A magnetic flux storage device based on π junction and preparation method thereof

By adopting the π junction design in superconducting flux storage devices, using the characteristics of ferromagnetic and normal metal materials, the problems of low integration and high static power consumption are solved, and high integration and low power consumption are achieved. Effect.

CN115020580BActive Publication Date: 2024-11-19SHANGHAI INST OF MICROSYSTEM & INFORMATION TECH CHINESE ACAD OF SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210655748.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-06-10
Publication Date
2024-11-19
Estimated Expiration
2042-06-10

AI Technical Summary

Technical Problem

Existing superconducting flux memory devices have low integration and high static power consumption, making it difficult to match the response speed and power consumption requirements of superconducting CPUs.

Method used

Using a magnetic flux memory device design based on π junction, the π junction Josephson junction and normal metal Josephson junction are formed on the substrate, and the strong exchange effect and properties of ferromagnetic materials and normal metal materials are used to form a π junction to replace the tradition. The magnetic flux circuit is formed in the zero structure to reduce the demand for bias current and reduce static power consumption.

Benefits of technology

It realizes the integration of superconducting flux memory devices and reduces static power consumption, shortens device size, reduces bias current requirements, and achieves fast non-volatile flux storage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115020580B_ABST
    Figure CN115020580B_ABST
Patent Text Reader

Abstract

The present invention provides a magnetic flux storage device based on π junction and a preparation method. The preparation of the magnetic flux storage device based on π junction includes: providing a substrate, forming a first type Josephson junction and a second type Josephson junction spaced apart in the horizontal direction, forming an isolation layer and a wiring layer, the first wiring part of the wiring layer is electrically connected to the top electrode of the first type Josephson junction, the second wiring part of the wiring layer is electrically connected to the top electrode of the second type Josephson junction, forming a storage loop based on the first type Josephson junction, and forming a readout circuit based on the second type Josephson junction. Among them, the first type Josephson junction uses a ferromagnetic barrier layer. Due to the strong exchange effect of the ferromagnetic material, the π phase offset can be achieved under a certain ferromagnetic thickness to form a π junction. The π junction replaces the traditional 0 junction and will generate a magnetic flux of 0.5Φ0, thereby pulling the hysteresis zone back to the 0 bias current, reducing the demand for inductance, shortening the size of the device, and reducing the bias current to reduce static power consumption.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of electronic information technology, and relates to a low-temperature storage device, in particular to a magnetic flux storage device based on π junction and a preparation method thereof. Background Art

[0002] Due to the high energy efficiency ratio (2.5TOPS / W) and extremely fast response speed (operating frequency up to 770GHZ), superconducting computers are expected to have high computing power and power consumption in the post-Moore era. In order to match the response speed of superconducting CPUs and be compatible with the preparation process of superconducting CPUs, the materials used to construct the memory must be superconducting materials. Currently, the most effective way to achieve data storage using superconducting electronic devices is to control the single flux quantum in the superconducting loop. Considering the critical current I of the Josephson junction, the critical current I of the Josephson junction is 1. C At the order of 100μA, the inductance of the storage unit needs to be around 10pH. At the same time, in order to effectively control the magnetic flux of the superconducting loop, additional superconducting wires are essential. These factors result in the physical space of the superconducting memory being too large, and it is impossible to achieve a highly integrated circuit. In addition, the storage unit composed of traditional 0-structures needs to add a constant bias current to maintain the magnetic flux information in the loop, and the bias current is generated by voltage passing through a large resistor, resulting in the static power consumption of the superconducting memory being two orders of magnitude higher than the dynamic power consumption of the superconducting device itself, which weakens the low power consumption advantage of the superconducting electronic device itself.

[0003] In order to solve the two problems of low integration and high static power consumption, people have turned their research direction to the superconducting-ferromagnetic-superconducting (SFS) Josephson junction. The superconducting pseudospin valve structure is constructed by using two layers of ferromagnetic barrier layers to realize low-temperature memory. The magnetization directions of the two layers of ferromagnetic are modulated to be parallel or anti-parallel by applying an external magnetic field, and the ferromagnetic junction can be adjusted to 0 or π state, and the single junction critical current I C The switch is used to store data, avoiding the regulation of magnetic flux and requiring no inductor, which can save a lot of space and increase the density of the device [B Baek et al. Nat Commun, 5, 3888 (2014)]. However, to trigger the junction, the magnetic polarization direction of the entire ferromagnetic layer needs to be flipped, and the triggering speed cannot be compared with the junction phase flipping speed.

[0004] Therefore, how to provide a π-junction-based magnetic flux storage device and a preparation method to improve the integration of superconducting magnetic flux storage devices and reduce static power consumption has become an urgent problem to be solved by those skilled in the art. Summary of the invention

[0005] In view of the above-mentioned shortcomings of the prior art, the purpose of the present invention is to provide a π-junction-based flux storage device and a preparation method, which are used to solve the problems of low integration and high static power consumption of the storage device composed of a 0-junction Josephson structure in the prior art.

[0006] To achieve the above-mentioned object and other related objects, the present invention provides a method for preparing a magnetic flux storage device based on a π junction, comprising the following steps:

[0007] providing a substrate;

[0008] A first type Josephson junction is formed on the substrate, wherein the first type Josephson junction is a π-junction Josephson junction, including a first junction bottom electrode, a first junction ferromagnetic barrier layer and a first junction top electrode stacked sequentially from bottom to top;

[0009] A second type Josephson junction is formed on the substrate, wherein the second type Josephson junction is spaced apart from the first type Josephson junction in a horizontal direction, and the second type Josephson junction comprises a second junction bottom electrode, a second junction normal metal barrier layer and a second junction top electrode which are sequentially stacked from bottom to top;

[0010] forming an isolation layer on the substrate, the isolation layer covering the first type Josephson junction and the second type Josephson junction, and patterning the isolation layer to obtain a first contact hole exposing the first junction top electrode and a second contact hole exposing the second junction top electrode;

[0011] A wiring layer is formed on the isolation layer, and the wiring layer is patterned to obtain a first wiring portion and a second wiring portion, wherein the first wiring portion is filled into the first contact hole and electrically connected to the first junction top electrode, and the second wiring portion is filled into the second contact hole and electrically connected to the second junction top electrode.

