Polycrystalline silicon reduction silicon core component, reduction equipment and silicon core component heating method
By inverting the "U"-shaped silicon core component structure and multi-point contact design, combined with temperature measurement control, the problem of slow temperature rise of the silicon core component is solved, rapid and uniform temperature rise in the polysilicon reduction furnace is achieved, and production efficiency and products are improved. quality.
Patent Information
- Application Number
- CN202310179520.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2043-02-28
AI Technical Summary
In existing polysilicon reduction furnaces, it is difficult to achieve rapid heating and temperature uniformity of silicon core components, resulting in long heating times in the furnace and affecting production efficiency and product quality.
Adopting an inverted "U"-shaped silicon core component structure, through multi-point contact between the beam silicon core and the first and second silicon cores and increasing the contact area, the breakdown time is shortened, the contact resistance is reduced, a conduction loop is quickly formed, and the The temperature measuring device detects the temperature in real time and controls the voltage and current to ensure that the silicon core components heat up evenly.
It achieves rapid and uniform heating of silicon core components, shortens the heating time in the furnace, improves polysilicon production efficiency and product consistency, and ensures the effectiveness of the reduction reaction.
Smart Images

Figure HDA0004102047300000011 
Figure HDA0004102047300000021 
Figure HDA0004102047300000022
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of polysilicon production for photovoltaic industry, and in particular to a polysilicon reduction silicon core component, reduction equipment and a silicon core component heating method. Background Art
[0002] The main raw material used in photovoltaic modules is monocrystalline silicon, which is prepared by purifying polycrystalline silicon. The production of polycrystalline silicon is particularly important. Among the existing manufacturers, most use reduction furnaces to produce polycrystalline silicon. In the reduction reaction, the raw materials are hydrogen and trichlorosilane gas phase mixture entering the reduction furnace, and the temperature in the furnace is controlled to make the two react. The silicon element in trichlorosilane is reduced by hydrogen. The reduced elemental silicon is silicon powder, which adheres to the surface of the silicon core in the furnace. As the amount of silicon attached to the surface of the silicon core increases, the diameter of the silicon rod increases, forming a silicon rod, that is, a polycrystalline silicon rod. After being crushed, it forms polycrystalline silicon material and is provided to downstream monocrystalline silicon manufacturers.
[0003] Before the reduction reaction begins, it is first necessary to preheat the temperature in the furnace to the process requirements, such as 1000°C and above. The increase in the temperature in the furnace is achieved by heating up multiple groups of silicon core components. Therefore, the rapid heating of the silicon core components to the process requirements can shorten the heating time in the furnace, and it is also necessary to consider that the various parts of the silicon core components must reach a uniform temperature during the rapid heating process. In the prior art, most silicon core components are implemented in a U-shaped overlap manner, and the overlap methods between adjacent silicon cores are different. It is necessary for the present invention to propose a different overlap method and a reduction furnace prepared using the overlap structure, that is, a method for heating the temperature in the furnace. Summary of the invention
[0004] In view of this, it is necessary to provide a polysilicon reduction silicon core component, including a first silicon core, a second silicon core, and a cross-beam silicon core, and the cross-sectional area of each of the square silicon cores is square, the first silicon core and the second silicon core are arranged vertically, the cross-beam silicon core is overlapped on the top between the first silicon core and the second silicon core, forming an inverted "U" silicon core component, the lower ends of the first silicon core and the second silicon core are used to connect with the electrode, the upper part of the first silicon core is provided with a first connection surface, the upper part of the second silicon core is provided with a second connection surface, two inner cavities are opened at both ends of the cross-beam silicon core, the inner cavity has a circular bottom, and is used to insert the upper end connection surface of the first silicon core and the second silicon core, and the first connection surface of the first silicon core is provided with a second connection surface. The joint surface is connected to the cross-beam silicon core to form a first joint, and the second connection surface of the second silicon core is connected to the cross-beam silicon core to form a second joint, the first connection surface and the second connection surface have circular bottom edges, and the diameters of the circular bottom edges of the first connection surface and the second connection surface are equal to the side length of the square silicon core, and four fan-shaped planes are also arranged outside the circular bottom edge of the first connection surface for surface-to-surface contact with the cross-beam silicon core, and four fan-shaped contact surfaces are formed between the lower surface of the cross-beam silicon core and the four fan-shaped planes, and at the same time, the circular bottom edge of the first connection surface forms four tangent points with the fan-shaped plane, and the four tangent points also form the same four contact points with the bottom of the inner cavity of the cross-beam silicon core.
