A flip-chip light-emitting diode chip and its preparation method
By adjusting the P-type electrode structure and adding a reflective layer and other technical means, the problems of uneven current and high operating voltage in flip-chip light-emitting diode chips have been solved, and the brightness and photoelectric performance have been improved.
Patent Information
- Application Number
- CN202310887079.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-07-19
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-07-19
AI Technical Summary
The existing flip-chip light-emitting diode chip has uneven current diffusion due to the existence of the current blocking layer, the operating voltage is high, the brightness is low, and the metal reflectivity is low and cannot effectively reflect photons.
By adjusting the structure of the P-type electrode, adding a reflective layer, a protective layer, a conductive layer and an ohmic contact layer, the metal reflectivity is enhanced, the current is prevented from flowing vertically into the P-type semiconductor layer, the current blocking layer is eliminated, and the light reflection efficiency is improved through the Bragg reflective layer and current transmission.
It realizes the uniform diffusion of LED chip current, reduces the operating voltage, increases the brightness, prevents the oxidation of active metals, and improves the photoelectric performance of the chip.
Smart Images

Figure CN116825923B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a flip-chip light-emitting diode chip and a preparation method thereof. Background Art
[0002] Flip-chip light-emitting diodes are widely used in various fields such as lighting, car lights, and display screens due to their many advantages such as back-light emission, strong heat dissipation capacity, high luminous efficiency, and energy saving. The existing flip-chip light-emitting diode chips place the current blocking layer between the current spreading layer and the P-type semiconductor, and the first electrode is placed on the current spreading layer, and coincides with or is smaller than the current blocking layer. The function of the current blocking layer is to prevent the current passing through the P-type electrode from flowing directly vertically into the P-type semiconductor layer below the first electrode, resulting in uneven current diffusion in the LED chip, high operating voltage, and low brightness of the LED chip. With the function of the current blocking layer, the current passing through the P-type electrode can be forced to first be transmitted horizontally from the current spreading layer, and then vertically transmitted from the current spreading layer to all P-type semiconductor layers, so that the current of the LED chip is evenly diffused.
[0003] The bottom layer of the electrode layer of the existing flip-chip LED chip is metal Cr or Ni, which can form an ohmic contact with the current spreading layer. However, Cr or Ni has a low reflectivity and cannot effectively reflect light from the P-type semiconductor layer away from the substrate surface. Summary of the Invention
[0004] In order to solve the above technical problems, the present invention provides a flip-chip light emitting diode chip and a preparation method thereof.
[0005] The present invention adopts the following technical solution: a flip-chip light-emitting diode chip, comprising at least a substrate and an N-type semiconductor layer, an active light-emitting layer, and a P-type semiconductor layer sequentially stacked on the substrate, a current spreading layer stacked on the P-type semiconductor layer, a P-type electrode disposed between the P-type semiconductor layer and the current spreading layer, an N-type semiconductor conductive step disposed on the N-type semiconductor layer, and an N-type electrode disposed on the N-type semiconductor conductive step;
[0006] The P-type electrode includes a reflective layer, a protective layer, a conductive layer, an over-etched layer, and an ohmic contact layer stacked in sequence along the chip growth direction, wherein the reflective layer is an Al layer, the protective layer is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer is an Au layer or a Cu layer, the over-etched layer is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer is a Cr layer or a Ni layer.
[0007] The flip-chip light-emitting diode chip of one embodiment of the present invention effectively enhances the metal reflectivity of the side of the P-type electrode close to the P-type semiconductor layer by adjusting the structure of the P-type electrode, thereby reflecting more light from the P-type semiconductor layer; the reflective layer does not form an ohmic contact with the P-type semiconductor layer, so the current passing through the P-type electrode will not flow vertically into the P-type semiconductor layer, and then there is no need to set a current blocking layer; the protective layer can prevent the active metal Al underneath from oxidizing or migrating; the conductive layer has a high conductivity and is responsible for long-distance lateral current transmission; the over-etching layer is responsible for ensuring that the conductive through hole placed on the P-type electrode is etched cleanly and preventing the presence of an oxide layer on the contact surface between the pad and the P-type electrode, which causes the LED chip voltage to be too high; the ohmic contact layer forms an ohmic contact with the current spreading layer, increasing the ohmic contact area between the current spreading layer and the P-type electrode, thereby effectively reducing the operating voltage of the LED chip.
