Preparation method of antireflective coating, molding and antireflective coating

A molding die is formed by aligning and assembling the first and second templates. The anti-glare protrusions and moth-eye protrusions are then formed on the substrate by transfer printing, which solves the problem of high manufacturing difficulty of the molding die and realizes the controllable preparation and excellent reflection effect of the anti-reflection film.

CN117471848BActive Publication Date: 2026-11-17SHENZHEN CHINA STAR OPTOELECTRONICS SEMICON DISPLAY TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310802687.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-30
Publication Date
2026-11-17
Estimated Expiration
2043-06-30

AI Technical Summary

Technical Problem

In the existing antireflective coating process, the molding process is difficult and the reflection effect is uncontrollable.

Method used

A molding die is formed by aligning and assembling a first template and a second template. An anti-reflective film is formed on the substrate by a transfer method. Anti-glare protrusions and moth-eye protrusions are formed by transferring the recesses on the first template and the second template, and the shape and size of the recesses are controlled.

Benefits of technology

The preparation process of the antireflective film was simplified, the manufacturing difficulty was reduced, and the reflection effect of the prepared antireflective film was controllable, thus improving the antireflective effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117471848B_ABST
    Figure CN117471848B_ABST
Patent Text Reader

Abstract

This application discloses a method for preparing an anti-reflective film, a molding die, and an anti-reflective film. The method comprises the following steps: providing a first template, which includes a flat body and a plurality of spaced-apart first recesses; providing a first substrate and forming a material layer on the surface of the first substrate; transferring a pattern on the first substrate to the material layer, forming a second template, which also includes a flat body and a plurality of spaced-apart second recesses; aligning and assembling the first and second templates to form a molding die; during assembly, the second template deforms along with the first recesses of the first template to generate third recesses, the density of the second recesses on the molding die being greater than the density of the third recesses on the molding die; and providing a substrate, transferring the second and third recesses from the molding die to the substrate to form an anti-reflective film. This method overcomes the technical problem of high manufacturing difficulty in the molding die manufacturing process of existing anti-reflective films.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of anti-glare technology, and in particular to a method for preparing an anti-reflective film, a molding process, and the anti-reflective film itself. Background Technology

[0002] Currently, due to the reflection of ambient light on the surface of display devices, strong reflections affect the human eye's visual function, resulting in "glare" during the application of display devices. Anti-reflective coatings are generally used to improve the "glare" problem of display devices.

[0003] In related technologies, the preparation method of antireflective film includes coating a substrate with a resin that is curable by visible light to form a film, transferring the surface shape of the mold onto the film using a die to form a textured film, and then curing the textured film to obtain the antireflective film. Before preparing the antireflective film using this method, a die is prepared by etching a textured structure on the surface of an aluminum substrate. The etching process requires high precision, and it is impossible to control the size and morphology of the textured structure. The die is also difficult to manufacture, and the reflective effect of the antireflective film prepared using the die is uncontrollable. Summary of the Invention

[0004] This application provides a method for preparing an antireflective film, a molding die, and an antireflective film, in order to solve the technical problem of high manufacturing difficulty in the molding die manufacturing process of existing antireflective films.

[0005] To address the above issues, the technical solution provided in this application is as follows: In a first aspect, this application provides a method for preparing an antireflective film, comprising the following steps: A first template is provided, the first template comprising a flat body, and the first template further having a plurality of spaced-apart first recesses; A first substrate is provided, and a material layer is formed on the surface of the first substrate. A pattern on the first substrate is transferred to the material layer, and the material layer forms a second template. The second template includes a flat body and has a plurality of spaced second recesses. The first template and the second template are aligned and assembled to form a mold. During the assembly process, the second template deforms along with the first recess of the first template to generate a third recess. The density of the second recess on the mold is greater than the density of the third recess on the mold. A substrate is provided, and the second and third recesses on the mold are transferred onto the substrate to form an anti-reflective film.