[0012] Optionally, forming the first type Josephson junction comprises the following steps:

[0013] forming a first type Josephson junction material layer on the substrate, wherein the first type Josephson junction material layer comprises a first junction superconducting bottom material layer, a first junction ferromagnetic barrier material layer and a first junction superconducting top material layer stacked sequentially from bottom to top;

[0014] forming a first photoresist layer on the first type Josephson junction material layer, and patterning the first photoresist layer to define a first junction bottom electrode region, wherein the patterned first photoresist layer covers the first junction bottom electrode region;

[0015] Using the patterned first photoresist layer as a mask, etching the first junction superconducting top material layer and the first junction ferromagnetic barrier material layer until the first junction superconducting bottom material layer is exposed;

[0016] forming a second photoresist layer and patterning it to define a first junction top electrode region, wherein the patterned second photoresist layer covers the first junction top electrode region;

[0017] The first junction superconducting top material layer is etched using the patterned second photoresist layer as a mask to form the first junction top electrode, and the first junction superconducting bottom material layer outside the first junction bottom electrode region and the current conduction region is etched to form the first junction bottom electrode.

[0018] Optionally, forming the second type Josephson junction comprises the following steps:

[0019] forming a second type Josephson junction material layer on the substrate, wherein the second type Josephson junction material layer comprises a second junction superconducting bottom material layer, a second junction normal metal barrier material layer and a second junction superconducting top material layer stacked in sequence from bottom to top;

[0020] forming a first photoresist layer on the second type Josephson junction material layer, and patterning the first photoresist layer to define a second junction bottom electrode region, wherein the patterned first photoresist layer covers the second junction bottom electrode region;

[0021] Using the patterned first photoresist layer as a mask, etching the second junction superconducting top material layer and the second junction normal metal barrier material layer;

[0022] Forming a second photoresist layer and patterning it to define a second junction top electrode region, wherein the patterned second photoresist layer covers the second junction top electrode region;

[0023] The second junction superconducting top material layer is etched using the patterned second photoresist layer as a mask to form the second junction top electrode, and the second junction superconducting bottom material layer outside the second junction bottom electrode region and the current conduction region is etched to form the second junction bottom electrode.

[0024] Optionally, forming the second type Josephson junction material layer further comprises the following steps:

[0025] forming a protective layer on the substrate, wherein the protective layer covers the first type Josephson junction;

[0026] Patterning the protective layer to expose a predetermined area of ​​the substrate;

[0027] forming the second junction superconducting bottom material layer on the surface of the protective layer and the exposed surface of the substrate;

[0028] forming the second junction normal metal barrier material layer on the surface of the second junction superconducting bottom material layer;

[0029] forming the second junction superconducting top material layer on the surface of the second junction normal metal barrier material layer;

[0030] The second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer outside the preset area are removed.

[0031] Optionally, the material of the protective layer includes photoresist, and the method of removing the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer outside the preset area includes peeling off the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer in the area where the protective layer is located by ultrasonic wave in an organic solution, leaving the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer located in the preset area.

[0032] Optionally, the material of the first junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the first junction ferromagnetic barrier layer includes at least one of NiCu, NiFe and NiPd, and the material of the first junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0033] Optionally, the thickness of the first junction bottom electrode is in the range of 100 nm to 150 nm, the thickness of the first junction ferromagnetic barrier layer is in the range of 12 nm to 18 nm, and the thickness of the first junction top electrode is in the range of 80 nm to 120 nm.

[0034] Optionally, the material of the second junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the second junction normal metal barrier layer includes at least one of normal metal state NbN, TaN, TiN, AlN, and the material of the second junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0035] Optionally, the thickness range of the second junction bottom electrode is 100nm~150nm, the resistivity range of the second junction normal metal barrier layer is 0.3mΩ·cm~0.7mΩ·cm, the output voltage range is 8μV~12μV, and the thickness range of the second junction top electrode is 80nm~120nm.

[0036] Optionally, the method further comprises the following steps:

[0037] forming a storage loop based on the first type Josephson junction, wherein the storage loop comprises a loop formed by connecting a superconducting wire and one of the first type Josephson junctions;

[0038] forming a readout circuit based on the second type Josephson junction, the readout circuit comprising a circuit formed by connecting a superconducting wire and two second type Josephson junctions;

[0039] connecting a bias current line to the storage loop and connecting two magnetic flux feedback coils to the readout circuit;

[0040] The π-junction-based magnetic flux storage device includes at least one magnetic flux storage unit, and the magnetic flux storage unit includes at least one storage loop and at least one readout circuit.

[0041] The present invention also provides a magnetic flux storage device based on a π junction, comprising:

[0042] substrate;

[0043] A first type Josephson junction is located on the substrate, wherein the first type Josephson junction is a π-junction Josephson junction, comprising a first junction bottom electrode, a first junction ferromagnetic barrier layer and a first junction top electrode stacked sequentially from bottom to top;

[0044] A second type of Josephson junction, located on the substrate, comprises a second junction bottom electrode, a second junction normal metal barrier layer and a second junction top electrode stacked in sequence from bottom to top, wherein the second type of Josephson junction and the first type of Josephson junction are arranged at intervals in the horizontal direction;

[0045] An isolation layer is located on the substrate and covers the first-type Josephson junction and the second-type Josephson junction.

[0046] The wiring layer is located on the isolation layer and includes a first wiring portion and a second wiring portion, wherein the first wiring portion is electrically connected to the first junction top electrode, and the second wiring portion is electrically connected to the second junction top electrode.

[0047] Optionally, the material of the first junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the first junction ferromagnetic barrier layer includes at least one of NiCu, NiFe and NiPd, and the material of the first junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0048] Optionally, the thickness of the first junction bottom electrode is in the range of 100 nm to 150 nm, the thickness of the first junction ferromagnetic barrier layer is in the range of 12 nm to 18 nm, and the thickness of the first junction top electrode is in the range of 80 nm to 120 nm.

[0049] Optionally, the material of the second junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the second junction normal metal barrier layer includes at least one of normal metal state NbN, TaN, TiN, AlN, and the material of the second junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0050] Optionally, the thickness range of the second junction bottom electrode is 100nm~150nm, the resistivity range of the second junction normal metal barrier layer is 0.3mΩ·cm~0.7mΩ·cm, the output voltage range is 8μV~12μV, and the thickness range of the second junction top electrode is 80nm~120nm.

[0051] Optionally, it also includes:

[0052] A storage loop, the storage loop comprising a loop formed by connecting a superconducting wire and a Josephson junction of the first type;

[0053] a bias current line connected to the storage loop;

[0054] A readout circuit, the readout circuit comprising a circuit formed by connecting a superconducting wire and two of the second-type Josephson junctions;

[0055] two flux feedback coils connected to the readout circuit;

[0056] The π-junction-based magnetic flux storage device includes at least one magnetic flux storage unit, and the magnetic flux storage unit includes at least one storage loop and at least one readout circuit.

