Methods for establishing adhesive joints
By locally heating the adhesive, the problems of orientation changes and thermal deformation caused by adhesive hardening in the bonding process were solved, thus achieving the stability of the bonding and the precise orientation of optical components, improving energy efficiency and shortening the processing time.
Patent Information
- Application Number
- CN202180084059.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-12-21
- Filing Date
- 2021-12-13
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-12-13
AI Technical Summary
In the prior art, the volume shrinkage of adhesive bonding during adhesive hardening leads to changes in the orientation of optical components and instability in the optical image, and heat treatment causes thermal deformation and positioning deviation of the components.
By heating the adhesive locally using methods such as laser or infrared radiation, heat can be introduced into the adhesive area, avoiding heat treatment of the entire structural assembly.
It achieves stable bonding and precise orientation of optical components, avoids component deformation caused by heat treatment, improves energy efficiency and shortens processing time.
Smart Images

Figure CN116583572B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for establishing an adhesive connection between a first member and a second member, wherein the first member has at least one cavity and the second member has at least one pin, wherein the cavity is at least partially filled with adhesive and the members are oriented relative to each other such that the pin extends at least partially into the adhesive within the cavity. Background Technology
[0002] In modern automotive lighting equipment, especially headlights, there are high requirements for the precise positioning and orientation of optical components such as lenses or reflectors relative to their respective light sources. This necessitates consideration of these high tolerance requirements in manufacturing, and furthermore, the orientation of the optical components must remain within tolerance limits during the actual and continuous operation of the lighting equipment. Optical components or their associated retaining devices are typically fixed to a carrier in their theoretical orientation by means of adhesive connections, particularly those where a pin on the component side extends as a connecting pin into an adhesive-filled cavity in the carrier. Such adhesive connections provide the possibility of fine-tuning the orientation of the optical components, typically in the operation of the light source and the observation of the light image cast on the projection surface.
[0003] A disadvantage of using adhesive bonding is the volume shrinkage of the adhesive during curing, which can cause changes in the orientation of the optical components and corresponding undesirable changes in the light image produced by the lighting device. Numerous measures are known in the prior art to avoid the effects associated with adhesive shrinkage, such as the use of distance retainers and pre-fixing the adhesive bonding with a fast-curing UV adhesive. To achieve the required final strength of the adhesive bonding, a heat-curable adhesive, especially a two-component adhesive, is then applied to the remaining free space of the cavity. For the curing of this adhesive, the entire structural assembly is introduced into a furnace and subjected to corresponding heat treatment. This approach disadvantageously leads to undesirable misalignment of the optical components because these components are subjected to thermal deformation during heat treatment, especially when the bonded components are made of different materials, such as thermoplastics and thermosetting plastics. This thermal deformation causes, to a certain extent, changes in the remaining shape of the components and changes in the relative arrangement of the components. Summary of the Invention
[0004] Therefore, the object of the present invention is to provide a further configuration of a method for establishing an adhesive connection, wherein an adhesive connection is formed between a first member including a cavity and a second member including a pin extending into the cavity.
[0005] The task is solved by starting from the method according to the present invention.
[0006] The present invention includes the following technical teachings, namely, in order to harden the adhesive, heating is implemented on the adhesive by introducing heat into the adhesive in a localized area targeting the adhesive.
[0007] The present invention arises from the idea that, instead of the heat treatment known in the art, which involves furnace aging and is specifically limited to the volume of the adhesive to be cured, the components to be bonded are substantially not subjected to heat introduction and therefore not to undesirable thermal expansion, whereas the heat treatment forces and disadvantageously results in heating of the entire structural assembly. The heat introduced for the curing of the adhesive is significantly less than the energy requirements of furnace treatment of the entire structural assembly, thus achieving energy efficiency advantages using the method according to the invention. As will be explained in more detail below, according to the invention, heat is introduced locally into the adhesive, particularly by means of targeted irradiation or concentrated hot airflow.
[0008] Heat introduction into the adhesive is preferably achieved through a free adhesive surface, i.e., a surface not formed by one of the joint portions but exposed to ambient air and, in particular, through a gap extending circumferentially around the pin, having sufficient accessibility for heat introduction. Heat introduction occurs through the free adhesive surface and radiation absorption within the adhesive, wherein the introduced heat is also distributed throughout the adhesive volume via thermal conduction and convection. Alternatively, heat can, in principle, also be introduced into a covered, internal adhesive volume when electromagnetic radiation is used, provided that the covered component has high transmittance to the radiation used and the adhesive has sufficiently high absorptivity for suitable heating.
