A welding nail for connecting different grades of aluminum alloys
By opening gradually reduced through holes at the aluminum alloy connection position and using special welding nails for resistance spot welding, double welding core connection is formed, the problem of poor welding of aluminum alloys of different grades is solved, and a stable aluminum alloy connection is achieved, reducing the The occurrence of welding defects.
Patent Information
- Application Number
- CN202311292969.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2043-09-28
AI Technical Summary
Different grades of aluminum alloys are difficult to connect stably and firmly during welding, especially the welding effect of 7-Series aluminum alloys and 5-Series or 6-Series aluminum alloys is poor, and welding defects such as pores and thermal cracks are prone to occur.
A connection method is adopted, including opening a through hole at the first aluminum alloy connection position, gradually reducing its inner diameter, and making welding nails using materials that can meet the spot welding performance standards with the second aluminum alloy. The welding nails are round table structures and the bottom surface is The conical surface has several grooves, and a double weld core connection is formed by spot welding by resistive spot welding machine.
It realizes stable connections of aluminum alloys of different grades, reduces welding defects, improves welding quality and safety, and ensures a firm connection of aluminum alloys.
Smart Images

Figure CN117428306B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of welding, and in particular to a connection method and welding nails for aluminum alloys of different grades. Background Art
[0002] With the global energy crisis and the intensification of environmental pollution, the automotive industry has begun to use aluminum alloys as structural materials to reduce the weight of cars. Lightweight technology is a common basic technology for both traditional fuel vehicles and new energy vehicles. Aluminum alloys, as a lightweight material with a variety of excellent properties, have become the preferred material in the development of automotive lightweight technology. The weight of the car body accounts for about 40% of the total weight of the car. For the lightweight of the entire vehicle, the lightweight of the car body plays a vital role.
[0003] However, since aluminum alloys have many grades, such as 5-series aluminum alloy, 6-series aluminum alloy, and 7-series aluminum alloy, different grades of aluminum alloys sometimes have poor welding effects when welding. For example, 7-series aluminum alloy is difficult to be stably and firmly welded with 5-series or 6-series aluminum alloy. Summary of the invention
[0004] In view of this, it is necessary to provide a connection method and welding pins for aluminum alloys of different grades to solve the technical problem that aluminum alloys of different grades are difficult to weld stably and firmly in the prior art.
[0005] The invention provides a connection method for aluminum alloys of different grades, and the connection method comprises the following steps: S1, a through hole is opened at a connection position of a first aluminum alloy, and the inner diameter of the through hole gradually decreases in a direction close to a second aluminum alloy; S2, a welding pin is made of a material that can meet the spot welding performance standards with the second aluminum alloy, and the height of the welding pin is greater than the thickness of the through hole, so that when the welding pin is placed in the through hole, the bottom surface of the welding pin protrudes out of the through hole and a gap is formed between the side surface of the welding pin and the through hole; S3, the connection position of the first aluminum alloy is superimposed on the connection position of the second aluminum alloy, the welding pin is placed in the through hole, and the welding pin is spot welded by a resistance spot welding machine.
[0006] The present invention also provides a welding nail, which is a truncated cone structure, the top surface diameter of the welding nail is larger than the bottom surface diameter, and the height of the welding nail is larger than the through hole.
[0007] Furthermore, the bottom surface of the welding nail is a conical surface, and the center of the circle is raised to form a tip.
[0008] Furthermore, the welding nail has a plurality of grooves, and the grooves extend from the bottom surface of the welding nail to the side surface of the welding nail until they are connected to the top surface of the welding nail.
[0009] Furthermore, the groove includes a plurality of side segments, the side segments are evenly distributed on the sides of the welding nail, and the upper end and the lower end of the side segments are connected to the top surface and the bottom surface of the welding nail respectively.
[0010] Furthermore, the groove also includes a plurality of bottom surface segments, which are radially distributed on the bottom surface of the welding stud, and each bottom surface segment is connected to at least one side surface segment.
