plate (671), the inner plate wall of the rubber pressing plate (671) is elastically connected to the mounting cavity provided on the inner wall of the table plate via a plurality of springs (672) having the same elastic coefficient, and the rubber pressing plates (671) in the lower table plate (62) and the upper table plate (63) are in contact with each other; the head end of the truss (1) is provided with an anti-tension mechanism (3), and the anti-tension mechanism (3) comprises a mounting plate (31), and the lower plate surface of the mounting plate (31) is provided with a rotating A rotating frame (32) is provided, and a double-axis roller frame (33) is installed at the bottom of the rotating frame (32), and two guide rollers (34) are installed on the double-axis roller frame (33) and are arranged in parallel with each other. A connecting plate (35) is fixedly installed on the top of the double-axis roller frame (33), and the connecting plate (35) is elastically connected to the mounting plate (31) through a plurality of tension springs (36) with the same elastic coefficient. The mounting plate (31) is fixedly installed on the inner top wall of the end of the truss (1) by screws.

2. The wet heat aging test device according to claim 1, characterized in that: A limited slip component (4) is installed on the truss (1) behind the anti-tension mechanism (3), and the limited slip component (4) includes a U-shaped frame (41), a rotatably connected lead screw (42) is installed in the U-shaped frame (41), and one end of the lead screw (42) is fixedly connected to the output end of a drive motor (43) mounted on the side wall of the U-shaped frame (41), the lead screw (42) is provided with two opposite threaded sections, and each threaded section is provided with a threaded connecting plate (44) connected in a threaded manner, and a U-shaped clamp (45) is installed at the bottom of each of the threaded connecting plates (44), the openings of the two U-shaped clamps (45) are arranged opposite to each other, and the upper and lower inner surfaces of the U-shaped clamp (45) are both provided with rotatably connected rotating rods (46).

3. The wet heat aging test device according to claim 2, characterized in that: A limiting rod (47) is fixedly installed in the U-shaped frame (41) and is distributed parallel to the lead screw (42). The limiting rod (47) passes through two threaded connection plates (44) and is slidably connected to the threaded connection plates (44).

4. The wet heat aging test device according to claim 1, characterized in that: The winding assembly (2) comprises a reel, which is rotatably mounted on the truss (1) via a bracket, and a rotating motor for driving the reel to rotate is mounted on the bracket.

Citation Information

Patent Citations

  • Corrugated base paper microwave hot air drying device for producing carton

    CN108895802A

  • Anti-wrinkle processing equipment for PE (polyethylene) antibacterial preservative film production

    CN113071945A

  • Battery separator coiling mechanism with fixed knot constructs

    CN208394444U

  • Solar backboard protective film coating equipment

    CN211247143U

  • Food heat-seal packaging device

    CN213443340U