[0006] Optionally, the process may also include the following steps to prepare the first template, specifically: A second substrate is provided, and a material layer is formed on the surface of the second substrate. A pattern on the second substrate is transferred to the material layer, and the material layer forms the first template.

[0007] Optionally, the method further includes the following step: preparing the second substrate using an etching process, wherein the surface of the second substrate has a plurality of first protrusions, and the first protrusions correspond to the first recesses.

[0008] Optionally, the method further includes the following steps: preparing the first substrate using an etching process, wherein the surface of the first substrate has a plurality of second protrusions, and the second protrusions correspond to the second recesses.

[0009] Optionally, the etching process is laser etching, ion beam etching, or electron beam etching.

[0010] Optionally, the material layer may be formed on the surface of the first or second substrate using polydimethylsiloxane or photocurable resin.

[0011] Optionally, the following steps may also be included: A curing material is used to cure the surface of the transferred substrate. Optionally, the second template and the first template are connected by vacuum compression.

[0012] Secondly, embodiments of this application provide a molding die, including: The first template includes a flat body, and the surface of the first template is provided with a plurality of spaced-apart first recesses; The second template includes a flat body. The surface of the second template is provided with a plurality of spaced second recesses. The second template is aligned and connected with the first template. The second template deforms with the first recess of the first template to generate a third recess. The size of the second recess is smaller than the size of the third recess. The number of the first recesses is greater than the number of the third recesses.

[0013] Optionally, the side of the first template near the first recess is glued to the side of the second template away from the second recess.

[0014] Optionally, the first template is made of polydimethylsiloxane or a photocurable resin. And / or, the second template is prepared using polydimethylsiloxane material or photocurable resin material.

[0015] Thirdly, embodiments of this application provide an antireflective film, prepared using the antireflective film preparation method described above, comprising: Substrate; Multiple anti-glare protrusions are spaced apart on the surface of the substrate; Multiple moth-eye protrusions are provided on the surface of each anti-glare protrusion, and multiple moth-eye protrusions are provided on the substrate between adjacent anti-glare protrusions.

[0016] Optionally, the size of the anti-glare protrusion is between 1-5 μm; and / or, the size of the moth-eye protrusion is between 10-100 nm.

[0017] Optionally, the substrate may be made of polyester resin, tricellulose acetate, polymethyl methacrylate, polystyrene, polypropylene, polyethylene and polyvinyl chloride, polycarbonate, polyamide or other hardened resins.

[0018] Beneficial effects: This application discloses a method for preparing an anti-reflective film, a molding die, and an anti-reflective film. A second template is prepared by transfer printing. A first template has multiple first recesses, and a second template has second recesses. The first and second templates are aligned and assembled to form a molding die. During assembly, the second template deforms along with the first recesses of the first template to form a third recess. The molding die is then transferred using a transfer printing method to form an anti-reflective film. The second recesses form the moth-eye protrusions of the anti-reflective film, and the third recesses form the anti-glare protrusions of the anti-reflective film. The preparation process of the anti-reflective film is simple and easy to manufacture, overcoming the technical problem of high manufacturing difficulty of molding dies in the existing anti-reflective film manufacturing process. The shape and size of the first recesses on the first template and the second recesses on the second template are controllable, and the shape and size of the moth-eye protrusions and anti-glare protrusions on the prepared anti-reflective film are also controllable, thereby producing an anti-reflective film with excellent anti-reflection effect. Attached Figure Description

[0019] The technical solution and other beneficial effects of this application will become apparent from the following detailed description of specific embodiments in conjunction with the accompanying drawings.

[0020] Figure 1 This is a schematic cross-sectional view of the compression mold provided in an embodiment of this application.

[0021] Figure 2 This is a cross-sectional schematic diagram of the first template of the compression mold provided in an embodiment of this application.

[0022] Figure 3 This is a cross-sectional schematic diagram of the second template before molding assembly, provided in an embodiment of this application.

[0023] Figure 4 This is a cross-sectional schematic diagram of the second substrate provided in an embodiment of this application.

