A method for monitoring automatic pre-bonding of rail vehicle glass
By monitoring the dosage and glue pattern of surface activation, primer and glue coating processes in the automatic bonding process of rail vehicle glass, combined with secondary manual inspection, the problem of difficult to monitor robot construction abnormalities is solved, and product quality is improved Construction reliability.
Patent Information
- Application Number
- CN202210986600.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-17
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2042-08-17
Smart Images

Figure CN115354947B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of rail vehicle production and manufacturing, and more specifically, relates to a rail vehicle glass automatic bonding pre-processing monitoring method. Background Art
[0002] The glass bonding process for rail vehicles is a special process. In the glass bonding process, after the glass surface is cleaned, it is necessary to activate the glass surface and apply a primer to improve the bonding surface performance. Surface activation, primer application and glue coating are all important steps in the special bonding process.
[0003] Since the glass used in rail vehicles is usually large in size, it is difficult to monitor the bonding area in real time when robots are used for automatic bonding construction. If any abnormality occurs during automatic construction, it is not easy to be discovered, which in turn affects product production quality and creates quality risks. Summary of the invention
[0004] The purpose of the present invention is to address the above shortcomings and provide a method for monitoring the automatic pre-bonding of rail vehicle glass. The method is used in the robot automatic glass bonding process. By comparing theoretical values with actual values, the construction quality of each process of surface activation, primer coating, and glue coating is monitored. An inspection process is set up to conduct a manual secondary inspection and confirmation on unqualified products discovered during monitoring, and unqualified products are repaired to ensure product quality.
[0005] To achieve the above object, the present invention is implemented by the following technical solutions:
[0006] A method for monitoring automatic pre-treatment of rail vehicle glass bonding, wherein the pre-treatment comprises a surface activation process, a primer coating process and a glue coating process.
[0007] In the surface activation process, calculate the actual amount of activator used and compare it with the theoretical amount of activator to determine whether the surface activation process is qualified;
[0008] In the primer application process, calculate the actual amount of primer used and compare it with the theoretical amount of primer to determine whether the primer application is qualified;
[0009] In the gluing process, the glue profile section and gluing trajectory are scanned in real time to form an actual three-dimensional glue profile map, which is compared with the theoretical glue profile map; the actual amount of adhesive used is calculated and compared with the theoretical amount of adhesive used; and whether the gluing process is qualified is determined;
[0010] In the above process, those judged as qualified enter the next process, and those judged as unqualified undergo secondary inspection. If they are still unqualified after the secondary inspection, repair operations are performed.
[0011] Furthermore, the theoretical adhesive pattern diagram is a diagram of the theoretical adhesive cross section and adhesive trajectory set according to the bonding technical requirements. The theoretical adhesive cross section is a triangular cross section diagram. According to the final adhesive pattern design, the height h of the adhesive cross section triangle is usually twice the base width a.
[0012] Furthermore, the theoretical amount of the activator, the theoretical amount of the primer and the theoretical amount of the adhesive are calculated based on the area of the surface to be bonded, the coating thickness, the volume of the adhesive and the density of the activator / primer / adhesive, and the calculation formula is:
[0013] M' 活 =S×d 活 ×ρ 活 ;
[0014] M' 底 =S×d 底 ×ρ 底 ;
[0015]
[0016] In the above formula, M' 活 , M' 底 , M' 粘 are the theoretical dosages of activator, primer and adhesive, respectively; S is the area of the surface to be bonded, d 活 d 底 are the coating thickness of the activator and primer, h is the height of the triangle of the theoretical coating section, ρ 活 , 底 , 粘 They are the densities of activator, primer and adhesive respectively.
[0017] Furthermore, the actual amount of the activator and the primer used is calculated by using an electronic liquid level meter to measure the liquid level height in the tank and convert it into the liquid volume; the actual amount of the adhesive used is measured by using a glue supply metering pump to measure the volume of the adhesive.
[0018] Furthermore, the actual three-dimensional glue pattern diagram is formed by real-time laser scanning of the glue pattern section when the robot automatically applies glue to the glass, forming a number of cross-sectional graphics, and sending the cross-sectional graphics to the computer to form a complete glue pattern section and glue application trajectory.
[0019] Furthermore, the surface activation process and the primer coating process are monitored only by the amount of the activator and the primer. The qualification standard for the surface activation process is: the difference between the actual amount of the activator and the theoretical amount is within the range of -20% to +10% of the theoretical amount; the qualification standard for the primer coating process is: the difference between the actual amount of the primer and the theoretical amount is within the range of ±30% of the theoretical amount.
[0020] Furthermore, in the gluing process, the amount of adhesive used, the cross section of the adhesive and the gluing track need to be monitored. Only when both meet the technical requirements can it be judged as qualified. The qualified standard is that the actual amount of adhesive used is not less than 90% of the theoretical amount, and the actual size of the base and height of the triangle of the adhesive cross section is not less than 95% of the theoretical size value.