[0008] Furthermore, the thickness of the reflective layer is between The thickness of the Ni layer and the Pt layer or the Ti layer and the Pt layer of the protective layer is between The thickness of the conductive layer is between The thickness of the over-etched layer is between The thickness of the ohmic contact layer is between
[0009] Furthermore, the P-type electrode gradually narrows along the growth direction of the chip, and the angle between the side surface of the P-type electrode and the P-type semiconductor layer is between 5° and 30°.
[0010] Furthermore, the distance between the edge of the current spreading layer and the edge of the P-type semiconductor layer is between 3 μm and 10 μm.
[0011] Furthermore, the flip-chip light-emitting diode chip also includes a Bragg reflection layer stacked on the current spreading layer, the Bragg reflection layer covers the N-type electrode, and the Bragg reflection layer is composed of TiO2 and SiO2 periodically alternately stacked, and the number of alternating stacking periods is 20-40.
[0012] Furthermore, a P-type pad and an N-type pad are stacked on the Bragg reflector layer, and a P-type Bragg reflector layer through-hole and an N-type Bragg reflector layer through-hole are provided on the Bragg reflector layer. The P-type pad passes through the P-type Bragg reflector layer through-hole and penetrates the current spreading layer to be electrically connected to the P-type electrode, and the N-type pad passes through the N-type Bragg reflector layer through-hole to be electrically connected to the N-type electrode.
[0013] Furthermore, the flip-chip LED chip is further provided with an isolation trench 114 , and the Bragg reflection layer covers the isolation trench.
[0014] Furthermore, the N-type electrode is composed of one or more layers selected from the group consisting of Cr layer, Ni layer, Al layer, AlCu layer, Ti layer, Pt layer, Au layer, Ag layer, Cu layer, and Sn layer, stacked alternately.
[0015] Accordingly, the present invention further provides a method for preparing a flip-chip light-emitting diode chip, which is used to prepare the flip-chip light-emitting diode chip as described above, and the method comprises:
[0016] providing a substrate;
[0017] sequentially growing an N-type semiconductor layer, an active light-emitting layer, and a P-type semiconductor layer on the substrate;
[0018] Depositing a P-type electrode on the P-type semiconductor layer, wherein the P-type electrode comprises a reflective layer, a protective layer, a conductive layer, an over-etching layer, and an ohmic contact layer sequentially deposited along a chip growth direction;
[0019] Depositing a current spreading layer on the P-type semiconductor layer to cover the P-type electrode;
[0020] preparing an isolation trench on the N-type semiconductor layer;
[0021] depositing an N-type electrode on the N-type semiconductor layer;
[0022] depositing a Bragg reflection layer on the current spreading layer, wherein the Bragg reflection layer covers the isolation groove;
[0023] A P-type pad and an N-type pad are deposited on the Bragg reflective layer respectively.
[0024] A method for preparing a flip-chip light-emitting diode chip according to an embodiment of the present invention effectively enhances the metal reflectivity of the side of the P-type electrode close to the P-type semiconductor layer by adjusting the structure of the P-type electrode, thereby reflecting more light from the P-type semiconductor layer. The reflective layer does not form ohmic contact with the P-type semiconductor layer, so the current passing through the P-type electrode does not flow vertically into the P-type semiconductor layer, and thus there is no need to set a current blocking layer. The protective layer can prevent the active metal Al underneath from oxidizing or migrating. The conductive layer has a high conductivity and is responsible for long-distance lateral current transmission. The over-etching layer is responsible for ensuring that the conductive through-hole placed on the P-type electrode is etched cleanly and preventing the presence of an oxide layer on the contact surface between the pad and the P-type electrode, which causes the LED chip voltage to be too high. The ohmic contact layer forms ohmic contact with the current spreading layer, increasing the ohmic contact area between the current spreading layer and the P-type electrode, thereby effectively reducing the operating voltage of the LED chip.
[0025] Furthermore, the reflective layer is an Al layer, the protective layer is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer is an Au layer or a Cu layer, the over-etching layer is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer is a Cr layer or a Ni layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0027] Figure 1 A schematic structural diagram of a flip-chip light-emitting diode chip according to a first embodiment of the present invention;
[0028] Figure 2 Schematic diagram of the top structure of a flip-chip light emitting diode chip according to the first embodiment of the present invention;
[0029] Figure 3 is a schematic cross-sectional view of a P-type current transmission strip portion of a P-type electrode in a flip-chip light-emitting diode chip according to a first embodiment of the present invention;
[0030] Figure 4 FIG. 1 is a flow chart of a method for preparing a flip-chip light emitting diode chip according to a first embodiment of the present invention.
