A semiconductor transistor structure and fabrication method

By filling the bottom of the contact hole and the surrounding area of ​​the source/drain region with low-concentration impurity ions and injecting inversion ions, the problems of leakage current and electric field strength in semiconductor transistors are solved, and the performance of the device is improved.

CN115565979BActive Publication Date: 2026-11-10CHANGXIN MEMORY TECH INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202110749993.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-07-02
Publication Date
2026-11-10
Estimated Expiration
2041-07-02

AI Technical Summary

Technical Problem

In existing semiconductor transistors, the leakage current between the source/drain region and the substrate is large due to contact hole doping, and the electric field strength at the bottom of the contact hole is high, which affects the device performance.

Method used

The peripheral region at the bottom of the contact hole, which is in contact with the source/drain region, is filled with impurity ion concentrations lower than those in the middle region. By injecting inverted ions to neutralize the impurity ions, the ion concentration difference between the source/drain region and the substrate is reduced, thereby decreasing the leakage current.

Benefits of technology

It effectively reduces leakage current, decreases the electric field strength at the bottom of the contact hole, and improves the performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115565979B_ABST
    Figure CN115565979B_ABST
Patent Text Reader

Abstract

This application discloses a semiconductor transistor structure, comprising: a substrate having a first conductivity type well region, and a gate structure disposed on the substrate; a second conductivity type source / drain region disposed within the first conductivity type well region, with the source / drain region located on opposite sides of the gate structure; contact holes formed at corresponding positions of the source / drain regions, the contact holes extending downward into the first conductivity type well region; the contact holes being filled with conductive metal, and impurity ions implanted at the bottom of the contact holes to reduce their contact resistance; the impurity ion concentration in the peripheral region of the bottom of the contact holes in contact with the source / drain regions being lower than the impurity ion concentration in the intermediate region. This application reduces the ion concentration difference between the source / drain regions and the well region by maintaining a lower impurity ion concentration at the peripheral region of the bottom of the contact holes in contact with the source / drain regions than the impurity ion concentration in the intermediate region during the filling of the contact holes, thereby reducing leakage current.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the technical field of semiconductor integrated circuits, and more particularly to a semiconductor transistor structure and fabrication method. Background Technology

[0002] Metal-oxide-semiconductor (MOS) transistors are crucial electronic components in modern semiconductor products, and their electrical performance is key to the quality of integrated circuits. A MOS transistor is a four-terminal electronic device consisting of a gate, source, drain, and substrate, with an oxide insulating layer between the gate and the substrate. When a MOS transistor operates, applying a voltage to the gate causes an inversion channel to form on the substrate side closest to the oxide insulating layer. Since the source and drain are also inverted, they become conductive, thus controlling the transistor's switching operation.

[0003] Currently, after the source and drain regions of a MOSFET are formed, a specific area is opened using a photolithographic mask, etched to form contact holes, and then conductive material is deposited within the contact holes. To reduce the contact resistance of the contact holes, the current process typically involves injecting another layer of impurity ions (of the same type, typically one-tenth the source / drain doping concentration) into the bottom of the contact hole after the source / drain regions are doped, before the conductive material is deposited. This increases the doping concentration of impurity ions in the source / drain regions, forming a PN junction with a larger ion concentration difference between the source / drain regions and the substrate. Applying voltage to the source / drain regions makes it easier for the PN junction to conduct, resulting in leakage current. Furthermore, higher electric field strengths are formed at the bottom corners or sharp points of the contact holes, further amplifying the leakage current of the PN junction. Leakage current has a significant impact on device performance; therefore, a novel MOS transistor structure and fabrication method are needed to reduce leakage current. Summary of the Invention

[0004] (I) Purpose of the Invention

[0005] The purpose of this application is to provide a semiconductor transistor structure that addresses the leakage current problem between the source / drain region and the substrate caused by contact hole doping in existing semiconductor transistors. By making the impurity ion concentration in the peripheral region where the bottom of the contact hole contacts the source / drain region lower than the impurity ion concentration in the middle region, the ion concentration difference between the source / drain region and the substrate is reduced while keeping the vertical resistance of the contact hole constant, thereby reducing the leakage current.