[0057] As described above, the first type of Josephson junction in the π-junction-based flux storage device of the present invention uses ferromagnetic material as the intermediate barrier layer. Due to the strong exchange effect of the ferromagnetic material, the junction phase is shifted. Under a certain ferromagnetic thickness, the π phase of the junction can be shifted to form a π junction. Replacing the flux loop formed by the 0-junction with the π junction will generate a flux of 0.5Φ0, and pull the hysteresis zone back to 0 bias current. There is no need to apply a constant bias current to maintain the storage of flux information, thereby realizing a fast non-volatile flux storage function, effectively reducing static power consumption, and improving integration. BRIEF DESCRIPTION OF THE DRAWINGS

[0058] Figure 1 Shown is a process flow chart of preparing a magnetic flux storage device based on a π junction of the present invention.

[0059] Figure 2 The schematic diagram shows a substrate provided in the preparation of a π-junction-based magnetic flux memory device of the present invention.

[0060] Figure 3 It is a schematic diagram showing the formation of a first type Josephson junction material layer on a substrate in the preparation of a π-junction based magnetic flux memory device of the present invention.

[0061] Figure 4 It is a schematic diagram showing the definition of the first junction bottom electrode region in the preparation of the π-junction based magnetic flux storage device of the present invention.

[0062] Figure 5It is a schematic diagram showing the formation of a first type Josephson junction (SFS Josephson junction) by defining a first junction top electrode region in the preparation of a π-junction-based magnetic flux storage device according to the present invention.

[0063] Figure 6 It is a schematic diagram showing the formation of a protective layer and partial exposure of the substrate during the preparation of a π-junction-based magnetic flux memory device according to the present invention.

[0064] Figure 7 It is a schematic diagram showing the process of forming a second type Josephson junction material layer and removing the second type Josephson junction material layer outside a preset area in the preparation of a π-junction-based magnetic flux storage device according to the present invention.

[0065] Figure 8 It is a schematic diagram showing the definition of the second junction bottom electrode region in the preparation of the π-junction based magnetic flux storage device of the present invention.

[0066] Fig. 9 It is a schematic diagram showing the formation of a second type Josephson junction (SNS Josephson junction) by defining a second junction top electrode region in the preparation of a π-junction-based magnetic flux memory device according to the present invention.

[0067] Fig.10 It is a schematic diagram showing the process of preparing a π-junction-based magnetic flux storage device according to the present invention after forming an isolation layer and etching.

[0068] Fig.11 It is a schematic diagram showing the process of preparing a π-junction-based magnetic flux memory device according to the present invention after forming a wiring layer and etching.

[0069] Fig.12 The critical current density J of the SFS Josephson junction in the π-junction-based flux storage device of the present invention is shown as C With the ferromagnetic thickness d F of changes.

[0070] Fig.13 It is a schematic structural diagram of a magnetic flux storage device based on a π junction of the present invention.

[0071] Fig.14 The diagram shows the change of magnetic flux with bias current in the storage loop of the magnetic flux storage device based on π junction of the present invention.

[0072] Component number description

[0073] 1 Substrate

[0074] 2 Type I Josephson Junction Material Layer

[0075] 20. Josephson junction of the first kind

[0076] 201 First junction superconducting bottom material layer

[0077] 2011 The first bottom electrode

[0078] 202 first junction ferromagnetic barrier material layer

[0079] 2021 First junction ferromagnetic barrier layer

[0080] 203 First junction superconducting top material layer

[0081] 2031 First junction top electrode

[0082] 3. Protective layer

[0083] 4 Second Josephson junction material layer

[0084] 40 Josephson knot of the second kind

[0085] 401 Second junction superconducting bottom material layer

[0086] 4011 Second junction bottom electrode

[0087] 402 Second junction normal metal barrier material layer

[0088] 4021 Second junction normal metal barrier layer

[0089] 403 Second junction superconducting top material layer

[0090] 4031 Second junction top electrode

[0091] 5 Isolation layer

[0092] 61 First contact hole

[0093] 62 Second contact hole

[0094] 7 Wiring layer

[0095] 71 First wiring section

[0096] 72 Second wiring section

[0097] 81 Storage loop

[0098] 82 Readout circuit

[0099] Steps S1 to S5 DETAILED DESCRIPTION

[0100] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0101] See also Figures 1 to 14 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0102] Embodiment 1

[0103] This embodiment provides a method for preparing a magnetic flux storage device based on a π junction. Figure 1 , shown as a process flow chart of the method, comprising the following steps:

[0104] S1: providing a substrate;

[0105] S2: forming a first type Josephson junction on the substrate, wherein the first type Josephson junction is a π-junction Josephson junction, including a first junction bottom electrode, a first junction ferromagnetic barrier layer, and a first junction top electrode stacked sequentially from bottom to top;

[0106] S3: forming a second type of Josephson junction on the substrate, wherein the second type of Josephson junction is spaced apart from the first type of Josephson junction in a horizontal direction, and the second type of Josephson junction comprises a second junction bottom electrode, a second junction normal metal barrier layer, and a second junction top electrode stacked sequentially from bottom to top;

[0107] S4: forming an isolation layer on the substrate, the isolation layer covering the first type Josephson junction and the second type Josephson junction, and patterning the isolation layer to obtain a first contact hole exposing the first junction top electrode and a second contact hole exposing the second junction top electrode.

[0108] S5: forming a wiring layer on the isolation layer, and patterning the wiring layer to obtain a first wiring portion and a second wiring portion, wherein the first wiring portion is filled into the first contact hole and electrically connected to the first junction top electrode, and the second wiring portion is filled into the second contact hole and electrically connected to the second junction top electrode.

[0109] First see Figure 2 , perform step S1: provide a substrate 1.

[0110] As an example, the material of the substrate 1 includes a silicon wafer covered with at least one of oxides such as SiO2, HfO2, Al2O3, etc., and may also be other suitable substrates.

[0111] Specifically, in this embodiment, a substrate of a silicon wafer covered with SiO2 is preferably used, because it is easier to generate SiO2 on Si and it is easier to form a high-quality substrate.

[0112] Please see again Figures 3 to 5 , perform step S2: forming a first type Josephson junction 20 on the substrate 1, wherein the first type Josephson junction includes a first junction bottom electrode 2011, a first junction ferromagnetic barrier layer 2021, and a first junction top electrode 2031 stacked in sequence from bottom to top.

[0113] As an example, Figure 3 As shown, a first type Josephson junction material layer 2 is formed on the substrate 1, and the first type Josephson junction material layer 2 includes a first junction superconducting bottom material layer 201, a first junction ferromagnetic barrier material layer 202 and a first junction superconducting top material layer 203 stacked in sequence from bottom to top, that is, a superconducting-ferromagnetic-superconducting three-layer film.

[0114] As an example, in order to meet the requirements of use in a liquid helium environment, the material of the first junction superconducting bottom material layer 201 and the first junction superconducting top material layer 203 includes at least one of Nb, NbN, NbTi and NbTiN, or other suitable superconducting materials; the material of the first junction ferromagnetic barrier material layer 202 includes at least one of NiCu, NiFe, NiPd, or other suitable ferromagnetic materials.

