Photoelectric conversion receiver based on polymer materials and preparation method thereof
Through the photoelectric conversion receiver based on polymer materials, using polyimide-iron oxide-silicon nitride films and other materials, the problems of high cost and complex process of traditional photoelectric receivers are solved, and the photoelectric conversion efficiency and cost reduction are achieved , has wide application prospects.
Patent Information
- Application Number
- CN202410631491.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-21
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-05-21
AI Technical Summary
The photoelectric receivers prepared by traditional inorganic semiconductor materials are costly and complex in preparation, which limits their wide application.
A photoelectric conversion receiver based on polymer materials is adopted, including a cat electrode, a substrate layer, a depletion layer, a doping layer, an anode and a passivation zone, and a polyimide-iron oxide-silicon nitride film is used as the passivation zone Materials are formed by special preparation methods such as photolithography, ion implantation, evaporation and thermal imidation.
It has achieved improvement in photoelectric conversion efficiency, while reducing production costs and process complexity, with significant application prospects and socio-economic benefits.
Smart Images

Figure CN118338687B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of optoelectronic technology, and in particular to a photoelectric conversion receiver based on polymer materials and a preparation method thereof. Background Art
[0002] With the development of science and technology, photoelectric conversion devices are widely used in energy, communication, sensors and other fields. However, the high cost and complex preparation process of traditional inorganic semiconductor materials limit their wide application. Summary of the invention
[0003] The present invention provides a photoelectric conversion receiver based on polymer materials and a preparation method thereof, aiming to solve at least one of the technical problems existing in the prior art.
[0004] The technical solution of the present invention is a photoelectric conversion receiver based on polymer materials and a preparation method thereof. The photoelectric conversion receiver based on polymer materials comprises:
[0005] cathode electrode;
[0006] A substrate layer, wherein the substrate layer is disposed above the cathode electrode;
[0007] a depletion layer, the depletion layer being arranged above the substrate layer;
[0008] a doping layer, the doping layer being disposed above the depletion layer;
[0009] an anode electrode, the anode electrode comprising a first anode electrode and a second anode electrode, the first anode electrode and the second anode electrode being respectively disposed above the doping layer;
[0010] A photosensitive region, the photosensitive region is arranged above the doping layer and between the first anode electrode and the second anode electrode;
[0011] A passivation region is disposed on an outer side of the first anode electrode and an outer side of the second anode electrode.
[0012] Furthermore, the material of the passivation region is a polyimide-iron oxide-silicon nitride film.
[0013] Furthermore, the anode electrode is a silicon-aluminum electrode.
[0014] Furthermore, the doped layer is a P-type semiconductor, and the doped ions of the doped layer are high-concentration boron ions.
[0015] Furthermore, the depletion layer is an intrinsic layer, and the depletion layer is undoped.
[0016] Furthermore, the depletion layer is a single crystal silicon substrate.
[0017] Furthermore, the cathode electrode is made of gold or silver.
[0018] Furthermore, the present invention also proposes a method for preparing a photoelectric conversion receiver based on a polymer material, comprising the following steps:
[0019] S100, after cleaning the surface of the epitaxial wafer, a silicon dioxide layer is grown on the surface of the silicon epitaxial wafer, and then a window is opened on the surface by photolithography, and boron ions are accumulated on the surface of the silicon wafer by ion implantation, and the ions accumulated on the surface are pushed into the silicon wafer by high-temperature diffusion distribution to form a heavily doped region, which is a P-type semiconductor;
[0020] S200, in a high temperature environment, the silicon near the surface of the silicon wafer will be oxidized into silicon dioxide. Two windows are opened on the left and right sides of the chip through photolithography, and then the metal layer is evaporated onto the chip surface through sputtering evaporation, and the left and right electrodes are retained through photolithography;
[0021] S300, place the material on a coating machine, spread the polyimide-iron oxide-silicon nitride solution evenly on the wafer surface, place the wafer in a 120°C oven for pre-baking, and the polyimide-iron oxide-silicon nitride solution gradually heats up for thermal imidization. After baking for one hour, take the material out of the oven, and after cooling to room temperature, remove the film part on the pad wire area through exposure and development, and the remaining film adheres to the wafer surface;
[0022] S400, diffusing phosphorus ions on the back side of the substrate layer, and then evaporating silver to form a back electrode.