[0006] (II) Technical Solution

[0007] To address the aforementioned technical problems, a first aspect of this application provides a semiconductor transistor structure, characterized in that it comprises: a substrate having a first conductivity type well region, on which a gate structure is disposed; a second conductivity type source / drain region disposed within the first conductivity type well region, with the source and drain regions located on opposite sides of the gate structure; a contact hole formed at a position corresponding to the source / drain region, the contact hole extending downward into the first conductivity type well region; the contact hole being filled with a conductive metal, and impurity ions for reducing its contact resistance being implanted at the bottom of the contact hole, wherein the impurity ion concentration in the peripheral region of the bottom of the contact hole in contact with the source / drain region is lower than the impurity ion concentration in the middle region.

[0008] By adopting the above technical solution, when filling the contact hole with impurity ions, the impurity ion concentration in the peripheral area where the bottom of the contact hole contacts the source / drain region is lower than that in the middle area. While ensuring that the vertical resistance in the contact hole remains unchanged, the ion concentration difference between the source / drain region and the substrate is reduced, thereby reducing the leakage current. At the same time, the electric field strength at the location where the bottom of the contact hole contacts the source / drain region is lowered, and the PN junction leakage current can be reduced when a voltage is applied to the source / drain region.

[0009] Preferably, the peripheral area at the bottom of the contact hole that contacts the source / drain region is filled with inverse ions for neutralizing the concentration of impurity ions.

[0010] Preferably, the injection energy of the anti-ion is 15 keV, the injection dose is 5e13 atom, and the anti-ion is selected from any one of phosphorus ions, arsenic ions, and antimony ions.

[0011] Preferably, the injection energy of the impurity ions is 2-3 keV, the injection dose is 8E14-1E15 atom, and the impurity ions are selected from any one of boron ions, aluminum ions, and indium ions.

[0012] Preferably, the first conductivity type well region is N-type doped, and the doping ion is selected from any one of phosphorus ions, arsenic ions, and antimony ions; the second conductivity type source / drain region is P-type doped, and the doping ion is selected from any one of boron ions, aluminum ions, and indium ions.

[0013] Preferably, the conductive metal of the contact hole includes metal silicides and metallic materials.

[0014] Preferably, the metallic material includes tungsten, aluminum, and molybdenum.

[0015] Preferably, the contact hole extends downward to a depth of 20-50 nm.

[0016] Preferably, the gate structure includes a dielectric layer, a polysilicon conductive layer, an insulating silicon nitride layer, and a silicon oxide layer sequentially stacked on a first conductivity type well region.

[0017] A second aspect of this application provides a method for fabricating a semiconductor transistor, comprising: forming a substrate having a well region of a first conductivity type; forming a gate structure on the surface region of the first conductivity type well region; forming a source region and a drain region of a second conductivity type in the first conductivity type well regions on both sides of the gate structure; forming contact holes in the source region / drain region; forming a high concentration region of impurity ions in the middle region at the bottom of the contact hole, and forming a low concentration region of impurity ions in the peripheral region at the bottom of the contact hole that contacts the source region / drain region; and depositing a conductive layer in the contact hole to form a conductive contact.

[0018] Preferably, forming a high-concentration region with impurity ions in the middle region of the contact hole includes: vertically injecting impurity ions into the contact hole to fill the bottom region of the contact hole, and then activating them through RTP to diffuse them through the bottom of the contact hole to the source / drain region.

[0019] Preferably, forming a low-concentration region with impurity ions in the peripheral area of ​​the bottom of the contact hole that contacts the source / drain region includes: injecting inverted ions into the contact hole so that the inverted ions are uniformly distributed in the peripheral area of ​​the bottom of the contact hole that contacts the source / drain region.

[0020] Preferably, the inverse ions are implanted at an angle of 8-12 degrees.

[0021] Preferredly, depositing a conductive layer within the contact hole to form a conductive contact includes: sputtering and depositing metallic cobalt within the contact hole, followed by thermal oxidation to react the cobalt with silicon in the source / drain region to form a metal silicide; then depositing a metal material to fill the contact hole and form a conductive layer.