[0115] It should be noted that the ferromagnetic material NiCu refers to an alloy with adjustable Ni and Cu contents, not a fixed 1:1 ratio. Similarly, NiFe and NiPd refer to alloys with adjustable Ni and Fe, and Ni and Pd contents.

[0116] Specifically, in this embodiment, the first junction superconducting bottom material layer 201 and the first junction superconducting top material layer 203 are made of Nb material. The superconducting Nb process is mature in the existing process, and the superconducting coherence length of Nb can reach 30nm. When the thickness of the barrier layer is less than the coherence length of the superconducting material, it is more effectively ensured that the supercurrent will not decay or be suppressed.

[0117] Specifically, in this embodiment, the thickness of the first junction superconducting bottom material layer 201 is in the range of 100nm to 150nm, the thickness of the first junction superconducting top material layer 203 is 100nm, the first junction ferromagnetic barrier material layer 202 uses NiCu with weaker magnetism, and its thickness range is 12nm to 18nm. The ferromagnetic alloy NiCu has different thickness ranges according to the different Ni and Cu contents. In this embodiment, the mass component of Ni is 52%, that is, Nb-Ni is used. 52 Cu 48 -Nb three-layer film to prepare the first type Josephson junction 20, the Ni 52 Cu 48 The thickness range is 12nm~15.1nm.

[0118] As an example, the method for forming the superconducting-ferromagnetic-superconducting three-layer film includes magnetron sputtering or other suitable methods. The sample stage is rotated during the film formation process so that the grown film has better uniformity.

[0119] As an example, Figure 4 As shown, defining the first junction bottom electrode region includes the following steps: first, spin coating a first photoresist layer on the surface of the first junction superconducting top material layer 203, and patterning the first photoresist layer to define the first junction bottom electrode region, wherein the patterned first photoresist layer covers the first junction bottom electrode region; second, etching the first junction superconducting top material layer 203 using the patterned first photoresist layer as a mask; and third, etching the first junction ferromagnetic barrier material layer 202 using the patterned first photoresist layer as a mask until the first junction superconducting bottom material layer 201 is exposed.

[0120] Specifically, in the process of defining the first junction bottom electrode region in this embodiment, a reactive ion beam etching (RIE) method is used, and reasonable process parameters are selected to etch away the first junction superconducting top material layer 203 in the area not covered by the first photoresist layer. An ion beam etching (IBE) method is used, and reasonable process parameters are selected to etch away the first junction ferromagnetic barrier material layer 202 in the area not covered by the first photoresist layer. Other suitable methods may also be used to etch the first junction superconducting top material layer 203 and the first junction ferromagnetic barrier material layer 202.

[0121] As an example, Figure 5 The method of defining the first junction top electrode region and forming the first type Josephson junction 20 comprises the following steps: first, Figure 4 A second photoresist layer is formed on the surface of the superconducting top material layer of the superconducting-ferromagnetic-superconducting three-layer film shown and is patterned, wherein the patterned second photoresist layer covers the first junction top electrode region; secondly, the first junction superconducting top material layer 203 is etched using the patterned second photoresist layer as a mask to form the first junction top electrode 2031, and the first junction superconducting bottom material layer 201 outside the first junction bottom electrode region and the current conduction area is etched to form the first junction bottom electrode 2011, thereby forming the first type Josephson junction 20 (SFS Josephson junction).

[0122] Specifically, in the process of defining the first junction top electrode region in this embodiment, the RIE method is adopted and reasonable process parameters are selected to etch away the first junction superconducting top material layer 203 in the area not covered by the second photoresist layer, the first junction bottom electrode region and the first junction superconducting bottom material layer 201 outside the current conduction area. Other suitable etching methods may also be adopted.

[0123] As an example, Figure 6As shown, before forming the second type Josephson junction material layer 4, a protective layer 3 is formed on the substrate 1, the protective layer 3 covers the first type Josephson junction 20, and the protective layer 3 is patterned to expose the substrate 1 in a preset area.

[0124] As an example, the protection layer 3 is a photoresist layer, and the protection layer 3 is patterned by an exposure method to expose a predetermined area of ​​the substrate 1 .

[0125] Please refer to Figures 7 to 9 , perform step S3: form a second type Josephson junction 40 on the substrate 1, the second type Josephson junction 40 and the first type Josephson junction 20 are arranged in a horizontal direction, and the second type Josephson junction 40 includes a second junction bottom electrode 4011, a second junction normal metal barrier layer 4021, and a second junction top electrode 4031 stacked in sequence from bottom to top.

[0126] As an example, Figure 7 As shown, a second junction superconducting bottom material layer 401, a second junction normal metal barrier material layer 402 and a second junction superconducting top material layer 403 are formed on the surface of the protective layer 3 and the exposed surface of the substrate 1, which are stacked in sequence from bottom to top, that is, a superconducting-normal metal-superconducting three-layer film, and the second junction superconducting bottom material layer 401, the second junction normal metal barrier material layer 402 and the second junction superconducting top material layer 403 outside the preset area are removed, leaving the second junction superconducting bottom material layer 401, the second junction normal metal barrier material layer 402 and the second junction superconducting top material layer 403 located in the preset area.

[0127] As an example, the method for forming the superconducting-normal metal-superconducting triple-layer film includes magnetron sputtering or other suitable methods. During the film forming process, the sample stage is rotated so that the grown thin film has better uniformity.

[0128] As an example, the material of the second junction superconducting bottom material layer 401 and the second junction superconducting top material layer 403 includes at least one of Nb, NbN, NbTi and NbTiN, or other suitable superconducting materials, and the material of the second junction normal metal barrier material layer 402 includes at least one of normal metal state NbN, TaN, TiN, AlN, or other suitable materials.

[0129] It should be noted that the stoichiometric ratio of the elements such as NbN, TaN, TiN and AlN in the normal metal state is adjustable. By adjusting the process parameters during sputtering, the stoichiometric ratio of the chemical elements of the normal metal state material is changed to achieve regulation of its resistivity and output voltage.

[0130] Specifically, in this embodiment, the second junction superconducting bottom material layer 401 is made of Nb film with a thickness range of 100 nm to 150 nm. The second junction superconducting top material layer 403 is made of Nb film with a thickness of 100 nm. The second junction normal metal barrier material layer 402 is made of NbN X (0 < x < 1), the atomic ratio x of N atoms is adjustable according to the process parameters during the sputtering process. Its resistivity is preferably about 0.5 mΩ·cm, and the output voltage is about 10 μV.

