Coreless substrate and processing method thereof, circuit board and electronic device
Through specific processing methods of coreless substrates, including stacking and hot pressing curing treatment, combined with the use of insulating filler glue and fiber cloth, the warping problem of coreless substrates is solved, the flatness and structural strength are improved, and the performance of electronic devices is enhanced .
Patent Information
- Application Number
- CN202310630312.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-30
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-05-30
AI Technical Summary
Coreless substrates are prone to warping problems during processing, resulting in poor flatness and affecting the performance and reliability of electronic devices.
A coreless substrate processing method is adopted, by stacking the first carrier board composite structure and the second carrier board composite structure, and performing hot pressing and curing treatment, peeling off the temporary carrier board and release layer, peeling off both sides to release stress, and combining The insulating filling glue fills the circuit gaps in the central circuit layer, improves circuit density and structural strength, and prevents the fiber cloth from contacting and extruding the central circuit layer.
It effectively avoids the warping problem of the coreless substrate, improves the flatness and structural strength, and enhances the performance and reliability of electronic equipment.
Smart Images

Figure CN117729694B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of circuit board processing and manufacturing, and in particular to a coreless substrate and a processing method thereof, a circuit board and an electronic device. Background Art
[0002] At present, 3C electronic devices such as smart watches, mobile phones, and laptops are becoming one of the necessities of modern people's lives. In order to realize the relevant functions of electronic devices, circuit boards are usually arranged inside the electronic devices.
[0003] In the related art, the circuit board adopts a coreless substrate. However, the coreless substrate has a warping problem and poor flatness. Summary of the invention
[0004] The present application provides a coreless substrate and a processing method thereof, a circuit board and an electronic device, which are helpful in solving the warping problem of the coreless substrate.
[0005] In order to achieve the above purpose, this application adopts the following technical solutions:
[0006] In a first aspect, the present application provides a processing method for a coreless substrate, comprising the following steps: providing a first carrier composite structure and a second carrier composite structure respectively; wherein the first carrier composite structure comprises a first temporary carrier, a first release layer and a first composite layer structure stacked in sequence, the first composite layer structure comprises a first semi-cured sheet and a first metal circuit layer, the first semi-cured sheet has a first surface facing away from the first temporary carrier, and the first metal circuit layer is arranged on the first surface, the second carrier composite structure comprises a second temporary carrier, a second release layer and a second composite layer structure stacked in sequence, the second composite layer structure comprises a second semi-cured sheet, and the second semi-cured sheet has a second surface facing away from the second temporary carrier; the second surface is facing the first surface, and the first carrier composite structure and the second carrier composite structure are stacked; hot pressing and curing the stacked first carrier composite structure and the second carrier composite structure; peeling off and removing the first temporary carrier and the first release layer, as well as the second temporary carrier and the second release layer.
[0007] In the processing method of the coreless substrate of the embodiment of the present application, when stacking the first carrier composite structure and the second carrier composite structure, the first surface of the first semi-cured sheet facing away from the first temporary carrier is stacked toward the second surface of the second semi-cured sheet facing away from the second temporary carrier to obtain the first stacking structure. In this way, the first metal circuit layer is located between the first semi-cured sheet and the second semi-cured sheet, and the first temporary carrier and the second temporary carrier are located at both ends of the thickness direction of the entire first stacking structure. On this basis, after the first stacking structure is subjected to hot pressing curing treatment, in the obtained second stacking structure, the first temporary carrier and the second temporary carrier are still located at both ends of the thickness direction of the second stacking structure. In this way, before peeling off and removing the first temporary carrier and the first release layer, as well as the second temporary carrier and the second release layer, the stress on both sides of the second stacking structure in its own thickness direction is relatively symmetrical. After peeling off the first temporary carrier and the first release layer, as well as the second temporary carrier and the second release layer, since the temporary carrier is peeled off on both sides, compared with the single-sided peeling of the temporary carrier in the related art, on the one hand, the residual stress of the coreless substrate during the pressing process and circuit manufacturing process can be released on both sides, and after the stress is released, the stresses at both ends of the thickness direction of the third stacking structure in its own thickness direction are relatively symmetrical, so that the stress inside the coreless substrate is relatively balanced, which is beneficial to avoid the warping problem of the coreless substrate at least to a certain extent and improve the flatness of the coreless substrate.
[0008] In a possible implementation of the present application, the second composite layer structure also includes a second metal circuit layer, which is arranged on the second surface; in the step of facing the second surface toward the first surface and stacking the first carrier composite structure and the second carrier composite structure, the second wiring of the second metal circuit layer is spaced apart from the first wiring of the first metal circuit layer in a direction perpendicular to the second surface, and at least a portion of the second wiring of the second metal circuit layer is located within the first wiring gap of the first metal circuit layer; wherein the first metal circuit layer and the second metal circuit layer as a whole form a central circuit layer between the first semi-cured sheet and the second semi-cured sheet. Therefore, by making the first metal circuit layer of the central circuit layer on the first semi-cured sheet, and making the second metal circuit layer of the central circuit layer on the second semi-cured sheet, the line spacing of the entire central circuit layer is not limited by the circuit manufacturing process and can be adjusted according to actual needs, so that without changing the line spacing of the circuit manufacturing that can be achieved by the current circuit manufacturing process, when stacking the first carrier composite structure and the second carrier composite structure, the second routing of the second metal circuit layer is spaced apart from the first routing of the first metal circuit layer in a direction perpendicular to the second surface 232a, and at least a portion of the second routing of the second metal circuit layer is located in the first circuit gap of the first metal circuit layer 133, which is beneficial to reduce the line spacing of the central circuit layer, improve the line density of the central circuit layer, and realize the high density of the central circuit layer.
[0009] On this basis, in order to further improve the high density of the central circuit layer, while the second surface is facing the first surface and the first carrier composite structure and the second carrier composite structure are stacked, the second routing of the second metal circuit layer is spaced apart from the first routing of the first metal circuit layer in a direction perpendicular to the second surface, and at least a portion of the second routing of the second metal circuit layer is located in the first routing gap of the first metal circuit layer, and at least a portion of the first routing of the first metal circuit layer is located in the second routing gap.
[0010] Specifically, a plurality of first wirings are arranged in a row. A plurality of second wirings are arranged in a row. A first sub-circuit gap is formed between two adjacent first wirings. When the second surface is directed toward the first surface and the first carrier composite structure and the second carrier composite structure are stacked, the second wirings of the second metal wiring layer are spaced apart from the first wirings of the first metal wiring layer in a direction perpendicular to the second surface, and a second wiring is accommodated between two adjacent first wirings, and a first wiring is accommodated between two adjacent second wirings. Thus, in the first stacking structure, the first wirings and the second wirings are alternately arranged. This is conducive to further improving the high density of the central wiring layer.
[0011] In a possible implementation of the present application, in order to improve the reliability of coreless substrate processing, before stacking the first carrier composite structure and the second carrier composite structure, the first metal circuit layer on the first carrier composite structure and the first metal circuit layer on the second carrier composite structure may be inspected for quality defects. For example, automatic optical inspection equipment is used for inspection. This prevents the first carrier composite structure from having a defective first metal circuit layer and the second carrier composite structure from having a defective second metal circuit layer, and prevents the second carrier composite structure from being used in the coreless substrate, which is beneficial to improving the yield of the coreless substrate.
[0012] In a possible implementation of the present application, in order to improve the reliability of coreless substrate processing, before stacking the first carrier composite structure and the second carrier composite structure, the first metal circuit layer on the first carrier composite structure may be subjected to surface browning treatment, and the second metal circuit layer on the second carrier composite structure may be subjected to surface browning treatment. In this way, the surface of the first metal circuit layer and the second metal circuit layer may be roughened, the bonding area between the metal circuit layer and other structures may be increased, and their surface bonding force may be increased.
[0013] In a possible implementation of the present application, in the step of facing the second surface toward the first surface and stacking the first carrier composite structure and the second carrier composite structure, at least a portion of the first routing line of the first metal circuit layer is located in the second circuit gap of the second metal circuit layer.
[0014] In a possible implementation of the present application, before the step of placing the second surface toward the first metal circuit layer and stacking the first carrier composite structure and the second carrier composite structure, the method further includes: disposing a liquid or semi-cured insulating filling glue on the first surface and / or on the second surface;
[0015] In the step of performing a heat-pressing curing process on the stacked first carrier composite structure and the second carrier composite structure, the insulating filling glue fills the circuit gaps of the central circuit layer and is cured into a filling glue portion.
[0016] In a possible implementation of the present application, the first metal circuit layer forms a central circuit layer between the first prepreg and the second prepreg; before the step of facing the second surface toward the first surface and stacking the first carrier composite structure and the second carrier composite structure, the method further includes: arranging a liquid or semi-cured insulating filling glue on the first surface and / or on the second surface; in the step of hot pressing and curing the stacked first carrier composite structure and the second carrier composite structure, the insulating filling glue fills the first circuit gap of the first metal circuit layer and solidifies into a filling glue portion. In this way, the first adhesive layer and the second adhesive layer can be prevented from being embedded in the circuit gap of the central circuit layer, thereby avoiding contact between the central circuit layer and the fiber cloth, and further preventing the problem of cracks caused by contact and extrusion between the fiber cloth and the central circuit layer due to excessive pressure, excessive temperature, and / or low content of the adhesive layer in the first and second prepregs to a certain extent. Furthermore, since the insulating filling glue fills the line gaps of the central circuit layer, the distance between the central circuit layer and the second fiber cloth and the distance between the central circuit layer and the first fiber cloth can be close to being equal, which can help improve the symmetry of the second stacking structure with the central circuit layer as the center, and further help the entire coreless substrate to be symmetrically arranged with the central circuit layer as the center, and then can reduce or eliminate the difference in thermal expansion coefficients of the parts on both sides of the thickness direction of the central circuit layer, further avoid the warping and deformation problem of the coreless substrate, and improve the flatness of the coreless substrate.
[0017] In a possible implementation of the present application, the first prepreg includes a first adhesive layer and a first fiber cloth, the first adhesive layer is in a semi-cured state, and the first fiber cloth is embedded in the first adhesive layer. Therefore, by using the first prepreg including the first fiber cloth as a processing material for the coreless substrate, it is helpful to ensure the structural strength of the coreless substrate.
[0018] In a possible implementation of the present application, the first adhesive layer includes a first resin matrix and a first filler distributed in the first resin matrix; the first filler can play a role in heat conduction, enhancing the structural strength of the first resin matrix and reducing the thermal expansion coefficient of the first resin matrix. The insulating filling glue includes a third resin matrix and a third filler distributed in the third resin matrix; the third filler can play a role in heat conduction, enhancing the structural strength of the third resin matrix and reducing the thermal expansion coefficient of the third resin matrix. In order to further improve the thermal conductivity and structural strength of the insulating filling glue and further reduce the thermal expansion coefficient of the insulating filling glue, the mass percentage of the third filler in the insulating filling glue is greater than the mass percentage of the first filler in the first adhesive layer. And / or, in order to improve the compatibility of the resin matrix and the third resin matrix in the first semi-cured sheet and the second semi-cured sheet, thereby improving their connection strength. The material of the third resin matrix is the same as that of the first resin matrix. For example, the material of the third resin matrix and the material of the first resin matrix are both epoxy resin and bismaleimide.
[0019] In order to improve the connection reliability of the insulating filling glue to the first prepreg and the second prepreg, and the compatibility of the insulating filling glue with the first resin matrix, in a possible implementation, the third filler can be in a granular form. In this way, compared with the third filler in a sheet or line form, the granular third filler is easier to be evenly distributed in the insulating filling glue, so that the composition uniformity of the insulating filling glue is better, and the connection reliability of the insulating filling glue to the first prepreg and the second prepreg is improved.
[0020] In a possible implementation of the present application, the insulating filling glue includes a third resin matrix and a third filler distributed in the third resin matrix. The third filler can play the role of heat conduction, enhancing the structural strength of the third resin matrix and reducing the thermal expansion coefficient of the third resin matrix. This is conducive to improving the structural strength and heat dissipation performance of the coreless substrate.
[0021] In a possible implementation of the present application, the first prepreg includes a first adhesive layer and a first fiber cloth, the first adhesive layer is in a semi-cured state, the first fiber cloth is embedded in the first adhesive layer, the first adhesive layer includes a first resin matrix, and the material of the first resin matrix includes epoxy resin and / or bismaleimide. Therefore, epoxy resin and / or bismaleimide are cheap, which can reduce manufacturing costs.
[0022] In a possible implementation of the present application, the first prepreg and the second prepreg are made of the same material and have the same thickness. In this way, the distance between the central circuit layer and the second fiber cloth and the distance between the central circuit layer and the first fiber cloth can be equal, which can help improve the symmetry of the second stacking structure with the central circuit layer as the center, and further help the entire coreless substrate to be symmetrically arranged with the central circuit layer as the center, and then reduce or eliminate the difference in thermal expansion coefficients of the parts on both sides of the thickness direction of the central circuit layer, further avoid the warping deformation problem of the coreless substrate, and improve the flatness of the coreless substrate.
[0023] In a possible implementation of the present application, the first carrier composite structure also includes a first metal layer, and the first metal layer is stacked between the first semi-cured sheet and the first release layer; the processing method of the coreless substrate includes a processing method of the first carrier composite structure, and the processing method of the first carrier composite structure includes: providing a first carrier structure and a first semi-cured sheet structure; wherein the first carrier structure includes a first temporary carrier, a first release layer and a first metal layer stacked in sequence; the first semi-cured sheet structure includes a first semi-cured sheet and a third metal layer stacked, and the third metal layer is arranged on the first surface; the surface of the first semi-cured sheet opposite to the first surface is facing the first metal layer, and the first semi-cured sheet structure and the first carrier structure are stacked; the first semi-cured sheet structure and the first carrier structure are pressed together; and the third metal layer is patterned to form a first metal circuit layer.
[0024] In a possible implementation of the present application, patterning the third metal layer to form a first metal circuit layer specifically includes: forming a first photoresist layer on a surface of the third metal layer away from the first semi-solid; exposing and developing the first photoresist layer to form a first photoresist pattern layer, the first photoresist pattern layer having a first window, and the third metal layer including a first portion exposed at the first window and a second portion covered by the first photoresist pattern layer; etching away the first portion to obtain a first metal circuit layer formed by the second portion; and stripping off the first photoresist pattern layer.
[0025] In a possible implementation of the present application, patterning the third metal layer to form a first metal circuit layer specifically includes: forming a first photoresist layer on the surface of the third metal layer away from the first semi-solid; exposing and developing the first photoresist layer to form a first photoresist pattern layer, the first photoresist pattern layer having a first window, and the third metal layer including a first portion exposed at the first window and a second portion covered by the first photoresist pattern layer; electroplating at the first window to form a first target coating; stripping off the first photoresist pattern layer to expose the second portion; etching away the second portion to obtain a first metal circuit layer formed by the first portion and the first target coating.