[0031] Description of reference numerals:
[0032] 10. Substrate; 111. N-type semiconductor layer; 112. Active light-emitting layer; 113. P-type semiconductor layer; 114. Isolation trench; 115. N-type semiconductor conductive step; 12. P-type electrode; 121. P-type disk portion; 122. P-type current transmission strip portion; 123. Reflective layer; 124. Protective layer; 125. Conductive layer; 126. Over-etched layer; 127. Ohmic contact layer; 13. Current spreading layer; 131. Spreading layer through hole; 14. N-type electrode; 141. N-type disk portion; 142. N-type current transmission strip portion; 15. Bragg reflector; 151. P-type Bragg reflector through hole; 152. N-type Bragg reflector through hole; 161. P-type pad; 162. N-type pad. DETAILED DESCRIPTION
[0033] The following describes embodiments of the present invention in detail, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the embodiments of the present invention, and should not be construed as limiting the present invention.
[0034] In the description of the embodiments of the present invention, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the embodiments of the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention.
[0035] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be understood to indicate or imply relative importance or implicitly specify the number of the technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the embodiments of the present invention, "plurality" means two or more, unless otherwise specifically defined.
[0036] In the embodiments of the present invention, unless otherwise expressly specified or limited, the terms "installed," "connected," "connected," "fixed," etc. should be understood in a broad sense. For example, they may refer to fixed connection, detachable connection, or integration; mechanical connection or electrical connection; direct connection or indirect connection through an intermediate medium; internal communication between two components or interaction between two components. Those skilled in the art will understand the specific meanings of the above terms in the embodiments of the present invention based on specific circumstances.
[0037] Example 1
[0038] Reference Figures 1 to 4 In a first embodiment of the present invention, a flip-chip light-emitting diode chip includes at least a substrate 10 and an N-type semiconductor layer 111, an active light-emitting layer 112, and a P-type semiconductor layer 113 sequentially stacked on the substrate 10. A current spreading layer 13 is stacked on the P-type semiconductor layer 113. A P-type electrode 12 is provided between the P-type semiconductor layer 113 and the current spreading layer 13. An N-type semiconductor conductive step 115 is provided on the N-type semiconductor layer 111. An N-type electrode 14 is provided on the N-type semiconductor conductive step 115.
[0039] The P-type electrode 12 includes a reflective layer 123, a protective layer 124, a conductive layer 125, an over-etching layer 126, and an ohmic contact layer 127 stacked in sequence along the growth direction of the chip, wherein the reflective layer 123 is an Al layer, the protective layer 124 is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer 125 is an Au layer or a Cu layer, the over-etching layer 126 is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer 127 is a Cr layer or a Ni layer.
[0040] In this embodiment, the protective layer 124 is a periodically stacked structure of a Ti layer and a Pt layer, with the stacking period number being 2; the conductive layer 125 is an Au layer; the over-etched layer 126 is a Pt layer; and the ohmic contact layer 127 is a Cr layer.
[0041] The flip-chip light-emitting diode chip of one embodiment of the present invention effectively enhances the metal reflectivity of the side of the P-type electrode 12 close to the P-type semiconductor layer 113 by adjusting the structure of the P-type electrode 12, thereby reflecting more light from the P-type semiconductor layer 113; the reflective layer 123 does not form an ohmic contact with the P-type semiconductor layer 113, so the current passing through the P-type electrode 12 does not flow vertically into the P-type semiconductor layer 113, and then there is no need to set a current blocking layer; the protective layer 124 can prevent the active metal Al underneath from oxidizing or migrating; the conductive layer 125 has a high conductivity and is responsible for long-distance lateral current transmission; the over-etching layer 126 is responsible for ensuring that the conductive through hole placed on the P-type electrode 12 is etched cleanly and preventing the presence of an oxide layer on the contact surface between the pad and the P-type electrode 12, which causes the LED chip voltage to be too high; the ohmic contact layer 127 forms an ohmic contact with the current spreading layer 13, increasing the ohmic contact area between the current spreading layer 13 and the P-type electrode 12, thereby effectively reducing the operating voltage of the LED chip.
