Production equipment and processes for puncture-resistant films

By setting up detection and judgment units in the puncture-resistant film production equipment, and adjusting production parameters in real time, the problem of equipment parameters being unable to adapt to changes in the physical properties of the film was solved, thereby improving production efficiency and yield.

CN117465021BActive Publication Date: 2026-11-17ZHEJIANG HENGXI ADVANCED MATERIALS TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310254144.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-03-16
Publication Date
2026-11-17
Estimated Expiration
2043-03-16

AI Technical Summary

Technical Problem

Existing technology cannot adjust the equipment parameters in the production process of the next cycle to the corresponding values ​​based on the physical properties of the puncture-resistant film in the current cycle, resulting in low production efficiency.

Method used

The system includes a detection unit and a judgment unit. By detecting parameters such as the film's transparency, stripe density, and thickness, it determines whether the film's physical properties meet the requirements. Based on the reasons for non-compliance, it adjusts the parameters of the blow molding unit, traction unit, constraint unit, and hot pressing unit, including the blown film speed, traction speed, hot pressing roller spacing, and constraint roller group angle.

Benefits of technology

This improved the yield and production efficiency of puncture-resistant films, reduced the generation of defective products, and ensured the quality of finished products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117465021B_ABST
    Figure CN117465021B_ABST
Patent Text Reader

Abstract

This invention relates to the field of film technology, and more particularly to a production equipment and process for puncture-resistant film. The equipment includes: a blow molding unit for blowing out semi-finished film; a feeding unit disposed at the feeding end of the blow molding unit for conveying raw materials to the blow molding unit; a traction unit including several traction roller groups for progressively extruding the semi-finished film into a layered film; a hot pressing unit for hot pressing the layered film output from the traction unit to form a single-layer puncture-resistant film; and a detection unit for testing the physical properties of the puncture-resistant film. The detection unit includes a transparency tester for detecting film transparency, a densitometer for detecting stripe density, and a thickness gauge for detecting film thickness. This invention determines whether the physical properties of the film meet requirements by detecting its transparency, and adjusts the equipment parameters to corresponding values ​​in the next cycle based on the determination result, effectively improving production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of thin film technology, and in particular to a production equipment and process for a puncture-resistant thin film. Background Technology

[0002] A thin film is a thin, flexible, transparent sheet made of plastics, adhesives, rubber, or other materials. Scientifically, a thin film is defined as a two-dimensional material formed by the deposition of atoms, molecules, or ions onto a substrate surface. Examples include optical thin films, composite thin films, superconducting thin films, polyester films, nylon films, and plastic films. Thin films are widely used in the electronics, machinery, and printing industries. Puncture-resistant films are particularly prevalent in the food, pharmaceutical, and chemical industries. However, currently produced puncture-resistant films often suffer from poor adhesion between the two phases and the addition of excessive modifying substances, leading to a decline in the film's physical properties and weakened puncture resistance.

[0003] The puncture resistance of plastic or composite films is a crucial indicator for packaging materials, especially for packaged cooked meat products. For poultry products, the bones pose a significant puncture risk to the packaging material. Therefore, testing the puncture strength of composite films is essential to minimize the impact of external factors on the packaging, preventing spoilage or leakage. Consequently, many food packaging manufacturers and food production companies include puncture strength testing as a mandatory inspection item for their packaging bags.

[0004] Chinese Patent Publication No. CN111114007A discloses a production device and processing technology for puncture-resistant packaging bags. The device includes a processing table. From left to right, a robotic arm assembly, a conveyor belt, and a pressing table are fixedly connected to the upper end of the processing table. A suction cup mechanism is connected to the working end of the robotic arm assembly. A glue applicator is connected to the processing table. The conveyor belt passes through the glue applicator. An inverted "U"-shaped support frame is fixedly connected to the pressing table. A cylinder is fixedly connected to the center of the lower end of the support frame. A hot press plate is connected to the piston end of the cylinder.

[0005] It is evident that existing technologies cannot adjust equipment parameters in the production process of the next cycle to the corresponding values ​​based on the physical properties of the puncture-resistant film in the current cycle, resulting in low production efficiency. Summary of the Invention

[0006] To address this issue, the present invention provides a production equipment and process for puncture-resistant films to overcome the problem in the prior art where the equipment parameters in the production process for the next cycle cannot be adjusted to the corresponding values ​​based on the physical properties of the puncture-resistant film in the current cycle, resulting in low production efficiency.

