A method for desulfurization, decyanation and resource utilization of blast furnace gas

By using an iron/activated carbon hydrolysis catalyst to convert COS and HCN in blast furnace gas, and using NH3 for wet desulfurization, we successfully achieved the efficient removal of sulfur and cyanide in blast furnace gas, formed sulfur resources, and solved the problems of sulfur and cyanide in the existing technology. It solves the waste problem and is efficient, economical and environmentally friendly.

CN115945044BActive Publication Date: 2024-10-18INSTITUTE OF PROCESS ENGINEERING CHINESE ACADEMY OF SCIENCES
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202211687206.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-27
Publication Date
2024-10-18
Estimated Expiration
2042-12-27

AI Technical Summary

Technical Problem

The existing blast furnace gas desulfurization process cannot effectively remove cyanide, and fails to realize the resource utilization of sulfur, resulting in the waste of sulfur and cyanide.

Method used

Iron/activated carbon hydrolysis catalyst is used for hydrolysis treatment of blast furnace gas, converting COS and HCN into H2S and NH3, and further removing H2S through pressure and temperature control, using NH3 as an alkali source for wet desulfurization, and sulfur is produced through a sulfur melting kettle Turn into commercial sulfur and realize the resource utilization of sulfur and cyanide.

Benefits of technology

It achieves efficient removal of COS, H2S and HCN in blast furnace gas, with hydrolysis efficiency reaching 97.5% and 98%, reducing equipment footprint and pressure drop, and reducing pipeline corrosion and blockage, which has technical and economic advantages.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115945044B_ABST
    Figure CN115945044B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for desulfurization, decyanation and resource utilization of blast furnace gas, the method comprising the following steps: (1) the blast furnace gas is subjected to dust removal treatment and iron / activated carbon hydrolysis catalyst hydrolysis treatment in sequence to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted into H2S and CO2, and HCN is converted into NH3 and CO; (2) the converted blast furnace gas obtained in step (1) is subjected to pressure reduction treatment, heat exchange treatment and desulfurization treatment in sequence to obtain purified blast furnace gas, and the gas phase obtained by steam-water separation enters the gas pipeline network; the desulfurization liquid used in the desulfurization treatment absorbs NH3 as an external alkali source; the obtained mixed desulfurization liquid is subjected to regeneration treatment and recycled for desulfurization treatment, and the sulfur foam of the mixed desulfurization liquid is subjected to heat treatment and then cooled to obtain sulfur. The present invention uses an iron / activated carbon hydrolysis catalyst to hydrolyze and convert COS and HCN, thereby achieving the purification and resource utilization of sulfur and cyanide.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of coal gas purification and resource processing, and in particular to a method for desulfurization, decyanation and resource utilization of blast furnace coal gas. Background Art

[0002] As the largest source of air pollution in the industry, air pollution prevention and control has become the key to improving air quality. Blast furnace gas accounts for 64% of the "three gases" of steel enterprises, which is the combustible gas with the largest output. After dust removal and power generation by the residual pressure turbine power generation system (TRT), it is sent to the blast furnace hot blast furnace, steel rolling heating furnace and gas boiler as fuel.

[0003] At present, more than 90% of blast furnaces use coke. The organic sulfur in the coke enters the blast furnace gas after combustion, accounting for more than 60% of the total sulfur content in the gas, resulting in excessive sulfur content in the gas. The total amount of sulfur components in blast furnace gas is about 200-300 mg / m 3 , of which more than 90% is carbonyl sulfide (COS), H 2 S is about 5-50 mg / m 3 The remainder is carbon disulfide (CS 2 ) and other organic sulfur, about 5 mg / m 3 The concentration of hydrocyanic acid (HCN) in blast furnace gas is higher than that of sulfur, generally 150-700 mg / m 3 There are two main sources of cyanide. One is the volatilization of organic cyanide in coal and coke in the blast furnace. The other is the reduction of alkali metal compounds such as potassium and sodium in the blast furnace to form vapor, which reacts with fixed carbon and nitrogen to form potassium cyanide and sodium cyanide. Alkali metal cyanide enters the dust removal system with blast furnace gas in the form of dust, and further forms hydrocyanic acid through condensation of water vapor in the gas, and enters all links of blast furnace gas use with the gas. Therefore, it is urgent to study the desulfurization and decyanation technology of blast furnace gas.