[0023] Further, in step S300, preparing the polyimide-iron oxide-silicon nitride solution comprises the following steps:
[0024] S310, adding tetraethoxysilane TEOS to a beaker containing ethanol to dissolve, adding ammonia water, wherein the mass ratio of tetraethoxysilane TEOS to ammonia water is 1:1.6-1:2.5, stirring fully after adding, adding an acid catalyst after stirring to obtain a mixed solution, making the pH value of the mixed solution in an environment of 1.3-1.5, and stirring for 2-4 hours to form a polysiloxane grid;
[0025] S320, as the polycondensation polymerization proceeds to a semi-sol state, drying at a temperature of 15° C. to 30° C. for 18 to 36 hours in an air-dried and nitrogen environment to obtain a high-purity silicon nitride sol;
[0026] S330, take 4,4-diaminodiphenyl ether ODA into a beaker, add an appropriate amount of NN-dimethylacetamide DMAc solution, wherein the mass ratio of 4,4-diaminodiphenyl ether ODA:NN-dimethylacetamide DMAc is 1:6-1:10, shake the beaker until the 4,4-diaminodiphenyl ether ODA is completely dissolved, add silicon nitride sol, and stir evenly at a temperature of 15°C-30°C after adding;
[0027] S340, at room temperature and nitrogen environment, slowly adding PMDA in batches and stirring to dissolve the sol, slowly adding 2 ml-12 ml of iron oxide solution and stirring under water bath heating at 40° C., and as the stirring time increases, a polyamic acid-iron oxide-silicon nitride solution is obtained, wherein the iron oxide ratio in the polyamic acid-iron oxide-silicon nitride solution is about 5%-15%, and the silicon nitride content is about 15%-25%;
[0028] S350, dropping a polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer, and using a coating machine to evenly spread the polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer. After coating, the wafer is placed in an oven for pre-baking treatment, and the baking temperature is set to 120° C.-150° C. and baked for one hour. At this time, the polyamic acid-iron oxide-silicon nitride is gradually heated up for thermal imidization to polyimide-iron oxide-silicon nitride;
[0029] S360, taking out the wafer from the oven, and after the wafer cools down to room temperature, removing the film on the bonding wire area on the chip anode electrode through exposure and development, and the remaining film adheres to the wafer surface.
[0030] The beneficial effects of the present invention are:
[0031] The polymer material-based photoelectric receiver provided by the present invention utilizes the unique advantages of polymer materials to achieve improved photoelectric conversion efficiency, while reducing production costs and process complexity, and has significant application prospects and social and economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 Shown is a schematic structural diagram of a photoelectric conversion receiver based on polymer materials according to the present invention.
[0033] Figure 2 FIG. 1 is a top view of a polymer material-based photoelectric conversion receiver according to the present invention.
[0034] Figure 3 Shown is a flow chart of a method for preparing a photoelectric conversion receiver based on polymer materials according to the present invention.
[0035] Figure 4The flowchart shown is a method for preparing a polyimide-iron oxide-silicon nitride solution in a method for preparing a photoelectric conversion receiver based on a polymer material according to the present invention.
[0036] Reference numerals: 100, cathode electrode; 200, substrate layer; 300, depletion layer; 400, doping layer; 500, first anode electrode; 510, second anode electrode; 600, photosensitive region; 700, passivation region. DETAILED DESCRIPTION
[0037] The following will be combined with the embodiments and drawings to clearly and completely describe the concept, specific structure and technical effects of the present invention, so as to fully understand the purpose, scheme and effect of the present invention. It should be noted that the embodiments and features in the embodiments of this application can be combined with each other without conflict.
[0038] It should be noted that, unless otherwise specified, when a feature is referred to as being "fixed" or "connected" to another feature, it may be directly fixed or connected to the other feature, or it may be indirectly fixed or connected to the other feature. In addition, the descriptions of up, down, left, right, top, bottom, etc. used in the present invention are only relative to the relative positional relationship of the components of the present invention in the drawings.
[0039] In addition, unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art. The terms used in this specification are only for describing specific embodiments, not for limiting the present invention. The term "and / or" used herein includes any combination of one or more related listed items.
[0040] It should be understood that, although the terms first, second, third, etc. may be used to describe various elements in the present disclosure, these elements should not be limited to these terms. These terms are only used to distinguish elements of the same type from each other. For example, without departing from the scope of the present disclosure, the first element may also be referred to as the second element, and similarly, the second element may also be referred to as the first element.