[0007] On one hand, the present invention provides a production apparatus for puncture-resistant films, comprising: A blow molding unit for blowing out a semi-finished film; the blow molding unit is provided with a discharge slit for allowing the semi-finished film to pass through; A feeding unit is provided at the feeding end of the blow molding unit to convey raw materials to the blow molding unit; The traction unit includes several traction roller groups disposed at the output end of the blow molding unit. Each traction roller group forms an angle at the end away from the blow molding unit to gradually extrude the barrel-shaped semi-finished film output from the blow molding unit into a layered film. The constraint unit includes several constraint roller groups disposed at the output end of the blow molding unit. Each constraint roller group forms an included angle at the end away from the blow molding unit to constrain the width of the semi-finished film when the traction unit extrudes the semi-finished film. Each constraint roller group is disposed between two traction roller groups. A hot-pressing unit is disposed at the output end of the traction unit to perform hot-pressing treatment on the layered film output by the traction unit to form a single-layer puncture-resistant film. The detection unit, which is set at the output end of the hot pressing unit, is used to detect the performance parameters of the puncture-resistant film output by the hot pressing unit, including a transparency tester for detecting the transparency of the film, a densitometer for detecting the stripe density, and a thickness measuring instrument for detecting the thickness of the film. The determination unit, which is connected to each component in the detection unit, is used to determine whether the physical properties of the puncture-resistant film in a single cycle meet the requirements based on the transparency of the puncture-resistant film output by the hot pressing unit in a single cycle, and when it is determined that the physical properties of the puncture-resistant film do not meet the requirements in a single cycle, the reasons for the non-compliance of the physical properties of the puncture-resistant film are determined based on the stripe density and transparency of the puncture-resistant film, respectively. An adjustment unit, which is connected to the blow molding unit, the traction unit, the constraint unit, the hot pressing unit, and the determination unit, is used to adjust the operating parameters of the corresponding components to the corresponding values ​​according to the determined reasons when the determination unit completes the determination of the reasons why the physical properties of the puncture-resistant film in the cycle do not meet the requirements. The operating parameters adjusted by the adjustment unit include the blow molding speed of the blow molding unit, the traction speed of each traction roller group in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit, and the angle between each constraint roller group in the constraint unit and the output direction of the blow molding unit.

[0008] Furthermore, the determination unit determines whether the physical properties of the puncture-resistant film within a single cycle meet the requirements based on the transparency of the puncture-resistant film measured by the detection unit within a single cycle under a first preset condition. The first determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density of the puncture-resistant film; the first determination method satisfies that the transparency of the puncture-resistant film is greater than the second preset standard transparency set by the determination unit. The second determination method is that the determination unit determines that the physical properties of the puncture-resistant film meet the requirements, and controls the detection unit to detect the transparency of the puncture-resistant film in the next cycle; the second determination method satisfies that the transparency of the puncture-resistant film is greater than or equal to the first preset standard transparency set by the determination unit and less than or equal to the second preset standard transparency, wherein the first preset standard transparency is less than the second preset standard transparency. The third determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film; the third determination method satisfies that the transparency of the puncture-resistant film is less than the transparency of the first preset standard. The first preset condition is that the determination unit controls the detection unit to detect the transparency of the puncture-resistant film output by the hot pressing unit within a preset period.

[0009] Furthermore, the determination unit controls the densitometer to detect the stripe density of the puncture-resistant film under the first determination method, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density, wherein... The first cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the puncture-resistant film is stretched, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the first preset standard density and the stripe density set by the determination unit; the first cause determination method satisfies that the stripe density is less than or equal to the first preset standard density. The second cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the material output rate of the blow molding unit is higher than the standard, resulting in damage to the surface of the puncture-resistant film. Based on the difference between the stripe density and the first preset standard density, the blow molding speed of the blow molding unit is adjusted to the corresponding value. The second cause determination method satisfies that the stripe density is greater than the first preset standard density and less than or equal to the second preset standard density set by the determination unit, wherein the first preset standard density is less than the second preset standard density. The third cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the width of the puncture-resistant film does not meet the requirements, and adjusts the angle between the constraint roller group and the output direction of the blow molding unit to the corresponding value according to the difference between the stripe density and the second preset standard density; the third cause determination method satisfies that the stripe density is greater than the second preset standard density.

[0010] Furthermore, the determination unit, under the third determination method, determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film. The fourth cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the distance between the two hot-pressing rollers of the hot-pressing unit does not meet the requirements. It then controls the thickness measuring instrument to detect the thickness of the puncture-resistant film and adjusts the distance between the two hot-pressing rollers of the hot-pressing unit to the corresponding value based on the difference between the thickness of the puncture-resistant film and the preset standard thickness set by the determination unit. The fourth cause determination method satisfies the condition that the difference between the first preset standard transparency and the transparency of the puncture-resistant film is less than or equal to the preset excessive difference set by the determination unit. The fifth cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the traction speed of the traction unit does not meet the requirements, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the thickness of the puncture-resistant film and the preset standard thickness; the fifth cause determination method satisfies that the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film is greater than the preset excessive difference.

[0011] Furthermore, under the first cause determination method, the adjustment unit determines the adjustment method of the traction speed of the traction unit based on the difference between the first preset standard density and the stripe density, wherein, The first traction speed adjustment method is that the adjustment unit uses a first traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the first traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is less than or equal to the first preset density too low difference set by the adjustment unit. The second traction speed adjustment method is that the adjustment unit uses a second traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the second traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference set by the adjustment unit, wherein the first preset density too low difference is less than the second preset density too low difference. The third traction speed adjustment method is that the adjustment unit uses a third traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the third traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the difference of the second preset density being too low.

[0012] Furthermore, under the second cause determination method, the adjustment unit determines the adjustment method of the blown film speed of the blow molding unit based on the difference between the stripe density and the first preset standard density, wherein, The first blown film speed adjustment method is that the adjustment unit uses a first blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the first blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is less than or equal to the first preset density too low difference. The second blown film speed adjustment method is that the adjustment unit uses a second blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the second blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference; The third blown film speed adjustment method is that the adjustment unit uses a third blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the third blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the difference of the second preset density being too low.

