Equipment and method for enhancing anti-seepage performance of permeable area of ​​earth dam

Through the melting characteristics of phase change materials and active pressure grouting, the weak interlayer area of ​​the dam is cemented, which solves the problem of high cost and long time of anti-seepage reinforcement in the permeable area of ​​the dam, shortening the construction period and improving efficiency, and is suitable for a variety of applications Leakage situation.

CN118007579BActive Publication Date: 2024-10-11NANJING HYDRAULIC RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410253164.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-06
Publication Date
2024-10-11
Estimated Expiration
2044-03-06

AI Technical Summary

Technical Problem

The anti-seepage performance strengthening methods in the permeable areas of existing dams are relatively time-consuming, long in construction time, high in cost, difficult to predict, and poorly targeted.

Method used

Equipment including material phase change kettles, heated and insulated conveying pipes, pumping devices and grouting devices are used to cement the soil particles in the weak interlayer area through the melting characteristics of the phase change material and the active pressure grouting method, and use surface modifiers Improve the rheological properties of the slurry and predict the construction period through neural networks.

Benefits of technology

It achieves a short construction period, less consumption, less disturbance to the surrounding soil, improves the grouting efficiency, is suitable for parts where leakage is occurring or has already occurred, and expands the scope of application.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118007579B_ABST
    Figure CN118007579B_ABST
Patent Text Reader

Abstract

The present invention discloses an anti-seepage performance enhancement device and method for the permeable area of ​​an earthen dam, and relates to the technical field of dam reinforcement. Compared with the previous anti-seepage performance enhancement methods, the present invention improves the problems of the current anti-seepage performance reinforcement methods, such as high cost, long construction time, and difficulty in prediction, high cost, and poor pertinence. The fusion characteristics of phase change materials and active pressurized grouting are used to achieve the purpose of using phase change materials to bond soil particles in the weak interlayer area and enhance the local anti-seepage capacity of the dam. The method has a short construction period and low cost, and has little disturbance to the surrounding soil. The composite phase change material is prepared by surface modifiers and the like to improve the rheological properties of the slurry, greatly improve the grouting efficiency, and further shorten the construction period. At the same time, the construction period is predicted by a neural network to provide data support; and the present invention is also applicable to parts that are leaking or have already leaked, and has a wide range of applications.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of dam reinforcement, and in particular to equipment and methods for enhancing the anti-seepage performance of a permeable area of ​​an earth dam. Background Art

[0002] Levees are an important line of defense against floods and waterlogging disasters, and are also a lifeline for protecting people's lives and property. However, poor filling during construction, rotten roots left by plant growth, and ant nests formed by animal activities can all become weak and permeable areas of the levee. After the water level rises during the flood season, these weak and permeable areas are very likely to develop into leakage channels, endangering the safety of the levee. Therefore, the permeable areas of the levee need to be treated promptly and effectively to improve their anti-seepage performance.

[0003] At present, the commonly used methods for improving anti-seepage performance are mostly construction methods such as pouring anti-seepage walls and grouting. For example, patent CN202321472661.5 discloses a high-pressure rotary jet pile anti-seepage wall structure, patent CN202110847263.6 discloses a grouting device for the construction of dam anti-seepage curtains; patent CN201910760855.7 discloses a self-setting mortar and its dam anti-seepage reinforcement method. However, the current anti-seepage performance reinforcement methods have shortcomings such as high cost, long and unpredictable construction time, high cost, and poor pertinence.

[0004] In order to solve the above problems, the present invention proposes a device and method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam. Summary of the invention

[0005] The purpose of the present invention is to propose a device and method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam to solve the problems raised in the background technology:

[0006] The current anti-seepage reinforcement methods have problems such as high cost, long and unpredictable construction time, high cost, and poor targeting.

