Semiconductor device and method for manufacturing the same
By using a multi-layer mask structure and specific process technology under the conditions of a photolithography machine, a target pattern with smaller line width and good uniformity is achieved, which solves the difficulty of achieving smaller line width and uniformity with the photolithography machine in the existing technology. sexual issues and improve semiconductor manufacturing capabilities.
Patent Information
- Application Number
- CN202210927471.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-03
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-08-03
AI Technical Summary
Under the limitations of the photolithography machine, it is difficult for the existing dual patterning process to achieve target patterns with smaller line widths and good line width uniformity and topography.
By forming a patterned multi-layer mask structure, including first, second and third mask layers, using atomic layer deposition and atomic layer etching processes to fill and remove the mask layers, forming the target pattern, and using the fourth mask layer The film layer is etched as a mask, and unnecessary mask layers are removed to achieve the formation of the target pattern.
Under the constraints of the lithography machine, the target pattern with a smaller size line width is achieved, while ensuring the line width uniformity and morphology of the target pattern, breaking through the technical blockade of the lithography machine, and improving the manufacturing capacity of the semiconductor process.
Smart Images

Figure CN115132572B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a semiconductor device and a manufacturing method thereof. Background Art
[0002] As logic processes continue to pursue smaller line widths, lithography technology becomes increasingly important. However, extreme ultraviolet lithography machines are expensive, and the corresponding process manufacturing costs are extremely high. The design of process methods to obtain smaller line widths is also gaining more and more attention. The double patterning process widely used in the industry is an effective process method to obtain smaller line widths, but a serious disadvantage of the graphics produced by this process method is that it has a left-right asymmetry in its physical structure, and it is difficult to obtain better line width roughness and smoother morphology in the process of smaller line widths.
[0003] See also Figure 1a to Figure 1c The steps of the double patterning process include: first, Figure 1a As shown, a substrate 11 is provided, a layer 12 to be patterned is formed on the substrate 11, and a plurality of mandrels 13 arranged at intervals are formed on the layer 12 to be patterned; then, as shown in FIG. Figure 1b As shown, a mask layer 14 is deposited on the layer to be patterned 12 and the surface of the mandrel 13; then, as shown in Figure 1c As shown, an etching process is performed to remove the top surface of the core shaft 13 and the mask layer 14 on the layer to be patterned 12, and the mask layer 14 retained on the side wall of the core shaft 13 serves as the side wall 15; then, the core shaft 13 is etched away, and subsequently the layer to be patterned 12 is etched using the side wall 15 as a mask to form a desired pattern in the layer to be patterned 12. Among them, since one side of the mask layer 14 on the side wall of the core shaft 13 is in contact with the core shaft 13 and the other side is not in contact with the core shaft 13, after the mask layer 14 is etched to form the side wall 15, the other side that is not in contact with the core shaft 13 is in an arc structure, and the side in contact with the core shaft 13 is in a vertical structure due to the existence of the core shaft 13. After removing the core shaft 13, the side in contact with the core shaft 13 maintains a vertical structure, resulting in each side wall 15 formed having a vertical structure on one side close to the core shaft 13 and an arc structure on the side away from the core shaft 13. The structure of the side wall 15 is asymmetric. Therefore, when the layer to be patterned 12 is subsequently etched using the side wall 15 as a mask, the line width uniformity and morphology of the pattern formed in the layer to be patterned 12 will be greatly affected, and it is difficult to solve this problem through process adjustment.
[0004] Therefore, how to form a pattern with smaller line width and good line width uniformity under the limitation of the lithography machine is a problem that needs to be solved urgently. Summary of the invention
[0005] The object of the present invention is to provide a semiconductor device and a method for manufacturing the same, so that a target pattern with a smaller line width can be achieved under the condition of a photolithography machine limitation, and the target pattern can have good line width uniformity and morphology.