[0009] In an advantageous embodiment of the method according to the invention, the heat introduction is achieved by irradiating the adhesive with laser radiation. For applications requiring targeted, locally defined heat introduction, the laser radiation is characterized by a suitable combination of high intensity, clear (sharp) beam focusing, and a narrow frequency range.
[0010] It is preferable to irradiate the adhesive with laser radiation from the infrared spectral range. For example, short-wave infrared radiation with a wavelength of 980 nm has proven suitable for curing two-component adhesives used in typical applications. In particular, the adhesive should be irradiated with laser radiation from a spectral range in which the adhesive has a high spectral absorption rate. This ensures efficient heating of the adhesive and prevents a significant portion of radiation from being emitted through the adhesive and causing undesirable heating of adjacent component sections.
[0011] Preferably, the laser radiation is drawn out via a waveguide with an output coupling optics mechanism for irradiating the adhesive. This configuration provides high flexibility in the orientation of the laser radiation relative to the components to be bonded, thus enabling the irradiation of hard-to-access adhesive joints, particularly free adhesive surfaces, which can be directly irradiated by the laser radiation.
[0012] For example, the laser radiation can be guided in a grid pattern on a free adhesive surface. In this case, the beam cross-section is, for example, smaller than the free adhesive surface, and the adhesive is continuously heated by moving the laser spot along the surface, wherein, for example, it may be suitable to move the laser spot multiple times on the surface.
[0013] For example, the adhesive is irradiated with laser radiation having a beam diameter of 1 mm to 10 mm, especially 5 mm, and / or the irradiation is carried out for an irradiation duration of 10 s to 100 s, preferably 45 s to 75 s. These short process times constitute another advantage of the method according to the invention compared to furnace processing known in the prior art.
[0014] Alternatively, laser radiation can be used, or heat can be introduced by irradiating the adhesive with thermal radiation from conventional infrared radiators or multicolor radiation from incandescent lamps, especially halogen radiators. In particular, the heat introduction can be carried out by focused irradiation, i.e., by using a suitable focusing optical mechanism, the radiation is focused and directed to the free surface of the adhesive, thereby creating a high-intensity localized radiation input.
[0015] In another embodiment, the heat introduction is achieved by applying a directional flow of hot air to the adhesive. Compared to locally defined laser irradiation, in this alternative embodiment, heating of the component sections attached to the adhesive joint must typically be considered (accepted).
[0016] For example, adhesives are heated to temperatures of 150°C to 250°C, preferably 170°C to 190°C, and especially 180°C, for curing.
[0017] Preferably, the adhesive is selected as a two-component adhesive typically consisting of a resin and a hardener, or as a thermosetting one-component adhesive. After the heat introduction according to the invention has ended, in commonly used two-component adhesives, treatment strength typically exists after about one minute and final strength is achieved after about three minutes.
[0018] In particular, the method according to the invention is advantageous for establishing such adhesive connections in which the first component is selected as a carrier and the second component is selected as a light source or optical component of a motor vehicle lighting device. Attached Figure Description
[0019] Preferred embodiments of the present invention
[0020] Next, other improvements to the invention will be described with reference to the accompanying drawings, using the description of preferred embodiments of the invention. Detailed Implementation
[0021] The figure illustrates a method according to the invention for establishing an adhesive connection 100 between a first component 1 comprising a cavity 10 and a second component 2 comprising a pin 20. For example, the first component 1 constitutes a carrier and the second component 2 constitutes an optical component of a motor vehicle lighting device, such as a lens or reflector holder, wherein the components 1 and 2 are in a theoretical optical orientation relative to each other, in which the pin 20 partially extends into an adhesive 3 within the cavity 10, and this theoretical orientation should be durablely secured by the adhesive connection 100 established according to the invention.
[0022] In this example, a temporary and conditionally load-bearing adhesive bond has been constructed in the preceding process steps using a flexible distance retainer 8 and an ultraviolet-cured adhesive 7. The adhesive 3, intended for final strength, is preferably a two-component adhesive and is applied to the cavity 10 in a homogenized, curable state, in which the adhesive circumferentially surrounds the pin 20. According to the invention, for curing, heating is implemented on the adhesive 3 by means of targeted, localized heat introduction into the adhesive 3, wherein, exemplarily, this heat introduction is achieved by irradiation through the free adhesive surface 30 using laser radiation 4. By absorbing the laser radiation 4, preferably near-infrared, the adhesive 3 receives the heat required for its curing and is heated to a temperature typically 150°C–200°C. In the illustrated application, an irradiation duration of approximately one minute is sufficient to generate the required heating of the adhesive 3. The laser radiation is preferably from a continuous-wave laser and is directed onto the free adhesive surface 30 via a waveguide 5 and an output coupling optics mechanism 6, wherein the beam diameter 40 is, for example, 1–10 mm, preferably 5 mm. For example, the laser radiation can be guided in a grid pattern on the adhesive surface 30, or the beam diameter can be selected as shown here such that the beam diameter substantially corresponds to the diameter of the cavity 10, wherein the portion of the pin 20 is irradiated.
