Semiconductor devices
By adopting a stacked structure and ion implantation technology in the semiconductor device, the problem of difficulty in controlling the electrical characteristics of pnp and pn regions in the prior art is solved, and independent control and electrical characteristics are achieved.
Patent Information
- Application Number
- CN202210629378.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2016-09-26
- Filing Date
- 2017-09-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2037-09-26
AI Technical Summary
When the conventional power semiconductor device forms a pn pattern, it is difficult to independently control the electrical characteristics of the pnp region and the pn region, and the bonding depth between the p-type and n-type impurity regions is shallow, making it difficult to form a suitable ohmic characteristic electrode.
Design of a semiconductor device with a laminated structure, including a first semiconductor layer of the first conductivity type, a second semiconductor layer of the second conductivity type, a third semiconductor layer of the first conductivity type, and a fourth and fifth semiconductors of the second conductivity type The layer forms a laminated structure on the back surface, the first electrode covers the second semiconductor layer, the second electrode covers the fourth and fifth semiconductor layers, and an appropriate thickness and height difference is formed by ion implantation and heat treatment to achieve independent control.
Independent control of the pnp region and the pn region is achieved, the low on-resistance and low on-off loss of the IGBT, as well as the improvement of the breakdown resistance and ohmic characteristics of the diode.
Smart Images

Figure CN115064535B_ABST
Abstract
Description
[0001] This application is based on Chinese National Application No. filed on September 26, 2017
[0002] This application is a divisional application of application No. 2017108812631 (semiconductor device), the contents of which are cited below. Technical Field
[0003] The present invention relates to a semiconductor device, and in particular to a back surface structure of a power semiconductor device. Background Art
[0004] In recent years, RFC (Relaxed Field of Cathode) diodes and RC-IGBT (Reverse Conducting Insulated Gate Bipolar Transistor) have been manufactured as power semiconductor devices, which can control electrical characteristics by forming a pn pattern on the back side. Here, the pn pattern is in the following state, that is, on the back side of the semiconductor substrate constituting the power semiconductor device, when viewed from above, a region where a p-type impurity is formed and a region where an n-type impurity is formed are formed adjacent to each other.
[0005] When forming a pn pattern on the back side of a power semiconductor device, if a p-type impurity region and an n-type impurity region are formed by high-speed energy injection or high-concentration injection, there is a problem that the semiconductor substrate is more damaged due to the injection. As a countermeasure to such a problem, it is conceivable that, for the above-mentioned power semiconductor device, the back side of the semiconductor substrate using Si is melted, so that the concentration of the region where the impurities are introduced is uniformed and the concentration is fixed. A step-shaped impurity concentration distribution (for example, refer to patent document 1) is applied. In addition, for the above-mentioned power semiconductor device, a technology is disclosed in which an electrode having ohmic characteristics suitable for p-type and n-type is formed on the entire back side (for example, refer to patent documents 2 and 3).
[0006] Patent Document 1: Japanese Patent No. 5309360
[0007] Patent Document 2: Japanese Patent Application Publication No. 2007-184486
[0008] Patent Document 3: Japanese Patent Application Publication No. 2015-211149
[0009] When the technology of Patent Document 1 is applied to the above-mentioned power semiconductor device, the back side of the semiconductor substrate needs to be melted, so the p-type impurity region and the n-type impurity region can be joined only in a shallow region less than or equal to 1 μm from the back side. Therefore, it is difficult to independently control the electrical characteristics of the pnp region formed in the p-type impurity region and the electrical characteristics of the pn region formed in the n-type impurity region. In other words, it is difficult to independently control the operation of the pnp region and the operation of the pn region.
[0010] In addition, in Patent Documents 2 and 3, the junction depth between the p-type impurity region and the n-type impurity region is shallow and the depth is approximately the same, so it is difficult to form electrodes with ohmic characteristics suitable for the p-type and n-type regions respectively. Summary of the invention
[0011] The present invention is made to solve such a problem, and an object of the present invention is to provide a semiconductor device capable of independently controlling the operation of a pnp region and the operation of a pn region.