[0007] In order to achieve the above object, the present invention adopts the following technical solutions:

[0008] Equipment and method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam, including: a material phase change kettle, a heating and heat-insulating conveying pipe, a pumping device, and a grouting device;

[0009] The material phase change kettle is a cylindrical structure, which is used to provide a storage and reaction environment for the material, and includes a multi-layer cylinder, a temperature control module, a stirring module and a gate valve;

[0010] The heating and heat-insulating delivery pipe is used to ensure that the phase change material is delivered in liquid form, and includes an inner layer, a heating wire, a temperature controller, a heat-insulating layer, and an insulating sleeve;

[0011] The pumping device is used to provide power for the transmission of phase change materials, and includes a screw pump and an auxiliary heat device;

[0012] The grouting device is used for grouting and comprises a flower pipe grouting head and a sealing device.

[0013] Preferably, the multilayer cylinder in the material phase change kettle is used for material storage and phase change; the multilayer cylinder comprises a heat generating layer, a heat insulating layer 1, a structural layer and a heat insulating layer 2 from the innermost side to the outermost side;

[0014] The heat generating layer is made of iron material with a thickness of 0.2 mm to 2 mm; the heat insulating layer 1 is made of aerogel material to prevent heat loss from the heat generating layer; the structural layer is a material phase change kettle skeleton, with an electromagnetic coil laid inside, and the electromagnetic coil is a mica high-temperature wire, which is wound on the side and bottom of the heat insulating layer 1; the heat insulating layer 2 is made of hard plastic material and is the outer shell of the multi-layer cylinder body, which is used to protect the internal structure;

[0015] The temperature control module is used to control the heating temperature of the material phase change kettle, and includes an electromagnetic coil, a rectifier, a temperature sensor and a control module; the electromagnetic coil is a coil laid in the structural layer of the material phase change kettle, and its structure is a copper core wire and a high-temperature resistant glass fiber sleeve on the outside, and mica and silica gel are filled between the copper core wire and the high-temperature resistant glass fiber sleeve; the rectifier is used to convert conventional mains electricity into high-frequency high-voltage electricity, and then transmit it to the electromagnetic coil; the temperature sensor is installed inside the material phase change kettle to monitor the temperature of the internal phase change material; the control module controls the rectifier to work based on the set temperature and the data monitored and sent back by the temperature sensor to control the heating temperature;

[0016] The stirring module is used to mix the phase change material melted into liquid evenly, and includes a lifting platform, a motor, a transmission rod and a dispersion plate; the motor is installed on the top of the lifting platform, and the transmission rod connects the motor and the dispersion plate; the lifting platform controls the lifting to realize the action of lifting the dispersion plate and dropping it into the material phase change kettle; the rotation of the motor drives the dispersion plate to rotate to realize the stirring function;

[0017] The gate valve is installed at the bottom of the side wall of the material phase change kettle and is used to control the transmission of the material; one end of the gate valve is connected to the material phase change kettle, and the other end is connected to the heating and insulation conveying pipe.

[0018] Preferably, the inner layer of the heating and heat-insulating conveying pipe is a hose made of stainless steel wire; the heating wire is a nickel-chromium alloy, which generates heat when powered on; the temperature controller includes a temperature probe and a heating module, the temperature probe is installed in the inner layer to monitor the fluid temperature inside the equipment, the heating module is connected to the heating wire, and is heated using the resistance wire heating principle; the insulation layer has heat insulation functions to prevent internal heat loss; the insulating sleeve is a flame-retardant insulating material.

[0019] Preferably, the inlet and outlet of the screw pump are both connected to the heating and heat preservation delivery pipe, and the screw pump comprises a sealed cabin, a rotor and a transmission module; the interior of the sealed cabin is a spiral cavity structure; the rotor is a spiral rod installed in the spiral cavity inside the sealed cabin; the transmission module is connected to the rotor to provide power for the rotor to rotate;

[0020] The auxiliary heating device heats two different parts in two ways:

[0021] The first type: the induction coil of the auxiliary heating device is wound around the outside of the sealed cabin, and heat is generated inside the sealed cabin through induction heating;

[0022] The second type: the electric heating rod is placed inside the rotor, and generates resistance wire heat when powered on. A temperature sensing module is provided inside the sealed cabin to feedback the temperature;

[0023] The sealed cabin and the rotor both contain iron material layers.