[0011] Furthermore, the groove also includes a plurality of transverse sections located on the bottom surface of the welding stud, and two ends of the transverse section are respectively connected to the two bottom surface sections.
[0012] Furthermore, the transverse section is in the shape of an arc, and the center of the arc coincides with the center of the bottom surface of the welding stud.
[0013] Furthermore, a plurality of concentric circles are formed on the bottom surface of the transverse section welding stud.
[0014] Furthermore, two ends of a part of the bottom surface segment are respectively connected to the two side surface segments, and a part of the bottom surface segment is connected to the side surface segment and the transverse segment.
[0015] Compared with the prior art, the welding pin structure provided by the present invention is larger at the top and smaller at the bottom, and the corresponding through hole on the first aluminum alloy is also larger at the top and smaller at the bottom. The welding pin and the side wall of the through hole form an annular welding core. At the same time, the welding pin is made of a material that can meet the spot welding performance standards of the second aluminum alloy, and can form a stable and firm circular welding core with the second aluminum alloy. By forming a double welding core spot welding connection, the first aluminum alloy and the second aluminum alloy can be firmly connected together.
[0016] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention and implement it according to the contents of the specification, the preferred embodiments of the present invention are described in detail as follows with reference to the accompanying drawings. The specific implementation of the present invention is given in detail by the following embodiments and their accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0018] Figure 1 A schematic diagram of the structure of the method for connecting aluminum alloys of different grades provided by the present invention when it is implemented;
[0019] Figure 2 A flow chart of a method for connecting aluminum alloys of different grades provided by the present invention;
[0020] Figure 3 This is a schematic structural diagram of the welding stud provided by the present invention. DETAILED DESCRIPTION
[0021] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings, wherein the accompanying drawings constitute a part of this application and are used together with the embodiments of the present invention to illustrate the principles of the present invention, but are not used to limit the scope of the present invention.
[0022] See also Figure 1 and Figure 2 The present invention provides a welding nail. The welding nail can be applied to aluminum alloy welding in automobile production to obtain a more stable welding effect. It should be noted that the welding nail of the present invention is used for but not limited to the field of automobile production, and can also be applied to other scenes requiring welding of aluminum alloys. In the present invention, only the application of welding nails to automobile production is used as an example for explanation, and the principle of applying welding nails to other fields is substantially the same as that of applying them to automobile production, which will not be repeated here.
[0023] The connection method comprises the following steps: S1: a through hole 110 is opened at the connection position of the first aluminum alloy 100, and the inner diameter of the through hole 110 gradually decreases in the direction close to the second aluminum alloy 200. The first aluminum alloy 100 and the second aluminum alloy 200 are different grades of aluminum alloys that are difficult to weld or have poor welding effects. The first aluminum alloy 100 is stacked on the second aluminum alloy 200 for connection.
[0024] S2 uses a material that can meet the spot welding performance standards with the second aluminum alloy 200 to make the welding nail 300. The height of the welding nail 300 is greater than the thickness of the through hole 110, so that when the welding nail 300 is placed in the through hole 110, the bottom surface of the welding nail 300 protrudes outside the through hole 110. In addition, the radial dimension of the welding nail 300 is slightly smaller than the through hole 110, so that when the welding nail 300 is placed in the through hole 110, a gap is formed between the side of the welding nail 300 and the through hole 110.
[0025] Those skilled in the art can easily understand that the welding stud 300 can be made of not only the same material as the second aluminum alloy 200, but also other materials having better spot welding performance than the second aluminum alloy 200, as long as the spot welding performance of the material and the second aluminum alloy 200 can meet the standard. The standard here is selected according to actual production needs. For example, when used in Volkswagen, the Volkswagen standard PV 6723:2013-04 is implemented. When used in the aerospace field, the technical conditions for aluminum alloy resistance spot welding and seam welding of China Aerospace Industry-QJ_2205-1995 are implemented.
