A novel method for preparing food-grade calcium acetate

Through the reaction of phosphogypsum with carbonization liquid and acetic acid, combined with pH adjustment and auxiliary material treatment, high-purity food-grade calcium acetate was successfully prepared, which solved the problem of insufficient utilization of phosphogypsum and achieved high-efficiency, low-cost and high-value utilization. .

CN117720411BActive Publication Date: 2024-10-18HUBEI THREE GORGES LAB
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311464111.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-06
Publication Date
2024-10-18
Estimated Expiration
2043-11-06

AI Technical Summary

Technical Problem

The utilization of phosphogypsum in the existing technology suffers from excessive regional distribution, unstable quality, and lack of key technologies. As a result, its comprehensive treatment and high-value utilization have not yet been realized, and the problem of processing large amounts of phosphogypsum has not been effectively solved.

Method used

Phosphogypsum is reacted with carbonization liquid to generate an insoluble solid, which is then reacted with acetic acid solution. After pH adjustment, addition of auxiliary materials, evaporation and crystallization, etc., high-purity food-grade calcium acetate powder is obtained to achieve high-value utilization of phosphogypsum.

Benefits of technology

This method realizes the preparation of food-grade calcium acetate with simple process, high product purity and low preparation cost. It has the characteristics of high efficiency, low energy consumption and green environmental protection, and provides a new direction for the reduction and high-value utilization of phosphogypsum.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117720411B_ABST
    Figure CN117720411B_ABST
Patent Text Reader

Abstract

The invention discloses a novel method for preparing food-grade calcium acetate, wherein phosphogypsum is added to a carbonizing liquid for carbonization reaction, and insoluble solid I and sulfate solution are separated after the reaction is completed; acidification reaction is performed, and solid residue I and calcium acetate mixed solution I are separated after the reaction is completed; the calcium acetate mixed solution I is adjusted to pH, and solid residue II and calcium acetate mixed solution II are separated; auxiliary materials are added to the calcium acetate mixed solution II for reaction, and solid residue III and calcium acetate mixed solution III are separated after the reaction is completed; the calcium acetate mixed solution III is evaporated and concentrated to obtain solid residue IV and refined calcium acetate solution; the refined calcium acetate solution is adjusted to pH, evaporated, crystallized, and dried to obtain food-grade calcium acetate powder. The invention uses phosphogypsum as a calcium source to synthesize calcium acetate, and after further separation and purification, food-grade calcium acetate powder with more economic value is obtained, further broadening the comprehensive application range of phosphogypsum.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of chemical preparation and relates to a method for separating, purifying and preparing food-grade calcium acetate. Background Art

[0002] Calcium acetate is commonly known as acetic acid stone, and its molecular formula is C 4 H 6 CaO 4 , relative molecular mass 158.17, white needle-shaped crystals, slight acetic acid smell, very hygroscopic. Calcium acetate is a strong electrolyte ionic compound, which can be ionized into Ca 2 + and CH 3 COO - . At 150°C, calcium acetate does not lose all its water content; when heated to 160°C, it decomposes into acetone and calcium carbonate. Calcium acetate is highly soluble in water and slightly soluble in alcohol at room temperature.

[0003] Calcium acetate is an ionic, highly efficient nutritional calcium supplement that can participate in bone formation and bone tissue reconstruction after fracture, as well as muscle contraction, nerve transmission, coagulation mechanism, and reduce capillary permeability. The aqueous solution of calcium acetate is neutral, and the acetate radical decomposed in the body is a component of human metabolism. There is no discomfort in the stomach and intestines after taking it. Calcium acetate can be used as a medicine, food additive, health food, etc. to prevent and treat gestational hypertension during pregnancy, promote fetal growth and development, sterilize, reduce inflammation, treat gastroenteritis, sterilize wounds, and relieve toothache. In addition, calcium acetate is used as a blood and peritoneal dialysis agent to remove toxic substances from the blood, and can be used as a drug for treating hyperphosphatemia to remove excess phosphorus in the blood.

