Method and apparatus for improving the performance of flexible magnetic drive structures using magnetic vibrating screen
By using an alternating magnetic field method to disperse and uniformly distribute hard magnetic particle chains, the problem of hard magnetic particles agglomerating after multiple orientations is solved, improving the performance of flexible magnetic drive structures, especially magnetic responsiveness and surface morphology, and making them suitable for a variety of matrix materials.
Patent Information
- Application Number
- CN202311578244.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-11-24
AI Technical Summary
In existing technologies, hard magnetic particles tend to aggregate after multiple orientations, leading to a decline in the performance of flexible magnetic drive structures. In particular, the driving effect of magnetic field-assisted photopolymerization molding products is inaccurate, making it difficult to solve the problem of hard magnetic particles agglomerating after multiple magnetic field arrangements.
The alternating magnetic field method is used to disperse unoriented hard magnetic particles into uniform small particle chain units through the alternating action of the xy-plane rotating oscillating magnetic field and the z-axis oscillating magnetic field, and make them uniformly distributed in the plane. Then, the arrangement magnetic field is used to arrange them to form a dense and uniform hard magnetic particle chain.
It significantly improves the orientation and stabilization time of hard magnetic particle chains, enhances the performance of flexible magnetic drive structures, including magnetic responsiveness and surface morphology, is applicable to different matrix materials, and maintains good performance when repeatedly used in the same plane.
Smart Images

Figure CN117601169B_ABST
Abstract
Description
Technical Field
[0001] This invention designs a method for enhancing the performance of flexible magnetic drive structures, specifically providing a magnetic field oscillation screen method and device for improving the performance of flexible magnetic drive structures. Background Technology
[0002] Compared to traditional rigid robots, soft robots possess greater adaptability, flexibility, and higher degrees of freedom, making them a current research hotspot. They can produce many elegant and imaginative deformations as needed, enabling their application in various fields, including biology, medicine, and deep-sea exploration. The extensive deformability of soft robots stems from both their structural design and the numerous actuation methods available. Among these methods, magnetic field actuation stands out due to its rapid response, high penetration, biocompatibility, and, most importantly, non-contact nature, allowing it to adapt well to diverse environments. Therefore, magnetic field actuation is considered one of the most promising actuation methods.
[0003] The application of magnetically driven soft robots relies on the presence of magnetic materials in the robot's structure. These materials form microstructures with magnetic anisotropy during robot formation by applying a magnetic field. Typically, these microstructures consist of hard magnetic particles (neodymium iron boron). With the help of such microstructures, soft robots can exhibit multifunctional behavior in magnetic fields. As research into magnetic soft robots deepens, various methods have been proposed to create the necessary magnetic microstructures. Many of these methods involve the integration of magnetic fields with 3D printing technology. For example, the direct ink writing (DIW) method for magnetic soft robots utilizes a magnetic field to align magnetic particles embedded in the extruded material, thereby achieving magnetic anisotropy in the printed plane. Another method is magnetic field-assisted stereolithography, where magnetic particles are arranged into specific microstructures (arrangement) by permanent magnets and then cured using ultraviolet light (to complete orientation) to fabricate functional magnetically driven soft robots. This method achieves magnetization distribution in three dimensions and has the potential to fabricate complex magnetic soft robots.
[0004] However, after multiple orientations, hard magnetic particles in the photocurable raw material tend to aggregate due to their high remanent magnetization, leading to inaccurate orientation and subsequent loss of overall remanent magnetization in unnecessary directions. This problem significantly reduces the driving effect of magnetic field-assisted photocurable molding products. Current research on the microstructure of magnetic particle aggregates mainly focuses on soft magnetic particle aggregates, such as the decomposition and diffusion changes of Fe3O4 nanoparticle clusters in a magnetic field. Research on hard magnetic particle aggregates is mostly limited to the analysis of the overall morphology of the aggregates. Without solving this microstructure problem, the performance of flexible magnetic drive structures cannot be improved. Unfortunately, the conflict between the need for multiple magnetization directions and the particle aggregation problem caused by repeated orientation has not been effectively resolved. Therefore, a method is urgently needed to solve the aggregation problem of hard magnetic particles after multiple magnetic field arrangements. Summary of the Invention
[0005] This invention provides a magnetic field oscillation sieve method for improving the performance of flexible magnetic drive structures by utilizing an alternating magnetic field to enhance the properties of hard magnetic particle chains. This method can significantly improve the orientation and stabilization time of hard magnetic particle chains, thereby improving various aspects of the performance of flexible magnetic drive structures. Furthermore, this method can be repeatedly applied within the same plane without losing its effectiveness, and it is also applicable to different matrices.
[0006] A magnetic field oscillation sieve method for improving the performance of flexible magnetic drive structures is disclosed. This method is mainly applied in the process of preparing flexible magnetic drive structural components using magnetic field-assisted selective photopolymerization. The method includes: before the next arrangement, treating the remaining unoriented hard magnetic particles as follows:
[0007] (1) Use the xy plane rotating oscillating magnetic field to disperse the remaining unoriented hard magnetic particles into small particle chain units with uniform length and relatively uniform thickness.