[0021] Furthermore, the secondary inspection is a manual inspection and judgment.
[0022] Furthermore, if the unqualified products in the surface activation process and the primer coating process are still unqualified after the second inspection, they can be repaired manually without returning to the current process for re-construction.
[0023] Furthermore, if the unqualified products in the gluing process are still unqualified after the second inspection, it is necessary to determine the repair method of the gluing defects, and use manual repair or robot automatic repair. If manual repair is possible, it will be repaired manually and then enter the next process; if manual repair cannot be completed, the already applied adhesive will be removed and the process will return to the gluing process, and the robot will repeat the gluing to complete the automatic repair until it is qualified.
[0024] Compared with the prior art, the present invention has the following beneficial effects:
[0025] The method of the present invention changes the original visual or manual measurement method, divides the pre-treatment construction process of the robot automatic glass bonding process into three processes of surface activation, primer coating and glue coating, and sets four monitoring indicators of activator dosage, primer dosage, glue pattern diagram of automatic glue coating and adhesive dosage. By calculating the theoretical dosage of chemical products and the preset glue coating section and trajectory, the actual dosage and glue pattern are calculated using special measuring instruments and computer-aided calculation technology, the actual construction situation is compared with the theoretical data to judge whether the construction process is qualified, and a secondary inspection is set to perform manual secondary inspection and confirmation on unqualified products found in the monitoring. The monitoring of the pre-treatment process during the construction of the robot automatic glass bonding process can be realized, and the process failure caused by poor automatic operation and product quality problems can be effectively avoided. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 A process flow chart of a method for monitoring automatic pre-bonding of rail vehicle glass provided in an embodiment. DETAILED DESCRIPTION
[0027] The preferred embodiments of the present invention will be described in more detail below in conjunction with the accompanying drawings and specific examples.
[0028] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and the like are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, features defined as "first", "second", and the like may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.
[0029] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.
[0030] Example 1
[0031] This embodiment provides a monitoring method for automatic pre-bonding of rail vehicle glass, which is used in the robot automatic glass bonding process. After the glass is thoroughly cleaned, its surface must be activated, primed and glued. During the construction process, the construction quality of each process must be monitored. The entire pre-bonding process is divided into four monitoring steps: surface activation, primer, automatic glue and glue quantity inspection. A secondary inspection is set to manually check and confirm the unqualified products found by the monitoring. The process flow chart is as follows: Figure 1 shown.
[0032] The specific steps of the monitoring method described in this embodiment are as follows:
[0033] 1. According to the construction area of the surface to be bonded, the coating thickness and the density of each chemical product, the theoretical amount of activator, primer and adhesive required for the bonding construction is calculated. This amount can be in an interval range. Then, according to the bonding technical requirements, the theoretical glue coating section and glue coating trajectory diagram of the adhesive are set to form a theoretical glue type diagram. The theoretical amount can also be obtained based on the accumulation of process test data.
[0034] 2. Monitoring step 1: Surface activation
[0035] After the robot automatically applies the activator to the glass surface, a special measuring instrument is used to measure the actual amount of activator used in the construction. Specifically, an electronic liquid level meter can be used to measure the liquid level in the tank, convert it into the volume of the liquid outflow, and compare it with the theoretical amount. If the result is qualified, proceed to the next step. If the result is unqualified, the robot moves the glass to the inspection table for a second inspection and confirmation. This step can be manually inspected by professionals. If repair is required, it will be manually repaired by professionals, and then the robot will be restarted to proceed to the next step; if repair is not required, the robot will be directly started to proceed to the next step.
[0036] 3. Monitoring step 2: Apply primer
[0037] After the robot automatically applies the primer to the glass surface, a special measuring instrument is used to measure the actual amount of primer used in the construction. Specifically, an electronic liquid level meter can be used to measure the liquid level in the tank, convert it into the volume of the liquid outflow, and compare it with the theoretical amount. If the result is qualified, proceed to the next step. If the result is unqualified, the robot moves the glass to the inspection table for a second inspection and confirmation. This step can be manually inspected by professionals. If repair is required, it will be manually repaired by professionals, and then the robot will be restarted to proceed to the next step; if no repair is required, the robot will be directly started to proceed to the next step.
[0038] 4. Glue
[0039] The process includes two monitoring steps: automatic gluing and glue quantity checking.
[0040] (1) Monitoring step 3: automatic gluing
[0041] When the robot automatically applies glue to the glass, it uses a laser to scan the cross-section of the glue pattern in real time, forming countless cross-sectional graphics, and sends the cross-sectional graphics to the computer to form a complete glue pattern cross-section and trajectory, that is, the actual three-dimensional glue pattern diagram.
