Method for manufacturing a board

By using hard particles and surface structure modifying agents in the multi-layer trimming layer of the plate to form notches, the problems of poor printing pattern structure and insufficient wear resistance in the prior art are solved, and deeper and larger notches and better waterproof.

CN115626000BActive Publication Date: 2024-11-26UNILIN BVBA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211273334.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-01-04
Filing Date
2018-12-20
Publication Date
2024-11-26
Estimated Expiration
2038-12-20

AI Technical Summary

Technical Problem

Prior art When manufacturing plates, it is difficult to smoothly realize the structure of the printed pattern, and the pattern is not protected against wear and moisture penetration, and the use of hard particles in the top layer adversely affects viscosity and surface tension, resulting in insufficient formation of recesses.

Method used

The multi-layer trimming layer method is used, wherein the first trimming layer comprises hard particles, and the second trimming layer forms a notch above it, and the notch is formed by a surface structure changing agent such as a chemical agent, preferably using a transparent or translucent material, hard The particles do not affect the surface of the second trimming layer after partial hardening in the first trimming layer.

Benefits of technology

A deeper and larger depth-to-width ratio is achieved, improving the wear resistance and water resistance of the plate, while avoiding the impact of hard particles on the formation of recesses on the top surface, enhancing the overall performance of the plate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115626000B_ABST
    Figure CN115626000B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for manufacturing a board. The method for manufacturing a board using a substrate (2) and a decorative top layer (3), the decorative top layer comprising a printed pattern and a transparent or translucent protective layer (9) formed thereon, wherein the method comprises at least the following steps: a step of applying a first trimming layer (6) and a second trimming layer (7) for forming the first and second parts of the protective layer (9); a step of forming a recess (16) on the surface (17) of the second trimming layer (7), characterized in that the first trimming layer (6) comprises hard particles (13).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of the invention patent application with the application date of December 20, 2018, application number 201880085328.4, and invention name “Method for Manufacturing Plates”. Technical Field

[0002] The present invention relates to a method for manufacturing panels, more particularly decorative panels, such as floor panels, wall panels, ceiling panels and furniture panels.

[0003] More specifically, the invention relates to a method for producing a board of the type comprising at least a substrate and a decorative top layer arranged on the substrate, for example with a printed motif. In this context, this may relate, for example, to floor panels, furniture panels, ceiling panels, wall panels, etc., which consist essentially of an MDF or HDF (medium or high density fiberboard) base board or substrate and a top layer arranged thereon, or which consist essentially of a synthetic material, for example based on PVC (polyvinyl chloride) and a top layer arranged thereon.

[0004] In particular, the invention relates to a method in which one or more material layers are arranged on a substrate, wherein at least one of these material layers comprises a printed pattern. Preferably, in this context this relates to a pattern that is at least partly obtained by printing carried out directly or indirectly on a substrate. However, the invention is also applicable to boards in which the pattern is realized in another way, for example by printing the pattern on a carrier sheet and arranging the carrier sheet on the above-mentioned substrate, as is the case for example for DPL (direct pressure laminated) laminates, in which the individual carrier sheets typically consist of paper, or as can be the case for LVT (luxury vinyl tile) boards, in which the individual carrier sheets typically consist of a synthetic foil, such as a PVC foil. Background Art

[0005] For example, plates having a pattern obtained by printing on a substrate are known from, for example, US 1,971,067, US 3,173,804, US 3,554,827, US 3,811,915, WO 01 / 48333, WO 01 / 47724, US 2004 / 0026017, WO 2004 / 042168, EP 1 872959, DE 197 25 829 C1 or DE 195 32 819 A1. According to the above documents, it is also known that the material layer can comprise one or more base layers, wherein these base layers extend substantially below the print (print, printing, imprint, impression), and / or can comprise one or more finishing layers (finishing layer), which extend substantially above the pattern. These finishing layers may comprise, for example, a transparent or translucent synthetic layer which forms a protective layer over the pattern (whether printed or not) and which may contain, for example, wear-resistant particles, such as aluminium oxide. It is not excluded that the protective layer contains a sheet of material, such as a sheet of paper, provided with, for example, a synthetic material, such as an amino resin, as may be the case with a DPL type laminate. In the case of LVT panels, preferably, a protective layer consisting essentially of transparent PVC is used.

[0006] According to the above-mentioned patent document, a variety of methods for providing a plate surface with a certain structure of coating are known. According to WO 2004 / 042168, it is known to provide a recess (recess, groove, recess) in the substrate itself or in the base layer and print in a pattern on the substrate of the structure. According to WO 01 / 47725, US 3,811,915 and US 3,554,827, it is known to provide a reagent (lacquer-repelling agent, paint-repelling agent) for repelling paint on the printed pattern, thereby selectively hardening the transparent lacquer layer arranged thereon, thereby forming a structure on the final plate. According to WO01 / 48333, it is known to provide an embossing by a template or a pressing roller on the lacquer layer arranged on the pattern. According to WO 01 / 47724, it is known to selectively set a transparent lacquer layer on the pattern by inkjet and realize the structure in this way, wherein the lacquer layer thus arranged only partially covers the pattern and a part of the pattern is not protected from wear. According to DE 197 25 829 C1, it is known to provide an embossing in a protective layer arranged above a pattern by means of a template or a pressure roller. In DE 197 25 829 C1, a protective layer applied in liquid form is applied, which contains a thermosetting resin, such as melamine.