[0005] A polysilicon reduction device comprises a furnace bottom, a bell jar, a plurality of silicon core components, and a temperature measuring device. The bell jar and the furnace bottom are combined to form a reduction chamber. A hydrogen and trichlorosilane mixed gas is introduced into the reduction chamber from bottom to top. The plurality of silicon core components are vertically arranged inside the bell jar. The bottom of the silicon core component is connected to an external electrode. The temperature measuring device comprises a plurality of temperature measuring heads. At least one temperature measuring head is a first temperature measuring head. The temperature measuring point of the first temperature measuring head is directly facing the overlapping corner of the first silicon core and the crossbeam silicon core or the second silicon core and the crossbeam silicon core of a silicon core group, and is used to detect the temperature of the silicon core at the corner. A second temperature measuring head is arranged below the first temperature measuring head to detect the temperature of the vertical part of the second silicon core.
[0006] A method for heating a polysilicon reduction silicon core component, comprising the following steps:
[0007] Replace the reduction furnace with hydrogen to fill the reduction chamber with hydrogen for protection;
[0008] Apply voltage to the silicon core, and simultaneously detect the silicon core temperature T1 at the overlapping corners of a group of U-shaped silicon cores and the temperature T2 at the vertical part of the vertical silicon core;
[0009] When T1>T2, the applied voltage remains unchanged;
[0010] When the error between T1 and T2 is less than 20°C, a large resistance conduction loop has been formed, the current increases, and the temperature continues to be detected;
[0011] When T1≈T2=(1050~1100℃), a mixed gas of hydrogen and trichlorosilane begins to flow into the furnace and the reduction reaction begins.
[0012] Beneficial effects: The overlapping method of adjacent silicon cores of the present invention sets multiple point contacts and increases multiple fan-shaped contact surfaces, shortens the breakdown time by point contact, reduces the contact resistance by increasing the contact surface, and accelerates the rapid formation of the current loop. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 is a schematic diagram of a silicon core assembly of the present invention;
[0014] Figure 2 for Figure 1 Bottom view of
[0015] Figure 3 for Figure 2 Sectional view of AA in the middle;
[0016] Figure 4 , 5 Schematic diagrams of the ends of the silicon core of the beam in two implementation modes.
[0017] Figure 6 Schematic diagram of the structure of the first silicon core.
[0018] Figure 7 for Figure 6 Top view of the .
[0019] Figure 8 for Figure 6 A partial diagram of .
[0020] Figure 9-11 , 12-13 are schematic diagrams of the prior art.
[0021] Fig.14 A schematic diagram of the restoration device.
[0022] Figure 15-18 They are curve diagrams of voltage-time, current-time, T1-time, and T2-time in one implementation manner respectively.