[0013] Furthermore, under the third cause determination method, the adjustment unit determines the adjustment method of the angle between the constraint roller group and the output direction of the blow molding unit based on the difference between the stripe density and the second preset standard density, wherein, The first angle adjustment method is that the adjustment unit uses a first angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the first angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is less than or equal to the first preset density too high difference set by the adjustment unit; The second angle adjustment method is that the adjustment unit uses a second angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the second angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the first preset density too high difference and less than or equal to the second preset density too high difference set by the adjustment unit, wherein the first preset density too high difference is less than the second preset density too high difference; The third angle adjustment method is that the adjustment unit uses a third angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the third angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the second preset density too high difference.

[0014] Furthermore, under the fourth cause determination method, the adjustment unit determines the adjustment method of the distance between the two hot-pressing rollers in the hot-pressing unit based on the difference between the thickness of the puncture-resistant film and the preset standard thickness, wherein, The first spacing adjustment method is that the adjustment unit uses a first spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to a corresponding value; the first spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference set by the adjustment unit. The second spacing adjustment method is that the adjustment unit uses a second spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to the corresponding value; the second spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference set by the adjustment unit, wherein the first preset thickness difference is less than the second preset thickness difference; The third spacing adjustment method is that the adjustment unit uses a third spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to the corresponding value; the third spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

[0015] Furthermore, under the fifth cause determination method, the adjustment unit determines the adjustment method of the traction speed of the traction unit based on the difference between the thickness of the anti-puncture film and the preset standard thickness, wherein, The fourth traction speed adjustment method is that the adjustment unit uses a fourth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fourth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference. The fifth traction speed adjustment method is that the adjustment unit uses a fifth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fifth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference; The sixth traction speed adjustment method is that the adjustment unit uses a sixth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the sixth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

[0016] On the other hand, the present invention provides a process for producing a puncture-resistant film, comprising: Step S1: After dispersing and mixing the raw materials, the mixture is added to the feeding unit, and the feeding unit conveys the mixture to the blow molding unit. In step S2, after the mixture is melted in the blow molding unit, it is blown out through the discharge gap to obtain a semi-finished film. The blow molding unit conveys the semi-finished film to the traction unit, which gradually extrudes the barrel-shaped semi-finished film into a layered film. The traction unit conveys the layered film to the hot pressing unit, which performs hot pressing on the layered film to form a single-layer puncture-resistant film. In step S3, the hot pressing unit delivers the manufactured puncture-resistant film to the detection unit, which detects the transparency, stripe density, and film thickness of the puncture-resistant film. Step S4: The determination unit determines whether the physical properties of the puncture-resistant film meet the requirements in a single cycle based on the transparency of the puncture-resistant film. When the physical properties of the puncture-resistant film meet the requirements in a single cycle, the detection unit is controlled to detect the transparency of the puncture-resistant film in the next cycle. When the physical properties of the puncture-resistant film do not meet the requirements in a single cycle, the reason why the physical properties of the puncture-resistant film do not meet the requirements is determined based on the stripe density of the puncture-resistant film and the difference between the transparency of the puncture-resistant film and the transparency of the second preset standard. Step S5: The adjustment unit adjusts the blown film speed of the blow molding unit, the traction speed of each traction roller group in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit, and the angle between each constraint roller group in the constraint unit and the output direction of the blow molding unit to the corresponding values ​​according to the results output by the determination unit.

[0017] Compared with the prior art, the beneficial effects of the present invention are as follows: The present invention is equipped with a detection unit. After the puncture-resistant film is prepared in a single cycle, the detection unit detects its transparency. The judgment unit compares the measured transparency with the preset standard transparency and determines whether the physical properties of the puncture-resistant film meet the requirements based on the comparison results, effectively ensuring the quality of the finished product. At the same time, when it is determined that the physical properties of the puncture-resistant film do not meet the requirements, the adjustment unit of the present invention adjusts the parameters of the corresponding equipment in the next cycle, effectively ensuring the yield of the puncture-resistant film, reducing the generation of defective products, and further improving production efficiency.

[0018] Furthermore, by setting up a detection unit, the present invention detects the transparency of the film after it is prepared in a single cycle. By comparing the measured transparency with the preset standard transparency, it is determined whether the physical properties of the produced puncture-resistant film meet the requirements. By timely detecting the transparency, the yield rate is effectively guaranteed, and the generation of a large number of defective products due to untimely detection is avoided.

[0019] Furthermore, when the physical properties of the puncture-resistant film are determined to be non-compliant, the present invention determines the cause of the non-compliance by detecting the stripe density of the puncture-resistant film, analyzes the causes by observing the phenomena on the surface of the puncture-resistant film, and makes different adjustments for different causes, thereby effectively improving the yield of the puncture-resistant film and further improving the production efficiency of the equipment described in the present invention.

[0020] Furthermore, when the physical properties of the puncture-resistant film are determined to be non-compliant, the present invention determines the reasons for the non-compliance based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film. The reasons include non-compliance of the distance between the two hot-pressing rollers of the hot-pressing unit and non-compliance of the traction speed of the traction unit. Different adjustments are made for different reasons, thereby effectively improving the yield of the puncture-resistant film and further improving the production efficiency of the equipment of the present invention.