[0026] S3 overlaps the connection position of the first aluminum alloy 100 on the connection position of the second aluminum alloy 200, puts the welding nail 300 into the through hole 110, and uses a resistance spot welding machine to spot weld the welding nail 300. During welding, the welding nail 300 will be melted and pressed into the through hole 110 to fill the gap in the through hole 110. Since the through hole 110 is a large upper and small lower structure, the welding nail 300 forms an annular welding core with the side wall of the through hole 110 after solidification, and the welding nail 300 can form a stable and firm circular welding core with the second aluminum alloy 200. By forming a connection form of double welding core spot welding, the first aluminum alloy 100 and the second aluminum alloy 200 of different grades can be firmly connected together.
[0027] In this embodiment, since the 7 series aluminum alloy contains a considerable amount of low-melting-point zinc, magnesium and other components, this type of super-hard aluminum alloy has poor weldability and is prone to defects such as pores and thermal cracks during welding. Therefore, it is currently impossible to directly connect them through resistance spot welding.
[0028] When the first aluminum alloy 100 is a 7-series aluminum alloy and the second aluminum alloy 200 is a 5-series or 6-series aluminum alloy, it is difficult to directly weld them together or the welding effect is poor. The welding nail 300 can be made of a 5-series or 6-series aluminum alloy or other materials that can meet the spot welding performance standards of the second aluminum alloy 200, and connected in the above manner to achieve the goal of firmly connecting the first aluminum alloy 100 and the second aluminum alloy 200.
[0029] See also Figure 3 The present invention also provides a welding nail 300, which is a truncated cone structure. The top diameter of the welding nail 300 is larger than the bottom diameter, and the height of the welding nail 300 is larger than the through hole 110, and the radial dimension is smaller than the inner diameter of the corresponding position of the through hole 110. When the welding nail 300 is placed in the through hole 110, the top of the welding nail 300 protrudes outside the through hole 110, and there is a gap between the side wall of the welding nail 300 and the through hole 110. And this structure of large top and small bottom can prevent the welding nail 300 from being reversely placed in the through hole 110, which has a fool-proof effect.
[0030] In some embodiments, the bottom surface of the welding nail 300 is a conical surface, and the center of the circle is raised to form a tip. When using a pressure welding machine for pressure welding, the design of the tip can increase the pressure, so that the tip first pierces the oxide layer on the surface of the second aluminum alloy 200. At the same time, the bottom surface of the welding nail 300 gradually pierces the oxide layer from the center to the surroundings, pushing the cut oxide layer to the surroundings, so as to facilitate the uniform crushing and dispersion of the oxide layer and the discharge of welding gas.
[0031] In some embodiments, the welding nail 300 has a plurality of grooves 310, and the grooves 310 extend from the bottom surface of the welding nail 300 to the side surface of the welding nail 300 until they are connected to the top surface of the welding nail 300. During welding, the pressure welding machine applies pressure to the welding nail 300, pressing the welding nail 300 toward the object to be welded. Due to the presence of the grooves 310, the edges of the notches of the grooves 310 can cut the annular surface oxide layer of the aluminum alloy 100 like a cutting edge, contact the internal aluminum alloy, and evenly crushed aluminum oxide particles are dispersed on the welding surface to form a firm annular weld core. The hydrogen and other gases generated during welding can also be discharged from the grooves 310, avoiding the generation of hydrogen pores and other pore defects in the annular weld core. At the same time, a small part of the cut oxide film can also be blown out by hydrogen and other gases through the grooves 310, reducing the content of oxide film particles in the weld core and further improving the welding quality.
[0032] In some embodiments, the groove 310 includes a plurality of side segments 311 , which are evenly distributed on the sides of the welding nail 300 , and the upper and lower ends of the side segments 311 are connected to the top and bottom surfaces of the welding nail 300 , respectively.
