Laterally diffused metal-oxide semiconductor devices and their fabrication methods

By setting trenches and dielectric layers to cover the drift region in a laterally diffused metal-oxide-semiconductor device, the technical contradiction between on-resistance and breakdown voltage is resolved, thereby improving device performance and reducing size.

CN117637840BActive Publication Date: 2026-11-10CSMC TECH FAB2 CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202210976315.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-15
Publication Date
2026-11-10
Estimated Expiration
2042-08-15

AI Technical Summary

Technical Problem

Existing laterally diffused metal-oxide-semiconductor devices struggle to simultaneously improve performance while reducing on-resistance and increasing breakdown voltage, and their size is difficult to shrink, hindering the reduction of chip area.

Method used

In the device, trenches are set around the drift region, and the sidewalls and part of the bottom wall of the drift region are covered by the dielectric layer. The gate is also covered by part of the bottom wall on the dielectric layer to form a field plate structure, which helps the depletion of the drift region, thereby reducing the surface peak electric field and increasing the critical breakdown electric field.

Benefits of technology

By flexibly adjusting the breakdown voltage while reducing the on-resistance, especially by increasing the breakdown voltage of the device while reducing the on-resistance, the device performance can be improved and the lateral size reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117637840B_ABST
    Figure CN117637840B_ABST
Patent Text Reader

Abstract

This application relates to a laterally diffused metal-oxide-semiconductor (MOSFET) device and its fabrication method. The MOSFET includes: a substrate with trenches; a drift region located within the substrate; wherein the trenches surround the drift region; a dielectric layer located on the substrate and surrounding the drift region; wherein the dielectric layer covers at least a portion of a first sidewall and a portion of a bottom wall connected to the first sidewall; and a gate surrounding the drift region. The gate covers a portion of the surface of the dielectric layer and extends towards the bottom wall of the trench to cover a portion of the bottom wall of the trench. The MOSFET provided by this application can improve the critical breakdown electric field of the drift region, thereby allowing for flexible adjustment of the device's breakdown voltage while reducing on-resistance, particularly improving the breakdown voltage while reducing on-resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of integrated circuit technology, and in particular to a laterally diffused metal-oxide-semiconductor device and its fabrication method. Background Technology

[0002] With the continuous development of semiconductor technology, the application of Lateral Double-Diffuse Metal-Oxide-Semiconductor (LDMOS) devices is becoming increasingly widespread, while also placing higher demands on their performance. However, for LDMOS devices, there is an unavoidable technical contradiction between reducing on-resistance and ensuring high breakdown voltage, making it difficult to further improve device performance. Furthermore, while improving device performance, it is also difficult to further reduce device size, thus affecting the reduction of the overall chip area. Summary of the Invention

[0003] Therefore, it is necessary to provide a laterally diffused metal-oxide semiconductor device and its fabrication method to address at least one of the above-mentioned problems.

[0004] To achieve at least one of the above objectives, this application provides a laterally diffused metal-oxide-semiconductor device, comprising:

[0005] A substrate having trenches, the trenches including a first sidewall and a bottom wall connected to the first sidewall;

[0006] A drift region is located within the substrate, wherein the trench is disposed around the drift region;

[0007] A dielectric layer is located on the substrate and disposed around the drift region; wherein the dielectric layer covers at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall;

[0008] A gate is disposed around the drift region, wherein the gate covers a portion of the dielectric layer and extends toward the bottom wall to cover a portion of the bottom wall.

[0009] The aforementioned laterally diffused metal-oxide-semiconductor device, by surrounding the drift region with trenches, effectively "stretches" a portion of the drift region, extending it vertically. This ensures a significant reduction in the device's lateral dimensions while improving performance. Furthermore, the dielectric layer covers the first sidewall and part of the bottom wall, achieving large-area coverage of the drift region. The portion of the gate covering the dielectric layer acts as a field plate. Because the trenches surround the drift region, the portion of the gate covering the dielectric layer assists in the depletion of the drift region from its surroundings, effectively reducing the peak electric field on the drift region surface and increasing the critical breakdown electric field. This allows for flexible adjustment of the device's breakdown voltage while reducing on-resistance, particularly improving the breakdown voltage simultaneously.

[0010] In one embodiment, the trench is at least located on both sides of the drift region along a first direction; the first direction is perpendicular to the thickness direction of the substrate.

[0011] In one embodiment, the number of grooves is two, and the two grooves are located on both sides of the drift region along the first direction;

[0012] At least a portion of the drift region is located within the substrate between the two first sidewalls of the two trenches.

[0013] In one embodiment, the dielectric layer covers the entire first sidewall.

[0014] In one embodiment, the laterally diffused metal-oxide-semiconductor device further includes:

[0015] A body region is disposed within the substrate at the bottom of the trench; wherein the orthographic projection of the gate on the substrate overlaps with the body region.

[0016] A source region is disposed within the body region; wherein the orthographic projection of the gate on the substrate is tangent to or overlaps with the source region, and there is a gap between the end of the source region near the drift region and the end of the body region near the drift region;

[0017] The drain region is located within the substrate, on the side of the gate region away from the source region;

[0018] A buried layer is located within the substrate and on the side of the drift region away from the gate.

[0019] In one embodiment, the dielectric layer includes a high-temperature oxide layer.

[0020] In one embodiment, the gate includes a gate oxide layer and a polysilicon layer stacked together, the gate oxide layer being located on the side of the polysilicon layer closer to the dielectric layer, and the thickness of the dielectric layer being greater than the thickness of the gate oxide layer.

[0021] In one embodiment, the outer contour of the orthogonal projection of the dielectric layer onto the substrate lies within the outer contour of the drift region.

[0022] And / or, the outer contour of the gate's orthogonal projection on the bottom wall is located outside the outer contour of the drift region.