[0012] In order to solve the above-mentioned problems, the semiconductor device involved in the present invention is characterized in that it has a stacked structure, and the stacked structure is composed of the following parts: a first semiconductor layer of a first conductivity type; a second semiconductor layer of a second conductivity type, which is formed on the surface of the first semiconductor layer; and a third semiconductor layer of the first conductivity type, which is formed on the back side of the first semiconductor layer.
[0013] The fourth semiconductor layer of the first conductivity type and the fifth semiconductor layer of the second conductivity type are formed on the back side of the third semiconductor layer, or on the back sides of the first semiconductor layer and the third semiconductor layer, adjacent to each other or overlapping with each other in a plan view; a first electrode formed in a manner covering the surface of the second semiconductor layer; and
[0014] The second electrode is formed in a manner of covering the back sides of the fourth semiconductor layer and the fifth semiconductor layer, the stacking height position of the fourth semiconductor layer in the stacking structure is different from the stacking height position of the fifth semiconductor layer in the stacking structure, the second semiconductor layer overlaps with the fourth semiconductor layer and the fifth semiconductor layer when viewed from above, and the stacking structure constitutes an RFC diode, wherein RFC means releasing a cathode field, the thickness of the first semiconductor layer in the stacking structure including the fourth semiconductor layer is different from the thickness of the first semiconductor layer in the stacking structure including the fifth semiconductor layer, and the difference between the thickness of the first semiconductor layer in the stacking structure including the fourth semiconductor layer and the thickness of the first semiconductor layer in the stacking structure including the fifth semiconductor layer is the same as the height difference between the fourth semiconductor layer and the fifth semiconductor layer.
[0015] Effects of the Invention
[0016] According to the present invention, a semiconductor device has a stacked structure, which is composed of the following parts: a first semiconductor layer of a first conductivity type; a second semiconductor layer of a second conductivity type, which is formed on the surface of the first semiconductor layer; a third semiconductor layer of the first conductivity type, which is formed on the back side of the first semiconductor layer; a fourth semiconductor layer of the first conductivity type and a fifth semiconductor layer of the second conductivity type, which are formed on the back side of the third semiconductor layer adjacent to each other or overlapping with adjacent parts when viewed from above, or formed on the back sides of the first semiconductor layer and the third semiconductor layer; a first electrode, which is formed in a manner covering the surface of the second semiconductor layer; and a second electrode, which is formed in a manner covering the back sides of the fourth semiconductor layer and the fifth semiconductor layer, the stacking height position of the fourth semiconductor layer in the stacked structure is different from the stacking height position of the fifth semiconductor layer in the stacked structure, so that the action of the pnp region and the action of the pn region can be independently controlled. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a cross-sectional view showing an example of the structure of the semiconductor device according to the first embodiment of the present invention.
[0018] Figure 2 It is a cross-sectional view showing an example of the structure of a semiconductor device according to Embodiment 2 of the present invention.
[0019] Figure 3 It is a cross-sectional view showing an example of the structure of a semiconductor device according to Embodiment 3 of the present invention.
[0020] Figure 4 It is a cross-sectional view showing an example of the structure of a semiconductor device according to Embodiment 4 of the present invention.
[0021] Figure 5 It is a cross-sectional view showing an example of the structure of a semiconductor device according to Embodiment 5 of the present invention.
[0022] Figure 6 It is a cross-sectional view showing an example of the structure of a semiconductor device according to Embodiment 5 of the present invention.
[0023] Figure 7 It is a cross-sectional view showing an example of the structure of a semiconductor device according to the prerequisite technology.
[0024] Description of the label
[0025] 1 semiconductor device, 2 semiconductor substrate, 3 n-i layer, 4 p anode layer, 5 n+ cathode layer, 6 p collector layer, 7 n- buffer layer, 8 surface electrode, 9 back electrode, 10 pin
[0026] region, 11pnp region, 12, 13, 14 semiconductor device, 15n-type electrode, 16p-type electrode, 17, 18, 19 semiconductor device DETAILED DESCRIPTION
[0027] Hereinafter, embodiments of the present invention will be described based on the drawings.
[0028] <Prerequisite Technology>
[0029] Next, the technology that is the premise of the present invention, that is, the prerequisite technology, will be described.
[0030] Figure 7 It is a cross-sectional view showing an example of the structure of a semiconductor device 19 according to the underlying technology.