[0004] CN 113372965A discloses a blast furnace gas desulfurization process. The blast furnace gas desulfurization process comprises the following steps: (1) passing the blast furnace gas to be treated after passing through a TRT or a pressure regulating valve group through a pretreatment reactor to remove acidic corrosive substances and form pretreated gas; a calcium-based absorbent as a pretreatment agent is arranged in the pretreatment reactor, and the temperature of the blast furnace gas to be treated is 70-120°C; (2) passing the pretreated gas through a hydrolysis tower to convert organic sulfur into hydrogen sulfide to form hydrolyzed gas; an aluminum oxide-based hydrolysis catalyst is arranged in the hydrolysis tower; (3) passing the hydrolyzed gas through a desulfurization reactor to form purified gas; the desulfurization reactor is filled with an iron oxide absorbent. However, the process does not take into account the presence of HCN in the blast furnace gas, and cannot realize the resource utilization of sulfur.

[0005] CN 114907889A discloses a highly efficient blast furnace gas dechlorination and desulfurization system and process. The system comprises: (a) at least one level of gravity dust collector; (b) at least one level of bag dust collector / electrostatic dust collector; (c) at least one level of blast furnace gas dechlorination tower; (d) at least one level of blast furnace gas catalytic tower; and (f) at least one level of desulfurization tower; a blast furnace TRT and a pressure regulating valve group are arranged in parallel between the blast furnace gas dechlorination tower and the blast furnace gas catalytic tower; the blast furnace gas catalytic tower comprises: a tower body with a catalyst inside; and a feeding component for adding a spherical catalyst to the inside of the tower body. The hydrolysis device is arranged in the low-pressure section of blast furnace gas, the device is large in scale, and the removal of HCN is not considered, and sulfur resource utilization cannot be realized at the same time.

[0006] The difficulty of desulfurization and decyanation of blast furnace gas lies in the following: the amount of blast furnace gas is large but the concentration of sulfur and cyanide is not high, which requires the desulfurization and decyanation technology to be highly efficient and have a high sulfur capacity; after wet desulfurization and decyanation, sulfur- and cyanide-containing wastewater is difficult to treat, and it is impossible to realize the resource utilization of sulfur and cyanide; the traditional dry decyanation process usually adopts the adsorption method, and the catalyst after adsorption is difficult to reuse, resulting in a waste of resources.

[0007] Therefore, in view of the shortcomings of the existing technology, it is urgently necessary to provide a method with high desulfurization and decyanation efficiency and realize resource utilization of thiocyanate. Summary of the invention

[0008] The object of the present invention is to provide a method for desulfurization, decyanation and resource utilization of blast furnace gas, wherein the blast furnace gas is hydrolyzed by an iron / activated carbon hydrolysis catalyst to convert COS and HCN, and the converted blast furnace gas is further desulfurized by pressure and temperature control. 2 S, NH 3 It continues to play a desulfurization role as an alkali source, and the purified coal gas is introduced into the coal gas network. The sulfur in the desulfurization liquid is converted into sulfur through a sulfur melting kettle, thereby achieving the purification and resource utilization of sulfur and cyanide.

[0009] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:

[0010] The present invention provides a method for desulfurization, decyanation and resource utilization of blast furnace gas, which comprises the following steps:

[0011] (1) The blast furnace gas is subjected to dust removal treatment and hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in sequence to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted into H 2 S and CO 2 , HCN is converted to NH 3 With CO;

[0012] (2) The converted blast furnace gas obtained in step (1) is subjected to pressure reduction treatment, heat exchange treatment and desulfurization treatment in sequence to obtain purified blast furnace gas, and the gas phase obtained by steam-water separation enters the gas pipeline network;

[0013] The desulfurization liquid used in the desulfurization treatment absorbs NH 3 as an external alkali source; the obtained mixed desulfurization liquid is recycled back to the desulfurization treatment after regeneration treatment, and the sulfur foam in the mixed desulfurization liquid is cooled after heat treatment to obtain sulfur.

[0014] The method provided by the present invention can simultaneously realize the hydrolysis of COS and HCN in blast furnace gas by using an iron / activated carbon hydrolysis catalyst, and the reaction formula is as follows:

[0015] COS+H 2 O=H 2 S+CO 2

[0016] HCN+H 2 O=NH 3 +CO

[0017] The obtained CO, CO 2 They are all existing components in blast furnace gas, and the amount produced is far less than the content of blast furnace gas, and will not affect the composition of blast furnace gas; H 2 S and H originally contained in the gas 2 S enters the downstream wet desulfurization tower for removal, and the NH 3 It can be used as an alkali source for wet desulfurization, further promoting H 2 The removal efficiency of S. The wet desulfurization reaction formula is as follows:

[0018] NH 3 +H 2 S=NH 4 HS

[0019] NH 4 HS+1 / 2O 2 =NH 3 +S+H 2 O

[0020] The sulfur in blast furnace gas is converted into elemental sulfur, which becomes commercial sulfur after passing through the sulfur melting system; the hydrolysis product of HCN, NH 3 It can be recycled in wet desulfurization, thereby achieving the purification and resource utilization of sulfur and cyanide.