[0021] Furthermore, when the present invention determines that the physical properties of the puncture-resistant film do not meet the requirements because the puncture-resistant film is stretched, it reduces the traction speed of the traction unit to prevent stretching, thereby ensuring that the transparency of the produced puncture-resistant film meets the requirements. This effectively ensures the product qualification rate and further improves the production efficiency of the equipment described in the present invention.

[0022] Furthermore, in this invention, if the physical properties of the puncture-resistant film are determined to be unsatisfactory because the material output rate of the blow molding unit is higher than the standard, resulting in damage to the surface of the puncture-resistant film, the present invention can adjust the blowing speed of the blow molding unit to make the film uniform and undamaged, thereby effectively improving the production efficiency of the equipment described in this invention.

[0023] Furthermore, when the present invention determines that the physical properties of the puncture-resistant film do not meet the requirements because the width of the puncture-resistant film does not meet the requirements, it adjusts the angle between the constraint roller group and the output direction of the blow molding unit to make the length of the film within a reasonable range, thereby making the transparency of the puncture-resistant film meet the requirements. By adjusting the film width, it effectively ensures that the film is not stretched, thereby making the obtained puncture-resistant film meet the requirements, and further improving the production efficiency of the equipment described in the present invention.

[0024] Furthermore, when the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the distance between the two hot-pressing rollers of the hot-pressing unit does not meet the requirements, the present invention adjusts the distance between the hot-pressing rollers to make the thickness of the film meet the requirements, thereby avoiding the film being too thick and affecting the transparency, thus making the puncture-resistant film meet the requirements and effectively improving the production efficiency of the equipment of the present invention.

[0025] Furthermore, when the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the traction speed of the traction unit does not meet the requirements, resulting in an excessively thick film that affects transparency, the present invention increases the traction speed to prevent the accumulation of raw materials, thereby ensuring that the thickness of the film meets the requirements and its transparency meets the requirements, thus effectively improving the production efficiency of the equipment described in the present invention. Attached Figure Description

[0026] Figure 1 This is a side view of the equipment for producing the puncture-resistant film according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the blow molding unit according to an embodiment of the present invention; Figure 3 This is a schematic diagram of the constraint unit in an embodiment of the present invention; Figure 4 This is a flowchart illustrating the production process of the puncture-resistant film according to an embodiment of the present invention. Detailed Implementation

[0027] To make the objectives and advantages of the present invention clearer, the present invention will be further described below with reference to embodiments; it should be understood that the specific embodiments described herein are merely for explaining the present invention and are not intended to limit the present invention.

[0028] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are merely illustrative of the technical principles of the present invention and are not intended to limit the scope of protection of the present invention.

[0029] It should be noted that in the description of this invention, the terms "upper", "lower", "left", "right", "inner", "outer", etc., which indicate directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings. This is only for the convenience of description and is not intended to indicate or imply that the device or element must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, it should not be construed as a limitation of this invention.

[0030] Furthermore, it should be noted that, in the description of this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.

[0031] Please see Figure 1 and Figure 2 The figures shown are a side view of the puncture-resistant film production equipment according to an embodiment of the present invention and a structural schematic diagram of the blow molding unit according to an embodiment of the present invention. The puncture-resistant film production equipment of the present invention includes: Blow molding unit 1 is used to blow out a semi-finished film; the blow molding unit 1 is provided with a discharge slit 11 for allowing the semi-finished film to pass through; Feeding unit 2 is disposed at the feeding end of the blow molding unit 1 and is used to convey raw materials to the blow molding unit 1; The traction unit (not shown in the figure) includes several traction roller groups 31 arranged at the output end of the blow molding unit 1. Each traction roller group 31 forms an angle at the end away from the blow molding unit 1 to gradually extrude the barrel-shaped semi-finished film output from the blow molding unit 1 into a layered film. The constraint unit (not shown in the figure) includes several constraint roller groups 41 disposed at the output end of the blow molding unit. Each constraint roller group 41 forms an included angle at the end away from the blow molding unit 1 to constrain the width of the semi-finished film when the traction unit 3 extrudes the semi-finished film. Each constraint roller group 41 is disposed between two traction roller groups 31. Please see Figure 3 As shown, it is a structural schematic diagram of the constraint unit in an embodiment of the present invention. Each constraint roller group 41 adjusts the angle between each constraint roller group 41 and the output direction of the blow molding unit 1 through the sliding gear 42 and the connecting rod 43. Hot pressing unit 5 is disposed at the output end of the traction unit 3 and is used to hot press the layered film output by the traction unit 3 to form a single-layer puncture-resistant film. The detection unit, which is located at the output end of the hot pressing unit 5, is used to detect the performance parameters of the puncture-resistant film output by the hot pressing unit 5, including a transparency tester (not shown in the figure) for detecting the transparency of the film, a densitometer (not shown in the figure) for detecting the stripe density, and a thickness measuring instrument (not shown in the figure) for detecting the thickness of the film. The determination unit (not shown in the figure) is connected to each component in the detection unit. It is used to determine whether the physical properties of the anti-puncture film in a single cycle meet the requirements based on the transparency of the anti-puncture film output by the hot pressing unit 5 in a single cycle. When it is determined that the physical properties of the anti-puncture film in a single cycle do not meet the requirements, the reasons for the failure to meet the requirements are determined based on the stripe density and transparency of the anti-puncture film, respectively. An adjustment unit (not shown in the figure) is connected to the blow molding unit 1, the traction unit, the constraint unit, the hot pressing unit 5, and the determination unit. When the determination unit determines the reason why the physical properties of the puncture-resistant film in the cycle do not meet the requirements, the adjustment unit adjusts the operating parameters of the corresponding components to the corresponding values ​​according to the determined reason. The operating parameters adjusted by the adjustment unit include the blow molding speed of the blow molding unit 1, the traction speed of each traction roller group 31 in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit 5, and the angle between each constraint roller group 41 in the constraint unit and the output direction of the blow molding unit 1.