[0006] To achieve the above object, the present invention provides a method for manufacturing a semiconductor device, comprising:
[0007] Forming a patterned first mask layer and a second mask layer on a substrate, wherein a first opening exposing the surface of the substrate is formed in the patterned first mask layer, and the second mask layer fills the first opening;
[0008] Forming a patterned third mask layer on the patterned first mask layer and the second mask layer, wherein the patterned third mask layer is formed with a second opening that simultaneously exposes a portion of the patterned first mask layer and a portion of the second mask layer;
[0009] Using the patterned third mask layer as a mask, etching and removing the patterned first mask layer or the second mask layer exposed by the second opening to form a third opening exposing the surface of the substrate;
[0010] Filling a fourth mask layer in the third opening;
[0011] removing the patterned first mask layer and the second mask layer;
[0012] The substrate is patterned using the fourth mask layer as a mask to form a target pattern in the substrate.
[0013] Optionally, an atomic layer deposition process is used to fill the second mask layer in the first opening.
[0014] Optionally, an atomic layer etching process is used to etch and remove the patterned first mask layer or the second mask layer exposed by the second opening.
[0015] Optionally, the etching selectivity ratio of the patterned first mask layer to the second mask layer is greater than 100, and the patterned first mask layer exposed by the second opening is etched away; the etching selectivity ratio of the second mask layer to the patterned first mask layer is greater than 100, and the second mask layer exposed by the second opening is etched away.
[0016] Optionally, after forming the third opening exposing the surface of the substrate and before filling the fourth mask layer in the third opening, the method for manufacturing the semiconductor device further includes:
[0017] The patterned third mask layer is removed.
[0018] Optionally, a spin coating process is used to fill the fourth mask layer in the third opening.
[0019] Optionally, the patterned first mask layer and the second mask layer are removed by etching using a wet etching process or a dry etching process.
[0020] Optionally, an etching selectivity ratio of the patterned first mask layer, the second mask layer and the fourth mask layer is greater than 20.
[0021] Optionally, the material of the patterned first mask layer is at least one of silicon oxide, silicon nitride and silicon oxynitride, the material of the second mask layer is at least one of amorphous silicon, polycrystalline silicon and silicon germanium, and the material of the fourth mask layer is at least one of spin-coated carbon, amorphous carbon and an organic dielectric layer.
[0022] Optionally, the base includes a substrate to be patterned, or the base includes a substrate and a layer to be patterned formed on the substrate.
[0023] The present invention also provides a semiconductor device manufactured by adopting the manufacturing method of the semiconductor device.
[0024] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0025] 1. The method for manufacturing a semiconductor device of the present invention comprises: forming a patterned first mask layer and a second mask layer on a substrate, wherein a first opening exposing the surface of the substrate is formed in the patterned first mask layer, and the second mask layer is filled in the first opening; forming a patterned third mask layer on the patterned first mask layer and the second mask layer, wherein a second opening exposing a portion of the patterned first mask layer and a portion of the second mask layer is formed in the patterned third mask layer; using the patterned third mask layer as a mask, etching and removing the patterned first mask layer or the second mask layer exposed by the second opening to form a third opening exposing the surface of the substrate; filling a fourth mask layer in the third opening; removing the patterned first mask layer and the second mask layer; and patterning the substrate using the fourth mask layer as a mask to form a target pattern in the substrate, so that a target pattern with a smaller line width can be achieved under the condition of the limitation of the lithography machine, and the target pattern can have good line width uniformity and morphology, so as to break through the technical blockade of the lithography machine and improve the manufacturing capacity of the semiconductor process.
[0026] 2. The semiconductor device of the present invention is manufactured by the semiconductor device manufacturing method, so that under the condition of the limitation of the lithography machine, a target pattern with a smaller line width can be achieved, and the target pattern can have good line width uniformity and morphology. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1a to Figure 1c A schematic diagram of a device in a method for manufacturing a semiconductor device;
[0028] Figure 2 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;
[0029] Figure 3a to Figure 3i yes Figure 2 A schematic diagram of a device in a method for manufacturing a semiconductor device is shown.