[0007] The techniques mentioned above are still far from what is desired with respect to flexibility and / or with respect to the structures that can be realized. Thus, for example, it is difficult to realize with these techniques a structure corresponding to a pattern applied by printing in a smooth manner. Moreover, according to some known techniques, the pattern is still partially unprotected, for example, against abrasion or moisture penetration.

[0008] As a solution to the above problems, WO 2010 / 070485 discloses a variety of technologies for flexibly providing structures on coated boards. Among them, WO'485 involves applying digital technology to provide agents for repelling paint, wherein the applied agents determine at least a portion of the board surface structure. DE2015 110 236A1 involves similar technology.

[0009] The known techniques show the disadvantage that the top layers achieved are not really resistant to scratches or other abrasions. The inventors have found that the use of sufficiently large hard particles in a top layer structured by a lacquer-repelling agent has an adverse effect on the desired formation of the recesses. The hard particles have an influence on the viscosity, flow, surface tension and other characteristics of the top layer material.

[0010] Furthermore, the maximum achievable depth and / or aspect ratio of digital structures obtained according to the prior art is still far from what is desired. Summary of the invention

[0011] According to its several independent aspects, the present invention is mainly directed to an alternative method for manufacturing panels, which, according to its several preferred embodiments, can be implemented more smoothly and / or more economically than the prior art methods and / or provides a solution to one or more disadvantages of the prior art methods.

[0012] To this end, according to its first independent aspect, the present invention relates to a method for manufacturing panels, wherein these panels comprise at least a substrate and a decorative top layer, wherein the decorative top layer comprises at least a printed pattern and a transparent or translucent protective layer formed thereon, wherein the method comprises at least the following steps:

[0013] - a step of providing a substrate;

[0014] - a step of applying a first trimming layer for forming a first portion of the above-mentioned protective layer;

[0015] - a step of at least partially hardening said first finishing layer;

[0016] - a step of applying a second trimming layer for forming a second portion of the above-mentioned protective layer;

[0017] - a step of forming a recess at the surface of said second finishing layer,

[0018] The invention is characterized in that the first finishing layer contains hard particles. Since the hard particles are located in the first at least partially hardened finishing layer, they have almost no influence on the step of forming the recesses in the surface of the second finishing layer located thereon.

[0019] It is noted that according to the invention, the second finishing layer is located above the first finishing layer, or in other words, the second finishing layer is located closer to the upper surface of the final corresponding plate than the first finishing layer.

[0020] Furthermore, it is noted that, of course, the top layer may also contain further layers or parts. Thus, for example, below the first trimming layer, there is also at least a printing layer, and below the first trimming layer, an earlier formed trimming layer may be arranged. Between the first and second trimming layers and / or above the second trimming layer, one or more further trimming layers may also be arranged.

[0021] It will be apparent that the method of the first aspect also preferably comprises complete hardening of the first and second trim layers and this is preferably performed after the step of forming the recess in the surface of the second trim layer has been completed.

[0022] Preferably, the second finishing layer described above does not contain hard particles so that the step of forming the recesses can be performed in an optimal manner.

[0023] According to another possibility, the above-mentioned second trimming layer also comprises hard particles. In this case, the average diameter of the hard particles in the second trimming layer is preferably smaller than the average diameter of the hard particles in the first trimming layer. According to another possibility or in combination therewith, the second trimming layer also comprises hard particles, wherein the shape of the hard particles in the second trimming layer is different from the shape of the hard particles in the first trimming layer. Thus, for example, in the second trimming layer, relatively oblong particles can be used, while in the first trimming layer relatively spherical particles are used, or vice versa.

[0024] Preferably, the hard particles of the first finishing layer protrude beyond the surface of the first finishing layer. In this way, they can penetrate upwards into the second finishing layer in the final plate. Thus, a good wear resistance of the second finishing layer can be obtained without the hard particles having a significant effect on the step of forming the recesses in the surface of the second finishing layer located above it. Obviously in these embodiments, the second finishing layer may or may not be provided with hard particles, as also explained above in this article.

[0025] As hard particles, preferably corundum or aluminum oxide particles are used. According to other possibilities, silicon carbide or silicon dioxide can also be used, or mixtures of the abovementioned possibilities of hard particles.

[0026] Preferably, the above-mentioned first and / or second finishing layer is at least partially obtained by further applying a hardening material in liquid form on the substrate, such as, for example, a lacquer to be cured, for example, a lacquer to be cured by ultraviolet (UV) or electron beam, etc. The application in liquid form can be carried out, for example, by one or more rollers. The above-mentioned hard particles can be provided in the first and possibly the second finishing layer by mixing in the material to be applied in liquid form and hardened, or by spreading them in the still wet finishing layer concerned or depositing them in another way, or by forming part of a sheet of material provided in or on the still wet finishing layer.

