A polyaluminium chloride water treatment agent and its preparation method and application

Through the preparation of polyaluminum chloride water treatment agent, the ion exchange and flocculation of inorganic-organic hybrid polymer products are used to solve the problem of residual aluminum and chloride ions in fluorine-containing wastewater, and achieve efficient fluoride ion reduction and oil pollution. The removal improves the wastewater treatment effect.

CN117417048BActive Publication Date: 2024-10-18JIANGXI JIANHENG ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202311673784.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-07
Publication Date
2024-10-18
Estimated Expiration
2043-12-07

AI Technical Summary

Technical Problem

The existing technology is prone to residual aluminum and chloride ions when treating fluorine-containing wastewater, and the treatment effect is poor, resulting in environmental pollution.

Method used

Polyaluminum chloride, acrylamide, butyl acrylate and organically modified Zn-Al hydrotalcite are used as raw materials to prepare polyaluminum chloride water treatment agent through copolymerization to form an inorganic-organic hybrid polymer product, using ion exchange, Mechanisms such as electrostatic interaction and chemical complexation reduce the concentration of fluoride ions, and enhance flocculation performance through organic modification to avoid excessive residues of aluminum and chloride ions.

Benefits of technology

It can effectively reduce the concentration of fluoride ions in fluoride-containing wastewater, avoid excessive residues of aluminum and chloride ions, and show good flocculation and adsorption effects in oily wastewater, improving the purification capacity of wastewater.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention discloses a polyaluminium chloride water treatment agent and a preparation method and application thereof, belonging to the technical field of water treatment agents. The preparation steps are as follows: mixing polyaluminium chloride, acrylamide and deionized water and transferring the mixture to a flask, adding hexadecyltrimethylammonium bromide, urea, butyl acrylate and organically modified Zn-Al hydrotalcite, stirring and mixing for 20-40min to obtain a dispersion; controlling the temperature to 25-30°C, dripping an initiator solution under a nitrogen atmosphere, sealing and reacting for 4-6h after the dripping is completed, then adding the reaction product into distilled water, precipitating, washing and drying; the preparation method of the water treatment agent is simple, and the water treatment agent is applied to fluorine-containing wastewater to effectively reduce the concentration of fluorine ions in the fluorine-containing wastewater, and avoid excessive residues of aluminum ions and chloride ions; and the water treatment agent is applied to oily sewage to destabilize, aggregate and remove oil pollution through electrical neutralization, adsorption bridging and net capture and sweeping.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of water treatment agents, and specifically relates to a polyaluminium chloride water treatment agent and a preparation method and application thereof. Background Art

[0002] Chemical coagulation is one of the main methods for treating fluoride-containing wastewater at present. It is widely used because of its strong adaptability, simple operation and low infrastructure investment. The choice of coagulant directly affects the coagulation treatment effect and cost. A company uses the lime milk-aluminum sulfate two-stage method to treat the discharged fluoride-containing wastewater. This process has the characteristics of simple production and relatively low price, but it has problems such as large dosage, loose and broken precipitates formed during the treatment process, and suspension in water that is not easy to precipitate. As a result, fluoride ions fail to meet the GB8979-1996 first-level emission standard, causing pollution to the environment.

[0003] Polyaluminium chloride is a new type of inorganic polymer coagulant. It is a water-soluble inorganic polymer between AlCl3 and Al(OH)3 and has good coagulation efficiency. However, when using polyaluminium chloride to treat fluoride-containing wastewater, 50-1000g needs to be added per cubic meter of wastewater, depending on the quality of the wastewater. This will cause the effluent to contain a certain amount of residual aluminum and chloride ions, introduce new sources of pollution, and cause poor effluent quality. Summary of the invention

[0004] The purpose of the present invention is to provide a polyaluminium chloride water treatment agent and a preparation method and application thereof, so as to solve the problem that aluminium and chloride ions are easily left in the prior art polyaluminium chloride treatment of fluorine-containing wastewater and the treatment effect is poor.

[0005] The purpose of the present invention can be achieved through the following technical solutions:

[0006] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0007] Mix polyaluminium chloride, acrylamide and deionized water and transfer them to a flask, add hexadecyltrimethylammonium bromide, urea, butyl acrylate and organically modified Zn-Al hydrotalcite, stir and mix for 20-40 minutes to obtain a dispersion; control the temperature at 25-30°C, add the initiator solution dropwise under a nitrogen atmosphere, and after the addition is completed, seal and react for 4-6 hours, then add the reaction product into distilled water, precipitate with acetone, wash with anhydrous ethanol, and finally place it at 55-60°C and vacuum dry to constant weight.