[0021] Preferably, the dust removal process in step (1) includes gravity dust removal and / or bag dust removal.

[0022] Preferably, the dust concentration after the dust removal treatment in step (1) is less than 5 mg / m 3, for example, 4 mg / m 3 , 3mg / m 3 , 2mg / m 3 , 1mg / m 3 or 0.5 mg / m 3 , but not limited to the listed values, other unlisted values ​​within the numerical range are also applicable.

[0023] Preferably, in the iron / activated carbon hydrolysis catalyst of step (1), iron is the active component and activated carbon is the carrier. The iron loading is 4-6wt% of the total amount of the iron / activated carbon hydrolysis catalyst, for example, it can be 4wt%, 4.5wt%, 5wt%, 5.5wt% or 6wt%, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0024] The iron / activated carbon hydrolysis catalyst has a stable and efficient hydrolysis effect. Compared with the existing commercially available hydrolysis catalysts, the iron / activated carbon hydrolysis catalyst can ensure a service life of more than 1 year, and the hydrolysis efficiency can reach more than 90%.

[0025] Preferably, the temperature of the blast furnace gas in step (1) is 100-150°C, for example, 100°C, 110°C, 120°C, 130°C or 150°C, but is not limited to the listed values, and other values ​​not listed within the numerical range are also applicable.

[0026] Preferably, the pressure of the blast furnace gas in step (1) is 240-250 kPa, for example, 240 kPa, 242 kPa, 245 kPa, 248 kPa or 250 kPa, but is not limited to the listed values, and other values ​​not listed within the numerical range are also applicable.

[0027] Preferably, the hydrolysis treatment in step (1) is carried out in a hydrolysis tower.

[0028] Preferably, the hydrolysis tower is a fixed bed.

[0029] The heat source of the fixed bed is the temperature of blast furnace gas, and no additional heat source is needed for heating. The pressure comes from the pressure of blast furnace gas.

[0030] Preferably, the pressure drop of the hydrolysis tower is less than 3 kPa, for example, it may be 2.8 kPa, 2.5 kPa, 2.2 kPa, 2 kPa or 1 kPa, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0031] Preferably, the concentration of COS in the converted blast furnace gas in step (1) is less than 10 mg / m 3 , for example, 9 mg / m 3 , 8mg / m3 , 7mg / m 3 , 6mg / m 3 or 5 mg / m 3 , but not limited to the listed values, other unlisted values ​​within the numerical range are also applicable.

[0032] Preferably, the concentration of HCN in the converted blast furnace gas in step (1) is less than 10 mg / m 3 , for example, 9 mg / m 3 , 8mg / m 3 , 7mg / m 3 , 6mg / m 3 or 5 mg / m 3 , but not limited to the listed values, other unlisted values ​​within the numerical range are also applicable.

[0033] Preferably, in step (1), the CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas, for example, it can be 0.5‰, 0.45‰, 0.4‰, 0.35‰ or 0.3‰, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0034] Among the hydrolysis products of COS and HCN, CO and CO 2 It is an original component of blast furnace gas and its concentration is relatively low, so it does not affect the composition of blast furnace gas.

[0035] Preferably, the pressure endpoint of the pressure reduction treatment in step (2) is 19.8-20.2 kPa, for example, it can be 19.8 kPa, 19.9 kPa, 20 kPa, 20.1 kPa or 20.2 kPa, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0036] Preferably, the pressure reduction treatment in step (2) is carried out in a residual pressure turbine power generation device.

[0037] Preferably, the temperature end point of the heat exchange treatment in step (2) is 35-40°C, for example, it can be 35°C, 36°C, 37°C, 38°C or 40°C, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0038] Preferably, the heat exchange treatment in step (2) is carried out in a heat exchange device.

[0039] Preferably, the desulfurization treatment step in step (2) comprises: countercurrent contact reaction between the converted blast furnace gas after the heat exchange treatment and the desulfurization liquid.

[0040] Preferably, after the desulfurization treatment in step (2), 2S concentration <10 mg / m 3 , for example, 9 mg / m 3 , 8mg / m 3 , 7mg / m 3 , 6mg / m 3 or 5 mg / m 3 , but not limited to the listed values, other unlisted values ​​within the numerical range are also applicable.

[0041] Preferably, the desulfurization liquid comprises an aqueous solution of a cobalt phthalocyanine desulfurization agent.

[0042] Preferably, the cobalt phthalocyanine desulfurizing agent includes a PDS desulfurizing agent.

[0043] Preferably, the desulfurization liquid absorbs NH 3 The final pH value is 8.2-8.6, for example, 8.2, 8.3, 8.4, 8.5 or 8.6, but is not limited to the listed values, and other values ​​not listed within the numerical range are also applicable.