[0008] (2) The z-axis oscillating magnetic field is applied to the particle chain unit obtained in the preliminary treatment of step (1), so that the particle chain unit collectively turns to the z-axis direction, and the particle chain unit is more uniform in thickness, while realizing the uniform distribution of particle chain unit in the plane.
[0009] Optionally, steps (1) and (2) can be repeated alternately once or multiple times until the particle chains are uniformly distributed in the plane with the same spacing, and all hard magnetic particle chain units are of uniform length and thickness. Applying an arrangement magnetic field to the obtained hard magnetic particle chain units can produce dense and uniform hard magnetic particle chains, improving their performance in all aspects.
[0010] As a preferred method, when agglomeration occurs in the remaining unoriented hard magnetic particles after one orientation is completed in the process of preparing flexible magnetic drive structural parts using magnetic field-assisted selective photopolymerization, the above method is used for treatment.
[0011] Specifically, a magnetic field oscillation screen method for improving the performance of flexible magnetic drive structures includes:
[0012] (1) Use the rotating oscillating magnetic field in the xy plane to disperse the aggregated particle chains into small particle chain units with uniform length and relatively uniform thickness.
[0013] (2) Use the z-axis oscillating magnetic field to collectively rotate the particle chain units obtained in (1) to the z-axis direction, and then use the repulsive force between the particle chains with the same orientation to make the particle chains move away from each other in the plane and finally distribute them evenly in the plane with the same spacing.
[0014] (3) Repeat steps (1) and (2) alternately. After repeated many times, the dispersed uniform-sized particle agglomerates will be evenly distributed in the plane.
[0015] After completing the above processing, subsequent arrangement operations can be performed, namely:
[0016] Using a magnetic field to arrange particles into a chain structure in the desired direction imparts magnetic anisotropy to the flexible magnetic drive structure.
[0017] If a flexible magnetic drive structure requires magnetic moments in multiple directions, the above process can be performed before each arrangement, which can greatly improve the performance of the magnetic particle chain in each arrangement direction, thereby improving the overall performance of the flexible magnetic drive structure.
[0018] This invention allows the use of an alternating magnetic field (magnetic oscillating screen) to decompose particle chain agglomerates that affect the performance of flexible magnetic drive structures into fine particle agglomerate units and to distribute them uniformly in a plane. Subsequently, by using an array magnetic field, dense, uniform particle chains with higher remanence in the desired direction can be obtained. This improvement greatly enhances the performance of flexible magnetic drive structures.
[0019] In this invention, for specific hard magnetic particles, the oscillation frequency and magnetic field amplitude of the z-axis oscillating magnetic field are determined through prior experiments; as well as the rotation frequency, oscillation frequency, and magnetic field amplitude of the xy-plane rotating oscillating magnetic field.
[0020] Preferably, the method for determining the oscillation frequency and amplitude of the z-axis oscillating magnetic field is as follows:
[0021] The oscillation frequency of the z-axis oscillating magnetic field is determined by applying a single-amplitude z-axis magnetic field to the same type of hard magnetic particles after agglomeration pretreatment, based on the change in the z-axis projected area of the hard magnetic particles.
[0022] The amplitude of the z-axis oscillating magnetic field: Different maximum amplitude z-axis oscillating magnetic fields are applied to the same type of hard magnetic particles after agglomeration pretreatment. The optimal range B of the maximum amplitude of the z-axis magnetic field is obtained by using the best distribution uniformity of particle agglomeration units, unit diameter, and unit spacing as the criteria. max1 ~B max2 Obtain the maximum amplitude B of the z-axis magnetic field. max .
[0023] Preferably, the amplitude range of the z-axis oscillating magnetic field is 0 to B. max The amplitude range of the rotating oscillating magnetic field in the xy plane is B. max1 ~B max2 .
[0024] As a preferred method, different rotational and oscillation frequencies of xy-plane rotating oscillating magnetic fields are applied to the same type of hard magnetic particles after agglomeration pretreatment, and then a z-axis oscillating magnetic field with determined parameters is applied. The two are applied alternately, and the rotational and oscillation frequencies of the xy-plane rotating oscillating magnetic fields are obtained based on the orientation of the magnetic particle chains and the optimal spacing between the particle chains.
[0025] Preferably, this method is based on generating a magnetic field using a three-dimensional Helmholtz coil, specifically, the xy-plane rotating oscillating magnetic field and the z-axis oscillating magnetic field are generated by a three-dimensional Helmholtz coil. Generating a magnetic field using a three-dimensional Helmholtz coil offers numerous advantages, including non-contact operation, fast response speed, strong penetration, and good biocompatibility, which are not found in other driving methods.
[0026] Preferably, the amplitude B0 of the rotating oscillating magnetic field in the xy plane, and the rotating oscillating magnetic field in the xy plane... Oscillating magnetic field in the z-axis direction They are respectively:
[0027]
[0028]
[0029]
[0030] Among them, B max Let f be the maximum amplitude of the magnetic field in the xy plane and along the z-axis (60 mT in the verification of this method), B0 be the amplitude of the rotating oscillating magnetic field in the xy plane, and f be a scalar value that varies with time. x-y Let be the rotational frequency of the rotating oscillating magnetic field in the xy plane, and k be the ratio of the oscillation frequency to the rotational frequency of the rotating oscillating magnetic field in the xy plane. Different values of k will show different oscillation shapes of the rotating oscillating magnetic field. This represents a rotating oscillating magnetic field in the xy plane, composed of two vector components. and and These represent the unit vectors in the x and y directions, respectively. This represents the oscillating magnetic field along the z-axis. f1 is the oscillation frequency of the z-axis oscillating magnetic field. t represents the unit vector in the z-direction. x-y t z , where represents the time corresponding to the rotating oscillating magnetic field in the xy plane and the oscillating magnetic field along the z-axis, respectively.