[0008] The mass ratio of polyaluminium chloride, acrylamide, deionized water, hexadecyltrimethylammonium bromide, urea, butyl acrylate and organically modified Zn-Al hydrotalcite is 1.5-2.5:10-14:100-150:0.1-0.2:3:1-5:0.4-1, the amount of initiator is 0.1-0.2% of the mass of acrylamide, butyl acrylate and organically modified Zn-Al hydrotalcite, the initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1, and the mass fraction of the initiator solution is 10%.

[0009] The invention uses polyaluminium chloride, acrylamide, butyl acrylate and organically modified Zn-Al hydrotalcite as raw materials, and obtains the polyaluminium chloride water treatment agent through copolymerization. The polyaluminium chloride water treatment agent is an inorganic-organic hybrid polymer product, wherein the polyaluminium chloride is connected to an organic long chain through ion bonding, and the acrylamide, butyl acrylate and organically modified Zn-Al hydrotalcite are chemically bonded to present a three-dimensional spatial network structure. The effective contact area with the pollution source is large during the water treatment process, and the wastewater can be purified through ion exchange, electrostatic action, physical adsorption, chemical complexation and the like. The invention has obvious advantages in particular in fluorine-containing wastewater. On the one hand, the fluorine in the zeolite is reduced through ion exchange. - On the other hand, the active groups such as hydroxyl, carboxyl and amino groups are used to - Providing adsorption sites, so that the water treatment agent and F- generate adsorption bridges through intermolecular forces to form a three-dimensional network and precipitate, effectively reducing the concentration of fluoride ions in fluoride-containing wastewater, and avoiding excessive residual aluminum ions and chloride ions. In addition, the water treatment agent also has a good application effect in oily wastewater, which is mainly attributed to the introduction of organically modified Zn-Al hydrotalcite, acrylamide, and hydrophobic groups (ester groups) to enhance the flocculation performance of polyaluminum chloride. Polyaluminum chloride neutralizes the surface charge of oil pollution and reduces the electrostatic repulsion between particles. The long polymer chain plays the role of adsorption bridging and net capture and sweeping, and finally destabilizes the oil pollution and aggregates to form a dense and easy-to-remove floc, thereby achieving the purification of oily wastewater.

[0010] As a further embodiment of the present invention, the organically modified Zn-Al hydrotalcite is obtained by the following steps:

[0011] S1. Dissolve zinc nitrate hexahydrate and aluminum nitrate nonahydrate in deionized water to form solution a, dissolve L-histidine in deionized water to form solution b and transfer to a flask, control the temperature at 40°C, add solution a dropwise to the flask under nitrogen protection while stirring, and control the pH value of the system to 8 with sodium hydroxide solution. After the addition is completed, let stand for 4 hours, wash, filter, and dry the obtained solid product in a 40°C oven to constant weight to obtain amino acid intercalated Zn-Al hydrotalcite;

[0012] Using zinc nitrate hexahydrate, aluminum nitrate nonahydrate and L-histidine as raw materials, amino acid intercalated Zn-Al hydrotalcite was obtained by coprecipitation method. The interlayer ions of the Zn-Al hydrotalcite were exchangeable and had good stability. - and Cl - It has good adsorption properties and contains structures such as carboxyl and imidazole rings, which have good coordination effects with metal ions such as aluminum ions;

[0013] S2, placing the amino acid intercalated Zn-Al type hydrotalcite in anhydrous methanol, adding KOH after ultrasonic dispersion, and dripping the anhydrous methanol solution of 3-allyl salicylaldehyde. After the dripping is completed, stirring and reacting at 50-55° C. for 2-4 hours. After the reaction is completed, cooling and filtering, washing the filter cake with anhydrous ethanol, and vacuum drying at 80° C. to constant weight to obtain an organically modified Zn-Al type hydrotalcite;

[0014] Amino acid intercalated Zn-Al hydrotalcite and 3-allyl salicylaldehyde were used as raw materials. Under alkaline conditions, a Schiff base structure was formed on the surface of the amino acid intercalated Zn-Al hydrotalcite through the condensation reaction between the amino group and the aldehyde group, and allyl groups and phenolic hydroxyl groups were introduced. On the one hand, the allyl groups were used as active sites to endow the organically modified Zn-Al hydrotalcite with reaction activity. On the other hand, the introduction of the Schiff base structure and phenolic hydroxyl groups enhanced the adsorption capacity of the organically modified Zn-Al hydrotalcite for metal ions based on the good coordination ability between the electronegative N and O atoms and metal ions.