[0044] The NH 3 As an external alkali source entering the desulfurization liquid, it can increase the pH of the desulfurization liquid and enhance H 2 The absorption of S plays a positive role in improving the efficiency of wet desulfurization.

[0045] Preferably, the mixed desulfurization liquid is desulfurization liquid, NH 3 and HS - of mixed liquid.

[0046] Preferably, the desulfurization treatment in step (2) is carried out in a desulfurization tower.

[0047] Preferably, the desulfurization tower is provided with a ball ring.

[0048] The blast furnace gas contacts the desulfurization liquid on the ball ring, and the H in the blast furnace gas 2 S is absorbed into the desulfurization liquid and converted into HS - .

[0049] Preferably, the pressure drop of the desulfurization tower is less than 1 kPa, for example, it can be 0.9 kPa, 0.8 kPa, 0.7 kPa, 0.6 kPa or 0.5 kPa, but it is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0050] Preferably, the steam-water separation in step (2) is carried out in a steam-water separator.

[0051] Preferably, the regeneration process is carried out in a regeneration tank.

[0052] Preferably, the mixed desulfurization liquid is discharged to the regeneration tank through the bottom of the desulfurization tower.

[0053] Preferably, the regeneration process is to blow compressed air into the regeneration tank.

[0054] The regeneration tank is filled with compressed air through an air injector into the mixed desulfurized liquid, and the O in the air 2 It can react with the mixed desulfurization liquid, and the regenerated desulfurization liquid enters the desulfurization tower through a pump for recycling.

[0055] Preferably, the heat treatment is carried out in a molten sulfur kettle.

[0056] Preferably, the molten sulfur kettle is provided with a jacket, and the jacket is used for injecting steam to provide a heat source.

[0057] Preferably, the temperature of the heat treatment is 80-120°C, for example, 80°C, 90°C, 100°C, 110°C or 120°C, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0058] Preferably, the end point of the heat treatment is to collapse the sulfur foam to form molten sulfur.

[0059] Preferably, the molten sulfur is cooled to obtain sulfur.

[0060] The sulfur foam generated by the regeneration treatment of the mixed desulfurization liquid floats on the top of the mixed desulfurization liquid due to its low density, and enters the sulfur melting kettle through overflow. The sulfur foam breaks into molten sulfur and settles into the lower layer of the sulfur melting kettle. After the bottom of the sulfur melting kettle is cooled, the molten sulfur is converted into sulfur.

[0061] As a preferred technical solution of the method of the present invention, the method comprises the following steps:

[0062] (1) Blast furnace gas at 100-150° C. and 240-250 kPa is subjected to gravity dust removal and / or bag dust removal treatment in sequence, and hydrolyzed in a hydrolysis tower using an iron / activated carbon hydrolysis catalyst to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted into H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is less than 10 mg / m 3 ; The concentration of HCN is less than 10 mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0063] The dust concentration after dust removal is less than 5 mg / m 3; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 4-6wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0064] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 19.8-20.2 kPa in a residual pressure turbine power generation device, heat exchange treatment to 35-40° C. in a heat exchange device, and countercurrent contact reaction with a desulfurization liquid in a desulfurization tower to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator enters the gas pipeline network;

[0065] After desulfurization treatment, H 2 S concentration <10 mg / m 3 The desulfurization liquid used in the desulfurization treatment absorbs NH 3 The pH value after adding the alkali source is 8.2-8.6; the obtained mixed desulfurization liquid is discharged to the regeneration tank through the bottom of the desulfurization tower, and compressed air is blown into the regeneration tank and then recycled for desulfurization treatment. The sulfur foam of the mixed desulfurization liquid is subjected to steam heat treatment at 80-120°C in a sulfur melting kettle until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0066] Compared with the prior art, the present invention has the following beneficial effects:

[0067] (1) The method provided by the present invention uses an iron / activated carbon hydrolysis catalyst to convert COS and HCN in the same tower, which reduces the floor space and promotes the possibility of promoting the process in an existing blast furnace. The converted blast furnace gas is further degassed with H 2 S, while the hydrolysis product NH 3 As an alkali source, it continues to play a desulfurization role. The sulfur in the desulfurization liquid is converted into sulfur through the sulfur melting kettle, thereby achieving the purification and resource utilization of sulfur and cyanide, effectively slowing down the corrosion and blockage of the pipeline. The hydrolysis efficiency of COS can reach 97.5%, and the hydrolysis efficiency of HCN can reach 98%. In addition, the pressure drop of the hydrolysis tower and the desulfurization tower is no more than 1.25% of the blast furnace gas pressure, which will not affect the residual pressure power generation efficiency.

