Method for chemical cleaning of cast metal parts having a porous ceramic core
By filling the pores of the ceramic core before chemical cleaning, the acid retention problem caused by the communication between the porous ceramic core and the acid bath liquid is solved, ensuring the metal structure integrity and service life of the turbine blades.
Patent Information
- Application Number
- CN202180022299.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-03-18
- Filing Date
- 2021-03-15
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2041-03-15
AI Technical Summary
In metal parts manufactured by investment casting, the communication between the porous ceramic core and the acid bath liquid leads to acid retention, affecting the material distribution and service life of the blade metal structure.
Before chemical cleaning, liquids such as water or alkaline solutions with moderate viscosity are selected by filling the pores of the ceramic core to prevent the penetration of the bath liquid, preferably using a liquid to soak or inject into the metal shell until the pores are saturated.
Effectively prevent acid penetration, avoid the ceramic core from retaining acid, and ensure the integrity and service life of the metal structure of the blade.
Smart Images

Figure HDA0003851425100000011 
Figure HDA0003851425100000012 
Figure HDA0003851425100000021
Abstract
Description
Technical Field
[0001] The invention belongs to the field of manufacturing metal parts by investment casting.
[0002] More particularly, the present invention relates to a method for chemically pickling cast metal parts having a porous ceramic core.
[0003] The invention also relates to a method for producing a metal component by investment casting, in which such a chemical cleaning method is implemented.
[0004] The invention applies in particular to the production of turbine blades for turbomachines having complex geometries, in particular forming an inner cavity of a cooling circuit, such as those mounted on aircraft turbojets. Background Art
[0005] Metal parts such as turbine blades for turbines are usually manufactured using a casting technique known as "investment casting".
[0006] In principle, manufacturing a turbine blade consisting of a metal structure comprising one or more cavities separated from one another by walls by investment casting first involves manufacturing a ceramic component (called “ceramic core”) which will form the blade cavity.
[0007] For each blade that is desired to be manufactured, a wax model is produced, for example by injecting liquid wax under pressure into a metal mold which has the outer shape of the blade inside and in which one or more ceramic cores have been placed depending on the number of cavities the blade should have.
[0008] After demoulding the wax model thus obtained, it is covered with a shell of refractory material (generally ceramic), also called "shell mould", through a successive dipping operation in a slurry followed by a sandblasting operation called "stucco".
[0009] After curing and drying, the shell mold undergoes an operation known as "dewaxing", which consists in draining the wax model from the mold by melting the wax.
[0010] The shell mold is then sintered to remove any traces of wax present in the shell mold, consolidate the mold and bring it to the casting temperature of the metal or alloy.
[0011] After checking the shell mold for internal and external integrity, molten metal or metal alloy is poured into the shell mold and occupies the space existing between the inner wall of the shell mold and the ceramic core after dewaxing and also occupies the space between the ceramic cores if multiple cores are present.
[0012] After the metal or alloy solidifies, the shell mold is broken, usually by vibration or water jets, and the ceramic core is then removed, usually by dissolving in a suitable alkaline solution (KOH or NaOH). These operations are called "shake-out".
[0013] The shakeout operation is followed by various finishing operations and then by checking the turbine blades for compliance.
[0014] Thus, in the investment casting method, the metal structure of the blade is formed by the space into which the metal or alloy has been cast, while the blade cavity is formed by the space left empty by the falling sand ceramic core.
[0015] During the manufacture of some blades, the outer surface of the blade metal structure exposed by the knockout shell mold is chemically cleaned between the knockout shell mold and the knockout ceramic core.
[0016] This cleaning, aimed at suppressing residual surface stresses, is usually carried out by immersing the blades in a bath based on hydrochloric acid.
[0017] Because the ceramic cores are in fluid communication with the acid bath and have a porous structure, they become saturated with and retain the acid during the chemical cleaning process.
[0018] Since sanding of the ceramic core is not necessarily carried out simultaneously with pickling, the acid retained by the ceramic core may lead to a more or less noticeable lack of material in the metal structure of the blade, especially in the inner surface of what is commonly called the "bathtub" in the blade field and in the walls that separate the enclosed internal cavity in this structure.
[0019] Below a certain depth, lack of material does not justify scrapping the blade for non-compliance with the defined specifications, but it will affect the useful life of the blade, whereas above this depth, the blade is susceptible to scrapping. Summary of the invention
[0020] The present invention aims precisely at providing a simple and economical solution to this problem by providing a method for chemically cleaning a cast metal part, wherein the cast metal part comprises a metal shell defining an inner space and an outer space, wherein at least one porous ceramic core is accommodated in the inner space and is in fluid communication with the outer space, the method comprising:
[0021] filling the pores of the ceramic core with a liquid; then
[0022] Chemical cleaning of cast metal parts.