[0015] As a further scheme of the present invention, in step S1, the volume ratio of solution a to solution b is 1:2.5, solution a is composed of zinc nitrate hexahydrate, aluminum nitrate nonahydrate and deionized water in a dosage ratio of 0.75 mol:0.25 mol:1 L, the concentration of L-histidine in solution b is 0.1 mol / L, and the mass fraction of the sodium hydroxide solution is 30-40%.

[0016] As a further solution of the present invention, the mass ratio of amino acid intercalated Zn-Al hydrotalcite, KOH and 3-allyl salicylaldehyde in S2 is 1:0.15-0.3:0.2-0.4.

[0017] A polyaluminium chloride water treatment agent is prepared by the above preparation method.

[0018] The invention discloses an application of a polyaluminium chloride modified flocculant in fluorine-containing wastewater and oily wastewater.

[0019] Beneficial effects of the present invention:

[0020] 1. The present invention provides a polyaluminum chloride water treatment agent, which has a simple preparation method. When applied to fluorine-containing wastewater, the concentration of fluoride ions in the fluorine-containing wastewater can be effectively reduced, and excessive residual aluminum ions and chloride ions can be avoided. When applied to oily wastewater, the oil can be destabilized, aggregated and removed through electrical neutralization, adsorption bridging and net capture and sweeping.

[0021] 2. The present invention provides a polyaluminum chloride water treatment agent, which is an inorganic-organic hybrid polymer product. Compared with compound flocculants, it has an obvious three-dimensional spatial network structure. The components are bonded by chemical bonds, the interface interaction is increased, and the stability is high. It not only combines the strong electrical neutralization performance of inorganic flocculants and the adsorption bridging effect of organic flocculants, but also has the flocculation effect produced by the synergistic effect of the two. Therefore, it has a higher purification capacity for wastewater treatment. DETAILED DESCRIPTION

[0022] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0023] Example 1

[0024] An organic modified Zn-Al type hydrotalcite is obtained by the following steps:

[0025] S1. Dissolve 0.25 mol zinc nitrate hexahydrate and 0.75 mol aluminum nitrate nonahydrate in 1 L of deionized water to form solution a, dissolve 0.25 mol L-histidine in 2.5 L of deionized water to form solution b and transfer to a flask, control the temperature at 40°C, add solution a dropwise to the flask under nitrogen protection while stirring, and use 30 wt% sodium hydroxide solution to control the pH value of the system to 8. After the addition is completed, let stand for 4 hours, wash, filter, and dry the obtained solid product in a 40°C oven to constant weight to obtain amino acid intercalated Zn-Al hydrotalcite;

[0026] S2. Place 10 g of amino acid intercalated Zn-Al hydrotalcite in 100 mL of anhydrous methanol, add 1.5 g of KOH after ultrasonic dispersion, and drop a solution consisting of 2 g of 3-allyl salicylaldehyde and 20 mL of anhydrous methanol. After the addition is complete, stir the reaction at 50 °C for 2 h. After the reaction is completed, cool and filter. Wash the filter cake with anhydrous ethanol and vacuum dry it at 80 °C to constant weight to obtain an organically modified Zn-Al hydrotalcite.

[0027] Example 2

[0028] An organic modified Zn-Al type hydrotalcite is obtained by the following steps:

[0029] S1. Dissolve 0.25 mol zinc nitrate hexahydrate and 0.75 mol aluminum nitrate nonahydrate in 1 L of deionized water to form solution a, dissolve 0.25 mol L-histidine in 2.5 L of deionized water to form solution b and transfer to a flask, control the temperature at 40°C, add solution a dropwise to the flask under nitrogen protection while stirring, and control the pH value of the system to 8 with 40 wt% sodium hydroxide solution. After the addition is completed, let stand for 4 hours, wash, filter, and dry the obtained solid product in a 40°C oven to constant weight to obtain amino acid intercalated Zn-Al hydrotalcite;

[0030] S2. Place 10 g of amino acid intercalated Zn-Al hydrotalcite in 100 mL of anhydrous methanol, add 3 g of KOH after ultrasonic dispersion, and drop a solution consisting of 4 g of 3-allyl salicylaldehyde and 20 mL of anhydrous methanol. After the addition is complete, stir the reaction at 55 °C for 4 h. After the reaction is completed, cool and filter. Wash the filter cake with anhydrous ethanol and vacuum dry it at 80 °C to constant weight to obtain an organically modified Zn-Al hydrotalcite.