[0024] Preferably, the floral tube grouting head allows the slurry to flow out through the small holes in the side wall, so as to evenly reinforce the weak interlayer area. The floral tube grouting head is installed at the end of the heating and insulation conveying pipe and is a copper structure. The end of the floral tube grouting head is sealed and small holes are opened on the side wall; the sealing device includes an airbag and an inflation and deflation module; the airbag is annular, installed on the heating and insulation conveying pipe, and a certain distance away from the floral tube grouting head; the inflation and deflation module is used to inflate and deflate the airbag.

[0025] The method for enhancing the anti-seepage performance of the permeable area of ​​an earth dam comprises the following steps:

[0026] S1: Based on the physical detection method, the location of the weak interlayer area of ​​the dam is obtained. The anti-seepage reinforcement holes are set along the longitudinal axis of the dam and cover the entire weak area. The hole spacing is no more than 5 times the hole diameter.

[0027] S2: Use a drilling rig to drill holes, and the first drilling depth exceeds a certain distance from the bottom of the weak interlayer;

[0028] S3: Assemble the anti-seepage performance enhancement equipment of the permeable area of ​​the dam, and connect the gate valve of the phase change material reactor, the heating and insulation delivery pipe, the pumping device, the heating and insulation delivery pipe, and the grouting device in sequence;

[0029] S4: Place the flower tube grouting head at the bottom of the hole drilled by the drilling rig, and inflate the sealing device so that the sealing device fits tightly with the hole to form a closed space;

[0030] S5: placing the composite phase change material in a phase change material reactor, and starting the phase change material reactor to melt the composite phase change material into a liquid state and stir it evenly;

[0031] S6: preheating the heat preservation conveying pipe and the pumping device, and setting the preheating temperature to 150°C to 200°C;

[0032] S7: Start the pumping device to perform zero-pressure grouting, monitor the pumping pressure that gradually increases with the injection of slurry, and stop pumping when the pressure rises to 0.5 MPa or the pressure suddenly increases several times;

[0033] S8: The sealing device is evacuated, and the grouting device is lifted to a height not higher than 2 times the height of the flower tube grouting head, and steps S4 to S7 are repeated until the flower tube grouting head is lifted to the upper edge of the weak interlayer;

[0034] S9: Start grouting at the next hole. The grouting process is the same as S2 to S8.

[0035] Preferably, in S2, the distance is not less than the height of the floral tube grouting head.

[0036] Preferably, in S5, the composite phase change material includes a phase change material and a surface modifier, a phenol polymer, a cross-linking agent, a toughening agent and a foaming agent, the phase change material includes paraffin, rosin, stearic acid, and the surface modifier is sodium dodecyl sulfate; the phase change material is weighed in a mass ratio of 3:2:0.5, and then the phase change material and the surface modifier are mixed in a ratio of 20:1, and then 7.5% of the mass fraction of the phenol polymer, 2.7% of the mass fraction of the cross-linking agent, 3.4% of the mass fraction of the toughening agent and 0.9% of the mass fraction of the foaming agent are weighed, added into the phase change material reactor, and the heating temperature is set to 200°C for melting.

[0037] Preferably, in S5, the internal viscosity of the slurry prepared by the composite phase change material is fitted by software to calculate the permeability parameter α of the weak area:

[0038]

[0039] Among them, δ represents the water permeability of the underground soil in the weak area; β represents the viscosity of the slurry; g represents the gravitational acceleration; ρ a represents the water density in the weak area; ρ b Indicates the slurry density;

[0040] The penetration parameter α is also corrected based on the least square method to minimize the sum of square errors, and the slurry penetration time and slurry penetration radius are calculated based on the columnar diffusion theory, and the construction period is predicted based on the neural network.