[0027] According to an alternative method for applying the material still at least partially to be hardened of the first and / or second finishing layer, a carrier sheet, for example a paper sheet, can be used, which is initially provided with the corresponding material by, for example, an impregnation technique, such as immersion, spraying, roller coating, and wherein the carrier sheet is then arranged on a substrate together with the material still at least partially to be hardened for forming the first and / or second finishing layer. As mentioned above, in this case, the hard particles of the first and / or second finishing layer can form part of such a treated material sheet.

[0028] Preferably, the step of forming the recess comprises at least the application of a surface structure-modifying agent, preferably a chemical agent. In particular, the method of the invention shows its advantages by means of these techniques. However, it is not excluded that the method is implemented in combination with the techniques for forming recesses known from the prior art mentioned in the introduction, such as, for example, in combination with techniques in which the surface of the second finishing layer is mechanically deformed, for example by means of a structured press element or a structuring foil.

[0029] As mentioned above, the step of forming the recesses preferably comprises at least the application of a surface structure-changing agent. Preferably, in this context, this involves a chemical agent. This method can be implemented in several specific ways, of which three specific possibilities are listed below in a non-exhaustive manner.

[0030] According to a first possibility, the method exhibits the following features: the above-mentioned surface structure-changing agent is a chemical agent, which breaks open the material of the second finishing layer. This may involve, for example, a chemical agent that has an etching effect on the respective material or has an abrasive or corrosive effect. The residual products of the opening must be removed from the surface to form the recess. The respective agent may be provided before and / or after providing the second finishing layer material, however, preferably at least after providing the second finishing layer material.

[0031] According to the second possibility, the method shows the following characteristics: the above-mentioned surface structure modifier is a chemical agent that repels the material of the above-mentioned second finishing layer, wherein it has a surface tension different from, specifically lower than, the finishing layer material. Therefore, local repulsion of the material and the formation of the notch can be achieved. The corresponding agent can be provided before and / or after the second finishing layer material is provided, however, preferably at least after the second finishing layer material is provided. Obviously, for the good effect of the chemical agent, it is necessary that the second finishing layer is still wet when the chemical agent is applied, and / or the second finishing layer is wet applied to the existing chemical agent. Preferably, the chemical agent and the finishing layer material show a surface tension difference between 5 and 15 mN / m, wherein the chemical agent has a lower surface tension. As such, the chemical agent can show the basic composition of the inkjet ink and the finishing material that must be applied in a liquid state, the basic composition of common paints or other finishing materials. The surface tension of both can be adjusted, for example, by using a small amount of surfactants, for example, silicone-containing surfactants, such as BYK333.

[0032] According to a third possibility, the method exhibits the following characteristics: the above-mentioned surface structure-modifying agent is an agent whose volume can be changed, thereby mechanically generating the surface structure. In this context, this can involve, for example, expandable, preferably heat-expandable microspheres. Preferably, microspheres consisting of a polymer surface layer encapsulating a hydrocarbon gas are applied. The surface polymer can be based on acrylonitrile. The hydrocarbon gas can be based on, for example, butane or pentane. Commercially available heat-expandable microspheres include, for example, the TEFLON® from Akzo Nobel. The respective agent may be applied before and / or after the second trimming layer material is applied, however, preferably before the second trimming layer material is applied.According to a variant, by a third possibility of the invention, protrusions may be provided in the surface instead of recesses.

[0033] It is not excluded to combine two or more of the three possibilities mentioned above for forming structures on the surface of the same plate. Thus, for example, the second possibility can be applied for forming recesses, whereas the third possibility is applied for forming protrusions. In addition, it is not excluded to combine the above-mentioned possibilities with method steps in which the substrate and / or the top layer are formed by structured extruded elements or extruded foils.

[0034] Preferably, the material of the first and / or second finishing layer comprises a UV-curing layer or consists essentially of a UV-curing lacquer, and possibly hard particles, as also described above. When in this case the second possibility for forming the recess is applied, the chemical agent is preferably an agent that repels lacquer. According to another possibility, the wear-resistant material consists essentially of a thermoplastic synthetic material, such as, for example, polyvinyl chloride (PVC), whether or not with a plasticizer, or essentially of polyurethane (PU) or essentially of polyethylene (PE) or essentially of polyethylene terephthalate (PET). In the case of PVC, benzotriazole or tolyltriazole can be used as the chemical agent.

[0035] By the same viewpoint as the first independent aspect, according to its second independent aspect, the present invention also relates to a method for manufacturing panels, wherein these panels comprise at least a substrate and a decorative top layer, wherein the above-mentioned decorative top layer comprises at least a printed pattern and a transparent or translucent protective layer formed thereon, and wherein the method comprises at least the following steps:

[0036] - a step of providing a substrate;

[0037] - a step of applying a first trimming layer for forming a first portion of the above-mentioned protective layer;

[0038] - a step of forming a recess on the surface of the first finishing layer,

[0039] - a step of applying a second trimming layer for forming a second portion of the above-mentioned protective layer;

[0040] - A step of forming recesses on the surface of said second finishing layer.

[0041] Since the protective layer is composed of at least two layers, each of which is provided with a recess on a corresponding surface, a greater depth and / or a greater aspect ratio and / or a greater variation of the recess can be achieved.

