EUV-level substrate, EUV mask blank, EUV mask and method for manufacturing the same

By forming a coating layer with a negative thermal expansion coefficient on the EUV mask substrate and a spin-coated carbon layer, the thermal expansion and surface defect problems of EUV mask substrate are solved, and the manufacturing of low-cost and high-performance EUV mask substrate and mask substrate is achieved, which improves lithography accuracy and reduces manufacturing costs.

CN115327851BActive Publication Date: 2025-07-18SHANGHAI CHUANXIN SEMICON CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211077807.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-05
Publication Date
2025-07-18
Estimated Expiration
2042-09-05

AI Technical Summary

Technical Problem

The existing EUV mask plates are susceptible to thermal expansion during the manufacturing process, resulting in a decrease in photolithography accuracy and difficult to effectively control the defects on the substrate surface, affecting the lithography effect.

Method used

A coating layer with a negative thermal expansion coefficient is formed on the substrate surface, and a spin-coated carbon layer is formed by spin-coated carbon material, and the thickness of the coating layer is adjusted to compensate for the difference in elastic modulus, so as to achieve a thermal expansion coefficient close to 0, repair surface defects, and form a low-cost, high-flatness EUV-level substrate and mask substrate.

Benefits of technology

The thermal expansion and surface defects of the EUV mask plate are reduced, the lithography effect is improved, and the manufacturing cost is reduced through the removability of the spin-coated carbon layer, achieving high-performance EUV mask substrate and mask plate recycling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115327851B_ABST
    Figure CN115327851B_ABST
Patent Text Reader

Abstract

The present invention provides an EUV-level substrate, an EUV mask blank, an EUV mask, and a manufacturing method thereof. A coating layer is covered on a substrate, and the thickness of the coating layer is adjusted to compensate for differences in physical parameters such as elastic modulus. Further, a spin-on carbon layer (SOC) is covered on the surface of the coating layer, so that the coefficient of thermal expansion of the surface of the EUV-level substrate is close to 0, and thus an EUV-level substrate, an EUV mask blank, and an EUV mask with low cost, high performance, and low defects can be obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of integrated circuit manufacturing technology, and particularly relates to an EUV-level substrate, an EUV mask blank, an EUV mask, and a manufacturing method thereof, and a substrate. Background Art

[0002] With the continuous development of the integrated circuit manufacturing industry, advanced lithography technologies such as extreme ultraviolet lithography (EUVL) have been widely used. Among them, an EUV mask is an important component in the lithography process. In the lithography process, usually, a photoresist layer such as a photoresist is coated on the surface of a wafer. After the photoresist layer is dried, the pattern on the EUV mask is exposed on the photoresist layer by an exposure device with a specific light source (such as extreme ultraviolet light EUV). Subsequently, the exposed photoresist layer is developed with a developer, and the pattern of the developed photoresist layer is used as a mask to perform processes such as etching on the wafer, and finally, the pattern on the EUV mask is transferred to the wafer.

[0003] Since EUV lithography uses a reflective optical system, the accuracy of EUV lithography will be affected by the slight thermal expansion of the EUV mask. Therefore, it is crucial to manufacture an EUV-level substrate, an EUV mask blank, and an EUV mask with low thermal expansion and high flatness. Summary of the Invention

[0004] The purpose of the present invention is to provide an EUV-level substrate, an EUV mask blank, an EUV mask, and a manufacturing method thereof, which can help reduce the defects of the EUV mask and thus improve the effect of EUV lithography.

[0005] To achieve the above purpose, the present invention provides a manufacturing method of an EUV-level substrate, which includes:

[0006] Providing a substrate, and forming a coating layer with a negative thermal expansion coefficient on the surface of the substrate, wherein the material of the coating layer includes a polyimide with an amide structure in the main chain;

[0007] Spin-coating a carbon material on the top surface of the coating layer to form a spin-coated carbon layer with a flat top surface, thereby forming an EUV-level substrate;

[0008] Wherein, during the process of forming the coating layer or after forming the coating layer, the thickness of the coating layer is adjusted to a corresponding thickness to compensate for the difference in the elastic modulus between the coating layer and the substrate, so that the thermal expansion coefficient of the top surface of the coating layer is lower than 10 -7 / °K.

[0009] Optionally, the step of forming a coating layer on the surface of the substrate includes:

[0010] Step a, immersing the substrate into a corresponding organic polymer material solution;

[0011] Step b, placing the substrate with the organic polymer material solution attached to its surface in an oven, and performing curing and / or thermal chemical reaction by using a stepped temperature program to form a coating layer;

[0012] Step c, repeatedly performing Step a and Step b until the formed coating layer reaches a corresponding thickness.

[0013] Optionally, the step of forming a coating layer on the surface of the substrate includes: coating an organic polymer material solution on the top surface of the substrate, and performing baking and curing to form a coating layer with a corresponding thickness.

[0014] Optionally, after forming the coating layer, the thickness of the coating layer is adjusted by thinning the top surface of the coating layer.

[0015] Based on the same inventive concept, the present invention further provides a method for manufacturing an EUV mask blank, which includes:

[0016] Adopting the method for manufacturing an EUV-level substrate as described in the present invention to form an EUV-level substrate;

[0017] Successively forming a reflective film stack layer and an absorption layer on the spin-coated carbon layer of the EUV-level substrate to form an EUV mask blank.

[0018] Optionally, after forming the reflective film stack layer on the spin-coated carbon layer and before forming the absorption layer, it further includes: forming a covering layer on the reflective film stack layer; and,

[0019] After forming the absorption layer, it further includes: forming a back conductive layer on the surface of the substrate facing away from the spin-coated carbon layer.

[0020] Based on the same inventive concept, the present invention further provides a method for manufacturing an EUV mask, which includes:

[0021] Adopting the method for manufacturing an EUV mask blank as described in the present invention to form an EUV mask blank;

[0022] Etching the absorption layer of the EUV mask blank to form a first pattern in the absorption layer;

[0023] Etching the absorption layer and the reflective film stack layer of the EUV mask blank outside the periphery of the first pattern, and stopping the etching on the surface of the spin-coated carbon layer of the EUV mask blank to form a second pattern.