[0031] The semiconductor device 19 has a semiconductor substrate 2 made of Si (silicon); a surface electrode 8 as a first electrode formed on the surface of the semiconductor substrate 2; and a back electrode 9 as a second electrode formed on the back of the semiconductor substrate 2. The semiconductor substrate 2 has a ni layer 3, a p anode layer 4, an n+ cathode layer 5, a p collector layer 6, and an n-buffer layer 7. The pin region 10 is a stacked structure consisting of the p anode layer 4, the ni layer 3, the n-buffer layer 7, and the n+ cathode layer 5. The pnp region 11 is a stacked structure consisting of the p anode layer 4, the ni layer 3, the n-buffer layer 7, and the p collector layer 6.
[0032] Here, "n" and "p" represent conductivity types, n-type is the first conductivity type, and p-type is the second conductivity type. "n-" represents that the impurity concentration of n-type is lower than that of other n-types. "n+" represents that the impurity concentration of n-type is higher than that of other n-types. In addition, below, it is described that n-type is the first conductivity type and p-type is the second conductivity type, but it is also possible that p-type is the first conductivity type and n-type is the second conductivity type.
[0033] The first semiconductor layer of the first conductivity type, i.e., the ni layer 3, is formed as an intrinsic semiconductor layer of the n type. The second semiconductor layer of the second conductivity type, i.e., the p anode layer 4, is formed on the surface side of the semiconductor substrate 2 compared to the ni layer 3. The third semiconductor layer of the first conductivity type, i.e., the n- buffer layer 7, is formed on the back side of the semiconductor substrate 2 compared to the ni layer 3. The fourth semiconductor layer of the first conductivity type, i.e., the n+ cathode layer 5, and the fifth semiconductor layer of the second conductivity type, i.e., the p collector layer 6, are formed on the back side of the semiconductor substrate 2 compared to the ni layer 3, and are adjacent to each other when viewed from above. That is, a pn pattern is formed by the n+ cathode layer 5 and the p collector layer 6.
[0034] like Figure 7 As shown, the n+ cathode layer 5 and the p collector layer 6 are formed at substantially the same depth from the back surface of the semiconductor substrate 2. That is, the stacking height position of the n+ cathode layer 5 in the pin region 10 is substantially the same as the stacking height position of the p collector layer 6 in the pnp region 11. Therefore, as described above, it is difficult to independently control the operation of the pin region 10 and the operation of the pnp region 11.
[0035] The present invention is proposed to solve such problems and is described in detail below.
[0036] <Implementation Method 1>
[0037] <Structure>
[0038] First, the structure of a semiconductor device according to an embodiment of the present invention will be described. Figure 1 It is a cross-sectional view showing an example of the structure of the semiconductor device 1 according to the first embodiment.
[0039] The semiconductor device 1 according to the first embodiment is characterized in that the thickness of the ni layer 3 in the pin region 10 is different from the thickness of the ni layer 3 in the pnp region 11. Specifically, the thickness of the ni layer 3 in the pnp region 11 is thinner than the thickness of the ni layer 3 in the pin region 10. In addition, the stacking height position of the n+ cathode layer 5 in the pin region 10 is different from the stacking height position of the p collector layer 6 in the pnp region 11. Other structures are the same as Figure 7The semiconductor device 19 involved in the underlying technology shown is the same, so the detailed description is omitted here.
[0040] In the semiconductor device 1, the difference between the thickness of the ni layer 3 at the pin region 10 and the thickness of the ni layer 3 at the pnp region 11 is the same as the height difference between the n+ cathode layer 5 and the p collector layer 6. Here, the height difference between the n+ cathode layer 5 and the p collector layer 6 refers to the difference between the interface between the n+ cathode layer 5 and the back electrode 9 and the interface between the p collector layer 6 and the back electrode 9.
[0041] like Figure 1 As shown, n+ cathode layer 5 and p collector layer 6 are formed on the back side of n- buffer layer 7. In a plan view, n+ cathode layer 5 and p collector layer 6 are adjacent, and adjacent portions of n+ cathode layer 5 and p collector layer 6 do not overlap.
[0042] <Manufacturing method>
[0043] Next, a method for manufacturing the semiconductor device 1 will be described.