[0032] Specifically, the determination unit determines whether the physical properties of the puncture-resistant film within a single cycle meet the requirements based on the transparency of the puncture-resistant film measured by the detection unit within a single cycle under a first preset condition. The first determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density of the puncture-resistant film; the first determination method satisfies that the transparency of the puncture-resistant film is greater than the second preset standard transparency set by the determination unit. The second determination method is that the determination unit determines that the physical properties of the puncture-resistant film meet the requirements, and controls the detection unit to detect the transparency of the puncture-resistant film in the next cycle; the second determination method satisfies that the transparency of the puncture-resistant film is greater than or equal to the first preset standard transparency set by the determination unit and less than or equal to the second preset standard transparency, wherein the first preset standard transparency is less than the second preset standard transparency. The third determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film; the third determination method satisfies that the transparency of the puncture-resistant film is less than the transparency of the first preset standard. The first preset condition is that the determination unit controls the detection unit to detect the transparency of the puncture-resistant film output by the hot-pressing unit 5 within a preset period.

[0033] Specifically, the determination unit controls the densitometer to detect the stripe density of the puncture-resistant film under the first determination method, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density. The first cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the puncture-resistant film is stretched, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the first preset standard density and the stripe density set by the determination unit; the first cause determination method satisfies that the stripe density is less than or equal to the first preset standard density. The second cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the material output rate of the blow molding unit 1 is higher than the standard, resulting in damage to the surface of the puncture-resistant film. Based on the difference between the stripe density and the first preset standard density, the blow molding speed of the blow molding unit 1 is adjusted to the corresponding value. The second cause determination method satisfies that the stripe density is greater than the first preset standard density and less than or equal to the second preset standard density set by the determination unit, wherein the first preset standard density is less than the second preset standard density. The third cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the width of the puncture-resistant film does not meet the requirements, and adjusts the angle between the constraint roller group 41 and the output direction of the blow molding unit 1 to the corresponding value according to the difference between the stripe density and the second preset standard density; the third cause determination method satisfies that the stripe density is greater than the second preset standard density.

[0034] Specifically, the determination unit, under the third determination method, determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film. The fourth cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the distance between the two hot-pressing rollers of the hot-pressing unit 5 does not meet the requirements. It then controls the thickness measuring instrument to detect the thickness of the puncture-resistant film and adjusts the distance between the two hot-pressing rollers of the hot-pressing unit 5 to the corresponding value based on the difference between the thickness of the puncture-resistant film and the preset standard thickness set by the determination unit. The fourth cause determination method satisfies the condition that the difference between the first preset standard transparency and the transparency of the puncture-resistant film is less than or equal to the preset excessive difference set by the determination unit. The fifth cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the traction speed of the traction unit does not meet the requirements, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the thickness of the puncture-resistant film and the preset standard thickness; the fifth cause determination method satisfies that the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film is greater than the preset excessive difference.

[0035] Specifically, under the first cause determination method, the adjustment unit determines the adjustment method of the traction unit's traction speed based on the difference between the first preset standard density and the stripe density, wherein... The first traction speed adjustment method is that the adjustment unit uses a first traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the first traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is less than or equal to the first preset density too low difference set by the adjustment unit. The second traction speed adjustment method is that the adjustment unit uses a second traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the second traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference set by the adjustment unit, wherein the first preset density too low difference is less than the second preset density too low difference. The third traction speed adjustment method is that the adjustment unit uses a third traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the third traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the difference of the second preset density being too low.

[0036] Specifically, under the second cause determination method, the adjustment unit determines the adjustment method of the blown film speed of the blow molding unit 1 based on the difference between the stripe density and the first preset standard density, wherein, The first blown film speed adjustment method is that the adjustment unit uses a first blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the first blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is less than or equal to the first preset density too low difference. The second blown film speed adjustment method is that the adjustment unit uses a second blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the second blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference; The third blown film speed adjustment method is that the adjustment unit uses a third blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the third blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the difference of the second preset density being too low.

[0037] Specifically, under the third cause determination method, the adjustment unit determines the adjustment method of the angle between the constraint roller group 41 and the output direction of the blow molding unit 1 based on the difference between the stripe density and the second preset standard density, wherein, The first angle adjustment method is that the adjustment unit uses a first angle adjustment coefficient to adjust the angle between the constraint roller group 41 and the output direction of the blow molding unit 1 to a corresponding value; the first angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is less than or equal to the first preset density too high difference set by the adjustment unit; The second angle adjustment method is that the adjustment unit uses a second angle adjustment coefficient to adjust the angle between the constraint roller group 41 and the output direction of the blow molding unit 1 to a corresponding value; the second angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the first preset density too high difference and less than or equal to the second preset density too high difference set by the adjustment unit, wherein the first preset density too high difference is less than the second preset density too high difference. The third angle adjustment method is that the adjustment unit uses a third angle adjustment coefficient to adjust the angle between the constraint roller group 41 and the output direction of the blow molding unit 1 to a corresponding value; the third angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the second preset density too high difference.