[0023] In the figure: a first silicon core 10, a cone 11, a first contact point 111, a fan-shaped plane 12, a second contact point 121, a second silicon core 20, a beam silicon core 30, a conical inner cavity 31, a right-angle step 32, a corner bulge 321, an arc surface 33, an arc-shaped corner protrusion 34, a furnace bottom 40, a bell jar 50, a first temperature measuring head 61, and a first temperature measuring head 62. DETAILED DESCRIPTION
[0024] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0025] Please see Figure 1 , 2 A polysilicon reduction silicon core component comprises a first silicon core 10, a second silicon core 20, and a cross-beam silicon core 30, and the cross-sectional areas of the square silicon cores are all square. The first silicon core 10 and the second silicon core 20 are arranged vertically, and the cross-beam silicon core 30 is overlapped at the top between the first silicon core 10 and the second silicon core 20 to form an inverted "U"-shaped silicon core component. The lower ends of the first silicon core 10 and the second silicon core 20 are used to connect with electrodes. The upper part of the first silicon core 10 is provided with a first connection surface, and the upper part of the second silicon core 20 is provided with a second connection surface. Two inner cavities are opened at both ends of the cross-beam silicon core 30, and the inner cavity has a circular bottom for inserting the upper end connection surfaces of the first silicon core 10 and the second silicon core 20, and the first connection surface of the first silicon core 10 It is connected to the crossbeam silicon core 30 to form a first connection, and the second connection surface of the second silicon core 20 is connected to the crossbeam silicon core 30 to form a second connection, the first connection surface and the second connection surface have a circular bottom edge, the diameter of the circular bottom edge of the first connection surface and the second connection surface is equal to the side length of the square silicon core, and four fan-shaped planes 12 are also arranged outside the circular bottom edge of the first connection surface for surface-to-surface contact with the crossbeam silicon core 30, and four fan-shaped contact surfaces are formed between the lower surface of the crossbeam silicon core 30 and the four fan-shaped planes 12, and at the same time, the circular bottom edge of the first connection surface forms four tangent points with the fan-shaped plane 12, and the four tangent points also form the same four contact points (i.e., second contact points 121) with the bottom of the inner cavity of the crossbeam silicon core 30.
[0026] It is well known to those skilled in the art that at the point contact position, the contact area approaches 0 and the contact resistance is theoretically very large. Therefore, the present solution sets four point contact positions (the four sector planes 12 and the four contact points are formed by processing the upper part of the square first silicon core 10 and the second silicon core 20, as shown in FIG. Figure 6 When voltage is applied, the contact resistance is the largest here, the heat is the most serious, and it is the weakest position for high voltage breakdown. It is most likely to break down here. After breakdown, the resistance here drops instantly, forming a conduction loop with a large resistance. Therefore, the setting of four contact points can shorten the time for the silicon material at the connection to break down, thereby shortening the time for the loop to form. In addition, the original design of the same industry only uses surface-to-surface contact (truncated cone surface-to-surface contact, such as Figure 9-11), the temperature rises slowly, and the temperature at the contact surface is balanced, there is no weak point of breakdown, resulting in a longer circuit formation time. In the process of applying voltage, this scheme, compared with the scheme of simply using surface-to-surface contact, artificially increases the location of voltage breakdown, thereby further reducing the breakdown voltage and shortening the time required for breakdown.
[0027] Furthermore, the first connecting surface and the second connecting surface are conical surfaces, and conical inner cavities 31 for inserting the cone 11 are opened at both ends of the cross-beam silicon core 30. The height of the cone and the height of the conical inner cavity 31 are the same as the cross-sectional side length of the cross-beam silicon core 30, so that conical surface contact and end point contact are formed between the first silicon core 10 and the cross-beam silicon core 30, and between the second silicon core 20 and the cross-beam silicon core 30.
[0028] This is the first contact point 111. Since the height is equal, the end of the cone is in point contact with the tip of the conical inner cavity 31. This point contact also has the function of the second contact point 121 mentioned above. On the basis of the above scheme, another point contact position is added, thereby further increasing the breakdown position points, increasing the breakdown probability, and shortening the breakdown time. In addition, this scheme designs the contact surface to be conical, and the conical surface and the four fan-shaped planes 12 together form a contact surface. Compared with the use of a conical contact surface or a truncated cone contact surface alone, on this basis, the scheme increases the contact area, so that the contact area between the first silicon core 10 and the crossbeam silicon core 30, and the second silicon core 20 and the crossbeam silicon core 30 is increased from the original S1 to S1+4*Sfan. The contact area of the four fan-shaped planes 12 is increased, the total contact surface is increased, the resistance of the connection can be reduced, and the current is facilitated to pass quickly, so that the three silicon cores are quickly connected to a conductor and the temperature rises quickly.