[0022] (III) Beneficial Effects

[0023] The above-mentioned technical solution of this application has the following beneficial technical effects: by filling the contact hole with impurity ions, the impurity ion concentration in the peripheral area where the bottom of the contact hole contacts the source / drain region is lower than the impurity ion concentration in the middle area, thereby reducing the ion concentration difference between the source / drain region and the substrate while ensuring that the vertical resistance in the contact hole remains unchanged, thereby reducing leakage current and improving the performance of the device. Attached Figure Description

[0024] Figure 1 This is a full sectional structural diagram of an embodiment of this application;

[0025] Figure 2This is a flowchart illustrating the method for forming a MOS transistor structure according to an embodiment of this application;

[0026] Figures 3-8 This is a schematic diagram of the main process cross-sections during the formation of the MOS transistor structure in a specific embodiment of this application.

[0027] Figure label:

[0028] 1. Substrate; 11. First conductivity type well region; 2. Gate structure; 21. Dielectric layer; 22. Polysilicon gate layer; 221. First side exterior; 222. Second side exterior; 23. Insulating silicon nitride layer; 24. Silicon oxide layer; 3. Source region; 4. Drain region; 5. Impurity ions; 6. Inversion ions; 7. Metal silicide; 8. Metal material. Detailed Implementation

[0029] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to specific embodiments and the accompanying drawings. It should be understood that these descriptions are merely exemplary and not intended to limit the scope of the invention.

[0030] like Figure 1 As shown, this specific embodiment provides a semiconductor transistor structure, including: a substrate 1, and a first conductivity type well region 11 formed on the surface region of the substrate 1. The first conductivity type well region 11 is N-type doped, and the doping ions are selected from any one of phosphorus ions, arsenic ions, and antimony ions. Optionally, the substrate 1 is a silicon substrate.

[0031] A gate structure 2 is disposed on the surface of the first conductivity type well region 11. The gate structure 2 includes a dielectric layer 21 and a polysilicon gate layer 22. The dielectric layer 21 is located on the surface of the first conductivity type well region 11. The constituent material of the dielectric layer 21 can be one of the high-k materials such as hafnium oxide, hafnium silicate, lanthanum oxide, zinc oxide, zinc silicate, tantalum oxide, titanium oxide, barium strontium titanate, barium titanate, strontium titanate, yttrium oxide, aluminum oxide, ferroelectric thin film, zinc niobate, and lead titanate. The polysilicon gate layer 22 is disposed on the dielectric layer 21. The constituent material of the polysilicon gate layer 22 can include, for example, one or more of polysilicon, hafnium, titanium, tantalum, aluminum, zirconium, ruthenium, palladium, platinum, cobalt, nickel, and their oxides and carbides.

[0032] A source region 3 and a drain region 4, doped with a second conductivity type, are formed within the surface of the first conductivity type well region 11. The source region 3 and drain region 4 are symmetrically disposed on both sides of the dielectric layer 21. The source region 3 and drain region 4 can be formed by inversion ion implantation into the regions located on both sides of the gate structure 2 on the surface of the first conductivity type well region 11. The type of conductive ions doped in the source region 3 and drain region 4 is determined by the specific semiconductor device type in which they are formed. In this embodiment, a PMOS device is used, so the source and drain regions are P-type doped, and the doping ions are selected from any one of boron ions, aluminum ions, and indium ions.

[0033] Contact holes 111 are etched in the corresponding regions of source region 3 and drain region 4. The contact holes 111 extend downwards into the first conductivity type well region 11, with a downward extension depth of 20-50 nm. Impurity ions 5 are doped into the bottom region of the contact holes 111. The impurity ions 5 are selected from any one of boron ions, aluminum ions, and indium ions; in this embodiment, boron ions are used as an example. The boron ions are activated by a rapid thermal processing (RTP) process, causing them to diffuse in the bottom region of the contact holes 111, thereby reducing the contact resistance of the contact holes 111.