[0038] Specifically, under the fourth cause determination method, the adjustment unit determines the adjustment method of the distance between the two hot pressing rollers in the hot pressing unit 5 based on the difference between the thickness of the puncture-resistant film and the preset standard thickness. The first spacing adjustment method is that the adjustment unit uses a first spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit 5 to the corresponding value; the first spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference set by the adjustment unit. The second spacing adjustment method is that the adjustment unit uses a second spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit 5 to the corresponding value; the second spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference set by the adjustment unit, wherein the first preset thickness difference is less than the second preset thickness difference; The third spacing adjustment method is that the adjustment unit uses a third spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit 5 to the corresponding value; the third spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

[0039] Specifically, under the fifth cause determination method, the adjustment unit determines the adjustment method of the traction speed of the traction unit based on the difference between the thickness of the anti-puncture film and the preset standard thickness, wherein, The fourth traction speed adjustment method is that the adjustment unit uses a fourth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fourth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference. The fifth traction speed adjustment method is that the adjustment unit uses a fifth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fifth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference; The sixth traction speed adjustment method is that the adjustment unit uses a sixth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the sixth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

[0040] Please see Figure 4 The diagram shows a flowchart of the production process of the puncture-resistant film according to an embodiment of the present invention. The present invention provides a production process for an puncture-resistant film, comprising: Step S1: After dispersing and mixing the raw materials, the mixture is added to the feeding unit, and the feeding unit conveys the mixture to the blow molding unit 1. In step S2, the mixture is melted in the blow molding unit 1 and blown out through the discharge gap to obtain a semi-finished film. The blow molding unit 1 transports the semi-finished film to the traction unit, which gradually extrudes the barrel-shaped semi-finished film into a layered film. The traction unit transports the layered film to the hot pressing unit 5, which performs hot pressing on the layered film to form a single-layer puncture-resistant film. In step S3, the hot pressing unit 5 delivers the manufactured puncture-resistant film to the detection unit, which detects the transparency, stripe density, and film thickness of the puncture-resistant film. Step S4: The determination unit determines whether the physical properties of the puncture-resistant film meet the requirements in a single cycle based on the transparency of the puncture-resistant film. When the physical properties of the puncture-resistant film meet the requirements in a single cycle, the detection unit is controlled to detect the transparency of the puncture-resistant film in the next cycle. When the physical properties of the puncture-resistant film do not meet the requirements in a single cycle, the reason why the physical properties of the puncture-resistant film do not meet the requirements is determined based on the stripe density of the puncture-resistant film and the difference between the transparency of the puncture-resistant film and the transparency of the second preset standard. In step S5, the adjustment unit adjusts the blown film speed of the blow molding unit 1, the traction speed of each traction roller group 31 in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit 5, and the angle between each constraint roller group 41 in the constraint unit and the output direction of the blow molding unit 1 to the corresponding values ​​according to the results output by the determination unit.

[0041] It should be noted that the data in the above embodiments are all derived from a comprehensive analysis and evaluation of historical test data and corresponding historical test results from the three months prior to this test using the puncture-resistant film production process described in this invention. The puncture-resistant film production process described in this invention satisfies the relationship between the operating parameters of the puncture-resistant film production equipment in a cumulative total of 63,218 cycles during the three months prior to this test. Those skilled in the art will understand that the determination method for any of the above parameters in the puncture-resistant film production process described in this invention can be based on the value with the highest percentage in the data distribution, as long as the values ​​obtainable by the method described in this invention clearly define the different specific situations in the individual judgment process.

[0042] The technical solution of the present invention has been described above with reference to the preferred embodiments shown in the accompanying drawings. However, it will be readily understood by those skilled in the art that the scope of protection of the present invention is obviously not limited to these specific embodiments. Without departing from the principles of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will all fall within the scope of protection of the present invention.