[0024] Based on the same inventive concept, the present invention further provides an EUV-level substrate, which includes:

[0025] a substrate;

[0026] a coating layer with a negative thermal expansion coefficient, at least formed on the surface of the substrate, and the material of the coating layer includes a polyimide with an amide structure in the main chain;

[0027] a removable spin-on carbon layer, formed on the top surface of the coating layer;

[0028] wherein, the coating layer is adjusted to a corresponding thickness to compensate for the difference in elastic modulus between the coating layer and the substrate, so that the thermal expansion coefficient of the top surface of the coating layer is lower than 10 -7 / °K.

[0029] Based on the same inventive concept, the present invention further provides an EUV mask blank, which includes:

[0030] the EUV-level substrate as described in the present invention;

[0031] a reflective film stack layer, formed on the spin-on carbon layer of the EUV-level substrate;

[0032] an absorption layer, formed on the reflective film stack layer.

[0033] Optionally, the EUV mask blank further includes:

[0034] a cover layer, formed between the top reflective film of the reflective film stack layer and the absorption layer; and, a back conductive layer, formed on the surface of the EUV-level substrate facing away from the reflective film stack layer.

[0035] Based on the same inventive concept, the present invention further provides an EUV mask. The EUV mask has the EUV mask blank as described in the present invention, and the EUV mask further has a first pattern and a second pattern. The first pattern is formed in the absorption layer of the EUV mask blank, and the second pattern penetrates through the absorption layer and the reflective film stack layer of the EUV mask blank and exposes the surface of the spin-on carbon layer of the EUV mask blank.

[0036] Compared with the prior art, the technical solution of the present invention has at least one of the following beneficial effects:

[0037] 1. By forming a coating layer comprising a polyimide material with an amide structure in the main chain on a substrate such as quartz glass at DUV level or lower, and adjusting the thickness of the coating layer to a corresponding thickness during or after the formation of the coating layer to compensate for the difference in elastic modulus between the coating layer and the substrate, so that the coefficient of thermal expansion (CTE) of the working surface of the coating layer is lower than 10 -7 / °K (i.e., close to 0), the surface of the EUV substrate with a CTE close to zero is achieved.

[0038] 2. Further spin-coat a carbon material on the coating layer to repair the surface defects of the coating layer and provide a flat and smooth process surface for subsequent processes (with a planarization degree reaching a surface defect size lower than 10 nm), which is beneficial to the formation of an EUV-level substrate, an EUV mask blank, and an EUV mask with low thermal expansion, high flatness, and low defects, thereby improving the EUV lithography effect.

[0039] 3. The spin-coated carbon layer can serve as a regenerative "sacrificial layer" and can be easily removed by oxygen plasma ashing. The EUV-level substrate can be recycled without reducing the surface quality of the EUV-level substrate for the manufacture of new EUV masks, further reducing the manufacturing cost of new EUV masks. Among them, the spin-coated carbon layer is commercially available from companies such as Brewer Science in the United States. Description of the Drawings

[0040] Figure 1 is a schematic cross-sectional structure diagram of an existing EUV mask.

[0041] Figures 2 to 4 is a schematic structure diagram of five typical defects in an existing EUV mask or EUV mask blank.

[0042] Figure 5 is a schematic flow diagram of the manufacturing method of the EUV-level substrate in a specific embodiment of the present invention.

[0043] Figure 6 is a schematic cross-sectional structure diagram in the manufacturing method of the EUV-level substrate in a specific embodiment of the present invention.

[0044] Figures 7 to 8 is a schematic diagram of the filling ability and surface planarization degree of the spin-coated carbon layer.

[0045] Figure 9 is a schematic cross-sectional structure diagram in the manufacturing method of the EUV mask blank in an embodiment of the present invention.

[0046] Figure 10It is a schematic flowchart of a method for manufacturing an EUV mask according to a specific embodiment of the present invention.

[0047] Figure 11 It is a schematic cross-sectional structure diagram in a method for manufacturing an EUV mask according to a specific embodiment of the present invention.

[0048] Figure 12 It is a schematic cross-sectional structure diagram in a substrate recycling method according to a specific embodiment of the present invention. Specific Embodiments

[0049] In the following description, numerous specific details are given to provide a more thorough understanding of the present invention. However, it is obvious to those skilled in the art that the present invention can be implemented without one or more of these details. In other instances, some well-known technical features are not described to avoid confusion with the present invention. It should be understood that the present invention can be implemented in different forms and should not be construed as limited to the embodiments presented herein. On the contrary, these embodiments are provided to make the disclosure thorough and complete, and to fully convey the scope of the present invention to those skilled in the art. In the drawings, for clarity, the dimensions and relative dimensions of layers and regions may be exaggerated. The same reference numerals denote the same elements throughout the drawings.

[0050] It should be understood that when an element or layer is referred to as "on" another element or layer, it can be directly on, adjacent to, connected to, or coupled to the other element or layer, or there may be intervening elements or layers. In contrast, when an element is referred to as "directly on" another element or layer, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, parts, and / or processes, these elements, components, regions, layers, parts, and / or processes should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, part, and / or process from another element, component, region, layer, part, and / or process. Thus, without departing from the teachings of the present invention, the first element, component, region, layer, part, and / or process discussed below may be referred to as the second element, component, region, layer, part, and / or process.

[0051] Spatial relationship terms such as "under", "below", "lower", "beneath", "above", "upper", "on the top surface", "on the bottom surface", "front", "back", etc. may be used herein for convenience of description to describe the relationship of one element or feature shown in the figure with other elements or features. It should be understood that the spatial relationship terms are intended to include different orientations of the device in use and operation in addition to the orientation shown in the figure. For example, if the device in the drawing is flipped, then the element or feature described as "under other elements" or "beneath it" or "under it" or "on the bottom surface" or "on its back surface" will be oriented "above" or "on the top" or "front" of other elements or features. Thus, the exemplary terms "under", "beneath" and "on the back" can include both the upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or other orientations) and the spatial descriptors used herein are to be interpreted accordingly.

[0052] The purpose of the terms used herein is only to describe specific embodiments and is not a limitation of the present invention. As used herein, the singular forms "a", "an" and "the" are also intended to include the plural forms unless the context clearly dictates otherwise. It should also be understood that the terms "comprising" and / or "including", when used in this specification, specify the presence of the stated features, integers, steps, operations, elements and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups. As used herein, the term "and / or" includes any and all combinations of the related listed items.