[0023] This application also provides a method for fabricating a laterally diffused metal-oxide-semiconductor device, comprising:

[0024] Provide substrate;

[0025] A trench is formed on the substrate; the trench includes a first sidewall and a bottom wall that are interconnected.

[0026] A dielectric layer is formed on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall;

[0027] A drift region is formed within the substrate, wherein the trench and the dielectric layer are both disposed around the drift region;

[0028] A gate is formed on the substrate, wherein the gate is disposed around the drift region; the gate covers a portion of the dielectric layer and extends toward the bottom wall to cover a portion of the bottom wall.

[0029] The fabrication method of the aforementioned laterally diffused metal-oxide-semiconductor device, by setting trenches around the drift region, is equivalent to "stretching" part of the drift region, extending this part of the drift region in the vertical direction. This ensures that the device performance is improved while significantly reducing the lateral size of the device. Furthermore, the dielectric layer covers the first sidewall and part of the bottom wall to achieve large-area coverage of the drift region, with the portion of the gate covering the dielectric layer acting as a field plate. Since the trenches are positioned around the drift region, the portion of the gate covering the dielectric layer assists in the depletion of the drift region from its surroundings, effectively reducing the peak electric field on the surface of the drift region and increasing the critical breakdown electric field. This allows for flexible adjustment of the device's breakdown voltage while reducing on-resistance, particularly increasing the breakdown voltage simultaneously.

[0030] In one embodiment, the step of forming a dielectric layer on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall includes:

[0031] A first oxide layer is formed on the substrate using a high-temperature oxide deposition technique;

[0032] The first oxide layer is etched to form the dielectric layer.

[0033] or,

[0034] A mask layer is formed on the surface of the substrate, exposing at least a portion of the surface of the first sidewall and a portion of the surface of the bottom wall connected to the first sidewall;

[0035] A first oxide layer is formed on the exposed surface of the substrate and on the surface of the mask layer;

[0036] The mask layer and the first oxide layer located on the surface of the mask layer are removed to form the dielectric layer.

[0037] In one embodiment, prior to the step of forming trenches on the surface of the substrate, the method further includes:

[0038] A buried layer is formed within the substrate.

[0039] In one embodiment, the step of forming a gate on the substrate, wherein the gate is disposed around the drift region, includes:

[0040] A second oxide layer is formed on the surface of the substrate;

[0041] A polycrystalline silicon material layer is formed on the surface of the second oxide layer;

[0042] The second oxide layer and the polysilicon material layer are etched to form the gate oxide layer and the polysilicon layer.

[0043] In one embodiment, after the step of forming a gate on the substrate, wherein the gate is disposed around the drift region, the method further includes:

[0044] A body region is formed within the substrate, wherein the body region is disposed within the substrate at the bottom of the trench, and the orthogonal projection of the gate on the substrate overlaps with the body region;

[0045] A source region is formed within the substrate, wherein the source region is disposed within the body region, the orthogonal projection of the gate on the substrate is tangent to or overlaps with the source region, and there is a gap between the end of the source region near the drift region and the end of the body region near the drift region. Attached Figure Description

[0046] To more clearly illustrate the technical solutions in the embodiments or exemplary embodiments of this application, the drawings used in the description of the embodiments or exemplary embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0047] Figure 1 This is a flowchart of a method for fabricating a laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application;

[0048] Figure 2 This is a flowchart illustrating the fabrication process of the dielectric layer in a method for fabricating a laterally diffused metal-oxide-semiconductor device according to an embodiment of this application.

[0049] Figure 3 This is another flowchart illustrating the fabrication process of the dielectric layer in a method for fabricating a laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application.

[0050] Figure 4 This is a flowchart illustrating the fabrication process of the gate in a method for fabricating a laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application.

[0051] Figures 5 to 13 This is a schematic cross-sectional view of the device structure during the fabrication process of the laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application.

[0052] Figure 14 for Figure 13 A partial cross-sectional schematic diagram of a laterally diffused metal-oxide-semiconductor device.

[0053] Figure 15 This is a top view of a laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application;

[0054] Figure 16 This is a top view of another laterally diffused metal-oxide-semiconductor device provided in one embodiment of this application.

[0055] Explanation of reference numerals in the attached figures:

[0056] 1- Laterally diffused metal-oxide-semiconductor device; 10- Substrate; 11- Base layer; 12- Epitaxial layer; 13- Heavily doped region; 14- Isolation region; 141- First doped region; 1411- First connection region; 15- Buried layer; 16- Trench; 16a- First sidewall; 16b- Bottom wall; 17- Isolation trench; 18- Second doped region; 181- Second connection region; 20- Dielectric layer; 21- First oxide layer; 30- Drift region; 31- Buffer zone; 32- Drain region; 40- Gate; 41- Gate oxide layer; 42- Polysilicon layer; 43- Second oxide layer; 44- Polysilicon material layer; 50- Body region; 51- Source region; 52- Body lead-out region; 60- Channel region; 70- Accumulation region. Detailed Implementation

[0057] To facilitate understanding of this application, a more complete description will be provided below with reference to the accompanying drawings, which illustrate embodiments of the present application. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that the disclosure of this application will be thorough and complete.

[0058] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein in the specification of this application is for the purpose of describing particular embodiments only and is not intended to be limiting of this application.

[0059] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, parts, regions, layers, doping types, and / or portions, these elements, parts, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, part, region, layer, doping type, or portion from another element, part, region, layer, doping type, or portion. Therefore, without departing from the teachings of this application, the first element, component, region, layer, doping type, or portion discussed below may be represented as a second element, component, region, layer, or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.

[0060] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, the element or feature described as “below,” “under,” or “below” will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. Furthermore, the device may also include other orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptive terms used herein will be interpreted accordingly.

[0061] When used herein, the singular forms of “a,” “an,” and “the” may also include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising / including” or “having,” etc., specify the presence of the stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not preclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. Meanwhile, in this specification, the term “and / or” includes any and all combinations of the associated listed items.