[0041] Preferably, during the grouting process of S1 to S9, the phase change material reactor, the heating and heat preservation delivery pipe, and the pumping device are all kept in a heated and temperature-maintaining state.

[0042] Compared with the prior art, the present invention provides a device and method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam, which has the following beneficial effects:

[0043] The present invention utilizes the melting characteristics of phase change materials and an active pressurized grouting method to achieve the purpose of utilizing phase change materials to bond soil particles in weak interlayer areas and enhance the local anti-seepage capacity of local dams. The construction period is short, the cost is low, and the disturbance to the surrounding soil is small. The composite phase change material is prepared by surface modifiers, etc. to improve the rheological properties of the slurry, greatly improve the grouting efficiency, further shorten the construction period, and at the same time predict the construction period through a neural network to provide data support. The present invention is also applicable to locations where leakage is occurring or has occurred, and has a wide range of applications. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] Figure 1 This is the device architecture diagram mentioned in Example 1 of the present invention;

[0045] Figure 2 This is a schematic diagram of the device structure connection mentioned in Example 1 of the present invention;

[0046] Figure 3 is a schematic cross-sectional view of the electromagnetic coil mentioned in Example 1 of the present invention;

[0047] Figure 4 This is a flow chart of the method mentioned in Example 2 of the present invention. DETAILED DESCRIPTION

[0048] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0049] The present invention utilizes the melting characteristics of phase change materials and the active pressurized grouting method to achieve the purpose of using phase change materials to bond soil particles in the weak interlayer area and enhance the local anti-seepage capacity of the local dam. The construction period is short, the cost is low, and the disturbance to the surrounding soil is small. The composite phase change material is prepared by surface modifiers to improve the rheological properties of the slurry, which greatly improves the grouting efficiency and further shortens the construction period. At the same time, the construction period is predicted by a neural network to provide data support. The present invention is also applicable to parts that are leaking or have already leaked, and has a wide range of applications. Specifically, it includes the following contents.

[0050] Embodiment 1:

[0051] See also Figure 1-3 The anti-seepage performance enhancement device for the permeable area of ​​the earth dam of the present invention comprises: a material phase change kettle, a heating and heat-insulating conveying pipe, a pumping device, and a grouting device.

[0052] The material phase change kettle includes a multi-layer cylinder, a temperature control module, a stirring module, a gate valve and other modules.

[0053] The multi-layer cylinder of the material phase change kettle has an inner layer of stainless steel with a diameter of 0.4m, a height of 0.8m, and a thickness of 0.2mm; the insulation layer is an aerogel cloth with a thickness of 10mm; the structural layer is a lightweight aluminum alloy skeleton; the electromagnetic coil is a copper wire with a diameter of 2.5mm and covered with an insulating layer coating, a flame-retardant insulation sleeve on the outer cover, and a mica sandwich in the middle; the insulation layer 2 is a high-temperature resistant plastic shell. The temperature control module uses Jiangxin 3.5kV induction controller, including electromagnetic coils, rectifiers, temperature sensors, control modules, etc. The temperature control module rectifies conventional alternating current into high-frequency high-voltage electricity, transmits it to the electromagnetic coil, and the electromagnetic coil generates an alternating magnetic field that cuts the inner layer of the cylinder multiple times, that is, generates heat, to achieve the purpose of heating the phase change material. The temperature sensor monitors and transmits the heating temperature back to the control module, which is used to adjust the heating power to achieve the purpose of constant temperature heating and insulation. The stirring module stirs the phase change material to ensure that the phase change material is evenly mixed after melting into a liquid state. The gate valve is made of stainless steel, specifically a butterfly valve system.