[0004] The wet phosphoric acid process produces a large amount of solid residue phosphogypsum, the main component of which is calcium sulfate, with a content of more than 70%. Untreated phosphogypsum does not have gelling properties and contains harmful impurities such as phosphides, fluorides, and organic matter. It is difficult to use directly and is generally treated by open-air storage. As for the disposal and comprehensive utilization of phosphogypsum, the current utilization of phosphogypsum in China is still in the primary stage, with about 30% used to make cement retarders, 25% for external sales or supply, and only 14% for the production of gypsum boards. The utilization of phosphogypsum has problems such as overly concentrated regional distribution, far from the consumer market, unstable quality, and lack of key technologies. At present, there is no relatively complete utilization system for the comprehensive treatment of large amounts of phosphogypsum. Finding a resource utilization method with simple process and high value is the key to solving the phosphogypsum problem. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a method for preparing food-grade calcium acetate from phosphogypsum in view of the above-mentioned deficiencies in the prior art. The method prepares calcium acetate from phosphogypsum, and obtains food-grade calcium acetate through further separation and purification. The method has simple process, high product purity, low preparation cost, and can be mass-produced.

[0006] To this end, the present invention provides a novel method for preparing food-grade calcium acetate, which comprises:

[0007] Step A, dissolving a carbonizing agent in water to prepare a carbonizing liquid. Adding phosphogypsum into the carbonizing liquid for reaction, and separating after the reaction to obtain an insoluble solid I and a sulfate solution;

[0008] Step B, adding the insoluble solid I obtained in step A to an acetic acid solution for reaction, and separating after the reaction to obtain a solid residue I and a calcium acetate mixed solution I;

[0009] Step C, adjusting the pH of the calcium acetate mixed solution I obtained in step B, stirring at a constant temperature, and separating to obtain a solid residue II and a calcium acetate mixed solution II after the reaction is completed;

[0010] Step D, adding the calcium acetate mixed solution II obtained in step C to the auxiliary material for reaction, stirring at a constant temperature, and separating after the reaction to obtain solid residue III and calcium acetate mixed solution III;

[0011] Step E, evaporating and concentrating the calcium acetate mixed solution III obtained in step D, and separating to obtain a solid residue IV and a refined calcium acetate solution;

[0012] Step F, adjusting the pH of the refined calcium acetate solution obtained in step E, evaporating, crystallizing and drying to obtain food-grade calcium acetate powder.

[0013] In some embodiments of the present invention, in step A, the carbonized liquid has a concentration of 0.1 to 2 mol / L. The carbonized liquid components include one or more of carbonic acid, sodium carbonate, potassium carbonate, ammonium carbonate, sodium bicarbonate, potassium bicarbonate and ammonium bicarbonate.

[0014] In some embodiments of the present invention, in step A, the mass ratio of the phosphogypsum to the carbonizing agent is 1:0.4-1:1, preferably 1:0.5-1:8. The reaction temperature is 20-100°C, and the reaction time is 0.5-5 h.

[0015] In some embodiments of the present invention, in step B, the concentration of the acetic acid solution is 50 wt% to 99 wt%, and the mass ratio of the acetic acid solution to the phosphogypsum is 1:0.4-1:2.

[0016] In some embodiments of the present invention, in step C, the pH adjuster is one or more of calcium oxide, calcium hydroxide, sodium hydroxide, and potassium hydroxide.

[0017] In some embodiments of the present invention, in step C, the pH adjustment range is 9-14, the stirring temperature is 20-60° C., and the reaction time is 0.5-3 h.

[0018] In some embodiments of the present invention, in step D, the auxiliary material is one or more of barium hydroxide, calcium chloride, aluminum chloride, polyaluminum chloride, and calcium oxide.

[0019] In some embodiments of the present invention, in step D, the mass ratio of the auxiliary material to phosphogypsum is 1:0.01-1:0.5, the stirring temperature is 20-60° C., and the reaction time is 0.5-3 h.