[0062] Embodiments of the application are described herein with reference to cross-sectional views illustrating ideal embodiments (and intermediate structures), thus allowing for the expectation of variations in the illustrated shapes due to, for example, manufacturing techniques and / or tolerances. Therefore, embodiments of the application should not be limited to the specific shapes of the regions shown herein, but rather include shape deviations due to, for example, manufacturing techniques. For instance, implantation regions shown as rectangular typically have rounded or curved features at their edges and / or implantation concentration gradients, rather than a binary change from implantation regions to non-implantation regions. Similarly, buried regions formed by implantation can result in some implantation in the region between the buried region and the surface traversed during implantation. Therefore, the regions shown in the figures are substantially schematic, and their shapes do not represent the actual shapes of regions of the device and do not limit the scope of the application.

[0063] This application provides a method for fabricating a laterally diffused metal-oxide-semiconductor device and the laterally diffused metal-oxide-semiconductor device, which can flexibly adjust the breakdown voltage of the laterally diffused metal-oxide-semiconductor device while reducing the on-resistance, and in particular, can increase the breakdown voltage of the laterally diffused metal-oxide-semiconductor device while reducing the on-resistance.

[0064] In this embodiment, the laterally diffused metal-oxide-semiconductor device is an N-type laterally diffused metal-oxide-semiconductor device, with the first doping type being P-type and the second doping type being N-type. In other embodiments, the laterally diffused metal-oxide-semiconductor device can also be a P-type laterally diffused metal-oxide-semiconductor device, with the first doping type being N-type and the second doping type being P-type.

[0065] In a first aspect, embodiments of this application provide a method for fabricating a laterally diffused metal-oxide-semiconductor device. (Refer to...) Figure 1 As shown, the fabrication method of this laterally diffused metal-oxide-semiconductor device includes the following steps:

[0066] S100: Provides a substrate. The structure of substrate 10 is shown in the reference diagram. Figure 5 As shown, the substrate 10 can be made of monocrystalline silicon, polycrystalline silicon, amorphous silicon, germanium-silicon compound, silicon-on-insulator (SOI), or low-temperature polycrystalline silicon (LTPS), or other materials known to those skilled in the art. The substrate 10 can provide a supporting foundation for the structural layers on it. In this embodiment, the substrate 10 includes a base layer 11 and an epitaxial layer 12 located on the base layer 11.

[0067] S100: The step of providing a substrate may specifically include the following steps:

[0068] S110: Provides the body layer. The substrate layer 11 is a P-type semiconductor.

[0069] S120: A heavily doped region is formed within the substrate layer. Specifically, N-type ions can be implanted into the substrate layer 11 to form the heavily doped region 13.

[0070] S130: An epitaxial layer is formed on the substrate layer. The epitaxial layer 12 can be grown on the substrate layer 11 by vapor phase epitaxy or molecular beam epitaxy.

[0071] The substrate 10 can be formed through the above steps. After forming the substrate 10, the following steps may also be included:

[0072] S140: A buried layer is formed within the substrate. Specifically, P-type ions can be implanted into the epitaxial layer 12 to form a buried layer 15, which serves as the depletion drift region 30.

[0073] S150: An isolation region is formed within the substrate. Specifically, two isolation regions 14 are formed by implanting N-type ions into the epitaxial layer 12 via ion implantation. The two isolation regions 14 are located on either side of the buried layer 15 and are adjacent to the heavily doped region 13. Thus, the isolation regions 14 and the heavily doped region 13 form an isolation shield, and the main device of the laterally diffused metal-oxide-semiconductor device 1 is located within the isolation shield. The structure after the formation of the buried layer 15 and the isolation regions 14 is as follows... Figure 5 As shown.

[0074] Once quarantine zone 14 is established, the following steps can be taken:

[0075] S200: Forming trenches on the substrate. This step may include the following steps:

[0076] S210: A mask layer is formed on the substrate surface. The mask layer can be a photoresist layer or a hard mask layer such as a silicon nitride layer or a carbon layer.

[0077] S220: Pattern the mask layer to obtain a patterned mask layer with openings that expose the substrate and define the shape and location of the trenches.

[0078] S220: The substrate is etched based on a patterned mask layer to form trenches within the substrate.

[0079] S230: Remove the patterned mask layer. The structure after trench 16 is formed is as follows. Figure 6 As shown.

[0080] Understandably, in this step, isolation trenches 17 can also be formed on the surface of substrate 10, with the isolation trenches 17 primarily serving an isolation function. The structure after trench 16 is formed is as follows: Figure 6As shown. In one embodiment, the trench 16 includes a first sidewall 16a and a bottom wall 16b that are connected to each other. There can be two trenches 16, spaced apart, with the two sidewalls of the two trenches 16 adjacent to each other forming the first sidewall 16a. It is understood that the cross-sectional shape of the trench 16 can be an inverted trapezoid, rectangle, semicircle, etc.

[0081] S300: A dielectric layer is formed on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall. The structure of the dielectric layer 20 after its formation is as follows: Figure 8 As shown. The dielectric layer 20 is made of silicon dioxide. It is understood that the dielectric layer 20 may cover only a portion of the first sidewall 16a or cover the entire first sidewall 16a. This embodiment of the application is illustrated by taking the example of the dielectric layer 20 covering the entire first sidewall 16a.

[0082] S400: A drift region is formed within the substrate, wherein trenches and dielectric layers are both disposed around the drift region. Specifically, N-type ions can be implanted into the epitaxial layer 12 via ion implantation to form the drift region 30. The structure after the drift region 30 is formed is as follows. Figure 9 As shown, the substrate 10 between the two trenches 16 is equivalent to a protrusion, the drift region 30 is located within this protrusion and extends towards the buried layer 15, and a portion of the drift region 30 is located at the bottom of the two trenches 16. Compared to the existing planar laterally diffused metal-oxide-semiconductor devices with no trenches around the drift region, the embodiments of this application are equivalent to "stretching" a portion of the drift region 30 in a direction away from the substrate 10, so that this portion of the drift region 30 extends in the vertical direction (the thickness direction of the substrate 10).