[0030] Among them, Figure 1a to Figure 3i The reference numerals are described as follows:
[0031] 11-substrate; 12-layer to be patterned; 13-core; 14-mask layer; 15-side wall; 21-base; 211-substrate; 212-etching stop layer; 213-layer to be patterned; 22-patterned first mask layer; 221-first mask layer; 222-patterned photoresist layer; 223-first opening; 23-second mask layer; 24-patterned third mask layer; 241-second opening; 25-third opening; 26-fourth mask layer. DETAILED DESCRIPTION
[0032] In order to make the purpose, advantages and features of the present invention more clear, the semiconductor device and the manufacturing method thereof proposed by the present invention are further described in detail below in conjunction with the accompanying drawings. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0033] An embodiment of the present invention provides a method for manufacturing a semiconductor device. Figure 2 , Figure 2 1 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention, wherein the method for manufacturing a semiconductor device comprises:
[0034] Step S1, forming a patterned first mask layer and a second mask layer on a substrate, wherein a first opening exposing the surface of the substrate is formed in the patterned first mask layer, and the second mask layer fills the first opening;
[0035] Step S2, forming a patterned third mask layer on the patterned first mask layer and the second mask layer, wherein the patterned third mask layer is formed with a second opening that simultaneously exposes a portion of the patterned first mask layer and a portion of the second mask layer;
[0036] Step S3, using the patterned third mask layer as a mask, etching and removing the patterned first mask layer or the second mask layer exposed by the second opening to form a third opening exposing the surface of the substrate;
[0037] Step S4, filling the third opening with a fourth mask layer;
[0038] Step S5, removing the patterned first mask layer and the second mask layer;
[0039] Step S6: patterning the substrate using the fourth mask layer as a mask to form a target pattern in the substrate.
[0040] See below Figure 3a to Figure 3i The method for manufacturing the semiconductor device provided in this embodiment is described in more detail. Figure 3a to Figure 3i It is a cross-sectional schematic diagram of a semiconductor device.
[0041] Follow step S1, refer to Figure 3a to Figure 3c , provide a substrate 21, form a patterned first mask layer 22 and a second mask layer 23 on the substrate 21, the patterned first mask layer 22 is formed with a first opening 223 exposing the surface of the substrate 21, and the second mask layer 23 is filled in the first opening 223.
[0042] The base 21 may only include a substrate 211 to be patterned; or Figure 3a As shown, the base 21 includes a substrate 211 and a layer to be patterned 213 formed on the substrate 211. An etching stopper layer 212 may be formed between the substrate 211 and the layer to be patterned 213, so that the etching stops in the etching stopper layer 212 when the layer to be patterned 213 is subsequently etched. The layer to be patterned 213 may be a single-layer structure or a structure of at least two stacked layers.
[0043] The steps of forming the patterned first mask layer 22 on the substrate 21 include: first, Figure 3a As shown, a first mask layer 221 is formed to cover the substrate 21; then, a patterned photoresist layer 222 is formed on the first mask layer 221; then, as shown Figure 3bAs shown, the patterned photoresist layer 222 is used as a mask, and the first mask layer 221 is etched by a wet or dry etching process to form a patterned first mask layer 22, in which a first opening 223 exposing the surface of the substrate 21 is formed; then, the patterned photoresist layer 222 is removed.
[0044] like Figure 3c As shown, the step of filling the second mask layer 23 in the first opening 223 includes: first, filling the material of the second mask layer 23 in the first opening 223, and the material of the second mask layer 23 covers the patterned first mask layer 22; then, using a chemical mechanical polishing process to remove the material of the second mask layer 23 covering the patterned first mask layer 22, and retaining the material of the second mask layer 23 in the first opening 223 as the second mask layer 23, and the top surface of the second mask layer 23 is flush with the top surface of the patterned first mask layer 22.