[0042] Obviously, the step of forming the recess on the surface of the first and / or second finishing layer preferably comprises applying a surface structure modifier. The method of the second aspect is of particular interest when the surface structure modifier is a chemical agent that increases the surface tension of the respective finishing layer material, for example, in the case where it involves an agent that repels paint, as within the scope of the first aspect, in the second possibility discussed above in this article. By means of the method of the second aspect, recesses with a large aspect ratio can be obtained in a simpler way. Since the protective layer is provided in several thinner partial layers, the repelling force of the chemical agent can be limited, or in other words, the amount of chemical agent that must be applied can be limited, while still achieving a relief change.

[0043] According to a particular embodiment, the step of forming recesses in the surface of the first trimming layer comprises applying a surface structure modifying agent, whereas the step of forming recesses in the surface of the second trimming layer occurs automatically due to the surface structure modifying agent previously applied to form recesses in the first trimming layer.

[0044] According to another particular embodiment, the step of forming notches on the surface of the first finishing layer and the step of forming notches on the surface of the second finishing layer comprise applying a surface structure modifier, which, however, preferably has a different composition and / or has a different action, i.e., an action according to the different possibilities mentioned herein above within the scope of the first aspect, respectively. It is clear that in this way, specific reliefs can be produced on the surface of the final board. According to variants that may or may not be combined therewith, specific effects can also be produced by hardening the individual finishing layers in different ways, for example, by further selecting the volume or drop volume of the surface structure modifier, by further selecting the layer thickness of the individual finishing layers, etc., so that they harden after different times. All these parameters make it possible to adjust the relief finely or coarsely as desired.

[0045] Preferably, the recess in the second finishing layer is formed at the position of the recess in the first finishing layer. By this technique, the maximum depth of the recess can be achieved.

[0046] Obviously the method of the second aspect may also further show features of the method of the first independent aspect. In this context, the hard particles of the first independent aspect may then be arranged in the above-mentioned first finishing layer of the second independent aspect and / or in a layer provided on the substrate before the first finishing layer and preferably containing no recesses and / or not subjected to a technique for forming recesses on its surface.

[0047] Typically, therefore, both by the first as well as by the second independent aspect of the invention, the material of the first and / or second trimming layer is preferably transparent or translucent.

[0048] It is possible that the wear-resistant material of the first and second finishing layers exhibit different gloss levels from one another. In this way, specific embodiments can be achieved according to the first as well as according to the second independent aspect. When, for example, the first finishing layer is produced glossy and the second finishing layer is produced matte or more matte, glossy recesses can additionally be produced in the matte surface, or when the first finishing layer is matte and the second finishing layer is glossy, matte recesses can additionally be produced in the glossy surface. Preferably, the gloss level of the layer produced matte is 10 or less, while the gloss level of the layer produced glossy is greater than 10, or even greater than 15 or 20, as measured according to DIN 67530. For optimal results, the difference in gloss level between the first and second finishing layers is preferably at least 10 points, as measured according to DIN 67530.

[0049] According to the invention, the top layer comprises a printed pattern extending below the first finishing layer. In this context, the recesses are preferably formed corresponding to the printed pattern. In other words, by the method of the first and / or second independent aspects, a relief is obtained on the board surface with a recess pattern corresponding to the pattern of the printed pattern. In the case of a printed pattern representing a wood structure, wood pores or wood nerves can be simulated by a recess structure located at the location of wood pores and / or next to wood nerves.

[0050] Typically, the notches obtained in the first and / or second aspects preferably involve notches that imitate the concave-convex features of natural materials, such as wood, stone, leather, textiles, etc. In the case of wood, this preferably involves imitating wood pores. According to another possibility, the notches obtained in the first and / or second aspects form a chamfer or simulated chamfer on one or more edges of the final board or in the center of the board. Such a chamfer can form, for example, a bevel or a V-shaped groove or can form an imitation cement joint.

[0051] Wherein within the scope of the first and / or second independent aspects, a surface structure modifier is provided, which is preferably implemented by a printing technique. In this way, the desired relief or pattern of the recess can be obtained in a simple, smooth and flexible manner. Thus, for example, the same printing technique can be applied for forming the printed pattern and for providing the surface structure modifier, so that possibly similar resolution can be obtained in the pattern and relief. Preferably, the printing is implemented by a digital printing technique, such as inkjet printing. However, of course, it is not excluded that a printing technique, such as offset printing or gravure printing, is implemented, for example, by a printing cylinder.

[0052] Methods in which the surface structure-modifying agent is provided by digital techniques generally have the further advantage that a large number of reliefs can be produced. Furthermore, it is possible to switch smoothly between different desired structures.

[0053] In the first as well as in the second aspect, the surface structure modifier is preferably transparent. According to a specific possibility, the surface structure modifier is colored, which is opaque or translucent. The coloring of the surface structure modifier is carried out by blending the coating or pigment in the corresponding chemical reagent. By using a colored surface structure modifier, a concavity or color change consistent with the pattern can be obtained in a smooth manner. As such, the use of a colored surface structure modifier forms a specific independent aspect of the present invention. In other words, according to its third independent aspect, the present invention relates to a method for manufacturing a board, which has the following characteristics: the board comprises at least a substrate and a decorative top layer, wherein the decorative top layer comprises at least a printed pattern and a transparent or translucent protective layer formed thereon, and wherein the method comprises at least the following steps:

[0054] - a step of providing a substrate;

[0055] - a step of applying a finishing layer for forming at least a part of the above-mentioned protective layer;

[0056] - a step of forming recesses in the surface of the first finishing layer, wherein the step includes the step of applying a surface structure modifying agent;

[0057] The invention is characterized in that the surface structure changing agent is colored.