[0031] A method for preparing flexible magnetic drive structural components using a magnetic field-assisted selective photopolymerization method includes: after completing one or more orientations, processing the remaining hard magnetic particles using the magnetic field oscillation sieve method described in any of the above technical solutions.
[0032] The method of this invention can solve the problem of agglomeration of residual hard magnetic particles after multiple orientations; at the same time, even when agglomeration does not occur, the method of this invention can still be used to process the product, which can also significantly improve the product performance.
[0033] An apparatus for implementing the magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures as described in any of the above technical solutions, comprising:
[0034] The magnetic field generating unit generates the aforementioned xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field;
[0035] The control unit controls the magnetic field generating unit to generate the required xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field.
[0036] Preferably, the magnetic field generating unit is a three-dimensional Helmholtz coil, consisting of three pairs of coils perpendicular to each other.
[0037] Preferably, the control unit consists of a microcontroller and a host computer. The host computer sends instructions to the microcontroller, and the microcontroller outputs signals to control the current of the coil according to the instructions, thereby generating the required xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field.
[0038] This method can manipulate and disperse hard magnetic particles using a uniform magnetic field without the need for a gradient magnetic field, making the method relatively simple and quick to implement.
[0039] This method significantly improves the performance of hard magnetic particle chains, including the most important orientation index, which directly affects the remanence of the particle chain in the desired direction.
[0040] The performance improvement of the magnetic particle chain enhanced by this method can be reflected in the flexible magnetic drive structure, thereby improving the performance of the flexible magnetic drive structure.
[0041] This method can achieve similar results in different matrices.
[0042] In summary, this invention proposes a strategy to address the aggregation problem of hard magnetic particles after multiple orientations using an alternating magnetic field. The alternating magnetic field consists of two parts: a rotating oscillating magnetic field in the xy-plane and an oscillating magnetic field along the z-axis. The magnetic fields in the xy-plane and z-axis alternate. By selecting appropriate magnetic field parameters, the aggregated hard magnetic particle chains (taking NdFeB as an example) are uniformly distributed in the plane with a consistent size. Furthermore, the performance of the rearranged particle chains is enhanced in various aspects, including the orientation, uniformity, density, and stabilization time of the magnetic particle chains. The improvements in orientation and stabilization time are particularly significant, increasing to 200% of their original values and exceeding 120 minutes, respectively. This performance enhancement of the particle chain microstructure can greatly improve the performance of flexible magnetic drive structures obtained through "magnetic field-assisted SLA," including, most importantly, magnetic responsiveness and surface morphology. This method is also applicable to different matrix materials and maintains good results even when repeatedly used within the same plane. Attached Figure Description
[0043] Figure 1 The components of the alternating magnetic field of this invention are: a: schematic diagram of the alternating magnetic field; b: three-dimensional shape diagram of the alternating magnetic field; c: top view of the alternating magnetic field; d: side view of the alternating magnetic field; e: schematic diagram of the working mode of the alternating magnetic field.
[0044] Figure 2 The principles of each part of the magnetic field oscillating screen of the present invention are as follows: a: Schematic diagram of the principle of shortening and homogenizing the length of the particle chain by using a rotating magnetic field; b: Schematic diagram of the principle of moving the particle chains away from each other by using a z-axis magnetic field; c: Schematic diagram of switching the magnetic particle chains between a loose and tight binding state by using an oscillating magnetic field (taking the z-axis oscillating magnetic field as an example).
[0045] Figure 3 To demonstrate the effectiveness of this invention, each arrangement was performed using a 60mT arrangement magnetic field for 2 seconds: a: particle chain morphology after one arrangement; b: particle chain morphology after eight arrangements in different directions; c: particle chain morphology after eight arrangements and dispersion by this method, followed by another arrangement.
[0046] Figure 4 The diagram shows the shape of the magnetic field oscillation during the investigation of the xy magnetic field parameters, representing 0, 4, 6, 8, and 10 oscillations within a single period.
[0047] Figure 5 Size analysis of particle elements when a z-axis magnetic field is applied.
[0048] Figure 6 This demonstrates the improvement in microstructure performance brought about by the method (stabilization time).
[0049] Figure 7 This demonstrates the adaptability of the method to different matrix materials.
[0050] Figure 8 This demonstrates the effect of implementing the method multiple times on the same plane.
[0051] Figure 9 This demonstrates how the method improves the magnetic response performance of flexible magnetic drive structures.