[0054] The inner layer of the heating and insulation conveying pipe is a hose made of stainless steel wire; the heating wire is a nickel-chromium alloy, which can generate heat when powered on; the temperature controller includes a temperature probe and a heating module. The temperature probe is installed in the inner layer to monitor the internal fluid temperature. The heating module is connected to the heating wire and is heated using the resistance wire heating principle; the insulation layer is insulation foam; and the insulating sleeve is a flame-retardant insulating rubber material.

[0055] The pumping device is a screw pump and an auxiliary heating device. The inlet and outlet of the screw pump are connected to the heating and insulation conveying pipe. The auxiliary heating device heats two parts: one is that the induction coil of the auxiliary heating device is wound around the outside of the sealed cabin, and the inside of the sealed cabin is heated by induction heating (high-frequency alternating current is passed); the other is that the electric heating rod is placed inside the stator, and the resistance wire heat is generated after power is turned on. A temperature sensing module is installed inside the sealed cabin to feedback the temperature and adjust the heating setting. The sealed cabin and the rotor both contain iron material layers.

[0056] In the grouting device, the flower tube grouting head is a copper structure with a length of 0.5m, a wall thickness of 2mm, a side wall hole diameter of 3mm, and a hole spacing of 2mm. The airbag of the sealing device is made of annular rubber, with a thickness of 1mm and a height of 0.5m, and can be inflated and deflated by electricity.

[0057] Embodiment 2:

[0058] See also Figure 4 The method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam of the present invention comprises the following steps:

[0059] S1: Based on the physical exploration method, the location of the weak interlayer area of ​​the dam is obtained, including the mileage pile number, depth range, etc. The anti-seepage reinforcement holes are set along the longitudinal axis of the dam and cover the entire weak area; the details are as follows:

[0060] The ground penetrating radar method was used to detect hidden dangers in a certain embankment section. It was found that there was a hidden danger of loose soil in the range of pile number K10+050~K10+066 and depth of 2.0m~3.3m, which was a weak area of ​​the embankment. The designed drilling diameter was 0.1m, and the hole spacing should not be greater than 5 times the hole diameter, so the designed drilling spacing was 0.5m.

[0061] S2: Use a drilling rig to drill holes. The initial drilling depth exceeds a certain distance from the bottom of the weak interlayer, and the distance is not less than the height of the grouting head of the flower tube; the details are as follows:

[0062] A core drill with a diameter of 0.1m was used to drill a hole downward from the dam top to a depth of 4.0m.

[0063] S3: Assemble the anti-seepage performance enhancement equipment of the permeable area of ​​the dam, and connect the gate valve of the phase change material reactor, the heating and insulation delivery pipe, the pumping device, the heating and insulation delivery pipe, and the grouting device in sequence;

[0064] S4: Place the flower tube grouting head at the bottom of the drilling hole, inflate the sealing device, make the sealing device fit tightly with the hole, and form a closed space; the details are as follows:

[0065] The grouting head for the flower pipe is a copper grouting head with a diameter of 0.08m and a height of 0.5m, which is placed at the bottom of the drilled hole. Inflate the sealing device so that the sealing device fits tightly with the hole, so that the grouting head forms a closed space in the drilled hole.

[0066] S5: placing the composite phase change material in a phase change material reactor, and starting the phase change material reactor to melt the composite phase change material into a liquid state and stir it evenly; the details are as follows:

[0067] The composite phase change material prepared by mixing phase change material, surface modifier, phenol polymer, crosslinking agent, toughening agent and foaming agent is placed in the phase change material reactor, and the phase change material reactor is started to melt the composite phase change material into liquid and stir evenly. The phase change material is paraffin, rosin, and stearic acid, which are prepared according to a mass ratio of 3:2:0.5, the surface modifier is sodium dodecyl sulfate, the phase change material and the surface modifier are mixed in a ratio of 20:1, and then weigh 7.5% of the mass fraction of phenol polymer, 2.7% of the mass fraction of crosslinking agent, 3.4% of the mass fraction of toughening agent and 0.9% of the mass fraction of foaming agent, add them into the reactor, and set the heating temperature to 200°C. By adding a surface modifier to the phase change material, the fluidity of the phase change material liquid can be enhanced, which can greatly improve the grouting efficiency.

