Integrated lens preparation method

Through the integrated pressing method, the assembly problem caused by the non-round shape of the edge of the optical lens is solved, the mold processing cost is reduced, the yield of the optical lens is improved, and the economic benefits of mass production of optical lenses are realized.

CN115113307BActive Publication Date: 2024-10-08HUATONG OPTICAL TECHNOLOGY (ZHEJIANG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210394807.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-14
Publication Date
2024-10-08
Estimated Expiration
2042-04-14

AI Technical Summary

Technical Problem

The problem of existing optical lenses being unable to assemble due to the non-round edge shape during the assembly process, as well as the high cost and complex equipment structure, limits the mass production and yield of optical lenses.

Method used

Adopting an integrated pressing method, by setting up a mold and metal gasket with a spherical crown-shaped pit structure, using laser cutting or metal etching to form a ring pattern, combined with motor drive and heating technology, the symmetrical pressing of optical lenses is achieved, reducing the cost Mold processing costs and improved yield.

Benefits of technology

It improves the yield rate of optical lenses, reduces mold processing costs, simplifies the processing process, significantly reduces costs and increases the yield rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115113307B_ABST
    Figure CN115113307B_ABST
Patent Text Reader

Abstract

The present invention relates to a preparation method for integrated pressing of an optical lens. A metal gasket is placed on a lower mold. The size of the metal gasket can be consistent with the surface area of ​​the lower mold, or slightly larger or smaller. The thickness is generally the same as or slightly thicker than the outer edge of the optical lens to be prepared. An annular pattern is formed in the center of the metal gasket by laser cutting or metal etching. The annular pattern is connected to the metal gasket as a whole through a support bar; after the pressing step, an annular metal hoop generated by the annular pattern is fixed to the periphery of the generated optical lens. Using the preparation method of the present invention, the annular metal hoop 502 is chamfered or edged, which replaces the chamfering or edge grinding of the optical lens itself, thereby improving the yield rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing an optical lens, and in particular to a method for preparing an optical lens by integrally pressing the optical lens. Background Art

[0002] Glass has better light transmittance and there are hundreds of varieties of glass. Therefore, for optical lenses, optical lenses have significant advantages in terms of light transmittance and variety selection. It can be seen from the fact that high-end digital camera lenses are all optical lenses that the development trend of lenses is to replace plastic with glass. At present, the lens industry, which is mainly composed of three categories: mobile phones, security lenses, and automotive lenses, is developing towards the trend of glass-plastic hybrid lenses. Previously, due to cost considerations, 5-7 lenses in mobile phone lenses were plastic lenses, and only high-end security lenses used glass-plastic hybrid lenses. However, with the development of plastic lenses, it has reached a bottleneck. Its physical property-light transmittance cannot be changed, and equipment manufacturers continue to pursue higher optical performance. Therefore, since 2021, some mobile phones have begun to try to add an optical lens to the lens. And this trend will become more and more obvious in the next few years. However, the main reason for limiting the large-scale application of optical lenses in mobile phones, security, and automotive lenses is cost and production capacity.

[0003] In response to the above needs, glass molding technology, as a technology that can quickly manufacture optical lenses, has become a hot technology in the optical lens industry in recent years. CN112099205A discloses a method for preparing a wide-angle lens, which uses a glass-made anti-curved aspheric lens to replace a plastic aspheric lens, which can greatly improve the thermal stability and imaging quality of the lens, and is achieved through a lens group consisting of nine lenses and a filter, wherein the second lens, the fifth lens, the eighth lens and the ninth lens in the wide-angle lens are all glass aspheric lenses, and the first lens, the third lens, the fourth lens, the sixth lens and the seventh lens are all glass spherical lenses.

[0004] CN114057382A discloses a precision molded glass aspheric lens manufacturing device for preparing glass aspheric lenses. The device reduces movement during the production process by strengthening and fixing the optical lens, thereby reducing errors and improving the yield rate.

[0005] However, the equipment structure used in these methods is complex and costly, which is not conducive to reducing costs in large-scale production. They also rarely consider the defects of finished optical lenses during the assembly process. It is necessary to ensure that the yield rate of molded optical lenses is appropriate, so that the finished optical lenses can be well assembled and the processing cost of the molding process can be reduced. Summary of the invention

[0006] The object of the present invention is to provide a method for preparing an optical lens, and more particularly to provide a method for preparing an optical lens by integrated pressing for the situation that the edge shape of the optical lens is not round and cannot be assembled after glass molding.