[0045] Furthermore, since the filling capability of the atomic layer deposition (ALD) process is better than that of the chemical vapor deposition process, it is preferred that the atomic layer deposition process is used to fill the second mask layer 23 in the first opening 223, and the atomic layer deposition process is particularly suitable for filling the first opening 223 with a high aspect ratio. In other embodiments, the second mask layer 23 may also be filled in the first opening 223 by a plasma enhanced chemical vapor deposition (PECVD) process.
[0046] Step S2: Refer to Figure 3d A patterned third mask layer 24 is formed on the patterned first mask layer 22 and the second mask layer 23, and a second opening 241 is formed in the patterned third mask layer 24 to expose a portion of the patterned first mask layer 22 and a portion of the second mask layer 23 at the same time.
[0047] Preferably, the material of the patterned third mask layer 24 is photoresist.
[0048] Among them, the step of forming the patterned third mask layer 24 may include: first, forming a third mask layer covering the patterned first mask layer 22 and the second mask layer 23; then, aligning the opening in the mask of a specific pattern with the boundary area between the patterned first mask layer 22 and the second mask layer 23 below, that is, the projection of the opening in the mask in a direction perpendicular to the substrate 21 simultaneously covers the adjacent part of the patterned first mask layer 22 and the part of the second mask layer 23; then, performing an exposure and development process to form the third mask layer into the patterned third mask layer 24, and the opening in the mask is transferred to the second opening 241 in the patterned third mask layer 24, so that at least one of the second openings 241 simultaneously exposes the adjacent part of the patterned first mask layer 22 and the part of the second mask layer 23.
[0049] Step S3: Refer to Figure 3e , using the patterned third mask layer 24 as a mask, etching and removing the patterned first mask layer 22 or the second mask layer 23 exposed by the second opening 241 to form a third opening 25 exposing the surface of the substrate 21 .
[0050] Preferably, an atomic layer etching (ALE) process is used to etch and remove the patterned first mask layer 22 or the second mask layer 23 exposed by the second opening 241 .
[0051] Among them, since the atomic layer etching process only involves chemical etching of the structure to be etched, and there is no physical etching (physical etching will physically bombard the structure to be etched and other structures other than the structure to be etched, causing both to be etched), that is, the atomic layer etching process removes the structure to be etched by selecting a suitable etching gas to chemically react with the structure to be etched. Therefore, by selecting an etching gas that only chemically reacts with the structure to be etched, etching of structures other than the structure to be etched can be avoided, thereby making the structure to be etched and the structure other than the structure to be etched have a very high etching selectivity, for example, the etching selectivity can reach greater than 100.
[0052] When the atomic layer etching process is used to remove the structure to be etched, the etching gas will first react chemically with the surface of the structure to be etched to produce a compound, and then a vacuum pump will be used to extract the compound on the surface, so that the structure to be etched below the compound continues to react with the etching gas, and this cycle will be repeated until the entire structure to be etched is removed.
[0053] In this embodiment, if the selected etching gas chemically reacts only with the patterned first mask layer 22, the etching selectivity ratio of the patterned first mask layer 22 to the second mask layer 23 is greater than 100, and the patterned first mask layer 22 exposed by the second opening 241 is removed by etching using an atomic layer etching process. Figure 3e As shown, the second mask layer 23 exposed by the second opening 241 will not be etched; if the selected etching gas only chemically reacts with the second mask layer 23, the etching selectivity ratio of the second mask layer 23 to the patterned first mask layer 22 is greater than 100, and the second mask layer 23 exposed by the second opening 241 is etched and removed by an atomic layer etching process, and the patterned first mask layer 22 exposed by the second opening 241 will not be etched.
[0054] The material of the patterned first mask layer 22 may be at least one of silicon oxide, silicon nitride and silicon oxynitride, and the etching gas used to etch and remove the patterned first mask layer 22 exposed by the second opening 241 by using the atomic layer etching process may be C4F6 or C4F8; the material of the second mask layer 23 may be at least one of amorphous silicon, polycrystalline silicon and silicon germanium, and the etching gas used to etch and remove the second mask layer 23 exposed by the second opening 241 by using the atomic layer etching process may be CH x F y , SiCl4, O2 and He, or it can be NH3, NF3 and H2.
