Semiconductor device manufacturing method and semiconductor device

By adjusting the process parameters of the etching equipment, the formation of oxide layer trenches with different widths in the semiconductor device is achieved, and the thickness of the bottom oxide layer is consistent, which solves the problem of uneven bottom of the oxide layer trench in the existing technology and improves the device performance. reliability and etching efficiency.

CN117612944BActive Publication Date: 2024-10-01GUANGZHOU CANSEMI TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311720707.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-14
Publication Date
2024-10-01
Estimated Expiration
2043-12-14

AI Technical Summary

Technical Problem

Existing high-voltage MOS devices have a problem of uneven bottom etching during the oxide layer trench etching process, resulting in inconsistent oxide layer thickness on the bottom of the trench, affecting the reliability of the device.

Method used

By adjusting process parameters in the reaction chamber of the etching equipment, such as chamber pressure, radio frequency power and reaction gas flow, oxide layer trenches with different widths are formed. The thickness of the bottom oxide layer is the same. A one-step etching process is used to control the etching residue. Quantity uniformity.

Benefits of technology

The formation of oxide layer trenches with different widths is achieved, and the thickness of the bottom oxide layer is consistent, which improves the reliability and etching efficiency of the semiconductor device, simplifies the process, and avoids the need for multi-step etching.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117612944B_ABST
    Figure CN117612944B_ABST
Patent Text Reader

Abstract

The present application discloses a method for manufacturing a semiconductor device and a semiconductor device. The method for manufacturing a semiconductor device includes providing a semiconductor structure to be etched, wherein the semiconductor structure to be etched includes a semiconductor substrate, an oxide layer and an anti-reflection layer stacked in sequence from bottom to top; forming a photoresist layer with a preset pattern on the anti-reflection layer; using the photoresist layer as a mask, performing a one-step etching process on the anti-reflection layer and the oxide layer in a reaction chamber of an etching device by adjusting the process parameters of the etching device, forming a first oxide layer groove and a second oxide layer groove, wherein the widths of the first oxide layer groove and the second oxide layer groove are different, and the oxide layer thicknesses at the bottoms of the first oxide layer groove and the second oxide layer groove are the same, so as to achieve the purpose of controlling the uniformity of the etching margin through a one-step etching process; and removing the photoresist layer and the anti-reflection layer. The scheme can make the oxide layer thicknesses at the bottoms of the oxide layer grooves with different widths the same.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a method for manufacturing a semiconductor device and a semiconductor device. Background Art

[0002] For existing high-voltage MOS (HVMOS) devices, in order to ensure that the silicon surface on the active layer of the MOS device is not damaged, it is necessary to ensure that the oxide layer on its upper surface still retains a certain amount of remainder after dry etching, that is, the bottom of the oxide layer trench has a certain etching remainder. However, during the etching process of the oxide layer trench, the problem of uneven etching of the bottom oxide layer remainder (oxide remainloading) is usually encountered. The main reasons are:

[0003] First, in the same etching groove, during the etching process, the closer the oxide layer is to the groove sidewall, the greater the etching rate is, and the corresponding etching margin is smaller, resulting in the etching margin on both sides of the groove bottom surface being less than the etching margin in the middle of the groove bottom surface, and presenting an uneven phenomenon of high in the middle of the groove bottom surface and low on both sides; second, the width of each groove is different, and the etching margin of the oxide layer will be different after etching, that is, the larger the width of the groove, the larger the etching margin of the oxide layer after etching is completed, and the etching margin of each groove will be different, which is manifested as inconsistent horizontal surfaces of the bottom surfaces of different grooves. Summary of the invention

[0004] In view of this, an embodiment of the present application provides a method for manufacturing a semiconductor device and a semiconductor device, which can make the oxide layer thickness at the bottom of oxide layer trenches with different widths the same.