[0034] The peripheral region at the bottom of contact hole 111 that contacts source region 3 / drain region 4 is filled with inverted ions 6. These inverted ions 6 neutralize boron ions. The inverted ions 6 are selected from any one of phosphorus ions, arsenic ions, and antimony ions; in this embodiment, phosphorus ions are used as an example. Adding phosphorus ions reduces the majority carrier boron ion concentration in the peripheral region at the bottom of contact hole 111 that contacts source region 3 / drain region 4 compared to the concentration in the middle region. This reduces the ion concentration difference between source region 3 / drain region 4 and the first conductivity type well region 11 without affecting the vertical resistance of contact hole 111, thereby reducing leakage current.

[0035] Appendix Figure 2 This is a flowchart of the method for forming the MOS transistor structure in this application;

[0036] Appendix Figure 3-8 This is a schematic diagram of the main process cross-sections during the formation of the MOS transistor structure in this application.

[0037] This application also provides a method for fabricating a semiconductor transistor structure, including the following steps:

[0038] Step S11, a first conductivity type well region is formed, such as Figure 2 , 3 As shown,

[0039] Specifically, a P-type substrate 1 is provided, and N-type doping is performed on the P-type substrate 1 by ion implantation to form an N-type first conductivity type well region 11. Optionally, the specific material of the substrate 1 can be selected by those skilled in the art according to actual needs. This specific embodiment uses a silicon substrate as an example for illustration.

[0040] Step S12, forming a dielectric layer covering the well region of the first conductivity type, such as Figure 2 , 4 As shown,

[0041] Specifically, a dielectric layer 21 is deposited on the surface of the first conductivity type well region 11 of the substrate 1 using a thermal oxidation process, such that the dielectric layer 21 covers the surface area of ​​the first conductivity type well region 11. The dielectric layer 21 is made of an insulating material, and its specific type can be selected by those skilled in the art according to actual needs. The thickness of the dielectric layer 21 can be set as needed, with a preferred thickness of 30–50 angstroms.

[0042] Step S13, forming a polysilicon gate layer on the dielectric layer, such as Figure 2 , 4 As shown,

[0043] Specifically, the semiconductor wafer, including the dielectric layer 21, is transferred into a low-pressure chemical vapor deposition (LPCVD) apparatus. Silane is introduced into the process chamber of the apparatus, and after the silane decomposes, polysilicon is deposited on the surface of the dielectric layer 21. After the polysilicon deposition is completed, polysilicon doping can be performed. In the photoresist layer, a gate pattern is formed through exposure and development processes. Using the photoresist layer as a mask, the dielectric layer 21 and the polysilicon layer outside the gate pattern are removed through an etching process to form a polysilicon gate layer 22.

[0044] Step S14: Form an insulating layer on the polysilicon gate layer, such as... Figure 2 , 5 As shown,

[0045] In the figure, an insulating silicon nitride layer 23 is formed by chemical vapor deposition, covering the top and sidewalls of the polysilicon gate layer 22. The top thickness is generally between 0.1 μm and 3 μm, and the sidewall thickness is generally between 10 nm and 30 nm. A silicon oxide layer 24 is formed on the insulating silicon nitride layer 23, extending to the side of the insulating silicon nitride layer 23. That is, the insulating silicon nitride layer 23 is encased in the silicon oxide layer 24 to prevent the gate structure 2 from being affected during subsequent source / drain ion implantation. The side thickness of the silicon oxide layer 24 defines the position of the source / drain region. The insulating silicon nitride layer 23 / silicon oxide layer 24 also serves as a self-aligned structure for subsequent source / drain ion implantation.

[0046] Step S15, a drain region and a source region are formed within the well region of the first conductivity type, such as... Figure 4 , 5 As shown,

[0047] Specifically, self-alignment can be achieved using the gate structure 2 / silicon oxide layer 24. Source / drain formation regions are formed on the surface of the first conductivity type well region 11 and on both sides of the gate structure 2. During source / drain implantation, the two sides of the silicon oxide layer 24 serve as self-alignment boundaries. Conductive impurities are simultaneously implanted into the source / drain formation regions by ion implantation to form source region 3 and drain region 4.