[0052] Figure 10 The time taken for the projected size of a hard magnetic particle agglomerate to change from its largest projected area to its smallest projected area. Detailed Implementation
[0053] The present invention will be further described below with reference to the accompanying drawings:
[0054] The implementation process of this method is as follows: Figure 1 As shown, firstly, a rotating oscillating magnetic field in the xy-plane disperses the agglomerated hard magnetic particle chains into fine particle clusters. Next, an oscillating magnetic field along the z-axis rotates these clusters, aligning them in the z-axis direction. This utilizes the repulsive forces between the particle chains to move them apart, ultimately achieving a uniform distribution within the plane. Repeating the alternating operation of these two magnetic field components solves the particle chain agglomeration problem, resulting in uniformly sized and distributed particles within the plane. Subsequently, an arrangement magnetic field is used to arrange these particles into the desired orientation. The strengthened particle chains exhibit superior performance compared to the original chains. Applying this method to magnetic field-assisted selective photopolymerization (SPR) can yield more powerful flexible magnetic drive structures.
[0055] Specifically, a magnetic field oscillation sieve method for improving the performance of flexible magnetic drive structures is disclosed. This method is mainly applied in the process of preparing flexible magnetic drive structural components using magnetic field-assisted selective photopolymerization. The method is characterized by including the following treatment of the remaining unoriented hard magnetic particles before the next arrangement:
[0056] (1) Use the xy plane rotating oscillating magnetic field to disperse the remaining unoriented hard magnetic particles into small particle chain units with uniform length and relatively uniform thickness.
[0057] (2) The z-axis oscillating magnetic field is applied to the particle chain unit obtained in the preliminary treatment of step (1), so that the particle chain unit collectively turns to the z-axis direction, and the particle chain unit is more uniform in thickness, while realizing the uniform distribution of particle chain unit in the plane.
[0058] Optionally, steps (1) and (2) can be repeated once or multiple times (the specific number of repetitions can be determined according to the actual application) to eventually make the particle chains evenly distributed in the plane with the same spacing, and all hard magnetic particle chain units have uniform length and uniform thickness.
[0059] By further applying an arrangement magnetic field to the obtained hard magnetic particle chain unit, a dense and uniform hard magnetic particle chain can be obtained, and the performance in all aspects is improved.
[0060] In magnetic field-assisted SLA (Simplified Lamination) processes, the hard magnetic particles can be treated using the method of this invention after each or several orientation steps, significantly improving the performance of the final product. Alternatively, depending on the occurrence of agglomeration, the method of this invention can be added as needed to prevent agglomeration from affecting the next arrangement.
[0061] The principle of the present invention will now be described with reference to the accompanying drawings:
[0062] Figure 1 middle: This is a rotating oscillating magnetic field in the xy plane; The alternating magnetic field of this invention mainly consists of two parts: a rotating oscillating magnetic field in the xy-plane and an oscillating magnetic field along the z-axis. The rotating oscillating magnetic field in the xy-plane refers to the rotating magnetic field whose amplitude changes with time; it is equivalent to a rotating magnetic field superimposed with an amplitude oscillating magnetic field. Its main parameters include rotation frequency, oscillation frequency, and magnetic field strength (amplitude). The z-axis oscillating magnetic field refers to the z-axis magnetic field whose amplitude changes with time; its main parameters include oscillation frequency and oscillation amplitude. Both magnetic fields share a common characteristic: oscillation. "Oscillation" refers to the magnetic field amplitude changing with time in a sinusoidal shape. Furthermore, the magnetic field in the xy-plane and the magnetic field along the z-axis do not operate simultaneously; they alternate, such as... Figure 1 As shown.
[0063] Figure 2 This describes the working principle of the magnetic field oscillating sieve of the present invention. The alternating magnetic field used in this method consists of two parts: a rotating oscillating magnetic field in the xy plane and an oscillating magnetic field in the z-axis direction. These two magnetic fields can be decomposed into a rotating magnetic field superimposed with amplitude oscillation and a z-axis magnetic field superimposed with amplitude oscillation. Specifically: the rotating magnetic field in the xy plane shortens the length of the particle chain and keeps it uniform by balancing the magnetic torque and viscous drag torque; the z-axis magnetic field keeps the particle chains away from each other through the repulsive force between the particle chains; the oscillating magnetic field alternately changes the magnitude of the magnetic field strength, causing the particle chains to switch between loose and tight bonding repeatedly, thereby separating loosely connected particles.
[0064] Figure a in the upper left corner illustrates the principle of a single rotating magnetic field. By utilizing the viscous resistance encountered by the particle chain during rotation, the particle chain breaks at its center, thereby reducing the length of the particle chain while maintaining a uniform length.
[0065] Figure b in the upper right corner illustrates the principle of a single z-axis magnetic field. The z-axis magnetic field uses the mutual repulsion between magnetic particles facing the same direction to make the particle chains move away from each other and eventually distribute them stably and uniformly in the plane with the same spacing.
[0066] Figure c below illustrates the working principle of magnetic field oscillation, taking the z-axis oscillating magnetic field as an example. The amplitude oscillation of the magnetic field causes the particle chain to repeatedly switch between two states of tight bonding and loose bonding through amplitude changes, thereby playing a role in peeling off particles from the surface of the particle chain, even reducing the radial size of the particle chain.