[0020] In some embodiments of the present invention, in step E, the evaporation temperature is 50-150° C., and the ratio of the volume of the evaporated solution to the phosphogypsum is 5:1-10:1 ml / g.

[0021] In some embodiments of the present invention, in step F, the pH adjuster is acetic acid, and the pH adjustment range is 6-7.

[0022] In some embodiments of the present invention, in step F, the evaporation crystallization temperature is 50-150° C., the drying temperature is 60-120° C., and the drying time is 2-6 h.

[0023] In the present invention, the content of calcium acetate in the food-grade calcium acetate is ≥98 wt %.

[0024] Compared with the prior art, the present invention has the following advantages:

[0025] (1) Innovatively use phosphogypsum as a calcium source to construct a calcium acetate preparation route, and obtain high-value-added food-grade calcium acetate through reaction, separation and purification.

[0026] (2) A new process for comprehensive impurity removal, separation and purification of calcium acetate after phosphogypsum is transformed into calcium acetate is innovatively proposed. This process has a series of advantages such as high efficiency, simple operation, low energy consumption, green environmental protection, and easy industrialization, providing a new direction for the reduction of phosphogypsum and high-value utilization. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to make the present invention easy to understand, the present invention will be described in detail below with reference to the accompanying drawings.

[0028] Figure 1 The present invention is a process flow chart of preparing food-grade calcium acetate using phosphogypsum.

[0029] I. Terminology

[0030] The term "water" in the present invention, unless otherwise specified or limited, refers to deionized water, distilled water or ultrapure water. DETAILED DESCRIPTION

[0031] II. Implementation Plan

[0032] As mentioned above, phosphogypsum has many types of impurities and a large amount of accumulation. Low-cost reduction treatment and high-value utilization of phosphogypsum are the most critical factors in solving the problem of phosphogypsum storage and backlog. It is urgent to study low-cost harmless treatment and high-value utilization technology of phosphogypsum. In order to solve this problem, the inventors have conducted a lot of research on the high-value utilization technology of phosphogypsum. The present invention has studied and designed a new method for preparing food-grade calcium acetate, and its process flow chart is as follows: Figure 1 shown.

[0033] from Figure 1 It can be seen that the present invention relates to a method for synthesizing calcium acetate from phosphogypsum, separating and purifying the prepared food-grade calcium acetate, which comprises the following steps:

[0034] (1) Prepare a carbonizing liquid (one or more of carbonic acid, sodium carbonate, potassium carbonate, ammonium carbonate, sodium bicarbonate, potassium bicarbonate and ammonium bicarbonate) with a concentration of 0.1 to 2 mol / L, add the carbonizing liquid according to the mass ratio of phosphogypsum to carbonizing agent of 1:0.4 to 1:1, and perform carbonization reaction at 20 to 100°C for 0.5 to 5 h. After the reaction is completed, separate and obtain insoluble solid I and sulfate solution;

[0035] (2) adding an acetic acid solution having a concentration of 50 wt% to 99 wt% to the insoluble solid I obtained in step (1), wherein the amount of the acetic acid solution is 40% to 200% of the mass of the phosphogypsum; acidifying the reaction at 20 to 100° C. for 0.5 to 5 h, and separating after the reaction to obtain a solid residue I and a calcium acetate mixed solution I;

[0036] (3) Add a pH adjuster (one or more of calcium oxide, calcium hydroxide, sodium hydroxide, and potassium hydroxide) to the calcium acetate mixed solution I obtained in step (2), adjust the pH to 9-14, and react at 20-60° C. for 0.5-3 h. After the reaction, a solid residue II and a calcium acetate mixed solution II are obtained;

[0037] (4) Add auxiliary materials (one or more of barium hydroxide, calcium chloride, aluminum chloride, polyaluminum chloride, and calcium oxide) to the calcium acetate mixed solution II obtained in step (3), with the amount of auxiliary materials being 1% to 50% of the mass of the phosphogypsum, and reacting at 20 to 60° C. for 0.5 to 3 h. After the reaction is completed, solid residue III and calcium acetate mixed solution III are obtained;

