Progressive cold heading mechanism, cold heading die, cold heading equipment and cold heading process

By using a progressive cold heading mechanism and cold heading process, and employing a cold heading punch with a gradually decreasing clearance groove volume for multiple cold heading operations, the problems of cracking of already-headed workpieces and low production efficiency are solved, thus achieving efficient mass production.

CN116117057BActive Publication Date: 2025-10-28DONGGUAN DARUI NEW ENERGY TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310156355.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-02-21
Publication Date
2025-10-28
Estimated Expiration
2043-02-21

AI Technical Summary

Technical Problem

Existing cold heading equipment is prone to causing cracks in the headed workpiece during cold heading operations, and the CNC milling thinning process is inefficient, especially in mass production.

Method used

The progressive cold heading mechanism is adopted, which uses cold heading punches with gradually decreasing clearance groove volume to cold head the workpiece, providing additional deformation space, avoiding cracking, and making the cold heading area completely flat through multiple cold heading operations.

Benefits of technology

It effectively avoids the problem of cracking in upset workpieces, while improving production efficiency. It is suitable for mass production and is more efficient than CNC milling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116117057B_ABST
    Figure CN116117057B_ABST
Patent Text Reader

Abstract

This invention relates to the field of machining technology, specifically disclosing a progressive cold heading mechanism, a cold heading die, a cold heading equipment, and a cold heading process. The progressive cold heading mechanism includes: a base for placing the workpiece to be cold-headed; and a punch assembly comprising a plurality of cold heading punches, each cold heading punch having a relief groove at its bottom, the volume of which gradually decreases. Each cold heading punch is configured to sequentially cold-head the workpiece after being driven. The progressive cold heading mechanism, cold heading die, cold heading equipment, and cold heading process provided by this invention effectively solve the problem of cracking of already cold-headed workpieces caused by existing cold heading equipment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of machining technology, and in particular to a progressive cold heading mechanism, cold heading mold, cold heading equipment, and cold heading process. Background Technology

[0002] Cold heading is a common machining process. See also Figure 1 The cold heading equipment includes a base 2 for placing the workpiece 1 to be headed and a cold heading punch 3 for pressing the workpiece 1 downwards.

[0003] When it is necessary to perform cold heading on the workpiece 1, the cold heading punch 3 is driven to press the workpiece 1 downward. The cold heading area 101 corresponding to the workpiece 1 and the cold heading punch 3 will be recessed downward, thereby thinning the cold heading area 101, and the workpiece 1 becomes the already headed workpiece.

[0004] During the cold heading process, the material in the cold heading area 101 is not reduced, but is pushed by the cold heading punch 3 in various directions of the cold heading area 101 (specifically including the front, back, left, right and bottom of the cold heading area 101).

[0005] When the concave dimension of the cold heading region 101 is small, the material of the cold heading region 101 can be smoothly extruded outward, so the headed workpiece will not crack; however, when the concave dimension of the cold heading region 101 is large, the material of the cold heading region 101 is difficult to be smoothly extruded outward instantly, so the headed workpiece is prone to cracking.

[0006] To prevent cracking of the upset workpiece, when the concave dimension of the cold-forged area 101 is large, it is currently common to thin the cold-forged area 101 by CNC milling. However, CNC equipment can only perform thinning operations on one workpiece at a time, and each milling operation takes a long time, resulting in low production efficiency. This problem is particularly evident in mass production.

[0007] Therefore, existing cold heading equipment needs to be improved to solve the problem that it easily causes the headed workpiece to crack.

[0008] The information disclosed in this background section is included only to enhance the understanding of the context of this disclosure, and therefore may contain information that does not constitute prior art known to those skilled in the art. Summary of the Invention

[0009] One objective of this invention is to provide a progressive cold heading mechanism, cold heading mold, cold heading equipment, and cold heading process, which can effectively solve the problem that existing cold heading equipment easily causes cracks in the headed workpiece.

[0010] To achieve the above objectives, in a first aspect, the present invention provides a progressive cold heading mechanism, comprising:

[0011] A base for placing the workpiece to be upset;

[0012] A punch assembly, comprising a plurality of cold heading punches, wherein the bottom of each cold heading punch is provided with a relief groove, and the volume of the relief groove on each cold heading punch gradually decreases.