[0068] A control group with only phase change material, an experimental group 1 including phase change material + surface modifier, and an experimental group 2 including phase change material + surface modifier + phenol polymer + cross-linking agent + toughening agent + foaming agent were set up respectively. For the control group, experimental group 1 and experimental group 2, three experimental groups A, B and C corresponding to three different temperatures of 180°C, 200°C and 220°C were set up respectively. The specific experimental results can be referred to Table 1:

[0069] Table 1 Grouting results of different phase change materials and temperatures

[0070] Group Moisture content <![CDATA[Density (g / cm 3 )]]> Grouting time(s) Maximum diffusion width (cm) Before grouting 9.2% 1.28 - - Control group A - 1.52 12.15 34 Control group B - 1.55 12.11 35 Control group-C - 1.54 12.27 32 Experimental Group A - 1.63 10.47 37 Experimental Group 1B - 1.66 10.32 38 Experimental Group C - 1.65 10.56 36 Experimental Group II A - 1.75 9.15 42 Experimental Group 2B - 1.77 9.01 43 Experimental Group II C - 1.76 9.34 41

[0071] It can be seen from the table that the optimal grouting temperature of the phase change material is 200°C, and the grouting effect of the composite phase change material with the addition of surface modifier, phenol polymer, cross-linking agent, toughening agent and foaming agent is better than that of the simple phase change material and the composite phase change material with only the addition of surface modifier.

[0072] The software is based on fitting the internal viscosity of the slurry of the composite phase change material with the addition of surface modifier, phenol polymer, cross-linking agent, toughening agent and foaming agent, and the permeation parameter of the weak area is calculated based on this. The permeation parameter α is corrected by the least squares method to minimize the sum of square errors. The slurry penetration time and slurry penetration radius are calculated based on the columnar diffusion theory, and the construction period is predicted based on the neural network, which can provide data support, facilitate the planning of construction plans and provide reference.

[0073] S6: preheating the heat preservation conveying pipe and the pumping device, and setting the preheating temperature to 150°C to 200°C;

[0074] S7: Start the pumping device. The pumping plan is to transport at zero pressure first. As the slurry is injected, the pressure will gradually increase. Monitor the pumping pressure. When the monitored pumping pressure rises to 0.5MPa, stop pumping.

[0075] S8: The sealing device is evacuated, and the grouting device is lifted to a height not higher than 2 times the height of the flower tube grouting head, and steps S4 to S7 are repeated until the flower tube grouting head is lifted to the upper edge of the weak interlayer; the details are as follows:

[0076] The sealing device is evacuated to lift the grouting head of the flower tube, and the height of the grouting flower tube is raised by 0.5m. Steps S4 to S7 are repeated until the grouting head of the flower tube is raised to a depth of 1.5m.

[0077] S9: Start grouting at the next hole, and the grouting process is the same as S2 to S8. The details are as follows:

[0078] Start grouting at the next hole, and the grouting process is the same as S2 to S8 until the grouting of all grouting holes is completed.