[0067] Theoretical Formula
[0068] 1. Mathematical expression of the magnetic field of an alternating magnetic field (magnetic vibrating screen)
[0069] The alternating magnetic field used in this invention consists of two parts: a rotating oscillating field in the xy plane and an oscillating field in the z-axis direction, such as... Figure 1 As shown. In this invention, "oscillation" refers to the sinusoidal change in magnetic field strength over time. This is one of the key reasons why hard magnetic particle chain agglomerates can be dispersed. It is precisely because of this property that the magnetic field used in this invention is called a "magnetic field oscillating sieve".
[0070]
[0071]
[0072]
[0073] Among them, B max Let f be the maximum amplitude of the magnetic field in the xy plane and along the z-axis (60 mT in the verification of this method), B0 be the amplitude of the rotating oscillating magnetic field in the xy plane, and f be a scalar value that varies with time. x-y Let be the rotational frequency of the rotating oscillating magnetic field in the xy plane, and k be the ratio of the oscillation frequency to the rotational frequency of the rotating oscillating magnetic field in the xy plane. Different values of k will show different oscillation shapes of the rotating oscillating magnetic field. This represents a rotating oscillating magnetic field in the xy plane, composed of two vector components. and and These represent the unit vectors in the x and y directions, respectively. This represents the oscillating magnetic field along the z-axis. f z Let be the oscillation frequency of the z-axis oscillating magnetic field. t represents the unit vector in the z-direction. x-y t z , where represents the time corresponding to the rotating oscillating magnetic field in the xy plane and the oscillating magnetic field along the z-axis, respectively.
[0074] The materials used in the detection experiments in this invention are all hard magnetic particles (NdFeB), a typical hard magnetic material. Its most significant difference from soft magnetic materials is that once magnetized by a strong magnetic field, it retains its remanent magnetization even after the magnetic field disappears, and is not easily remagnetized by weaker magnetic fields. The hard magnetic particles used in the detection experiments are all pre-magnetized, so they will not be magnetized by the experimental magnetic field during the experiment. At a certain magnetic particle concentration, the hard magnetic particles will respond to the external magnetic field, exhibiting a tendency to align along their own magnetic moment direction, forming a chain-like microstructure. This process of using an experimental magnetic field to assemble particles into an oriented chain-like microstructure is called "arrangement," and the experimental magnetic field is called the "arrangement magnetic field." The arranged hard magnetic particle chain microstructure is fixed by curing with photosensitive resin; this process is called "orientation." The resulting product is a sample with magnetic anisotropy, exhibiting the greatest remanent magnetic induction intensity in the direction of the chain structure. The biggest problem caused by particle chain agglomeration due to multiple arrangements is that the particle chains are uneven and inaccurately aligned, thus weakening the remanent magnetic induction intensity of the sample in the desired direction. The method proposed in this invention is precisely intended to solve this problem.
[0075] Parameter selection:
[0076] The main function of the xy-plane rotating oscillating magnetic field is to reduce the individual size of particle aggregates along and perpendicular to the chain direction. It makes the aggregated particle chains shorter and finer while maintaining the uniform and small size of each unit. This is achieved by superimposing the rotating magnetic field component and the oscillating magnetic field component. The main parameters include: 1) the rotational frequency of the rotating magnetic field; 2) the ratio of the oscillation frequency to the rotational frequency (or the oscillation frequency itself); and 3) the range of magnetic field amplitude variation.
[0077] The main function of the z-axis oscillating magnetic field is to utilize the repulsive force between particle chains with a uniform magnetic moment orientation, thereby distributing the particle chains evenly in a plane with approximately the same spacing. Simultaneously, the oscillating component of the magnetic field breaks down particle chain agglomerates, further reducing the size of the agglomerates. The main parameters involved are: 1) the oscillation frequency of the oscillating magnetic field; and 2) the range of magnetic field amplitude variation.
[0078] The primary application of this method is photopolymerization printing of flexible magnetic drive soft structures. Therefore, improving the orientation of the magnetic particle chains is the primary objective. Furthermore, the more uniform, denser, and more stable the magnetic particle chains, the greater the performance improvement for the product. In general, when selecting magnetic field parameters, the finer and more uniform the dispersion units of the processed magnetic particle agglomerates, the better. Simultaneously, the more accurate and denser the orientation of the particle chains formed after the re-arrangement of these dispersion units, the better. Therefore, the uniformity of the particle agglomeration units and the orientation and density of the magnetic particle chains obtained after re-arrangement are crucial evaluation indicators.
[0079] First, the oscillation frequency of the z-axis oscillating magnetic field is determined. Taking the hard magnetic particles (NdFeB) used in this paper as an example, based on the principle that the oscillating magnetic field reduces the radial size of particle agglomerates, we need to utilize the oscillation characteristics to repeatedly switch the particle agglomerates between tight and loose binding. Therefore, after eight pre-processing arrangements simulating agglomeration (i.e., eight arrangements at 45° intervals in different directions to induce particle chain agglomeration), a single z-axis magnetic field is applied to the hard magnetic particles. The projected size change of the particle agglomerates is then captured using a microscope (frame-by-frame comparison), and the time taken for the projected area to change from the largest to the smallest is calculated. Figure 10 As shown. Since switching between tight and loose states is not suitable for bringing the particle chain to its tightest state, as this would weaken the switching effect, the midpoint of the entire contraction time (approximately 3 frames, with a shooting speed of 60 frames / s) was ultimately selected as the time for the amplitude of the z-axis oscillating magnetic field to change from 0 to its peak value, which was converted into an oscillation frequency of 10Hz for the z-axis oscillating magnetic field.