[0026] In a possible implementation of the present application, a processing method for a coreless substrate includes a processing method for a first carrier structure; the processing method for the first carrier structure includes: arranging a first release layer and a first metal seed layer on a first temporary carrier; wherein the first metal seed layer is arranged on a surface of the first release layer away from the first temporary carrier; forming a second photoresist layer on a surface of the first metal seed layer away from the first temporary carrier; exposing and developing the second photoresist layer to form a second photoresist pattern layer, the second photoresist pattern layer having a second window, the first metal seed layer including a first seed portion exposed at the second window and a second seed portion covered by the second photoresist pattern layer; electroplating at the second window to form a second target coating covering the first seed portion; stripping off the second photoresist pattern layer to expose the second seed portion to obtain a first metal layer formed by the second target coating and the first metal seed layer; after the steps of stripping off and removing the first temporary carrier and the first release layer, as well as the second temporary carrier and the second release layer, the method also includes: etching away the entire first metal seed layer to obtain a first circuit layer formed by the second target coating.
[0027] In this way, by first making the second target coating on the first temporary carrier, when the first carrier structure is pressed with the first semi-cured sheet structure, it is beneficial for the second target coating to be embedded in the first semi-cured sheet, and the second target coating is made on the second temporary carrier, so that after etching away the first metal seed layer, the exposed first circuit layer is embedded in the first dielectric structure, which is beneficial to reduce the thickness of the coreless substrate and achieve further thinning of the coreless substrate.
[0028] On this basis, the processing method of the second carrier structure is the same as the processing method of the first carrier structure, thereby being helpful to reduce the thickness of the coreless substrate and further thinning the coreless substrate.
[0029] In a possible implementation of the present application, after the step of stripping off the first temporary carrier and the first release layer, and the second temporary carrier and the second release layer, and before the step of etching away the entire first metal seed layer to obtain a first circuit layer formed by the second target plating layer, the processing method of the coreless substrate also includes: drilling the first metal layer and the first dielectric structure to form a first through hole; wherein the first through hole penetrates the first metal layer and the first dielectric structure; the first dielectric structure is formed by hot pressing and curing the first semi-cured sheet, and a first metal conductive portion is formed in the first through hole, and the first metal conductive portion is respectively connected to the first metal layer and the central circuit layer; wherein the central circuit layer includes the first metal circuit layer.
[0030] In a second aspect, the present application provides a coreless substrate, which is processed by using the processing method of the coreless substrate in any of the above technical solutions.
[0031] In a third aspect, the present application provides a coreless substrate, comprising: a first fiber cloth, a second fiber cloth and an intermediate layer structure. The first fiber cloth and the second fiber cloth are stacked, the intermediate layer structure is arranged between the first fiber cloth and the second fiber cloth, the intermediate layer structure comprises an adhesive layer and a central circuit layer, the adhesive layer comprises a first adhesive layer, a filling adhesive portion and a second adhesive layer stacked in sequence, the first adhesive layer is bonded to the first fiber cloth, the second adhesive layer is bonded to the second fiber cloth, the central circuit layer and the filling adhesive portion are integrally fixed and connected between the first adhesive layer and the second adhesive layer, and the central circuit layer is embedded in the filling adhesive portion.
[0032] In the coreless substrate of the embodiment of the present application, the line gap of the central circuit layer is filled by the additional filling glue part. Compared with the method of not setting the filling glue part but using the first glue layer and / or the second glue layer to fill the line gap of the central circuit layer, this method is helpful to avoid the problem that the size between the central circuit layer and the first fiber cloth and / or the size between the central circuit layer and the second fiber cloth is too small due to the first glue layer and / or the second glue layer filling the line gap of the central circuit layer, or even causing the fiber cloth and the central circuit layer to be in direct contact, and in the processing of the coreless substrate, the fiber cloth and the central circuit layer are contacted and squeezed due to hot pressing and curing, resulting in cracks, which is helpful to ensure the yield of the coreless substrate. On the other hand, it is helpful to make the distance between the central circuit layer and the second fiber cloth and the distance between the central circuit layer and the first fiber cloth equal, so as to improve the symmetry of the coreless substrate with the central circuit layer as the center, and then it is helpful to reduce or eliminate the difference in the thermal expansion coefficient of the parts on both sides of the thickness direction of the central circuit layer, avoid the warping deformation problem of the coreless substrate, and improve the flatness of the coreless substrate.
[0033] In a possible implementation manner of the third aspect, a distance between the central wiring layer and the second fiber cloth is equal to a distance between the central wiring layer and the first fiber cloth.
[0034] In a possible implementation of the third aspect, the first adhesive layer includes a first resin substrate and a first filler distributed in the first resin substrate; the filling adhesive portion includes a third resin substrate and a third filler distributed in the third resin substrate; wherein the mass percentage of the third filler in the filling adhesive portion is greater than the mass percentage of the first filler in the first adhesive layer; and / or the material of the third resin substrate is the same as that of the first resin substrate.
[0035] In a possible implementation of the third aspect, the central circuit layer includes a first metal circuit layer and a second metal circuit layer, the first metal circuit layer includes a plurality of first routing lines, the plurality of first routing lines are spaced apart to form a first circuit gap of the first metal circuit layer, the second metal circuit layer includes a plurality of second routing lines, the plurality of second routing lines are spaced apart to form a second circuit gap of the second metal circuit layer, at least a portion of the second routing lines is located within the first circuit gap and is spaced apart from the first routing lines; wherein, in a direction from the first fiber cloth to the second fiber cloth, a cross-sectional area of the first routing lines gradually decreases, and a cross-sectional area of the second routing lines gradually increases.
[0036] In a fourth aspect, the present application provides a circuit board, comprising: a coreless substrate and an electronic device in any of the above technical solutions, wherein the electronic device is fixed on the coreless substrate.
[0037] In a possible implementation manner of the fourth aspect, the circuit board is a main circuit board and / or a sub-circuit board of the electronic device.
[0038] In a fifth aspect, the present application provides an electronic device, which includes: a housing and the above-mentioned circuit board, and the circuit board is arranged in the housing.
[0039] It can be understood that the technical effects brought about by any design method in the second aspect, the fourth aspect and the fifth aspect provided above can refer to the technical effects brought about by different design methods in the first aspect, and will not be repeated here. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 A schematic diagram of a processing process of a coreless substrate in the related art;
[0041] Figure 2 It is a schematic diagram for analyzing the warping of a plate caused by different thermal expansion coefficients at both ends of the plate in the thickness direction when heated or cooled;
[0042] Figure 3 A flow chart of processing a coreless substrate provided for a first embodiment of the present application;
[0043] Figure 4 Based on Figure 3 Schematic diagram of the relative position relationship between the vertical projection of the first metal circuit layer in the first carrier composite structure on the first prepreg and the first prepreg;
[0044] Figure 5 For processing provided in the embodiment of the present application Figure 3 A schematic diagram of the processing process of the first carrier composite structure required in the process;
[0045] Figure 6 For processing provided in the embodiment of the present application Figure 5A schematic diagram of a specific processing process of the first carrier composite structure;
[0046] Figure 7 For processing provided in the embodiment of the present application Figure 3 A schematic diagram of the processing process of the second carrier composite structure required in the process;
[0047] Figure 8 The application provided in Figure 3 Schematic diagram of further processing of the coreless substrate after the processing flow shown;
[0048] Fig. 9 A schematic diagram of the processing process of a coreless substrate provided in the second embodiment of the present application;
[0049] Fig.10 Based on Figure 3-Figure 9 A cross-sectional view of the first carrier composite structure shown in ;
[0050] Fig.11 A schematic diagram of the processing process of the second carrier composite structure of the coreless substrate provided in the third embodiment of the present application;
[0051] Fig.12 Based on Fig.11 A schematic diagram showing the relative position relationship between the vertical projection of the second metal circuit layer in the second carrier composite structure on the second prepreg and the second prepreg;
[0052] Fig.13 To adopt Fig.11 Schematic diagram of the processing process of the coreless substrate of the second carrier composite structure shown in ;
[0053] Fig.14 Based on Fig.13 A schematic diagram of the relative position relationship of the vertical projections of the first metal circuit layer and the second metal circuit layer on the second prepreg in the first stacking structure shown;
[0054] Fig.15 A schematic diagram of the processing process of the first carrier structure of the coreless substrate provided in the fourth embodiment of the present application;
[0055] Fig.16 A schematic diagram of the processing process of the second carrier structure of the coreless substrate provided in the fourth embodiment of the present application;
[0056] Fig.17 To adopt Fig.15 A schematic diagram of a processing process of a coreless substrate of a first carrier structure and a first carrier composite structure shown;
[0057] Fig.18A schematic diagram of the cross-sectional structure of the second carrier composite structure obtained by processing the second metal circuit layer by the MSAP process;
[0058] Fig.19 To adopt Fig.17 The first carrier composite structure shown and the Fig.18 A schematic diagram of the processing process of the coreless substrate of the second carrier composite structure shown;
[0059] Fig. 20 A schematic diagram of a processing process of a coreless substrate provided in a fifth embodiment of the present application;
[0060] Fig.21 To adopt Fig. 9 A schematic cross-sectional structure diagram of a coreless substrate processed by the processing method of the coreless substrate shown;
[0061] Fig. 22 Based on Fig.13 A cross-sectional view of a coreless substrate processed by the processing method of the coreless substrate shown;
[0062] Fig.23 A perspective view of an electronic device provided for some embodiments of the present application;
[0063] Fig.24 for Fig.23 An exploded schematic diagram of the electronic device shown. DETAILED DESCRIPTION
[0064] In the embodiments of the present application, the terms "exemplarily" or "for example" are used to indicate examples, illustrations or descriptions. Any embodiment or design described as "exemplarily" or "for example" in the embodiments of the present application should not be interpreted as being more preferred or more advantageous than other embodiments or designs. Specifically, the use of words such as "exemplarily" or "for example" is intended to present related concepts in a specific way.
[0065] In the description of the embodiments of the present application, the term "and / or" refers to and covers any and all possible combinations of one or more of the associated listed items. The term "and / or" is a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in the present application generally indicates that the associated objects before and after are in an "or" relationship.
[0066] In the description of the embodiments of the present application, unless otherwise clearly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, "connection" can be a detachable connection or a non-detachable connection; it can be a direct connection or an indirect connection through an intermediate medium.
[0067] In the description of the embodiments of the present application, the terms "comprise", "include" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the statement "comprises a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element. In the absence of further restrictions, an element defined by the statement "comprises a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element.
[0068] As used herein, "parallel", "perpendicular", and "equal" include the situations described and situations similar to the situations described, and the range of the similar situations is within the acceptable deviation range, wherein the acceptable deviation range is determined by a person of ordinary skill in the art taking into account the measurement in question and the errors associated with the measurement of a particular quantity (i.e., the limitations of the measurement system). For example, "parallel" includes absolute parallelism and approximate parallelism, wherein the acceptable deviation range of approximate parallelism can be, for example, a deviation within ±10°; "perpendicular" includes absolute perpendicularity and approximate perpendicularity, wherein the acceptable deviation range of approximate perpendicularity can also be, for example, a deviation within ±10°. "Equal" includes absolute equality and approximate equality, wherein the acceptable deviation range of approximate equality can be, for example, the difference between the two equalities is less than or equal to 5% of either one.
[0069] Under the current development trend of electronic devices, in order to meet the user's requirements for thinness and lightness of electronic devices, it is required that the stacking thickness of the devices, structural parts, circuit boards and packaging structures inside the electronic devices along the thickness direction of the electronic devices is getting smaller and smaller. The circuit board occupies a certain thickness space in the whole machine. In particular, when the circuit board is a hard printed circuit board (PCB), since there is a rigid core board (core) in the substrate (also known as a core substrate) of this type of circuit board, the thickness of the rigid core board is relatively thick, therefore, the thickness of this type of circuit board is relatively thick, and this type of circuit board occupies more thickness space in the whole machine. The removal of the rigid core board and the reduction of the odd-numbered layer of board material can effectively reduce the total thickness of the circuit board. Based on this, the thinning demand of electronic equipment and the thinning demand of circuit boards can promote the development of coreless technology and odd-numbered layer boards. Among them, in the circuit board, the circuit board with the rigid core board removed is generally called a coreless substrate.
[0070] See also Figure 1 , Figure 1 Schematic diagram of the processing process of a coreless substrate in the related art. Specifically, the processing method of the coreless substrate includes the following steps:
[0071] Provide as Figure 1 The temporary carrier 31 shown in (a) .
[0072] A release layer 32 is provided on both sides of the temporary carrier plate 31 in the thickness direction to obtain a Figure 1 The structure shown in (b) in FIG.
[0073] like Figure 1 In (c), a double-sided semi-cured structure is pressed on the surfaces of the release layer 32 on both sides of the temporary carrier 31 to obtain Figure 1 The double-sided prepreg structure includes a prepreg 33 and two metal layers 34. The two metal layers 34 are respectively arranged on both sides of the prepreg 33 in the thickness direction. Figure 1 In the structure shown in (d) in FIG. 1 , one metal layer 34 in each double-sided prepreg structure is located between the prepreg sheet 33 and the release layer 32 . The other metal layer 34 is located on the surface of the prepreg sheet 33 that is away from the temporary carrier 31 .
[0074] A circuit is fabricated on the metal layer 34 of the double-sided semi-cured structure away from the temporary carrier 31 to form a central circuit layer 341, thereby obtaining Figure 1 The structure shown in (e) in FIG.
[0075] like Figure 1 In (f), the single-sided prepreg structure is heat-pressed and cured on the surface of the central circuit layer 341 to obtain Figure 1 The structure shown in (g) in FIG. The single-sided prepreg structure includes a prepreg layer 33 and a metal layer 34. Figure 1 In the structure shown in (g), the metal layer of the single-sided prepreg structure is located on the side of the prepreg away from the temporary carrier 31. In this way, the temporary carrier 31 has two coreless substrates with metal layers on both sides and a central circuit layer 341 in the middle.
[0076] like Figure 1 In (h), the coreless substrates on both sides of the temporary carrier 31 are peeled off from the temporary carrier 31 at the release layer 32 to obtain Figure 1 The coreless substrate is shown in (i) in FIG. The coreless substrate is subsequently subjected to drilling, in-hole electroplating, and the like.
[0077] The coreless substrate manufactured by the above processing technology often has internal stress inside. When the internal stress of the coreless substrate is greater than its own structural strength, the coreless substrate will warp and deform after the temporary carrier 31 is removed. The main reasons are as follows:
[0078] Reason 1: During the processing of the coreless substrate, the coreless substrate is compressed due to the force on both sides in the thickness direction. Before removing the temporary carrier 31, the stress on both sides of the entire coreless substrate in its own thickness direction is relatively symmetrical. However, after removing the temporary carrier 31, the surface of the coreless substrate that was originally supported by the temporary carrier 31 loses its support, and the symmetry of the stress of the entire coreless substrate in its own thickness direction is destroyed. The stress is released from the side of the coreless substrate toward the temporary carrier 31. The stress release causes the rebound of the coreless substrate, which in turn causes the warping deformation of the plate.