[0042] The thickness of the reflective layer 123 is between The thickness of the Ni layer and the Pt layer or the Ti layer and the Pt layer of the protective layer 124 is between The thickness of the conductive layer 125 is between The thickness of the over-etched layer 126 is between The thickness of the ohmic contact layer 127 is between The thickness of the reflective layer 123 is less than The reflectivity will decrease, the emission effect will decrease, and the thickness will be between Can meet the reflectivity requirements, thickness greater than The Al layer will expand more when heated, so more protective layers 124 will be needed. If the thickness is too thick, the cost will increase. If the thickness of the protective layer 124 is too thin, the coverage of the reflective layer 123 will be too poor, and it will not be able to protect the reflective layer 123 from oxidation migration. Too much thickness will increase the cost. The conductive layer 125 mainly plays the role of current transmission. The thicker the thickness, the better the conductive effect and the lower the operating voltage of the LED chip. Of course, too large a thickness will also increase the cost. The thickness of the over-etching layer 126 is less than It is very easy to have the P-type conductive through hole on the P-type electrode not etched cleanly, resulting in a high voltage on the LED chip. Too thick a thickness will increase the cost. The thickness of the ohmic contact layer 127 is less than It is unable to form ohmic contact with the current spreading layer 13 placed above it, causing the operating voltage of the LED chip to be too high, greater than Any thickness can form an ohmic contact. Of course, increasing the thickness will increase the cost.
[0043] In this embodiment, the protective layer 124 is a structure composed of a Ni layer and a Pt layer periodically stacked, with the number of periods being 2-4. In a specific implementation, the number of periods is 2.
[0044] The P-type electrode 12 gradually narrows along the growth direction of the chip, and the angle between the side of the P-type electrode 12 and the P-type semiconductor layer 113 is between 5° and 30°. The smaller angle can ensure that the thickness of the current expansion layer 13 coated on the side of the P-type electrode 12 is close to the thickness of the P-type electrode 12, effectively preventing the current expansion layer 13 on the side of the P-type electrode 12 from being too thin, which may cause the operating voltage of the LED chip to increase. In this embodiment, the angle between the side of the P-type electrode 12 and the P-type semiconductor layer 113 is 27°.
[0045] In this embodiment, the P-type electrode 12 includes a P-type disk portion 121 and a P-type current transmission strip portion 122. The P-type disk portion 121 is responsible for electrically connecting to the P-type pad 161 to introduce current, and the P-type current transmission strip portion 122 is responsible for transmitting current over long distances. The P-type disk portion 121 is projected into a circle with a diameter between 15um and 35um. The P-type current transmission strip portion 122 is projected into a rectangle with a width between 2um and 10um, and the length depends on the length of the LED chip. The total area of the P-type electrode 12 accounts for 1% to 5% of the area of the P-type semiconductor layer 113. In this embodiment, the diameter of the P-type disk portion 121 is 30um, the width of the P-type current transmission strip portion 122 is 7um, and the total area of the P-type electrode 12 accounts for 3% of the area of the P-type semiconductor layer 113.
[0046] The distance between the edge of the current spreading layer 13 and the edge of the P-type semiconductor layer 113 is between 3 μm and 10 μm; this can prevent the LED chip from being turned on under reverse current, causing the LED chip to fail; in this embodiment, except for the portion of the current spreading layer 13 placed on the P-type electrode 12, the rest of the current spreading layer 13 is placed on the P-type semiconductor layer 113, and the area of the current spreading layer 13 is smaller than the area of the P-type semiconductor layer 113. The current spreading layer 13 can be one of an In2O3 layer, a SnO layer, a ZnO layer, and an ITO layer, and has a thickness between The current spreading layer 13 is provided with an expansion layer through hole 131 on the P-type disc portion 121 to ensure the connection between the P-type pad 161 and the P-type electrode 12; the projected area of the expansion layer through hole 131 is smaller than the area of the P-type disc portion 121; in this embodiment, the distance between the edge of the current spreading layer 13 and the edge of the P-type semiconductor layer 113 is 5μm, and the current spreading layer 13 is an ITO layer with a thickness of
[0047] The flip-chip LED chip further includes a Bragg reflector 15 stacked on the current spreading layer 13. The Bragg reflector 15 covers the N-type electrode 14. The Bragg reflector 15 is composed of TiO2 and SiO2 periodically and alternately stacked, with the number of alternating stacking periods being 20-40. The Bragg reflector 15 is responsible for reflecting light from the P-type semiconductor layer 113 out from under the substrate 10. In this embodiment, the number of alternating stacking periods of the Bragg reflector 15 is 30.