[0029] In order to ensure that the three silicon cores have the same unit surface area and the same heating surface area when the power is subsequently turned on, the cross-sectional shape and side length of the three silicon cores are the same. For example, the cross-sectional area of the silicon core is a square, and the side length is 15 mm, that is, a square silicon core. After the three silicon cores of the above structure are overlapped, an inverted "U"-shaped silicon core assembly is formed. The shape of the outer surface of adjacent silicon cores after connection is the same, that is, except for the connected conical surface and four fan-shaped planes 12 inside, the outer surface is a regular rectangular parallelepiped without redundant and protruding heterogeneous structures. Compared with the structure using cylindrical silicon cores spliced together (such as Fig.12 , 13) At the overlap, there will be extra arc-shaped corner protrusions 34 (as can be seen in the top view). In the subsequent reduction process, the silicon single substance generated by the reaction will adhere to the surface of the silicon core. The protruding arc-shaped corners and other special-shaped structures here will cause the surface shape of the silicon core matrix to be different (cauliflower head, bulge). The thickness or shape of the grown silicon rod here will also be different from that at other positions. The process requires that the grown silicon rods have the same diameter and good appearance consistency, especially at the overlap corners, which should form a smoothly transitioned arc structure instead of a protruding cauliflower head or other corner bulge 321 structure. In this solution, a right-angle structure is formed at the corner without any protruding special structure. The surface of the silicon core assembly formed by the overlap is butt-jointed to form a plane without any protruding bosses or tips. Therefore, the silicon core matrix structure of the grown silicon rod is regular, and the silicon rod grown on this basis is also uniform in thickness, with a smooth transition on the surface and no special shape. It is precisely because of the square silicon core that four fan-shaped surfaces can be formed, and a cylindrical shape cannot be formed.
[0030] Furthermore, the upper surfaces of the two ends of the crossbeam silicon core 30 are arc-shaped surfaces. Originally, there were right-angle steps 32. The sharp right angles hindered the descent of trichlorosilane, which easily caused the reaction to generate silicon single substance accumulation, and also formed a corner bulge 321 at this position (as shown in the figure). Therefore, after the arc chamfer, an arc surface 33 is formed here, and there is no step. When trichlorosilane descends, it slides down along the arc surface, with little blocking force, avoiding the formation of corner bulges.
[0031] A polysilicon reduction device comprises a furnace bottom 40, a bell jar 50, a plurality of silicon core assemblies, and a temperature measuring device. The bell jar 50 and the furnace bottom 40 are combined to form a reduction chamber. A mixture of hydrogen and trichlorosilane is introduced into the reduction chamber from bottom to top. The plurality of silicon core assemblies are vertically arranged inside the bell jar 50. The bottom of the silicon core assembly is connected to an external electrode. The temperature measuring device comprises a plurality of temperature measuring heads. At least one temperature measuring head is a first temperature measuring head 61. The temperature measuring point of the first temperature measuring head 61 is directly opposite (the understanding of directly opposite is not limited to being aligned within the vertical height) a corner where a first silicon core 10 of a silicon core group and a crossbeam silicon core 30 or a second silicon core 20 and a crossbeam silicon core 30 are overlapped, and is used to detect the temperature of the silicon core at the corner. The second temperature measuring head 62 is arranged below the first temperature measuring head 61, and is used to detect the temperature of the vertical part of the first silicon core 10 or the second silicon core 20.