[0031] Comparative Example 1

[0032] This comparative example is the amino acid intercalated Zn-Al type hydrotalcite obtained in step S1 of Example 1.

[0033] Example 3

[0034] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0035] 1.5 g of polyaluminium chloride, 10 g of acrylamide and 100 mL of deionized water were mixed and transferred to a flask, 0.1 g of hexadecyltrimethylammonium bromide, 3 g of urea, 1 g of butyl acrylate and 0.4 g of the organically modified Zn-Al hydrotalcite of Example 1 were added, and the mixture was stirred for 20 min to obtain a dispersion. The temperature was controlled at 25 ° C., and an initiator solution was added dropwise under a nitrogen atmosphere. After the addition was completed, the mixture was sealed and reacted for 4 hours. The reaction product was then added to distilled water, precipitated with acetone, washed with anhydrous ethanol, and finally dried in vacuo at 55 ° C to constant weight. The mass fraction of the initiator solution was 10%, and the initiator was composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1. The amount of the initiator was 0.1% of the mass of acrylamide, butyl acrylate and the organically modified Zn-Al hydrotalcite.

[0036] Example 4

[0037] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0038] 2 g of polyaluminium chloride, 12 g of acrylamide and 130 mL of deionized water were mixed and transferred to a flask, 0.15 g of hexadecyltrimethylammonium bromide, 3 g of urea, 2 g of butyl acrylate and 0.6 g of the organically modified Zn-Al hydrotalcite of Example 2 were added, and the mixture was stirred for 30 min to obtain a dispersion. The temperature was controlled at 28 ° C, and the initiator solution was added dropwise under a nitrogen atmosphere. After the addition was completed, the mixture was sealed and reacted for 5 h. Thereafter, the reaction product was added to distilled water, precipitated with acetone, washed with anhydrous ethanol, and finally dried in vacuo at 58 ° C to constant weight. The mass fraction of the initiator solution was 10%, and the initiator was composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1. The amount of the initiator was 0.1% of the mass of acrylamide, butyl acrylate and the organically modified Zn-Al hydrotalcite.

[0039] Example 5

[0040] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0041] 2.5 g of polyaluminium chloride, 14 g of acrylamide and 150 mL of deionized water were mixed and transferred to a flask, 0.2 g of hexadecyltrimethylammonium bromide, 3 g of urea, 5 g of butyl acrylate and 1 g of the organically modified Zn-Al hydrotalcite of Example 2 were added, and the mixture was stirred for 40 min to obtain a dispersion. The temperature was controlled at 30 ° C, and the initiator solution was added dropwise under a nitrogen atmosphere. After the addition was completed, the mixture was sealed and reacted for 6 hours. Thereafter, the reaction product was added to distilled water, precipitated with acetone, washed with anhydrous ethanol, and finally dried in vacuo at 60 ° C to constant weight. The mass fraction of the initiator solution was 10%, and the initiator was composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1. The amount of the initiator was 0.2% of the mass of acrylamide, butyl acrylate and the organically modified Zn-Al hydrotalcite.

[0042] Comparative Example 2

[0043] Compared with Example 3, on the substrate of Example 3, the organically modified Zn—Al type hydrotalcite in Example 3 is replaced by the substance in Comparative Example 1, and the remaining raw materials and preparation process are the same as in Example 3.

[0044] Comparative Example 3

[0045] Compared with Example 3, on the substrate of Example 3, the organically modified Zn—Al type hydrotalcite in Example 3 is removed, and the remaining raw materials and preparation process are the same as in Example 3.

[0046] Comparative Example 4

[0047] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0048] 10 g of acrylamide and 100 mL of deionized water were mixed and transferred to a flask, 0.1 g of hexadecyltrimethylammonium bromide, 3 g of urea, 1 g of butyl acrylate and 0.4 g of the organically modified Zn-Al hydrotalcite of Example 1 were added, and the mixture was stirred for 20 min to obtain a dispersion. The temperature was controlled at 25° C., and the initiator solution was added dropwise under a nitrogen atmosphere. After the addition was completed, the mixture was sealed and reacted for 4 h. The reaction product was then washed with a mixed solution of anhydrous ethanol and acetone in a volume ratio of 1:1, and dried at 55° C. for 24 h to obtain a product 1. The product 1 was stirred and mixed with 1.5 g of polyaluminum chloride for 10 min to obtain the polyaluminum chloride water treatment agent.