[0068] (2) The present invention can realize the reduction of COS and H in blast furnace gas. 2 The efficient removal of S and HCN has the characteristics of small footprint, simple equipment, small pressure drop, high desulfurization accuracy and little impact on the original equipment. The overall technical and economic advantages are very obvious. BRIEF DESCRIPTION OF THE DRAWINGS

[0069] Figure 1 It is a schematic diagram of the structure of the device for desulfurization, decyanation and resource utilization of blast furnace gas provided by the present invention;

[0070] Among them: 1, hydrolysis tower; 2, waste pressure turbine power generation device; 3, heat exchange device; 4, desulfurization tower; 5, steam-water separator; 6, regeneration tank; 7, molten sulfur kettle. DETAILED DESCRIPTION

[0071] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.

[0072] In the following examples, the initial COS concentration of blast furnace gas is 200 mg / m 3 , the initial HCN concentration is 250 mg / m 3 .

[0073] Example 1

[0074] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The structural schematic diagram of the device for desulfurization, decyanation and resource utilization of blast furnace gas is as follows: Figure 1 As shown, the method comprises the following steps:

[0075] (1) The blast furnace gas at 120° C. and 245 kPa is subjected to gravity dust removal and bag dust removal treatment in sequence, and is subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower 1 to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted to H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is 5 mg / m 3 ; The concentration of HCN is 5mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0076] The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 5wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0077] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 20 kPa in a residual pressure turbine power generation device 2, heat exchange treatment to 37° C. in a heat exchange device 3, and countercurrent contact reaction with a PDS desulfurization liquid in a desulfurization tower 4 to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator 5 enters the gas pipeline network;

[0078] After desulfurization treatment, H 2 The concentration of S is 5 mg / m 3The PDS desulfurization liquid used in the desulfurization treatment absorbs NH 3 The pH value after adding an external alkali source is 8.4; the obtained mixed desulfurization liquid is discharged to the regeneration tank 6 through the bottom of the desulfurization tower 4, and compressed air is blown into the regeneration tank 6 and then circulated back for desulfurization treatment. The sulfur foam in the mixed desulfurization liquid is subjected to steam heat treatment at 100°C in the sulfur melting kettle 7 until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0079] The hydrolysis efficiency of COS is 97.5%, and the hydrolysis efficiency of HCN is 98%.

[0080] Example 2

[0081] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The structural schematic diagram of the device for desulfurization, decyanation and resource utilization of blast furnace gas is as follows: Figure 1 As shown, the method comprises the following steps:

[0082] (1) The blast furnace gas at 110° C. and 248 kPa is subjected to gravity dust removal and bag dust removal treatment in sequence, and is subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower 1 to obtain converted blast furnace gas; COS in the obtained converted blast furnace gas is converted to H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is 6 mg / m 3 ; The concentration of HCN is 7mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0083] The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 4.5wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0084] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 19.9 kPa in a residual pressure turbine power generation device 2, heat exchange treatment to 38° C. in a heat exchange device 3, and countercurrent contact reaction with a PDS desulfurization liquid in a desulfurization tower 4 to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator 5 enters the gas pipeline network;

[0085] After desulfurization treatment, H 2 The concentration of S is 6 mg / m 3 The PDS desulfurization liquid used in the desulfurization treatment absorbs NH 3The pH value after adding the alkali source is 8.3; the obtained mixed desulfurization liquid is discharged to the regeneration tank 6 through the bottom of the desulfurization tower 4, and compressed air is blown into the regeneration tank 6 and then circulated back for desulfurization treatment. The sulfur foam of the mixed desulfurization liquid is subjected to steam heat treatment at 90°C in the sulfur melting kettle 7 until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0086] The hydrolysis efficiency of COS is 97%, and the hydrolysis efficiency of HCN is 97.2%.

[0087] Example 3

[0088] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The structural schematic diagram of the device for desulfurization, decyanation and resource utilization of blast furnace gas is as follows: Figure 1 As shown, the method comprises the following steps:

[0089] (1) The blast furnace gas at 130° C. and 242 kPa is subjected to gravity dust removal and bag dust removal treatment in sequence, and is subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower 1 to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted to H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is 7 mg / m 3 ; The concentration of HCN is 6mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0090] The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 5.5wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0091] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 20.1 kPa in a residual pressure turbine power generation device 2, heat exchange treatment to 36° C. in a heat exchange device 3, and countercurrent contact reaction with a PDS desulfurization liquid in a desulfurization tower 4 to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator 5 enters the gas pipeline network;

[0092] After desulfurization treatment, H 2 The concentration of S is 7 mg / m 3 The PDS desulfurization liquid used in the desulfurization treatment absorbs NH 3The pH value after adding an external alkali source is 8.4; the obtained mixed desulfurization liquid is discharged to the regeneration tank 6 through the bottom of the desulfurization tower 4, and compressed air is blown into the regeneration tank 6 and then circulated back for desulfurization treatment. The sulfur foam in the mixed desulfurization liquid is subjected to steam heat treatment at 100°C in the sulfur melting kettle 7 until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0093] The hydrolysis efficiency of COS is 96.5%, and the hydrolysis efficiency of HCN is 97.6%.