[0083] Understandably, please continue to refer to Figure 9 As shown, in this step, N-type ions can be implanted in the isolation region 14 to form a first doped region 141, P-type ions can be implanted in the substrate 10 on the side of the isolation region 14 away from the drift region 30 to form a second doped region 18, and N-type ions can be implanted in the top (region near the surface of the substrate 10) of the drift region 30 to form a buffer zone 31 within the drift region 30. It should be noted that the buffer zone 31 is also part of the drift region 30, but the doping concentration of the buffer zone 31 is greater than the doping concentration of other regions in the drift region 30 (regions outside the buffer zone 31).

[0084] Understandably, the substrate 10 can be annealed after ion implantation. Annealing can repair the lattice loss caused to the substrate 10 during ion implantation and activate the dopant ions. Specifically, rapid thermal annealing (RTA) can be used to anneal the ion-implanted substrate 10. Compared with ordinary annealing, rapid thermal annealing has a shorter annealing time, avoids prolonged high temperatures that could lead to dopant ion diffusion, and reduces the instantaneous enhanced diffusion of dopant ions.

[0085] S500: A gate is formed on the substrate, wherein the gate is disposed around the drift region. The structure after the gate 40 is formed is as follows. Figure 12 As shown in the figure, the gate 40 covers a portion of the surface of the dielectric layer 20 and extends towards the bottom wall 16b of the trench 16 to cover a portion of the bottom wall 16b of the trench 16. This can be understood as the gate 40 not only covering the surface of the dielectric layer 20 facing away from the substrate 10, but also covering a portion of the surface of the bottom wall 16b of the trench 16.

[0086] The fabrication method of the laterally diffused metal-oxide-semiconductor device provided in this application embodiment, by setting trench 16 around the drift region 30, is equivalent to "stretching" a portion of the drift region 30, causing this portion of the drift region 30 to extend in the vertical direction. This ensures that the performance of the laterally diffused metal-oxide-semiconductor device 1 is maintained while significantly reducing the lateral size of the device. Furthermore, the dielectric layer 20 covers the first sidewall 16a and a portion of the bottom wall 16b to achieve large-area coverage of the drift region 30. The portion of the gate 40 covering the dielectric layer 20 serves as a field plate. Since the trench 16 is located around the drift region 30, the portion of the gate 40 covering the dielectric layer 20 assists in the depletion of the drift region 30 from its surroundings. This effectively reduces the peak electric field on the surface of the drift region 30 and increases the critical breakdown electric field of the drift region 30. Therefore, the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1 can be flexibly adjusted while reducing the on-resistance, especially increasing the breakdown voltage while reducing the on-resistance.

[0087] Assuming the breakdown voltage of existing laterally diffused metal-oxide-semiconductor (LMDS) devices is taken as the standard value, the breakdown voltage of the LMDS device 1 in this application has a "margin." Therefore, in the technical solution of this application, the on-resistance can be reduced by increasing the doping concentration of the drift region 30 or reducing the size of the LMDS device 1. While reducing the on-resistance, the breakdown voltage of the LMDS device 1 decreases until it reaches the standard value, thus achieving flexible adjustment of the breakdown voltage of the LMDS device 1 while reducing the on-resistance. Furthermore, compared with existing LMDS devices, this application can achieve a lower on-resistance at the same breakdown voltage. In other words, the LMDS device 1 provided by this application can maintain a high breakdown voltage while reducing the on-resistance.

[0088] In one embodiment, reference Figure 2 As shown, S300: The step of forming a dielectric layer on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall specifically includes the following steps:

[0089] S310: A first oxide layer is formed on the substrate using a high-temperature oxide deposition technique. The structure of the first oxide layer 21 after its formation is as follows: Figure 7 As shown.

[0090] S320: The first oxide layer is etched to form a dielectric layer. The first oxide layer 21 can be etched using either dry etching or wet etching processes. The structure of the dielectric layer 20 after formation is as follows... Figure 8 As shown.

[0091] In another embodiment, refer to Figure 3 As shown, S300: The step of forming a dielectric layer on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall specifically includes the following steps:

[0092] S310: A mask layer is formed on the surface of the substrate, exposing at least a portion of the surface of the first sidewall and a portion of the surface of the bottom wall connected to the first sidewall.

[0093] As an example, a nitride layer and a photoresist layer can be formed sequentially on the surface of the substrate 10, and then the nitride layer and the photoresist layer can be etched to expose at least a portion of the surface of the first sidewall and a portion of the surface of the bottom wall connected to the first sidewall.

[0094] S320: A first oxide layer is formed on the exposed surface of the substrate and on the surface of the mask layer. The first oxide layer can be formed by a local thermal oxidation process.

[0095] S330: Remove the mask layer and the first oxide layer located on the surface of the mask layer to form a dielectric layer.

[0096] In one embodiment, reference Figure 4 As shown, S500: Forming a gate on the substrate, wherein the step of the gate being disposed around the drift region specifically includes the following steps:

[0097] S510: A second oxide layer is formed on the surface of the substrate. The second oxide layer 43 can be formed by methods such as dry oxidation, high-temperature oxidation, or wet oxidation. The structure of the second oxide layer 43 after formation is as follows... Figure 10 As shown, the second oxide layer 43 covers the exposed surface of the substrate 10 and the surface of the dielectric layer 20, and the thickness of the second oxide layer 43 is less than the thickness of the dielectric layer 20. The material of the second oxide layer 43 can be silicon dioxide.