[0048] A P-type pad 161 and an N-type pad 162 are stacked on the Bragg reflector 15. A P-type Bragg reflector through-hole 151 and an N-type Bragg reflector through-hole 152 are provided on the Bragg reflector 15. The P-type pad 161 passes through the P-type Bragg reflector through-hole 151 and penetrates the current spreading layer 13 to be electrically connected to the P-type electrode 12. The N-type pad 162 passes through the N-type Bragg reflector through-hole 152 to be electrically connected to the N-type electrode 14. In this embodiment, the P-type Bragg reflector through-hole 151 corresponds to the spreading layer through-hole 131.
[0049] The flip-chip LED chip is also provided with an isolation groove 114, and the Bragg reflector layer 15 covers the isolation groove 114; the isolation groove 114 is placed around the LED chip. By pre-setting the isolation groove 114 and then covering the isolation groove 114 with the insulating Bragg reflector layer 15, it is possible to prevent external moisture and pollutants from oxidizing and corroding the N-type semiconductor layer 111 and the active light-emitting layer 112.
[0050] The N-type electrode 14 is composed of one or more alternately stacked layers of Cr layer, Ni layer, Al layer, ALCu layer, Ti layer, Pt layer, Au layer, Ag layer, Cu layer, and Sn layer; in this embodiment, the N-type electrode 14 also includes an N-type disk portion 141 and an N-type current transmission strip portion 142, and the N-type electrode 14 is an ALCu layer.
[0051] Accordingly, the present invention also provides a method for preparing a flip-chip light-emitting diode chip, which is used to prepare the above flip-chip light-emitting diode chip, and the method comprises:
[0052] S1: Provide a substrate 10; the substrate 10 is a light-transmitting material, and may be a GaN layer, an AlN layer, or an Al2O3 layer; in this embodiment, the substrate 10 is a GaN layer.
[0053] S2: An N-type semiconductor layer 111 , an active light emitting layer 112 and a P-type semiconductor layer 113 are sequentially grown on the substrate 10 . The specific implementation method is well known to those skilled in the art and will not be described in detail here.
[0054] S3: A P-type electrode 12 is deposited on the P-type semiconductor layer 113. The P-type electrode 12 includes a reflective layer 123, a protective layer 124, a conductive layer 125, an over-etching layer 126, and an ohmic contact layer 127, which are sequentially deposited along the growth direction of the chip. The reflective layer 123 is an Al layer, the protective layer 124 is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer 125 is an Au layer or a Cu layer, the over-etching layer 126 is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer 127 is a Cr layer or a Ni layer.
[0055] Specifically, a negative photoresist is coated on the surface of the P-type semiconductor layer 113, and then exposed and developed to remove part of the photoresist to form a preset P-type electrode 12 photoresist pattern. Then, an Al layer, a periodically stacked Ti layer and Pt layer, an Au layer, a Pt layer, and a Cr layer (the thickness of each layer is 1 / 400 nm, 1 / 800 nm, respectively) are sequentially deposited using an electron beam evaporation process. ), and then use the blue film stripping process to remove the metal outside the P-type electrode 12, and then remove the photoresist to obtain the P-type electrode 12.
[0056] S4: depositing a current spreading layer 13 covering the P-type electrode 12 on the P-type semiconductor layer 113; specifically, depositing a current spreading layer 13 with a thickness of 100 nm on the surface of the P-type semiconductor layer 113 and the P-type electrode 12 using magnetron sputtering technology. The ITO layer is then coated with photoresist on the surface of the ITO layer, and then exposed and developed to remove part of the photoresist, exposing part of the ITO layer, and then using an ITO etching solution to remove the exposed ITO layer, and then removing the photoresist to obtain a current spreading layer 13.
[0057] S5: preparing an isolation trench 114 on the N-type semiconductor layer 111; specifically, coating photoresist on the surface of the current spreading layer 13 and the P-type semiconductor layer 113, then exposing and developing to remove part of the photoresist located above the P-type semiconductor layer 113, exposing part of the P-type semiconductor layer 113, then using an inductively coupled plasma etching process to remove the exposed P-type semiconductor layer 113 and the active light-emitting layer 112 thereunder, exposing part of the N-type semiconductor layer 111, and then removing the photoresist. This part of the N-type semiconductor layer 111 is the N-type semiconductor conductive step 115, which is used to deposit the N-type electrode 14 thereon and prepare the isolation trench 114; coating photoresist on the N-type semiconductor layer 111, the P-type semiconductor layer 113, and the current spreading layer 13, then exposing and developing to remove part of the photoresist, exposing part of the N-type semiconductor layer 111 around the LED chip, and then using an inductively coupled plasma etching process to remove the exposed N-type semiconductor layer 111, forming an isolation trench 114 around the LED chip.