[0094] Example 4

[0095] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The structural schematic diagram of the device for desulfurization, decyanation and resource utilization of blast furnace gas is as follows: Figure 1 As shown, the method comprises the following steps:

[0096] (1) The blast furnace gas at 100°C and 250 kPa is subjected to gravity dust removal and bag dust removal treatment in sequence, and is subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower 1 to obtain converted blast furnace gas; COS in the obtained converted blast furnace gas is converted to H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is 8 mg / m 3 ; The concentration of HCN is 8mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0097] The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 6wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0098] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 19.8 kPa in a residual pressure turbine power generation device 2, heat exchange treatment to 40° C. in a heat exchange device 3, and countercurrent contact reaction with a PDS desulfurization liquid in a desulfurization tower 4 to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator 5 enters the gas pipeline network;

[0099] After desulfurization treatment, H 2 The concentration of S is 8 mg / m 3 The PDS desulfurization liquid used in the desulfurization treatment absorbs NH 3The pH value after adding the alkali source is 8.2; the obtained mixed desulfurization liquid is discharged to the regeneration tank 6 through the bottom of the desulfurization tower 4, and compressed air is blown into the regeneration tank 6 and then circulated back for desulfurization treatment. The sulfur foam of the mixed desulfurization liquid is subjected to steam heat treatment at 80°C in the sulfur melting kettle 7 until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0100] The hydrolysis efficiency of COS is 96%, and the hydrolysis efficiency of HCN is 96.8%.

[0101] Example 5

[0102] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The structural schematic diagram of the device for desulfurization, decyanation and resource utilization of blast furnace gas is as follows: Figure 1 As shown, the method comprises the following steps:

[0103] (1) The blast furnace gas at 150° C. and 240 kPa is subjected to gravity dust removal and bag dust removal treatment in sequence, and is subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower 1 to obtain converted blast furnace gas; COS in the obtained converted blast furnace gas is converted to H 2 S and CO 2 , HCN is converted to NH 3 and CO; the concentration of COS is 9 mg / m 3 ; The concentration of HCN is 9mg / m 3 ; The CO 2 The concentration of CO is ≤ 0.5‰ of the concentration of blast furnace gas;

[0104] The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 4wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa;

[0105] (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 20.2 kPa in a residual pressure turbine power generation device 2, heat exchange treatment to 35° C. in a heat exchange device 3, and countercurrent contact reaction with a PDS desulfurization liquid in a desulfurization tower 4 to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator 5 enters the gas pipeline network;

[0106] After desulfurization treatment, H 2 The concentration of S is 9 mg / m 3 The PDS desulfurization liquid used in the desulfurization treatment absorbs NH 3The pH value after adding the alkali source is 8.6; the obtained mixed desulfurization liquid is discharged to the regeneration tank 6 through the bottom of the desulfurization tower 4, and compressed air is blown into the regeneration tank 6 and then circulated back for desulfurization treatment. The sulfur foam of the mixed desulfurization liquid is subjected to steam heat treatment at 120°C in the sulfur melting kettle 7 until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

[0107] The hydrolysis efficiency of COS is 95.5%, and the hydrolysis efficiency of HCN is 96.4%.

[0108] Example 6

[0109] This embodiment provides a method for desulfurization, decyanation and resource recovery of blast furnace gas. The difference from Example 1 is that, except for adjusting the iron loading amount in step (1) to 2 wt% of the total amount of iron / activated carbon hydrolysis catalyst, the rest is the same as Example 1.

[0110] The content of the active iron component in the iron / activated carbon hydrolysis catalyst is too low, resulting in a decrease in the hydrolysis efficiency. The hydrolysis efficiency of COS is 65%, and the hydrolysis efficiency of HCN is 50%.

[0111] Example 7

[0112] This embodiment provides a method for desulfurization, decyanation and resource recovery of blast furnace gas. The difference from Example 1 is that, except for adjusting the iron loading amount in step (1) to 8wt% of the total amount of iron / activated carbon hydrolysis catalyst, the rest is the same as Example 1.

[0113] If the content of the active iron component in the iron / activated carbon hydrolysis catalyst is too high, the hydrolysis efficiency will not continue to increase, but it will cause a waste of resources. The hydrolysis efficiency of COS is 97%, and the hydrolysis efficiency of HCN is 98%.