[0080] The amplitude of the z-axis magnetic field is determined primarily by comparing three key indicators: the uniformity of particle agglomeration unit distribution when the z-axis oscillating magnetic field is applied, unit diameter, and unit spacing. Uniformity is compared using the two-dimensional information entropy of the image calculated by an image processing algorithm. Unit diameter and unit spacing are measured using conventional image processing methods (using ImageJ software to randomly select a certain number of units in the image, measure their diameter and spacing, and calculate the average of the measured values). Better uniformity indicates more optimized parameters.
[0081] Experimental comparisons revealed that, taking NdFeB as an example, magnetic field strengths of 40 mT and 60 mT are more suitable. Magnetic field strengths within this range can quickly and accurately induce a response in the particles, while 20 mT is less effective. This strength range will also be used as the strength range of the rotating oscillating magnetic field in the xy plane. That is, for hard magnetic particles NdFeB, the strength (amplitude) range of the rotating oscillating magnetic field in the xy plane is 40 mT to 60 mT; and the amplitude range of the z-axis oscillating magnetic field is 0 to 60 mT.
[0082] After determining the parameters of the z-axis magnetic field, these suitable parameters were applied to the subsequent investigation of the parameters of the xy-plane rotating oscillating magnetic field. Different xy-axis magnetic field rotation frequencies were matched with different oscillation shapes (i.e., the projection patterns of the rotating oscillating magnetic field, such as...). Figure 4 As shown, the parameters of the xy-plane rotating oscillating magnetic field are determined by comparing the effects of different combinations and alternating operation of the z-axis magnetic field with predetermined parameters on the dispersed particles after re-arranging. Similarly, before the experiment, the hard magnetic particles need to undergo simulated agglomeration pretreatment (i.e., arranging them in different directions at 45° intervals eight times to cause particle chain agglomeration) before subsequent experiments. Specifically, the agglomeration pretreatment involves arranging the sample to be tested (a mixture of NdFeB and photosensitive resin) eight times at 45° intervals, using a magnetic field strength of 60mT and an arrangement time of 2s, to simulate the phenomenon of particle agglomeration after multiple arrangements.
[0083] Using a rotating oscillating magnetic field in the xy plane with a magnetic field strength between 40 mT and 60 mT and a z-axis oscillating magnetic field with an amplitude between 0 and 60 mT, the orientation and spacing of particle chains obtained by arranging magnetic particle aggregates under different rotation frequencies and combinations of five different rotating oscillating magnetic field shapes were compared. Figure 4 As shown, from left to right, these represent 0 oscillations, 4 oscillations, 6 oscillations, 8 oscillations, and 10 oscillations within one cycle.
[0084] Two key indicators were compared at different rotation frequencies of rotating oscillating magnetic fields: the orientation of the magnetic particle chains (calculated through image processing), and the spacing between the particle chains (smaller and more uniform spacing indicates a denser and more uniform chain distribution).
[0085] Specifically, orientation was calculated using the Tamura algorithm; higher orientation indicates more precise alignment of the particle chain in the desired direction. First, the orientation was calculated when particles agglomerated after eight arrangement iterations. Then, the particles were processed using this method and arranged again, and the orientation of the particle chain was calculated. The percentage improvement was compared between the two methods. The results are shown in Table 1. Subsequently, ImageJ software was used to randomly select a certain number of adjacent particle chains in the image to measure the spacing, and the average value of the measurements was calculated. The results are shown in Table 2.
[0086] Table 1. Experimental Results of Percentage Increase in Orientation
[0087]
[0088] Table 2. Experimental results of particle chain spacing measurement
[0089]
[0090] The results show that combinations of different shapes and rotation frequencies all resulted in nearly 100% improvement in orientation. Comparison revealed that the best particle chain performance was achieved by combining a high rotation frequency with a high number of oscillations per cycle, as shown in Tables 1 and 2. The optimal combination was a magnetic field shape with 10 oscillations per cycle (i.e., the ratio of oscillation frequency to rotation frequency) and a rotation frequency of 10 Hz.
[0091] To further verify the above conclusions and compare the effects of the number of oscillations and rotation frequency within a single period on particle dispersion, ImageJ software was used to analyze the size of particle agglomeration units when a z-axis magnetic field was applied. The results are as follows: Figure 5 As shown, the number of particle units exceeding 200 pixels and the number of pixels contained in the largest unit are compared under different combinations. Analysis reveals that the combination of a rotation frequency of 10Hz and an alternating magnetic field oscillating 10 times within a single cycle still achieves the best dispersion effect. When a z-axis magnetic field is applied, the number of particle units exceeding 200 pixels is the fewest, and the size of the largest unit is the smallest among the three combinations, resulting in the finest particle unit size.