[0058] S6: depositing an N-type electrode 14 on the N-type semiconductor layer 111; specifically, coating the isolation trench 114, the N-type semiconductor layer 111, the P-type semiconductor layer 113, and the current spreading layer 13 with a negative photoresist, then exposing and developing, removing the photoresist on a portion of the N-type semiconductor conductive step 115, forming a preset N-type electrode 14 photolithography pattern on the N-type semiconductor conductive step 115, and then using an electron beam evaporation process to evaporate an AlCu layer (thickness of ), and then use the blue film stripping process to remove the metal other than the N-type electrode 14, and then remove the photoresist to form the N-type electrode 14.
[0059] S7: Depositing a Bragg reflector 15 on the current spreading layer 13, the Bragg reflector 15 covering the isolation trench 114; specifically, using an electron beam evaporation process to sequentially deposit 30 groups of TiO2 and SiO2 stacks on the surfaces of the isolation trench 114, the N-type semiconductor layer 111, the N-type electrode 14, the P-type semiconductor layer 113, and the current spreading layer 13 to form the Bragg reflector 15, then coating the surface of the Bragg reflector 15 with photoresist, then exposing and developing to remove a portion of the photoresist to expose a portion of the Bragg reflector 15 located above the N-type disk portion 141 and the P-type disk portion 121, then using an inductively coupled plasma etching process to remove the Bragg reflector 15 exposed on the N-type disk portion 141 to form an N-type Bragg reflector through hole 152, and removing the Bragg reflector 15 exposed on the P-type disk portion 121 and the current spreading layer 13 below the Bragg reflector 15 to form a P-type Bragg reflector through hole 151 and a spreading layer through hole 131.
[0060] S8: depositing a P-type pad 161 and an N-type pad 162 on the Bragg reflector 15; specifically, coating a negative photoresist on the surface of the Bragg reflector 15, the P-type Bragg reflector through hole 151, and the N-type Bragg reflector through hole 152, and then exposing and developing to remove part of the photoresist to form a preset photoresist pattern of the pad layer, and then using an electron beam evaporation process to evaporate a Cu layer (thickness of ), and then use the blue film stripping process to remove the metal except the pad, and then remove the photoresist to form a P-type pad 161 and an N-type pad 162.
[0061] According to an embodiment of the present invention, a method for preparing a flip-chip light-emitting diode chip effectively enhances the metal reflectivity of the side of the P-type electrode 12 close to the P-type semiconductor layer 113 by adjusting the structure of the P-type electrode 12, thereby reflecting more light from the P-type semiconductor layer 113. The reflective layer 123 does not form an ohmic contact with the P-type semiconductor layer 113, so the current passing through the P-type electrode 12 does not flow vertically into the P-type semiconductor layer 113, and thus there is no need to provide a current blocking layer. The protective layer 124 can prevent the active metal Al underneath from oxidizing or migrating. The conductive layer 125 has a high conductivity and is responsible for long-distance lateral current transmission. The over-etching layer 126 is responsible for ensuring that the conductive through hole placed on the P-type electrode 12 is etched cleanly and preventing the presence of an oxide layer on the contact surface between the P-type pad 161 and the P-type electrode 12, which causes the LED chip voltage to be too high. The ohmic contact layer 127 forms an ohmic contact with the current spreading layer 13, increasing the ohmic contact area between the current spreading layer 13 and the P-type electrode 12, thereby effectively reducing the operating voltage of the LED chip.
[0062] A 10×24 mil chip was prepared using the same chip process conditions as in Example 1 and the control example. 500 LED chips were extracted from each example, and the photoelectric performance of the chip was tested at a current of 60 mA. The brightness of the chip obtained in Example 1 was 116.18 mw, which was 103.6% of the brightness of the chip obtained in the control example. The operating voltage was 2.715 V, and other electrical properties were good. The specific results are shown in Table 1.
[0063] Example 2
[0064] The difference between this embodiment and embodiment 1 is that the thickness of the reflective layer 123 in this embodiment is The thickness of the protective layer 124 is The thickness of the conductive layer 125 is The thickness of the over-etched layer 126 is The thickness of the ohmic contact layer 127 is
[0065] A 10×24 mil chip was prepared using the same chip process conditions as in Example 2 and the control example. 500 LED chips were extracted from each example, and the photoelectric performance of the chip was tested at a current of 60 mA. The brightness of the chip obtained in Example 2 was 112.74 mw, which was 100.5% of the brightness of the chip obtained in the control example. The operating voltage was 2.729 V, and other electrical properties were good. The specific results are shown in Table 1.