[0131] As an example, after the superconducting-normal metal-superconducting trilayer film is grown, the second junction superconducting bottom material layer 401, the second junction normal metal barrier material layer 402, and the second junction superconducting top material layer 403 outside the preset region are removed by ultrasonic waves in an organic solvent such as acetone, leaving the superconducting-normal metal-superconducting trilayer film region for preparing a superconducting quantum interference device (SQUID). In other embodiments, other suitable methods may also be used to remove the second junction superconducting bottom material layer 401, the second junction normal metal barrier material layer 402, and the second junction superconducting top material layer 403 outside the preset region.

[0132] As an example, as Figure 8 shown, defining the second junction bottom electrode region includes the following steps: First, a first photoresist layer is formed on the second type Josephson material layer 4, and the first photoresist layer is patterned to define the second junction bottom electrode region, where the patterned first photoresist layer covers the second junction bottom electrode region; Second, the second junction superconducting top material layer 403 and the second junction normal metal barrier material layer 402 are etched using the patterned first photoresist layer as a mask.

[0133] Specifically, during the process of defining the second junction bottom electrode region in this embodiment, the RIE method is used, and reasonable process parameters are selected to etch away the second junction superconducting top material layer 403 and the second junction normal metal barrier layer 402 in the region not covered by the first photoresist layer. Other suitable etching methods may also be used.

[0134] As an example, as Fig. 9 shown, defining the second junction top electrode region and forming the second type Josephson junction 40 includes the following steps: First, on Figure 8A second photoresist layer is formed on the surface of the superconducting top material layer of the superconducting-normal metal-superconducting three-layer film shown and is patterned to define a second junction top electrode region, wherein the patterned second photoresist layer covers the second junction top electrode region; secondly, the second junction superconducting top material layer 403 is etched using the patterned second photoresist layer as a mask to form the second junction top electrode 4031, and the second junction superconducting bottom material layer 401 outside the second junction bottom electrode region and the current conduction area is etched to form the second junction bottom electrode 4011, thereby forming the second type Josephson junction 40 (SNS Josephson junction).

[0135] Specifically, in the process of defining the second junction top electrode region and forming the second type Josephson junction 40 in the present embodiment, the RIE method is adopted and reasonable process parameters are selected to etch away the second junction superconducting top material layer 403 in the area not covered by the second photoresist layer, the second junction bottom electrode region and the second junction superconducting bottom material layer 401 outside the current conduction area. Other suitable etching methods may also be adopted.

[0136] As an example, the material of the first photoresist layer and the second photoresist layer includes photoresist.

[0137] Please refer to Fig.10 , perform step S4: form an isolation layer 5 on the substrate 1, the isolation layer 5 covers the first type Josephson junction 20 and the second type Josephson junction 40, and pattern the isolation layer 5 to obtain a first contact hole 61 exposing the first junction top electrode 2031 and a second contact hole 62 exposing the second junction top electrode 4031.

[0138] As an example, the isolation layer 5 includes an insulating layer, and the material of the isolation layer 5 includes at least one of dense oxides such as SiO2, HfO2, and Al2O3, preferably a SiO2 isolation layer, which matches the SiO2 lattice of the substrate 1 to grow a high-quality isolation layer. In order to completely block the wiring layer 6, the first junction bottom electrode 2011, and the second junction bottom electrode 4011, the isolation layer 5 is preferably formed by plasma enhanced chemical vapor deposition (PE-CVD), and the thickness of the isolation layer 5 is preferably about 300nm. Other suitable methods can also be used to form the isolation layer 5.

[0139] As an example, after the isolation layer 5 is formed, a photoresist layer is formed on the surface of the isolation layer 5, and photolithography is performed according to the required pattern to form the first contact hole 61 of the drainage channel of the first junction top electrode 2031 and the second contact hole 62 of the drainage channel of the second junction top electrode 4031, and then the isolation layer 5 in the area not covered by the photoresist layer is etched away.

[0140] Specifically, in this embodiment, the RIE method is adopted to select reasonable process parameters to etch away the isolation layer 5 in the area not covered by the photoresist layer. Other suitable etching methods may also be adopted.

[0141] Please refer to Fig.11 , execute step S5: form a wiring layer 7 on the isolation layer 5, and graph the wiring layer 7 to obtain a first wiring portion 71 and a second wiring portion 72, the first wiring portion 71 is filled into the first contact hole 61 and is electrically connected to the first junction top electrode 2031, and the second wiring portion 72 is filled into the second contact hole 62 and is electrically connected to the second junction top electrode 4031.

[0142] As an example, the material of the wiring layer 7 includes at least one of Nb, NbN, NbTi and NbTiN. In this embodiment, a Nb film consistent with the material of the first junction top electrode 2031 and the second junction top electrode 4031 is preferably used, and the wiring layer 7 is formed by magnetron sputtering or other suitable methods.

[0143] As an example, Fig.11 As shown, after the wiring layer 7 is formed, a photoresist layer is formed on the wiring layer 7, and photolithography is performed according to the required pattern to define the wiring area; then, the superconducting film of the wiring layer 7 in the area not covered by the photoresist layer is etched away to leave the wiring layer 7 pattern, and the wiring layer 7 includes a first wiring portion 71 and a second wiring portion 72, the first wiring portion 71 is connected to the first junction top electrode 2031, and the second wiring portion 72 is connected to the second junction top electrode 4031.

[0144] Specifically, in this embodiment, the RIE method is adopted to select reasonable process parameters to etch away the superconducting film of the wiring layer 7 in the area not covered by the photoresist layer. Other suitable etching methods may also be adopted.

[0145] It should be noted that, in the present embodiment, in all photolithography processes, the photoresist used is preferably a positive photoresist.

[0146] As an example, Fig.13As shown, it also includes the steps of forming a storage loop 81 based on the first type Josephson junction 20 and forming a readout circuit 82 based on the second type Josephson junction 40, the storage loop 81 includes a loop formed by connecting a superconducting wire and one of the first type Josephson junctions 20, connecting a bias current line to the storage loop 81, and the readout circuit 82 includes a circuit formed by connecting a superconducting wire and two of the second type Josephson junctions 40, connecting two flux feedback coils to the readout circuit, wherein the π-junction-based flux storage device includes at least one flux storage unit, and the flux storage unit includes at least one storage loop 81 and at least one readout circuit 82.