[0079] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. Equipment for enhancing the anti-seepage performance of permeable areas of earth dams. It is characterized in that include: Material phase change kettle, heating and insulation conveying pipe, pumping device, grouting device; The material phase change kettle is a cylindrical structure, which is used to provide a storage and reaction environment for the material, and includes a multi-layer cylinder, a temperature control module, a stirring module and a gate valve; The heating and heat-insulating delivery pipe is used to ensure that the phase change material is delivered in liquid form, and includes an inner layer, a heating wire, a temperature controller, a heat-insulating layer, and an insulating sleeve; The pumping device is used to provide power for the transmission of phase change materials, and includes a screw pump and an auxiliary heat device; The grouting device is used for grouting, and comprises a flower tube grouting head and a sealing device; The multi-layer cylinder in the material phase change kettle is used for material storage and phase change; the multi-layer cylinder comprises a heat generating layer, a heat insulation layer 1, a structural layer and a heat insulation layer 2 from the innermost side to the outermost side; The heat generating layer is made of iron material with a thickness of 0.2 mm to 2 mm; the heat insulating layer 1 is made of aerogel material to prevent heat loss from the heat generating layer; The structural layer is a material phase change kettle skeleton, and an electromagnetic coil is laid inside. The electromagnetic coil is a mica high-temperature wire, which is wound around the side and bottom of the thermal insulation layer 1; the thermal insulation layer 2 is made of hard plastic material and is the outer shell of the multi-layer cylinder body, which is used to protect the internal structure; The temperature control module is used to control the heating temperature of the material phase change kettle, and includes an electromagnetic coil, a rectifier, a temperature sensor and a control module; the electromagnetic coil is a coil laid in the structural layer of the material phase change kettle, and its structure is a copper core wire and a high-temperature resistant glass fiber sleeve on the outside, and mica and silica gel are filled between the copper core wire and the high-temperature resistant glass fiber sleeve; the rectifier is used to convert conventional mains electricity into high-frequency high-voltage electricity, and then transmit it to the electromagnetic coil; the temperature sensor is installed inside the material phase change kettle to monitor the temperature of the internal phase change material; the control module controls the rectifier to work based on the set temperature and the data monitored and sent back by the temperature sensor to control the heating temperature; The stirring module is used to mix the phase change material melted into liquid evenly, and includes a lifting platform, a motor, a transmission rod and a dispersion plate; the motor is installed on the top of the lifting platform, and the transmission rod connects the motor and the dispersion plate; the lifting platform controls the lifting to realize the action of lifting the dispersion plate and dropping it into the material phase change kettle; the rotation of the motor drives the dispersion plate to rotate to realize the stirring function; The gate valve is installed at the bottom of the side wall of the material phase change kettle to control the transmission of the material; one end of the gate valve is connected to the material phase change kettle, and the other end is connected to the heating and insulation conveying pipe; The inner layer of the heating and heat-insulating conveying pipe is a hose made of stainless steel wire; the heating wire is a nickel-chromium alloy, which generates heat when powered on; the temperature controller includes a temperature probe and a heating module, the temperature probe is installed in the inner layer to monitor the fluid temperature inside the equipment, the heating module is connected to the heating wire, and is heated using the resistance wire heating principle; the insulation layer has heat insulation functions to prevent internal heat loss; the insulating sleeve is a flame-retardant insulating material.

2. The anti-seepage performance enhancement device for the permeable area of ​​an earthen dam according to claim 1, It is characterized in that The inlet and outlet of the screw pump are both connected to the heating and heat preservation delivery pipe. The screw pump includes a sealed cabin, a rotor and a transmission module. The interior of the sealed cabin is a spiral cavity structure. The rotor is a spiral rod installed in the spiral cavity inside the sealed cabin. The transmission module is connected to the rotor to provide power for the rotor to rotate. The auxiliary heating device heats two different parts in two ways: The first type: the induction coil of the auxiliary heating device is wound around the outside of the sealed cabin, and heat is generated inside the sealed cabin through induction heating; The second type: the electric heating rod is placed inside the rotor, and generates resistance wire heat when powered on. A temperature sensing module is provided inside the sealed cabin to feedback the temperature; The sealed cabin and the rotor both contain iron material layers.

3. The anti-seepage performance enhancement device for the permeable area of ​​an earthen dam according to claim 1, It is characterized in that The floral tube grouting head allows the slurry to flow out through the small holes in the side wall, so as to evenly reinforce the weak interlayer area. The floral tube grouting head is installed at the end of the heating and insulation conveying pipe and is a copper structure. The end of the floral tube grouting head is sealed and small holes are opened on the side wall; the sealing device includes an airbag and an inflation and deflation module; the airbag is annular, installed on the heating and insulation conveying pipe, and a certain distance away from the floral tube grouting head; the inflation and deflation module is used to inflate and deflate the airbag.