[0044] First, a semiconductor substrate 2 having a ni layer 3 is prepared. Next, ion implantation of B (boron) is performed from the surface side of the semiconductor substrate 2 to form a p-anode layer 4. At this time, the concentration of the implanted B is 1E13 to 1E16 (1 / cm 2 ). In addition, the driving conditions are 900° C. to 1200° C. and 30 minutes to 120 minutes.
[0045] Next, the surface electrode 8 is formed so as to cover the p-anode layer 4. Then, the semiconductor substrate 2 is cut from the back side of the semiconductor substrate 2 to a desired thickness. After the cutting of the semiconductor substrate 2, P (phosphorus) ions constituting the n+ cathode layer 5 are implanted into the entire back side of the semiconductor substrate 2. At this time, the concentration of the implanted P is 1E14 to 1E16 (1 / cm 2 ).
[0046] Next, a pn pattern is formed on the back side of the semiconductor substrate 2, and then the semiconductor substrate 2 in the region where the p collector layer 6 is to be formed is etched to a desired thickness, wherein the pn pattern covers the region where the n+ cathode layer 5 is to be formed and opens the region where the p collector layer 6 is to be formed. Then, B is ion-implanted into the region where the p collector layer 6 is to be formed, and the B constitutes the p collector layer 6. At this time, the concentration of the ion-implanted B is 1E13 to 1E16 (1 / cm 2 ). Thus, an n+ cathode layer 5 and a p collector layer 6 are formed.
[0047] Next, after removing the pn pattern, P ions are implanted from the back side of the semiconductor substrate 2, bypassing the n+ cathode layer 5 and the p collector layer 6, to form an n- buffer layer 7. At this time, the concentration of the implanted P is 1E13 to 1E15 (1 / cm 2 ). Thus, an n-buffer layer 7 having an n-type impurity concentration higher than that of the n-layer 3 is formed.
[0048] Next, the semiconductor substrate 2 is subjected to a heat treatment to activate the n+ cathode layer 5, the p collector layer 6, and the n- buffer layer 7. Examples of the heat treatment include laser annealing.
[0049] Finally, a back electrode 9 with a thickness of several μm is formed by plating, sputtering, or vapor deposition so as to cover the n+ cathode layer 5 and the p collector layer 6. Thus, the semiconductor device 1 having the pin region 10 and the pnp region 11 is completed.
[0050] As described above, according to the first embodiment, the thickness of the ni layer 3 in the pin region 10 is different from the thickness of the ni layer 3 in the pnp region 11 , so the operation of the pin region 10 and the operation of the pnp region 11 can be controlled independently.
[0051] In addition, the thickness of the Ni layer 3 in the pnp region 11 is thinner than the thickness of the Ni layer 3 in the pin region 10. Therefore, in the case of the IGBT, low on-resistance and low switching loss can be achieved. In addition, in the case of the diode, the breakdown resistance in the recovery operation can be improved.
[0052] In addition, Figure 1 In the above description, the semiconductor substrate 2 has the ni layer 3, but the present invention is not limited thereto. The ni layer 3 may also be a semiconductor layer containing more n-type impurities. In this case, Figure 1 The pin region 10 in the transistor becomes a pn region.
[0053] <Implementation Method 2>
[0054] Figure 2 It is a cross-sectional view showing an example of the structure of a semiconductor device 12 according to the second embodiment of the present invention.
[0055] The semiconductor device 12 according to the second embodiment is characterized in that the difference between the thickness of the ni layer 3 in the pin region 10 and the thickness of the ni layer 3 in the pnp region 11 is the sum of the height difference between the n+ cathode layer 5 and the p collector layer 6 and the thickness of the n- buffer layer 7 in the pnp region 11. Figure 1 The semiconductor device 1 according to the first embodiment shown is the same, and therefore a detailed description thereof will be omitted here.
[0056] like Figure 2 As shown, the n-buffer layer 7 is not formed in the pin region 10, and the n-buffer layer 7 is formed in the pnp region 11. In addition, the n+ cathode layer 5 is formed on the back side of the ni layer 3, and the p collector layer 6 is formed on the back side of the n-buffer layer 7. When viewed from above, the n+ cathode layer 5 and the p collector layer 6 are adjacent, and the adjacent parts of the n+ cathode layer 5 and the p collector layer 6 do not overlap.