[0024] Figure 5 This is a cross-sectional schematic diagram of the first substrate provided in an embodiment of this application.

[0025] Figure 6 This is a partial structural schematic diagram of the antireflective film provided in an embodiment of this application.

[0026] Figure 7 This is a side view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application.

[0027] Figure 8 This is a top view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application.

[0028] Figure 9 This is a flowchart illustrating the preparation method of the compression mold provided in an embodiment of this application.

[0029] Figure 10 This is a flowchart illustrating the preparation method of the antireflective film provided in the embodiments of this application.

[0030] Figure 11 This is a flowchart illustrating a method for preparing an antireflective film according to another embodiment of this application. Detailed Implementation

[0031] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.

[0032] Please see Figure 1 , Figure 2 and Figure 3 , Figure 1 This is a schematic cross-sectional view of the compression mold provided in an embodiment of this application. Figure 2 This is a cross-sectional schematic diagram of the first template of the compression mold provided in the embodiments of this application. Figure 3 This is a cross-sectional schematic diagram of the second template before molding assembly, provided in an embodiment of this application.

[0033] This application provides a molding die for preparing an antireflective film 10. The molding die includes a first template 100 and a second template 200. Both the first template 100 and the second template 200 are flat plate structures, which can be rectangular flat plates. The first template 100 has a first side 120 and a second side 130 arranged opposite to each other. The second side 130 has a plurality of spaced-apart first recesses 110. The second template 200 has a third side 230 and a fourth side 240 arranged opposite to each other. The fourth side 240 has a plurality of spaced-apart second recesses 210. The size of the recess 210 is smaller than the size of the first recess 110. The number of second recesses 210 is greater than the number of first recesses 110. The second template 200 is aligned and connected with the first template 100. The second side 130 of the first template 100 is attached to the third side 230 of the second template 200. The second template 200 deforms with the first recess 110 of the first template 100 to generate a third recess 220. The third recess 220 is recessed from the fourth side 240 to the first side 120. The number of third recesses 220 is the same as the number of first recesses 110.

[0034] Please see Figure 6 , Figure 7 and Figure 8 , Figure 6 This is a partial structural diagram of the antireflective film provided in an embodiment of this application. Figure 7 This is a side view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application. Figure 8 This is a top view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application.

[0035] This is understandable; please refer to [link / reference]. Figure 2 and Figure 3 In this application, both the first template 100 and the second template 200 are flat plate structures. A first recess 110, which is hemispherical, is formed on the first template 100. A second recess 210, which is hemispherical or conical, is formed on the second template 200. The second template 200 deforms with the first recess 110 of the first template to form a third recess 220. The preparation methods of the first template 100 and the second template 200 are simple. The morphology and size of the first recess 110 of the first template 100 are controllable, as are the morphology and size of the second recess 210 on the second template 200. The morphology and size of the third recess 220 formed by the deformation of the first recess 110 on the second template 200 are also controllable. The antireflective film prepared by this molding process has a controllable morphology and size, and can produce antireflective films with excellent antireflective effects.

[0036] In order for the second template 200 to adapt to the deformation of the first recess 110 of the first template 100, the material of the second template 200 should have a certain deformation capacity to avoid deformation of the second recess 210 during the deformation process of the second template 200, and to ensure the shape and size of the second recess 210.

[0037] In some embodiments, the side of the first template 100 near the first recess 110 is glued to the side of the second template 200 opposite to the second recess 210.

[0038] The first recess 110 on the first template 100 is recessed from the second side 130 toward the first side 120, and the second recess 210 on the second template 200 is recessed from the fourth side 240 toward the third side 230. Adhesive is applied to the second side 130 of the first template 100 to bond the second side 130 of the first template 100 to the third side 230 of the second template 200. During the alignment and assembly of the first template 100 and the second template 200, vacuum compression is used to deform the second template 200 along with the first recess 110 of the first template 100 to create a third recess 220. The adhesive bonding between the first template 100 and the second template 200 facilitates the molding assembly operation.