[0049] The mass fraction of the initiator solution is 10%, the initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1, and the amount of the initiator is 0.1% of the mass of acrylamide, butyl acrylate and organically modified Zn-Al hydrotalcite.

[0050] Comparative Example 5

[0051] A method for preparing a polyaluminium chloride water treatment agent comprises the following steps:

[0052] 10 g of acrylamide and 100 mL of deionized water were mixed and transferred to a flask, 0.1 g of hexadecyltrimethylammonium bromide, 3 g of urea and 1 g of butyl acrylate were added, and the mixture was stirred for 20 min to obtain a dispersion; the temperature was controlled at 25° C., and an initiator solution was added dropwise under a nitrogen atmosphere. After the addition was completed, the mixture was sealed and reacted for 4 h. The reaction product was then washed with a mixture of anhydrous ethanol and acetone in a volume ratio of 1:1, and dried at 55° C. for 24 h to obtain a product 2. The product 2 was stirred and mixed with 1.5 g of polyaluminum chloride for 10 min to obtain the polyaluminum chloride water treatment agent.

[0053] The mass fraction of the initiator solution is 10%, the initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:1, and the amount of the initiator is 0.1% by mass of acrylamide and butyl acrylate.

[0054] The water treatment agents obtained from Examples 3 to 5 and Comparative Examples 2 to 5 were tested, and the test items were as follows:

[0055] Fluoride-containing wastewater treatment:

[0056] Place 500 mL of deionized water in a beaker and add sodium fluoride to make F -The concentration was 70 mg / L to obtain a simulated wastewater solution. The same method was used to obtain 7 groups of simulated wastewater solutions. 400 mg / L of polyaluminum chloride water treatment agent was added to each group of simulated wastewater solutions, which were the products obtained in the embodiment and the comparative example, respectively. After stirring at a speed of 150 r / min for 2 min, stirring at a speed of 40 r / min for 10 min, and settling for 120 min, the supernatant was taken for analysis and determination of F - , Cl - 、Al 3+ content,

[0057] Oily wastewater treatment:

[0058] 4 g crude oil, 8 g sodium bicarbonate, 0.2 g sodium dodecylbenzene sulfonate, 4 g polyacrylamide, and 600 mL distilled water at 40° C. were added to a 1 L beaker, and the mixture was sheared at a speed of 8000 r / min for 15 min using a high-speed shearing machine to obtain a shearing liquid, and the shearing liquid was mixed with 0.08 mol sodium chloride and 3400 mL distilled water at 40° C. and stirred for 10 min, and then allowed to stand for 30 min to remove the surface floating oil to obtain a simulated oily wastewater with an oil content of 500 mg / L; 20 mg / L of polyaluminum chloride water treatment agent was added to each group of simulated wastewater solutions, which were the products obtained in the embodiment and the comparative example, respectively, and stirred at a speed of 160 r / min for 8 min, then stirred at a speed of 60 r / min for 8 min, and allowed to stand for 120 min, and the supernatant was tested for oil content analysis;

[0059] The oil content test steps are as follows:

[0060] Transfer a certain amount of the supernatant to be tested into a 500mL separatory funnel, wash the container for dissolving and transferring the supernatant with an appropriate amount of petroleum ether, then transfer it to the separatory funnel, add 2mL of 6mol / L hydrochloric acid solution, fully shake the separatory funnel and release the gas, let the solution stand for a period of time, release the water layer, transfer the remaining liquid into a 50mL colorimetric tube, use petroleum ether as a blank control, and use a UV spectrophotometer to measure the absorbance value A of the remaining liquid at a wavelength of 430nm. The oil content calculation formula is:

[0061] C=AV O / KV W ×n, where C is the oil content of the supernatant, mg / L, A is the absorbance of the supernatant, V O is the volume of the remaining liquid, mL, V W is the volume of the supernatant, mL, K is the absorbance coefficient, and n is the dilution multiple;

[0062] The test results are shown in Table 1:

[0063] Table 1

[0064]