[0058] Obviously, the present invention also relates to a board obtained according to a method having the features of one or more aspects of the present invention. In this context, this may relate, for example, to a coated board of the type comprising at least a substrate and a top layer with a printed pattern arranged on the substrate, wherein the top layer also comprises a transparent or translucent synthetic layer arranged above the printed pattern. Preferably, in the first as well as in the second aspect, the material of the first and second layers substantially forms such a transparent or translucent synthetic layer.

[0059] According to all aspects, for the substrate of the coated board of the invention, substrates comprising wood-based materials, such as MDF or HDF, can be used. According to another possibility, synthetic substrates can be used, such as substrates based on PVC (polyvinyl chloride), whether or not filled with fillers such as chalk, or substrates based on PET (polyethylene terephthalate), PU (polyurethane) or PP (polypropylene). According to another possibility, mineral-based substrates can be used, for example, gypsum fiberboard, cement fiberboard or magnesia board.

[0060] Preferably, the coated plate refers to a plate having the above-mentioned printed pattern obtained by directly or indirectly carrying out printing on the above-mentioned substrate.

[0061] It is evident that the coated plate obtained by the method having the features of the invention exhibits on the surface a relief obtained by a technique according to one or more of the above aspects herein.

[0062] According to all aspects of the invention, the top layer, and in particular the protective layer, such as the first and second finishing layers mentioned within the scope of the first and second aspects, preferably extends substantially over the entire surface of the substrate. In this way, a relief or structure can be obtained over the entire surface of the substrate. Preferably, the protective layer material will also remain present in the deeper structured parts of the protective layer. In this way, good protection of the printed pattern can be achieved.

[0063] Preferably, according to all aspects of the invention, the above-mentioned pattern relates to a printed pattern, which is preferably obtained by printing on the above-mentioned substrate, either directly or indirectly. Indirect printing can be obtained, for example, wherein printing is carried out on one or more base layers already provided on the substrate. According to the present invention, it is of course not excluded to use a pattern printed on a sheet of flexible material, which is then completely or partially provided on the substrate. This may involve, for example, a sheet of paper or a thermoplastic foil, such as a PVC foil or a PET foil. Preferably, the above-mentioned pattern is obtained by printing with an inkjet printer having one or more print heads.

[0064] Obviously, the steps mentioned in all the steps of the present invention can be implemented on larger plates, wherein the final coated plate is formed, for example, by subdividing these larger plates with a sawing machine into plates of the approximate size of the plate that has been finally coated. In order to react smoothly in sequence and to exclude excess raw materials, it is advantageous to realize the structure and / or pattern as late as possible in production. In this case, they are preferably arranged directly on the plate of the approximate or complete size of the plate that has been finally coated. In the same case, possible edge treatments can also be provided to each plate, such as milled coupling means or other profiled edge portions. Of course, it is not excluded that these profiled edge portions are provided subsequently during production. Providing structures or concave-convex shapes on each plate has the following advantages: for example, the risk of disappearance of such structures that are ground off or sawed off or removed in another way is significantly reduced, even if this involves relatively limited structures located at the edge of the plate, such as chamfers with a depth of less than 1 mm.

[0065] Preferably, according to all aspects of the invention, the position of the relief or structure is referenced to the final edge or final corner point of the coated plate, regardless of whether this edge still has to be obtained. This preferred embodiment can be realized most simply when the substrate already shows the respective final edge or corner point, however, it is not excluded that positioning is still carried out relative to the final edge or corner point to be formed even when the substrate does not show such a final edge or corner point, for example, wherein other reference means representing the position of the respective final edge or corner point are provided. Preferred embodiments of the invention make it possible, for example, to obtain symmetrical structures in a smooth manner, such as imitation tiles or imitation flooring sections with two-sided or four-sided lower edges, wherein the widths of the lower edges on opposite sides of the coated plate are preferably made equal or approximately equal.

[0066] Furthermore, it is apparent that according to all aspects of the invention preferably a structure corresponding to the above-mentioned printed pattern is obtained.

[0067] In general, it is noted that the depth of the relief mentioned in all aspects of the invention can also be limited so that in practice it concerns patterns with different glossiness.

[0068] Furthermore, it is also noted that the relief is preferably present tactilely on the surface of the final coated board. However, according to certain embodiments, it is not excluded that the individual reliefs are present inside the top layer of the coated board and are not tactile, but in fact only visibly present on the surface of the coated board. Such an embodiment can be achieved when the relief obtained by the technology of the present invention is further finished with other finishing layers.