[0092] Through the above experiments, it was finally obtained that for hard magnetic particles (NdFeB), the rotation frequency of the rotating oscillating magnetic field in the xy plane is 10Hz, the oscillation frequency is 100Hz, and the magnetic field strength amplitude range is 40mT~60mT; the oscillation frequency of the oscillating magnetic field in the z-axis direction is 10Hz, and the magnetic field strength amplitude range is 0~60mT.
[0093] Figure 3 To demonstrate the effectiveness of this invention, each arrangement was performed using a 60mT magnetic field for 2 seconds. Here, "1 arrangement" refers to the hard magnetic particles being arranged into chains using a single magnetic field; "8 arrangements" refers to the hard magnetic particles being arranged into chains using eight different directions; and "8 arrangements with reinforcement" refers to the hard magnetic particles being dispersed using this method after eight different orientations, followed by a final arrangement to obtain a dense particle chain.
[0094] Figure a shows the morphology of the magnetic particle chain after only one directional arrangement; Figure b shows the morphology of the particle chain after eight different directional arrangements; Figure c shows the morphology of the particle chain after eight directional arrangements, followed by the application of this method to uniformly disperse the aggregates in a plane with the smallest possible size, and then another directional arrangement. It can be observed that the magnetic particle chains treated by this method are more dense and uniform, and their orientation is significantly improved.
[0095] Furthermore, this invention further compared the particle chain orientation stabilization time in two scenarios: 8 arrangements and 8 arrangements followed by processing using the method of this invention and then rearranging. After removing the arrangement magnetic field, the stability and orientation changes of the particle chains are as follows: Figure 6 As shown in the results, the particle chains enhanced by this method exhibit stronger stability, maintaining high orientation over a 120-minute timescale without being disrupted by particle chain interactions. Conversely, the orientation of particle chains not enhanced by this method decreased within 5 minutes due to mutual attraction.
[0096] Applying this method to magnetic field-assisted selective photopolymerization (SLA) can significantly enhance the performance of flexible magnetic drive structures, with the most important improvement being the remanence of the sample in the desired direction. The remanence of samples under various conditions in the same direction (arrangement direction) was tested. The sample thickness was 0.1 mm, and the dimensions were 3 mm × 20 mm. The samples were obtained by magnetic field-assisted selective photopolymerization (SLA), with the photopolymerization material consisting of a mixture of NdFeB and photosensitive resin, where the mass fraction of NdFeB was 10%. The particles inside the five groups of samples underwent the following treatments: 1) zero arrangement; 2) one arrangement; 3) one arrangement followed by dispersion using this method and then re-arranged (referred to as one arrangement + reinforcement); 4) eight arrangements in different directions; 5) eight arrangements in different directions followed by dispersion using this method and then re-arranged (referred to as eight arrangements + reinforcement). Due to the size limitations of the VSM measuring instrument, the same portion and size were cut from each sample of the same size for the remanence test. The measurement results are shown in Table 3. It can be observed that arranging the magnetic field causes the hard magnetic particles inside the flexible magnetic drive structure to form a particle chain, thereby endowing the sample with magnetic anisotropy in the direction of the particle chain. In contrast, the magnetic field without arrangement does not exhibit significant remanence. On the other hand, the sample enhanced by this method exhibits significantly higher remanence than the unenhanced sample, and this enhancement has a good improvement effect regardless of how many times the arrangement is implemented, with the improvement in remanence approaching 100%.
[0097] Table 3 Remanence of flexible magnetic drive samples prepared by magnetic field-assisted SLA
[0098]
[0099] Figure 9This demonstrates how the method of this invention improves the magnetic response performance of flexible magnetic drive structures. We further compared the response of some of the aforementioned samples under a magnetic field. The comparison reveals that the samples treated with this method exhibit greater deformation. This is because the method distributes the aggregated particle chains in a uniform and dense manner within the plane. The particle chains obtained by arranging these units are more uniform and dense, resulting in a greater remanent magnetic induction intensity, which is consistent with the remanent magnetization test results of the samples. Stronger response deformation under a magnetic field is one of the most important performance indicators of flexible magnetic drive structures.
[0100] like Figure 7 As shown, this method can obtain an approximate dense particle chain structure in different matrix materials by adjusting some parameters of the magnetic field, which proves the applicability of this method in different matrix materials. Figure 7 In the figures, the matrix material of Figure a is Resione's F29T photosensitive resin; the matrix material of Figure b is Formlabs' Flexible 80A photosensitive resin; the matrix material of Figure c is Aladdin's PEGDA; and the matrix material of Figure d is Formlabs' Clear photosensitive resin.
[0101] In addition, due to the increasing complexity of flexible magnetic drive structures, the stability of this method when applied multiple times in the same plane is also very important. Taking a six-arm flexible magnetic drive gripper as an example... Figure 8 As shown, after multiple applications in a plane, each arm of the gripper can be assigned a different magnetization direction, ultimately enabling each arm of the gripper to achieve uniform bending deformation. Experiments demonstrate that applying the method of this invention to the same plane a total of 13 times maintains a stable effect and produces a considerable deformation effect in the flexible magnetic drive structure. This proves the stability of this method after multiple applications.