[0042] The computer will then compare the dimensions with the theoretical glue pattern diagram. If the glue pattern section and glue pattern trajectory are both qualified, the glue coating process can be judged to be qualified. If the result is qualified, proceed to the next step. If the result is unqualified, that is, there are defects in the glue coating trajectory and section, the robot will move the glass to the inspection table for a second inspection and confirmation. This step can be manually inspected by professionals. If repair is required, then determine the form of repair based on the glue coating defects. If manual repair is required, it will be manually repaired and the robot will be restarted to enter the next step. If the repair cannot be completed manually and the robot needs to repair it automatically, the adhesive that has been applied will be removed manually, and the robot will be restarted to repeat the automatic gluing until the process is qualified.
[0043] (2) Monitoring step 4: glue quantity inspection
[0044] After completing the inspection of the glue coating section and trajectory, use a special measuring instrument to measure the actual amount of adhesive used in the construction. Specifically, you can use a glue metering pump to measure the volume of adhesive and compare it with the theoretical amount. If the result is qualified, proceed to the next step. If the result is unqualified, the robot moves the glass to the inspection table for a second inspection and confirmation. This step can be manually inspected by professionals. If repair is required, it will be determined by manual repair based on the glue coating defects. If manual repair is required, it will be manually repaired and then restarted to enter the next step. If the repair cannot be completed manually and the robot needs to repair it automatically, the adhesive that has been applied will be removed manually and the robot will be restarted to automatically apply glue until the process is qualified.
[0045] 5. After the above three processes are qualified, the construction process can be judged to be qualified, and the monitoring of the glass automatic bonding pre-treatment process is completed.
[0046] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Without departing from the scope and technical principles of the described embodiments, many modifications and changes are obvious to those of ordinary skill in the art, and these modifications and changes should also be regarded as the scope of protection of the present invention.
Claims
1. A method for monitoring the automatic pre-bonding of rail vehicle glass, characterized in that: The pre-treatment includes a surface activation process, a primer coating process and a glue coating process. In the surface activation process, calculate the actual amount of activator used and compare it with the theoretical amount of activator to determine whether the surface activation process is qualified; In the primer application process, calculate the actual amount of primer used and compare it with the theoretical amount of primer to determine whether the primer application is qualified; In the gluing process, the glue profile section and gluing trajectory are scanned in real time to form an actual three-dimensional glue profile map, which is compared with the theoretical glue profile map; the actual amount of adhesive used is calculated and compared with the theoretical amount of adhesive used; and whether the gluing process is qualified is determined; In the above process, those judged as qualified will enter the next process, and those judged as unqualified will undergo a second inspection. If they are still unqualified after the second inspection, they will undergo repair operations; The theoretical glue pattern diagram is a diagram of the theoretical glue coating section and glue coating trajectory of the adhesive set according to the bonding technical requirements; the theoretical glue coating section is a triangle; The theoretical amount of the activator, the theoretical amount of the primer and the theoretical amount of the adhesive are calculated based on the area of the surface to be bonded, the coating thickness, the volume of the adhesive and the density of the activator / primer / adhesive. The calculation formula is: M’ 活 =S×d 活 ×ρ 活 ; M’ 底 =S×d 底 ×ρ 底 ; M’ 粘 = ×S×h×ρ 粘 ; In the above formula, M' 活 , M' 底 , M' 粘 are the theoretical dosages of activator, primer and adhesive, respectively; S is the area of the surface to be bonded, d 活 d 底 are the coating thickness of the activator and primer, h is the height of the triangle of the theoretical coating section, ρ 活 , 底 , 粘 They are the densities of activator, primer and adhesive respectively.
2. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: The actual amount of the activator and the primer used are calculated by measuring the height difference of the liquid level in the tank using an electronic liquid level meter and converting it into the volume of the discharged liquid; The actual usage amount of the adhesive is obtained by measuring the volume of the adhesive delivered by using an adhesive metering pump.
3. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: The actual three-dimensional glue pattern diagram is formed by real-time laser scanning of the glue pattern section when the robot automatically applies glue to the glass, forming several cross-sectional graphics, and sending the cross-sectional graphics to the computer to form a complete glue pattern section and glue application trajectory.
4. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: The surface activation process and the primer application process are monitored by the dosage of the activator and the primer.
5. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: In the gluing process, the amount of adhesive used, the glue section and the gluing trajectory need to be monitored. Only when both meet the technical requirements can it be judged as qualified.
6. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: The secondary inspection is a manual inspection and judgment.
7. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: If the unqualified products in the surface activation process and the primer coating process are still unqualified after the second inspection, they will be repaired manually.
8. The method for monitoring the automatic pre-bonding of rail vehicle glass according to claim 1, characterized in that: If the unqualified products in the gluing process are still unqualified after the second inspection, it is necessary to determine the repair method of the gluing defects, and adopt manual repair or robot automatic repair.
Citation Information
Patent Citations
Automatic precise gluing device of automobile sound device
CN109351554A
Dispensing device and method
CN109701822A
Production and glue coating process
CN110152960A
Intelligent production line for rail transit door plate and glass bonding
CN110465451A
Automatic gluing system and method for building glass doors and windows
CN111774247A