[0038] (5) The calcium acetate mixed solution III obtained in step (4) is evaporated and concentrated at 50-150° C. until the volume ratio of the solution to phosphogypsum is 5:1-10:1 ml / g, and solid residue IV and refined calcium acetate solution are separated;

[0039] (6) The refined calcium acetate solution obtained in step (5) is added with acetic acid to adjust the pH to 6-7, and evaporated and crystallized at 50-150° C. The obtained crystals are dried at 60-120° C. for 0.5-5 h to obtain food grade calcium acetate powder.

[0040] The present invention provides a novel method for preparing food-grade calcium acetate. The method consists of a carbonization reaction, an acidification reaction, a separation and purification, and an evaporation and crystallization process. First, phosphogypsum and a carbonization liquid are subjected to a carbonization reaction to separate an insoluble solid I containing calcium carbonate; the insoluble solid I containing calcium carbonate is subjected to an acidification reaction with acetic acid to separate a mixed solution containing calcium acetate; the solution containing calcium acetate is separated and purified to remove impurities to obtain a refined calcium acetate solution; finally, the refined calcium acetate solution is evaporated, crystallized, and dried to obtain food-grade calcium acetate. Compared with the prior art, the present invention has the following advantages: phosphogypsum is innovatively used as a calcium source, and a new process for comprehensive impurity removal, separation and purification of calcium acetate after phosphogypsum is converted into calcium acetate is proposed. The process has a series of advantages such as high efficiency, simple operation, low energy consumption, green environmental protection, and easy industrialization, providing a new direction for the reduction treatment and high-value utilization of phosphogypsum.

[0041] II. Embodiment

[0042] In order to make the present invention easier to understand, the present invention will be further described in detail below in conjunction with examples, which are merely illustrative and are not intended to limit the scope of application of the present invention. The raw materials or components used in the present invention can be purchased from commercial sources or prepared by conventional methods unless otherwise specified.

[0043] Example 1

[0044] (1) A potassium carbonate solution with a concentration of 0.5 mol / L was prepared, and 50% of the potassium carbonate by mass of the phosphogypsum was added to the potassium carbonate solution, and the carbonization reaction was carried out at 20°C for 3 h. After the reaction was completed, an insoluble solid I containing calcium carbonate and a sulfate solution were separated;

[0045] (2) adding an acetic acid solution with a concentration of 50 wt% to the insoluble solid I obtained in step (1), wherein the amount of the acetic acid solution is 200% of the mass of the phosphogypsum, and performing an acidification reaction at 20° C. for 3 h. After the reaction is completed, a solid residue I and a calcium acetate mixed solution I are separated;

[0046] (3) Calcium hydroxide is added to the calcium acetate mixed solution I obtained in step (2), the pH is adjusted to 14, and the mixture is reacted at 20° C. for 2 h. After the reaction is completed, a solid residue II and a calcium acetate mixed solution II are obtained;

[0047] (4) Add a mixture of barium hydroxide and calcium oxide to the calcium acetate mixed solution II obtained in step (3), with the total amount of the mixture being 10% of the mass of the phosphogypsum, and react at 20° C. for 2 h. After the reaction is completed, solid residue III and calcium acetate mixed solution III are obtained;

[0048] (5) The calcium acetate mixed solution III obtained in step (4) is evaporated and concentrated at 100° C. until the volume ratio of the solution to the phosphogypsum is 5:1 ml / g, and solid residue IV and a refined calcium acetate solution are obtained by separation;

[0049] (6) The refined calcium acetate solution obtained in step (5) was added with acetic acid to adjust the pH to 7, and evaporated and crystallized at 100° C. The obtained crystals were dried at 100° C. for 4 h to obtain white loose food-grade calcium acetate powder. The calcium acetate content was tested to be 99.26%, and the sulfate, chloride, fluoride, lead, arsenic and moisture contents all met the national standard GB1903.15-2016.