[0069] According to all its aspects, the present invention obtains specific application when producing the board whose substrate comprises thermoplastic component and / or polyurethane.Except polyurethane, for example, PVC, PP, PE or PET can be used.Preferably, the substrate consisting of synthetic material composite material is used, i.e. the substrate comprising synthetic material and filler, such as the substrate based on filled PVC.In this article, filler can be composed of CaCO3, wood particles and / or bamboo particles.The content of filler can be between 15 and 85% by weight of the substrate.When synthetic material relates to PVC, soft PVC, semi-rigid PVC or rigid PVC can be used, which respectively comprises 15phr (parts per hundred parts of PVC resin) or higher, between 5 to 15phr or 5phr or less plasticizer content.

[0070] The technology of the present invention enables the formation of structures or concavo-convex shapes on the surface of the board without mechanical pressure and heat supply or with only limited mechanical pressure and heat supply. This possibility is of particular concern for the above-mentioned substrates comprising thermoplastic components and / or polyurethanes. In particular, for these boards, it is difficult to form structures or concavo-convex shapes in a reliable and repeatable manner by mechanical pressure and / or heat. That is, the material of such substrates is easily deformed in these cases, and the possible stretching of the substrate and the printed concavo-convex shapes located thereon is unfavorable for the correct application of the desired concavo-convex shapes. Therefore, the present invention also provides the possibility of obtaining satisfactory results using these boards. Preferably, the various methods of the present invention are implemented on the substrate in the form of a board, and therefore are not implemented on a continuous web of the substrate material. This helps to obtain the repeatability of the structure or concavo-convex shape.

[0071] As is clear from the above, according to a fourth aspect, the invention also relates to a board, wherein the board comprises at least a substrate and a decorative top layer, wherein the decorative top layer comprises at least a printed pattern and a transparent or translucent protective layer formed thereon, characterized in that the substrate comprises a thermoplastic synthetic material and / or a polyurethane, wherein the substrate further comprises 15 to 85% by weight of a filler, and the above-mentioned protective layer consists essentially of a radiation-cured, for example, UV- and / or excimer- and / or electron beam-cured lacquer layer and / or acrylate layer, wherein the protective layer is provided with recesses, which preferably correspond to the above-mentioned printed pattern. Preferably, the printed pattern consists of an imprint formed on the substrate, more particularly, by an intermediate layer of one or more base layers already provided on the substrate, preferably by a digital printing process, such as by inkjet printing, preferably by UV-cured or water-based inks.

[0072] Obviously the protective layer within the scope of the fourth aspect is basically composed of radiation-cured lacquers and / or acrylates. Therefore, this means that in essence the entire thickness of the protective layer is formed by the respective lacquers and / or acrylates, i.e. preferably from the printed pattern to the upper surface of the board.

[0073] According to the most important embodiment, the substrate of the panel according to the fourth aspect consists of highly filled PVC, preferably rigid PVC, i.e. PVC with a plasticizer content of 5 phr or less. The degree of filling is preferably greater than 50% by weight of the substrate, or even greater than 70% by weight.

[0074] Obviously, the panel according to the fourth aspect may also show the features of the panels obtained by the first, second and / or third aspect and / or preferred embodiments thereof.

[0075] Preferably, the board according to the fourth aspect is a floor panel.Preferably, the board obtained in the first, second and / or third aspect is a floor panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0076] For the purpose of better illustrating the characteristics of the invention, some preferred embodiments are described below, by way of example and without any limiting nature, with reference to the accompanying drawings, in which:

[0077] Figure 1 schematically show some steps in a method having the features of the first independent aspect mentioned in the introduction;

[0078] Figures 2 to 8 Shown respectively according to Figure 1 A section along line II-II to VIII-VIII shown in ;

[0079] Fig. 9 schematically showing some steps of a method having the features of the second independent aspect mentioned in the introduction;

[0080] Figures 10 to 14 Shown respectively according to Fig. 9 A section from line XX to XIV-XIV shown in ;

[0081] Fig.15 schematically showing some steps of a method having the features of the second independent aspect mentioned in the introduction; and

[0082] Figures 16 to 20 Shown respectively according to Fig. 9 The cross section along line XVI-XVI to XX-XX is shown in FIG. DETAILED DESCRIPTION

[0083] Figure 1 Schematically shown are some steps S1-step S8 in a method for producing a coated board 1 having the features of the first aspect of the invention. Each coated board 1 is of the type comprising at least a substrate 2, for example an MDF or HDF base board and a decorative top layer 3 arranged on the substrate 2. In this embodiment, the top layer 3 consists of a plurality of material layers 4 to 7, wherein a material layer 5 showing a pattern and provided in the form of an imprint 8 during step S2 is realized directly on the substrate 2.

[0084] In the previous step S1, one or more base layers 4 are provided on the surface of the substrate 2 on which the pattern must be printed. These can have the purpose of providing a flat lower surface and / or a uniform or quasi-uniform base color and / or an adhesive lower surface for the material layers 5 to 7 that must be provided later, such as the material layer 5 with the pattern or the first trimming layer 6 and the second trimming layer 7 for forming the protective layer 9.

[0085] Figure 2The result of step S1 is represented and shows that a possibly non-uniform surface 10 of a substrate 2 can be made flat or substantially flat by the one or more base layers 4 .