[0039] In some embodiments, the first template 100 is made of polydimethylsiloxane (PDMS) or a photocurable resin material; and / or, the second template 200 is made of polydimethylsiloxane (PDMS) or a photocurable resin material.

[0040] Polydimethylsiloxane (PDS) is a hydrophobic organosilicon material. Its chemical state, dimethyl silicone oil, varies depending on its relative molecular mass, ranging from a colorless, transparent volatile liquid to an extremely viscous liquid or silica gel. It is odorless, highly transparent, and possesses heat resistance, cold resistance, minimal viscosity change with temperature, water resistance, low surface tension, and thermal conductivity (0.134-0.159 W / (m·K)). It has 100% light transmittance. Dimethyl silicone oil is non-toxic, odorless, physiologically inert, and exhibits good chemical stability. Photocurable resin materials can be flexible resins, which offer good shaping properties and high surface smoothness.

[0041] Please see Figure 9 , Figure 9 This is a flowchart illustrating the preparation method of the compression mold provided in an embodiment of this application.

[0042] This application provides a method for preparing a compression mold, comprising the following steps: S1, a first template 100 is provided. The first template 100 includes a flat body and a plurality of spaced-apart first recesses 110. Please see Figure 2 The diagram shows the structure of the first template 100 prepared in step S1. The main body of the first template 100 is a flat plate structure. Multiple first recesses 110 are arranged at intervals on the second side 130 of the first template 100. The first recesses 110 are hemispherical and their size is 5-8 μm, which can be 5 μm, 6 μm, 7 μm or 8 μm. It is relatively easy to process the first recesses 110 on the flat first template 100. The shape and size of the first recesses 110 are controllable.

[0043] S2, a first substrate 400 is provided, and a material layer is formed on the surface of the first substrate 400. The pattern on the substrate 400 is transferred to the material layer, and the material layer forms a second template 200. The second template 200 includes a flat body and also has a plurality of spaced second recesses 210. Please see Figure 5 , Figure 5 A cross-sectional schematic diagram of the first substrate 400 provided in an embodiment of this application.

[0044] The first substrate 400 is a flat plate, and the surface of the first substrate 400 is provided with a plurality of nanoscale second protrusions 410. The first substrate 400 is made of rigid plate.

[0045] Please see Figure 3 The diagram shows the structure of the second template 200 prepared in step S2. The second template 200 encloses a flat body. Multiple spaced second recesses 210 are formed on the fourth side 240 of the second template 200. The second recesses 210 are hemispherical, conical, or rectangular, etc. The size of the second recesses 210 is between 10-100 nm, and can be 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm or 100 nm. It is relatively easy to prepare the nanoscale second recesses 210 on the second template 200 by transfer printing. The shape and size of the second recesses 210 are controllable and the processing technology is simple.

[0046] S3, the first template 100 and the second template 200 are aligned and assembled to form a mold. During the assembly process, the second template 200 deforms with the first recess 110 of the first template 100 to generate a third recess 220. The density of the second recess 210 on the mold is greater than the density of the third recess 220 on the mold.

[0047] Please see Figure 1During the alignment and assembly of the first template 100 and the second template 200, the second template 200 deforms along with the first recess 110 of the first template 100, and a third recess 220 is formed at the position corresponding to the first recess 110 of the second template 200. The shape of the third recess 220 is the same as the shape of the first recess 110, which can be hemispherical or conical. The processing method of machining the third recess 220 on the second template 200 is simple. The shape and size of the first recess 110 determine the shape and size of the third recess 220. When the shape and size of the first recess 110 is controllable, the shape and size of the third recess 220 is controllable.

[0048] Understandably, in this embodiment, a flat first template 100 and a second template 200 are first provided, and then the first template 100 and the second template 200 are assembled. During the assembly process, the second template 200 forms a third recess 220. Compared with the related technologies, the preparation method of the mold prepared by electrochemical etching on aluminum sheet is simpler. The shape and size of the second recess 210 and the third recess 220 during the preparation process are controllable, with good flexibility. Customized anti-reflective film 10 production can be realized, and the manufacturing process of the mold is simple.