[0053] As described in the background art, it is crucial to manufacture EUV masks with low cost, low defects and high performance.

[0054] The EUV mask is a key component for an EUV lithography (EUVL) system. EUV lithography employs a scanner that uses light in the extreme ultraviolet (EUV) region (i.e., the exposure light), the wavelength of which is from about 1 nm to about 100 nm, for example 13.6 nm. Since optical materials are opaque to EUV radiation, the EUV mask is a reflective mask. The blank of the EUV mask generally has a substrate (such as glass or quartz, etc.), a reflective film stack layer (for example, alternately stacked by molybdenum Mo and silicon Si, also known as a reflective structure), and an absorption layer (which can be a single-layer film or a multi-layer film) stacked in sequence. The reflective film stack layer is used to reflect the exposure light, and the absorption layer is used to absorb the exposure light and will be etched into a specified pattern (i.e., a circuit pattern) required for integrated circuit manufacturing. The absorption layer has a low EUV reflectivity, for example less than 3-5%.

[0055] Among them, please refer to Figures 1 to 4, A conventional EUV mask blank (also known as an EUV mask substrate, a blank EUV mask) generally includes a substrate 100, a reflective film stack layer 101, a capping layer 102, and an absorber layer 103. A conventional EUV mask is formed with a first pattern 103a and a second pattern 104 in the EUV mask blank.

[0056] The inventors' research found that EUV lithography technology is very sensitive to defects in EUV mask blanks and EUV masks. One of the sources of its defects is the defects induced by surface defects of the substrate 100 (such as pits, slits, grooves, bumps, contamination particles, or scratches, etc.). Specifically, it includes: a) The first type of defect 101a caused by pits (or slits, scratches) defects 100a with a relatively large size (>10 nm) already existing on the surface of the substrate 100, as Figure 2 shown. These pit defects 100a on the substrate 100 are formed on the surface of the substrate 100 by processes such as chemical mechanical polishing (CMP) and cleaning, and will induce into each layer of the reflective film stack layer 101 deposited upward from the substrate 100, thereby forming the first type of defect 101a; b) The second type of defect 101b caused by bumps defects or contamination particles, etc. with a relatively large size (>10 nm) already existing on the surface of the substrate 100, as Figure 3 shown. These bump defects 101b or contamination particles, etc. on the substrate 100 are formed on the surface of the substrate 100 by processes such as chemical mechanical polishing (CMP) and cleaning, and will induce into each layer of the reflective film stack layer 101 deposited upward from the substrate, and may cause the defect size to increase due to factors such as stress and thickness change during the upward induction process, thereby forming the second type of defect 101b; c) The third type of defect 101c caused by defects 100c (being pits, slits, bumps, contamination particles, or scratches, etc.) with a relatively large size (>10 nm) already existing on the surface of the substrate 100, as Figure 4 shown. The defects 100c on the substrate 100 induce into each layer of the reflective film stack layer 101 deposited upward from the substrate 100, and may cause a lateral position shift due to factors such as stress and thickness change during the upward induction process, thereby forming the third type of defect 101c.

[0057] All the above-mentioned defects on the substrate surface will cause defects in the EUV mask, which will in turn affect the final effect of EUV lithography using this EUV mask.

[0058] In the prior art, in order to reduce the defects introduced by the substrate 100, fused quartz with a relatively flat and smooth surface is generally selected. With the development of technology, in order to solve the problem that the thermal expansion of the substrate 100 in subsequent processes will further introduce defects, it is further proposed to use silicon, glass-ceramics (Zerodur), ultra-low expansion fused quartz (ULE, also known as zero-expansion glass), etc. to replace fused quartz as the substrate 100.

[0059] However, no matter what material the substrate 100 in the prior art is made of, its synthesis difficulty and processing cost are very high, and the defects caused by processes such as chemical mechanical polishing (CMP) and cleaning of the substrate on its surface will affect the performance of the EUV mask blank.

[0060] Based on this, the present invention provides an EUV-level substrate, an EUV mask blank, an EUV mask blank and a manufacturing method thereof, which can provide an EUV-level substrate with a process surface having a thermal expansion coefficient close to 0, and further can manufacture an EUV-level substrate, an EUV mask blank and an EUV mask blank with low cost, low thermal expansion and high flatness.

[0061] The following combines Figures 5 to 12 with specific embodiments to detail the technical solution of the present invention.

[0062] Please refer to Figure 5 , an embodiment of the present invention provides a manufacturing method of an EUV-level substrate, which includes:

[0063] S11, providing a substrate, forming a coating layer with a negative thermal expansion coefficient on the surface of the substrate, the material of the coating layer includes polyimide with an amide structure in the main chain, and during or after forming the coating layer, adjusting the thickness of the coating layer to a corresponding thickness to compensate for the difference in elastic modulus between the coating layer and the substrate, so that the thermal expansion coefficient of the working surface of the coating layer is lower than 10 -7 / °K;

[0064] S12, spin-coating a carbon material on the top surface of the coating layer to form a spin-coated carbon layer with a flat top surface, and further forming an EUV-level substrate.

[0065] Please refer to Figure 6 , in step S11, first, the provided substrate 200a can be a DUV-level or lower-grade fused quartz substrate, and its material is synthetic fused quartz material, which has a low positive thermal expansion coefficient, and the specific thermal expansion coefficient is, for example, less than or equal to 10 -6 / °K. Among them, the DUV-grade fused silica substrate is the standard substrate for the blank mask substrate of 193nm, 248nm or 365nm DUV lithography, which can have a high transmittance in the DUV range (for example, the transmittance is greater than 80%). Then, the substrate 200a can be cleaned and the following steps can be carried out: Step a, immerse the substrate into the corresponding organic polymer material solution; Step b, place the substrate with the organic polymer material solution attached to its surface in an oven, and use a stepwise temperature increase program for curing and / or thermal chemical reaction to form a coating layer; Step c, repeat Steps a and b until the formed coating layer reaches the corresponding thickness.

[0066] The material of the coating layer 200b includes polyimide with an amide structure in the main chain (i.e., polyamide-polyimide film). The introduction of this amide structure can form strong hydrogen bond interactions between the linear rigidity of the molecular main chain in the coating layer 200b and the amide structures, which is beneficial to the regular arrangement and close packing of the molecular main chain in the coating layer 200b, thereby significantly improving the tensile strength (for example, 244.6 - 280.5 MPa) and elastic modulus (for example, 9.3 GPa - 11.6 GPa) of the coating layer 200b.