[0079] Reason 2: In the process of processing coreless substrate, combined with Figure 1 In (d) and (e), when the central circuit layer 341 is made, since the central circuit layer 341 is made on the metal layer 34 of the double-sided semi-cured structure away from the temporary carrier 31, the central circuit layer 341 is protruding from the surface of the semi-cured 33 where it is located. Figure 1 In (f) and (d), when the single-sided prepreg structure is hot-pressed on the central circuit layer 341, the central circuit layer 341 is embedded in the prepreg 33 of the single-sided prepreg structure. Although, before removing the temporary carrier 31, the stacked structure formed by lamination is symmetrically distributed with respect to the temporary carrier 31. However, after removing the temporary carrier 31, Figure 1 From the cross-sectional view of the coreless substrate shown in (i) in FIG. 1 , the two prepreg sheets 33 on both sides of the central circuit layer 341 cannot be symmetrically arranged with the central circuit layer 341 as the center, which results in a difference in the coefficient of thermal expansion (CTE) of the parts of the coreless substrate on both sides of the central circuit layer 341. Figure 2 , Figure 2 The following is a schematic diagram of the analysis of the warping of the plate caused by the different thermal expansion coefficients at both ends of the plate in the thickness direction. Figure 2 As shown, when the temperature of the plate increases, the plate bends toward the side with a high thermal expansion coefficient. When the temperature of the plate decreases, the plate may deform toward the side with a low thermal expansion coefficient. Based on this, the difference in the coefficient of thermal expansion (CTE) of the parts of the coreless substrate located on both sides of the central circuit layer 341 will increase the risk of warping of the coreless substrate.
[0080] Reason three: The substrate manufactured by this lamination method will also introduce internal stress into the board due to the process differences between layers, resulting in differences in the internal stress distribution of the coreless substrate and causing the warping problem of the coreless substrate.
[0081] In summary, in the related art, the coreless substrate has a warping problem. Therefore, it is very important to design a processing method that can at least prevent the coreless substrate from warping to a certain extent.
[0082] Based on this, in order to be able to solve the warpage problem of coreless substrates at least to some extent, please refer to Figure 3 , Figure 3 A schematic diagram of the processing process of a coreless substrate provided in the first embodiment of the present application. Specifically, the processing method of the coreless substrate includes the following steps:
[0083] S10: providing a first carrier composite structure 10 and a second carrier composite structure 20 respectively.
[0084] It is worth noting that the first carrier composite structure 10 and the second carrier composite structure 20 can be processed simultaneously, or the first carrier composite structure 10 can be processed first and then the second carrier composite structure 20; or, the second carrier composite structure 20 can be processed first and then the first carrier composite structure 10. This application does not impose any specific restrictions on this.
[0085] like Figure 3 The structure shown in (a1) is a first carrier composite structure 10. The first carrier composite structure 10 comprises a first temporary carrier 11, a first release layer 12 and a first composite layer structure 13 which are stacked in sequence.
[0086] Specifically, the first temporary carrier 11, the first release layer 12 and the first composite layer structure 13 are stacked in sequence. After the coreless substrate is processed by the processing method of the coreless substrate, the stacking direction of the first temporary carrier 11, the first release layer 12 and the first composite layer structure 13 is the thickness direction of the coreless substrate.
[0087] The first temporary carrier plate 11 is a rigid structure and can support the first composite layer structure 13 , so that the first composite layer structure 13 can be easily processed on the first temporary carrier plate 11 .
[0088] Specifically, the first release layer 12 may be a temporary bonding adhesive. By arranging the first release layer 12 on the first temporary carrier 11, the first temporary carrier 11 and the first release layer 12 can be separated from the first composite layer structure 13 at the first release layer 12.
[0089] Please continue reading Figure 3In (a1), the first composite layer structure 13 includes a first metal layer 131, a first prepreg 132, and a first metal circuit layer 133. The first metal layer 131, the first prepreg 132, and the first metal circuit layer 133 are stacked in sequence in a direction consistent with the stacking direction of the first temporary carrier 11, the first release layer 12, and the first composite layer structure 13. That is, the stacking direction of the first metal layer 131, the first prepreg 132, and the first metal circuit layer 133 is consistent with the stacking direction of the first temporary carrier 11, the first release layer 12, and the first composite layer structure 13.
[0090] The first metal layer 131 is stacked between the first semi-cured film and the first release layer 12. Exemplarily, the material of the first metal layer 131 is copper.
[0091] The first prepreg 132 has a first surface 132a facing away from the first temporary carrier 11. The first metal circuit layer 133 is disposed on the first surface 132a. Thus, the first metal layer 131 and the first metal circuit layer 133 are located on both side surfaces of the first prepreg in the thickness direction.
[0092] Please continue reading Figure 3 and Figure 4 ,in, Figure 4 Based on Figure 3 Schematic diagram of the relative position relationship between the vertical projection of the first metal circuit layer 133 on the first semi-cured sheet 132 and the first semi-cured sheet 132 in the first carrier composite structure 10 shown in (a1). The first metal circuit layer 133 has a plurality of first wirings 1331 and a first wiring gap 1332. Among them, the plurality of first wirings 1331 are arranged spaced apart. The extension paths between the plurality of first wirings 1331 can be the same or different, or, among the plurality of first wirings 1331, the extension paths of some of the first wirings 1331 are the same, and the extension paths of other first wirings 1331 are different. The present application does not make any specific limitation on this, as long as the plurality of first wirings 1331 are spaced apart. In the first metal circuit layer 133, the spacing spaces between the plurality of first wirings 1331 form the first wiring gap 1332 as a whole.
[0093] The "plurality" in the plurality of first routing lines 1331 refers to two or more. Figure 3 (a1) and Figure 4 In the specific example shown, there are four first routing lines 1331, which does not constitute a special limitation on the present application. In other examples, there may be two, five, ten, twenty, one hundred or more first routing lines 1331.
[0094] Exemplarily, the material of the first metal circuit layer 133 is copper.
[0095] Please continue reading Figure 3 In (a1), specifically, the first prepreg sheet 132 includes: a first adhesive layer 132b and a first fiber cloth 132c. The first adhesive layer 132b is in a semi-cured state.
[0096] The first adhesive layer 132b has a certain adhesive property. The first fiber cloth 132c is embedded in the first adhesive layer 132b. Since the structural strength of the first fiber cloth 132c is relatively high, the first prepreg sheet 132 including the first fiber cloth 132c is used as the processing material of the coreless substrate, which is conducive to ensuring the structural strength of the coreless substrate.
[0097] Exemplarily, the material of the first fiber cloth 132c is glass fiber. In other examples, it may also be aluminum oxide fiber, silicon carbide fiber, silicon nitride fiber or boron nitride fiber.
[0098] The first adhesive layer 132b includes a first resin matrix and a first filler. The first filler is distributed in the first resin matrix. Specifically, the first filler is uniformly distributed in the first resin matrix. The first filler can play a role in heat conduction, enhancing the structural strength of the first resin matrix, and reducing the thermal expansion coefficient of the first resin matrix.
[0099] The first resin matrix can be a thermosetting resin. Since the thermosetting resin is in liquid state at room temperature, in the actual processing of the semi-cured sheet, on the one hand, it is beneficial to fully mix the first filler in the thermosetting resin, which is beneficial to the uniform distribution of the first filler in the first semi-cured sheet 132; on the other hand, when the thermosetting resin is in liquid state, the prepreg resin mixture made of the first filler and the thermosetting resin can be used to impregnate the fiber cloth, and then the fiber cloth provided with the prepreg resin mixture is semi-cured to obtain the semi-cured sheet. In this way, the impregnation effect between the prepreg resin mixture and the fiber cloth is good, the contact area is large, which is beneficial to improve the bonding effect of the semi-curing, and on the other hand, it is also beneficial to embed the first filler in the prepreg resin mixture into the surface of the first fiber cloth 132c, thereby increasing the contact area between the first filler and the first fiber cloth 132c, optimizing the thermal conductivity of the first semi-cured sheet 132, etc. In addition, the thermosetting resin also has excellent properties such as high strength, good heat resistance, corrosion resistance, aging resistance, and good dimensional stability.
[0100] Specifically, the thermosetting resin includes at least one of epoxy resin, bismaleimide, cyanate ester and bismaleimide triazine (BT) resin. That is, the thermosetting resin can be epoxy resin, bismaleimide, cyanate ester or bismaleimide triazine (BT) resin, and can also be a blended resin of two or more of epoxy resin, bismaleimide, cyanate ester and bismaleimide triazine (BT) resin.
[0101] For example, when the thermosetting resin includes bismaleimide-triazine, the bismaleimide-triazine may have good rigidity and modulus after curing, and high structural strength, thus being beneficial to improving the structural strength of the coreless substrate.
[0102] Exemplarily, when the thermosetting resin includes epoxy resin and / or bismaleimide, the manufacturing cost can be reduced.
[0103] Exemplarily, the first filler may be in the form of particles, sheets, or lines. The first filler may include fillers in at least two forms of particles, sheets, or lines. For example, the first filler may be in the form of particles, sheets, and lines.
[0104] When the first filler has at least two forms of fillers including granular, flaky, and linear, first fillers of different forms can fill each other, thereby increasing the contact area between the first fillers and improving the distribution density of the first filler in the first resin matrix. Thus, first fillers of different forms can be used to construct a structural skeleton in the first resin matrix with poor structural strength, thereby improving the structural strength of the first semi-cured sheet 132.
[0105] The first filler being in a linear form refers to a filler extending in a linear shape, for example, a one-dimensional filler, and the linear shape includes but is not limited to a straight line, a curve, or a broken line. The first filler being in a sheet form refers to a filler that is particularly thin in a certain dimension and forms a thin sheet, for example, a two-dimensional filler. The first filler being in a granular form refers to a filler that is spherical or irregular, and whose dimensions in each direction are not much different, for example, a three-dimensional thermal conductive filler.
[0106] The material of the first filler includes, but is not limited to, carbon nanotubes, carbon fibers, graphene, graphene oxide, fluorinated graphene, boron nitride, aluminum nitride, silicon nitride, silicon carbide, aluminum oxide, magnesium oxide, zinc oxide, and the like.
[0107] like Figure 3The second carrier composite structure 20 is shown in (a2) of FIG. Specifically, the second carrier composite structure 20 includes a second temporary carrier 21, a second release layer 22, and a second composite layer structure 23 which are stacked in sequence.
[0108] Specifically, the second temporary carrier 21, the second release layer 22 and the second composite layer structure 23 are stacked in sequence. The stacking direction of the second temporary carrier 21, the second release layer 22 and the second composite layer structure 23 is consistent with the stacking direction of the first temporary carrier 11, the first release layer 12 and the first composite layer structure 13.
[0109] The second temporary carrier plate 21 is a rigid structure and can support the second composite layer structure 23. In this way, it is convenient to process the second composite layer structure 23 on the second temporary carrier plate 21.
[0110] Exemplarily, the material of the second temporary carrier 21 may be the same as that of the first temporary carrier 11. In this way, the second temporary carrier 21 and the first temporary carrier 11 may be processed using the same material. In other examples, the material of the second temporary carrier 21 may be different from that of the first temporary carrier 11.
[0111] Exemplarily, the specifications of the second temporary carrier 21 may be the same as those of the first temporary carrier 11. In this way, only one specification of temporary carrier needs to be processed, which can simplify the processing technology of the second temporary carrier 21 and the first temporary carrier 11. In other examples, the specifications of the second temporary carrier 21 may be different from those of the first temporary carrier 11.
[0112] Here, the specification of the second temporary carrier plate 21 being the same as that of the first temporary carrier plate 11 means that the shapes and sizes of the two are the same.
[0113] Specifically, the second release layer 22 may be a temporary bonding adhesive. By arranging the second release layer 22 on the second temporary carrier 21, the second temporary carrier 21 and the second release layer 22 can be separated from the second composite layer structure 23 at the second release layer 22.
[0114] The second composite layer structure 23 includes a second metal layer 231 and a second prepreg 232. The second metal layer 231 and the second prepreg 232 are stacked in sequence. The stacking direction of the second metal layer 231 and the second prepreg 232 is consistent with the stacking direction of the second temporary carrier 21, the second release layer 22 and the second composite layer structure 23.
[0115] The second metal layer 231 is located between the second prepreg 232 and the second release layer 22. Exemplarily, the second metal layer 231 is made of copper.
[0116] The second prepreg 232 has a second surface 232a facing away from the second temporary carrier 21. No metal circuit layer is disposed on the second surface 232a.
[0117] The second semi-cured sheet 232 includes: a second adhesive layer 232b and a second fiber cloth 232c. The second adhesive layer 232b is in a semi-cured state. The second fiber cloth 232c is embedded in the second adhesive layer 232b. The second adhesive layer 232b has a certain adhesive property. The second adhesive layer 232b includes a second resin matrix and a second filler.
[0118] The material of the second fiber cloth 232c can be the same as that of the first fiber cloth 132c, the second resin matrix can be the same as that of the first resin matrix, and the material of the second filler is the same as that of the first filler. That is, the material of the second prepreg 232 is the same as that of the first prepreg 132. The specific material of the second prepreg 232 can refer to the first prepreg 132 mentioned above, and will not be repeated here.
[0119] Please continue reading Figure 3 After step S10, the method for processing the coreless substrate further includes:
[0120] S20, the second surface 232a is directed toward the first surface 132a, and the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, so that the following can be obtained: Figure 3 In the first stacking structure, the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, and the second surface 232a faces the first surface 132a, and only the first metal circuit layer 133 is between the first prepreg 132 and the second prepreg 232. In this way, the first metal circuit layer 133 can be formed as a central circuit layer 105 between the first prepreg 132 and the second prepreg 232.
[0121] In order to improve the reliability of the coreless substrate processing, between step S10 and step S20, the first metal circuit layer 133 on the first carrier composite structure 10 may be inspected for quality defects. For example, an automated optical inspection (AOI) device may be used for inspection. This prevents the first metal circuit layer 133 with defects on the first carrier composite structure 10 from being used in the coreless substrate, which is beneficial to improving the yield of the coreless substrate.
[0122] In order to improve the reliability of the coreless substrate processing, before step S20, the first metal circuit layer 133 on the first carrier composite structure 10 may be subjected to a surface browning treatment. In this way, the surface of the first metal circuit layer 133 may be roughened, the bonding area between the first metal circuit layer 133 and other structures may be increased, and their surface bonding force may be increased.
[0123] Please continue reading Figure 3 After step S20, the method for processing the coreless substrate further includes:
[0124] S30: Performing a heat-pressing curing process on the stacked first carrier composite structure 10 and the second carrier composite structure 20. Figure 3 The second stacking structure shown in (c) is that Figure 3 The first stacking structure shown in (b) is subjected to heat pressing and curing treatment to obtain Figure 3 The second stacking structure shown in (c) in FIG. The first semi-cured sheet 132 forms a first medium structure after curing. The first medium structure includes a first bonding structure and a first fiber cloth 132c embedded in the first bonding structure. The first bonding structure is formed by curing the first bonding layer 132b. The second semi-cured sheet 232 forms a second medium structure after curing. The second medium structure includes a second bonding structure and a second fiber cloth 232c embedded in the second bonding structure. The second bonding structure is formed by curing the second bonding layer 232b.