[0041] Reference Figures 1 to 4 In some embodiments, the present invention provides a photoelectric conversion receiver based on a polymer material and a preparation method thereof, wherein the photoelectric conversion receiver based on a polymer material comprises:
[0042] cathode electrode 100;
[0043] A substrate layer 200, wherein the substrate layer 200 is disposed above the cathode electrode 100;
[0044] A depletion layer 300, wherein the depletion layer 300 is disposed above the substrate layer 200;
[0045] A doping layer 400 , wherein the doping layer 400 is disposed above the depletion layer 300 ;
[0046] An anode electrode, the anode electrode comprising a first anode electrode 500 and a second anode electrode 510, wherein the first anode electrode 500 and the second anode electrode 510 are respectively disposed above the doping layer 400;
[0047] A photosensitive region 600 , wherein the photosensitive region 600 is disposed above the doping layer 400 and between the first anode electrode 500 and the second anode electrode 510 ;
[0048] The passivation region 700 is disposed outside the first anode electrode 500 and outside the second anode electrode 510 .
[0049] The beneficial effects of the present invention are:
[0050] The polymer material-based photoelectric receiver provided by the present invention utilizes the unique advantages of polymer materials to achieve improved photoelectric conversion efficiency, while reducing production costs and process complexity, and has significant application prospects and social and economic benefits.
[0051] The substrate layer 200 is made of silicon. The substrate layer 200 is doped with a certain concentration of Group V ions such as phosphorus and arsenic to form an N-type semiconductor. The substrate layer 200 is an N-type semiconductor.
[0052] Further, refer to Figure 1 to Figure 2 The material of the passivation region 700 is a polyimide-iron oxide-silicon nitride film.
[0053] Specifically, the main structure of the passivation region 700 is a polyimide-iron oxide-silicon nitride improved thin film layer, which improves the absorption and conversion of green light and yellow-green light without affecting the absorption rate of the infrared band.
[0054] The polyimide-iron oxide-silicon nitride film is made of an organic polymer material with excellent photoelectric conversion performance, and can effectively absorb light energy and convert it into electrical energy. The polyimide-iron oxide-silicon nitride film has good optical properties, charge transfer performance and stability, and can effectively achieve the effective separation and transfer of photogenerated carriers.
[0055] Further, refer to Figure 1 to Figure 2 , the anode electrode is a silicon-aluminum electrode.
[0056] Specifically, the silicon-aluminum electrode is used to efficiently collect the current generated by photoelectric conversion and convert the optical signal into an electrical signal.
[0057] The upper surface of the photoelectric conversion receiver based on polymer materials has a large photosensitive area 600, and there is an anode electrode on the left and right of the photosensitive area 600, which are a first anode electrode 500 and a second anode electrode 510 respectively. The first anode electrode 500 and the second anode electrode 510 are aluminum electrodes, and their main components are silicon aluminum. The characteristics of silicon aluminum material can better contact with the silicon layer to produce an ohmic effect, which can improve the photoelectric conversion efficiency. At the same time, the use of two anode electrode welding wires can effectively reduce the probability of failure of the photoelectric conversion receiver based on polymer materials.
[0058] Further, refer to Figure 1 to Figure 2 The doping layer 400 is a P-type semiconductor, and the doping ions of the doping layer 400 are high-concentration boron ions.
[0059] Further, refer to Figure 1 to Figure 2 , the depletion layer 300 is an intrinsic layer, and the depletion layer 300 is undoped.
[0060] Further, refer to Figure 1 to Figure 2 , the depletion layer 300 is a single crystal silicon substrate.
[0061] Further, refer to Figure 1 to Figure 2 , the cathode electrode 100 is made of gold or silver material.
[0062] Further, refer to Figure 3 The present invention also proposes a method for preparing a photoelectric conversion receiver based on polymer materials, comprising the following steps:
[0063] S100, after cleaning the surface of the epitaxial wafer, a silicon dioxide layer is grown on the surface of the silicon epitaxial wafer, and then a window is opened on the surface by photolithography, and boron ions are accumulated on the surface of the silicon wafer by ion implantation, and the ions accumulated on the surface are pushed into the silicon wafer by high-temperature diffusion distribution to form a heavily doped region, which is a P-type semiconductor;
[0064] S200, in a high temperature environment, the silicon near the surface of the silicon wafer will be oxidized into silicon dioxide. Two windows are opened on the left and right sides of the chip through photolithography, and then the metal layer is evaporated onto the chip surface through sputtering evaporation, and the left and right electrodes are retained through photolithography;
[0065] S300, place the material on a coating machine, spread the polyimide-iron oxide-silicon nitride solution evenly on the wafer surface, place the wafer in a 120°C oven for pre-baking, and the polyimide-iron oxide-silicon nitride solution gradually heats up for thermal imidization. After baking for one hour, take the material out of the oven, and after cooling to room temperature, remove the film part on the pad wire area through exposure and development, and the remaining film adheres to the wafer surface;
[0066] S400 , diffusing phosphorus ions on the back side of the substrate layer 200 , and then evaporating silver to form a back electrode.