[0048] Step S16: Form contact holes in the source / drain region, such as... Figure 2 , 6 As stated above.

[0049] Specifically, a patterned photoresist layer is formed on the surface of drain region 4. Then, using this photoresist layer as a mask, the surface region of drain region 4 located on the outer side 222 of the second side of the polysilicon gate layer 22 is etched, forming contact holes 111 that expose their interior in the surface region of drain region 4. The method of forming contact holes 111 in source region 3 is the same as the method of forming contact holes 111 in drain region 4, and will not be described in detail here. The mask used for etching is not limited to the photoresist in this embodiment; other masking techniques, such as metal hard masks, can also be used.

[0050] Step S17: Fill the contact hole with impurity ions, such as... Figure 2 , 7 As shown,

[0051] Specifically, impurity ions 5 are implanted into the contact hole 111 using an ion implantation process. Boron ions and their fluorides are preferred because boron ions are lightweight and easily diffuse, while boron fluorides reduce boron diffusion and form amorphous regions, thus reducing the tunneling effect of ion implantation. The implanted ions are activated using rapid heat treatment or high-temperature annealing to allow the impurity ions 5 to diffuse at the bottom of the contact hole 111. Preferably, the impurity ions 5 are implanted vertically with an injection energy of 2–3 keV and an injection dose of 8E14–1E15 atoms.

[0052] Step S18: Inverted ions are injected at the bottom corner of the contact hole, such as... Figure 2 , 7 As shown,

[0053] Specifically, inverted ions 6, preferably phosphorus ions, are injected into the contact hole 111. The inverted ions 6 neutralize impurity ions 5. Specifically, an angled injection is used to ensure that the inverted ions 6 are evenly distributed in the peripheral area of ​​the bottom of the contact hole 111 where it contacts the source region 3 / drain region 4. This reduces the ion concentration difference between the source region 3 / drain region 4 and the first conductivity type trap region 11 without affecting the vertical resistance of the contact hole 111, thereby reducing leakage current. Preferably, the injection angle of the inverted ions 6 is 8-12 degrees, the injection energy is 15 keV, and the injection dose is 5 e13 atom.

[0054] Step S19: Deposit a conductive layer in the contact hole to form a conductive contact, such as... Figure 2 , 8 As shown,

[0055] Specifically, cobalt is deposited within the contact hole 111 of the source region 3 / drain region 4 via physical vapor deposition or ion sputtering. Heat treatment causes the silicon layer to react with the cobalt to form a metal silicide 7, i.e., a cobalt silicide layer. A metal material 8 is then deposited on the cobalt silicide layer via low-pressure chemical vapor deposition, rapid thermal chemical vapor deposition, or similar methods to fill the contact hole (111), forming a conductive layer. The optional metal material 8 can be at least one of tungsten, aluminum, and molybdenum.

[0056] The semiconductor transistor structure and fabrication method provided in this specific embodiment, without affecting the vertical resistance value inside the contact hole 111, involves tilting an inverted ion 6 into the contact hole 111 to neutralize the impurity ions 5. This causes the inverted ions 6 to be distributed in the peripheral area at the bottom of the contact hole 111 that is in contact with the source region 3 / drain region 4, thereby reducing the ion concentration difference between the source region 3 / drain region 4 and the first conductivity type well region 11, thus reducing leakage current and improving device performance.

[0057] It should be understood that the specific embodiments described above are merely illustrative or explanatory of the principles of the invention and do not constitute a limitation thereof. Therefore, any modifications, equivalent substitutions, improvements, etc., made without departing from the spirit and scope of the invention should be included within the protection scope of the invention. Furthermore, the appended claims are intended to cover all variations and modifications falling within the scope and boundaries of the appended claims, or equivalent forms of such scope and boundaries.