[0067] Further optionally, the main chain of the coating layer 200b also has at least one substituent group such as —H, —F, —CH3, etc., to adjust the tensile strength and elastic modulus of the polyimide film with the introduced amide structure, and further adjust the thermal expansion coefficient of the polyimide film with the introduced amide structure to make it as close to 0 as possible.

[0068] As an example, the following steps are carried out on the entire surface of the substrate 200a (including the upper surface, lower surface and peripheral side wall surfaces):

[0069] Step a, immerse the substrate into the corresponding polyamide solution;

[0070] Step b, place the substrate with the polyamide solution attached to its surface in an oven, and use a stepwise temperature increase program for thermal imidization to form a polyimide layer with an amide structure in the main chain, that is, a polyamide-polyimide film;

[0071] Step c, repeat Steps a and b until the formed polyamide-polyimide film reaches the corresponding thickness, thereby forming the required coating layer 200b.

[0072] Furthermore, the number of times of repeatedly performing steps a and b in step c can be controlled, thereby adjusting the thickness of the formed polyamide-polyimide film (i.e., the coating layer 200b), until the thickness of the stacked polyamide-polyimide film (i.e., the coating layer 200b) can compensate for the differences in physical parameters such as the elastic modulus of the substrate 200a and the formed polyamide-polyimide film (i.e., the coating layer 200b), so that the coefficient of thermal expansion of the surface of the polyamide-polyimide film (i.e., the coating layer 200b) is less than 10 -7 / °K (i.e., close to 0). When the mask is in the working state, mainly the working surface of the quartz glass is heated and expands. In this solution, the coating layer 200b wraps the substrate 200a on all sides, which can effectively disperse the stress on the working surface and can play a better role in controlling expansion and reducing surface warping.

[0073] As another example, the step of forming the coating layer 200b on the upper surface of the substrate includes: coating a solution of an organic polymer material on the upper surface (i.e., the top surface, the working surface) of the substrate, and baking and curing it at different temperatures in a vacuum or in an atmosphere of nitrogen or an inert gas according to a stepwise heating method, and then cooling to room temperature to form a coating layer 200b with a corresponding thickness. Optionally, after forming the coating layer 200b, the thickness of the coating layer 200b is adjusted by thinning the top surface (i.e., the working surface) of the coating layer 200b.

[0074] Optionally, after forming the coating layer 200b, the thickness of the coating layer 200b can be adjusted by a polishing process to thin the working surface of the coating layer 200b until it can compensate for physical parameters such as the elastic modulus, so that the coefficient of thermal expansion of the surface of the coating layer 200b is less than 10 -7 / °K (i.e., close to 0).

[0075] Among them, the covering thickness of the formed coating layer 200b can be reasonably set as needed, for example, 20 nm to 100 nm.

[0076] Please refer to Figure 6 , in step S12, a carbon material is spin-coated on the upper surface (i.e., the working surface, the top surface) of the coating layer 200b by a spin-coating process to form a spin-coated carbon layer 201. The spin-coated carbon layer 201 has a flat and smooth top surface, which is used as a repair layer for defects (such as pits, cavities, bumps, etc.) to meet the planarization requirements of EUV applications. Moreover, it can also be easily removed by plasma O2 ashing and can be used as a sacrificial layer in the substrate regeneration process. The top surface of the spin-coated carbon layer 201 can achieve a planarization degree with a surface defect size lower than 10 nm.

[0077] The specific process of forming the spin-coated carbon layer 201 includes: first, wet-cleaning the surface of the coating layer 200b; then, spin-coating a carbon material on the surface of the coating layer 200b to the required thickness by a spin-coating process; next, soft-baking the spin-coated carbon material at a first temperature (such as 100 °C to 200 °C, for example, 170 °C); thereafter, hard-baking the spin-coated carbon material at a second temperature (such as 250 °C to 500 °C), and the second temperature is higher than the first temperature, thereby forming the spin-coated carbon layer 201. Among them, the carbon material spin-coated on the surface of the coating layer 200b is heated at the first temperature and triggers a cross-linking reaction to partially cross-link the carbon backbone polymer therein, and maintains a certain degree of backflow of the spin-coated carbon material, which is beneficial to forming a flatter surface. Further, the spin-coated carbon material is heated at the second temperature and undergoes a more intense cross-linking reaction to further cross-link the carbon backbone polymer therein, and the backflow of the spin-coated carbon material decreases, and finally the solid spin-coated carbon layer 201 is formed.

[0078] As an example, the spin-coated carbon material (which has been commercialized by companies including Brewer Science, Inc. in the United States) is a liquid spin-coated carbon composite, which includes a solvent, a carbon backbone polymer, and a cross-linking agent. The carbon backbone polymer includes, for example, at least one of propylene glycol methyl ether PGME, propylene glycol methyl ether acetate PGMEA, cyclopentanone, cyclohexanone, polyhydroxystyrene, polyacrylate, or polymethyl methacrylate, etc. The cross-linking agent includes at least one of the group of A-(OR) x , A-(NR) x , A-(OH) x , A-(C=C) x and A-(C≡C) x , A is a single molecule, a polymer, or a second polymer with a molecular weight ranging from 100 to 20000, R is a hydrocarbon group, a cycloalkyl group, a cycloalkyl epoxy group, or a C3-C 15 heterocyclic group; OR is an alkoxy group, a cycloalkoxy group, a carbonate group, an alkyl carbonate group, an alkyl carboxylate group, a toluenesulfonate group, or a methanesulfonate group; NR is an alkyl amide group or an alkyl amino group; x ranges from 2 to 1000 or C3-C 15Heterocyclic group; OR is alkoxy, cycloalkoxy, carbonate group, alkyl carbonate group, alkyl carboxylate group, tosylate group or mesylate group, NR is alkyl amide group or alkyl amino group, and the range of x is from 2 to 1000. The carbon backbone polymer and the crosslinking agent are uniformly dissolved in a solvent and spin-coated onto the surface of the organic polymer substrate 200. In some embodiments, the solvent is an organic solvent, such as including at least one of ketones, alcohols, polyols, ethers, ethylene glycol ethers, cyclic ethers, aromatic hydrocarbons, esters, propionates, lactates, lactates, alkylene glycol monoalkyl ethers, alkyl lactates, alkyl alkoxy propionates, cyclic lactones, monoketone compounds containing a ring, alkylene carbonates, alkyl alkoxyacetates, alkyl pyruvates, lactates, ethylene glycol alkyl ether acetates, diethylene glycol, propylene glycol alkyl ether acetates, alkylene glycol alkyl ether esters, alkylene glycol monoalkyl esters, and the like.