[0033] See also Figure 3 The groove 310 further includes a plurality of bottom surface segments 312, which are radially distributed on the bottom surface of the welding nail 300, and each bottom surface segment 312 is connected to at least one side surface segment 311. By relying on the bottom surface segment 312 and the side surface segment 311, the hydrogen and the oxide layer generated during the bottom surface welding can be discharged, thereby improving the welding effect.
[0034] In a preferred embodiment, the groove 310 further includes a plurality of transverse sections 313 located at the bottom surface of the welding stud 300, and the two ends of the transverse section 313 are respectively connected to the two bottom surface sections 312. When part of the bottom surface section 312 or the side section 311 is blocked, hydrogen and the oxide layer can flow through the transverse section 313 to other bottom surface sections 312 for discharge, thereby avoiding being retained in the weld core and affecting the welding quality.
[0035] In some embodiments, the transverse segment 313 is in an arc shape, and its center coincides with the center of the bottom surface of the welding nail 300. A plurality of transverse segments 313 form a plurality of concentric circles on the bottom surface of the welding nail 300.
[0036] In some embodiments, the bottom surface segment 312 may be connected to two side surface segments 311 at both ends, and in other embodiments, the bottom surface segment 312 may be connected to one side surface segment 311 at one end and to one transverse segment 313 at the other end. In some embodiments, both of the above two connection modes may exist, that is, the two ends of a part of the bottom surface segment 312 are connected to the two side surface segments 311 respectively, and the part of the bottom surface segment 312 is connected to the side surface segment 311 and the transverse segment 313.
[0037] The welding nail structure provided by the present invention is larger at the top and smaller at the bottom, and the corresponding through hole on the first aluminum alloy is also larger at the top and smaller at the bottom. The welding nail and the side wall of the through hole form an annular welding core. At the same time, the welding nail is made of a material that can meet the spot welding performance standards of the second aluminum alloy, and can form a stable and firm circular welding core with the second aluminum alloy. By forming a double welding core spot welding connection, the first aluminum alloy and the second aluminum alloy can be firmly connected together.
[0038] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by any technician familiar with the technical field within the technical scope disclosed by the present invention should be covered within the protection scope of the present invention.
Claims
1. A welding nail, which is used to connect a first aluminum alloy and a second aluminum alloy, and a through hole is opened at the connection position of the first aluminum alloy. It is characterized in that The welding nail is a truncated cone structure, the top diameter of the welding nail is larger than the bottom diameter, and the height of the welding nail is larger than the through hole; the welding nail has a plurality of grooves, and the grooves extend from the bottom surface of the welding nail to the side surface of the welding nail until they are connected to the top surface of the welding nail.
2. The welding stud according to claim 1, It is characterized in that The bottom surface of the welding nail is a conical surface, and the center of the circle is raised to form a tip.
3. The welding stud according to claim 1, It is characterized in that The groove includes a plurality of side segments, the side segments are evenly distributed on the sides of the welding nail, and the upper end and the lower end of the side segment are connected to the top surface and the bottom surface of the welding nail respectively.
4. The welding nail according to claim 3, It is characterized in that The groove further comprises a plurality of bottom surface segments, which are radially distributed on the bottom surface of the welding stud, and each of the bottom surface segments is connected to at least one of the side surface segments.
5. The welding stud according to claim 4, It is characterized in that The groove further comprises a plurality of transverse sections located on the bottom surface of the welding stud, and two ends of the transverse section are respectively connected to two bottom surface sections.
6. The welding stud according to claim 5, It is characterized in that The transverse section is in an arc shape, and the center of the circle coincides with the center of the bottom surface of the welding stud.
7. The welding nail according to claim 6, It is characterized in that The transverse sections form a plurality of concentric circles on the bottom surface of the welding stud.
8. The welding stud according to claim 5, It is characterized in that Two ends of part of the bottom surface segment are respectively connected to the two side surface segments, and part of the bottom surface segment is connected to the side surface segment and the transverse segment.