[0055] In addition, after forming the third opening 25 exposing the surface of the substrate 21 in step S3 and before filling the third opening 25 with the fourth mask layer 26 in the subsequent step S4, the method for manufacturing the semiconductor device further includes: Figure 3f , remove the patterned third mask layer 24.
[0056] Step S4: Refer to Figure 3g , filling the third opening 25 with a fourth mask layer 26 .
[0057] Preferably, the fourth mask layer 26 is filled in the third opening 25 by a spin coating process.
[0058] Step S5: Refer to Figure 3h , remove the patterned first mask layer 22 and the second mask layer 23.
[0059] Among them, the patterned first mask layer 22 and the second mask layer 23 can be etched away by a wet etching process or a dry etching process. Preferably, the etching selectivity ratio of the patterned first mask layer 22 to the fourth mask layer 26 and the etching selectivity ratio of the second mask layer 23 to the fourth mask layer 26 are both greater than 20, so that when the patterned first mask layer 22 and the second mask layer 23 are etched away, the etching of the fourth mask layer 26 is reduced; and when the patterned first mask layer 22 and the second mask layer 23 are etched away by a wet etching process or a dry etching process, it is preferred that the etching selectivity ratio of the patterned first mask layer 22 to the second mask layer 23 is close to 1, so that the patterned first mask layer 22 and the second mask layer 23 are removed almost at the same time.
[0060] The material of the fourth mask layer 26 may be at least one of spin-on carbon (SOC), amorphous carbon and an organic dielectric layer (ODL).
[0061] Step S6: Refer to Figure 3i , the substrate 21 is patterned using the fourth mask layer 26 as a mask to form a target pattern in the substrate 21 .
[0062] exist Figure 3i In the illustrated embodiment, the fourth mask layer 26 is used as a mask and a dry etching or wet etching process is adopted to pattern the layer to be patterned 213 to form a target pattern in the layer to be patterned 213 .
[0063] In addition, after the target pattern is formed, the fourth mask layer 26 may be removed.
[0064] From the above content, it can be known that in step S2, under the condition of the photolithography machine limitation (that is, the photolithography condition of the photolithography machine remains unchanged), by setting the pattern of the mask at a specific position, the second opening 241 in the patterned third mask layer 24 can simultaneously expose the adjacent part of the patterned first mask layer 22 and part of the second mask layer 23, thereby making the third opening 25 formed in step S3 have a smaller width, so that the fourth mask layer 26 formed in step S4 and the target pattern formed by etching with the fourth mask layer 26 as a mask in step S6 have a smaller line width. Therefore, under the condition of the photolithography machine limitation, a target pattern with a smaller line width can be achieved. Wherein, the line width of the target pattern can be 10nm to 20nm.
[0065] Moreover, in the step S5, since the side wall on one side of the fourth mask layer 26 is in contact with the patterned first mask layer 22, and the side wall on the other side of the fourth mask layer 26 is in contact with the second mask layer 23, after the patterned first mask layer 22 and the second mask layer 23 are etched away, the side walls on both sides of the fourth mask layer 26 can maintain a vertical structure, and the structure of the fourth mask layer 26 is symmetrical on the left and right, so that the target pattern formed by patterning the substrate 21 with the fourth mask layer 26 as a mask in the step S6 can have good line width uniformity and morphology.