[0066] Example 3
[0067] The difference between this embodiment and embodiment 1 is that the thickness of the reflective layer 123 in this embodiment is The thickness of the protective layer 124 is The thickness of the conductive layer 125 is The thickness of the over-etched layer 126 is The thickness of the ohmic contact layer 127 is
[0068] A 10×24 mil chip was prepared using the same chip process conditions as in Example 3 and the control example. 500 LED chips were extracted from each chip, and the photoelectric performance of the chip was tested at a current of 60 mA. The brightness of the chip obtained in Example 3 was 115.69 mw, which was 103.2% of the brightness of the chip obtained in the control example. The operating voltage was 2.718 V, and other electrical properties were good. The specific results are shown in Table 1.
[0069] Example 4
[0070] The difference between this embodiment and embodiment 1 is that the thickness of the reflective layer 123 in this embodiment is The thickness of the protective layer 124 is The thickness of the conductive layer 125 is The thickness of the over-etched layer 126 is The thickness of the ohmic contact layer 127 is
[0071] A 10×24 mil chip was prepared using the same chip process conditions as in Example 4 and the control example. 500 LED chips were extracted from each example, and the photoelectric performance of the chip was tested at a current of 60 mA. The brightness of the chip obtained in Example 4 was 114.95 mw, which was 102.4% of the brightness of the chip obtained in the control example. The operating voltage was 2.722 V, and other electrical properties were good. The specific results are shown in Table 1.
[0072] Example 5
[0073] The difference between this embodiment and embodiment 1 is that the thickness of the reflective layer 123 in this embodiment is The thickness of the protective layer 124 is The thickness of the conductive layer 125 is The thickness of the over-etched layer 126 is The thickness of the ohmic contact layer 127 is
[0074] A 10×24 mil chip was prepared using the same chip process conditions as in Example 5 and the control example. 500 LED chips were extracted from each example, and the photoelectric performance of the chip was tested at a current of 60 mA. The brightness of the chip obtained in Example 5 was 113.23 mw, which was 101% of the brightness of the chip obtained in the control example. The operating voltage was 2.726 V, and other electrical properties were good. The specific results are shown in Table 1.
[0075] Table 1: Comparison of some parameters of various embodiments and comparative examples and corresponding brightness and operating voltage
[0076]
[0077] As can be seen from the above table, the flip-chip light-emitting diode chip provided by the present invention, the P-type electrode 12 includes a reflective layer 123, a protective layer 124, a conductive layer 125, an over-etched layer 126, and an ohmic contact layer 127 sequentially stacked along the chip growth direction, wherein the reflective layer 123 is an Al layer, the protective layer 124 is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer 125 is an Au layer or a Cu layer, the over-etched layer 126 is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer 127 is a Cr layer or a Ni layer; and the thickness of the reflective layer 123 is between The thickness of the protective layer 124 is between The thickness of the conductive layer 125 is between The thickness of the over-etched layer 126 is between The thickness of the ohmic contact layer 127 is between Compared with the control example, the chip obtained by the preparation method of the present invention has significantly improved brightness and effectively reduced operating voltage; that is, by adjusting the structure of the P-type electrode 12, the metal reflectivity of the P-type electrode 12 on the side close to the P-type semiconductor layer 113 is effectively enhanced, thereby reflecting more light from the P-type semiconductor layer 113; the reflective layer 123 does not form an ohmic contact with the P-type semiconductor layer 113, so the current passing through the P-type electrode 12 will not flow vertically into the P-type semiconductor layer 113, and then there is no need to set a current blocking layer; the protective layer 124 can prevent the active metal Al below from oxidizing or migrating; the conductive layer 125 has a high conductivity and is responsible for long-distance lateral current transmission; the over-etching layer 126 is responsible for ensuring that the conductive through hole placed on the P-type electrode 12 is etched cleanly and preventing the presence of an oxide layer on the contact surface between the P-type pad 161 and the P-type electrode 12, which causes the LED chip voltage to be too high; the ohmic contact layer 127 forms an ohmic contact with the current spreading layer 13, increasing the ohmic contact area between the current spreading layer 13 and the P-type electrode 12, thereby effectively reducing the operating voltage of the LED chip.
[0078] Throughout this specification, reference to terms such as "one embodiment," "some embodiments," "examples," "specific examples," or "some examples" means that a specific feature, structure, material, or characteristic described in conjunction with that embodiment or example is included in at least one embodiment or example of the present invention. In this specification, schematic representations of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in any one or more embodiments or examples.