[0147] As an example, in the preparation of the magnetic flux storage device based on the π junction provided in this embodiment, the first type Josephson junction 20 uses a ferromagnetic material as an intermediate barrier layer. Due to the strong exchange effect of the ferromagnetic material, the phase of the first type Josephson junction 20 can be shifted. Under a certain ferromagnetic thickness, the π phase shift can be achieved to form a π junction. In this embodiment, Nb-Ni 52 Cu 48 -Nb Josephson junction as a first type Josephson junction 20, such as Fig.12 As shown, the Nb-Ni 52 Cu 48 -Nb junction critical current density J C As mentioned Ni 52 Cu 48 Thickness d F Schematic diagram of the change of the horizontal axis represents the ferromagnetic Ni 52 Cu 48 The thickness of the junction is shown in the vertical axis. The test temperature is 4.2K. The dotted line is the thickness of the junction in the actual test. F J C The solid line represents the theoretical model under the “dirty limit” condition. It can be seen that as d F The increase of J C It shows an oscillating attenuation trend. F J at 15.1nm C It cannot be measured at all, indicating that the first type Josephson junction 20 has a 0-π transition. The realized data is in good agreement with the theoretical results, confirming that the device is 52 Cu 48 The thickness range is 12nm to 15.1nm, which is a π junction. 52 Cu 48The thickness ranges from 12nm to 15.1nm; the second type Josephson junction 40 uses normal metal material as the intermediate barrier layer. Since the superconducting-normal metal-superconducting Josephson junction has stable properties and high on-chip uniformity, it can simplify the device preparation process and facilitate the construction of the readout circuit.

[0148] It should be further explained that the storage principle of the magnetic flux storage device based on the π junction of this embodiment is as follows: a single Josephson junction is embedded in a superconducting loop. Due to the magnetic flux quantization behavior of the superconducting loop and the periodic current phase relationship of the Josephson junction, under a certain junction critical current and loop inductance, the jump of a single magnetic flux quantum in the loop is achieved by applying an external magnetic field, and the bias current I is scanned back and forth. Bias The flux curve shows flux hysteresis changes, realizing the storage of states "0" and "1".

[0149] As an example, the first type of Josephson junction 20 is a π junction. Since the π junction generates half a magnetic flux quantum in the superconducting loop, the magnetic flux Φ in the storage loop 81 T With the bias current I Bias The relationship can be expressed as the following formula:

[0150] Φ T =I Bias L r -I C sin(2πΦ T / Φ0)×L loop +0.5Φ0······(1)

[0151] Among them, L r is the right geometric inductance of the storage loop, L loop is the total inductance of the storage loop, I C is the critical current of the π junction, Φ0 is the magnetic flux quantum. From formula (1), it can be seen that the magnetic flux changes with I Bias The change is not linear, but jumps. Fig.14 , showing the magnetic flux in the storage loop of the present invention with the bias current I Bias The horizontal axis represents the change of I Bias The vertical axis represents the magnetic flux, which is the result of normalizing the magnetic flux quantum. It can be seen that the magnetic flux in the loop increases with I Bias The scan jumps by scanning back and forth. Bias, the flux curve shows flux hysteresis change, which is consistent with formula 1. The hysteresis represents the change of a flux quantum, so the storage of states "0" and "1" can be realized. In addition, the center of the hysteresis is at 0 bias current. This is due to the half-cycle offset provided by the π junction, which pulls the hysteresis center to 0 bias current. The hysteresis center is located at 0 bias current, which reduces the demand for inductance, shortens the size of the device and improves the integration, while reducing the bias current and reducing static power consumption. Moreover, the π junction does not need to apply additional bias current to generate half a flux quantum in the superconducting loop, realizing fast non-volatile flux storage.

[0152] As an example, the storage loop 81 is coupled to the readout circuit 82. For the readout circuit 82, two magnetic flux feedback coils are added to the SQUID circuit, corresponding to I Coil+ and I Coil- , the magnetic flux size in the SQUID can be locally changed, and the magnetic flux change in the storage loop 81 is determined by correcting the magnetic flux in the SQUID to achieve the reading of the states "0" and "1".

[0153] Embodiment 2

[0154] like Fig.11 and Fig.13 As shown, a π-junction-based magnetic flux storage device is provided in this embodiment, wherein the π-junction-based magnetic flux storage device can be prepared by the preparation method of the π-junction-based magnetic flux storage device described in Embodiment 1, or can be prepared by other processes, but is not limited thereto.

[0155] As an example, Fig.11 As shown, the π-junction-based magnetic flux storage device includes a substrate 1, a first-type Josephson junction 20, a second-type Josephson junction 40, an isolation layer 5 and a wiring layer 7, wherein the first-type Josephson junction 20 is located on the substrate 1, and the first-type Josephson junction 20 is a π-junction Josephson junction, including a first junction bottom electrode 2011, a first junction ferromagnetic barrier layer 2021, and a first junction top electrode 2031 stacked sequentially from bottom to top; the second-type Josephson junction 40 is located on the substrate 1, including a second junction bottom electrode 4011, a second junction ferromagnetic barrier layer 2021, and a first junction top electrode 2031 stacked sequentially from bottom to top. The normal metal barrier layer 4021 and the second junction top electrode 4031 are arranged in a horizontal direction with the second type Josephson junction 40 and the first type Josephson junction 20 spaced apart from each other; the isolation layer 5 is located on the substrate 1 and covers the first type Josephson junction 20 and the second type Josephson junction 40; the wiring layer 7 is located on the isolation layer 5, and includes a first wiring part 71 and a second wiring part 72, the first wiring part 71 is electrically connected to the first junction top electrode 2031, and the second wiring part 72 is electrically connected to the second junction top electrode 4031.

[0156] As an example, the material of the substrate 1 includes a silicon wafer covered with at least one of oxides such as SiO2, HfO2, Al2O3, etc., or other suitable substrates. In this embodiment, a substrate of a silicon wafer covered with SiO2 is preferably used, because it is easier to generate SiO2 on Si, and it is easier to form a high-quality substrate.

[0157] As an example, in order to meet the requirements of use in a liquid helium environment, the material of the first junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the first junction ferromagnetic barrier layer includes at least one of NiCu, NiFe and NiPd, and the material of the first junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0158] It should be noted that the ferromagnetic material NiCu refers to an alloy with adjustable Ni and Cu contents, not a fixed 1:1 ratio. Similarly, NiFe and NiPd refer to alloys with adjustable Ni and Fe, and Ni and Pd contents.

[0159] Specifically, in this embodiment, the first junction superconducting bottom material layer 201 and the first junction superconducting top material layer 203 are made of Nb material. The superconducting Nb process is mature in the existing process, and the superconducting coherence length of Nb can reach 30nm. When the thickness of the barrier layer is less than the coherence length of the superconducting material, it is more effectively ensured that the supercurrent will not decay or be suppressed.