[0066] In summary, the manufacturing method of the semiconductor device provided by the present invention comprises: forming a patterned first mask layer and a second mask layer on a substrate, wherein the patterned first mask layer is formed with a first opening exposing the surface of the substrate, and the second mask layer is filled in the first opening; forming a patterned third mask layer on the patterned first mask layer and the second mask layer, wherein the patterned third mask layer is formed with a second opening exposing a portion of the patterned first mask layer and a portion of the second mask layer at the same time; using the patterned third mask layer as a mask, etching The patterned first mask layer or the second mask layer exposed by the second opening is removed to form a third opening exposing the surface of the substrate; a fourth mask layer is filled in the third opening; the patterned first mask layer and the second mask layer are removed; the substrate is patterned using the fourth mask layer as a mask to form a target pattern in the substrate, so that a target pattern with a smaller line width can be achieved under the conditions of the limitations of the lithography machine, and the target pattern can have good line width uniformity and morphology, so as to break through the technical blockade of the lithography machine and improve the manufacturing capacity of the semiconductor process.
[0067] An embodiment of the present invention provides a semiconductor device, which is manufactured using the semiconductor device manufacturing method, and a target pattern is formed on the substrate, so that a target pattern with a smaller line width can be achieved under the conditions of the limitations of the lithography machine, and the target pattern can have good line width uniformity and morphology.
[0068] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: include: Forming a patterned first mask layer and a second mask layer on a substrate, wherein a first opening exposing the surface of the substrate is formed in the patterned first mask layer, and the second mask layer fills the first opening; Forming a patterned third mask layer on the patterned first mask layer and the second mask layer, wherein the patterned third mask layer is formed with a second opening that simultaneously exposes a portion of a single adjacent patterned first mask layer and a portion of a single adjacent second mask layer; Using the patterned third mask layer as a mask, etching and removing the patterned first mask layer or the second mask layer exposed by the second opening to form a third opening exposing the surface of the substrate; Filling a fourth mask layer in the third opening; removing the patterned first mask layer and the second mask layer; The substrate is patterned using the fourth mask layer as a mask to form a target pattern in the substrate.
2. The method for manufacturing a semiconductor device according to claim 1, wherein: The second mask layer is filled in the first opening by an atomic layer deposition process.
3. The method for manufacturing a semiconductor device according to claim 1, wherein: The patterned first mask layer or the second mask layer exposed by the second opening is etched away using an atomic layer etching process.
4. The method for manufacturing a semiconductor device according to claim 3, wherein: The etching selectivity ratio between the patterned first mask layer and the second mask layer is greater than 100, and the patterned first mask layer exposed by the second opening is removed by etching; The etching selectivity ratio of the second mask layer to the patterned first mask layer is greater than 100, and the second mask layer exposed by the second opening is removed by etching.
5. The method for manufacturing a semiconductor device according to claim 1, wherein: After forming the third opening exposing the surface of the substrate and before filling the fourth mask layer in the third opening, the method for manufacturing the semiconductor device further includes: The patterned third mask layer is removed.
6. The method for manufacturing a semiconductor device according to claim 1, wherein: The fourth mask layer is filled in the third opening by a spin coating process.
7. The method for manufacturing a semiconductor device according to claim 1, wherein: The patterned first mask layer and the second mask layer are removed by etching using a wet etching process or a dry etching process.
8. The method for manufacturing a semiconductor device according to claim 7, wherein: The etching selectivity ratios of the patterned first mask layer, the second mask layer and the fourth mask layer are all greater than 20.
9. The method for manufacturing a semiconductor device according to claim 8, wherein: The material of the patterned first mask layer is at least one of silicon oxide, silicon nitride and silicon oxynitride, the material of the second mask layer is at least one of amorphous silicon, polycrystalline silicon and silicon germanium, and the material of the fourth mask layer is at least one of spin-coated carbon, amorphous carbon and an organic dielectric layer.
10. The method for manufacturing a semiconductor device according to any one of claims 1 to 9, wherein: The base includes a substrate to be patterned, or the base includes a substrate and a layer to be patterned formed on the substrate.
11. A semiconductor device, characterized in that: The semiconductor device is manufactured by the method for manufacturing a semiconductor device according to any one of claims 1 to 10.
Citation Information
Patent Citations
Method for forming graph
CN101312113A
Patterning method and semiconductor device formed by same
CN111952154A