一种镍铁微硫化的资源化提取方法

By using micro-sulfurization smelting and oxidative acid leaching methods, the problems of low iron utilization and high energy consumption in nickel-iron extraction have been solved, realizing the high-value utilization of nickel-iron, reducing energy consumption, providing an environmentally friendly production process, and supporting the new energy industry.

CN117737405BActive Publication Date: 2026-07-17CENT SOUTH UNIV

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
CENT SOUTH UNIV
Filing Date
2023-12-21
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing nickel-iron extraction processes suffer from low iron utilization, high energy consumption, and severe environmental pollution, making it difficult to achieve high-value utilization of nickel-iron.

Method used

A method combining micro-sulfurization smelting and oxidative acid leaching was adopted. Micro-sulfurization smelting was carried out by mixing nickel-iron, sulfiding agent and slag-forming agent, followed by crushing, oxidative acid leaching, and finally roasting to separate nickel and iron, so as to prepare high-purity nickel sulfate and iron phosphate.

Benefits of technology

This technology enables efficient separation of nickel and iron, reduces the difficulty of nickel-iron processing, decreases energy consumption, makes production more environmentally friendly, provides a high-value utilization pathway, and supports the development of the new energy industry.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117737405B_ABST
    Figure CN117737405B_ABST
Patent Text Reader

Abstract

一种镍铁微硫化的资源化提取方法,包括以下步骤:(1)将镍铁、硫化剂和造渣剂混合配料,微硫化熔炼,得含硫镍铁、熔渣和烟气;(2)将所述含硫镍铁破碎,氧化酸浸,固液分离,得浸出液和浸出渣;(3)从所述浸出液中收集镍元素;所述浸出渣焙烧得磷酸铁。本发明通过微硫化熔炼,获得比较容易粉碎的含硫镍铁,降低镍铁的处理难度,镍铁利用率高;创新性采用氧化酸浸的方法处理含硫镍铁,实现镍铁的高值化利用;本发明相对于现有技术,所需熔炼时间减少,明显降低能耗,生产更加环保,所得产品可用于制备电池,为新能源产业发展提供支撑。
Need to check novelty before this filing date? Find Prior Art