[0007] The method for preparing an integrated pressed lens provided by the present invention comprises the following steps:

[0008] A lower mold is provided, wherein the lower mold is provided with a spherical crown-shaped pit structure, and the spherical crown-shaped pit structure is located at the center of the lower mold; a metal gasket is placed on the lower mold, and the size of the metal gasket can be consistent with the surface area of ​​the lower mold, or slightly larger or smaller, and the thickness is generally the same as or slightly thicker than the outer edge of the optical lens to be prepared, and an annular pattern is formed in the center of the metal gasket by laser cutting or metal etching, and the annular pattern is connected to the metal gasket as a whole through a support bar; an upper mold is provided, and the structure of the upper mold is symmetrical with that of the lower mold, so as to generate the upper surface of the optical lens and the outer edge of one side of the optical lens, thereby forming a symmetrical optical lens; the lens preparation material to be prepared is placed at the center of the annular pattern of the metal gasket, and the lower mold is driven by a motor The mold rises, and a voltage is used to heat the lower mold, thereby transferring heat to the lens preparation material and the metal gasket, so that the temperature of the lens preparation material rises to the conversion temperature (Tg) of the optical material and above; as the lower mold continues to rise, the metal gasket and the glass ball 303 are carried so that the metal gasket and the glass ball contact the upper mold to complete the pressing step, so as to generate the lower surface of the optical lens and the outer edge of the other side of the optical lens; the heating is stopped to cool the temperature, and an annular metal hoop generated by the annular pattern is fixed to the periphery of the generated optical lens, the remaining parts of the support bar and the metal gasket are removed, and the optical lens with the annular metal hoop is taken out; the size of the annular metal hoop is consistent with the outer edge size of the prepared optical lens, and the size difference between the two is controlled within ±0.01mm.

[0009] In another aspect of the method of the present invention, the metal gasket is a copper gasket; the lens preparation material is an optical glass material or an optical plastic material; the optical glass material is polymethyl methacrylate (PMMA), polycarbonate (PC), borosilicate glass, silicate glass, phosphate glass or lanthanum glass, and the optical plastic material is polymethyl methacrylate (PMMA) or polycarbonate (PC); the upper mold and the lower mold are both single crystal silicon materials with a graphene-like coating; the thickness of the copper gasket is 0.1-1 mm; and the metal etching method is wet etching or dry etching.

[0010] The preparation method of the present invention improves the yield rate on the one hand, that is, it prevents some lenses from becoming waste products due to the outer edge shape problem during the pressing process. On the other hand, it reduces the processing cost of the mold. Since the mold is processed by an ultra-precision processing method, the processing time is a key indicator of the processing cost. By avoiding the problem of directly processing the outer edge structure on the mold, the processing difficulty is reduced, the time can be reduced by nearly half, and thus the processing cost is reduced by half, which has significant economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments. Obviously, the drawings described below are only some examples of the present invention, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying innovative work.

[0012] Figure 1 This is a cross-sectional view of the molded optical lens prepared by the present invention.

[0013] Figure 2 This is an exploded view of the assembly of the molded optical lens and the lens barrel sleeve prepared by the present invention.

[0014] Figure 3 It is a schematic diagram of the pressing step in the lens preparation method of the present invention.

[0015] Figure 4 It is a cross-sectional view of the lower mold and a top view of the gasket in the lens preparation method of the present invention.

[0016] Figure 5 This is a comparison chart between an optical lens prepared by the lens preparation method of the present invention and an ordinary lens. DETAILED DESCRIPTION

[0017] Now, in conjunction with the corresponding drawings, specific embodiments of the present invention will be described. However, the present invention can be implemented in many different forms and should not be construed as being limited to the embodiments shown here. These embodiments are provided only so that the present invention can be detailed and comprehensive, so that the scope of the present invention can be fully described to those skilled in the art. The wording used in the detailed description of the embodiments illustrated in the drawings should not limit the present invention.