[0013] Each of the cold heading punches is configured to perform cold heading on the workpiece to be headed sequentially after being driven.

[0014] Optionally, the bottom surface of the last cold heading punch is a planar structure.

[0015] Optionally, the wall of the relief groove is a smooth curved surface.

[0016] Optionally, the cross-sectional shape of the smooth surface in the vertical plane is a circular arc or an elliptical arc.

[0017] Optionally, the depth of the relief groove on each of the cold heading punches gradually decreases.

[0018] Optionally, the clearance groove is located at the middle of the bottom surface of the cold heading punch.

[0019] Optionally, the cold heading punch is cylindrical in shape.

[0020] In a second aspect, a cold heading die is provided, comprising an upper die assembly, a lower die assembly, and the aforementioned progressive cold heading mechanism;

[0021] Each cold heading punch of the progressive cold heading mechanism is detachably connected to the bottom of the upper die assembly;

[0022] The base of the progressive cold heading mechanism is mounted on top of the lower die assembly.

[0023] Thirdly, a cold heading device is provided, including a drive mechanism and the aforementioned cold heading die.

[0024] The drive end of the drive mechanism is connected to the upper mold assembly, driving the upper mold assembly to move up and down.

[0025] Fourthly, a cold heading process is provided, applicable to the progressive cold heading mechanism, comprising: sequentially using each of the cold heading punches with progressively decreasing volumes of the relief groove to cold head the workpiece to be headed.

[0026] The beneficial effects of this invention are: it provides a progressive cold heading mechanism, a cold heading die, cold heading equipment, and a cold heading process.

[0027] When the cold heading punch moves downwards to cold heading the cold heading area of ​​the workpiece, the material on the cold heading area can be squeezed not only to the front, back, left, right and bottom of the cold heading area, but also into the relief groove because the bottom of the cold heading punch has a relief groove. That is, the relief groove provides a certain deformation space for the workpiece to be headed, avoiding cracking due to insufficient deformation space in the cold heading area. However, this operation will cause the cold heading area to bulge upwards at the position corresponding to the relief groove, that is, the cold heading area is not flat enough. Therefore, several more cold heading operations are required.

[0028] Furthermore, when cold heading begins, the workpiece requires the most deformation space. Therefore, a cold heading punch with a larger relief groove volume is used first for cold heading. As cold heading continues, the deformation space required by the workpiece gradually decreases. Therefore, cold heading punches with progressively smaller relief groove volumes are used for cold heading until finally a cold heading punch with a flat bottom surface is used to completely flatten the cold heading area.

[0029] Therefore, the progressive cold heading mechanism, cold heading mold, cold heading equipment, and cold heading process provided by the present invention can effectively solve the problem that existing cold heading equipment easily causes the already-headed workpieces to crack. Attached Figure Description

[0030] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0031] Figure 1 A schematic diagram of existing cold heading equipment provided for the background art;

[0032] Figure 2 This is a schematic diagram of the cold heading equipment provided in the embodiment.

[0033] In the picture:

[0034] 1. Workpiece to be upset; 101. Cold heading area;

[0035] 2. Base;

[0036] 3. Cold heading punch; 301, clearance groove;

[0037] 4. Upper mold assembly;

[0038] 5. Lower mold assembly;

[0039] 6. Drive mechanism;

[0040] 7. Conveying mechanism. Detailed Implementation

[0041] To make the objectives, features, and advantages of this invention more apparent and understandable, the technical solutions of the embodiments of this invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the embodiments described below are only some embodiments of this invention, and not all embodiments. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.

[0042] In the description of this invention, it should be understood that when a component is considered to be "connected" to another component, it can be directly connected to the other component or there may be an intermediate component present simultaneously. When a component is considered to be "set" on another component, it can be directly set on the other component or there may be an intermediate component present simultaneously.

[0043] Furthermore, terms such as “long,” “short,” “inner,” and “outer” indicate orientation or positional relationships based on the orientation or positional relationships shown in the accompanying drawings. They are used only for the purpose of describing the present invention and are not intended to indicate or imply that the device or component referred to must have this specific orientation or operate in a specific orientational configuration. Therefore, they should not be construed as limitations of the present invention.

[0044] The present invention will now be described in detail with reference to the specific embodiments shown in the accompanying drawings. However, these embodiments do not limit the present invention, and any structural, methodological, or functional modifications made by those skilled in the art based on these embodiments are included within the scope of protection of the present invention.