[0125] Specifically, a vacuum hot press is used to perform hot pressing and curing treatment on the stacked first carrier composite structure 10 and the second carrier composite structure 20. The hot pressing temperature of the first stacked structure is related to the semi-cured material. For example, when the material of the resin matrix in the first semi-cured sheet 132 and the second semi-cured sheet 232 includes epoxy resin and / or bismaleimide, the hot pressing temperature is between 120 and 170°C, for example, the hot pressing temperature is 150 to 170°C. The hot pressing pressure is 0.5 to 2MPa, for example, 1MPa. The curing time is 30 to 60min.
[0126] Specifically, during the hot pressing process of the first stacking structure, the first adhesive layer 132b in the first semi-cured sheet 132 and the second adhesive layer 232b in the second semi-cured sheet 232 will melt and soften to a certain extent, and under the action of pressure, a part of the first adhesive layer 132b and a part of the second adhesive layer 232b fill the line gap of the central line layer 105 (that is, the first line gap 1332 of the first metal line layer 133), and at the same time, the first adhesive layer 132b in the first semi-cured sheet 132 and the second adhesive layer 232b in the second semi-cured sheet 232 contact and blend with each other. Therefore, in the second stacking structure obtained after the first stacking structure is cured, an adhesive layer 1011 formed by curing a portion of the first adhesive layer 132b and a portion of the second adhesive layer 232b will be formed between the first fiber cloth 132c and the second fiber cloth 232c. The adhesive layer 1011 not only realizes the connection between the first carrier composite structure 10 and the second carrier composite structure 20, but also fills the circuit gap of the central circuit layer 105 (that is, the first circuit gap 1332 of the first metal circuit layer 133).
[0127] That is, see Figure 3 In (c), the second stacking structure includes a first fiber cloth 132c, a second fiber cloth 232c and an intermediate layer structure 101. The first fiber cloth 132c and the second fiber cloth 232c are stacked. The intermediate layer structure 101 is arranged between the first fiber cloth 132c and the second fiber cloth 232c. The intermediate layer structure 101 includes an adhesive layer 1011 and a central line layer 105. The central line layer 105 is embedded in the adhesive layer 1011 and stacked with the first fiber cloth 132c and the second fiber cloth 232c. The intermediate layer structure 101 is bonded to the first fiber cloth 132c and the second fiber cloth 232c respectively by means of the adhesive layer 1011.
[0128] Please refer again Figure 3 After step S30, the method for processing the coreless substrate further includes:
[0129] S40: Peel off and remove the first temporary carrier 11 and the first release layer 12, as well as the second temporary carrier 21 and the second release layer 22. In this way, a Figure 3 The third stacking structure is shown in (d).
[0130] Specifically, in the processing method of the coreless substrate of the embodiment of the present application, when stacking the first carrier composite structure 10 and the second carrier composite structure 20, the first surface 132a of the first prepreg 132 away from the first temporary carrier 11 is stacked toward the second surface 232a of the second prepreg 232 away from the second temporary carrier 21 to obtain the first stacking structure. In this way, the first metal circuit layer 133 is located between the first prepreg 132 and the second prepreg 232, and the first temporary carrier 11 and the second temporary carrier 21 are located at both ends of the thickness direction of the entire first stacking structure. On this basis, after the first stacking structure is subjected to hot pressing curing treatment, in the obtained second stacking structure, the first temporary carrier 11 and the second temporary carrier 21 are still located at both ends of the thickness direction of the second stacking structure. In this way, before peeling off the first temporary carrier 11 and the first release layer 12, and the second temporary carrier 21 and the second release layer 22, the stress on both sides of the second stacking structure in its own thickness direction is relatively symmetrical. After peeling off the first temporary carrier 11 and the first release layer 12, as well as the second temporary carrier 21 and the second release layer 22, since the temporary carrier is peeled off on both sides, compared with the temporary carrier peeled off on one side in the related art, on the one hand, the residual stress of the coreless substrate during the pressing process and circuit manufacturing process can be released on both sides, and after the stress is released, the stresses at both ends of the thickness direction of the third stacking structure in its own thickness direction are relatively symmetrical, so that the stress inside the coreless substrate is relatively balanced, which is beneficial to avoid the warping problem of the coreless substrate at least to a certain extent and improve the flatness of the coreless substrate.
[0131] In some embodiments, before step S10, the processing method of the coreless substrate further includes a specific processing method of the first carrier composite structure 10. For details, please refer to Figure 5 , Figure 5 For processing provided in the embodiment of the present application Figure 3 Specifically, the specific processing method of the first carrier composite structure 10 includes:
[0132] S1: providing a first carrier structure 10a and a first prepreg structure 10b.
[0133] Specifically, see Figure 5The structure shown in (a1) is a first carrier structure 10a. The first carrier structure 10a includes a first temporary carrier 11, a first release layer 12 and a first metal layer 131 stacked in sequence. That is, the first temporary carrier 11 is provided with a first release layer 12 and a first metal layer 131. The first release layer 12 is disposed between the first temporary carrier 11 and the first metal layer 131. The first release layer 12 can be used to bond the first temporary carrier 11 and the first metal layer 131. Exemplarily, the first release layer 12 can be first disposed on the first temporary carrier 11, and then the first metal layer 131 can be disposed on the first release layer 12, so as to obtain the first carrier structure 10a.
[0134] like Figure 5 The structure shown in (a2) is a first prepreg structure 10b. The first prepreg structure 10b includes a first prepreg 132 and a third metal layer 134 stacked in a stack. Specifically, the third metal layer 134 is disposed on the first surface 132a of the first prepreg 132.
[0135] Please continue reading Figure 5 After step S1, the specific processing method of the first carrier composite structure 10 further includes:
[0136] S2: The surface of the first prepreg 132 opposite to the first surface 132a is oriented toward the first metal layer 131, and the first prepreg structure 10b and the first carrier structure 10a are stacked. Figure 5 The structure shown in (b) in FIG.
[0137] S3: Press the first prepreg structure 10b and the first carrier structure 10a together. Thus, the first prepreg structure 10b and the first carrier structure 10a can be connected together. Figure 5 The structure shown in (c) in FIG.
[0138] S4: Patterning the third metal layer 134 to form the first metal circuit layer 133. Figure 5 The structure shown in (d) is the first carrier composite structure 10.
[0139] The patterning of the third metal layer 134 refers to manufacturing a circuit on the third metal layer 134 , thereby forming the first metal circuit layer 133 , and obtaining the first carrier composite structure 10 .
[0140] Specifically, in this embodiment, in step S4, the third metal layer 134 may be processed by a subtractive process (tenting) to obtain the first metal circuit layer 133. For the specific process of patterning the third metal layer 134 by the tenting process to form the first metal circuit layer 133, please refer to Figure 6 , Figure 6 For processing provided in the embodiment of the present application Figure 5 The specific processing flow chart of the first carrier composite structure 10 is shown in FIG. Figure 6 The structure shown in (a1) is similar to Figure 5 The same as (a1) in . Figure 6 The structure shown in (a2) is similar to Figure 5 The same as (a2) in . Figure 6 The structure shown in (b) is similar to Figure 5 Same as (b) in . Figure 6 The structure shown in (c) is similar to Figure 5 In addition, step S4 specifically includes the following steps:
[0141] Step S41: forming a first photoresist layer 1a on the surface of the third metal layer 134 away from the first prepreg 132, such as Figure 6 The structure shown in (d) in FIG. 1 is illustratively, the first photoresist layer 1a can be a dry film. Also, illustratively, the first photoresist layer 1a can be a positive photoresist or a negative photoresist. The positive photoresist has a portion that is exposed to light that dissolves in the photoresist developer, while the portion that is not exposed to light does not dissolve in the photoresist developer. The negative photoresist has a portion that is exposed to light that does not dissolve in the photoresist developer, while the portion that is not exposed to light dissolves in the photoresist developer.
[0142] Step S42: Expose and develop the first photoresist layer 1a to form a first photoresist pattern layer 1b. Figure 6 The structure shown in (e) in FIG. Specifically, a partially light-transmissive and partially opaque mask can be used to cover the surface of the first photoresist layer 1a to expose and develop the first photoresist layer 1a. When the photoresist is a positive photoresist, the portion of the first photoresist layer 1a that is exposed to light can be dissolved in the developer and removed, while the portion of the first photoresist layer 1a that is not exposed to light still exists; when the photoresist is a negative photoresist, the portion of the first photoresist layer 1a that is not exposed to light can be dissolved in the developer and removed, while the portion of the first photoresist layer 1a that is exposed to light still exists. Then remove the mask. Among them, the first photoresist pattern layer 1b has a first window 1b1. The third metal layer 134 includes a first portion 1341 exposed to the first window 1b1 and a second portion 1342 covered by the first photoresist pattern layer 1b.
[0143] For example, in order to prevent photoresist residues from being formed in the first opening 1 b 1 after development, the first photoresist pattern layer 1 b may be subjected to a debonding treatment, such as a plasma treatment, after development.
[0144] Step S43: Etching and removing the first portion 1341 exposed through the first opening 1b1 to obtain the first metal circuit layer 133 formed by the second portion 1342. Figure 6 The entire structure shown in (e) is immersed in an etching solution, and the etching solution is used to remove the first portion 1341 exposed through the first window 1b1.
[0145] Step S44: stripping off the first photoresist pattern layer 1b. Figure 6 The entire structure shown in (f) is immersed in a stripping solution, and the first photoresist pattern layer 1b that is not dissolved in the developer is stripped off by the stripping solution. Figure 6 (g) in Figure 3 The first carrier composite structure 10 shown in (a1) in FIG. 1 . Exemplarily, the stripping liquid is sodium bicarbonate or potassium hydroxide.
[0146] It should be noted that the shape of the first metal circuit layer 133 is related to the shape of the mask, and the drawing of the first metal circuit layer 133 can be designed according to actual needs, and then the mask can be prepared according to the drawing.
[0147] Therefore, the method of processing the first metal circuit layer 133 by adopting the above-mentioned tenting process is simple, low-cost and high-efficiency.
[0148] In order to ensure the flow capacity of the first metal circuit layer 133, the thickness of the first metal circuit layer 133 is exemplarily in the range of 12 microns to 30 microns. Based on this, in the first prepreg structure 10b, since the first metal circuit layer 133 is formed by etching the third metal layer 134, the thickness of the two is consistent. In order to meet the thickness requirement of the first metal circuit layer 133, the thickness of the third metal layer 134 is in the range of 12 microns to 30 microns. Exemplarily, the thickness of the third metal layer 134 is in the range of 13 microns, 14 microns, 15 microns, 16 microns, 17 microns, 18 microns, 19 microns, 20 microns, 21 microns, 22 microns, 23 microns, 24 microns, 25 microns, 26 microns, 27 microns, 28 microns or 29 microns.
[0149] Based on any of the above embodiments, in some embodiments, before step S10, the method for processing the coreless substrate further includes a specific method for processing the second carrier composite structure 20. Figure 7 , Figure 7 For processing provided in the embodiment of the present application Figure 3Flow chart of the processing method of the second carrier composite structure 20 required in the embodiment. The specific processing method of the second carrier composite structure 20 includes:
[0150] Step S1': providing a second carrier structure 20a and a second prepreg structure 20b. Figure 7 The structure shown in (a1) is a second carrier structure 20a. The second carrier structure 20a includes a second temporary carrier 21, a second release layer 22, and a second metal layer 231 stacked in sequence. That is, the second temporary carrier 21 is provided with a second release layer 22 and a second metal layer 231. The second release layer 22 is provided between the second temporary carrier 21 and the second metal layer 231. The second release layer 22 can be used to bond the second temporary carrier 21 and the second metal layer 231. Figure 7 The structure shown in (a2) is the second prepreg structure 20b. The second prepreg structure 20b is only one layer of the second prepreg 232.
[0151] Please continue reading Figure 7 After step S1', the specific processing method of the second carrier composite structure 20 further includes:
[0152] Step S2': Place the surface of the second prepreg 232 opposite to the second surface 232a toward the second metal layer 231, and stack the second prepreg structure 20b and the second carrier structure 20a. Figure 7 The structure shown in (b) in FIG.
[0153] Step S3': Laminating the stacked second prepreg structure 20b and the second carrier structure 20a. Thus, the second prepreg structure 20b and the second carrier structure 20a can be connected together. Figure 7 (c) in the Figure 3 The second carrier composite structure 20 is shown in (a2) in FIG.
[0154] Since the second prepreg structure 20b does not include a metal layer for forming a metal circuit layer, the processing method of the second carrier composite structure 20 omits step S4, the patterning process of the metal layer, in the processing method of the first carrier composite structure 10. In this way, the processing technology of the coreless substrate is simplified while ensuring the circuit density of the central circuit layer 105.
[0155] Based on any of the above embodiments, after step S40, the method for processing the coreless substrate further includes a step of processing the third stacking structure. Figure 8 , Figure 8 The application provided in Figure 3 Schematic diagram of further processing of the coreless substrate after the processing flow shown. Specifically, the specific processing method of the third stacking structure includes the following steps:
[0156] Step S50: drilling the first metal layer 131 and the first dielectric structure to form a first through hole 106, and drilling the second metal layer 231 and the second dielectric structure to form a second through hole 107, thereby obtaining Figure 8 The structure shown in (b) in FIG. 1 is a schematic diagram of a structure in which the first through hole 106 penetrates the first metal layer 131 and the first dielectric structure. The second through hole 107 penetrates the second metal layer 231 and the second dielectric structure. The first through hole 106 and the second through hole 107 do not penetrate the central circuit layer 105.
[0157] The provision of the first through hole 106 facilitates subsequent metallization in the hole to achieve electrical connection between the central circuit layer 105 and the first metal layer 131 .
[0158] The second through hole 107 facilitates subsequent in-hole metallization to achieve electrical connection between the central wiring layer 105 and the second metal layer 231 .
[0159] For example, the first through hole 106 and the second through hole 107 may be prepared by laser or laser process.
[0160] Step S60: forming a first conductive layer 1061 on the hole wall of the first through hole 106. At the same time, forming a second conductive layer 1071 on the hole wall of the second through hole 107, Figure 8 The structure shown in (c) in FIG. Exemplarily, the first conductive layer 1061 and the second conductive layer 1071 may also be metal layers, for example, the conductive layers are formed on the hole walls of the first through hole 106 and the second through hole 107 by chemical plating or sputtering. The provision of the first conductive layer 1061 and the second conductive layer 1071 can facilitate electroplating in the first through hole 106 and the second through hole 107 in the subsequent electroplating process.
[0161] Step S70: Electroplating is performed at the first through hole 106 to form a first metal conductive portion 108 filling the first through hole 106. At the same time, electroplating is performed at the second through hole 107 to form a second metal conductive portion 109 filling the second through hole 107. The first metal conductive portion 108 is connected to the first metal layer 131 and the central circuit layer 105 respectively. The second metal conductive portion 109 is connected to the second metal layer 231 and the central circuit layer 105 respectively. Thus, the following can be obtained: Figure 8 The structure shown in (d).