[0079] The spin-coated carbon layer 201 formed therein, on the one hand, is thick enough to fill and bury the defects on the top surface of the coating layer 200b, thereby improving a sufficiently flat and smooth top surface and avoiding defects induced by these defects in the subsequent deposited reflective film stack layer 202 and absorption layer 204; on the other hand, it is thin enough and opaque, while "resetting" the surface of the coating layer 200b to a new substrate that is flatter and has fewer defects, making the coefficient of thermal expansion of the EUV-level substrate surface close to 0. Thus, it is beneficial to manufacture EUV mask blanks and EUV masks with lower cost, fewer defects, and higher performance.

[0080] As an example, in step S12, a liquid carbon material is spin-coated onto the surface of the coating layer 200b at a speed of 1500 pm / 60 s until the thickness of the spin-coated carbon material meets the requirements; then, in an N2 atmosphere, the spin-coated carbon material is soft-baked at 100°C to 200°C for 1 min to 5 min; thereafter, in an N2 atmosphere, the spin-coated carbon material is hard-baked at 200°C to 400°C for 5 min to 20 min, and finally a solid spin-coated carbon layer 201 with a thickness not greater than 20 nm (for example, 10 nm or less than 10 nm) is formed, thereby obtaining an EUV-level substrate.

[0081] In step S12, the spin-coated carbon layer 201 is formed by a spin-coating method. The process is simple and low-cost, and compared with carbon layers formed by other methods such as CVD, ALD, or sputtering, it has stronger deep gap filling ability and local and global planarization ability, and it can form a globally flat process surface on the coating layer 200b (the top surface of which can be planarized to a scale of less than 10 nm). For example, the line widths of the gaps on the coating layer 200b are different (such as Figure 7 where some intervals L1 are very large and some intervals L2 are very small), and the intervals of the gaps are also of different sizes (such as Figure 7Among them, the line width W1 of the interval of some gaps is very large, and the line width W2 of the interval of some gaps is very small. By using the spin-coating method to form a spin-coated carbon layer, the gaps can also be filled and their intervals can be buried, and a globally flat process surface can be formed. For another example, the gaps on the top surface of the coating layer 200b are narrow slits with a high aspect ratio. As Figure 8 shown, after using the spin-coating method to form a spin-coated carbon layer, taking advantage of the small size of carbon atoms, it can be filled to the bottom of the gap, and after filling the gap, a globally flat process surface is formed.

[0082] On the premise of forming a carbon layer with the same thickness by using the spin-coating method, for the carbon layer formed by other methods such as CVD, ALD or sputtering, in the Figure 7 defect situation shown, due to the sparse and dense effects of the defects, problems such as pits or protrusions will occur, and the flatness of the top surface of the finally formed carbon layer is insufficient; in the Figure 8 defect situation shown, problems such as filling voids will occur due to failure to fill to the bottom of the slit or premature sealing of the slit, or problems such as pits or protrusions will occur on the top surface due to conformal deposition, and the flatness of the top surface of the finally formed carbon layer is insufficient. That is to say, forming a carbon layer on the substrate by other methods such as CVD, ALD or sputtering cannot meet the requirements of the higher-performance EUV mask blank or EUV mask for the flatness of the substrate top surface, and cannot achieve the technical effects of the present invention.

[0083] Please refer to Figure 6 , this embodiment also provides an EUV-level substrate for an EUV mask blank or an EUV mask, which can be formed by using the manufacturing method of the EUV-level substrate of this embodiment, and includes a substrate 200a, a coating layer 200b with a negative thermal expansion coefficient, and a removable spin-coated carbon layer 201 stacked in sequence.

[0084] Optionally, the material of the coating layer 200b includes polyimide with an amide structure in the main chain.

[0085] The thickness of the spin-coated carbon layer 201 is less than or equal to 20 nm, for example, 10 nm. This spin-coated carbon layer 201 can bury the surface defects of the coating layer 200b and provide a flat process surface. The thickness of the coating layer 200b is adjusted to an appropriate size to compensate for the elastic modulus, so that the thermal expansion coefficient of the EUV-level substrate surface is close to 0.

[0086] Optionally, the thickness of the coating layer 200b is 20 nm to 100 nm.

[0087] The coating layer 200b can only cover the working surface (i.e., the upper surface) of the substrate 200a, or can cover the entire substrate 200a (i.e., cover the upper surface, lower surface and side wall surface of the substrate 200a).

[0088] In addition, the spin-coated carbon layer 201 can be used as a removable sacrificial layer, which can be removed by an oxygen plasma ashing process when rework, recycling, and reuse of the EUV-level substrate are required.

[0089] For the EUV-level substrate and its manufacturing method of this embodiment, by combining the substrate 200a with a low positive thermal expansion coefficient and the coating layer 200b with a low negative thermal expansion coefficient, and by adjusting the thickness of the coating layer 200b (compensating for the differences in physical parameters such as the elastic modulus of the two), finally, the CTE of the coating layer 200b at the working temperature of the EUV mask blank is close to zero. Further, spin-coated carbon is formed on the surface of the relatively rough coating layer 200b for defect repair, so as to provide an EUV-level substrate with low cost, low thermal expansion, and low defects.

[0090] Please refer to Figure 9 , this embodiment also provides a manufacturing method of an EUV mask blank, which includes:

[0091] First, use the manufacturing method of the EUV-level substrate as described in the present invention to form an EUV-level substrate, which includes a substrate 200a, a coating layer 200b with a negative thermal expansion coefficient, and a spin-coated carbon layer 201.