[0067] Further, refer to Figure 4 In step S300, preparing the polyimide-iron oxide-silicon nitride solution comprises the following steps:
[0068] S310, adding tetraethoxysilane TEOS to a beaker containing ethanol to dissolve, adding ammonia water, wherein the mass ratio of tetraethoxysilane TEOS to ammonia water is 1:1.6-1:2.5, stirring fully after adding, adding an acid catalyst after stirring to obtain a mixed solution, making the pH value of the mixed solution in an environment of 1.3-1.5, and stirring for 2-4 hours to form a polysiloxane grid;
[0069] S320, as the polycondensation polymerization proceeds to a semi-sol state, drying at a temperature of 15° C. to 30° C. for 18 to 36 hours in an air-dried and nitrogen environment to obtain a high-purity silicon nitride sol;
[0070] S330, take 4,4-diaminodiphenyl ether ODA into a beaker, add an appropriate amount of NN-dimethylacetamide DMAc solution, wherein the mass ratio of 4,4-diaminodiphenyl ether ODA:NN-dimethylacetamide DMAc is 1:6-1:10, shake the beaker until the 4,4-diaminodiphenyl ether ODA is completely dissolved, add silicon nitride sol, and stir evenly at a temperature of 15°C-30°C after adding;
[0071] S340, at room temperature and nitrogen environment, slowly adding PMDA in batches and stirring to dissolve the sol, slowly adding 2 ml-12 ml of iron oxide solution and stirring under water bath heating at 40° C., and as the stirring time increases, a polyamic acid-iron oxide-silicon nitride solution is obtained, wherein the iron oxide ratio in the polyamic acid-iron oxide-silicon nitride solution is about 5%-15%, and the silicon nitride content is about 15%-25%;
[0072] S350, dropping a polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer, and using a coating machine to evenly spread the polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer. After coating, the wafer is placed in an oven for pre-baking treatment, and the baking temperature is set to 120° C.-150° C. and baked for one hour. At this time, the polyamic acid-iron oxide-silicon nitride is gradually heated up for thermal imidization to polyimide-iron oxide-silicon nitride;
[0073] S360, taking out the wafer from the oven, and after the wafer cools down to room temperature, removing the film on the bonding wire area on the chip anode electrode through exposure and development, and the remaining film adheres to the wafer surface.
[0074] Specifically, during the preparation process, a special film-forming process and technology are used to make the amic acid-iron oxide-silicon nitride evenly and densely cover the doping layer 400 to ensure the photoelectric conversion efficiency and device stability.
[0075] Film formation mechanism: Polyimide film is generally made by polycondensing and drooling of pyromellitic dianhydride (PMDA) and diaminodiphenyl ether (ODA) in a very strong solvent dimethylacetamide (DMAC) and then imidizing.
[0076] The above is only a preferred embodiment of the present invention. The present invention is not limited to the above implementation. As long as the technical effect of the present invention is achieved by the same means, any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present disclosure shall be included in the scope of protection of the present disclosure. All should belong to the protection scope of the present invention. Within the protection scope of the present invention, its technical scheme and / or implementation method can have various modifications and changes.
Claims
1. A photoelectric conversion receiver based on polymer materials, characterized in that: include: cathode electrode (100); A substrate layer (200), the substrate layer (200) being arranged above the cathode electrode (100); A depletion layer (300), the depletion layer (300) being arranged above the substrate layer (200); a doping layer (400), the doping layer (400) being arranged above the depletion layer (300); an anode electrode, the anode electrode comprising a first anode electrode (500) and a second anode electrode (510), the first anode electrode (500) and the second anode electrode (510) being respectively arranged above the doping layer (400); A photosensitive region (600), the photosensitive region (600) being arranged above the doping layer (400) and between the first anode electrode (500) and the second anode electrode (510); A passivation region (700), the passivation region (700) being arranged on the outside of the first anode electrode (500) and the outside of the second anode electrode (510), the material of the passivation region (700) being a polyimide-iron oxide-silicon nitride film.
2. The photoelectric conversion receiver based on polymer materials according to claim 1, characterized in that: The anode electrode is a silicon-aluminum electrode.
3. The photoelectric conversion receiver based on polymer materials according to claim 1, characterized in that: The doping layer (400) is a P-type semiconductor, and the doping ions of the doping layer (400) are high-concentration boron ions.