[0050] Example 2

[0051] (1) preparing a sodium bicarbonate solution with a concentration of 1 mol / L, adding 60% of the mass of sodium bicarbonate to the sodium bicarbonate solution according to the phosphogypsum, and carbonizing the solution at 70°C for 0.5 h. After the reaction is completed, an insoluble solid I containing calcium carbonate and a sulfate solution are separated;

[0052] (2) adding an acetic acid solution having a concentration of 90 wt% to the insoluble solid I obtained in step (1), wherein the amount of the acid solution is 100% of the mass of the phosphogypsum, and performing an acidification reaction at 70° C. for 0.5 h. After the reaction is completed, a solid residue I and a calcium acetate mixed solution I are separated;

[0053] (3) Calcium oxide is added to the calcium acetate mixed solution I obtained in step (2), the pH is adjusted to 13, and the mixture is reacted at 40° C. for 1 h. After the reaction is completed, a solid residue II and a calcium acetate mixed solution II are obtained;

[0054] (4) Add a mixture of barium chloride and aluminum oxide to the calcium acetate mixed solution II obtained in step (3), with the total amount of the mixture being 5% of the mass of the phosphogypsum, and react at 40° C. for 1 h. After the reaction is completed, solid residue III and calcium acetate mixed solution III are obtained;

[0055] (5) The calcium acetate mixed solution III obtained in step (4) is evaporated and concentrated at 100° C. until the volume ratio of the solution to the phosphogypsum is 5:1 ml / g, and solid residue IV and a refined calcium acetate solution are obtained by separation;

[0056] (6) The refined calcium acetate solution obtained in step (5) was added with acetic acid to adjust the pH to 7, and evaporated and crystallized at 100°C. The obtained crystals were dried at 110°C for 3 h to obtain white loose food-grade calcium acetate powder. The calcium acetate content was 99.85% after testing, and the sulfate, chloride, fluoride, lead, arsenic and moisture contents all met the national standard GB1903.15-2016.

[0057] Example 3

[0058] (1) preparing an ammonium carbonate solution with a concentration of 2 mol / L, adding ammonium carbonate in an amount of 50% of the mass of the phosphogypsum to the ammonium carbonate solution, and carbonizing the solution at 40°C for 1 h. After the reaction, an insoluble solid I containing calcium carbonate and a sulfate solution are separated;

[0059] (2) adding an acetic acid solution having a concentration of 99 wt% to the insoluble solid I obtained in step (1), wherein the amount of the acetic acid solution is 70% of the mass of the phosphogypsum, and performing an acidification reaction at 40° C. for 1 h. After the reaction is completed, a solid residue I and a calcium acetate mixed solution I are separated;

[0060] (3) Sodium hydroxide is added to the calcium acetate mixed solution I obtained in step (2), the pH is adjusted to 12, and the mixture is reacted at 50° C. for 0.5 h. After the reaction is completed, a solid residue II and a calcium acetate mixed solution II are obtained;

[0061] (4) Adding the calcium acetate mixed solution II obtained in step (3) to a mixture of polyaluminium chloride and calcium oxide, the total amount of the mixture being 30% of the mass of the phosphogypsum, and reacting at 50°C for 0.5 h, and obtaining solid residue III and calcium acetate mixed solution III after the reaction;

[0062] (5) The calcium acetate mixed solution III obtained in step (4) is evaporated and concentrated at 90° C. until the volume ratio of the solution to the phosphogypsum is 6:1 ml / g, and solid residue IV and a refined calcium acetate solution are obtained by separation;

[0063] (6) The refined calcium acetate solution obtained in step (5) was added with acetic acid to adjust the pH to 6, and evaporated and crystallized at 90°C. The obtained crystals were dried at 90°C for 5 h to obtain white loose food-grade calcium acetate powder. The calcium acetate content was 99.96% after testing, and the sulfate, chloride, fluoride, lead, arsenic and moisture contents all met the national standard GB1903.15-2016.