[0005] In a first aspect, the present application provides a method for manufacturing a semiconductor device, comprising:

[0006] Providing a semiconductor structure to be etched, the semiconductor structure to be etched comprising a semiconductor substrate, an oxide layer and an anti-reflection layer stacked in sequence from bottom to top;

[0007] forming a photoresist layer having a preset pattern on the anti-reflection layer;

[0008] Using the photoresist layer as a mask, performing a one-step etching process on the anti-reflective layer and the oxide layer to form a first oxide layer trench and a second oxide layer trench, wherein the widths of the first oxide layer trench and the second oxide layer trench are different, and the oxide layers at the bottoms of the first oxide layer trench and the second oxide layer trench are the same in thickness;

[0009] The photoresist layer and the anti-reflective layer are removed.

[0010] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the process parameters of the etching equipment include chamber pressure, high-frequency RF power, low-frequency RF power, first reaction gas flow rate, and second reaction gas flow rate.

[0011] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the chamber pressure is 20 to 100 mT.

[0012] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the high-frequency radio frequency power is 600~1000W.

[0013] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the low-frequency RF power is 150-500 W.

[0014] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the flow rate of the first reaction gas is 30 to 50 sccm.

[0015] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the flow rate of the second reaction gas is 100-200 sccm.

[0016] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the first reaction gas is CF4.

[0017] In the method for manufacturing a semiconductor device provided in an embodiment of the present application, the second reaction gas is Ar.

[0018] In a second aspect, an embodiment of the present application provides a semiconductor device, which is formed by using any of the above-mentioned methods for manufacturing a semiconductor device.

[0019] In summary, the manufacturing method of the semiconductor device provided by the embodiment of the present application includes providing a semiconductor structure to be etched, wherein the semiconductor structure to be etched includes a semiconductor substrate, an oxide layer and an anti-reflection layer stacked in sequence from bottom to top; forming a photoresist layer with a preset pattern on the anti-reflection layer; using the photoresist layer as a mask, performing a one-step etching process on the anti-reflection layer and the oxide layer in a reaction chamber of an etching device by adjusting the process parameters of the etching device to form a first oxide layer groove and a second oxide layer groove, wherein the widths of the first oxide layer groove and the second oxide layer groove are different, and the oxide layer thicknesses at the bottom of the first oxide layer groove and the second oxide layer groove are the same, so as to achieve the purpose of controlling the uniformity of the etching margin through a one-step etching process; removing the photoresist layer and the anti-reflection layer. This scheme can form oxide layer grooves with different widths and the same oxide layer thickness at the bottom through a one-step etching process. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0021] Figure 1 It is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present application.

[0022] Figure 2 It is a schematic diagram of the structure of a semiconductor structure to be etched provided in an embodiment of the present application.

[0023] Figure 3 It is a schematic diagram of the middleware structure provided in the embodiment of the present application.

[0024] Figure 4 It is a schematic diagram of the structure of a semiconductor device provided in an embodiment of the present application. DETAILED DESCRIPTION

[0025] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The implementations described in the following exemplary embodiments do not represent all implementations consistent with the present application. Instead, they are merely examples of devices and methods consistent with some aspects of the present application as detailed in the appended claims.

[0026] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used in this application and in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used in this application includes any and all combinations of one or more related listed items.

[0027] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present application, the first element, component, region, layer or part discussed below can be represented as a second element, component, region, layer or part.

[0028] Spatially relative terms such as "under," "below," "below," "under," "above," "above," etc., may be used herein for ease of description to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatially relative terms are intended to include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, then the elements or features described as "under other elements" or "under" or "under" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device may be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.

[0029] Embodiments of the application are described herein with reference to schematic diagrams as ideal embodiments of the application. Thus, variations from the shapes shown due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, embodiments of the application should not be limited to the specific shapes of the regions shown herein, but include deviations in shapes due to, for example, manufacturing.

[0030] The embodiments of the present application provide a method for manufacturing a semiconductor device and a semiconductor device. The technical solution shown in the present application will be described in detail below through specific embodiments. It should be noted that the description order of the following embodiments is not intended to limit the priority order of the embodiments.