[0092] Then, form a reflective film stack layer 202 on the spin-coated carbon layer 201 of the EUV-level substrate. Please refer to Figure 9, it is usually required that the reflective film stack layer 202 has a high reflectivity to the exposure light of a specific wavelength. For example, the reflectivity to extreme ultraviolet light of 13.6 nm is higher than 60%, and preferably higher than 65%. In this embodiment, the reflective film stack layer 202 is mainly formed by alternately laminating a first reflective film (not shown) and a second reflective film (not shown) in pairs, with a total of 40 to 50 pairs of laminations. The film thicknesses of the first reflective film and the second reflective film are each about 3 nm to 4 nm. The film thicknesses of the first reflective film and the second reflective film are any suitable materials that can achieve a high reflectivity (such as higher than 70%) for extreme ultraviolet light of a specific wavelength (such as 13.6 nm). For example, the material of the first reflective film is silicon (Si), and the material of the second reflective film is molybdenum (Mo). Another example is that the material of the first reflective film is Mo, and the material of the second reflective film is beryllium (Be). Specifically, the first reflective film and the second reflective film can be alternately formed by any suitable deposition process such as sputtering (PVD), chemical vapor deposition (Chemical Vapor Deposition, CVD), plasma-enhanced CVD (Plasma Enhanced Chemical Vapor Deposition, PECVD), atomic layer deposition (Atomic Layer Deposition, ALD), plasma-enhanced ALD (PEALD), IBD (Ion Beam Deposition, ion beam deposition), JVD (Jet Vapor Deposition, jet vapor deposition), etc., so as to form the required reflective film stack layer 202. Among them, in order to minimize the thermally induced defects during the formation of the reflective film stack layer 202, the deposition temperature of each film layer in the reflective film stack layer 202 is as close to room temperature as possible, for example, controlled to be between room temperature and 100 °C.

[0093] Next, a cover layer 203 is formed on the surface of the reflective film stack layer 202. Specifically, the cover layer 203 is formed on the top surface of the reflective film stack layer 202 by any suitable deposition process such as sputtering (PVD), CVD, PECVD, ALD, PEALD, IBD, JVD, etc. The cover layer 203 is used to prevent the reflective film stack layer 202 from being damaged by the etching process. Its material can include at least one of ruthenium (Ru), ruthenium alloy (such as RuB, RuSi or RuNb), or ruthenium oxide (such as RuO2 or RuNbO). It can be a single-layer film structure or a structure formed by laminating multiple layers of films. The thickness of the cover layer 203 is, for example, 2 nm to 4 nm. In other embodiments of the present invention, when the top layer film of the reflective film stack layer 202 is silicon, the manufacture of the cover layer 203 can also be omitted, or in other words, when forming the reflective film stack layer 202, an additional silicon film (i.e., the top first reflective film) is deposited as the cover layer 203.

[0094] Thereafter, an absorption layer 204 can be formed on the top surface of the cover layer 203 by any suitable deposition process such as sputtering (PVD), CVD, PECVD, ALD, PEALD, IBD, JVD, etc. The absorption layer 204 can be a single-layer film structure or a composite structure formed by stacking multiple layers of films. The materials thereof include at least one of cobalt (Co), tellurium (Te), hafnium (Hf), nickel (Ni), tantalum (Ta), chromium (Cr), tantalum-based materials, chromium-based materials, etc. The total thickness of the absorption layer 204 is, for example, 50 nm to 75 nm. When the absorption layer 204 is a composite structure formed by stacking multiple layers of films, the thickness of a single layer of film therein is, for example, 3 nm to 6 nm. Among them, in order to minimize the thermally induced defects during the formation of the reflective film stack layer 202 as much as possible, the deposition temperature of each film layer in the absorption layer 204 is as close to room temperature as possible, for example, controlled to be between room temperature and 100 °C.

[0095] Please continue to refer to Figure 9 , optionally, a back conductive layer 206 can be deposited on the surface of the EUV-level substrate facing away from the absorption layer 204 by any suitable deposition process such as sputtering, evaporation, CVD, PECVD, ALD, PEALD, molecular beam epitaxy, IBD, JVD, etc. The materials of the back conductive layer 206 can include at least one conductive material such as chromium, chromium-based materials (such as chromium nitride CrN or chromium oxynitride CrON), tantalum or tantalum-based materials (such as tantalum boride TaB, tantalum oxide TaO, tantalum nitride TaN, tantalum borate TaBO or tantalum boride nitride TaBN, etc.). The thickness of the back conductive layer 206 is, for example, 60 nm to 75 nm.

[0096] So far, the manufacturing of the EUV mask blank is completed.

[0097] It should be understood that in this embodiment, the back conductive layer 206 is formed after the deposition of the absorption layer 204. However, the technical solution of the present invention is not limited thereto. In other embodiments of the present invention, the deposition of the back conductive layer 206 can be performed before the deposition of the reflective film stack layer 202, or can be performed after the deposition of the reflective film stack layer 202 and before the deposition of the cover layer 203, or can also be performed after the deposition of the cover layer 203 and before the deposition of the absorption layer 204.

[0098] The manufacturing method of the EUV mask blank described in this embodiment, since it is formed based on the EUV-level substrate of the present invention, has the advantages of low thermal expansion and few defects, and can be beneficial to improving the EUV lithography effect.

[0099] Please refer to Figure 9, this embodiment also provides an EUV mask blank, which is preferably fabricated by using the manufacturing method of the EUV mask blank of this embodiment. The EUV mask blank includes an EUV-level substrate of the present invention stacked in sequence (i.e., including a substrate 200a, a coating layer 200b, and a spin-on carbon layer 201 stacked in sequence), a reflective film stack layer 202, and an absorption layer 204.

[0100] Optionally, the reflective film stack layer 202 includes first and second reflective films stacked in alternating pairs, and the number of stacked layers of the first and second reflective films is 30 to 60 pairs.

[0101] Optionally, the EUV mask blank further includes a cover layer 203 and a back conductive layer 206. The cover layer 203 is formed between the top reflective film of the reflective film stack layer 202 and the absorption layer 204, and the back conductive layer 206 is formed on the surface of the organic polymer substrate 200 facing away from the spin-on carbon layer 201.

[0102] In addition, the materials selected for the EUV-level substrate, the reflective film stack layer 202, the absorption layer 204, the cover layer 203, and the back conductive layer 206 can refer to the descriptions in the manufacturing method of the EUV mask blank of the present invention above, and will not be elaborated here.