[0057] Next, a method for manufacturing the semiconductor device 12 will be described. The following description will focus mainly on differences from the method for manufacturing the semiconductor device 1 according to Embodiment 1. The manufacturing method is the same as that of Embodiment 1 except for the following differences.
[0058] A pn pattern is formed on the back surface of the semiconductor substrate 2, and then the semiconductor substrate 2 in the region where the p collector layer 6 is to be formed is etched to a desired thickness, wherein the pn pattern covers the region where the n+ cathode layer 5 is to be formed and opens the region where the p collector layer 6 is to be formed. Then, B ions are implanted into the region where the p collector layer 6 is to be formed, and the B constitutes the p collector layer 6. Thus, the n+ cathode layer 5 and the p collector layer 6 are formed.
[0059] Next, in the state where the pn pattern is formed, P ions are implanted from the back side of the semiconductor substrate 2 across the p collector layer 6 to form an n-buffer layer 7. At this time, the concentration of P implanted is 1E13 to 1E15 (1 / cm 2 ). Thereafter, the pn pattern is removed to form the back electrode 9.
[0060] As described above, according to the second embodiment, the same effects as those of the first embodiment can be obtained. In addition, since the n-buffer layer 7 is not formed in the pin region 10, Figure 1 Compared with the pin region 10 shown in FIG. 1 , the n-type impurity concentration can be lowered, and the withstand voltage of the pin region 10 can be improved.
[0061] <Implementation Method 3>
[0062] Figure 3 It is a cross-sectional view showing an example of the structure of a semiconductor device 13 according to the third embodiment of the present invention.
[0063] The semiconductor device 13 involved in the present embodiment 3 is characterized in that the stacking height position of the p collector layer 6 in the pnp region 11 is located on the ni layer 3 side compared with the stacking height position of the n+ cathode layer 5 in the pin region 10, and the adjacent parts of the n+ cathode layer 5 and the p collector layer 6 are formed overlapping, and the p collector layer 6 is formed between the n+ cathode layer 5 and the p collector layer 6 at the overlapping part of the adjacent parts. Other structures are similar to Figure 1The semiconductor device 1 according to the first embodiment shown is the same, and therefore a detailed description thereof will be omitted here.
[0064] like Figure 3 As shown, n+ cathode layer 5 and p collector layer 6 are formed on the back side of n- buffer layer 7. In a plan view, n+ cathode layer 5 and p collector layer 6 are adjacent to each other, and adjacent portions of n+ cathode layer 5 and p collector layer 6 overlap.
[0065] Next, a method for manufacturing the semiconductor device 13 will be described. The following description will focus mainly on differences from the method for manufacturing the semiconductor device 1 according to Embodiment 1. The manufacturing method is the same as that of Embodiment 1 except for the following differences.
[0066] A pn pattern is formed on the back surface of the semiconductor substrate 2, and then the semiconductor substrate 2 in the region where the p collector layer 6 is to be formed is etched to a desired thickness, wherein the pn pattern covers the region where the n+ cathode layer 5 is to be formed and opens the region where the p collector layer 6 is to be formed. Then, B is rotated ion implanted in the region where the p collector layer 6 is to be formed, and the B constitutes the p collector layer 6. Here, the rotational ion implantation refers to performing ion implantation while rotating the semiconductor substrate 2.
[0067] As described above, according to the present embodiment 3, the same effects as those of the embodiment 1 can be obtained. In addition, since the junction between the n-buffer layer 7 having a low impurity concentration and the back electrode 9 disappears, the leakage current can be reduced.
[0068] <Implementation Method 4>
[0069] Figure 4 It is a cross-sectional view showing an example of the structure of a semiconductor device 14 according to the fourth embodiment of the present invention.
[0070] The semiconductor device 14 according to the fourth embodiment is characterized by having an n-type electrode 15 and a p-type electrode 16. The n-type electrode 15 is an electrode having ohmic characteristics suitable for the n-type, and the p-type electrode 16 is an electrode having ohmic characteristics suitable for the p-type.