[0045] This invention provides a progressive cold heading mechanism, cold heading mold, cold heading equipment, and cold heading process, which is applicable to applications where metal sheets awaiting heading are thinned to obtain the already-headed workpiece. It can effectively solve the problem that existing cold heading equipment is prone to workpiece cracking during cold heading operations.

[0046] Example 1

[0047] See Figure 2 This embodiment provides a cold heading device, including a drive mechanism 6 and a cold heading die. The cold heading die includes an upper die assembly 4, a lower die assembly 5, and a progressive cold heading mechanism. The drive end of the drive mechanism 6 is connected to the upper die assembly 4, driving the upper die assembly 4 to move up and down to perform die closing and punching or die opening and part removal operations. Optionally, the drive mechanism 6 can be a cylinder, a hydraulic cylinder, a motor screw assembly, or a robotic arm, etc., and this embodiment does not limit this.

[0048] In this embodiment, the progressive cold heading mechanism includes a punch assembly and a base 2 mounted on top of the lower die assembly 5. The base 2 is used to place the workpiece 1 to be headed. The punch assembly includes a plurality of cold heading punches 3, wherein each cold heading punch 3 can be detachably connected to the bottom of the upper die assembly 4. Each cold heading punch 3 has a relief groove 301 at its bottom, and the volume of the relief groove 301 on each cold heading punch 3 is different.

[0049] In this embodiment, each cold heading punch 3 is installed simultaneously on the upper die assembly 4 in sequence (the larger relief groove 301 volume is in front, and the smaller relief groove 301 volume is in the back). Then, a conveyor belt or other conveying mechanism 7 drives the lower die assembly 5 to move sequentially to below each cold heading punch 3, thereby realizing the sequential cold heading operation of each cold heading punch 3. In some other embodiments, the upper die assembly 4 can also be connected to only one cold heading punch 3 in the same group of punch assemblies at a time. After the previous cold heading punch 3 is disassembled, the next cold heading punch 3 is installed into the upper die assembly 4, and then the next cold heading operation is performed.

[0050] Furthermore, during cold heading, each cold heading punch 3 performs the cold heading operation in a fixed order. Specifically, the cold heading punch 3 with a larger volume of the clearance groove 301 is cold heading first, and the cold heading punch 3 with a smaller volume of the clearance groove 301 is cold heading later. That is, when each cold heading punch 3 is arranged in the order of cold heading operation, the volume of the clearance groove 301 on each cold heading punch 3 gradually decreases.

[0051] In this embodiment, when the driving mechanism 6 drives the cold heading punch 3 downward to cold heading the cold heading area 101 of the workpiece 1 to be cold heading through the upper die assembly 4, since the bottom of the cold heading punch 3 has a relief groove 301, the material on the cold heading area 101 can not only be squeezed to the front, back, left, right and bottom of the cold heading area 101, but also squeezed into the relief groove 301. That is, the relief groove 301 provides a certain deformation space for the workpiece 1 to be cold heading, avoiding the situation where the deformation space of the cold heading area 101 is insufficient and cracking occurs. However, such an operation will cause the cold heading area 101 to bulge upward at the position corresponding to the relief groove 301. That is, the cold heading area 101 is not flat enough. Therefore, several cold headings are required in the future.

[0052] Furthermore, when cold heading begins, the workpiece 1 to be headed requires the most deformation space. Therefore, a cold heading punch 3 with a larger relief groove 301 volume is used first for cold heading. As cold heading continues, the deformation space required by the workpiece 1 to be headed gradually decreases. Therefore, a cold heading punch 3 with a gradually decreasing relief groove 301 volume is used for cold heading until finally a cold heading punch 3 with a flat bottom surface is used to completely head the cold heading area 101.

[0053] It is understood that the progressive cold heading mechanism, cold heading mold, and cold heading equipment provided in this embodiment can thin the workpiece to be headed into a headed workpiece through multiple cold heading processes. This can avoid cracking problems and is more efficient than CNC milling. It is suitable for mass production and has great promotional value.

[0054] Optionally, the groove wall of the relief groove 301 is a smooth curved surface. For example, the cross-sectional shape of the smooth curved surface in the vertical plane is a circular arc or an elliptical arc. The smooth curved surface does not have obvious sharp corners, and the circular arc or elliptical arc matches the deformation shape of the cold heading region 101 under pressure, which helps to avoid damage to the cold heading region 101.