Claims

1. A semiconductor transistor structure, characterized in that, include: A substrate (1) having a first conductivity type well region (11) is provided with a gate structure (2) on the substrate (1). The source region (3) / drain region (4) of the second conductivity type is disposed in the well region (1) of the first conductivity type, and the source region (3) and the drain region (4) are located on both sides of the gate structure (2); A contact hole (111) is provided at the corresponding position of the source region (3) / drain region (4), and the contact hole (111) extends downward into the first conductivity type well region (11); The contact hole (111) is filled with conductive metal, and impurity ions (5) are injected at the bottom of the contact hole (111) to reduce its contact resistance. The peripheral area at the bottom of the contact hole (111) that is in contact with the source region (3) / drain region (4) is filled with inverse ions (6) to neutralize the concentration of impurity ions (5). The concentration of impurity ions (5) in the peripheral area at the bottom of the contact hole (111) that is in contact with the source region (3) / drain region (4) is lower than the concentration of impurity ions (5) in the middle region.

2. The semiconductor transistor structure according to claim 1, characterized in that, The injection energy of the trans ion (6) is 15 keV, and the injection dose is 5e13 atom. The trans ion (6) is selected from any one of phosphorus ion, arsenic ion and antimony ion.

3. A semiconductor transistor structure according to claim 1, characterized in that... The injection energy of the impurity ion (5) is 2~3 keV, the injection dose is 8E14~1E15 atom, and the impurity ion (5) is selected from any one of boron ion, aluminum ion and indium ion.

4. A semiconductor transistor structure according to claim 1, characterized in that, The first conductivity type well region (11) is N-type doped, and the doping ions are selected from any one of phosphorus ions, arsenic ions and antimony ions; The source region (3) / drain region (4) of the second conductivity type is P-type doped, and the doping ions are selected from any one of boron ions, aluminum ions and indium ions.

5. A semiconductor transistor structure according to claim 1, characterized in that, The conductive metal of the contact hole (111) includes metal silicide (7) and metal material (8).

6. A semiconductor transistor structure according to claim 5, characterized in that, The Metallic materials (8) include tungsten, aluminum, and molybdenum.

7. A semiconductor transistor structure according to claim 1, characterized in that, The contact hole (111) extends downward to a depth of 20-50 nm.

8. A semiconductor transistor structure according to claim 1, characterized in that, The gate structure (2) includes a dielectric layer (21), a polysilicon conductive layer (22), an insulating silicon nitride layer (23), and a silicon oxide layer (24) sequentially stacked on a first conductivity type well region (11).

9. A method for fabricating a semiconductor transistor, characterized in that, include: A substrate (1) is provided having a well region (11) of a first conductivity type formed thereon; A gate structure (2) is formed in the surface region of the first conductivity type well region (11); A source region (3) and a drain region (4) of a second conductivity type are formed in the first conductivity type well region (11) on both sides of the gate structure (2); Contact holes (111) are formed at the source region (3) and the drain region (4), respectively. A high concentration region with impurity ions (5) is formed in the middle region at the bottom of the contact hole (111). Inverted ions (6) are injected into the contact hole (111) so that the inverted ions (6) are evenly distributed in the peripheral region at the bottom of the contact hole (111) that is in contact with the source region (3) / drain region (4), forming a low concentration region with impurity ions (5). A conductive layer is deposited in the contact hole (111) to form a conductive contact.

10. The method according to claim 9, characterized in that, Forming a high-concentration region with impurity ions (5) in the middle region of the contact hole (111) includes: Impurity ions (5) are vertically injected into the contact hole (111) to fill the bottom region of the contact hole (111), and then activated by RTP to diffuse through the bottom of the contact hole (111) to the source region (3) / drain region (4).

11. The method according to claim 9, characterized in that, The inverse ion (6) is injected at an angle of 8-12 degrees.

12. The method according to claim 9, characterized in that, Depositing a conductive layer within the contact hole (111) to form a conductive contact includes: Cobalt metal is sputtered and deposited in the contact hole (111), and then oxidized by heating to react the cobalt with the silicon in the source region (3) / drain region (4) to form a metal silicide (7); then a metal material (8) is deposited to fill the contact hole (111) to form a conductive layer.

Citation Information

Patent Citations

  • Method for fabricating contact in semiconductor device

    KR1020070063363A

  • Method of manufacturing a semiconductor device having a lightly doped contact impurity region surrounding a highly doped contact impurity region

    US6162668A