[0023] Therefore, according to the invention, before chemically cleaning the cast metal part, the pores of the ceramic core are filled with a liquid in order to prevent or at least limit the penetration of the bath used for chemical cleaning into these pores.
[0024] Above and below, the term "metal envelope" is understood to mean an envelope made of a metal alloy as well as of metal.
[0025] According to the invention, filling the pores of the ceramic core is preferably performed by immersing the metal component in a liquid, preferably at room temperature.
[0026] However, it is also possible to inject the liquid into the metal component through an opening comprised in the metal shell of the cast metal component.
[0027] Preferably, the pores of the ceramic core are filled until the mass of liquid present in these pores is at least 90%, preferably 95% and ideally 100% of the mass of liquid contained in these pores if they were saturated with liquid.
[0028] The filling time required to obtain this mass of liquid in the pores of the porous core can be easily determined for a given type of cast metal part by weighing the metal part during the filling process - it being understood that, at saturation or quasi-saturation, the weight of the metal part will remain constant or quasi-constant - and then applied to all cast metal parts of the same type.
[0029] The choice of liquid is not particularly limited as long as its viscosity allows it to easily penetrate the pores of the ceramic core.
[0030] However, it is preferred that an aqueous solution is used, which may be a dilute solution of a base such as soda or potash, and preferably water, for example if the chemical clean is acidic.
[0031] Depending on the metal or alloy of which the metal housing of the cast metal part is made, chemical cleaning can be:
[0032] Pickling, which is carried out, for example, by immersing the cast metal part in a bath containing a mineral acid or a mixture of mineral acids of the hydrochloric, sulphuric, hydrofluoric, nitric, phosphoric acid type or the like, or by spraying such a bath on the metal part; or
[0033] Alkali washing, for example by immersing the cast metal parts in a bath containing an alkali of the soda or potash type, or by spraying such a bath onto the metal parts; or even
[0034] Pickling, which combines two consecutive treatments of the cast metal parts, one with a bath containing a mineral acid or a mixture of mineral acids and the other with a bath containing an alkali.
[0035] In all cases, washing can be done while hot.
[0036] According to the present invention, the chemical cleaning is preferably acid cleaning.
[0037] More specifically, such cleaning advantageously comprises immersing the cast metal part in a bath comprising hydrochloric acid.
[0038] According to the invention, the cast metal component is preferably a turbine blade for a turbomachine, and even more preferably a turbine blade for an aircraft turbojet.
[0039] The present invention also relates to a method for manufacturing a metal component by investment casting, comprising:
[0040] Providing a cast metal component, the cast metal component comprising a metal shell defining an interior space and an exterior space, at least one porous ceramic core being contained in the interior space and in fluid communication with the exterior space; and
[0041] The cast metal parts are chemically cleaned by carrying out the chemical cleaning method as previously described.
[0042] According to the invention, the metal component is preferably a turbine blade for a turbomachine and even more preferably a turbine blade for an aircraft turbojet engine.
[0043] Other advantages and characteristics of the invention will become more apparent on reading the following additional non-limiting description made with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 A perspective view of one example of a turbine blade for a turbine machine, likely manufactured by investment casting, is shown.
[0045] Figure 2 shows the production by investment casting Figure 1 A top view of a turbine blade after a shell mold used in manufacturing the turbine blade is sanded out but before a porous ceramic core used in its manufacturing is sanded out.
[0046] Figure 3 Shows Figure 2 The mass of water absorbed by the porous ceramic core of a turbine blade of the type shown (denoted by M in mg) varies with the immersion time of the blade in water (denoted by t in seconds). DETAILED DESCRIPTION
[0047] First reference Figure 1 , Figure 1 An example of a turbine blade 10 for a turbine is shown, which may be manufactured by an investment casting method.
[0048] The blade comprises a metal structure 20 consisting of three elements, namely:
[0049] a root portion 11, through which connection is made to a turbine disk (not shown);
[0050] an airfoil 12 delimited by a shell 13 twisted about an axis EV called the “span axis” forming a lower surface 14 and an upper surface 15 connected to a leading edge 16 and a trailing edge 17 ; and
[0051] An intermediate zone 18 , called the platform zone, extends substantially perpendicularly to the axis EV and connects the root 11 to the airfoil 12 .