[0055] In this embodiment, as an optional method to reduce volume, the groove depth of the relief groove 301 on each of the cold heading punches 3 is gradually reduced, and / or the groove opening size of the relief groove 301 on each of the cold heading punches 3 is gradually reduced.

[0056] In this embodiment, the relief groove 301 is located in the middle of the bottom surface of the cold heading punch 3. Furthermore, the cold heading punch 3 is cylindrical in shape, which is beneficial to the uniform force on the workpiece 1 to be upset and makes the cold heading area 101 of the workpiece 1 to be upset protrude toward the relief groove 301.

[0057] The progressive cold heading mechanism, cold heading mold, and cold heading equipment provided in this embodiment have the following advantages: the material on the cold heading area 101 can be squeezed into the relief groove 301, avoiding the situation where the deformation space of the cold heading area 101 is insufficient and cracking occurs. Then, the cold heading area 101 is flattened by multiple cold heading processes, so that the workpiece 1 to be headed is completely headed thin into a headed workpiece. This not only avoids the cracking problem, but is also more efficient than CNC milling, suitable for mass production, and has great promotional value.

[0058] Example 2

[0059] This embodiment provides a cold heading process, applicable to the progressive cold heading mechanism in Embodiment 1, and has the same beneficial effects.

[0060] In this embodiment, the cold heading process includes:

[0061] S10: Place the workpiece to be upset on the base;

[0062] S20: The workpiece to be cold-forged is cold-forged sequentially using cold-forging punches with progressively decreasing volumes of relief grooves.

[0063] Specifically, first use the cold heading punch with the largest relief groove volume to cold heading the workpiece, then use the cold heading punch with the second largest relief groove volume to cold heading the workpiece, and so on, until finally use the last cold heading punch with a flat bottom surface to cold heading the workpiece. This will flatten the cold heading area on the workpiece without cracking.

[0064] It should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This way of describing the specification is only for clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.

[0065] The detailed descriptions listed above are merely specific descriptions of feasible embodiments of the present invention, and are not intended to limit the scope of protection of the present invention. All equivalent embodiments or modifications made without departing from the spirit of the present invention should be included within the scope of protection of the present invention.

Claims

1. A progressive cold heading mechanism, characterized in that, include: A base for placing the workpiece to be upset; A punch assembly, comprising a plurality of cold heading punches, wherein the bottom of each cold heading punch is provided with a relief groove, and the volume of the relief groove on each cold heading punch gradually decreases. Each of the cold heading punches is configured to perform cold heading on the workpiece to be headed sequentially after being driven; The bottom surface of the last cold heading punch is a planar structure; The wall of the relief groove is a smooth curved surface; The cross-sectional shape of the smooth curved surface in the vertical plane is a circular arc or an elliptical arc; The depth of the relief groove on each of the aforementioned cold heading punches gradually decreases; The clearance groove is located in the middle of the bottom surface of the cold heading punch.

2. The progressive cold heading mechanism according to claim 1, characterized in that, The cold heading punch is cylindrical in shape.

3. A cold heading die, characterized in that, Includes an upper die assembly, a lower die assembly, and a progressive cold heading mechanism as described in any one of claims 1 to 2; Each cold heading punch of the progressive cold heading mechanism is detachably connected to the bottom of the upper die assembly; The base of the progressive cold heading mechanism is mounted on top of the lower die assembly.

4. A cold heading device, characterized in that, Includes a drive mechanism and the cold heading die as described in claim 3. The drive end of the drive mechanism is connected to the upper mold assembly, driving the upper mold assembly to move up and down.

5. A cold heading process, applicable to the progressive cold heading mechanism as described in any one of claims 1 to 2, characterized in that, include: The workpiece to be cold-forged is then cold-forged sequentially using cold-forging punches with progressively smaller relief groove volumes.

Citation Information

Patent Citations

  • Cold heading manufacturing process of copper ring for automobile generator

    CN102489643A

  • ET and RT type soft magnetic ferrite core cracking preventing molding die and working method thereof

    CN109016090A

  • Bar arc die

    CN209288093U

  • Progressive cold heading mechanism, cold heading die and cold heading equipment

    CN219443301U