[0049] In some embodiments, prior to step S1, a first template 100 is prepared, specifically including the following steps: A second substrate 300 is provided, and a material layer is formed on the surface of the second substrate 300. A pattern on the second substrate 300 is transferred to the material layer, and the material layer forms the first template 100.

[0050] Please see Figure 4 , Figure 4 This is a cross-sectional schematic diagram of the second substrate 300 provided in an embodiment of this application.

[0051] The second substrate 300 is a flat plate. The surface of the second substrate 300 is provided with multiple nanoscale first protrusions 310. The first protrusions 310 can form first recesses 110. The second substrate 300 is made of rigid plate material to avoid deformation of the second substrate 300.

[0052] Please see Figure 2 The first template 100 is flat, and the second side 130 of the first template 100 forms a plurality of spaced first recesses 110. The first recesses 110 are hemispherical or conical, etc. It is relatively easy to prepare the micron-level first recesses 110 on the first template 100 by means of transfer printing. The shape and size of the second recesses 210 are controllable and the processing technology is simple.

[0053] In other embodiments, the first template 100 may also be made of a rigid sheet material, and the first recess 110 may be processed by laser etching or electrochemical etching.

[0054] In some implementations, the following steps are also included: The second substrate 300 is prepared by etching process. The surface of the second substrate 300 has a plurality of first protrusions 310, and the first protrusions 310 correspond to the first recesses 110.

[0055] Please see Figure 4 The second substrate 300 has a flat structure and is made of a silicon substrate. A first template 100 is prepared by curing a polydimethylsiloxane material or a photocurable resin on the surface of the second substrate 300. First protrusions 310 form multiple first recesses 110 on the first template 100. The number, shape, and size of the first protrusions 310 on the second substrate 300 are the same as the number, shape, and size of the first recesses 110 on the first template 100. The first protrusions 310 can be hemispherical or conical. Taking a hemispherical shape as an example, the size of the first protrusion 310 is 5-8 μm, specifically 5 μm, 6 μm, 7 μm, or 8 μm. The processing technology of the second substrate 300 is simple, and the shape and size of the first protrusions 310 are controllable, facilitating processing.

[0056] In some implementations, the following steps are also included: The first substrate 400 is prepared by etching process. The surface of the first substrate 400 has a plurality of second protrusions 410, and the second protrusions 410 correspond to the second recesses 210.

[0057] Please see Figure 5 The first substrate 400 is a flat plate structure, fabricated from a silicon substrate. A second template 200 is prepared by curing a polydimethylsiloxane material or a photocurable resin on the surface of the first substrate 400. Second protrusions 410 form multiple second recesses 210 on the second template 200. The number, shape, and size of the second protrusions 410 on the first substrate 400 are the same as the number, shape, and size of the second recesses 210 on the second template 200. The second protrusions 410 are hemispherical, conical, or rectangular. Taking a hemispherical shape as an example, the size of the second protrusions 410 is between 10-100 nm, and can be 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, or 100 nm. The fabrication process of the first substrate 400 is simple, and the shape and size of the second protrusions 410 are controllable, facilitating processing.

[0058] Based on the above implementation method, the etching process is laser etching, ion beam etching, or electron beam etching.

[0059] The first protrusion 310 and the second protrusion 410 are etched on the second substrate 300 and the first substrate 400 respectively by high-precision etching processes such as laser etching, ion beam etching or electron beam etching. The shape and size of the first protrusion 310 and the second protrusion 410 are controllable. Compared with wet etching, the etching processes such as laser etching, ion beam etching or electron beam etching are simple, easy to operate and have high precision.

[0060] Based on the above embodiments, a material layer of the first template 100 is formed on the surface of the second substrate 300 using a polydimethylsiloxane material or a photocurable resin material; and / or, a material layer of the second template 200 is formed on the surface of the first substrate 400 using a polydimethylsiloxane material or a photocurable resin material.