[0032] During the heating process of the furnace body, the reactants hydrogen and trichlorosilane are not introduced, and the furnace is protected by gas. Since the turning position where the crossbeam silicon core 30 and the vertical silicon core overlap is the position with the largest connection resistance, the heating here is the most serious during the heating process of the furnace body. Although a larger conical surface and fan-shaped plane 12 are used for contact, due to the existence of five contact points, the temperature is higher than other positions of the silicon core. Therefore, during the heating process of the furnace body, the heating is the most serious in the early stage, and the temperature is much higher than other positions. Only when this position is broken down, the circuit is turned on, the resistance decreases, the current flow increases, and the current rises rapidly. The flow of large current causes other positions of the silicon core to heat up rapidly. The current flowing through the three silicon cores gradually tends to be the same, and the calorific value also tends to be the same. Then the temperature of the two temperature measurement points gradually tends to be the same. At this time, the three silicon cores of the U-shaped silicon core are steadily heated to the temperature required by the process, and hydrogen and trichlorosilane are introduced into the furnace to start the reduction reaction. In this scheme, two temperature measuring devices are used to detect the temperature at different positions respectively. The temperature measured by the first temperature measuring head 61 is T1, and the temperature measured by the second temperature measuring head 62 is T2. When T1>T2, the applied voltage is kept unchanged, there is no breakdown between adjacent silicon cores, and the conduction loop has not been formed; when the measured temperature difference between T1 and T2 is less than 20°C, it indicates that the adjacent silicon cores have been broken down, a large resistance conduction loop has been formed, and the current is in a large amount of flow and is constantly increasing. At this time, the temperature continues to be detected; when T1=T2=(1050~1100°C), the inside of each silicon core has been completely broken down and the process temperature has been reached, hydrogen and trichlorosilane are introduced into the furnace to start the reduction reaction.
[0033] Furthermore, the temperature measuring device is an infrared thermometer, and a window is provided on the side wall of the furnace body for infrared thermometer detection.
[0034] A method for heating a polysilicon reduction silicon core component, comprising the following steps:
[0035] Replace the reduction furnace with hydrogen to fill the reduction chamber with hydrogen for protection;
[0036] Apply voltage to the silicon core, and simultaneously detect the silicon core temperature T1 at the overlapping corners of a group of U-shaped silicon cores and the temperature T2 at the vertical part of the vertical silicon core;
[0037] When T1>T2, the applied voltage remains unchanged;
[0038] When the temperature difference between T1 and T2 is less than 20℃, a large resistance conduction loop has been formed, the current increases, and the temperature continues to be detected;
[0039] When T1≈T2=(1050~1100℃), the inside of each silicon core is fully conductive, and a mixed gas of hydrogen and trichlorosilane begins to flow into the furnace to start the reduction reaction.
[0040] Further, when the error between T1 and T2 is less than 20°C, the current increases instantaneously, and then the rate of current increase gradually decreases until the current reaches the process requirement of 1050-1100°C, the current does not change, and it is maintained continuously, the voltage does not change, and the output is constant. Since T1 and T2 are relatively close, it means that the inflection point has been broken down and connected, the resistance drops a lot instantly, the current increases instantaneously, and the position of the inflection point just broken down, the current is very large, the heat is serious, and the high temperature accelerates the internal breakdown of the nearby silicon core semiconductor silicon material, and then the current increases faster. The two complement each other and promote each other. Therefore, in a short period of time just after the breakdown, the current increases very quickly, accompanied by the connection of the adjacent silicon cores at the inflection point, the overall resistance of the U-shaped silicon core decreases, and the current continues to increase, but because the overall resistance of the U-shaped silicon core tends to steadily decrease, the current increases steadily, and the rate of increase decreases until all three silicon cores are broken down, the overall resistance of the U-shaped silicon core does not change, the voltage remains unchanged, and the current does not change, reaching the process requirement value. At this time, the temperature in the furnace meets the requirements and the material reaction begins.
[0041] In the heating method, the voltage applied in the furnace and the current curves flowing through the U-shaped silicon core, as well as the curves of T1 and T2 are as follows: Figure 15-18 .