[0103] Based on the same inventive concept, please refer to Figure 10 , this embodiment also provides a manufacturing method of an EUV mask, which includes:

[0104] S21, using the manufacturing method of the EUV mask blank of the present invention to form an EUV mask blank;

[0105] S22, etching the absorption layer of the EUV mask blank to form a first pattern in the absorption layer;

[0106] S23, etching the absorption layer and the reflective film stack layer of the EUV mask blank outside the first pattern, and stopping the etching on the surface of the spin-on carbon layer of the EUV mask blank to form a second pattern.

[0107] Among them, the process of step S21 is the manufacturing method of the EUV mask blank of the present invention described above, and will not be elaborated here.

[0108] In step S22, first, please refer to Figure 11, a hard mask layer 205 is formed on the top surface of the absorption layer 204 by any suitable deposition process such as sputtering, CVD, PECVD, ALD, PEALD, IBD, JVD, etc. Among them, the material of the hard mask layer 205 can be made of at least one of tantalum (Ta), tantalum-based materials (such as tantalum boride TaB, tantalum oxide TaO, tantalum nitride TaN, tantalum borate TaBO or tantalum boride nitride TaBN, etc.), silicon, silicon-based materials (such as silicon nitride SiN or silicon oxynitride SiON), ruthenium, ruthenium-based materials (such as ruthenium boride RuB), and the thickness of the hard mask layer 205 is, for example, 4 nm to 20 nm.

[0109] Among them, the deposition of the hard mask layer 205 can be carried out after the deposition of the absorption layer 204 and before the deposition of the back conductive layer 206, or can be carried out after the deposition of the absorption layer 204 and after the deposition of the back conductive layer 206.

[0110] In step S22, please continue to refer to Figure 11 , after depositing the hard mask layer 205, the following process is performed:

[0111] First, a first photoresist layer 207 is coated, and the first photoresist layer 207 is exposed and developed to pattern the first photoresist layer 207.

[0112] Then, using the patterned first photoresist layer 207 as a mask, the hard mask layer 205 is etched to the top surface of the absorption layer 204 by any suitable process such as atomic layer etching, plasma etching, etc., to transfer the pattern of the first photoresist layer 207 into the hard mask layer 205, forming a patterned hard mask layer 205'.

[0113] After that, the first photoresist layer 207 is removed by dry degluing such as plasma ashing (dry ashing) or a suitable wet degluing (wet stripping) process. For example, first, the first photoresist layer 207 is dry ashed with oxygen (O2) plasma, and then the first photoresist layer 207 is wet stripped with various organic acids, inorganic sulfuric acid, and H2O2 at high temperature, and then isopropyl alcohol (IPA) rinsing and CO2 rinsing are performed to remove the first photoresist layer 207.

[0114] Next, using the patterned hard mask layer 205' as a mask, the absorption layer 204 is etched to the top surface of the cover layer 203 or the top surface of the reflective film stack layer 202 by a suitable etching process such as atomic layer etching, to form a first pattern 204a in the absorption layer 204, and the first pattern 204a is the pattern of the circuit and / or device required for integrated circuit manufacturing.

[0115] Please refer to Figure 11, in step S23, first, a second photoresist layer 208 is coated on the patterned hard mask layer 205' and the EUV mask substrate, and the second photoresist layer 208 is exposed and developed to pattern the second photoresist layer 208. The patterned second photoresist layer 208 can protect the formation area of the first pattern 204a on the EUV mask substrate and expose the area of the EUV mask substrate where the second pattern is to be formed, and this area is located outside the first pattern 204a.

[0116] Then, using the patterned second photoresist layer 208 as a mask, the hard mask layer 205', the absorption layer 204, the covering layer 203, and the reflective film stack layer 202 are etched by a suitable etching process such as atomic layer etching, and the etching stops on the surface of the spin-on carbon layer 201 to form the second pattern 209, thereby obtaining an EUV mask blank, where the second pattern 209 is the border of the EUV mask blank.

[0117] After that, the second photoresist layer 208 is removed by a dry stripping process such as plasma ashing or a suitable wet stripping process. And the hard mask layer 205' is further removed, thereby forming an EUV mask blank having the first pattern 204a and the second pattern 209.

[0118] The manufacturing method of the EUV mask blank of this embodiment can manufacture an EUV mask blank with lower cost, fewer defects, and higher performance because it is made based on the EUV mask substrate of the present invention.

[0119] Please refer to Figure 11 , this embodiment also provides an EUV mask blank, which is formed by using the manufacturing method of the EUV mask blank of this embodiment. It not only has the EUV mask substrate of this embodiment but also has the required patterns. Specifically, as shown in the last figure in Figure 11 , this EUV mask blank has the first pattern 204a and the second pattern 209. The first pattern 204a penetrates through the absorption layer 204 and is located above the top reflective film of the reflective film stack layer 202 of the EUV mask substrate. The second pattern 209 penetrates through the absorption layer 204 and the reflective film stack layer 202 of the EUV mask substrate and exposes the top surface of the spin-on carbon layer 201 of the EUV mask substrate. The first pattern 204a is the required circuit pattern, and the second pattern 209 is the border pattern required for the periphery of the circuit.

[0120] In addition, it is worth noting that during the manufacturing process of the EUV mask substrate and the EUV mask blank of the present invention, and during the EUV lithography process using the EUV mask blank, if the corresponding operations are performed at a suitable ambient temperature (such as the EUV exposure temperature, specifically, for example, 100°C to 200°C), during the operation, the CTE on the surface of the coating layer 200b is close to 0, which can avoid the generation of unwanted deformations and defects and ensure the effect of the corresponding operations.

[0121] Moreover, due to the presence of the spin-coated carbon layer 201, the spin-coated carbon layer 201 can be regarded as a regenerated "sacrificial layer", and then removed by O2 plasma ashing to realize the recycling and reuse of the substrate.

[0122] Please refer to Body 12. Taking the recycling of the substrate of the EUV mask blank of the present invention as an example, the substrate recycling method of this embodiment specifically includes: First, using any process such as wet etching, plasma etching, chemical mechanical polishing, etc., sequentially remove the absorption layer 204, the covering layer 203 and the reflective film stack layer 202 of the EUV mask blank to expose the spin-coated carbon layer 201 of the EUV mask blank; Then, the spin-coated carbon layer 201 is removed by plasma ashing to expose the surface of the covering layer 200b of the EUV mask blank. Thus, the substrate of the EUV mask blank is recycled, and this substrate can be used to manufacture a new EUV mask blank or other devices.