[0098] S520: A polycrystalline silicon material layer is formed on the surface of the second oxide layer. The structure of the polycrystalline silicon material layer 44 after its formation is as follows. Figure 11 As shown. The polycrystalline silicon material layer 44 can be made of polycrystalline silicon.

[0099] S530: The second oxide layer and the polysilicon material layer are etched to form the gate oxide layer and the polysilicon layer. The gate oxide layer 41 and the polysilicon layer 42 form the gate 40, and the structure of the gate 40 after its formation is as follows. Figure 12 As shown. The second oxide layer 43 and the polysilicon material layer 44 can be etched using either dry etching or wet etching processes.

[0100] In one embodiment, S500: forming a gate on the substrate, wherein after the step of distributing the gate around the drift region, the method further includes:

[0101] S600: A body region is formed within the substrate, wherein the body region is located within the substrate at the bottom of the trench, and the orthogonal projection of the gate onto the substrate overlaps with the body region. The body region 50 can be formed by implanting P-type ions into the substrate 10 via ion implantation. The structure of the formed body region 50 is as follows... Figure 13 As shown in the figure, the body region 50 is disposed in the substrate 10 at the bottom of the trench 16, and the orthographic projection of the gate 40 on the substrate 10 overlaps with the body region 50.

[0102] S700: A source region is formed within a substrate, wherein the source region is disposed within a body region, the orthogonal projection of the gate onto the substrate is tangent to or overlaps with the source region, and there is a gap between the end of the source region near the drift region and the end of the body region near the drift region. (Refer to...) Figure 13 and Figure 14As shown in the figure, the orthogonal projection of the gate 40 onto the substrate 10 is tangent to the source region 51. There is a gap between the end of the source region 51 near the drift region 30 and the end of the body region 50 near the drift region 30. This gap is located in the channel region 60. Alternatively, it can be understood that the source region 51 and the gate 40 do not overlap in the thickness direction of the substrate 10, and the area where the gate 40 and the body region 50 overlap in the thickness direction of the substrate 10 is the channel region 60. In another embodiment, the gate 40 may also extend to cover the source region 51, ensuring that the channel can be completely inverted when the laterally diffused metal-oxide-semiconductor device 1 is operating.

[0103] In this step, N-type ions can be implanted into the first doped region 141 within the substrate 10 to form a first connection region 1411, and P-type ions can be implanted into the second doped region 18 within the substrate 10 to form a second connection region 181. The first connection region 1411 and the second connection region 181 can serve as electrical leads, connected to appropriate potentials as needed. It is understood that the doping concentration of the first connection region 1411 is greater than that of the first doped region 141, and the doping concentration of the second connection region 181 is greater than that of the second doped region 18.

[0104] In this embodiment, the drift region 30 and the drain region are integrated. In this step, N-type ions can also be implanted into the buffer zone 31 in the substrate 10 to form a drain lead-out region 32. The drain lead-out region 32 can serve as the electrical lead-out terminal of the drain electrode. The doping concentration of the drain lead-out region 32 is greater than the doping concentration of the buffer zone 31, and the doping concentration of the buffer zone 31 is greater than the doping concentration of the drift region 30. The buffer zone 31 can reduce the concentration gradient between the drain lead-out region 32 and the drift region 30, increase the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1 in the on-state, reduce the on-resistance, and reduce the peak electric field of the drain lead-out region 32.

[0105] In this step, P-type ions can be implanted into the body region 50 within the substrate 10 to form a body lead-out region 52. The source region 51 and the body lead-out region 52 are adjacent, and the doping concentrations of both the source region 51 and the body lead-out region 52 are greater than the doping concentration of the body region 50. The source region 51 can serve as the electrical lead-out terminal of the source electrode, and the body lead-out region 52 can serve as the electrical lead-out terminal of the body electrode.

[0106] Reference Figure 14 As shown, the region where the drift region 30 overlaps with the gate 40 in the thickness direction of the substrate 10 and does not overlap with the dielectric layer 20 in the thickness direction of the substrate 10 is the carrier accumulation region 70.

[0107] It should be understood that, although Figure 1The steps in the flowchart are shown sequentially as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order in which these steps are executed, and they can be performed in other orders. Figure 1 At least some of the steps in the process may include multiple steps or multiple stages. These steps or stages are not necessarily completed at the same time, but may be executed at different times. The execution order of these steps or stages is not necessarily sequential, but may be executed in turn or alternately with other steps or at least some of the steps or stages in other steps.

[0108] Secondly, embodiments of this application provide a laterally diffused metal-oxide-semiconductor device. (Refer to...) Figure 13 and Figure 14 As shown, the laterally diffused metal-oxide-semiconductor device 1 includes:

[0109] A substrate 10 has trenches 16 on its surface. The substrate 10 includes a base layer 11 and an epitaxial layer 12 located on the base layer 11. The base layer 11 is p-type doped, and the trenches 16 are located on the epitaxial layer 12. (Refer to...) Figure 6 As shown, the cross-sectional shape of the trench 16 is an inverted trapezoid, and the trench 16 includes a first sidewall 16a and a bottom wall 16b that are connected to each other. It can be understood that the cross-sectional shape of the trench 16 can also be rectangular, semi-circular, etc.

[0110] Drift region 30 is located within substrate 10, and the doping type of drift region 30 is N-type. (Refer to...) Figure 9 As shown, the drift region 30 is located within the epitaxial layer 12, and the trench 16 is disposed around the drift region 30. It should be noted that, taking the plane containing the substrate 10 as an example, [referring to...] Figure 15 As shown, the plane containing the substrate 10 has a first direction a and a second direction b. The drift region 30 has four sides, two sides in the first direction a and two sides in the second direction b. "Around" means that the trench 16 surrounds at least two sides of the drift region 30. For example, the trench 16 may surround two sides of the drift region 30 in the second direction b, or it may surround one side of the drift region 30 in the first direction a and one side of the drift region 30 in the second direction b. The trench 16 may be a continuous trench or a discontinuous trench.