[0018] The optical lens itself is circular, and the upper and lower surfaces 101 of the optical lens are convex, and the edge of the optical lens has upper and lower outer edges 104 with certain chamfers 102 and 103, respectively. The upper and lower outer edges 104 both have platform portions and form a circular cylinder around the circular optical lens. The outer edge 104 is used to assemble the optical lens itself into the lens barrel. In the case where multiple lenses need to be concentrically assembled in the lens barrel, if the outer circle size formed by the outer edge is inaccurate and cannot be accurately assembled with the inner circle of the sleeve, resulting in a situation where concentricity cannot be achieved, it is necessary to further correct the size of the chamfers 102 and 103 by edge grinding or other methods.

[0019] Figure 2 The figure is an exploded view of the molded optical lens and the lens barrel sleeve assembly prepared by the present invention. The outer edge 104 of the optical lens is embedded in the inner circle of the lens barrel sleeve, so that the optical lens is fixed in the sleeve, and then further integrated with other lenses to form a concentric state of multiple lenses, thereby preparing a complete lens.

[0020] Figure 3 Schematic diagram of the pressing step in the lens preparation method of the present invention. The integrated pressing lens preparation method of the present invention includes a heating step, wherein a glass product to be pressed, such as a glass ball 303, is placed on the lower mold 302. There is no particular restriction on the type of glass that can be used, and known glass can be selected to use according to the purpose. For example, optical glasses such as borosilicate glass, silicate glass, phosphate glass, and lanthanum glass are cited. The present invention can also be used to process plastic lenses. The premise for being suitable for plastic lenses is that the plastic material used meets the requirement of maintaining stable performance when heated to a certain temperature and can realize the function of the lens. The plastic material includes polymethyl methacrylate (PMMA), polycarbonate (PC), etc.

[0021] A motor (not shown) drives the lower mold 302 to rise, and heats the lower mold 302 with voltage, thereby transferring heat to the glass ball 303, so that the temperature of the glass ball 303 rises to the transition temperature (Tg) of the glass or above; in a pressing step, the motor of the lower mold 302 continues to drive the lower mold 302 to rise, while carrying the glass ball 303 to move, so that the glass ball 303 contacts the upper mold 301, and the pressing process is completed; in an annealing and cooling step, a slow annealing treatment is performed, and the molded lens is subjected to a preliminary annealing treatment in the molding mold to release internal stress; the annealed molded lens is taken out of the molding mold, placed on a cooling plate and cooled to room temperature alone; in a demolding step, the cooled molded product is separated from the upper mold 301 and the lower mold 302.

[0022] The upper mold 301 and the lower mold 302 described here are both made of single crystal silicon material with a graphene-like coating. In order to simultaneously process the surface 101 and the outer edge 104 of the glass lens, the structure of the lower mold 302 is set to have a spherical crown pit structure 401. Since the optical lens prepared in the preparation method of the present invention is symmetrical, in the present invention, the upper mold 301 adopts a structure completely consistent with the lower mold 302 and also has a spherical crown pit structure. The difference between the two is only in the different placement orientations.

[0023] Figure 4 The figure is a cross-sectional view of the lower mold and a top view of the gasket in the lens preparation method of the present invention. The gasket 503 is made of metal material, such as copper; the size of the gasket 503 can be consistent with the surface area of ​​the lower mold, or slightly larger or smaller, and the thickness is generally the same as or slightly thicker than the outer edge of the optical lens. In one embodiment, a gasket with a thickness of about 0.1-1 mm can be used; before the lens is prepared, a ring pattern 502, i.e., a ring metal hoop, is formed in the center of the gasket 503 by laser cutting or metal etching, such as wet etching or dry etching, in advance, and the ring pattern 502 is connected to the gasket 503 as a whole by means of a support bar 504. The size of the ring metal hoop 502 is consistent with the size of the outer edge 104 of the optical lens to be prepared, and the size difference between the two is controlled within ±0.01 mm. In the molding process of heating the lower mold 302 by the electrode 501, the glass ball 303 is softened by heat and then contacts and squeezes with the ring metal hoop 502. After the molding is completed, the temperature is cooled, and the annular metal hoop 502 is firmly fixed on the periphery of the optical lens. Then, the support bar 504 is removed, and the optical lens with the annular metal hoop 502 is taken out.