[0043] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A production equipment for puncture-resistant film, characterized in that, include: A blow molding unit for blowing out a semi-finished film; the blow molding unit is provided with a discharge slit for allowing the semi-finished film to pass through; A feeding unit is provided at the feeding end of the blow molding unit to convey raw materials to the blow molding unit; The traction unit includes several traction roller groups disposed at the output end of the blow molding unit. Each traction roller group forms an angle at the end away from the blow molding unit to gradually extrude the cylindrical semi-finished film output from the blow molding unit into a layered film. The constraint unit includes several constraint roller groups disposed at the output end of the blow molding unit. Each constraint roller group forms an included angle at the end away from the blow molding unit to constrain the width of the semi-finished film when the traction unit extrudes the semi-finished film. Each constraint roller group is disposed between two traction roller groups. A hot-pressing unit is disposed at the output end of the traction unit to perform hot-pressing treatment on the layered film output by the traction unit to form a single-layer puncture-resistant film. The detection unit, which is set at the output end of the hot pressing unit, is used to detect the performance parameters of the puncture-resistant film output by the hot pressing unit, including a transparency tester for detecting the transparency of the film, a densitometer for detecting the stripe density, and a thickness measuring instrument for detecting the thickness of the film. The determination unit, which is connected to each component in the detection unit, is used to determine whether the physical properties of the puncture-resistant film in a single cycle meet the requirements based on the transparency of the puncture-resistant film output by the hot pressing unit in a single cycle, and when it is determined that the physical properties of the puncture-resistant film do not meet the requirements in a single cycle, the reasons for the non-compliance of the physical properties of the puncture-resistant film are determined based on the stripe density and transparency of the puncture-resistant film, respectively. An adjustment unit, which is connected to the blow molding unit, the traction unit, the constraint unit, the hot pressing unit, and the determination unit, is used to adjust the operating parameters of the corresponding components to the corresponding values ​​according to the determined reasons when the determination unit completes the determination of the reasons why the physical properties of the puncture-resistant film in the cycle do not meet the requirements. The operating parameters adjusted by the adjustment unit include the blow molding speed of the blow molding unit, the traction speed of each traction roller group in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit, and the angle between each constraint roller group in the constraint unit and the output direction of the blow molding unit. The determination unit determines whether the physical properties of the puncture-resistant film within a single cycle meet the requirements based on the transparency of the puncture-resistant film measured by the detection unit within a single cycle under a first preset condition. The first determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density of the puncture-resistant film; the first determination method satisfies that the transparency of the puncture-resistant film is greater than the second preset standard transparency set by the determination unit. The second determination method is that the determination unit determines that the physical properties of the puncture-resistant film meet the requirements, and controls the detection unit to detect the transparency of the puncture-resistant film in the next cycle; the second determination method satisfies that the transparency of the puncture-resistant film is greater than or equal to the first preset standard transparency set by the determination unit and less than or equal to the second preset standard transparency, wherein the first preset standard transparency is less than the second preset standard transparency. The third determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the first preset standard transparency and the transparency of the puncture-resistant film; the third determination method satisfies that the transparency of the puncture-resistant film is less than the first preset standard transparency. The first preset condition is that the determination unit controls the detection unit to detect the transparency of the puncture-resistant film output by the hot pressing unit within a preset period.

2. The puncture-resistant film production equipment according to claim 1, characterized in that, The determination unit controls the densitometer to detect the stripe density of the puncture-resistant film under the first determination method, and determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the stripe density. The first cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the puncture-resistant film is stretched, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the first preset standard density and the stripe density set by the determination unit; the first cause determination method satisfies that the stripe density is less than or equal to the first preset standard density. The second cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the material output rate of the blow molding unit is higher than the standard, resulting in damage to the surface of the puncture-resistant film. Based on the difference between the stripe density and the first preset standard density, the blow molding speed of the blow molding unit is adjusted to the corresponding value. The second cause determination method satisfies that the stripe density is greater than the first preset standard density and less than or equal to the second preset standard density set by the determination unit, wherein the first preset standard density is less than the second preset standard density. The third cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the width of the puncture-resistant film does not meet the requirements, and adjusts the angle between the constraint roller group and the output direction of the blow molding unit to the corresponding value according to the difference between the stripe density and the second preset standard density; the third cause determination method satisfies that the stripe density is greater than the second preset standard density.

3. The puncture-resistant film production equipment according to claim 2, characterized in that, The determination unit, under the third determination method, determines the reason why the physical properties of the puncture-resistant film do not meet the requirements based on the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film. The fourth cause determination method is as follows: the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the distance between the two hot-pressing rollers of the hot-pressing unit does not meet the requirements. It then controls the thickness measuring instrument to detect the thickness of the puncture-resistant film and adjusts the distance between the two hot-pressing rollers of the hot-pressing unit to the corresponding value based on the difference between the thickness of the puncture-resistant film and the preset standard thickness set by the determination unit. The fourth cause determination method satisfies the condition that the difference between the first preset standard transparency and the transparency of the puncture-resistant film is less than or equal to the preset excessive difference set by the determination unit. The fifth cause determination method is that the determination unit determines that the physical properties of the puncture-resistant film do not meet the requirements because the traction speed of the traction unit does not meet the requirements, and adjusts the traction speed of the traction unit to the corresponding value according to the difference between the thickness of the puncture-resistant film and the preset standard thickness; the fifth cause determination method satisfies that the difference between the transparency of the first preset standard and the transparency of the puncture-resistant film is greater than the preset excessive difference.

4. The puncture-resistant film production equipment according to claim 3, characterized in that, The adjustment unit determines the adjustment method of the traction speed of the traction unit based on the difference between the first preset standard density and the stripe density under the first cause determination method, wherein, The first traction speed adjustment method is that the adjustment unit uses a first traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the first traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is less than or equal to the first preset density too low difference set by the adjustment unit. The second traction speed adjustment method is that the adjustment unit uses a second traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the second traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference set by the adjustment unit, wherein the first preset density too low difference is less than the second preset density too low difference. The third traction speed adjustment method is that the adjustment unit uses a third traction speed adjustment coefficient to reduce the traction speed of the traction unit to a corresponding value; the third traction speed adjustment method satisfies that the difference between the first preset standard density and the stripe density is greater than the difference of the second preset density being too low.