[0114] Example 8

[0115] This embodiment provides a method for desulfurization, decyanation and resource utilization of blast furnace gas. The difference from Example 1 is that, except for replacing the PDS desulfurization liquid isoflow rate in step (2) with HPF desulfurization liquid and introducing sodium carbonate as an alkali source, the rest is the same as Example 1.

[0116] Using the HPF desulfurization liquid, H 2 The removal efficiency of S was 80%.

[0117] Comparative Example 1

[0118] This comparative example provides a method for desulfurization, decyanation and resource recovery of blast furnace gas, which is different from Example 1 in that, in addition to replacing the mass of the iron / activated carbon hydrolysis catalyst in step (1) with γ-Al 2 O 3 Except for this, the rest are the same as in Example 1.

[0119] Using γ-Al 2 O 3 As a hydrolysis catalyst, it only has the removal efficiency of COS, and the catalyst is prone to sulfation, which greatly reduces the catalyst life. The hydrolysis efficiency of COS is 90%, and HCN cannot be effectively hydrolyzed.

[0120] In summary, the method provided by the present invention uses an iron / activated carbon hydrolysis catalyst to convert COS and HCN in the same tower, which reduces the floor space and promotes the possibility of promoting the process in the built blast furnace; the converted blast furnace gas further removes H 2 S, while the hydrolysis product NH 3 As an alkali source, it continues to play a desulfurization role. The sulfur in the desulfurization liquid is converted into sulfur through the sulfur melting kettle, thereby achieving the purification and resource utilization of sulfur and cyanide, effectively slowing down the corrosion and blockage of the pipeline. The hydrolysis efficiency of COS can reach 97.5%, and the hydrolysis efficiency of HCN can reach 98%. In addition, the pressure drop of the hydrolysis tower and the desulfurization tower is no more than 1.25% of the blast furnace gas pressure, which will not affect the residual pressure power generation efficiency.

[0121] The present invention can realize the reduction of COS and H in blast furnace gas. 2 The efficient removal of S and HCN has the characteristics of small footprint, simple equipment, small pressure drop, high desulfurization accuracy and little impact on the original equipment. The overall technical and economic advantages are very obvious.

[0122] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention are within the protection scope and disclosure scope of the present invention.

Claims

1. A method for desulfurization, decyanation and resource utilization of blast furnace gas, characterized in that: The method comprises the following steps: (1) Blast furnace gas is subjected to dust removal treatment and hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in sequence to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted into H2S and CO2, and HCN is converted into NH3 and CO; (2) The converted blast furnace gas obtained in step (1) is subjected to pressure reduction treatment, heat exchange treatment and desulfurization treatment in sequence to obtain purified blast furnace gas, and the gas phase obtained by steam-water separation enters the gas pipeline network; In step (1), the iron / activated carbon hydrolysis catalyst is an active component, the activated carbon is a carrier, and the iron loading is 4-6wt% of the total amount of the iron / activated carbon hydrolysis catalyst; The desulfurization liquid used in the desulfurization treatment absorbs NH3 as an external alkali source; the obtained mixed desulfurization liquid is recycled and reused in the desulfurization treatment after regeneration treatment, and the sulfur foam in the mixed desulfurization liquid is cooled after heat treatment to obtain sulfur.

2. The method according to claim 1, characterized in that The dust removal process in step (1) includes gravity dust removal and / or bag dust removal.

3. The method according to claim 1, characterized in that The dust concentration after the dust removal treatment in step (1) is less than 5 mg / m 3 .

4. The method according to claim 1, characterized in that: The temperature of the blast furnace gas in step (1) is 100-150°C.

5. The method according to claim 1, characterized in that The pressure of the blast furnace gas in step (1) is 240-250 kPa.

6. The method according to claim 1, characterized in that The hydrolysis treatment in step (1) is carried out in a hydrolysis tower.

7. The method according to claim 6, characterized in that The hydrolysis tower is a fixed bed.

8. The method according to claim 6, characterized in that The pressure drop of the hydrolysis tower is less than 3 kPa.

9. The method according to claim 1, characterized in that: The concentration of COS in the converted blast furnace gas in step (1) is less than 10 mg / m 3 .

10. The method according to claim 1, characterized in that The concentration of HCN in the converted blast furnace gas in step (1) is less than 10 mg / m 3 .

11. The method according to claim 1, characterized in that: The concentration of CO2 and CO in step (1) is ≤ 0.5‰ of the concentration of blast furnace gas.

12. The method according to claim 1, characterized in that The pressure endpoint of the pressure reduction treatment in step (2) is 19.8-20.2 kPa.