[0162] Specifically, since the entire structure is placed in the electroplating solution during the electroplating process in the first through hole 106 and the second through hole 107, the surface of the first metal layer 131 and the second metal layer 231 will also be covered by a layer of electroplated metal. In order to remove the electroplated metal on the surface of the first metal layer 131 and the second metal layer 231, an etching or copper reduction step may be included between step S70 and step S80 to remove at least a portion or all of the electroplated metal covering the surface of the first metal layer 131 and the second metal layer 231, so as to obtain the first metal layer 131 and the second metal layer 231 of the desired thickness.
[0163] Step S80: patterning the first metal layer 131 to form the first circuit layer 103, and patterning the second metal layer 231 to form the second circuit layer 102. Figure 8 As shown in (e) of FIG. 1 , the first metal conductive part 108 is respectively connected to the first circuit layer 103 and the central circuit layer 105 and is electrically connected thereto. The second metal conductive part 109 is respectively connected to the second circuit layer 102 and the central circuit layer 105 and is electrically connected thereto.
[0164] For example, in step S80, the specific processing method for the first circuit layer 103 can refer to the processing method for the first metal circuit layer 133 in the foregoing text, that is, the first metal layer 131 can be processed by a subtractive method (tenting) process, which will not be described in detail here. Similarly, in step S80, the specific processing method for the second circuit layer 102 can refer to the processing method for the first metal circuit layer 133 in the foregoing text, that is, the second metal layer 231 can be processed by a subtractive method (tenting) process, which will not be described in detail here.
[0165] In this way, a coreless substrate having three circuit layers (the first circuit layer 103, the central circuit layer 105 and the second circuit layer 102) can be obtained, and the processing process is simple.
[0166] For the previous Figure 3-Figure 8In the processing method of the coreless substrate shown, since both the first prepreg 132 and the second prepreg 232 contain fiber cloth, in step S30, during the hot pressing curing process of the second stacked structure, when the pressure is too large, the temperature is too high, and / or because the content of the adhesive layer in the first prepreg 132 and the second prepreg 232 is low, the fiber cloth may be squeezed with the central circuit layer 105, and the fiber cloth and / or the central circuit layer 105 may be broken or cracked, thereby causing the problem of the coreless substrate bursting. In addition, since the central circuit layer 105 (that is, the first metal circuit layer 133) is formed on the first surface 132a of the first prepreg 132 and protrudes from the first surface 132a. In this way, in the second stacked structure obtained in step S20, the second surface 232a of the second prepreg 232 is in direct contact with the first metal circuit layer 133. In addition, there is no metal circuit layer on the second surface 232a of the second prepreg 232, so in step S30, during the hot pressing of the second stacked structure, the adhesive layer on the second prepreg 232 is more embedded in the circuit gap (i.e., the first circuit gap 1332) of the central circuit layer 105 (i.e., the first metal circuit layer 133). Figure 8 In the third stacking structure shown in (a), when the second prepreg is the same as the first prepreg (that is, the two are made of the same material and have the same specifications), the distance d2 between the central circuit layer 105 and the second fiber cloth 232c is smaller than the distance d1 between the central circuit layer 105 and the first fiber cloth 132c, which results in that the processed coreless substrate cannot be symmetrically arranged with the central circuit layer 105 as the center. Therefore, in the entire second stacking structure, the thermal expansion coefficients of the parts on both sides of the thickness direction of the central circuit layer 105 are different. That is, the above Figure 3-Figure 8 The illustrated embodiment still cannot solve the second reason causing the warping of the coreless substrate in the related art, thus still causing the problem of warping and deformation of the coreless substrate.
[0167] To avoid this problem, please refer to Fig. 9 , Fig. 9 A schematic diagram of the processing process of a coreless substrate provided in the second embodiment of the present application. Fig. 9 The structure shown in (a1) is similar to Figure 3 The structure is the same as that shown in (a1). Fig. 9 The structure shown in (a2) is similar to Figure 3 In addition, the processing method of the coreless substrate in this embodiment is the same as that in the above-mentioned Figure 3-Figure 8 The difference between the processing methods of coreless substrates shown in is:
[0168] Between step S10 and step S20, the method for processing the coreless substrate further includes the following steps:
[0169] S101: Dispose a liquid or semi-cured insulating filler 132a1 on the first surface 132a and / or the second surface 232a. That is, the insulating filler 132a1 may be disposed only on the first surface 132a, or only on the second surface 232a, or both. The insulating filler 132a1 is in a liquid or semi-cured state. For example, Fig. 9 As shown in FIG. 5( b ), an insulating filler 132 a 1 is disposed on the first surface 132 a of the first carrier assembly 10 , while no insulating filler 132 a 1 is disposed on the second surface 232 a of the second carrier assembly 20 .
[0170] Thus, in step S20, when the second surface 232a is facing the first surface 132a and the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, the insulating filling glue 132a1 can be squeezed to fill the line gap of the central circuit layer 105 (that is, the first line gap 1332 of the first metal circuit layer 133) at least to a certain extent due to the stacking of the two. Fig. 9 The structure shown in (c) in FIG.
[0171] Furthermore, in step S30, when the first stacked structure is hot-pressed, the insulating filling glue 132a1 can be further made to fully fill the circuit gaps of the central circuit layer 105, such as Fig. 9 The structure shown in (d) in FIG. 1 can prevent the first adhesive layer 132b and the second adhesive layer 232b from being embedded in the line gap of the central line layer 105, thereby preventing the central line layer 105 from contacting the fiber cloth, thereby preventing the problem of cracks caused by the fiber cloth contacting and squeezing the central line layer 105 due to excessive pressure, high temperature, and / or low content of the adhesive layer in the first semi-cured sheet 132 and the second semi-cured sheet 232. In addition, since the insulating filling glue 132a1 fills the line gap of the central line layer 105. Therefore, as Fig. 9In the second stacking structure shown in (d), the distance d2 between the central circuit layer 105 and the second fiber cloth 232c and the distance d1 between the central circuit layer 105 and the first fiber cloth 132c may be close to each other, which may help improve the symmetry of the second stacking structure with the central circuit layer 105 as the center, and further help the entire coreless substrate to be symmetrically arranged with the central circuit layer 105 as the center, and then reduce or eliminate the difference in thermal expansion coefficients of the parts on both sides of the thickness direction of the central circuit layer 105, further avoid the warping and deformation problem of the coreless substrate, and improve the flatness of the coreless substrate.
[0172] On this basis, the second prepreg 232 is the same as the first prepreg 132. In this way, the distance d2 between the central circuit layer 105 and the second fiber cloth 232c and the distance d1 between the central circuit layer 105 and the first fiber cloth 132c can be equal, which can help improve the symmetry of the second stacking structure with the central circuit layer 105 as the center, and further help the entire coreless substrate to be symmetrically arranged with the central circuit layer 105 as the center, and then reduce or eliminate the difference in thermal expansion coefficients of the parts on both sides of the thickness direction of the central circuit layer 105, further avoid the warping deformation problem of the coreless substrate, and improve the flatness of the coreless substrate.
[0173] Please continue reading Fig. 9 In the structures shown in (d), (e), (f), (g), (h) and (i), the adhesive layer 1011 between the first fiber cloth 132c and the second fiber cloth 232c includes a first adhesive layer 10111, a filling adhesive portion 10113 and a second adhesive layer 10112 stacked in sequence. The first adhesive layer 10111 is formed by curing a portion of the first adhesive layer 132b and is bonded to the first fiber cloth 132c. The second adhesive layer 10112 is formed by curing a portion of the second adhesive layer 232b and is bonded to the second fiber cloth 232c. The filling adhesive portion 10113 is formed by curing the insulating filling adhesive 132a1. The filling adhesive portion 10113 fills the entire line gap of the central line layer 105 and is connected to the first adhesive layer 10111 and the second adhesive layer 10112.
[0174] It can be understood that in order to ensure that the insulating filling glue 132a1 can completely fill the line gap of the central circuit layer 105, and taking into account the possible reduction in volume of the insulating filling glue 132a1 after curing and the problem of glue overflow during the pressurization process, the filling amount (volume) of the insulating filling glue 132a1 is greater than the volume of the line gap of the central circuit layer 105.
[0175] For example, in the actual processing of the coreless substrate, in step S20, when the first carrier composite structure 10 and the second carrier composite structure 20 are arranged and stacked in the up-down direction, in step S101, the insulating filling glue 132a1 can be preferentially set on the carrier composite structure located at the lower side of the first carrier composite structure 10 and the second carrier composite structure 20, and the insulating filling glue 132a1 is not set on the carrier composite structure located at the upper side. In this way, the problem of dripping and overflowing of the insulating filling glue 132a1 caused by setting the insulating filling glue 132a1 on the carrier composite structure located at the upper side can be prevented.
[0176] In some embodiments, the insulating filling glue 132a1 includes a third resin matrix and a third filler distributed in the third resin matrix. Specifically, the third filler is evenly distributed in the third resin matrix. The third filler can play a role in heat conduction, enhancing the structural strength of the third resin matrix, and reducing the thermal expansion coefficient of the insulating filling glue 132a1.
[0177] Considering that the stacked first carrier composite structure 10 and the second carrier composite structure 20 are subjected to hot pressing curing treatment in step S30, in order to make the hot pressing temperature of the insulating filler 132a1 consistent with the hot pressing temperature of the resin matrix in the first prepreg 132 and the second prepreg 232 in this step, and to improve the compatibility of the resin matrix in the first prepreg 132 and the second prepreg 232 with the third resin matrix, the material of the third resin matrix is the same as that of the first resin matrix. For example, the material of the third resin matrix and the material of the first resin matrix are both epoxy resin and bismaleimide.
[0178] In other examples, the third resin matrix may also be polyimide or photosensitive polyimide.
[0179] On this basis, the material of the third filler is the same as that of the first filler, which is conducive to selecting fillers of the same material to make the first filler and the second filler respectively, thereby simplifying the process.
[0180] In order to improve the connection reliability of the insulating filling glue 132a1 to the first prepreg 132 and the second prepreg 232, and the compatibility of the insulating filling glue 132a1 with the first resin matrix, the third filler can be in a granular form. In this way, compared with the third filler in a sheet or line form, the granular third filler is easier to be evenly distributed in the insulating filling glue 132a1, so that the composition uniformity of the insulating filling glue 132a1 is better, and the connection reliability of the insulating filling glue 132a1 to the first prepreg 132 and the second prepreg 232 is improved.
[0181] In order to further improve the thermal conductivity and structural strength of the insulating filler 132a1 and further reduce the thermal expansion coefficient of the insulating filler 132a1, the mass percentage of the third filler in the insulating filler 132a1 is greater than the mass percentage of the first filler in the first adhesive layer 132b.
[0182] Exemplarily, the mass percentage of the third filler in the insulating filling glue 132 a 1 is greater than the mass percentage of the first filler in the first adhesive layer 132 b by 1%, 2%, 3%, 4% or 5%.
[0183] Regarding the previous article about Figure 3-Figure 9 In the processing method of the coreless substrate shown in the figure, in the second stacking structure, the central circuit layer 105 between the first prepreg 132 and the second prepreg 232 is only a first metal circuit layer 133. And the first metal circuit layer 133 is made on the first prepreg 132 by using the tenting process. Since the first metal circuit layer 133 is formed by etching the third metal layer 134 in the tenting process. Please refer to Fig.10 , Fig.10 Based on Figure 3-Figure 9 The cross-sectional view of the first carrier composite structure 10 in the method for processing the coreless substrate is shown in FIG. When processing the first metal circuit layer 133, it is theoretically desired that the shape of the first metal circuit layer 133 (eg Fig.10 The dotted box indicated by the arrow A2 in FIG. 1 and the shape of the first photoresist pattern layer 1b (as shown in FIG. Fig.10 However, since the third metal layer 134 is relatively thick, during the actual etching process, when etching away the first portion 1341 exposed through the first window 1b1, the etching liquid will also etch away a portion of the second portion 1342 having a thickness similar to that of the third metal layer 134 around the first portion 1341, so that the cross section of the first trace 1331 of the processed first metal circuit layer 133 is as follows: Fig.10 The trapezoid shown in the figure. This results in a large line pitch when the tenting process is used to make circuits, making it difficult to achieve fine line pitch. The line pitch made by the current tenting process is generally around 40-50μm. The minimum line pitch made by a processing plant with strong process control capabilities can only be 35-40μm. The size of the line pitch is an important factor affecting the high density of the circuit layer. How to develop a fine line pitch processing technology to improve the high density of the circuit layer is urgent.
[0184] Based on this, in order to reduce the line spacing of the central line layer 105 and thus increase the density of the lines of the central line layer 105, please refer to Fig.11 , Fig.11This is a processing flow chart of a second carrier composite structure 20 of a coreless substrate provided in the third embodiment of the present application. Fig.11 (a1) and Figure 7 The structure of (a1) is the same as that of (a1). Fig.11 (a1) and Figure 7 The structure of (a1) is the same as that of (a1).
[0185] The processing method of the coreless substrate in this embodiment is the same as that described above. Fig. 9 The difference between the processing methods of coreless substrates shown in is:
[0186] In the second prepreg structure 20b provided in step S1', the second prepreg structure 20b includes, in addition to the second prepreg 232, a fourth metal layer 234, such as Fig.11 As shown in (a2) in FIG. 4 . The fourth metal layer 234 is disposed on the second surface 232a of the second prepreg 232. Based on this, in step S2', when the surface of the second prepreg 232 opposite to the second surface 232a is directed toward the second metal layer 231, and the second prepreg structure 20b and the second carrier structure 20a are stacked, the fourth metal layer 234 is located on the surface of the second prepreg 232 opposite to the second temporary carrier 21.
[0187] Therefore, the structure obtained in step S2' and step S3' includes the fourth metal layer 234, such as Fig.11 (b) and (c) in .
[0188] Then, after step S3', the specific processing method of the second carrier composite structure 20 further includes:
[0189] S4': Patterning the fourth metal layer 234 to form a second metal circuit layer 233 to obtain a second carrier composite structure 20, such as Fig.11 As shown in (d) in FIG. 1 . It can be seen that, in this example, the second composite layer structure 23 includes a second metal circuit layer 233 in addition to the second metal layer 231 and the second semi-cured sheet 232. The second metal layer 231, the second semi-cured sheet 232 and the second metal circuit layer 233 are stacked in sequence. That is, the stacking direction of the second metal layer 231, the second semi-cured sheet 232 and the second metal circuit layer 233 is consistent with the stacking direction of the second temporary carrier 21, the second release layer 22 and the second composite layer structure 23. Among them, the second metal circuit layer 233 is arranged on the second surface 232a. As a result, the second metal layer 231 and the second metal circuit layer 233 are on the two side surfaces in the thickness direction of the second semi-cured sheet.
[0190] For example, in step S4', the fourth metal layer 234 may be processed by a tenting process to obtain the second metal circuit layer 233. The specific process flow of patterning the fourth metal layer 234 by the tenting process to form the second metal circuit layer 233 may refer to the process flow of the first metal circuit layer 133, which will not be repeated here.
[0191] Therefore, the process of processing the second metal circuit layer 233 by using the tenting process is simple and efficient.