[0111] A dielectric layer 20 is located on the substrate 10 and is disposed around the drift region 30. The dielectric layer 20 covers at least a portion of the first sidewall 16a and a portion of the bottom wall 16b connected to the first sidewall 16a. The dielectric layer 20 is made of silicon dioxide.

[0112] A gate 40 is disposed around the drift region 30. The gate 40 covers a portion of the surface of the dielectric layer 20 and extends towards the bottom wall 16b of the trench 16 to cover a portion of the bottom wall 16b of the trench 16. This can be understood as the gate 40 covering not only a portion of the surface of the dielectric layer 20 facing away from the substrate 10, but also a portion of the surface of the bottom wall 16b of the trench 16.

[0113] The laterally diffused metal-oxide-semiconductor (MMS) device 1 provided in this application embodiment, by setting trenches 16 around the drift region 30, is equivalent to "stretching" a portion of the drift region 30, causing this portion of the drift region 30 to extend in the vertical direction. This ensures that the performance of the MMS device 1 is maintained while significantly reducing its lateral dimensions. Furthermore, the dielectric layer 20 covers the first sidewall 16a and a portion of the bottom wall 16b, achieving a large-area coverage of the drift region 30 by the dielectric layer 20. The portion of the gate 40 covering the dielectric layer 20 serves as a field plate. Since the trenches 16 are positioned around the drift region 30, the portion of the gate 40 covering the dielectric layer 20 assists in the depletion of the drift region 30 from its surroundings. This effectively reduces the peak electric field on the surface of the drift region 30 and increases the critical breakdown electric field of the drift region 30. Therefore, the breakdown voltage of the MMS device 1 can be flexibly adjusted while reducing the on-resistance, especially increasing the breakdown voltage while reducing the on-resistance.

[0114] In one embodiment, trench 16 is at least disposed on both sides of drift region 30 along a first direction a; the first direction a is perpendicular to the thickness direction of substrate 10. In this way, the gate 40 on the surface of dielectric layer 20 acts as a field plate on both sides of drift region 30 along the first direction a to assist the depletion of drift region 30, which can effectively reduce the peak electric field on the surface of drift region 30 and increase the critical breakdown electric field of drift region 30.

[0115] In one embodiment, there are two trenches 16, located on either side of the drift region 30 along the first direction a. At least a portion of the drift region 30 is located within the substrate 10 between the two first sidewalls 16a of the two trenches 16. Alternatively, the substrate 10 between the two trenches 16 can be understood as a protrusion, with the drift region 30 located within this protrusion and extending towards the buried layer 15. A portion of the drift region 30 is also located at the bottom of the two trenches 16. The cross-sectional shape of the drift region 30 is "convex." It can be seen that this embodiment essentially "stretches" a portion of the drift region 30 in a direction away from the substrate 10, causing this portion of the drift region 30 to extend in a vertical direction.

[0116] In one embodiment, reference Figure 14 As shown, the laterally diffused metal-oxide-semiconductor device 1 further includes:

[0117] A body region 50 is disposed within the substrate 10 at the bottom of the trench 16, and the body region 50 is p-type doped. Near the bottom wall 16b of the trench 16 within the body region 50, there are adjacent source regions 51 and body lead-out regions 52. The source regions 51 and body lead-out regions 52 have opposite doping types: source region 51 can be n-type doped, and body lead-out regions 52 can be p-type doped. Both source regions 51 and body lead-out regions 52 are part of the body region 50, and their doping concentrations are greater than those of other regions within the body region 50 (regions outside source regions 51 and body lead-out regions 52). Source region 51 can serve as the electrical lead-out terminal of the source electrode, and body lead-out region 52 can serve as the electrical lead-out terminal of the body electrode.

[0118] The orthogonal projection of the gate 40 onto the substrate 10 is tangent to the source region 51. A gap exists between the end of the source region 51 near the drift region 30 and the end of the body region 50 near the drift region 30; this gap constitutes the channel region 60. Alternatively, the source region 51 and the gate 40 do not overlap in the thickness direction of the substrate 10, and the area where the gate 40 and the body region 50 overlap in the thickness direction of the substrate 10 constitutes the channel region 60. In another embodiment, the gate 40 may also extend over the source region 51 to ensure complete channel inversion during operation of the laterally diffused metal-oxide-semiconductor device 1.

[0119] The buried layer 15 is located within the epitaxial layer 12 of the substrate 10 and is situated on the side of the drift region 30 away from the gate 40. The buried layer 15 is p-type doped and can be used to deplete the drift region 30.

[0120] In this embodiment, the drain region (not shown) and part of the drift region 30 of the laterally diffused metal-oxide-semiconductor device 1 are integrally disposed, wherein the drain region is located within the substrate 10 and on the side of the gate 40 away from the body region 50. The top of the drift region 30 (the region near the surface of the substrate 10) also has a buffer 31, which is N-type doped. It should be noted that the buffer 31 is also part of the drift region 30, but the doping concentration of the buffer 31 is greater than that of other regions in the drift region 30 (the region outside the buffer 31). Simultaneously, the top of the buffer 31 (the region near the surface of the substrate 10) also has a drain lead-out region 32, which is N-type doped and can serve as the electrical lead-out terminal of the drain. It should be noted that the doping concentration of the drain lead-out region 32 is greater than that of the buffer 31. The buffer 31 can reduce the concentration gradient between the drain region 32 and the drift region 30, increase the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1 in the turn-on state, reduce the on-resistance, and reduce the peak electric field of the drain region 32.