[0079] Under the premise that no conflict occurs, those skilled in the art may freely combine and superimpose the above-mentioned additional technical features.
[0080] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A flip-chip light-emitting diode chip, comprising at least a substrate and an N-type semiconductor layer, an active light-emitting layer, and a P-type semiconductor layer sequentially stacked on the substrate, characterized in that: A current spreading layer is stacked on the P-type semiconductor layer, a P-type electrode is provided between the P-type semiconductor layer and the current spreading layer, an N-type semiconductor conductive step is provided on the N-type semiconductor layer, and an N-type electrode is provided on the N-type semiconductor conductive step; The P-type electrode comprises a reflective layer, a protective layer, a conductive layer, an overetched layer, and an ohmic contact layer stacked in sequence along the growth direction of the chip, wherein the reflective layer is an Al layer, the protective layer is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer is an Au layer or a Cu layer, the overetched layer is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer is a Cr layer or a Ni layer; The thickness of the reflective layer is between 1000Å-3000Å, the thickness of the Ni layer and the Pt layer or the Ti layer and the Pt layer of the protective layer are both between 400Å-4000Å, the thickness of the conductive layer is between 5000Å-50000Å, the thickness of the over-etching layer is between 500Å-3000Å, and the thickness of the ohmic contact layer is between 20Å-200Å; the distance between the edge of the current spreading layer and the edge of the P-type semiconductor layer is between 3μm-10μm.
2. The flip-chip light emitting diode chip according to claim 1, characterized in that: The P-type electrode gradually narrows along the growth direction of the chip, and the angle between the side surface of the P-type electrode and the P-type semiconductor layer is between 5° and 30°.
3. The flip-chip light emitting diode chip according to claim 1, characterized in that: The flip-chip light-emitting diode chip further comprises a Bragg reflection layer stacked on the current spreading layer, the Bragg reflection layer covers the N-type electrode, and the Bragg reflection layer is composed of TiO2 and SiO2 periodically and alternately stacked, and the number of the alternating stacking periods is 20-40.
4. The flip-chip light emitting diode chip according to claim 3, characterized in that: A P-type pad and an N-type pad are stacked on the Bragg reflection layer, and a P-type Bragg reflection layer through hole and an N-type Bragg reflection layer through hole are provided on the Bragg reflection layer. The P-type pad passes through the P-type Bragg reflection layer through hole and penetrates the current spreading layer to be electrically connected to the P-type electrode, and the N-type pad passes through the N-type Bragg reflection layer through hole to be electrically connected to the N-type electrode.
5. The flip-chip light emitting diode chip according to claim 3, characterized in that: The flip-chip light emitting diode chip is also provided with an isolation groove, and the Bragg reflection layer covers the isolation groove.
6. The flip-chip light emitting diode chip according to claim 1, characterized in that: The N-type electrode is composed of one or more layers selected from the group consisting of Cr layer, Ni layer, Al layer, AlCu layer, Ti layer, Pt layer, Au layer, Ag layer, Cu layer and Sn layer, which are alternately stacked.
7. A method for preparing a flip-chip light-emitting diode chip, for preparing the flip-chip light-emitting diode chip as claimed in any one of claims 1 to 6, characterized in that: The method comprises: providing a substrate; Growing an N-type semiconductor layer, an active light-emitting layer and a P-type semiconductor layer in sequence on the substrate; Depositing a P-type electrode on the P-type semiconductor layer, wherein the P-type electrode comprises a reflective layer, a protective layer, a conductive layer, an over-etching layer, and an ohmic contact layer sequentially deposited along a chip growth direction; Depositing a current spreading layer covering the P-type electrode on the P-type semiconductor layer; preparing an isolation trench on the N-type semiconductor layer; Depositing an N-type electrode on the N-type semiconductor layer; Depositing a Bragg reflection layer on the current spreading layer, wherein the Bragg reflection layer covers the isolation groove; A P-type pad and an N-type pad are deposited on the Bragg reflection layer respectively.
8. The method for preparing a flip-chip light-emitting diode chip according to claim 7, characterized in that: The reflective layer is an Al layer, the protective layer is a structure in which a Ni layer and a Pt layer or a Ti layer and a Pt layer are periodically stacked, the conductive layer is an Au layer or a Cu layer, the over-etching layer is any one of a Ni layer, a Ti layer, and a Pt layer, and the ohmic contact layer is a Cr layer or a Ni layer.