[0061] Polydimethylsiloxane material or photocurable resin is coated on the surfaces of the second substrate 300 and the first substrate 400. After curing, a first template 100 and a second template 200 are prepared. The first template 100 and the second template 200 have good structural stability. The dimethylsiloxane material or the photocurable resin has a certain deformation capability. During the assembly of the first template 100 and the second template 200, it is beneficial for the second template 200 to deform and form a third recess 220. This prevents the second recess 210 from deforming during the assembly process, ensuring the accuracy of the second recess 210 and the third recess 220, and improving the accuracy of the molding.

[0062] In the above embodiment, the second template 200 is connected to the first template 100 by vacuum compression.

[0063] The second template 200 is connected to the first template 100 by vacuum compression, which is beneficial for the second template 200 to deform along the edge of the first recess 110 of the first template 100 to form a third recess 220 that fits the first recess 110. No other tooling or mold is needed, making the assembly of the mold convenient and the processing cost low.

[0064] Please see Figure 10 , Figure 10 This is a flowchart illustrating the preparation method of the antireflective film provided in the embodiments of this application.

[0065] This application provides a method for preparing an antireflective film, comprising: S1, a first template 100 is provided. The first template 100 includes a flat body and a plurality of spaced-apart first recesses 110. S2, a first substrate 400 is provided, and a material layer is formed on the surface of the first substrate 400. The pattern on the substrate 400 is transferred to the material layer, and the material layer forms a second template 200. The second template 200 includes a flat body and also has a plurality of spaced second recesses 210. S3, the first template 100 and the second template 200 are aligned and assembled to form a mold. During the assembly process, the second template 200 deforms with the first recess 110 of the first template 100 to generate a third recess 220. The density of the second recess 210 on the mold is greater than the density of the third recess 220 on the mold. S4, a substrate 11 is provided, and the second recess 210 and the third recess 220 on the mold are transferred onto the substrate 11 to form an anti-reflective film.

[0066] Understandably, the fourth side 240 of the mold is bonded to the surface of the substrate 11, and the shape of the fourth side of the mold is transferred to the surface of the substrate 11. The second recess 210 is transferred to the surface of the substrate 11 to form a moth-eye protrusion 13, and the third recess 220 is transferred to the surface of the substrate 11 to form an anti-glare protrusion 12, thus preparing an anti-reflective film. The anti-reflective film 10 includes a substrate 11, multiple anti-glare protrusions 12, and multiple moth-eye protrusions 13. The processing technology of the anti-reflective film 10 is simple. Since the shape and size of the second recess 210 and the third recess 220 are controllable, the shape and size of the moth-eye protrusions 13 and the anti-glare protrusions 12 are also controllable. The anti-reflective film 10 is prepared by two transfers, and the processing technology of the anti-reflective film 10 is simple and the processing difficulty is low. Furthermore, the size and shape of the anti-glare protrusions 12 and moth-eye protrusions 13 on the anti-reflective film 10 are controllable, which can control the surface roughness, fineness, step difference, and internal and external haze of the anti-reflective film 10. The design is flexible and improves the anti-reflection effect of the anti-reflective film 10.

[0067] Please see Figure 11 , Figure 11 This is a flowchart illustrating a method for preparing an antireflective film according to another embodiment of this application.

[0068] Based on the above embodiments, the method for preparing the antireflective film further includes the following steps: S5, using a curing material, cures the surface of the transferred substrate 11.

[0069] Curing with a curing resin improves the stability and strength of the antireflective film 10. Various UV-curable resins can be used as curing materials. Prepolymers can be polyester-based acrylic resins, as well as epoxy-based acrylic resins, polyurethane-based acrylic resins, polyether-based acrylic resins, etc. Additionally, the curing material contains photoinitiators, antifouling agents, and other additives.

[0070] In some embodiments, prior to step S1, a first template 100 is prepared, specifically including the following steps: A second substrate 300 is provided, and a material layer is formed on the surface of the second substrate 300. A pattern on the second substrate 300 is transferred to the material layer, and the material layer forms the first template 100.