4. The photoelectric conversion receiver based on polymer materials according to claim 1, characterized in that: The depletion layer (300) is an intrinsic layer, and the depletion layer (300) is undoped.
5. The photoelectric conversion receiver based on polymer materials according to claim 1, characterized in that: The light-transmitting depletion layer (300) is a single crystal silicon substrate.
6. The photoelectric conversion receiver based on polymer materials according to claim 1, characterized in that: The cathode electrode (100) is made of gold or silver.
7. A method for preparing a photoelectric conversion receiver based on polymer materials, characterized in that: The following steps are involved: S100, after cleaning the surface of the epitaxial wafer, a silicon dioxide layer is grown on the surface of the silicon epitaxial wafer, and then a window is opened on the surface by photolithography, and boron ions are accumulated on the surface of the silicon wafer by ion implantation, and the ions accumulated on the surface are pushed into the silicon wafer by high-temperature diffusion distribution to form a heavily doped region, which is a P-type semiconductor; S200, in a high temperature environment, the silicon near the surface of the silicon wafer will be oxidized into silicon dioxide. Two windows are opened on the left and right sides of the chip through photolithography, and then the metal layer is evaporated onto the chip surface through sputtering evaporation, and the left and right electrodes are retained through photolithography; S300, placing the material on a coating machine, and evenly spreading the polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer. After coating, the wafer is placed in a 120°C oven for pre-baking. At this time, the polyamic acid-iron oxide-silicon nitride solution is gradually heated up for thermal imidization. After baking for one hour, the material is taken out of the oven, and after cooling to room temperature, the film part on the pad bonding line area is removed through exposure and development, and the remaining film adheres to the wafer surface; S400, diffusing phosphorus ions on the back side of the substrate layer (200), and then evaporating silver to form a back electrode.
8. The method for preparing a photoelectric conversion receiver based on polymer materials according to claim 7, characterized in that: In step S300, preparing the polyimide-iron oxide-silicon nitride solution comprises the following steps: S310, adding tetraethoxysilane TEOS to a beaker containing ethanol to dissolve, adding ammonia water, wherein the mass ratio of tetraethoxysilane TEOS to ammonia water is 1:1.6-1:2.5, stirring fully after adding, adding an acid catalyst after stirring to obtain a mixed solution, making the pH value of the mixed solution in an environment of 1.3-1.5, and stirring for 2-4 hours to form a polysiloxane grid; S320, as the polycondensation polymerization proceeds to a semi-sol state, drying at a temperature of 15° C. to 30° C. for 18 to 36 hours in an air-dried and nitrogen environment to obtain a high-purity silicon nitride sol; S330, take 4,4-diaminodiphenyl ether ODA into a beaker, add an appropriate amount of NN-dimethylacetamide DMAc solution, wherein the mass ratio of 4,4-diaminodiphenyl ether ODA:NN-dimethylacetamide DMAc is 1:6-1:10, shake the beaker until the 4,4-diaminodiphenyl ether ODA is completely dissolved, add silicon nitride sol, and stir evenly at a temperature of 15°C-30°C after adding; S340, at room temperature and nitrogen environment, slowly adding PMDA in batches and stirring to dissolve the sol, slowly adding 2 ml-12 ml of iron oxide solution and stirring under water bath heating at 40°C, and as the stirring time increases, a polyamic acid-iron oxide-silicon nitride solution is obtained, wherein the iron oxide ratio in the polyamic acid-iron oxide-silicon nitride solution is 5%-15%, and the silicon nitride content is 15%-25%; S350, dropping a polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer, and using a coating machine to evenly spread the polyamic acid-iron oxide-silicon nitride solution on the surface of the wafer. After coating, the wafer is placed in an oven for pre-baking treatment, and the baking temperature is set to 120° C.-150° C. and baked for one hour. At this time, the polyamic acid-iron oxide-silicon nitride is gradually heated up for thermal imidization to polyimide-iron oxide-silicon nitride; S360, taking out the wafer from the oven, and after the wafer cools down to room temperature, removing the thin film on the bonding wire area on the chip anode electrode by exposure and development, and the remaining thin film adheres to the wafer surface.
Citation Information
Patent Citations
Passivation film, coating material, solar-cell element, and silicon substrate with passivation film attached thereto
CN104471716A
Solar battery and manufacturing method thereof
CN104733616A
Thin film solar cell with high photoelectric conversion efficiency and preparation method thereof
CN115528181A
Manufacturing method of solar cell and solar cell manufactured by this method
JP2002076399A
Solution processible organic-inorganic hybrid insulator and fabrication method thereof
KR1020090120257A