[0023] The present invention is not limited in its implementation to the preferred embodiments described above. Instead, various variations are conceivable, which in principle also use the solutions shown in different types of implementations. All features and / or advantages derived from the specification or drawings, including structural details, spatial arrangements, and method steps, are important to the present invention not only in themselves but also in different combinations.
[0024] List of reference numerals
[0025] 100 adhesive connection
[0026] 1 First component
[0027] 10 sales
[0028] 2 Second component
[0029] 20-type cavity
[0030] 3 Adhesives
[0031] 30 Free Adhesive Surfaces
[0032] 4. Laser radiation
[0033] 40 beam diameter
[0034] 5. Optical waveguide
[0035] 6 Output Coupling Optical Mechanism
[0036] 7 Adhesives
[0037] 8 Distance Maintenance Section
Claims
1. A method for establishing an adhesive connection (100) between a first component (1) and a second component (2), wherein, The first component (1) has at least one cavity (10) and the second component (2) has at least one pin (20), wherein the cavity (10) is at least partially filled with adhesive (3) and the first component (1) and the second component (2) are oriented relative to each other such that the pin (20) extends at least partially into the adhesive (3) within the cavity (10), characterized in that a temporary and conditionally load-bearing bond between the first component (1) and the second component (2) has been constructed in the preceding process steps by means of a flexible distance retainer (8) disposed in the cavity and an ultraviolet light-curing adhesive (7) disposed in the cavity, and subsequently an adhesive (3) for final strength is applied in a homogenized mixture. In a hardenable state, the adhesive (3) is applied into the cavity (10). In order to harden the adhesive (3), heating is performed on the adhesive (3) by means of targeted local heat introduction into the adhesive (3). The heat introduction into the adhesive is performed through the free adhesive surface, i.e., the surface is not formed by one of the first and second components to be bonded, but is exposed to ambient air and has sufficient accessibility for the heat introduction through a gap extending circumferentially around the pin. The heat introduction is performed by means of irradiating the adhesive (3) with laser radiation (4), i.e., the laser radiation (4) is guided onto the adhesive (3) by a light waveguide (5) with an output coupling optical mechanism (6) for irradiation.
2. The method according to claim 1, characterized in that, The adhesive (3) is irradiated with laser radiation (4) from the infrared spectrum range.
3. The method according to claim 1 or 2, characterized in that, The adhesive (3) is irradiated with laser radiation (4) from the following spectral range, in which the adhesive (3) has a high spectral absorption rate.
4. The method according to claim 1, characterized in that, The laser radiation (4) is guided in a grid pattern onto the free adhesive surface (30).
5. The method according to claim 1, characterized in that, The adhesive (3) is irradiated with laser radiation (4) having a beam diameter (40) of 1 mm to 10 mm.
6. The method according to claim 1, characterized in that, The irradiation is carried out during an irradiation duration of 10 to 100 seconds.
7. The method according to claim 1 or 2, characterized in that, Heat the adhesive (3) to a temperature of 150°C to 250°C.
8. The method according to claim 1 or 2, characterized in that, The adhesive (3) is selected as a two-component adhesive or as a thermosetting one-component adhesive.
9. The method according to claim 1 or 2, characterized in that, Select the first component (1) as the carrier and the second component (2) as the light source or optical component of the motor vehicle lighting equipment.
10. The method according to claim 5, characterized in that, The adhesive (3) was irradiated with laser radiation (4) having a beam diameter of 5 mm (40).
11. The method according to claim 6, characterized in that, The irradiation is carried out during an irradiation duration of 45 to 75 seconds.
12. The method according to claim 7, characterized in that, Heat the adhesive (3) to a temperature of 170°C to 190°C.
13. The method according to claim 7, characterized in that, Heat the adhesive (3) to 180°C.
Citation Information
Patent Citations
Method for curing adhesive composition and method for manufacturing adhesive structure
CN110494520A
adhesive, component, method for non-contact temperature measurement of the adhesive, method for improved connection of two components with the adhesive and use of the adhesive
DE102015202415A1
Method for adhesively bonding two components arranged positionally accurately in relation to one another