[0102] The above description only covers some aspects of how this invention improves the performance of magnetic particle chains and flexible magnetic drive structures. In reality, this method has other potential applications for performance enhancement. It is impossible to exhaustively list all structures for which this invention can be applied to improve performance. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of this invention should be included within the scope of protection of this invention.
Claims
1. A magnetic field oscillation screening method for performance improvement of a flexible magnetic drive structure, the method being applied in a process of preparing a flexible magnetic drive structure by using a magnetic field assisted selective photocuring, characterized in that, include: Before proceeding with the next arrangement, the remaining unoriented hard magnetic particles are treated as follows: (1) Use the rotating oscillating magnetic field in the xy plane to disperse the remaining unoriented hard magnetic particles into small particle chain units with uniform length and relatively uniform thickness; (2) The z-axis oscillating magnetic field is applied to the particle chain unit obtained in the preliminary treatment of step (1), so that the particle chain unit collectively turns to the z-axis direction, and the particle chain unit is more uniform in thickness, while realizing the uniform distribution of particle chain unit in the plane. Steps (1) and (2) are repeated alternately once or multiple times until the particle chains are evenly distributed in the plane with the same spacing, and all hard magnetic particle chain units are of uniform length and uniform thickness. the amplitude of the x-y plane rotating oscillating magnetic field the x-y plane rotating oscillating magnetic field the magnetic field of the z-axis oscillating magnetic field respectively: (1) (2) (3) in, This represents the maximum amplitude of the magnetic field in the xy plane and along the z-axis. Let be the amplitude of the rotating oscillating magnetic field in the xy plane. Let be the rotational frequency of the rotating oscillating magnetic field in the xy plane. Let be the ratio of the oscillation frequency to the rotation frequency of the rotating oscillating magnetic field in the xy plane. The rotating oscillating magnetic field in the xy plane consists of two vector components, namely... and ; and These represent the unit vectors in the x and y directions, respectively. Represents the oscillating magnetic field along the z-axis; Let be the oscillation frequency of the z-axis oscillating magnetic field. Represents the unit vector in the z-direction; , , where represents the time corresponding to the rotating oscillating magnetic field in the xy plane and the oscillating magnetic field along the z-axis, respectively.
2. The magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures according to claim 1, characterized in that, For the same type of hard magnetic particles that have undergone agglomeration pretreatment, the oscillation frequency and magnetic field amplitude of the z-axis oscillating magnetic field, as well as the rotation frequency, oscillation frequency, and magnetic field amplitude of the xy-plane rotating oscillating magnetic field, are determined through preliminary experiments.
3. The magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures according to claim 2, characterized in that, The method for determining the oscillation frequency and amplitude of the z-axis oscillating magnetic field is as follows: Oscillation frequency: A single-amplitude z-axis magnetic field is applied to the same type of hard magnetic particles after agglomeration pretreatment, and the oscillation frequency of the z-axis oscillating magnetic field is determined based on the change in the z-axis projected area of the hard magnetic particles. Magnetic field amplitude: Applying z-axis oscillating magnetic fields with different maximum amplitudes to the same type of hard magnetic particles after agglomeration pretreatment, and using the optimal distribution uniformity of particle agglomeration units, unit diameter, and unit spacing as the criteria, the optimal range of the maximum amplitude of the z-axis magnetic field is obtained. Obtain the maximum amplitude of the z-axis magnetic field. .
4. The magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures according to claim 3, characterized in that, The amplitude range of the z-axis oscillating magnetic field is 0~ The amplitude range of the rotating oscillating magnetic field in the xy plane is: .
5. The magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures according to claim 3, characterized in that, After agglomeration pretreatment, the same type of hard magnetic particles are subjected to rotating and oscillating magnetic fields of different rotation and oscillation frequencies in the xy plane. Then, a z-axis oscillating magnetic field with determined parameters is applied. The two are applied alternately, and the rotation frequency and oscillation frequency of the rotating magnetic field in the xy plane are obtained by using the orientation of the magnetic particle chain and the optimal spacing between the particle chains as the judgment criteria.
6. The magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures according to claim 1, characterized in that, The xy-plane rotating oscillating magnetic field and the z-axis oscillating magnetic field are generated by a three-dimensional Helmholtz coil.
7. A method for preparing flexible magnetic drive structural components using a magnetic field-assisted selective photopolymerization method, characterized in that, include: After one or more orientations are completed, the remaining unoriented hard magnetic particles are processed using the magnetic field oscillation sieve method described in any one of claims 1 to 6.
8. An apparatus for implementing the magnetic field oscillating screen method for improving the performance of flexible magnetic drive structures as described in any one of claims 1 to 6, characterized in that, include: The magnetic field generating unit generates the aforementioned xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field; The control unit controls the magnetic field generating unit to generate the required xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field.
9. The apparatus according to claim 8, characterized in that, The magnetic field generating unit is a three-dimensional Helmholtz coil, consisting of three pairs of coils perpendicular to each other; the control unit consists of a microcontroller and a host computer. The host computer sends instructions to the microcontroller, and the microcontroller outputs signals to control the current of the coil according to the instructions, thereby generating the required xy-plane rotating oscillating magnetic field and z-axis oscillating magnetic field.
Citation Information
Patent Citations
Magneto-rheological finishing device based on alternating magnetic field