[0031] See also Figure 1 , Figure 1 : is a schematic flow chart of a method for manufacturing a semiconductor device provided by the present application, and the method for manufacturing a semiconductor device may include:

[0032] 101. Provide a semiconductor structure to be etched, wherein the semiconductor structure to be etched includes a semiconductor substrate, an oxide layer, and an anti-reflection layer stacked in sequence from bottom to top.

[0033] In some embodiments, the material of the semiconductor substrate 10 may be a germanium silicon substrate, a III-V group element compound substrate, a silicon carbide substrate or a laminated structure thereof, or a silicon-on-insulator structure, or a diamond substrate or other semiconductor material substrates known to those skilled in the art. For example, a P element may be implanted into single crystal silicon to form an N-type conductive semiconductor substrate, or a B element may be implanted into single crystal silicon to form a P-type conductive semiconductor substrate. In this embodiment, the semiconductor substrate 10 is a silicon wafer. That is, the material of the semiconductor substrate 10 is silicon.

[0034] The oxide layer 20 may be formed by a thermal oxidation process.

[0035] In some embodiments, the semiconductor structure to be etched may be Figure 2 shown.

[0036] 102. Form a photoresist layer with a preset pattern on the anti-reflection layer.

[0037] In the specific implementation process, the photoresist layer 40 with a preset pattern can be formed according to the number, position, width and length of the grooves to be etched in the device. Figure 3 Specifically, a photoresist coating layer may be formed by coating a photoresist on the top surface of the anti-reflection layer 30, and then etching the photoresist coating layer to form a photoresist layer 40 having a preset pattern.

[0038] It should be noted that the area on the anti-reflection layer 30 not covered by the photoresist can be etched by an etching process, so that the subsequent etching process can etch the area to be etched, thereby improving the etching accuracy and the production quality of the semiconductor device.

[0039] 103. Using the photoresist layer as a mask, a one-step etching process is performed on the anti-reflective layer and the oxide layer to form a first oxide layer groove and a second oxide layer groove. The widths of the first oxide layer groove and the second oxide layer groove are different, and the oxide layer thicknesses at the bottoms of the first oxide layer groove and the second oxide layer groove are the same.

[0040] Among them, the one-step etching process can be carried out in the reaction chamber of the etching equipment.

[0041] In the specific implementation process, the etching can be controlled by adjusting the process parameters of the etching equipment. Specifically, the etching rate and thus the etching margin (the oxide layer thickness at the bottom of the first oxide layer groove 21 and the second oxide layer groove 22) can be controlled by adjusting the chamber pressure, the radio frequency power of the radio frequency device, the flow rate of the first reaction gas and the flow rate of the second reaction gas.

[0042] It should be noted that the first reaction gas is carbon tetrafluoride (CF4) and the second reaction gas is argon (Ar). It is understandable that

[0043] Among them, the etching gas may include carbon tetrafluoride (CF4) and argon (Ar) gas, and the two gases are introduced into the reaction chamber at the same time; the radio frequency power of the radio frequency device may include high radio frequency power and low frequency radio frequency power, and the two radio frequency powers may exist at the same time to form two radio frequency signals of different powers in the reaction chamber.

[0044] In the embodiment of the present application, the chamber pressure is 20 to 100 mT. The high frequency RF power is 600 to 1000 W. The low frequency RF power is 150 to 500 W. The flow rate of the first reaction gas is 30 to 50 sccm. The flow rate of the second reaction gas is 100 to 200 sccm.

[0045] Preferably, the chamber pressure is 20 mT, the high-frequency RF power is 800 W, the low-frequency RF power is 300 W, the flow rate of the first reaction gas is 40 sccm, and the flow rate of the second reaction gas is 170 sccm.

[0046] It should be noted that the above process parameters can be obtained based on the experience of multiple experiments, so that after a one-step etching process is completed, the widths of the first oxide layer trench 21 and the second oxide layer trench 22 are different, and the oxide layer thicknesses at the bottom of the first oxide layer trench 21 and the second oxide layer trench 22 are the same.