[0123] Optionally, in this embodiment, before removing the absorption layer 204, or after removing the reflective film stack layer 202 and before removing the spin-coated carbon layer 201, or after removing the spin-coated carbon layer 201, the back conductive layer 206 on the surface of the substrate 200a facing away from the spin-coated carbon layer 201 is also removed.

[0124] Further optionally, the method of step S12 described above can be used to spin-coat a carbon material again on the exposed surface of the organic polymer material 200b to form a new spin-coated carbon layer to repair the surface defects of the organic polymer material, thereby obtaining again the EUV-level substrate of the present invention for the EUV mask blank and the EUV mask blank.

[0125] Obviously, in the present invention, the spin-coated carbon layer 201 serves as a sacrificial layer, and its thickness is relatively thin, and it can be easily removed by plasma ashing, and it will not cause problems such as a decrease in the surface smoothness and thermal expansion coefficient of the covering layer 200b due to damage to the surface of the covering layer 200b. It can be used for the recycling and reuse of the substrate in the EUV mask blank and the EUV mask blank, with low recycling cost, and since the substrate recovered from the old EUV mask blank and EUV mask blank can be used to further manufacture a new EUV mask blank and EUV mask blank, the manufacturing cost of the new EUV mask blank and EUV mask blank can be further reduced.

[0126] The above description is only a description of the preferred embodiments of the present invention, and does not limit the scope of the present invention in any way. Any changes and modifications made by those of ordinary skill in the art of the present invention according to the above disclosure are within the scope of the technical solution of the present invention.

Claims

1. A manufacturing method of an EUV-level substrate, characterized in that Comprising: Providing a substrate, and forming a coating layer with a negative thermal expansion coefficient on the surface of the substrate, wherein the material of the coating layer comprises a polyimide with an amide structure in the main chain; Spin-coating a carbon material on the top surface of the coating layer to form a spin-coated carbon layer with a flat top surface, thereby forming an EUV-level substrate, and the top surface of the spin-coated carbon layer reaches a planarization degree with a surface defect size of less than 10 nm; Wherein, during or after forming the coating layer, the thickness of the coating layer is adjusted to a corresponding thickness to compensate for the difference in elastic modulus between the coating layer and the substrate, so that the coefficient of thermal expansion of the top surface of the coating layer is lower than 10 -7 / o K.

2. The manufacturing method of the EUV-level substrate according to claim 1, wherein, The step of forming a coating layer on the surface of the substrate comprises: Step a, immersing the substrate into a corresponding organic polymer material solution; Step b, placing the substrate with the organic polymer material solution attached to its surface in an oven, and curing and / or performing a thermal chemical reaction by using a stepped temperature program to form a coating layer; Step c, repeating Step a and Step b until the formed coating layer reaches a corresponding thickness.

3. The manufacturing method of the EUV-level substrate according to claim 1, characterized in that, The step of forming a coating layer on the surface of the substrate comprises: coating an organic polymer material solution on the top surface of the substrate and baking and curing it to form a coating layer with a corresponding thickness.

4. The manufacturing method of the EUV-level substrate according to claim 2 or 3, characterized in that, After forming the coating layer, adjusting the thickness of the coating layer by thinning the top surface of the coating layer.

5. A manufacturing method of an EUV mask blank, characterized in that, Comprising: Adopting the manufacturing method of the EUV-level substrate according to any one of claims 1 to 4 to form an EUV-level substrate; Sequentially forming a reflective film stack layer and an absorption layer on the spin-coated carbon layer of the EUV-level substrate to form an EUV mask blank.

6. The manufacturing method of the EUV mask blank according to claim 5, wherein After forming the reflective film stack layer on the spin-coated carbon layer and before forming the absorption layer, it further comprises: forming a covering layer on the reflective film stack layer; and After forming the absorption layer, it further comprises: forming a back conductive layer on the surface of the substrate facing away from the spin-coated carbon layer.

7. A manufacturing method of an EUV mask, characterized in that, Comprising: Adopting the manufacturing method of the EUV mask blank according to claim 5 or 6 to form an EUV mask blank; Etching the absorption layer of the EUV mask blank to form a first pattern in the absorption layer; Etching the absorption layer and the reflective film stack layer of the EUV mask blank outside the periphery of the first pattern, and stopping the etching on the surface of the spin-coated carbon layer of the EUV mask blank to form a second pattern.

8. An EUV-level substrate, characterized in that, Comprising: A substrate; A coating layer with a negative thermal expansion coefficient, at least formed on the surface of the substrate, and the material of the coating layer comprises a polyimide with an amide structure in the main chain; A removable spin-coated carbon layer, formed on the top surface of the coating layer, and the top surface of the spin-coated carbon layer reaches a planarization degree with a surface defect size of less than 10 nm; Wherein, the cladding layer is adjusted to a corresponding thickness to compensate for the difference in elastic modulus between the cladding layer and the substrate, such that the coefficient of thermal expansion of the top surface of the cladding layer is less than 10 -7 / o K.

9. An EUV mask blank, characterized in that, Comprising: The EUV-level substrate according to claim 8; A reflective film stack layer, formed on the spin-coated carbon layer of the EUV-level substrate; An absorption layer, formed on the reflective film stack layer.

10. The EUV mask blank according to claim 9, characterized in that, It further comprises: A covering layer, formed between the top reflective film of the reflective film stack layer and the absorption layer; And a back conductive layer, formed on the surface of the EUV-level substrate facing away from the reflective film stack layer.

11. An EUV mask, characterized in that, The EUV mask blank has an EUV mask substrate as described in any one of claims 9 or 10, and the EUV mask blank further has a first pattern and a second pattern. The first pattern is formed in the absorption layer of the EUV mask substrate, and the second pattern penetrates through the absorption layer and the reflective film stack layer of the EUV mask substrate and exposes the surface of the spin-on carbon layer of the EUV mask substrate.

Citation Information

Patent Citations

  • Method for forming fine pattern of semiconductor device

    CN101335198A

  • Methods of forming relief images

    CN105589299A