[0071] In some implementations, the following steps are also included: The second substrate 300 is prepared by etching process. The surface of the second substrate 300 has a plurality of first protrusions 310, and the first protrusions 310 correspond to the first recesses 110.

[0072] In some implementations, the following steps are also included: The first substrate 400 is prepared by etching process. The surface of the first substrate 400 has a plurality of second protrusions 410, and the second protrusions 410 correspond to the second recesses 210.

[0073] Based on the above implementation method, the etching process is laser etching, ion beam etching, or electron beam etching.

[0074] Based on the above embodiments, a material layer of the first template 100 is formed on the surface of the second substrate 300 using a polydimethylsiloxane material or a photocurable resin material; and / or, a material layer of the second template 200 is formed on the surface of the first substrate 400 using a polydimethylsiloxane material or a photocurable resin material.

[0075] Please see Figure 6 , Figure 7 and Figure 8 , Figure 6 This is a partial structural schematic diagram of the antireflective film provided in an embodiment of this application. Figure 7 This is a side view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application. Figure 8 This is a top view of the anti-glare protrusion of the anti-reflective film provided in an embodiment of this application.

[0076] This application provides an antireflective film 10, which is prepared using the above-described method for preparing an antireflective film.

[0077] The anti-reflective film 10 includes a substrate 11, multiple anti-glare protrusions 12, and multiple moth-eye protrusions 13. The surface of the substrate 11 is provided with multiple anti-glare protrusions 12, which can be arranged regularly, such as in a matrix along a first direction and a second direction. The anti-glare protrusions 12 serve an anti-glare function. Multiple moth-eye protrusions 13 are provided on the anti-glare protrusions 12. The multiple moth-eye protrusions 13 on a single anti-glare protrusion 12 can be arranged regularly, such as in a matrix along the surface of the anti-glare protrusion 12. The substrate 11 between adjacent anti-glare protrusions 12 is provided with multiple moth-eye protrusions 13, which can be arranged regularly, such as in a matrix along a first direction and a second direction. The moth-eye protrusions 13 serve an anti-reflection function.

[0078] In some embodiments, the size of the anti-glare protrusion 12 is between 1 and 5 μm; and / or, the size of the eye protrusion 13 is between 10 and 100 nm.

[0079] Understandably, the number of anti-glare protrusions 12 is less than the number of moth-eye protrusions 13, and the size of the anti-glare protrusions 12 is larger than the size of the moth-eye protrusions 13. The size of the anti-glare protrusion 12 refers to the diameter of its outline on the substrate 11, and the size of the moth-eye protrusion 13 refers to the diameter of its outline on the substrate 11 or the anti-glare protrusion 12. The size of the anti-glare protrusion 12 is between 1-5 μm, and can be 1 μm, 2 μm, 3 μm, 4 μm, or 5 μm. The size of the moth-eye protrusion 13 is between 10-100 nm, and can be 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, or 100 nm. The structure of the anti-glare protrusion 12 is hemispherical or conical, and the structure of the moth-eye protrusion 13 is hemispherical or conical.

[0080] It is understandable that the size and shape of multiple anti-glare protrusions 12 located on the same substrate 11 may be different, and the size and shape of moth-eye protrusions 13 located on the same substrate 11 may be different.

[0081] In some embodiments, the substrate 11 is selected from commonly used polymeric materials with high light transmittance, such as polyester resin (PET), tricellulose acetate (TAC), polymethyl methacrylate (PMMA), polystyrene (PS), polypropylene (PP), polyethylene (PE), polyvinyl chloride (PVC), polycarbonate (PC), polyamide (PA), or other curable resins.

[0082] This application provides a display panel including the anti-reflective film 10 described above. The display panel can be a liquid crystal display panel, an OLED display panel, an LED display panel, a Micro-LED display panel, a Mini-LED display panel, or other display panels.

[0083] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions in other embodiments.