[0071] The third electrode, the n-type electrode 15, is formed so as to cover the n+ cathode layer 5. The p-type electrode 16 is formed so as to cover the n-type electrode 15 and the p collector layer 6. The difference between the thickness of the ni layer 3 in the pin region 10 and the thickness of the ni layer 3 in the pnp region 11 is the same as the sum of the height difference between the n+ cathode layer 5 and the p collector layer 6 and the thickness of the n-type electrode 15. Figure 1 The semiconductor device 1 according to the first embodiment shown is the same, and therefore a detailed description thereof will be omitted here.
[0072] like Figure 4 As shown, n+ cathode layer 5 and p collector layer 6 are formed on the back side of n- buffer layer 7. In a plan view, n+ cathode layer 5 and p collector layer 6 are adjacent, and adjacent portions of n+ cathode layer 5 and p collector layer 6 do not overlap.
[0073] Next, a method for manufacturing the semiconductor device 14 will be described. The following description will focus mainly on differences from the method for manufacturing the semiconductor device 1 according to Embodiment 1. The manufacturing method is the same as that of Embodiment 1 except for the following differences.
[0074] After forming n − buffer layer 7 , electrode 15 for n type is formed on n + cathode layer 5 . Then, electrode 16 for p type is formed so as to cover electrode 15 for n type and p collector layer 6 .
[0075] As described above, according to the present embodiment 4, the same effects as those of the embodiment 1 are obtained. In addition, since the n-type electrode 15 is formed on the n + cathode layer 5 and the p-type electrode 16 is formed on the p collector layer 6 , the ohmic characteristics are improved.
[0076] <Implementation method 5>
[0077] Figure 5 It is a cross-sectional view showing an example of the structure of a semiconductor device 17 according to the fifth embodiment of the present invention.
[0078] The semiconductor device 17 is characterized in that the thickness of the ni layer 3 in the pin region 10 is thinner than the thickness of the ni layer 3 in the pnp region 11. Figure 1 The semiconductor device 1 according to the first embodiment shown is the same, and therefore a detailed description thereof will be omitted here.
[0079] like Figure 5 As shown, n+ cathode layer 5 and p collector layer 6 are formed on the back side of n- buffer layer 7. In a plan view, n+ cathode layer 5 and p collector layer 6 are adjacent, and adjacent portions of n+ cathode layer 5 and p collector layer 6 do not overlap.
[0080] Next, a method for manufacturing the semiconductor device 17 will be described. The following description will focus mainly on differences from the method for manufacturing the semiconductor device 1 according to Embodiment 1. The manufacturing method is the same as that of Embodiment 1 except for the following differences.
[0081] After forming the surface electrode 8 and polishing the semiconductor substrate 2 , B ions are implanted into the entire back surface of the semiconductor substrate 2 . The B constitutes the p-collector layer 6 .
[0082] Next, a pn pattern is formed on the back surface of the semiconductor substrate 2, and then the semiconductor substrate 2 in the region where the n+ cathode layer 5 is to be formed is etched to a desired thickness, wherein the pn pattern covers the region where the p collector layer 6 is to be formed and opens the region where the n+ cathode layer 5 is to be formed. Then, P ions are implanted into the region where the n+ cathode layer 5 is to be formed, and the P ions constitute the n+ cathode layer 5.
[0083] Next, after the pn pattern is removed, P ions are implanted from the back side of the semiconductor substrate 2 across the n + cathode layer 5 and the p collector layer 6 to form an n − buffer layer 7 .
[0084] As described above, according to the fifth embodiment, the operation of the pin region 10 and the operation of the pnp region 11 can be independently controlled. In addition, the thickness of the ni layer 3 in the pin region 10 is thinner than the thickness of the ni layer 3 in the pnp region 11. Therefore, low on-resistance and low recovery loss of the diode can be achieved.
[0085] In addition, if Figure 6 As shown, a semiconductor device 18 having an n-type electrode 15 and a p-type electrode 16 may also be provided. The p-type electrode 16 is formed in a manner covering the p collector layer 6. The n-type electrode 15 is formed in a manner covering the n+ cathode layer 5 and the p-type electrode 16. In this case, similarly to the fourth embodiment, the n-type electrode 15 is formed for the n+ cathode layer 5, and the p-type electrode 16 is formed for the p collector layer 6, so that the ohmic characteristics are improved.