[0065] It can be seen from Table 1 that, under the same addition amount, the water treatment agents obtained in Comparative Examples 2-4 are mostly inferior to the water treatment agents obtained in Examples 3-5 in terms of the treatment effect of oily wastewater and fluorine-containing wastewater. It can be seen from the test data in Comparative Example 2 and Example 3 that the condensation reaction between the amino group and the aldehyde group forms a Schiff base structure on the surface of the amino acid intercalated Zn-Al type hydrotalcite and introduces allyl groups and phenolic hydroxyl groups, which is beneficial to enhance the water treatment agent's effect on F - , Cl - 、Al 3+ , oil removal performance. It can be seen from the test data in Comparative Example 3 and Example 3 that in the absence of the organically modified Zn-Al type hydrotalcite prepared by the present invention, the performance of the obtained water treatment agent in fluorine-containing anhydrous and oil-containing wastewater is significantly reduced. It can be seen from the test data in Example 3 and Comparative Example 4 and Comparative Example 3 and Comparative Example 5 that the water treatment prepared by the present invention has better performance than the water treatment obtained by physical compounding. In summary, the water treatment prepared by the present invention has a good application effect in fluorine-containing wastewater and oily wastewater.

[0066] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0067] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for preparing a polyaluminium chloride water treatment agent, characterized in that: The following steps are involved: The first step is to place the amino acid intercalated Zn-Al hydrotalcite in anhydrous methanol, add KOH after ultrasonic dispersion, and dropwise add an anhydrous methanol solution of 3-allyl salicylaldehyde. After the dropwise addition is completed, stir and react at 50-55° C. for 2-4 hours to obtain an organically modified Zn-Al hydrotalcite. Step 2: Mix polyaluminium chloride, acrylamide and deionized water and transfer them to a flask, add hexadecyltrimethylammonium bromide, urea, butyl acrylate and organically modified Zn-Al hydrotalcite, and stir and mix for 20-40 minutes to obtain a dispersion; control the temperature at 25-30°C, add the initiator solution dropwise under a nitrogen atmosphere, and after the addition is complete, seal and react for 4-6 hours, then add the reaction product into distilled water, precipitate with acetone, wash with anhydrous ethanol, and vacuum dry at 55-60°C to constant weight; The mass ratio of amino acid intercalated Zn-Al hydrotalcite, KOH and 3-allyl salicylaldehyde is 1:0.15-0.3:0.2-0.4; The amino acid intercalated Zn-Al hydrotalcite is obtained by the following steps: Dissolve zinc nitrate hexahydrate and aluminum nitrate nonahydrate in deionized water to form solution a, dissolve L-histidine in deionized water to form solution b and transfer to a flask, control the temperature at 40°C, add solution a dropwise to the flask under nitrogen protection with stirring, and control the pH value of the system to 8 with sodium hydroxide solution. After the addition is completed, let stand for 4 hours, wash, filter, and dry the obtained solid product in a 40°C oven to constant weight to obtain amino acid intercalated Zn-Al hydrotalcite; The volume ratio of solution a to solution b is 1:2.5, solution a is composed of zinc nitrate hexahydrate, aluminum nitrate nonahydrate and deionized water in a dosage ratio of 0.75 mol:0.25 mol:1 L, and the concentration of L-histidine in solution b is 0.1 mol / L.

2. The method for preparing a polyaluminium chloride water treatment agent according to claim 1, wherein: The mass ratio of polyaluminium chloride, acrylamide, deionized water, hexadecyltrimethylammonium bromide, urea, butyl acrylate and organically modified Zn-Al hydrotalcite is 1.5-2.5:10-14:100-150:0.1-0.2:3:1-5:0.4-1.

3. The method for preparing a polyaluminium chloride water treatment agent according to claim 1, characterized in that: The mass fraction of the initiator solution is 10%, the amount of the initiator is 0.1-0.2% of the mass of acrylamide, butyl acrylate and organic modified Zn-Al type hydrotalcite, and the initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 2:

1.

4. A polyaluminium chloride water treatment agent, characterized in that: Prepared by the preparation method according to any one of claims 1 to 3.

5. Use of a polyaluminium chloride modified flocculant according to claim 4 in fluorine-containing wastewater and oily wastewater.

Citation Information

Patent Citations

  • Cation-type hydrophobic association polymer and its preparation method and application

    CN101260174A

  • Polyacrylamide composite flocculant and preparation method thereof

    CN104724808A

  • Inorganic-organic hybridized flocculating material and preparation method of inorganic-organic hybridized flocculating material

    CN106745624A

  • Preparation method of catalyst for simply and effectively catalyzing asymmetric epoxidation of allyl alcohol

    CN110935488A

  • Method for enhancing heterogeneous asymmetric selectivity and catalytic activity

    US20120322647A1