4. A method for enhancing the anti-seepage performance of the earth dam permeable area according to any one of claims 1 to 3, It is characterized in that The steps include: S1: Based on the physical detection method, the location of the weak interlayer area of ​​the dam is obtained. The anti-seepage reinforcement holes are set along the longitudinal axis of the dam and cover the entire weak area. The hole spacing is no more than 5 times the hole diameter. S2: Use a drilling rig to drill holes, and the first drilling depth exceeds a certain distance from the bottom of the weak interlayer; S3: Assemble the anti-seepage performance enhancement equipment of the permeable area of ​​the dam, and connect the gate valve of the phase change material reactor, the heating and insulation delivery pipe, the pumping device, the heating and insulation delivery pipe, and the grouting device in sequence; S4: Place the flower tube grouting head at the bottom of the hole drilled by the drilling rig, and inflate the sealing device so that the sealing device fits tightly with the hole to form a closed space; S5: placing the composite phase change material in a phase change material reactor, and starting the phase change material reactor to melt the composite phase change material into a liquid state and stir it evenly; S6: preheating the heat preservation conveying pipe and the pumping device, and setting the preheating temperature to 150℃~200℃; S7: Start the pumping device to perform zero-pressure grouting, monitor the pumping pressure that gradually increases with the injection of slurry, and stop pumping when the pressure rises to 0.5 MPa or the pressure suddenly increases several times; S8: The sealing device is evacuated, and the grouting device is lifted to a height not higher than 2 times the height of the flower tube grouting head, and steps S4 to S7 are repeated until the flower tube grouting head is lifted to the upper edge of the weak interlayer; S9: Start grouting at the next hole. The grouting process is the same as S2 to S8.

5. The method for enhancing the anti-seepage performance enhancement device of the permeable area of ​​an earthen dam according to claim 4, It is characterized in that In S2, the distance is not less than the height of the floral tube grouting head.

6. The method for enhancing the anti-seepage performance enhancement device of the permeable area of ​​an earthen dam according to claim 5, It is characterized in that In S5, the composite phase change material includes a phase change material and a surface modifier, a phenol polymer, a cross-linking agent, a toughening agent and a foaming agent, the phase change material includes paraffin, rosin, and stearic acid, and the surface modifier is sodium dodecyl sulfate; the phase change material is weighed in a mass ratio of 3:2:0.5, and then the phase change material and the surface modifier are mixed in a ratio of 20:1, and then 7.5% of the mass fraction of the phenol polymer, 2.7% of the mass fraction of the cross-linking agent, 3.4% of the mass fraction of the toughening agent and 0.9% of the mass fraction of the foaming agent are weighed, added into the phase change material reactor, and the heating temperature is set to 200°C for melting.

7. The method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam according to claim 6, It is characterized in that In S5, the internal viscosity of the slurry prepared by the composite phase change material is fitted by software to calculate the permeability parameters of the weak area. : in, Indicates the water permeability of underground soil in weak areas; It indicates the internal viscosity of the slurry; represents the acceleration due to gravity; Indicates the water density in the weak area; Indicates the slurry density; The infiltration parameters were also calculated based on the least squares method. Corrections are made to minimize the sum of squared errors, and the slurry penetration time and slurry penetration radius are calculated based on the columnar diffusion theory, and the construction period is predicted based on the neural network.

8. The method for enhancing the anti-seepage performance of the permeable area of ​​an earthen dam according to claim 7, It is characterized in that During the grouting process of S1 to S9, the phase change material reactor, the heating and heat preservation delivery pipe, and the pumping device are all kept in a heated and temperature-maintaining state.