[0086] At once Figure 5 , 6 For the semiconductor devices 17 and 18 shown, the stacking height position of the n+ cathode layer 5 in the pin region 10 may be located on the ni layer 3 side compared to the stacking height position of the p collector layer 6 in the pnp region 11, and the adjacent portions of the n+ cathode layer 5 and the p collector layer 6 may be formed overlappingly, and the n+ cathode layer 5 may be formed between the n+ cathode layer 5 and the p collector layer 6 at the overlapping portion of the adjacent portions. In this case, as in the third embodiment, the junction position between the n-buffer layer 7 having a low impurity concentration and the back electrode 9 disappears, so that the leakage current can be reduced.
[0087] Furthermore, the present invention can freely combine the various embodiments, or appropriately modify or omit the various embodiments within the scope of the invention.
Claims
1. A semiconductor device, characterized in that: It has a stacked structure, which is composed of the following parts: a first semiconductor layer of a first conductivity type; a second semiconductor layer of a second conductivity type formed on a surface of the first semiconductor layer; The third semiconductor layer of the first conductivity type is formed on the back side of the first semiconductor layer; The fourth semiconductor layer of the first conductivity type and the fifth semiconductor layer of the second conductivity type are formed on the back side of the third semiconductor layer, or on the back side of the first semiconductor layer and the third semiconductor layer, adjacent to each other or overlapping adjacent parts when viewed from above; a first electrode formed so as to cover a surface of the second semiconductor layer; as well as a second electrode formed so as to cover the back surfaces of the fourth semiconductor layer and the fifth semiconductor layer, The stacking height position of the fourth semiconductor layer in the stacking structure is different from the stacking height position of the fifth semiconductor layer in the stacking structure, The second semiconductor layer overlaps with the fourth semiconductor layer and the fifth semiconductor layer in a plan view, The stacked structure constitutes an RFC diode, wherein RFC means releasing the cathode field. The thickness of the first semiconductor layer in the stacked structure including the fourth semiconductor layer is different from the thickness of the first semiconductor layer in the stacked structure including the fifth semiconductor layer. A difference between a thickness of the first semiconductor layer in the stacked structure including the fourth semiconductor layer and a thickness of the first semiconductor layer in the stacked structure including the fifth semiconductor layer and a height difference between the fourth semiconductor layer and the fifth semiconductor layer are the same.
2. The semiconductor device according to claim 1, wherein: The stacking height position of the fifth semiconductor layer in the stacking structure is located on the first semiconductor layer side compared to the stacking height position of the fourth semiconductor layer in the stacking structure, and the adjacent portions of the fourth semiconductor layer and the fifth semiconductor layer are formed overlappingly. The fifth semiconductor layer is formed between the fifth semiconductor layer and the fourth semiconductor layer at a location where the adjacent portions overlap.
3. The semiconductor device according to claim 1, wherein: The stacking height position of the fourth semiconductor layer in the stacking structure is located on the first semiconductor layer side compared to the stacking height position of the fifth semiconductor layer in the stacking structure, and the adjacent portions of the fourth semiconductor layer and the fifth semiconductor layer are formed overlappingly. The fourth semiconductor layer is formed between the fifth semiconductor layer and the fourth semiconductor layer at a location where the adjacent portions overlap.
4. The semiconductor device according to claim 1, wherein: further comprising a third electrode formed between the fourth semiconductor layer and the second electrode, The difference between the thickness of the first semiconductor layer in the stacked structure including the fourth semiconductor layer and the thickness of the first semiconductor layer in the stacked structure including the fifth semiconductor layer is the total thickness of the height difference between the fourth semiconductor layer and the fifth semiconductor layer and the thickness of the third electrode.
5. The semiconductor device according to claim 1, wherein: The thickness of the first semiconductor layer in the stacked structure including the fifth semiconductor layer is thinner than the thickness of the first semiconductor layer in the stacked structure including the fourth semiconductor layer.
6. The semiconductor device according to claim 1, wherein: The thickness of the first semiconductor layer in the stacked structure including the fourth semiconductor layer is thinner than the thickness of the first semiconductor layer in the stacked structure including the fifth semiconductor layer.