5. The puncture-resistant film production equipment according to claim 4, characterized in that, The adjustment unit determines the adjustment method of the blown film speed of the blow molding unit based on the difference between the stripe density and the first preset standard density under the second cause determination method, wherein, The first blown film speed adjustment method is that the adjustment unit uses a first blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the first blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is less than or equal to the first preset density too low difference. The second blown film speed adjustment method is that the adjustment unit uses a second blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the second blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the first preset density too low difference and less than or equal to the second preset density too low difference; The third blown film speed adjustment method is that the adjustment unit uses a third blown film speed adjustment coefficient to adjust the blown film speed of the blow molding unit to a corresponding value; the third blown film speed adjustment method satisfies that the difference between the stripe density and the first preset standard density is greater than the difference of the second preset density being too low.

6. The puncture-resistant film production equipment according to claim 5, characterized in that, Under the third cause determination method, the adjustment unit determines the adjustment method of the angle between the constraint roller group and the output direction of the blow molding unit based on the difference between the stripe density and the second preset standard density. The first angle adjustment method is that the adjustment unit uses a first angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the first angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is less than or equal to the first preset density too high difference set by the adjustment unit; The second angle adjustment method is that the adjustment unit uses a second angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the second angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the first preset density too high difference and less than or equal to the second preset density too high difference set by the adjustment unit, wherein the first preset density too high difference is less than the second preset density too high difference; The third angle adjustment method is that the adjustment unit uses a third angle adjustment coefficient to adjust the angle between the constraint roller group and the output direction of the blow molding unit to a corresponding value; the third angle adjustment method satisfies that the difference between the stripe density and the second preset standard density is greater than the second preset density too high difference.

7. The puncture-resistant film production equipment according to claim 6, characterized in that, The adjustment unit, under the fourth cause determination method, determines the adjustment method of the distance between the two hot-pressing rollers in the hot-pressing unit based on the difference between the thickness of the puncture-resistant film and the preset standard thickness. The first spacing adjustment method is that the adjustment unit uses a first spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to a corresponding value; the first spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference set by the adjustment unit. The second spacing adjustment method is that the adjustment unit uses a second spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to the corresponding value; the second spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference set by the adjustment unit, wherein the first preset thickness difference is less than the second preset thickness difference; The third spacing adjustment method is that the adjustment unit uses a third spacing adjustment coefficient to adjust the spacing between the two hot pressing rollers in the hot pressing unit to the corresponding value; the third spacing adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

8. The equipment for producing puncture-resistant film according to claim 7, characterized in that, Under the fifth cause determination method, the adjustment unit determines the adjustment mode of the traction speed of the traction unit based on the difference between the thickness of the anti-puncture film and the preset standard thickness, wherein... The fourth traction speed adjustment method is that the adjustment unit uses a fourth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fourth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is less than or equal to the first preset thickness difference. The fifth traction speed adjustment method is that the adjustment unit uses a fifth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the fifth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the first preset thickness difference and less than or equal to the second preset thickness difference; The sixth traction speed adjustment method is that the adjustment unit uses a sixth traction speed adjustment coefficient to increase the traction speed of the traction unit to a corresponding value; the sixth traction speed adjustment method satisfies that the difference between the thickness of the puncture-resistant film and the preset standard thickness is greater than the second preset thickness difference.

9. A process for producing an anti-puncture film using a production equipment based on the anti-puncture film of any one of claims 1-8, characterized in that, include: Step S1: After dispersing and mixing the raw materials, the mixture is added to the feeding unit, and the feeding unit conveys the mixture to the blow molding unit. Step S2: After the mixture is melted in the blow molding unit, it is blown out through the discharge gap to obtain a semi-finished film. The blow molding unit conveys the semi-finished film to the traction unit. The traction unit gradually extrudes the cylindrical semi-finished film into a layered film. The traction unit conveys the layered film to the hot pressing unit. The hot pressing unit performs hot pressing treatment on the layered film to form a single-layer puncture-resistant film. In step S3, the hot pressing unit delivers the manufactured puncture-resistant film to the detection unit, which detects the transparency, stripe density, and film thickness of the puncture-resistant film. Step S4: The determination unit determines whether the physical properties of the puncture-resistant film meet the requirements in a single cycle based on the transparency of the puncture-resistant film. When the physical properties of the puncture-resistant film meet the requirements in a single cycle, the detection unit is controlled to detect the transparency of the puncture-resistant film in the next cycle. When the physical properties of the puncture-resistant film do not meet the requirements in a single cycle, the reasons for the non-compliance of the physical properties of the puncture-resistant film are determined based on the stripe density and transparency of the puncture-resistant film, respectively. Step S5: The adjustment unit adjusts the blown film speed of the blow molding unit, the traction speed of each traction roller group in the traction unit, the distance between the two hot pressing rollers in the hot pressing unit, and the angle between each constraint roller group in the constraint unit and the output direction of the blow molding unit to the corresponding values ​​according to the results output by the determination unit.

Citation Information

Patent Citations

  • Production device for puncture-resistant packaging bag and processing technology thereof

    CN111114007A

  • Method for starting or ending production of film in film machine, film machine and computer program product

    CN114555326A