[0160] Specifically, in this embodiment, the thickness of the first junction superconducting bottom material layer 201 is in the range of 100nm to 150nm, the thickness of the first junction superconducting top material layer 203 is 100nm, the first junction ferromagnetic barrier material layer 202 uses NiCu with weaker magnetism, and its thickness range is 12nm to 18nm. The ferromagnetic alloy NiCu has different thickness ranges according to the different Ni and Cu contents. In this embodiment, the mass component of Ni is 52%, that is, Nb-Ni is used. 52 Cu 48 -Nb three-layer film to prepare the first type Josephson junction 20, the Ni 52 Cu 48 The thickness range is 12nm~15.1nm.

[0161] As an example, the material of the second junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the second junction normal metal barrier layer includes at least one of normal metal state NbN, TaN, TiN, AlN, and the material of the second junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

[0162] It should be noted that the material of the normal metal barrier material layer 402, such as NbN, TaN, TiN, and AlN, has an adjustable stoichiometric ratio of elements. By adjusting the process parameters during sputtering, the stoichiometric ratio of chemical elements in the material of the normal metal barrier layer 402 is changed to achieve the regulation of its resistivity and output voltage.

[0163] Specifically, the second junction superconducting bottom material layer 401 is made of Nb film with a thickness between 100 nm and 150 nm. The second junction superconducting top material layer 403 is made of Nb film with a thickness of 100 nm. The second junction normal metal barrier material layer 402 is made of NbN X (0 < x < 1), the atomic ratio x of N atoms is adjustable with the process parameters during sputtering. Its resistivity is preferably about 0.5 mΩ·cm, and the output voltage is about 10 μV.

[0164] As an example, as Fig.13 shown, it further includes a storage loop 81 formed based on the first Josephson junction and a readout circuit 82 formed based on the second type of Josephson junction. The storage loop 81 includes a loop formed by a superconducting wire and one of the first type of Josephson junctions 20, and a bias current line is connected to the storage loop 81. The readout circuit 82 includes a circuit formed by a superconducting wire and two of the second type of Josephson junctions, and two flux feedback coils are connected to the readout circuit.

[0165] As described above, for the flux storage device based on the π - junction provided in this embodiment, a single first type of Josephson junction is embedded in a superconducting loop. Due to the flux quantization behavior of the superconducting loop and the periodic current - phase relationship of the first type of Josephson junction, at a certain critical current of the junction and loop inductance, by applying an external magnetic field, the jump of a single flux quantum in the loop is achieved. By scanning the bias current back and forth, a flux hysteresis change appears in the flux - bias current curve, realizing the storage of states "0" and "1". And the first type of Josephson junction uses a ferromagnetic material as the intermediate barrier layer. Due to the strong exchange interaction of the ferromagnetic material, the phase of the first type of Josephson junction is shifted. At a certain ferromagnetic thickness, a π - phase shift can be achieved to form a π - junction. The flux loop formed by replacing the traditional 0 - junction with the π - junction will generate a flux of 0.5Φ0, thus pulling the hysteresis region back to the 0 - bias current position, reducing the requirement for inductance, being able to shorten the device size and improve the integration degree, while reducing the bias current and lowering the static power consumption. The second type of Josephson junction uses a normal - metal - state material as the intermediate barrier layer. Due to the stable properties of the superconducting - normal - metal - superconducting Josephson junction and high on - chip uniformity, it can simplify the device fabrication process and is beneficial for constructing a readout circuit. Two flux feedback coils are added to the readout circuit, which can locally change the magnitude of the magnetic flux in the readout circuit. By correcting the magnetic flux in the readout circuit, the magnetic flux change in the storage loop can be determined to realize the readout of states "0" and "1".

[0166] In summary, the present invention provides a magnetic flux storage device based on π junction and a preparation method thereof. The first type of Josephson junction in the magnetic flux storage device based on π junction adopts a ferromagnetic barrier layer. Due to the strong exchange effect of the ferromagnetic material, the phase of the first type of Josephson junction is shifted. Under a certain ferromagnetic thickness, the π phase shift can be achieved to form a π junction. The second type of Josephson junction adopts a normal metal barrier layer. Since the superconducting-normal metal-superconducting Josephson junction has stable properties and high on-chip uniformity, the device preparation process can be simplified. The magnetic flux storage device prepared based on the first type of Josephson junction and the second type of Josephson junction has a storage loop including a superconducting wire and a first type of about The first type of Josephson junction is a π junction, and a bias current line is connected to the storage loop. The readout circuit includes a circuit formed by connecting a superconducting wire and two second type Josephson junctions, and two magnetic flux feedback coils are connected to the readout circuit. Since the first type of Josephson junction is a π junction, the storage loop formed by replacing the traditional 0 junction with the π junction will generate a magnetic flux of 0.5Φ0, thereby pulling the hysteresis zone back to 0 bias current, reducing the demand for inductance, shortening the size of the device and improving the integration, while reducing the bias current and reducing static power consumption. Moreover, the π junction generates half a magnetic flux quantum in the superconducting loop without the need for additional bias current, thereby realizing fast non-volatile magnetic flux storage. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0167] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for preparing a magnetic flux storage device based on a π junction, characterized in that: The following steps are involved: providing a substrate; A first type Josephson junction is formed on the substrate, wherein the first type Josephson junction is a π-junction Josephson junction, comprising a first junction bottom electrode, a first junction ferromagnetic barrier layer and a first junction top electrode stacked in sequence from bottom to top, wherein the material of the first junction bottom electrode comprises at least one of Nb, NbN, NbTi and NbTiN, the material of the first junction ferromagnetic barrier layer comprises at least one of NiCu, NiFe and NiPd, the material of the first junction top electrode comprises at least one of Nb, NbN, NbTi and NbTiN, the thickness of the first junction bottom electrode ranges from 100 nm to 150 nm, the thickness of the first junction ferromagnetic barrier layer ranges from 12 nm to 18 nm, and the thickness of the first junction top electrode ranges from 80 nm to 120 nm; A second type Josephson junction is formed on the substrate, wherein the second type Josephson junction is spaced apart from the first type Josephson junction in a horizontal direction, and the second type Josephson junction comprises a second junction bottom electrode, a second junction normal metal barrier layer and a second junction top electrode which are sequentially stacked from bottom to top; forming an isolation layer on the substrate, the isolation layer covering the first type Josephson junction and the second type Josephson junction, and patterning the isolation layer to obtain a first contact hole exposing the first junction top electrode and a second contact hole exposing the second junction top electrode; forming a wiring layer on the isolation layer, and patterning the wiring layer to obtain a first wiring portion and a second wiring portion, wherein the first wiring portion is filled into the first contact hole to be electrically connected to the first junction top electrode, and the second wiring portion is filled into the second contact hole to be electrically connected to the second junction top electrode; forming a storage loop based on the first type Josephson junction, wherein the storage loop comprises a loop formed by connecting a superconducting wire and one of the first type Josephson junctions; forming a readout circuit based on the second type Josephson junction, the readout circuit comprising a circuit formed by connecting a superconducting wire and two second type Josephson junctions; connecting a bias current line to the storage loop and connecting two magnetic flux feedback coils to the readout circuit; The π-junction-based magnetic flux storage device includes at least one magnetic flux storage unit, and the magnetic flux storage unit includes at least one storage loop and at least one readout circuit.