[0042] It can be seen from the curve that at the beginning, the voltage applied is 6000V, the current gradually increases, and the temperature at the inflection point gradually increases. At the t1 time node, the temperature at the inflection point reaches the tolerance limit, and T1 reaches the highest, for example, 1800℃. The inflection point is first broken down, the resistance drops, the voltage drops, the current increases instantly, and a conduction loop is formed. The voltage continues to be applied, and the current continues to increase. At this time, the silicon material inside the three silicon cores is broken down to form a conductor, and the voltage and resistance continue to decrease. There is no local heat at T1, and it steadily decreases. The current continues to increase, and the temperature of T2 increases, indicating that the current flows smoothly inside each silicon core and rises steadily. At the t2 node, all three silicon cores are broken down to form a conductor, and the resistance no longer changes. The voltage and current tend to be stable, and the temperature in the furnace reaches the process requirement of 1100℃.
[0043] Depending on the different furnace capacities and the different qualities of different batches of silicon core raw materials, the t1 and t2 node times may vary. Usually, when 48 pairs of U-shaped silicon core components are used, the time from applying voltage to the current reaching a stable value and the temperature reaching a stable value, that is, the time to reach t2 is about 30-45 minutes, and the time to reach t1 varies from 10-20 minutes.
[0044] In one embodiment, the vertical silicon core is a square silicon core with a size of 15mm*15mm*3000mm, a side length of 15mm, and a length of 3000mm. The size of the crossbeam silicon core 30 is 15mm*15mm*(200-300mm). It can be calculated that the contact area of the first connection or the second connection is 588.51mm2 The calculation process is as follows:
[0045] The surface area of S contact surface = S cone + 4S fan = 395.37 + 4*48.29 = 588.51 mm 2
[0046] S cone = conical surface area = πrL = π*7.5mm*16.78mm = 395.37mm 2
[0047] S fan = S square - S circle = 15*15mm - π*r*r = 48.29mm 2
[0048] R is the height of the cone, which is also the side length of the silicon core, R = 15mm; r is the radius of the bottom of the cone, r = 7.5mm, and L is the generatrix length of the cone;
[0049] Through calculation, we know that the area of the four sectors is 4*48.29, which is the contact area added in the original design.
[0050] It can be seen from the above that the conical contact surface used alone has an area only equal to the surface area of the S cone, and does not have five contact points. In the present invention, the contact area is increased by 4S fans, and five contact points are added to form a breakdown weak point and shorten the silicon core heating time. In the prior art, since most manufacturers focus on the constant temperature state after the furnace temperature reaches the process requirements, they record the time of the reduction reaction from the constant temperature, while ignoring the control of the heating time. Whether the silicon core temperature is stable and continues to meet the process requirements after the temperature has been heated, the present invention controls the temperature in the furnace by measuring the silicon core temperature. Usually the industry detects the temperature inside the furnace to reflect whether the temperature inside the furnace meets the process requirements. In fact, it is most reasonable to detect the temperature of the silicon core to reflect the temperature inside the furnace. During the reduction reaction, the mixed gas can only react at the temperature required by the process, and the temperature of the silicon core happens to be the required temperature. In addition, the reaction occurs on the surface of the silicon core. Only when the surface of the silicon core reaches the temperature can silicon single substance be generated and attached to the surface of the silicon core. If the temperature in other spaces cannot reach the required temperature, the reaction will not produce effective silicon single substance, but other by-products, which cannot attach and grow on the silicon core. Therefore, controlling the temperature of the silicon core is the most accurate measure for controlling the temperature inside the furnace.
[0051] What is disclosed above is only a preferred embodiment of the present invention, which certainly cannot be used to limit the scope of rights of the present invention. A person skilled in the art can understand that all or part of the processes of the above embodiments and equivalent changes made according to the claims of the present invention still fall within the scope of the invention.