[0052] The metal structure 20 is a one-piece component which includes an inner cavity for cooling the blade in operation by passing fresh air through the blade. The inner cavity is formed, for example, from a mouth formed at the bottom of the root (thus at Figure 1 The blades are not visible in the figure, but extend to holes 19, called "dust holes", included in the wall 11 at the top of the blade. This wall forms the bottom of an open cavity commonly called a "bathtub".
[0053] If the blade is manufactured by investment casting, the negative and the inner cavity of the blade are obtained, for example, by using a ceramic core in the form of two parts: a first part forms the negative of the bathtub, and a second part forms the negative of the blade cavity, these two parts are connected by a ceramic bridge forming the negative of the hole 19, while the metal structure 20 of the blade is obtained by casting molten metal or metal alloy between the ceramic core and this mold, which is a refractory material (usually ceramic), after dewaxing and sintering the shell mold.
[0054] After the metal or alloy solidifies, the shell mold is sanded off.
[0055] Therefore, we obtain Figure 2 The blade is shown in a top view at the airfoil 12 .
[0056] As can be seen in this figure, the outer surface of the metal structure 20 of the blade 10 is exposed due to the destruction or demoulding of the shell mold, but the part of the ceramic core forming the recess of the bathtub (reference 21) still exists.
[0057] If the outer surface of the metal structure 20 of the blade is chemically cleaned by immersing the blade in a highly concentrated acid bath, the first and second portions of the ceramic core will be saturated with the acid by capillary action, since the core has a porous structure, and the acid will be retained as long as the ceramic core itself is not sanded.
[0058] As a result, after sanding the ceramic core, a lack of material may be observed at the inner surface of the metal structure 20 , in particular the inner surface of the wall 22 .
[0059] Therefore, in order to prevent this incomplete mould filling from occurring, the invention proposes to fill the pores of the ceramic core with a liquid, for example by soaking the blade in this liquid, preferably until these pores are saturated with the liquid, followed by chemical cleaning.
[0060] The liquid is preferably water.
[0061] like Figure 3 As shown, it is shown Figure 2 The mass of water absorbed by the porous ceramic core of the blade shown (represented by M, in mg) varies with the immersion time of the blade in water (represented by t, in seconds). 5 minutes of immersion time is sufficient to make the ceramic core horizontally saturated with water.
Claims
1. A method for chemically cleaning a cast metal component, the cast metal component comprising a metal shell defining an inner space and an outer space, wherein at least one porous ceramic core is contained in the inner space and the ceramic core is in fluid communication with the outer space, the method comprising: filling the pores of the ceramic core with a liquid; Then The cast metal component is chemically cleaned by immersing the cast metal component in a chemical cleaning bath; and the method further includes, before immersing the cast metal component in the chemical cleaning bath, filling the pores of the ceramic core with a liquid to prevent or limit the chemical cleaning bath from penetrating into the pores of the ceramic core.
2. The method according to claim 1, wherein: Filling the pores with a liquid includes immersing the cast metal component in the liquid.
3. The method according to claim 1, wherein: The pores are filled with a mass of liquid that is at least 90% of the mass of liquid that the pores would contain if they were saturated with liquid.
4. The method according to claim 3, wherein: The pores are filled with a mass of liquid that is at least 95% of the mass of liquid that the pores would contain if they were saturated with liquid.
5. The method according to claim 3, wherein: The pores are filled with a mass of liquid that is 100% of the mass of liquid that the pores would contain if they were saturated with liquid.
6. The method according to claim 1, wherein: The liquid is an aqueous solution.
7. The method according to claim 6, wherein: The liquid is water.
8. The method according to claim 1, wherein: The chemical cleaning bath is an acid cleaning bath.
9. The method according to claim 8, wherein: The pickling bath comprises hydrochloric acid.
10. The method according to any one of claims 1 to 9, wherein: The cast metal component is a turbine blade for a turbine.
11. The method according to claim 10, wherein: The turbine blade is used in an aircraft turbojet engine.
12. A method of manufacturing a metal part by investment casting, comprising: Providing a cast metal component, the cast metal component comprising a metal shell defining an interior space and an exterior space, at least one porous ceramic core being accommodated in the interior space and in fluid communication with the exterior space; as well as The cast metal component is chemically cleaned by carrying out the method according to claim 1 .
13. The method of claim 12, wherein: The metal component is a turbine blade for a turbine.
14. The method according to claim 13, wherein: The turbine blade is used in an aircraft turbojet engine.