[0192] See also Fig.12 , Fig.12 Based on Fig.11 A schematic diagram of the relative position relationship between the vertical projection of the second metal circuit layer 233 on the second prepreg 232 and the second prepreg 232 in the second carrier composite structure 20 shown. The second metal circuit layer 233 has a plurality of second wirings 2331 and second wiring gaps 2332. Among them, the plurality of second wirings 2331 are arranged spaced apart. The extension paths between the plurality of second wirings 2331 can be the same or different, or, among the plurality of second wirings 2331, the extension paths of some of the second wirings 2331 are the same, and the extension paths of other second wirings 2331 are different. This application does not make specific restrictions on this, as long as the plurality of second wirings 2331 are spaced apart.
[0193] The "plurality" in the plurality of second routing lines 2331 refers to two or more. Fig.12 In the specific example shown, there are three second routing lines 2331, which does not constitute a special limitation on the present application. In other examples, there may be two, four, five, ten, twenty, one hundred or more second routing lines 2331.
[0194] In the second metal wiring layer 233 , the spacing spaces between the plurality of second wirings 2331 form a second wiring gap 2332 as a whole.
[0195] In order to ensure the flow capacity of the second metal circuit layer 233, the thickness of the second metal circuit layer 233 is exemplarily in the range of 12 microns to 30 microns. Based on this, in the second prepreg structure 20b, since the second metal circuit layer 233 is formed by etching the fourth metal layer 234, the thickness of the two is consistent. In order to meet the thickness requirement of the second metal circuit layer 233, the thickness of the fourth metal layer 234 is in the range of 12 microns to 30 microns.
[0196] Exemplarily, the thickness of the fourth metal layer 234 ranges from 13 microns, 14 microns, 15 microns, 16 microns, 17 microns, 18 microns, 19 microns, 20 microns, 21 microns, 22 microns, 23 microns, 24 microns, 25 microns, 26 microns, 27 microns, 28 microns or 29 microns.
[0197] On this basis, based on the arrangement of the second metal circuit layer 233 on the second carrier composite structure 20, in step S20 of stacking the first carrier composite structure 10 and the second carrier composite structure 20, it is necessary to consider staggering the first metal circuit layer 133 and the second metal circuit layer 233 to prevent the first metal circuit layer 133 and the second metal circuit layer 233 from being stacked in the formed second stacked structure. For details, please refer to Fig.13 , Fig.13 To adopt Fig.11 Flow chart of a method for processing a coreless substrate of a second carrier composite structure 20 shown in FIG. Fig.13 (a1) and Fig. 9 The structure of (a1) is the same as that of (a1). Fig.13 (b) and Fig. 9 In addition, Fig.13 As shown in (a2), when the second carrier composite structure 20 further includes a second metal circuit layer 233, step S20 specifically includes:
[0198] When the second surface 232a is directed toward the first surface 132a and the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, the second wiring 2331 of the second metal wiring layer 233 is spaced apart from the first wiring 1331 of the first metal wiring layer 133 in a direction perpendicular to the second surface 232a, and at least a portion of the second wiring 2331 of the second metal wiring layer 233 is located within the first wiring gap 1332 of the first metal wiring layer 133, so as to obtain a first stacking structure. In this way, the first metal wiring layer 133 and the second metal wiring layer 233 form a central wiring layer 105 as a whole.
[0199] Compared with the method of manufacturing the central circuit layer 105 on the first prepreg 132, in the embodiment of the present application, the first metal circuit layer 133 of the central circuit layer 105 is manufactured on the first prepreg 132, and the second metal circuit layer 233 of the central circuit layer 105 is manufactured on the second prepreg 232. In this way, the line spacing of the entire central circuit layer 105 is not limited by the circuit manufacturing process and can be adjusted according to actual needs. Therefore, under the premise of not changing the line spacing of the circuit manufacturing that can be achieved by the current circuit manufacturing process, the first metal circuit layer 133 of the central circuit layer 105 is stacked. When the carrier composite structure 10 and the second carrier composite structure 20 are formed, the second wiring 2331 of the second metal circuit layer 233 is spaced apart from the first wiring 1331 of the first metal circuit layer 133 in a direction perpendicular to the second surface 232a, and at least a portion of the second wiring 2331 of the second metal circuit layer 233 is located within the first circuit gap 1332 of the first metal circuit layer 133, thereby facilitating reduction of the circuit spacing of the central circuit layer 105, improving the circuit density of the central circuit layer 105, and achieving high density of the central circuit layer 105.
[0200] Since the first metal circuit layer 133 and the second metal circuit layer 233 are both made by the tenting process, Fig.13 As shown in (c), (d), (e), (f), (g), (h) and (i) in the figure, in the direction from the first fiber cloth 132c to the second fiber cloth 232c, the cross-sectional area of the first routing line 1331 gradually decreases, and the cross-sectional area of the second routing line 2331 gradually increases. That is, the changes in the cross-sectional area of the first routing line 1331 and the second routing line 2331 are opposite.
[0201] In order to improve the reliability of the coreless substrate processing, before step S20, the second metal circuit layer 233 on the second carrier composite structure 20 may be inspected for quality defects. For example, an automated optical inspection (AOI) device may be used for inspection. This prevents the defective second metal circuit layer 233 on the second carrier composite structure 20 from being used in the coreless substrate, which is beneficial to improving the yield of the coreless substrate.
[0202] In order to improve the reliability of the coreless substrate processing, before step S20, the second metal circuit layer 233 on the second carrier composite structure 20 may be subjected to a surface browning treatment. In this way, the surface of the second metal circuit layer 233 may be roughened, the bonding area between the second metal circuit layer 233 and the insulating filler 132a1 may be increased, and the surface bonding force between the two may be increased.
[0203] It is worth noting that, in order to ensure signal conduction of the three-layer circuit layer of the coreless substrate, in step S50, a portion of the first through-holes 106 penetrate the first metal layer 131 and extend from the first metal layer 131 to connect with the first metal circuit layer 133 of the central circuit layer 105, and another portion of the first through-holes 106 penetrate the first metal layer 131 and extend from the first metal layer 131 to connect with the second metal circuit layer 233 of the central circuit layer 105. A portion of the second through-holes 107 penetrate the second metal layer 231 and extend from the second metal layer 231 to connect with the second metal circuit layer 233 of the central circuit layer 105, and another portion of the second through-holes 107 penetrate the second metal layer 231 and extend from the second metal layer 231 to connect with the second metal circuit layer 233 of the central circuit layer 105, as shown in FIG. Fig.13 As indicated in (f) in the figure.
[0204] Among them, at least a portion of the second routing 2331 of the second metal wiring layer 233 is located in the first wiring gap 1332 of the first metal wiring layer 133, which means that the second routing 2331 of the entire second metal wiring layer 233 may be located in the first wiring gap 1332 of the first metal wiring layer 133, or a portion of the second routing 2331 of the second metal wiring layer 233 may be located in the first wiring gap 1332 of the first metal wiring layer 133, and another portion of the second metal wiring layer 233 is located on the outer peripheral side of the entire first metal wiring layer 133.
[0205] On this basis, in order to further improve the high density of the central circuit layer 105, step S20 specifically includes: while the second surface 232a is facing the first surface 132a and the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, the second wiring 2331 of the second metal circuit layer 233 is spaced apart from the first wiring 1331 of the first metal circuit layer 133 in a direction perpendicular to the second surface 232a, and at least a portion of the second wiring 2331 of the second metal circuit layer 233 is located in the first wiring gap 1332 of the first metal circuit layer 133, and at least a portion of the first wiring 1331 of the first metal circuit layer 133 is located in the second wiring gap 2332, so as to obtain a first stacking structure.
[0206] For details, please refer to Fig.14 , Fig.14 Based on Fig.13 The first stacking structure is a schematic diagram showing the relative position relationship of the vertical projections of the first metal circuit layer 133 and the second metal circuit layer 233 on the second prepreg 232. The second traces 2331 of the entire second metal circuit layer 233 are all located in the first circuit gaps 1332 of the first metal circuit layer 133.
[0207] Exemplarily, a plurality of first wirings 1331 are arranged in a row. A plurality of second wirings 2331 are arranged in a row. A first sub-circuit gap is formed between two adjacent first wirings 1331. Step S20 specifically includes: while the second surface 232a is facing the first surface 132a and the first carrier composite structure 10 and the second carrier composite structure 20 are stacked, the second wirings 2331 of the second metal wiring layer 233 are spaced apart from the first wirings 1331 of the first metal wiring layer 133 in a direction perpendicular to the second surface 232a, and a second wiring 2331 is accommodated between two adjacent first wirings 1331, and a first wiring 1331 is accommodated between two adjacent second wirings 2331, so as to obtain a first stacking structure. Thus, in the first stacking structure, the first wirings 1331 and the second wirings 2331 are arranged alternately. This is conducive to further improving the high density of the central wiring layer 105.
[0208] As disclosed in the foregoing, the circuit layers (e.g., the first metal circuit layer 133, the second metal circuit layer 233, the first circuit layer 103, and the second circuit layer 102) are made by the tenting process. And, as mentioned above, the circuits made by the tenting process are prone to the defect of large line spacing. In order to solve the problem of large line spacing caused by the tenting process. The following provides a processing technology different from the tenting process for the production of circuit layers. Specifically, a modified semi-additive process (MSAP) can be used to produce circuit layers (e.g., the first metal circuit layer 133, the second metal circuit layer 233, the first circuit layer 103, and the second circuit layer 102). The specific differences are as follows:
[0209] See also Fig.15 , Fig.15 Schematic diagram of the processing process of the first carrier structure 10a of the coreless substrate provided in the fourth embodiment of the present application. Before step S1, the processing method of the coreless substrate also includes:
[0210] Step S01 : disposing a first release layer 12 and a first metal seed layer 136 on a first temporary carrier 11 ; wherein the first metal seed layer 136 is located on a surface of the first release layer 12 away from the first temporary carrier 11 .
[0211] Exemplarily, the first release layer 12 may be first disposed on the first temporary carrier 11, and then the first metal seed layer 136 may be disposed on the first release layer 12. Also exemplary, the first release layer 12 and the first metal seed layer 136 may be disposed together first, and then the first temporary carrier 11 and the first release layer 12 may be connected.
[0212] Step S02 : forming a second photoresist layer 2 a on the surface of the first metal seed layer 136 away from the first temporary carrier 11 ; the specific material of the second photoresist layer 2 a can refer to the first photoresist layer 1 a mentioned above, which will not be described again.
[0213] Step S03: Expose and develop the second photoresist layer 2a to form a second photoresist pattern layer 2b. The second photoresist pattern layer 2b has a second window 2b1, and the first metal seed layer 136 includes a first seed portion 1361 exposed in the second window 2b1 and a second seed portion 1362 covered by the second photoresist pattern layer 2b. The specific formation method of the second photoresist pattern layer 2b can refer to the first photoresist pattern layer 1b in the above text, which will not be repeated here.
[0214] Exemplarily, in order to prevent photoresist residues from being formed in the second window 2b1 after development, a debonding step may be provided between step S03 and step S04, that is, debonding the second photoresist pattern layer, for example, by plasma treatment.
[0215] Step S04: Electroplating is performed at the second window 2b1 to form a second target coating 138 covering the first seed portion 1361. Exemplarily, the thickness of the second target coating 138 ranges from 9 to 27 microns. For example, the thickness of the second target coating 138 is 10 microns, 12 microns, 15 microns, or 20 microns.
[0216] Step S05: stripping off the second photoresist pattern layer 2b to expose the second seed portion 1362, so as to obtain the first metal layer 131 formed by the second target plating layer 138 and the first metal seed layer 136. Thus, the first carrier structure 10a can be obtained.
[0217] See also Fig.16 , Fig.16 Schematic diagram of the processing of the second carrier structure 20a of the coreless substrate provided in the fourth embodiment. Before step S1, the processing method of the second carrier structure 20a includes the following steps:
[0218] Step S01 ′: disposing a second release layer 22 and a second metal seed layer 236 on the second temporary carrier 21 ; wherein the second metal seed layer 236 is disposed on a surface of the second release layer 22 away from the second temporary carrier 21 .
[0219] Exemplarily, the second release layer 22 may be first disposed on the second temporary carrier 21, and then the second metal seed layer 236 may be disposed on the second release layer 22. Also exemplary, the second release layer 22 and the second metal seed layer 236 may be disposed together first, and then the second temporary carrier 21 and the second release layer 22 may be connected.
[0220] Step S02 ′: forming a third photoresist layer 3 a on the surface of the second metal seed layer 236 away from the second temporary carrier 21 ; the specific material of the third photoresist layer 3 a can refer to the first photoresist layer mentioned above, which will not be described again.
[0221] Step S03': Expose and develop the third photoresist layer 3a to form a third photoresist pattern layer 3b. The third photoresist pattern layer 3b has a third window 3b1, and the second metal seed layer 236 includes a third seed portion 2361 exposed in the third window 3b1 and a fourth seed portion 2362 covered by the third photoresist pattern layer 3b. The specific formation method of the third photoresist pattern layer 3b can refer to the first photoresist pattern layer in the previous text, and will not be repeated here.
[0222] Exemplarily, in order to prevent photoresist residues from being formed in the third opening 3b1 after development, a debonding step may be provided between step S03' and step S04', that is, debonding the third photoresist pattern layer 3b, for example, by plasma treatment.
[0223] Step S04 ′: electroplating is performed at the third opening window 3 b 1 to form a third target plating layer 238 covering the third seed portion 2361 .
[0224] Step S05': stripping off the third photoresist pattern layer 3b to expose the fourth seed portion 2362, so as to obtain the second metal layer 231 formed by the third target plating layer 238 and the second metal seed layer 236. Thus, the second carrier structure 20a can be obtained.
[0225] See also Fig.17 , Fig.17 To adopt Fig.15 The specific processing diagram of the first carrier plate composite structure 10 of the first carrier plate structure 10a is shown in FIG. Fig. 9 The difference between the embodiments shown mainly lies in step S4. Specifically, step S4 includes the following steps:
[0226] Step S41: forming a first photoresist layer 1a on a surface of the third metal layer 134 away from the first prepreg 132. The third metal layer 134 is a seed layer.
[0227] Step S42: Expose and develop the first photoresist layer 1a to form a first photoresist pattern layer 1b, wherein the first photoresist pattern layer 1b has a first window 1b1. The third metal layer 134 includes a first portion 1341 exposed at the first window 1b1 and a second portion 1342 covered by the first photoresist pattern layer 1b.
[0228] For example, in order to prevent photoresist residues from being formed in the first opening 1 b 1 after development, the first photoresist pattern layer 1 b may be subjected to a debonding treatment, such as a plasma treatment, after development.
[0229] Step S43: Electroplating is performed at the first window 1b1 to form a first target coating 135 covering the first portion 1341. Exemplarily, the thickness of the first target coating 135 ranges from 9 to 27 micrometers. For example, the thickness of the first target coating 135 is 10 micrometers, 12 micrometers, 15 micrometers, or 20 micrometers.
[0230] Step S44: stripping the first photoresist pattern layer 1 b to expose the second portion 1342 .
[0231] Step S45 : etching and removing the second portion 1342 to obtain a first metal circuit layer 133 formed by the first portion 1341 and the first target plating layer 135 .