[0084] The preparation method, molding, and antireflection film of the antireflection film provided in the embodiments of this application have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of this application. The description of the above embodiments is only for the purpose of helping to understand the technical solutions and core ideas of this application. Those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A method for preparing an antireflective film, characterized in that, Includes the following steps: A first template is provided, the first template comprising a flat body, and the first template further having a plurality of spaced-apart first recesses; A first substrate is provided, and a material layer is formed on the surface of the first substrate. A pattern on the first substrate is transferred to the material layer, and the material layer forms a second template. The second template includes a flat body and a plurality of spaced second recesses. The first template and the second template are aligned and assembled to form a mold. During the assembly process, the second template deforms along with the first recess of the first template to generate a third recess. The density of the second recess on the mold is greater than the density of the third recess on the mold. A substrate is provided, and the second and third recesses on the mold are transferred onto the substrate to form an anti-reflective film.

2. The method for preparing the antireflective film according to claim 1, characterized in that, The process also includes the following steps to prepare the first template, specifically: A second substrate is provided, and a material layer is formed on the surface of the second substrate. A pattern on the second substrate is transferred to the material layer, and the material layer forms the first template.

3. The method for preparing the antireflective film according to claim 2, characterized in that, The method also includes the following steps: the second substrate is prepared by an etching process, and the surface of the second substrate has a plurality of first protrusions, the first protrusions corresponding to the first recesses.

4. The method for preparing the antireflective film according to claim 1, characterized in that, The method also includes the following steps: the first substrate is prepared by an etching process, and the surface of the first substrate has a plurality of second protrusions, the second protrusions corresponding to the second recesses.

5. The method for preparing the antireflective film according to claim 3 or 4, characterized in that, The etching process is laser etching, ion beam etching, or electron beam etching.

6. The method for preparing the antireflective film according to claim 2, characterized in that, The material layer is formed on the surface of the first substrate or the second substrate using polydimethylsiloxane or photocurable resin.

7. The method for preparing the antireflective film according to claim 1, characterized in that, It also includes the following steps: A curing material is used to cure the surface of the substrate after transfer.

8. The method for preparing the antireflective film according to claim 1, characterized in that, The second template is connected to the first template by vacuum compression.

9. A pressing mold, characterized in that, include: The first template includes a flat body, and the surface of the first template is provided with a plurality of spaced-apart first recesses; The second template includes a flat body. The surface of the second template is provided with a plurality of spaced second recesses. The second template is aligned and connected with the first template. The second template deforms with the first recess of the first template to generate a third recess. The size of the second recess is smaller than the size of the third recess. The number of the first recesses is greater than the number of the third recesses.

10. The molding die according to claim 9, characterized in that, The side of the first template near the first recess is glued to the side of the second template away from the second recess.

11. The molding die according to claim 9, characterized in that, The first template is made of polydimethylsiloxane or a photocurable resin. And / or, the second template is prepared using polydimethylsiloxane material or photocurable resin material.

12. An antireflective coating, characterized in that, Prepared by the method for preparing the antireflective film according to any one of claims 1 to 8, comprising: Substrate; Multiple anti-glare protrusions are spaced apart on the surface of the substrate; Multiple moth-eye protrusions are provided on the surface of each anti-glare protrusion, and multiple moth-eye protrusions are provided on the substrate between adjacent anti-glare protrusions.

13. The antireflective film according to claim 12, characterized in that, The size of the anti-glare protrusion is between 1-5 μm; and / or, the size of the moth-eye protrusion is between 10-100 nm.

14. The antireflective film according to claim 12, characterized in that, The substrate is made of polyester resin, tricellulose acetate, polymethyl methacrylate, polystyrene, polypropylene, polyethylene and polyvinyl chloride, polycarbonate, polyamide or other hardened resins.

Citation Information

Patent Citations

  • Method for manufacturing lens press back, lens press back, and light emitting diode lens

    CN102795007A

  • Original plate for manufacturing antireflection film

    JP2013142741A