[0121] It should be noted that the drift region 30 can be arranged adjacent to or spaced apart from the body region 50. When they are spaced apart, since the epitaxial layer 12 is also P-type, the area of ​​the epitaxial layer 12 covered by the gate 40 will also be inverted to serve as a conductive channel. The doping concentration of the epitaxial layer 12 is generally low. Although this part of the epitaxial layer 12 serves as the channel region 60, the turn-on voltage of the laterally diffused metal-oxide-semiconductor device 1 is still determined by the overlapping area of ​​the gate 40 and the body region 50.

[0122] In one embodiment, a heavily doped region 13 is also formed in the substrate layer 11, and two spaced-apart isolation regions 14 are formed in the epitaxial layer 12. The two isolation regions 14 are located on both sides of the buried layer 15 and are in contact with the heavily doped region 13. In this way, the isolation regions 14 and the heavily doped region 13 form an isolation shield, and the main devices of the laterally diffused metal-oxide-semiconductor device 1 (e.g., drift region 30, body region 50, and gate 40, etc.) are located in the area enclosed by the isolation shield.

[0123] In one embodiment, the isolation region 14 further includes a first doped region 141, and the first doped region 141 includes a first connection region 1411. Both the first doped region 141 and the first connection region 1411 are N-type doped, and the doping concentration of the first connection region 1411 is greater than that of the first doped region 141. A second doped region 18 is also provided on the side of the isolation region 14 away from the drift region 30. The second doped region 18 includes a second connection region 181. Both the second doped region 18 and the second connection region 181 are P-type doped, and the doping concentration of the second connection region 181 is greater than that of the second doped region 18. The first connection region 1411 and the second connection region 181 can serve as electrical leads, connected to corresponding potentials as needed.

[0124] In this embodiment, field plates (gate 40) are disposed on both sides of the drift region 30. The field plates on both sides jointly deplete the drift region 30 located in the middle, thereby better depleting the drift region 30, minimizing the peak electric field on the surface of the drift region 30, and thus increasing the critical breakdown electric field of the drift region 30, thereby increasing the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1. Therefore, the doping concentration of the drift region 30 can be made higher, thereby reducing the on-resistance of the laterally diffused metal-oxide-semiconductor device 1 and increasing the on-state current of the laterally diffused metal-oxide-semiconductor device 1. Alternatively, the same breakdown voltage can be maintained to reduce the size of the laterally diffused metal-oxide-semiconductor device 1 and improve the overall performance of the laterally diffused metal-oxide-semiconductor device 1.

[0125] In one embodiment, the dielectric layer 20 covers the entire first sidewall 16a. This allows the field plate formed by the gate 40 to cover a larger area of ​​the drift region 30, thereby better depleting the drift region 30, minimizing the peak electric field on the surface of the drift region 30, increasing the critical breakdown electric field of the drift region 30, and consequently increasing the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1. Therefore, a higher doping concentration in the drift region 30 can be achieved, thereby reducing the on-resistance of the laterally diffused metal-oxide-semiconductor device 1 and increasing its on-state current. Alternatively, the same breakdown voltage can be maintained while reducing the size of the laterally diffused metal-oxide-semiconductor device 1 and improving its overall performance.

[0126] In one embodiment, the dielectric layer includes a high-temperature oxidation (HTO) layer. The dielectric layer can be made of silicon dioxide, specifically fabricated using a high-temperature oxidation process.

[0127] In one embodiment, the gate 40 includes a gate oxide layer 41 and a polysilicon layer 42 stacked together, with the gate oxide layer 41 located on the side of the polysilicon layer 42 closest to the dielectric layer 20. The gate oxide layer 41 is made of silicon dioxide, and the polysilicon layer 42 is made of polysilicon. As an example, the thickness of the dielectric layer 20 is greater than the thickness of the gate oxide layer 41. This allows the dielectric layer 20 to withstand a higher electric field, preventing premature breakdown of the dielectric layer 20.

[0128] In one embodiment, the outer contour of the orthographic projection of the dielectric layer 20 onto the substrate 10 lies within the outer contour of the drift region 30. This can also be understood as follows: the drift region 30 at the bottom of the trench 16 and the dielectric layer 20 have a non-overlapping region in the thickness direction of the substrate 10; this non-overlapping region is the carrier accumulation region 70, and the field plate formed by the gate 40 has no depletion effect on the carrier accumulation region 70.

[0129] In one embodiment, the outer contour of the gate 40 projected onto the bottom wall 16b is located outside the outer contour of the drift region 30. Thus, the gate 40 can extend toward the body region 50, thereby having an overlapping region with the body region 50 in the thickness direction of the substrate 10, which is the channel region 60.

[0130] It should be noted that the laterally diffused metal-oxide-semiconductor device 1 provided in this application embodiment can be arranged in the following two ways. (Refer to...) Figure 15As shown, the first arrangement can be considered a "trench strip" arrangement, that is, the drift region 30 is located in the middle of the laterally diffused metal-oxide-semiconductor device 1, and the gate 40 and body region 50 are arranged sequentially in a direction away from the drift region 30. Simultaneously, in this arrangement, the trenches 16 can be considered as discontinuous trenches (or the number of trenches 16 can be considered as two), that is, trenches 16 are provided on both sides of the drift region 30 in the first direction a. (Refer to...) Figure 16 As shown, the second arrangement can be considered as a "groove ring" arrangement, with the drift region 30 located at the center of the laterally diffused metal-oxide-semiconductor device 1, the gate 40 surrounding the drift region 30, and the body region 50 surrounding the gate 40. In this arrangement, the trench 16 can be considered as a continuous trench (or as a single, annular trench).

[0131] In the second configuration, the field plate formed by the gate 40 is located around the drift region 30. Therefore, the field plate around the drift region 30 assists in the depletion of the drift region 30, minimizing the peak electric field on the surface of the drift region 30, thereby increasing the critical breakdown electric field of the drift region 30 and consequently increasing the breakdown voltage of the laterally diffused metal-oxide-semiconductor device 1. Thus, the doping concentration of the drift region 30 can be increased, thereby reducing the on-resistance of the laterally diffused metal-oxide-semiconductor device 1 and increasing its on-state current. Alternatively, the same breakdown voltage can be maintained while reducing the size of the laterally diffused metal-oxide-semiconductor device 1 and improving its overall performance.