2. The method for preparing a magnetic flux storage device based on a π junction according to claim 1, characterized in that: The formation of the first type of Josephson junction includes the following steps: forming a first type Josephson junction material layer on the substrate, wherein the first type Josephson junction material layer comprises a first junction superconducting bottom material layer, a first junction ferromagnetic barrier material layer and a first junction superconducting top material layer stacked sequentially from bottom to top; forming a first photoresist layer on the first type Josephson junction material layer, and patterning the first photoresist layer to define a first junction bottom electrode region, wherein the patterned first photoresist layer covers the first junction bottom electrode region; Using the patterned first photoresist layer as a mask, etching the first junction superconducting top material layer and the first junction ferromagnetic barrier material layer until the first junction superconducting bottom material layer is exposed; forming a second photoresist layer and patterning it to define a first junction top electrode region, wherein the patterned second photoresist layer covers the first junction top electrode region; The first junction superconducting top material layer is etched using the patterned second photoresist layer as a mask to form the first junction top electrode, and the first junction superconducting bottom material layer outside the first junction bottom electrode region and the current conduction region is etched to form the first junction bottom electrode.

3. The method for preparing a magnetic flux storage device based on a π junction according to claim 1, characterized in that: The formation of the second type Josephson junction includes the following steps: forming a second type Josephson junction material layer on the substrate, wherein the second type Josephson junction material layer comprises a second junction superconducting bottom material layer, a second junction normal metal barrier material layer and a second junction superconducting top material layer stacked sequentially from bottom to top; forming a first photoresist layer on the second type Josephson junction material layer, and patterning the first photoresist layer to define a second junction bottom electrode region, wherein the patterned first photoresist layer covers the second junction bottom electrode region; Using the patterned first photoresist layer as a mask, etching the second junction superconducting top material layer and the second junction normal metal barrier material layer; forming a second photoresist layer and patterning it to define a second junction top electrode region, wherein the patterned second photoresist layer covers the second junction top electrode region; The second junction superconducting top material layer is etched using the patterned second photoresist layer as a mask to form the second junction top electrode, and the second junction superconducting bottom material layer outside the second junction bottom electrode region and the current conduction region is etched to form the second junction bottom electrode.

4. The method for preparing a magnetic flux storage device based on a π junction according to claim 3, characterized in that: The forming of the second type Josephson junction material layer further comprises the following steps: forming a protective layer on the substrate, wherein the protective layer covers the first type Josephson junction; Patterning the protective layer to expose a predetermined area of ​​the substrate; forming the second junction superconducting bottom material layer on the surface of the protective layer and the exposed surface of the substrate; forming the second junction normal metal barrier material layer on the surface of the second junction superconducting bottom material layer; forming the second junction superconducting top material layer on the surface of the second junction normal metal barrier material layer; The second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer outside the preset area are removed.

5. The method for preparing a magnetic flux storage device based on a π junction according to claim 4, characterized in that: The material of the protective layer includes photoresist, and the method for removing the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer outside the preset area includes peeling off the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer in the area where the protective layer is located by ultrasonic wave in an organic solution, leaving the second junction superconducting bottom material layer, the second junction normal metal barrier material layer and the second junction superconducting top material layer located in the preset area.

6. The method for preparing a magnetic flux storage device based on a π junction according to claim 1, characterized in that: The material of the second junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the second junction normal metal barrier layer includes at least one of normal metal state NbN, TaN, TiN, AlN, and the material of the second junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

7. The method for preparing a magnetic flux storage device based on a π junction according to claim 6, characterized in that: The thickness range of the second junction bottom electrode is 100nm~150nm, the resistivity range of the second junction normal metal barrier layer is 0.3mΩ·cm~0.7mΩ·cm, the output voltage range is 8μV~12μV, and the thickness range of the second junction top electrode is 80nm~120nm.

8. A magnetic flux storage device based on a π junction, characterized in that: include: substrate; A first type Josephson junction, located on the substrate, the first type Josephson junction is a π-junction Josephson junction, comprising a first junction bottom electrode, a first junction ferromagnetic barrier layer and a first junction top electrode stacked in sequence from bottom to top, the material of the first junction bottom electrode comprising at least one of Nb, NbN, NbTi and NbTiN, the material of the first junction ferromagnetic barrier layer comprising at least one of NiCu, NiFe and NiPd, the material of the first junction top electrode comprising at least one of Nb, NbN, NbTi and NbTiN, the thickness of the first junction bottom electrode ranging from 100nm to 150nm, the thickness of the first junction ferromagnetic barrier layer ranging from 12nm to 18nm, and the thickness of the first junction top electrode ranging from 80nm to 120nm; A second type of Josephson junction, located on the substrate, comprises a second junction bottom electrode, a second junction normal metal barrier layer and a second junction top electrode stacked in sequence from bottom to top, wherein the second type of Josephson junction and the first type of Josephson junction are arranged at intervals in the horizontal direction; an isolation layer, located on the substrate and covering the first type Josephson junction and the second type Josephson junction; a wiring layer, located on the isolation layer, comprising a first wiring portion and a second wiring portion, wherein the first wiring portion is electrically connected to the first junction top electrode, and the second wiring portion is electrically connected to the second junction top electrode; A storage loop, the storage loop comprising a loop formed by connecting a superconducting wire and a Josephson junction of the first type; a bias current line connected to the storage loop; A readout circuit, the readout circuit comprising a circuit formed by connecting a superconducting wire and two of the second-type Josephson junctions; two flux feedback coils connected to the readout circuit; The π-junction-based magnetic flux storage device includes at least one magnetic flux storage unit, and the magnetic flux storage unit includes at least one storage loop and at least one readout circuit.

9. The magnetic flux storage device based on π junction according to claim 8, characterized in that: The material of the second junction bottom electrode includes at least one of Nb, NbN, NbTi and NbTiN, the material of the second junction normal metal barrier layer includes at least one of normal metal state NbN, TaN, TiN, AlN, and the material of the second junction top electrode includes at least one of Nb, NbN, NbTi and NbTiN.

10. The magnetic flux storage device based on π junction according to claim 9, characterized in that: The thickness range of the second junction bottom electrode is 100nm~150nm, the resistivity range of the second junction normal metal barrier layer is 0.3mΩ·cm~0.7mΩ·cm, the output voltage range is 8μV~12μV, and the thickness range of the second junction top electrode is 80nm~120nm.