[0086] In this embodiment, in step S1, an application technique is used by one or more rollers 11. Figure 1 In step S1, other application techniques can also be applied for realizing one or more base layers 4. In addition, it is clear that for the present invention, it is not necessary to apply these base layers 4, although this may be important for the quality of the pattern. Instead of using a base layer 4 applied in liquid form, it is also possible to use a base layer 4 that comprises a material sheet, such as a paper sheet, and is arranged on the substrate 2 in a dry or almost dry form.

[0087] As mentioned above, in Figure 1 In step S2, the pattern is realized by imprinting 8 realized directly on the substrate 2 or on a base layer 4 already provided on the substrate 2. The pattern obtained is related to a wood pattern spread over the entire length of the rectangular board 1. Of course, the invention is not limited to this pattern.

[0088] In this case, for applying the printed pattern, an inkjet printer 12 with one or more heads is used. Thus, for example, a technique and a device as known from EP 1 872 959 can be used, in which, for example, a series of inkjet print heads stand upright behind and close to each other, so that the entire surface of the plate 1 can be covered with a multi-color print. Obviously, for step S2, the invention is neither limited to the inkjet printing technique nor to patterns printed directly on the substrate 2.

[0089] Figure 3 It represents the result of a print 8 carried out directly on the substrate 2 , in this case on a base layer 4 already situated on the substrate 2 .

[0090] exist Figure 1 In step S3, material of the first transparent trimming layer 6 is provided over the printed pattern of the material layer 5 to form a first portion of the protective layer 9. According to an embodiment, an application technique working by means of one or more rollers 11 is used. Figure 4 The result of step S3 is shown in cross section.

[0091] According to a preferred embodiment of the first aspect of the invention, in step S4, hard particles 13 are provided on the first trimming layer 6. According to an embodiment, a scattering treatment 14 is applied. Figure 5 The results are shown. The hard particles 13 are aluminium oxide particles having an average particle size selected such that they protrude above the actual surface 15 of the first finishing layer 6 , ie have an average particle size greater than the thickness T of the first finishing layer 6 .

[0092] In step S5 , the obtained first finishing layer 6 comprising hard particles 13 is at least partially cured, preferably by UV radiation.

[0093] In step S6 , in this case in the same way as in step S3 , a second transparent finishing layer 7 is provided. Figure 6 Indicates the result.

[0094] The material of the first finishing layer 6 and the second finishing layer 7 preferably involves a synthetic material. Preferably, this involves a transparent or translucent matte, which is preferably spread over the entire corresponding plate 1. In the embodiment, for its application, a roller 11 is shown each time. However, it is obvious that the first finishing layer 6 and the second finishing layer 7 can be arranged in any way.

[0095] As shown in step S4, the first synthetic layer contains hard particles 13. According to an embodiment, these are provided in the still wet first trim layer 6 by a scattering process 14. According to a variant, they can also be blended or woven into the synthetic material of the first trim layer 6 beforehand, or can be provided in the first trim layer 6 already provided, other than by scattering.

[0096] In step S7-step S8, a recess 16 is formed in the surface 17 of the second finishing layer 7. In step S7, above the material of the second finishing layer 7, a further imprint 18 is provided. This involves the use of a chemical agent having a surface tension significantly lower than that of the material of the second finishing layer 7, or in other words, a further imprint 18 by a repellent. The further imprint 18 is implemented by a pattern that should determine the final structure or relief of the coated board 1. In this context, the pattern only covers specific locations and is therefore preferably not spread over the entire surface of the final coated board 1. In this case, by means of such a repellent, the pattern forms a mask that provides the edge 19 of the board 1 and certain locations 20 in the surface of the board 1. In this context, the location 20 in the surface of the board 1 corresponds to the wood flower or wood vein present in the wood pattern and will result in the creation of a recess 16 present in the final board 1, which simulates a wood hole. The location located at the edge 19 of the board 1 will result in the creation of a lower edge area or chamfer, such as a V-shaped groove.

[0097] The hardening in step S8 preferably has the sole purpose of fixing or hardening the relief obtained in step S7 . Figure 8The results obtained are shown. As mentioned in the introduction, the invention, according to its first aspect, details the obtaining of a wear-resistant surface by means of a relief obtained by digitization. Since the particles 13 in the first finishing layer 6 protrude above the surface 15 of this first finishing layer 6, they are effective as anti-wear agents in the second finishing layer 7, while only influencing to a limited extent the process of forming the recesses 16 in the second finishing layer 7. According to a non-representative variant, the second finishing layer 7 may also contain hard particles, which then preferably have a smaller average particle size than the particles 13 in the first finishing layer 6.

[0098] Figure 7 Also clearly shown are the edge 19 and the position 20 of the further imprint 18 provided in step S7 .

[0099] In step S7 it is shown that the further imprint 18 determining the relief or structure is provided by means of a digital printing technique, such as by means of an inkjet printer 12. It is obviously not excluded that the further imprint 18 or the repellent is provided in another way.

[0100] Fig. 9 Some steps S1-S2-S3-S6-S7A-S7B-S8A-S8B in the method having the features of the second aspect of the present invention are schematically shown. Steps S1, S2, S3 and S6 are similar, such as by Figure 1 Steps S7A-S7B and steps S8A-S8B are similar to the steps of Figure 1 Step S7 and step S8 described in the embodiment. Fig. 9 The details of the embodiment of the invention are that the recesses 16 are formed in the first trimming layer 6 as well as in the second trimming layer 7. According to the embodiment, this each comprises applying the surface structure-modifying agent in steps S7A-S7B by a digital application technique, for example, as in the present case, by an inkjet printer 12, and at least partially hardening the first trimming layer 6 and the second trimming layer 7 in steps S8A-S8B.