[0064] It should be noted that the embodiments described above are only used to explain the present invention and do not constitute any limitation to the present invention. The present invention has been described with reference to typical embodiments, but it should be understood that the words used therein are descriptive and explanatory words, rather than restrictive words. The present invention may be modified as specified within the scope of the claims of the present invention, and the present invention may be revised without departing from the scope and spirit of the present invention. Although the present invention described therein relates to specific methods, materials and embodiments, it does not mean that the present invention is limited to the specific examples disclosed therein, on the contrary, the present invention can be extended to all other methods and applications with the same functions.

Claims

1. A method for preparing food grade calcium acetate, It is characterized in that The steps include: Step A, dissolving a carbonizing agent in water to prepare a carbonizing liquid, adding phosphogypsum to the carbonizing liquid for reaction, and separating after the reaction to obtain an insoluble solid I and a sulfate solution, wherein the carbonizing liquid component includes one or more of carbonic acid, sodium carbonate, potassium carbonate, ammonium carbonate, sodium bicarbonate, potassium bicarbonate and ammonium bicarbonate; Step B, adding the insoluble solid I obtained in step A to an acetic acid solution for reaction, and separating after the reaction to obtain a solid residue I and a calcium acetate mixed solution I; Step C, adjusting the pH of the calcium acetate mixed solution I obtained in step B to a range of 9 to 14, stirring at a constant temperature, and separating to obtain a solid residue II and a calcium acetate mixed solution II after the reaction is completed; Step D, adding the calcium acetate mixed solution II obtained in step C to an auxiliary material for reaction, stirring at a constant temperature, and separating after the reaction to obtain a solid residue III and a calcium acetate mixed solution III, wherein the auxiliary material is one or more of barium hydroxide, calcium chloride, aluminum chloride, polyaluminum chloride, and calcium oxide; Step E, evaporating and concentrating the calcium acetate mixed solution III obtained in step D, and separating to obtain a solid residue IV and a refined calcium acetate solution; Step F, adjusting the pH of the refined calcium acetate solution obtained in step E to a pH range of 6 to 7, evaporating, crystallizing, and drying to obtain food-grade calcium acetate powder.

2. The method according to claim 1, It is characterized in that In step A, the concentration of the carbonized liquid is 0.1-2 mol / L; and / or the mass ratio of the phosphogypsum to the carbonizing agent is 1:0.4-1:1; and / or the reaction temperature is 20-100° C., and the reaction time is 0.5-5 h.

3. The method according to claim 1, It is characterized in that In step B, the concentration of the acetic acid solution is 50wt% to 99wt%; and / or the mass ratio of the acetic acid solution to phosphogypsum is 1:0.4 to 1:2; and / or the reaction temperature is 20 to 100°C, and the reaction time is 0.5 to 5 h.

4. The method according to claim 1, It is characterized in that In step C, the pH regulator is one or more of calcium oxide, calcium hydroxide, sodium hydroxide, and potassium hydroxide; and / or the stirring temperature is 20 to 60° C., and the reaction time is 0.5 to 3 hours.

5. The method according to claim 1, It is characterized in that In step D, the mass ratio of the auxiliary material to phosphogypsum is 1:0.01-1:0.5; and / or the stirring temperature is 20-60° C., and the reaction time is 0.5-3 h.

6. The method according to claim 1, It is characterized in that In step E, the evaporation temperature is 50-150° C.; and / or the volume ratio of the evaporated solution to phosphogypsum is 5:1-10:1 ml / g.

7. The method according to claim 1, It is characterized in that In step F, the pH regulator is acetic acid; the evaporation crystallization temperature is 50-150° C.; and / or the drying temperature is 60-120° C., and the drying time is 2-6 h.

Citation Information

Patent Citations

  • Resource recycling method of industrial phosphogypsum waste residues

    CN104211099A

  • Production process for food-grade calcium acetate

    CN106588634A