[0047] It should be noted that the width of the first oxide layer groove 21 and the second oxide layer groove 22 is 1-50 μm. In the specific implementation process, when the width of the first oxide layer groove 21 and the second oxide layer groove 22 is not within the range of 1-50 μm, the first reaction gas flow rate and the second reaction gas flow rate can be used to adjust the width of the first oxide layer groove 21 and the second oxide layer groove 22 to within the range of 1-50 μm, ensuring that the oxide layer thickness at the bottom of the first oxide layer groove 21 and the second oxide layer groove 22 is within a controllable range.

[0048] 104. Remove the photoresist layer and the anti-reflective layer.

[0049] The specific method of removing the photoresist layer 40 and the anti-reflection layer 30 can be implemented by common technical means in the art, such as ashing method, which will not be described in detail here.

[0050] In summary, the manufacturing method of the semiconductor device provided by the embodiment of the present application includes providing a semiconductor structure to be etched, the semiconductor structure to be etched includes a semiconductor substrate 10, an oxide layer 20 and an anti-reflection layer 30 stacked in sequence from bottom to top; forming a photoresist layer 40 with a preset pattern on the anti-reflection layer 30; using the photoresist layer 40 as a mask, in the reaction chamber of the etching equipment, by adjusting the process parameters of the etching equipment, a one-step etching process is performed on the anti-reflection layer 30 and the oxide layer 20 to form a first oxide layer groove 21 and a second oxide layer groove 22, the first oxide layer groove 21 and the second oxide layer groove 22 have different widths, and the oxide layer thickness at the bottom of the first oxide layer groove 21 and the second oxide layer groove 22 is the same; removing the photoresist layer 40 and the anti-reflection layer 30. This solution can form oxide layer grooves with different widths and the oxide layer thickness at the bottom is the same through a one-step etching process, thereby improving the reliability of the semiconductor device. That is, this solution can achieve the purpose of controlling the uniformity of the etching allowance through a one-step etching process, the process is simple, the control is convenient, and no multi-step etching is required, thereby improving the etching efficiency.

[0051] like Figure 4 As shown, an embodiment of the present application further provides a semiconductor device, which is formed by the above-mentioned semiconductor device manufacturing method. For details, please refer to the above-mentioned embodiment, which will not be described one by one here.

[0052] The above is a detailed introduction to the manufacturing method of the semiconductor device and the semiconductor device provided by the present application. Specific examples are used in the present application to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the core idea of ​​the present application. At the same time, for technical personnel in this field, according to the idea of ​​the present application, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: include: Providing a semiconductor structure to be etched, the semiconductor structure to be etched comprising a semiconductor substrate, an oxide layer and an anti-reflection layer stacked in sequence from bottom to top; forming a photoresist layer having a preset pattern on the anti-reflection layer; Using the photoresist layer as a mask, performing a one-step etching process on the anti-reflection layer and the oxide layer in a reaction chamber of an etching device by adjusting the process parameters of the etching device to form a first oxide layer groove and a second oxide layer groove, wherein the widths of the first oxide layer groove and the second oxide layer groove are different, and the oxide layer thicknesses at the bottoms of the first oxide layer groove and the second oxide layer groove are the same, so as to achieve the purpose of controlling the uniformity of the etching margin through a one-step etching process, wherein the process parameters include chamber pressure, high-frequency radio frequency power, low-frequency radio frequency power, a first reaction gas flow rate, and a second reaction gas flow rate, wherein the widths of the first oxide layer groove and the second oxide layer groove are 1 to 50 μm; the chamber pressure is 20 mT, the high-frequency radio frequency power is 800 W, the low-frequency radio frequency power is 300 W, the flow rate of the first reaction gas is 40 sccm, and the flow rate of the second reaction gas is 170 sccm; The photoresist layer and the anti-reflective layer are removed.

2. The method for manufacturing a semiconductor device according to claim 1, wherein: The first reaction gas is CF4.

3. The method for manufacturing a semiconductor device according to claim 1, wherein: The second reaction gas is Ar.

4. A semiconductor device, characterized in that: The semiconductor device is formed by the method for manufacturing a semiconductor device according to any one of claims 1 to 3.