[0024] Figure 5 The figure is a comparison between the optical lens prepared by the lens preparation method of the present invention and the ordinary lens. In the calibration process of the optical lens with the annular metal hoop 502, the annular metal hoop 502 is chamfered or edged instead of the chamfering or edged of the optical lens itself. Since the annular metal hoop 502 is softer than the optical lens material, in one embodiment, the Mohs hardness of the optical lens is 7, and the Mohs hardness of the copper metal hoop 502 is 3, it is much easier to grind the edge of the copper metal hoop 502 than to directly grind the edge of the optical lens, and it has the characteristic of being easier to operate, thus significantly reducing the calibration time and improving the yield rate.

[0025] References herein to "one embodiment," "embodiment," or "one or more embodiments" mean that a particular feature, structure, or characteristic described in conjunction with the embodiment is included in at least one embodiment of the present invention. In addition, please note that examples of the term "in one embodiment" do not necessarily all refer to the same embodiment.

[0026] The above is only used to illustrate the technical solution of the present invention. Any person skilled in the art can modify and change the above embodiments without violating the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be subject to the scope of the claims. The present invention has been described above in conjunction with examples. However, other embodiments other than the above embodiments within the scope of the present invention are also feasible. The different features and steps of the present invention can be combined in other ways than described. The scope of the present invention is limited only by the appended claims. More generally, a person skilled in the art can easily understand that all parameters, dimensions, materials and configurations described herein are for demonstration purposes and the actual parameters, dimensions, materials and / or configurations will depend on the specific application or application for which the present invention is taught.

Claims

1. A method for preparing an integrated pressed lens, comprising the following steps: A lower mold is provided, wherein the lower mold is provided with a spherical crown-shaped pit body structure, and the spherical crown-shaped pit body structure is located at the center of the lower mold; A metal gasket is placed on the lower mold. The size of the metal gasket can be consistent with the surface area of ​​the lower mold, or slightly larger or smaller. The thickness is generally the same as or slightly thicker than the outer edge of the optical lens to be prepared. A ring-shaped pattern is formed in the center of the metal gasket by laser cutting or metal etching. The ring-shaped pattern is connected to the metal gasket as a whole through a support bar. An upper mold is provided, wherein the structure of the upper mold is symmetrical with the structure of the lower mold, so as to generate an upper surface of the optical lens and an outer edge of one side of the optical lens, thereby forming a symmetrical optical lens; The lens preparation material to be prepared is placed at the center of the annular pattern of the metal gasket, the lower mold is driven to rise by a motor, and the lower mold is heated by a voltage to transfer heat to the lens preparation material and the metal gasket, so that the temperature of the lens preparation material rises to the transformation temperature (Tg) of the lens preparation material or above; as the lower mold continues to rise, the metal gasket and the lens preparation material are carried, and as the lens preparation material is softened by heat, the metal gasket and the lens preparation material are contacted with the upper mold to complete the pressing step through contact extrusion, so as to generate the lower surface of the optical lens and the outer edge of the other side of the optical lens; Stop heating to cool the temperature, fix the annular metal hoop formed by the annular pattern on the periphery of the generated optical lens, remove the remaining part of the support bar and the metal gasket, and take out the optical lens with the annular metal hoop; The size of the annular metal hoop is consistent with the outer edge size of the prepared optical lens, and the size difference between the two is controlled within ±0.01mm.

2. The lens preparation method according to claim 1, wherein the metal gasket is a copper gasket.

3. The lens preparation method according to claim 1, wherein the lens preparation material is an optical glass material or an optical plastic material.

4. The lens preparation method according to claim 3, wherein the optical glass material is polymethyl methacrylate (PMMA), polycarbonate (PC), borosilicate glass, silicate glass, phosphate glass or lanthanide glass, and the optical plastic material is polymethyl methacrylate (PMMA) or polycarbonate (PC). 5 . The lens manufacturing method according to claim 1 , wherein the upper mold and the lower mold are both made of single crystal silicon material with a graphene-like coating.

6. The lens manufacturing method as claimed in claim 2, wherein the thickness of the copper gasket is 0.1-1 mm.

7. The lens manufacturing method as claimed in claim 1, wherein the metal etching method is wet etching or dry etching.