[0232] Although there is a step of etching away the second part 1342 in the processing technology of the first metal circuit layer 133, since the third metal layer 134 is used as a seed layer to facilitate the coating on the third metal layer 134, the thickness of the third metal layer 134 is relatively small, generally 1 to 3 microns. Therefore, compared with the tenting process mentioned above, the etching here has less effect on the line spacing size of the first metal circuit layer 133. Therefore, the use of the MSAP process to make the first metal circuit layer 133 is conducive to reducing the size of the first line gap 1332 of the first metal circuit layer 133, which is conducive to the high density of the first metal circuit layer 133. In addition, the cross section of the first routing 1331 of the first metal circuit layer 133 will not have the problem of inconsistent width of the cross section of the first routing 1331 of the tenting process. On this basis, the use of the MSAP process to make the first metal circuit layer 133 is conducive to reducing the line width of the first metal circuit layer 133, and the circuit electrical performance is better.
[0233] It is understandable that when the second prepreg structure 20b includes the second metal circuit layer 233, the specific processing method of the second metal circuit layer 233 can also refer to the MSAP process described above, which will not be described in detail here. Fig.18 , Fig.18 It is a schematic diagram of the cross-sectional structure of the second carrier composite structure 20 obtained by processing the second metal circuit layer 233 by using the MSAP process.
[0234] See also Fig.19 , Fig.19 To adopt Fig.17 The first carrier composite structure 10 shown and the Fig.18FIG. 1 is a schematic diagram of a processing process of a coreless substrate of a second carrier composite structure 20 . Fig.19 (a1) in is Fig.17 The structure obtained in step S45. Fig.19 (a2) in is Fig.18 In addition, in the third stacking structure obtained after step S40, Fig.19 As shown in (e) in FIG. 1 , the first metal seed layer 136 and the second metal seed layer 236 are located at two ends of the third stacking structure along its thickness direction.
[0235] Based on this, in order to realize the electrical connection between each circuit layer of the coreless substrate, the processing method of the coreless substrate also includes the following steps:
[0236] S50: Drilling the first metal layer 131 and the first dielectric structure to form a first through hole 106; wherein the first through hole 106 penetrates the first dielectric structure, the first metal seed layer 136 and the second target plating layer 138. Drilling the second metal layer 231 and the second dielectric structure to form a second through hole 107. wherein the second through hole 107 penetrates the second dielectric structure, the second metal seed layer 236 and the third target plating layer 238. In this way, it can be obtained Fig.19 The structure shown in (f) in FIG. 1 is a schematic diagram of the structure of FIG. 1. The first through hole 106 and the second through hole 107 do not penetrate the central circuit layer 105. The first through hole 106 is provided to facilitate the subsequent in-hole metallization to achieve electrical connection between the central circuit layer 105 and the first metal layer 131. The second through hole 107 is provided to facilitate the subsequent in-hole metallization to achieve electrical connection between the central circuit layer 105 and the second metal layer 231.
[0237] For example, the first through hole 106 and the second through hole 107 may be prepared by laser or laser process.
[0238] Exemplarily, in order to prevent resin residues in the first through hole 106 and the second through hole 107 after drilling, a degumming step may be provided between step S50 and step S60, that is, degumming treatment, such as plasma treatment, is performed on the first through hole 106 and the second through hole 107.
[0239] S60: forming a conductive layer on the hole wall of the first through hole 106 and the second through hole 107. Exemplarily, the conductive layer may also be a metal layer, for example, formed on the hole wall of the first through hole 106 and the second through hole 107 by chemical plating or sputtering. The provision of the conductive layer can facilitate the deposition of a plated layer on the conductive layer in the subsequent electroplating process. Thus, the following can be obtained: Fig.19 The structure shown in (g) in FIG.
[0240] S70: Electroplating is performed at the first through hole 106 to form a first metal conductive portion 108 filling the first through hole 106. At the same time, electroplating is performed at the second through hole 107 to form a second metal conductive portion 109 filling the second through hole 107. Thus, the following can be obtained: Fig.19 The structure shown in (h) in FIG. 1 is a schematic diagram of a structure in which the first metal conductive part 108 is connected to the first metal layer 131 and the central circuit layer 105 respectively. The second metal conductive part 109 is connected to the second metal layer 231 and the central circuit layer 105 respectively.
[0241] S80: Etching and removing the entire first metal seed layer 136 to obtain the first circuit layer 103 formed by the second target plating layer 138. Etching and removing the entire second metal seed layer 236 to obtain the second circuit layer 102 formed by the third target plating layer 238. Fig.19 The structure shown in (i) in FIG.
[0242] In this way, by first making the second target coating 138 on the first temporary carrier 11, when the first carrier structure 10a and the first semi-cured sheet structure 10b are pressed together, it is conducive to the second target coating 138 to be embedded in the first semi-cured sheet 132, and by making the second target coating 138 on the second temporary carrier 21, when the second carrier structure 20a and the second semi-cured sheet structure 20b are pressed together, it is conducive to the second target coating 138 to be embedded in the second semi-cured sheet 232, so that after etching away the first metal seed layer 136 and the second metal seed layer 236, the exposed first circuit layer 103 is embedded in the first dielectric structure, and the exposed second circuit layer 102 is embedded in the second dielectric structure, which is conducive to reducing the thickness of the coreless substrate and achieving further thinning of the coreless substrate.
[0243] The above article introduces the processing of a three-layer coreless substrate. Based on any of the above embodiments, when a five-layer, seven-layer or nine-layer coreless substrate needs to be processed, the processing can be performed on the basis of the above three-layer coreless substrate. The following takes the processing of a five-layer substrate as an example for explanation.
[0244] See also Fig. 20 , Fig. 20 A schematic diagram of a processing process of a coreless substrate provided in a fifth embodiment of the present application. The processing method of the coreless substrate comprises the following steps:
[0245] Step S100: Provide a three-layer coreless substrate having three circuit layers. The three-layer coreless substrate may be composed of Figure 3-Figure 19 The centerless substrate is processed by the processing method of any one of the embodiments.
[0246] Step S200: symmetrically hot-pressing a third semi-cured structure on the surface of the first circuit layer 103 and the surface of the second circuit layer 102 of the three-layer coreless substrate. The third semi-cured structure includes a third semi-cured sheet 432 and a fifth metal layer 433. The third semi-cured sheet 432 is between the fifth metal layer 433 and the three-layer coreless substrate.
[0247] Step S300: drilling holes in the fifth metal layer 433 and the portion between the fifth metal layer 433 and the three-layer coreless substrate, forming a conductive layer in the hole, and electroplating a metal conductive portion in the hole. The drilling step in this step can refer to step S50 in the above text, the conductive layer in the hole can refer to step S60 in the above text, and the electroplating of the metal conductive portion in the hole can refer to step S70 in the above text. All of them will not be repeated here.
[0248] Step S400: patterning the fifth metal layer 433 to form the fifth circuit layer 1010. The specific processing technology of patterning the fifth metal layer 433 to form the fifth circuit layer 1010 can refer to the first metal circuit layer 133 mentioned above, which will not be repeated here.
[0249] At this point, a five-layer coreless substrate can be obtained.
[0250] It is worth noting that when more coreless substrates with odd layers are needed, the operations from step S100 to step S400 may be repeated after step S400.
[0251] It is worth noting that after the required circuit layer of the coreless substrate is manufactured, a solder resist layer may be covered on the surface circuit layer of the coreless substrate to improve the insulation of the surface of the coreless substrate.
[0252] In addition to the processing method of the coreless substrate described above, some embodiments of the present application further provide a coreless substrate. The coreless substrate can be processed by any processing method of the coreless substrate described above.
[0253] Next, the structure of the coreless substrate will be described.
[0254] See also Fig.21 , Fig.21 To adopt Fig. 9 The cross-sectional structure diagram of the coreless substrate 100 processed by the processing method of the coreless substrate 100 is shown. Specifically, the coreless substrate 100 includes: a first fiber cloth 132c, a second fiber cloth 232c and an intermediate layer structure 101.
[0255] The first fiber cloth 132c and the second fiber cloth 232c are stacked and arranged, and the intermediate layer structure 101 is arranged between the first fiber cloth 132c and the second fiber cloth 232c.
[0256] The intermediate layer structure 101 includes an adhesive layer 1011 and a central circuit layer 105. The adhesive layer 1011 includes a first adhesive layer 10111, a filling adhesive portion 10113, and a second adhesive layer 10112 stacked in sequence. The first adhesive layer 10111 is bonded to the first fiber cloth 132c, and the second adhesive layer 10112 is bonded to the second fiber cloth 232c. The central circuit layer 105 and the filling adhesive portion 10113 are integrally fixed and connected between the first adhesive layer 10111 and the second adhesive layer 10112. The central circuit layer 105 is embedded in the filling adhesive portion 10113.
[0257] In this way, the additionally provided filling glue part 10113 fills the line gap of the central line layer 105. Compared with the method of not providing the filling glue part 10113 but using the first glue layer 10111 and / or the second glue layer 10112 to fill the line gap of the central line layer 105, this method is helpful to avoid the problem that the size between the central line layer 105 and the first fiber cloth 132c and / or the size between the central line layer 105 and the second fiber cloth 232c is too small due to the first glue layer 10111 and / or the second glue layer 10112 filling the line gap of the central line layer 105, or even causing the fiber cloth to directly contact the central line layer 105, and cracks appearing due to the contact and extrusion of the hot-pressed cured fiber cloth with the central line layer 105 during the processing of the coreless substrate 100, which is helpful to ensure the yield of the coreless substrate 100. On the other hand, it is beneficial for the distance d2 between the central circuit layer 105 and the second fiber cloth 232c and the distance d1 between the central circuit layer 105 and the first fiber cloth 132c to be equal, which can help improve the symmetry of the coreless substrate 100 with the central circuit layer 105 as the center, and then can help reduce or eliminate the difference in thermal expansion coefficients on both sides of the thickness direction of the central circuit layer 105, avoid the warping deformation problem of the coreless substrate 100, and improve the flatness of the coreless substrate 100.
[0258] Specifically, the distance d2 between the central circuit layer 105 and the second fiber cloth 232c and the distance d1 between the central circuit layer 105 and the first fiber cloth 132c are equal. Therefore, the difference in the thermal expansion coefficient of the parts on both sides of the thickness direction of the central circuit layer 105 can be reduced or eliminated, the warping deformation problem of the coreless substrate 100 is avoided, and the flatness of the coreless substrate 100 is improved.
[0259] In some embodiments, the first adhesive layer 10111 includes a first resin substrate and a first filler distributed in the first resin substrate. The first resin substrate is formed by curing a portion of the first resin matrix described above. The first filler can play a role in heat conduction, enhancing the structural strength of the first resin matrix, and reducing the thermal expansion coefficient of the first adhesive layer 10111. The materials of the first filler and the first resin matrix can be found in the above text and will not be repeated here.
[0260] The filling glue part 10113 includes a third resin base material and a third filler distributed in the third resin base material. Specifically, the third filler is evenly distributed in the third resin base material. The third filler can play the role of heat conduction, enhancing the structural strength of the third resin base material and reducing the thermal expansion coefficient of the filling glue part 10113.
[0261] The material of the third resin substrate is the same as that of the first resin substrate. In this way, during the processing of the coreless substrate 100, it is helpful to ensure that the hot pressing temperature of the third resin substrate and the first resin substrate is consistent, thereby simplifying the processing technology.
[0262] For example, the third filler can be in the form of particles, which are easier to be evenly distributed in the filling glue part 10113, thereby making the composition of the filling glue part 10113 more uniform and improving the uniformity of each part of the filling glue part 10113 in terms of heat conduction, structural strength and thermal expansion coefficient.
[0263] Exemplarily, in order to further improve the thermal conductivity and structural strength of the filling glue part 10113 and further reduce the thermal expansion coefficient of the filling glue part 10113, the mass percentage of the third filler in the filling glue part 10113 is greater than the mass percentage of the first filler in the first glue layer 10111.
[0264] Exemplarily, the mass percentage of the third filler in the insulating filling glue 132 a 1 is greater than the mass percentage of the first filler in the first adhesive layer 132 b by 1%, 2%, 3%, 4% or 5%.
[0265] See also Fig. 22 , Fig. 22 Based on Fig.13 The cross-sectional view of the coreless substrate 100 processed by the processing method of the coreless substrate 100 is shown. Specifically, the central circuit layer 105 includes a first metal circuit layer 133 and a second metal circuit layer 233 .
[0266] The first metal circuit layer 133 includes a plurality of first routing lines 1331. The plurality of first routing lines 1331 are spaced apart to form a first circuit gap 1332 of the first metal circuit layer 133. The second metal circuit layer 233 includes a plurality of second routing lines 2331, and the plurality of second routing lines 2331 are spaced apart to form a second circuit gap 2332 of the second metal circuit layer 233. At least a portion of the second routing lines 2331 is located in the first circuit gap 1332 and is spaced apart from the first routing lines 1331. In the direction from the first fiber cloth 132c to the second fiber cloth 232c. The cross-sectional area of the first routing lines 1331 is gradually reduced. The cross-sectional area of the second routing lines 2331 is gradually increased. As a result, it is beneficial to reduce the circuit spacing of the central circuit layer 105, improve the circuit density of the central circuit layer 105, and realize the high density of the central circuit layer 105.
[0267] The specific application scenarios of the coreless substrate 100 are described in detail below.
[0268] The present application provides an electronic device, which is a type of electronic device having a circuit board. Specifically, the electronic device includes but is not limited to mobile phones, tablet personal computers, laptop computers, personal digital assistants (PDAs), personal computers, notebook computers, vehicle-mounted devices, wearable devices, and other electronic devices.
[0269] See also Fig.23 and Fig.24 , Fig.23 A perspective view of an electronic device 500 provided in some embodiments of the present application, Fig.24 for Fig.23 The electronic device 500 is an exploded schematic diagram of the electronic device 500. In this embodiment, the electronic device 500 is a mobile phone. The electronic device 500 includes a housing 501, a main circuit board 502, a secondary circuit board 503, a display screen 504 and a battery 505.
[0270] It should be noted that Fig.23 and Fig.24 Only some components of the electronic device 500 are schematically shown, and the actual shapes, sizes, positions, and structures of these components are not subject to the present invention. Fig.23 and Fig.24 limitation.
[0271] In order to facilitate the description of the following embodiments, an XYZ coordinate system is established for the electronic device 500. Specifically, the width direction of the electronic device 500 is defined as the X-axis direction, the length direction of the electronic device 500 is defined as the Y-axis direction, and the thickness direction of the electronic device 500 is defined as the Z-axis direction. It is understandable that the coordinate system setting of the electronic device 500 can be flexibly set according to actual needs, and is not specifically limited here.
[0272] The housing 501 is used to protect the internal circuit components of the electronic device 500. Figure 2 The housing 501 includes a front cover 5013 , a frame 5012 and a back cover 5011 .
[0273] Specifically, the front cover plate 5013 is in the shape of a flat plate. The front cover plate 5013 is a light-transmitting member. The material of the front cover plate 5013 includes but is not limited to glass, plastic and ceramic.
[0274] The rear cover 5011 is stacked and spaced apart from the front cover 5013. The rear cover 5011 is in the shape of a flat plate. The material of the rear cover 5011 includes but is not limited to metal and plastic.