[0132] In the description of this specification, the references to terms such as "some embodiments," "other embodiments," "ideal embodiments," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example that are included in at least one embodiment or example of this application. In this specification, the illustrative descriptions of the above terms do not necessarily refer to the same embodiments or examples.

[0133] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features of the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0134] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.

Claims

1. A laterally diffused metal-oxide-semiconductor device, characterized in that, include: A substrate having trenches, the trenches including a first sidewall and a bottom wall connected to the first sidewall; A drift region is located within the substrate, wherein the trench is disposed around the drift region; A dielectric layer is located on the substrate and disposed around the drift region; wherein the dielectric layer covers at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall; A gate is disposed around the drift region, wherein the gate covers a portion of the dielectric layer and extends toward the bottom wall to cover a portion of the bottom wall; the gate includes a gate oxide layer and a polysilicon layer stacked thereon, the gate oxide layer being located on the side of the polysilicon layer closer to the dielectric layer.

2. The laterally diffused metal-oxide-semiconductor device according to claim 1, characterized in that, The trench is at least located on both sides of the drift region along a first direction; the first direction is perpendicular to the thickness direction of the substrate.

3. The laterally diffused metal-oxide-semiconductor device according to claim 2, characterized in that, The number of grooves is two, and the two grooves are located on both sides of the drift area along the first direction; At least a portion of the drift region is located within the substrate between the two first sidewalls of the two trenches.

4. The laterally diffused metal-oxide-semiconductor device according to any one of claims 1-3, characterized in that, The dielectric layer covers the entire first sidewall.

5. The laterally diffused metal-oxide-semiconductor device according to any one of claims 1-3, characterized in that, The laterally diffused metal-oxide-semiconductor device further includes: A body region is disposed within the substrate at the bottom of the trench; wherein the orthographic projection of the gate on the substrate overlaps with the body region. A source region is disposed within the body region; wherein the orthographic projection of the gate on the substrate is tangent to or overlaps with the source region, and there is a gap between the end of the source region near the drift region and the end of the body region near the drift region; The drain region is located within the substrate and on the side of the gate furthest from the source region; A buried layer is located within the substrate and on the side of the drift region away from the gate.

6. The laterally diffused metal-oxide-semiconductor device according to any one of claims 1-3, characterized in that, The dielectric layer includes a high-temperature oxide layer.

7. The laterally diffused metal-oxide-semiconductor device according to any one of claims 1-3, characterized in that, The thickness of the dielectric layer is greater than the thickness of the gate oxide layer.

8. The laterally diffused metal-oxide-semiconductor device according to any one of claims 1-3, characterized in that, The outer contour of the orthogonal projection of the dielectric layer onto the substrate is located within the outer contour of the drift region; And / or, the outer contour of the gate's orthogonal projection on the bottom wall is located outside the outer contour of the drift region.

9. A method for fabricating a laterally diffused metal-oxide-semiconductor device, characterized in that, include: Provide substrate; Trenches are formed on the substrate; The trench includes a first sidewall and a bottom wall that are interconnected; A dielectric layer is formed on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall; A drift region is formed within the substrate, wherein the trench and the dielectric layer are both disposed around the drift region; A gate is formed on the substrate, wherein the gate is disposed around the drift region; the gate covers a portion of the dielectric layer and extends toward the bottom wall to cover a portion of the bottom wall; the gate includes a gate oxide layer and a polysilicon layer stacked thereon, the gate oxide layer being located on the side of the polysilicon layer closer to the dielectric layer.

10. The method for fabricating a laterally diffused metal-oxide-semiconductor device according to claim 9, characterized in that, The step of forming a dielectric layer on the substrate to cover at least a portion of the first sidewall and a portion of the bottom wall connected to the first sidewall includes: A first oxide layer is formed on the substrate using a high-temperature oxide deposition technique; The first oxide layer is etched to form the dielectric layer; or, A mask layer is formed on the surface of the substrate, exposing at least a portion of the surface of the first sidewall and a portion of the surface of the bottom wall connected to the first sidewall; A first oxide layer is formed on the exposed surface of the substrate and on the surface of the mask layer; The mask layer and the first oxide layer located on the surface of the mask layer are removed to form the dielectric layer.

11. The method for fabricating a laterally diffused metal-oxide-semiconductor device according to claim 9 or 10, characterized in that, Prior to the step of forming trenches on the surface of the substrate, the method further includes: A buried layer is formed within the substrate.

12. The method for fabricating a laterally diffused metal-oxide-semiconductor device according to claim 9 or 10, characterized in that, The step of forming a gate on the substrate, wherein the gate is disposed around the drift region, includes: A second oxide layer is formed on the surface of the substrate; A polycrystalline silicon material layer is formed on the surface of the second oxide layer; The second oxide layer and the polysilicon material layer are etched to form the gate oxide layer and the polysilicon layer.

13. The method for fabricating a laterally diffused metal-oxide-semiconductor device according to claim 9 or 10, characterized in that, After the step of forming a gate on the substrate, wherein the gate is disposed around the drift region, the method further includes: A body region is formed within the substrate, wherein the body region is disposed within the substrate at the bottom of the trench, and the orthogonal projection of the gate on the substrate overlaps with the body region; A source region is formed within the substrate, wherein the source region is disposed within the body region, the orthogonal projection of the gate on the substrate is tangent to or overlaps with the source region, and there is a gap between the end of the source region near the drift region and the end of the body region near the drift region.

Citation Information

Patent Citations

  • High voltage device and manufacturing method thereof

    US20200119189A1