13. The method according to claim 1, characterized in that The pressure reduction treatment in step (2) is carried out in a residual pressure turbine power generation device.

14. The method according to claim 1, characterized in that The end temperature of the heat exchange treatment in step (2) is 35-40°C.

15. The method according to claim 1, characterized in that The heat exchange treatment in step (2) is carried out in a heat exchange device.

16. The method according to claim 1, characterized in that The desulfurization step in step (2) includes: countercurrent contact reaction between the converted blast furnace gas after the heat exchange treatment and the desulfurization liquid.

17. The method according to claim 1, characterized in that The concentration of H2S after desulfurization treatment in step (2) is less than 10 mg / m 3 .

18. The method according to claim 16, characterized in that The desulfurization liquid includes an aqueous solution of a cobalt phthalocyanine desulfurization agent.

19. The method according to claim 16, characterized in that The pH value of the desulfurization liquid after absorbing NH3 is 8.2-8.

6.

20. The method according to claim 1, characterized in that The desulfurization treatment in step (2) is carried out in a desulfurization tower.

21. The method according to claim 20, characterized in that The desulfurization tower is provided with a ball ring.

22. The method according to claim 20, characterized in that The pressure drop of the desulfurization tower is less than 1 kPa.

23. The method according to claim 1, characterized in that The steam-water separation in step (2) is carried out in a steam-water separator.

24. The method according to claim 1, characterized in that The regeneration process is performed in a regeneration tank.

25. The method according to claim 20, characterized in that The mixed desulfurization liquid is discharged to the regeneration tank through the bottom of the desulfurization tower.

26. The method according to claim 1, characterized in that The regeneration process is to blow compressed air into the regeneration tank.

27. The method according to claim 1, characterized in that The heat treatment is carried out in a molten sulfur kettle.

28. The method according to claim 27, characterized in that The molten sulfur kettle is provided with a jacket, and the jacket is used for injecting steam to provide a heat source.

29. The method according to claim 1, characterized in that The temperature of the heat treatment is 80-120°C.

30. The method according to claim 1, characterized in that The end point of the heat treatment is to collapse the sulfur foam to form molten sulfur.

31. The method according to claim 30, characterized in that The molten sulfur is cooled to obtain sulfur.

32. The method according to any one of claims 1 to 31, characterized in that The method comprises the following steps: (1) Blast furnace gas at 100-150° C. and 240-250 kPa is subjected to gravity dust removal and / or bag dust removal treatment in sequence, and then subjected to hydrolysis treatment with an iron / activated carbon hydrolysis catalyst in a hydrolysis tower to obtain converted blast furnace gas; COS in the converted blast furnace gas is converted into H2S and CO2, and HCN is converted into NH3 and CO; the concentration of COS is less than 10 mg / m 3 ; The concentration of HCN is less than 10 mg / m 3 ; The concentration of CO2 and CO is ≤ 0.5‰ of the concentration of blast furnace gas; The dust concentration after dust removal is less than 5 mg / m 3 ; The iron / activated carbon hydrolysis catalyst is an active component of iron, activated carbon is a carrier, and the iron loading is 4-6wt% of the total amount of the iron / activated carbon hydrolysis catalyst; the hydrolysis tower is a fixed bed; the pressure drop of the hydrolysis tower is <3kPa; (2) The converted blast furnace gas obtained in step (1) is successively subjected to pressure reduction treatment to 19.8-20.2 kPa in a residual pressure turbine power generation device, heat exchange treatment to 35-40° C. in a heat exchange device, and countercurrent contact reaction with a desulfurization liquid in a desulfurization tower to perform desulfurization treatment to obtain purified blast furnace gas, and the gas phase obtained after steam-water separation in a steam-water separator enters the gas pipeline network; The concentration of H2S after desulfurization treatment is less than 10 mg / m 3 ; The pH value of the desulfurization liquid used in the desulfurization treatment is 8.2-8.6 after absorbing NH3 as an external alkali source; the obtained mixed desulfurization liquid is discharged to the regeneration tank through the bottom of the desulfurization tower, and compressed air is blown into the regeneration tank and then recycled for desulfurization treatment. The sulfur foam of the mixed desulfurization liquid is subjected to steam heat treatment at 80-120°C in a sulfur melting kettle until the sulfur foam bursts to form molten sulfur, and sulfur is obtained after cooling.

Citation Information

Patent Citations

  • Blast furnace gas desulfurization process

    CN113372965A

  • Method for hydrolysis-oxidation coupled purification of HCN

    CN103463972A

  • Blast furnace gas fine desulfurization method and fine desulfurization system

    CN111592917A

  • Wet purification device and process for total sulfur removal of blast furnace gas

    CN111826214A