[0275] The frame 5012 is located between the front cover plate 5013 and the back cover 5011, and is arranged around the edges of the front cover plate 5013 and the back cover 5011. Exemplarily, the frame 5012 can be fixedly connected to the back cover 5011 by gluing. The frame 5012 can also be an integrally formed structure with the back cover 5011, that is, the frame 5012 and the back cover 5011 are an integral structure. The front cover plate 5013 is fixed on the frame 5012. In some embodiments, the front cover plate 5013 can be fixed on the frame 5012 by gluing. The material of the frame 5012 includes but is not limited to metal and plastic.
[0276] The front cover 5013, the back cover 5011 and the frame 5012 form an internal storage space of the electronic device 500. The internal storage space stores the display screen 504, the main circuit board 502, the auxiliary circuit board 503 and the battery 505.
[0277] The display screen 504 is located between the front cover plate 5013 and the rear cover 5011, and is fixed to the front cover plate 5013. Exemplarily, the display screen 504 is fixed to the front cover plate 5013 by gluing. The display screen 504 is used to display images, videos, and the like.
[0278] The main circuit board 502 includes a circuit substrate and electronic devices disposed on the circuit substrate. For example, the main circuit board 502 can be fixed to the display screen 504 by means of threaded connection, snap connection, etc. Specifically, the main circuit board 502 can be fixed to the surface of the display screen 504 facing the rear cover 5011. In other embodiments, please refer to Fig.24, the electronic device 500 also includes a middle plate 5014. The middle plate 5014 is fixed to the inner surface of the frame 5012 and is between the display screen 504 and the back cover 5011. Exemplarily, the middle plate 5014 can be fixed to the frame 5012 by welding, clamping or gluing. The middle plate 5014 can also be an integrally formed structure with the frame 5012. The middle plate 5014 serves as the structural "skeleton" of the electronic device 500, and the main circuit board 502 can be fixed to the side surface of the middle plate 5014 facing the back cover 5011 by means of threaded connection, clamping, welding, etc.
[0279] Exemplarily, the electronic device on the main circuit board 502 is a control chip. The control chip may be, for example, an application processor (AP), a double data rate synchronous dynamic random access memory (DDR), and a universal flash storage (UFS). In some embodiments, the main circuit board 502 is electrically connected to the display screen 504, and the main circuit board 502 is used to control the display screen 504 to display images or videos.
[0280] In some embodiments, the circuit substrate of the main circuit board 502 may be a coreless substrate 100. This helps reduce the thickness of the main circuit board 502 and achieves a thinner and lighter electronic device 500. In other examples, the circuit substrate of the main circuit board 502 may also be a rigid circuit board.
[0281] The auxiliary circuit board 503 includes a circuit substrate and electronic components arranged on the circuit substrate. Exemplarily, the electronic components on the auxiliary circuit board 503 may include electronic components such as an antenna (such as a 5G antenna) radio frequency front end, a universal serial bus (USB) device, and an oscillator.
[0282] In some embodiments, the circuit substrate of the auxiliary circuit board 503 may be a coreless substrate 100. This helps reduce the thickness of the auxiliary circuit board 503 and achieves a thinner and lighter electronic device 500. In other examples, the circuit substrate of the auxiliary circuit board 503 may also be a rigid circuit board.
[0283] The auxiliary circuit board 503 is arranged with the main circuit board 502 in the Y-axis direction. The auxiliary circuit board 503 can be fixed to the surface of the middle plate 5014 facing the rear cover 5011. Specifically, the auxiliary circuit board 503 can be fixed to the surface of the middle plate 5014 facing the rear cover 5011 by means of threaded connection, clamping, gluing or welding. In other examples, when the electronic device 500 does not include the middle plate 5014, the auxiliary circuit board 503 can also be fixed to the surface of the display screen 504 facing the rear cover 5011.
[0284] The auxiliary circuit board 503 is electrically connected to the main circuit board 502 through a connection structure (not shown) to achieve data and signal transmission between the auxiliary circuit board 503 and the main circuit board 502. Exemplarily, the connection structure can be a flexible circuit board. Further, when the connection structure is a flexible circuit board, exemplarily, the flexible circuit board is the coreless substrate 100 mentioned above.
[0285] Please continue reading Fig.24 , a battery compartment a is provided in the housing 501. The battery compartment a is used to accommodate the battery 505. The battery compartment a is located between the main circuit board 502 and the auxiliary circuit board 503. Specifically, the battery compartment a is a groove provided on the surface of the middle plate 5014 facing the rear cover 5011. In some other embodiments, when the middle plate 5014 is not provided in the electronic device 500, the battery compartment a is provided in the housing 501. Fig.24 The display screen 504 forms the bottom wall of the battery compartment a, and the main circuit board 502, the auxiliary circuit board 503 and the frame 5012 form the side walls of the battery compartment a. No specific limitation is made here.
[0286] The battery 505 is installed in the battery compartment a, and the battery 505 is used to provide power to the display screen 504, the main circuit board 502 and the auxiliary circuit board 503 in the electronic device 500.
[0287] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.
[0288] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.
Claims
1. A method for processing a coreless substrate, characterized in that: The steps include: A first carrier composite structure and a second carrier composite structure are provided respectively; wherein the first carrier composite structure comprises a first temporary carrier, a first release layer and a first composite layer structure which are stacked in sequence, the first composite layer structure comprises a first prepreg and a first metal circuit layer, the first prepreg has a first surface away from the first temporary carrier, the first metal circuit layer is arranged on the first surface, the second carrier composite structure comprises a second temporary carrier, a second release layer and a second composite layer structure which are stacked in sequence, the second composite layer structure comprises a second prepreg, the second prepreg has a second surface away from the second temporary carrier; Disposing a liquid or semi-cured insulating filling glue on the first surface and / or on the second surface; The second surface is directed toward the first surface, and the first carrier composite structure and the second carrier composite structure are stacked; The stacked first carrier composite structure and the second carrier composite structure are subjected to a hot pressing curing process, so that the insulating filling glue fills the circuit gap of the central circuit layer between the first prepreg and the second prepreg, and is cured into a filling glue portion; wherein the central circuit layer includes the first metal circuit layer; The first temporary carrier and the first release layer, as well as the second temporary carrier and the second release layer are peeled off and removed.
2. The method for processing a coreless substrate according to claim 1, wherein: The second composite layer structure further includes a second metal circuit layer, and the second metal circuit layer is disposed on the second surface; In the step of facing the second surface toward the first surface and stacking the first carrier composite structure and the second carrier composite structure, the second wiring of the second metal wiring layer is spaced apart from the first wiring of the first metal wiring layer in a direction perpendicular to the second surface, and at least a portion of the second wiring of the second metal wiring layer is located in the first wiring gap of the first metal wiring layer; wherein the first metal wiring layer and the second metal wiring layer as a whole form a central wiring layer between the first semi-cured sheet and the second semi-cured sheet.
3. The method for processing a coreless substrate according to claim 2, wherein: In the step of placing the second surface toward the first surface and stacking the first carrier composite structure and the second carrier composite structure, at least a portion of the first wiring of the first metal wiring layer is located in the second wiring gap of the second metal wiring layer.
4. The method for processing a coreless substrate according to claim 1, wherein: The first metal circuit layer forms a central circuit layer between the first prepreg and the second prepreg.
5. The method for processing a coreless substrate according to any one of claims 1 to 4, characterized in that: The first prepreg sheet includes a first adhesive layer and a first fiber cloth, the first adhesive layer is in a semi-cured state, and the first fiber cloth is embedded in the first adhesive layer.
6. The method for processing a coreless substrate according to claim 5, characterized in that: The first adhesive layer includes a first resin matrix and a first filler distributed in the first resin matrix; The insulating filling glue comprises a third resin matrix and a third filler distributed in the third resin matrix; The mass percentage of the third filler in the insulating filling glue is greater than the mass percentage of the first filler in the first adhesive layer; and / or the third resin matrix and the first resin matrix are made of the same material.
7. The method for processing a coreless substrate according to any one of claims 1 to 5, characterized in that: The insulating filling adhesive includes a third resin matrix and a third filler distributed in the third resin matrix.
8. The method for processing a coreless substrate according to any one of claims 1 to 7, characterized in that: The first semi-cured sheet includes a first adhesive layer and a first fiber cloth, the first adhesive layer is in a semi-cured state, the first fiber cloth is embedded in the first adhesive layer, the first adhesive layer includes a first resin matrix, and the material of the first resin matrix includes epoxy resin and / or bismaleimide.
9. The method for processing a coreless substrate according to any one of claims 1 to 8, characterized in that: The first prepreg and the second prepreg are identical.
10. The method for processing a coreless substrate according to any one of claims 1 to 9, characterized in that: The first carrier composite structure further includes a first metal layer, and the first metal layer is stacked between the first prepreg and the first release layer; The processing method of the coreless substrate includes a processing method of the first carrier composite structure, and the processing method of the first carrier composite structure includes: Providing a first carrier structure and a first prepreg structure; wherein the first carrier structure comprises the first temporary carrier, the first release layer and the first metal layer stacked in sequence; the first prepreg structure comprises the first prepreg and a third metal layer stacked, the third metal layer being disposed on the first surface; Directing the surface of the first prepreg opposite to the first surface toward the first metal layer, and stacking the first prepreg structure and the first carrier structure; Performing a lamination process on the first prepreg structure and the first carrier structure; The third metal layer is patterned to form the first metal circuit layer.
11. The method for processing a coreless substrate according to claim 10, characterized in that: The patterning of the third metal layer to form the first metal circuit layer specifically includes: forming a first photoresist layer on a surface of the third metal layer away from the first semi-cured layer; Expose and develop the first photoresist layer to form a first photoresist pattern layer, wherein the first photoresist pattern layer has a first window, and the third metal layer includes a first portion exposed at the first window and a second portion covered by the first photoresist pattern layer; Etching and removing the first portion to obtain the first metal circuit layer formed by the second portion; The first photoresist pattern layer is stripped off.
12. The method for processing a coreless substrate according to claim 10, wherein: The patterning of the third metal layer to form the first metal circuit layer specifically includes: forming a first photoresist layer on a surface of the third metal layer away from the first semi-cured layer; Expose and develop the first photoresist layer to form a first photoresist pattern layer, wherein the first photoresist pattern layer has a first window, and the third metal layer includes a first portion exposed at the first window and a second portion covered by the first photoresist pattern layer; Electroplating at the first opening to form a first target coating; Stripping off the first photoresist pattern layer to expose the second portion; The second portion is removed by etching to obtain the first metal circuit layer formed by the first portion and the first target plating layer.
13. The method for processing a coreless substrate according to any one of claims 10 to 12, characterized in that: The processing method of the coreless substrate includes a processing method of the first carrier structure; The processing method of the first carrier structure comprises: The first release layer and the first metal seed layer are arranged on the first temporary carrier; wherein the first metal seed layer is arranged on the surface of the first release layer away from the first temporary carrier; forming a second photoresist layer on a surface of the first metal seed layer away from the first temporary carrier; Expose and develop the second photoresist layer to form a second photoresist pattern layer, wherein the second photoresist pattern layer has a second window, and the first metal seed layer includes a first seed portion exposed in the second window and a second seed portion covered by the second photoresist pattern layer; Electroplating at the second opening to form a second target plating layer covering the first seed portion; Stripping the second photoresist pattern layer to expose the second seed portion, so as to obtain the first metal layer formed by the second target plating layer and the first metal seed layer; After the step of peeling off the first temporary carrier and the first release layer, and the second temporary carrier and the second release layer, the method further includes: The entire first metal seed layer is removed by etching to obtain a first circuit layer formed by the second target plating layer.
14. The method for processing a coreless substrate according to claim 13, characterized in that: After the step of stripping and removing the first temporary carrier and the first release layer, and the second temporary carrier and the second release layer, and before the step of etching and removing the entire first metal seed layer to obtain a first circuit layer formed by the second target plating layer, The processing method of the coreless substrate also includes: The first metal layer and the first dielectric structure are drilled to form a first through hole; wherein the first through hole penetrates the first metal layer and the first dielectric structure; the first dielectric structure is formed by hot pressing and curing the first prepreg, A first metal conductive portion is formed in the first through hole, and the first metal conductive portion is connected to the first metal layer and the central circuit layer respectively; wherein the central circuit layer includes the first metal circuit layer.
15. A coreless substrate, characterized in that: The coreless substrate is processed by the processing method of a coreless substrate according to any one of claims 1 to 14.
16. A coreless substrate, characterized in that: include: A first fiber cloth and a second fiber cloth, wherein the first fiber cloth and the second fiber cloth are stacked; An intermediate layer structure, the intermediate layer structure is arranged between the first fiber cloth and the second fiber cloth, the intermediate layer structure comprises an adhesive layer and a central line layer, the adhesive layer comprises a first adhesive layer, a filling adhesive portion, and a second adhesive layer stacked in sequence, wherein the first adhesive layer is bonded to the first fiber cloth, the second adhesive layer is bonded to the second fiber cloth, the central line layer and the filling adhesive portion are integrally fixed and connected between the first adhesive layer and the second adhesive layer, and the central line layer is embedded in the filling adhesive portion; The first adhesive layer includes a first resin matrix and a first filler distributed in the first resin matrix; The filling glue part includes a third resin matrix and a third filler distributed in the third resin matrix; Wherein, the mass percentage of the third filler in the filling glue portion is greater than the mass percentage of the first filler in the first glue layer.
17. The coreless substrate according to claim 16, characterized in that: The distance between the central wiring layer and the second fiber cloth is equal to the distance between the central wiring layer and the first fiber cloth.
18. The coreless substrate according to claim 16 or 17, characterized in that: The material of the third resin substrate is the same as that of the first resin substrate.
19. The coreless substrate according to any one of claims 16 to 18, characterized in that: The central circuit layer includes a first metal circuit layer and a second metal circuit layer, the first metal circuit layer includes a plurality of first routing lines, the plurality of first routing lines are spaced apart to form a first circuit gap of the first metal circuit layer, the second metal circuit layer includes a plurality of second routing lines, the plurality of second routing lines are spaced apart to form a second circuit gap of the second metal circuit layer, at least a portion of the second routing lines is located in the first circuit gap and is spaced apart from the first routing lines; Wherein, in the direction from the first fiber cloth to the second fiber cloth, the cross-sectional area of the first wiring gradually decreases, and the cross-sectional area of the second wiring gradually increases.
20. A circuit board, characterized in that: include: The coreless substrate according to any one of claims 15 to 19; and An electronic device is fixed on the coreless substrate.
21. The circuit board according to claim 20, characterized in that: The circuit board is a main circuit board and / or a sub-circuit board of the electronic device.
22. An electronic device, characterized in that: include: shell; According to the circuit board according to claim 20 or 21, the circuit board is arranged in the housing.
Citation Information
Patent Citations
Metal wire layout structure on insulation layer and preparation method thereof
CN103874322A
Manufacturing method of circuit board
CN109769338A
Method of manufacturing wiring board
JP2013118301A
Circuit board and method for fabricating the same
TW200711077A
KR20190087032A