Claims
1. A polysilicon reduction silicon core component, Features: The invention comprises a square silicon core including a first silicon core, a second silicon core and a cross-beam silicon core, and the cross-sectional areas of the square silicon cores are all square. The first silicon core and the second silicon core are arranged vertically, and the cross-beam silicon core is overlapped at the top between the first silicon core and the second silicon core to form an inverted "U" silicon core assembly. The lower ends of the first silicon core and the second silicon core are used to connect with the electrode. The upper part of the first silicon core is provided with a first connecting surface, and the upper part of the second silicon core is provided with a second connecting surface. Two inner cavities are provided at both ends of the cross-beam silicon core, and the inner cavity has a circular bottom for inserting the upper end connecting surfaces of the first silicon core and the second silicon core. The first connecting surface of the first silicon core is connected to the cross-beam silicon core to form a first connection, and the second connecting surface of the second silicon core is connected to the cross-beam silicon core to form a second connection. The first connecting surface and the second connecting surface have a circular bottom edge, and the first connecting surface is connected to the cross-beam silicon core to form a second connection. The diameter of the circular bottom edge of the connection surface and the second connection surface is equal to the side length of the square silicon core. Four fan-shaped planes are also arranged outside the circular bottom edge of the first connection surface for surface-to-surface contact with the crossbeam silicon core, and four fan-shaped contact surfaces are formed between the lower surface of the crossbeam silicon core and the four fan-shaped planes. At the same time, the circular bottom edge of the first connection surface and the fan-shaped planes form four tangent points, and the four tangent points also form the same four contact points with the bottom of the inner cavity of the crossbeam silicon core. The first connection surface and the second connection surface are conical surfaces, and conical inner cavities for inserting cones are provided at both ends of the crossbeam silicon core. The height of the cone and the height of the conical inner cavity are the same as the side length of the cross-section of the crossbeam silicon core, so that conical surface contact and end point contact are formed between the first silicon core and the crossbeam silicon core, and between the second silicon core and the crossbeam silicon core.
2. The polysilicon reduction silicon core assembly according to claim 1, Features: The upper surfaces of the two ends of the crossbeam silicon core are arc-shaped surfaces.
3. A polysilicon reduction device, Features: The invention comprises a furnace bottom, a bell jar, a plurality of silicon core components and a temperature measuring device. The bell jar and the furnace bottom are combined to form a reduction chamber. A mixed gas of hydrogen and trichlorosilane is introduced into the reduction chamber from bottom to top. A plurality of silicon core components are vertically arranged inside the bell jar. The bottom of the silicon core component is connected to an external electrode. The temperature measuring device comprises a plurality of temperature measuring heads. At least one temperature measuring head is a first temperature measuring head. The temperature measuring point of the first temperature measuring head is directly facing the overlapping corner of the first silicon core and the crossbeam silicon core or the second silicon core and the crossbeam silicon core of a silicon core group, and is used to detect the temperature of the silicon core at the corner. A second temperature measuring head is arranged below the first temperature measuring head to detect the temperature of the vertical part of the second silicon core. The silicon core component is the polysilicon reduction silicon core component according to any one of claims 1 or 2.
4. The polysilicon reduction device according to claim 3, Features: The temperature measuring device is an infrared thermometer, and a window is provided on the side wall of the furnace body for infrared thermometer detection.
5. A method for heating a polycrystalline silicon reduction silicon core assembly, wherein the silicon core assembly is the polycrystalline silicon reduction silicon core assembly according to any one of claims 1 or 2, Features The following steps are involved: Replace the reduction furnace with hydrogen to fill the reduction chamber with hydrogen for protection; Apply voltage to the silicon core, and simultaneously detect the silicon core temperature T1 at the overlapping corners of a group of U-shaped silicon cores and the temperature T2 at the vertical part of the vertical silicon core; When T1>T2, the applied voltage remains unchanged; When the error between T1 and T2 is less than 20°C, a large resistance conduction loop has been formed, the current increases, and the temperature continues to be detected; When T1≈T2=(1050~1100℃), a mixture of hydrogen and trichlorosilane begins to flow into the furnace and the reduction reaction begins.
6. The method for heating a polysilicon reduction silicon core assembly according to claim 5, Features: When the error between T1 and T2 is less than 20°C, the current increases instantaneously, and then the rate of increase gradually decreases until the current reaches the process requirement of 1050~1100°C. The current no longer changes and remains constant, and the voltage no longer changes and is output at a constant level.