[0101] Fig.10 The result obtained after providing the material of the first trimming layer 6 in step S3 is shown in cross section. Fig.11 The result is shown after a further imprint 18 has been carried out by means of a repellent in step S7A. Fig.12 The concavoconvex shapes achieved in step S7A and step S8A are shown. Fig.13The second finishing layer 7 provided in step S6 and the further imprint 18 provided thereon by the repellent in step S7B are shown. Note that the roller 11 used in step S6 is preferably of a hard type, e.g. a steel roller, so that the material of the second finishing layer 7 is provided mainly on the actual surface 15 of the first finishing layer 6 and not or less in the recesses 16 already realized in the surface 15 of the first finishing layer 6. Fig.14 The final concave-convex shape is shown. Fig.14 Obviously, through the technology of the second aspect, recesses 16 with different geometric shapes can be realized. Therefore, for example, recesses 16A and 16B with different depth-to-width ratios are realized.

[0102] Fig.15 Shows the basic correspondence Fig.10 Another variant of the embodiment of the invention, however, in which the order of step S7A and step S3 and step S7B and step S6 is changed. This variant means that the repellent is provided below the first trimming layer 6 and the second trimming layer 7 each time instead of above them. Figures 16 to 20 shows that similar results can be achieved.

[0103] When, for example, Figures 15 to 20 In an embodiment, the repellent is coloured, an embodiment being obtained by the features of the third independent aspect mentioned in the introduction.

[0104] The invention is in no way limited to the embodiments described herein above, but rather these methods and panels can be implemented according to various variants without departing from the scope of the invention.

Claims

1. A method for producing a plate, wherein: These panels (1) comprise at least a substrate (2) and a decorative top layer (3), wherein the decorative top layer (3) comprises at least a printed pattern and a transparent or translucent protective layer (9) formed thereon, and wherein the method comprises at least the following steps: - a step of providing a substrate; - a step (S3) of applying a first trimming layer (6) for forming a first portion of the above-mentioned protective layer (9); - a step (S7A-S8A) of forming a notch (16) on the surface (15) of the first trimming layer (6); - a step (S6) of applying a second finishing layer (7) for forming a second portion of the above-mentioned protective layer (9); - a step of forming a recess (16) on the surface (17) of the second finishing layer (7), Characterized in that the step of forming the recess (16) at least comprises providing a surface structure changing agent, The method further comprises the step of at least partially hardening the first finishing layer (6), the first finishing layer (6) comprising hard particles (13), and the hard particles (13) of the first finishing layer (6) protruding above the surface (15) of the first finishing layer (6).

2. The method according to claim 1, characterized in that: The recess (16) in the second trimming layer (7) is formed at the location of the recess (16) in the first trimming layer (6).

3. The method according to claim 1, characterized in that The method exhibits one or a combination of the following features: - the above-mentioned surface structure modifying agent is a characteristic of a chemical agent which opens the material of the second finishing layer (7); - the surface structure modifying agent is a chemical agent that repels the material of the second finishing layer (7), wherein the chemical agent has a different surface tension than the material of the second finishing layer (7).

4. The method according to claim 1, characterized in that: The material of the first finishing layer and / or the second finishing layer is ultraviolet curing lacquer.

5. The method according to claim 4, characterized in that The above-mentioned surface structure-changing agent is an agent that repels paint.

6. The method according to claim 2, characterized in that The method exhibits one or a combination of the following features: - the above-mentioned surface structure modifying agent is a characteristic of a chemical agent which opens the material of the second finishing layer (7); - the surface structure modifying agent is a chemical agent that repels the material of the second finishing layer (7), wherein the chemical agent has a different surface tension than the material of the second finishing layer (7).

7. The method according to claim 2, characterized in that The material of the first finishing layer and / or the second finishing layer is ultraviolet curing lacquer.

8. The method according to claim 7, characterized in that The above-mentioned surface structure-changing agent is an agent that repels paint.

9. The method according to any one of claims 1 to 8, characterized in that The materials of the first finishing layer (6) and the second finishing layer (7) exhibit different glossiness from each other.

10. The method according to any one of claims 1 to 8, characterized in that The above-mentioned notch (16) is formed according to the printing pattern.

11. The method according to any one of claims 1 to 8, wherein: The board (1) comprises at least a substrate (2) and a decorative top layer (3), wherein the decorative top layer (3) comprises at least a printed pattern and a transparent or translucent protective layer (9) formed thereon, and wherein the method comprises at least the following steps: - a step of providing a substrate (2); - a step (S3) of applying a first finishing layer (6) for forming at least a part of the above-mentioned protective layer (9); - a step of forming a recess (16) on the surface (15) of the first finishing layer (6), wherein the step includes the step of applying a surface structure modifying agent; The invention is characterized in that the surface structure changing agent is colored.

12. The method according to claim 1, characterized in that The surface structure altering agent is a chemical agent.