A thin-gauge steel plate rolling mill structure
By setting cooling components on the side of the work roll and dynamically controlling the cooling water flow, the problem of uneven temperature drop when rolling thin steel plates in a heavy plate mill was solved. This achieved a slightly flattened state of the work roll crown, ensuring consistent fit between the workpiece and the work roll, improving rolling quality and efficiency, and shortening the production cycle.
Patent Information
- Application Number
- CN202410576068.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-10
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-05-10
AI Technical Summary
In the existing technology, when rolling thin steel plates, the wide and thick plate rolling mill has the problem of rapid and uneven temperature drop, which leads to problems such as plate warping, sickle bending and rolling frame scraping. This results in low production efficiency and uneven wear of the work roll surface, affecting the production cycle and quality.
The system employs dynamic linear cooling technology for the work rolls. By setting cooling components on the side of the work rolls and connecting nozzles through the main cooling pipes and branch pipes, dynamic control of the cooling water flow rate is achieved. Combined with the principle of thermal expansion and contraction of the work rolls, the system maintains a slightly flat convexity of the work rolls, ensuring reliable contact between the workpiece and the work rolls and preventing uneven wear on the roll surface.
It improves the rolling quality and production efficiency of thin steel plates, shortens the production cycle, ensures uniform force on the work rolls and support rolls, reduces roll surface wear, realizes full-process plate shape control, and enhances delivery capability.
Smart Images

Figure CN118341836B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of steel plate rolling mill technology, and more specifically, relates to a rolling mill structure for thin-gauge steel plates. Background Technology
[0002] Thin steel plates with a thickness of 5-6mm are widely used in engineering machinery, boiler containers, shipbuilding and other fields. For thin steel plates with a width of 1200-2000mm, hot continuous rolling and hot rolling mills are generally used. During the rolling process, the problem of excessive temperature drop of thin steel plates can be effectively overcome. However, thin steel plates with a width of more than 2000mm can only be rolled using heavy plate mills. Due to the large thickness of the billet and the number of rolling passes, while the finished steel plate has a small thickness and large width, the temperature drop during the rolling process is rapid and uneven, which can easily cause problems such as plate warping, sickle bending and rolling frame scraping.
[0003] To overcome the problem of rapid and uneven temperature drop when rolling thin steel plates in heavy plate mills, different manufacturers have made different attempts based on their own equipment. Manufacturers using single-stand mills generally adopt a two-fire rolling process, rolling the billet thickness from more than 200mm to 70-90mm. After cleaning the surface of the billet, it is reheated in the reheating furnace and rolled into a finished plate with a thickness of 5-6mm. Manufacturers using two-stand mills use a one-fire rolling process, rolling the billet thickness from more than 200mm to an intermediate billet with a thickness of 60-80mm in the roughing mill. The intermediate billet is then quickly rolled into a finished plate with a thickness of 5-6mm in the finishing mill. Whether it is a single-fired or two-fired rolling process, in order to ensure the matching of roll crown, rolling must be carried out within a specific time range of 7 to 10 days of use of the support rolls and 1 to 2 hours of use of the work rolls. This time range is only about 20% of the use cycle of the support rolls and 8% of the use cycle of the work rolls. Rolling cannot be carried out during other time periods, which prolongs the production cycle of thin-gauge steel plates and is not conducive to the timely delivery of steel plates.
[0004] Currently, the raw material for rolling 5-6mm thick steel plates using double-stand wide and thick plates is 180-210mm continuous casting billets. The heating process is as follows: heating in a walking beam furnace, with the preheating section temperature ≤900℃, the first heating section temperature 900℃~1200℃, the second heating section temperature 1200~1300℃, and the soaking section temperature 1220~1300℃. To ensure uniform heating of the billets, the furnace storage time for 180mm billets is ≥250 minutes, and the furnace storage time for 210mm billets is ≥290 minutes. In the rolling process, the initial roll crown of the support rolls on the finishing mill is +0.4mm. Rolling is scheduled about 7 to 10 days after they are put on the mill, at which time the roll crown is about +0.2mm. At the same time, the initial roll crown of the work rolls is -0.1mm. Rolling is carried out about 1 to 2 hours after the work rolls are put on the mill. In the roughing mill rolling stage, the initial rolling temperature is ≥1150℃ and the final rolling temperature is ≥1050℃. The thickness of the intermediate billet after rolling is 60 to 80mm. There are 5 to 7 rolling passes. High-pressure water is used for descaling in the first and third to last passes. Depending on the width of the finished product, the intermediate billet is widened in the second and fourth passes to make the width of the intermediate billet consistent with the width of the finished steel plate. After rolling, the intermediate billet is quickly transported to the front of the finishing mill by the conveyor roller table to ensure that the initial rolling temperature of the finishing mill is ≥1000℃. During the finishing mill rolling stage, the initial rolling temperature is ≥1000℃, and the final rolling temperature is ≥840℃. The rolling process is controlled to be completed in 5 passes, with high-pressure water descaling only applied in the first pass. The entire process is longitudinal rolling. During rolling, the sled coefficient is controlled at -0.2 to -0.3 to ensure a slight upward tilt of the plate head and prevent the steel plate from entering the roller gaps. After rolling, the steel plate is air-cooled. After rolling, the steel plate is straightened on an eleven-roll online hot straightener with a straightening force of 10000–25000 KN, an initial straightening temperature ≥700℃, and a final straightening temperature ≥500℃. The straightening process consists of 1–3 passes. After being segmented, the steel plate is naturally cooled on a cooling bed. Stacking of steel plates is prohibited; the spacing between each row of steel plates should be at least 300mm to ensure uniform cooling.
[0005] The objective drawbacks of existing technologies are:
[0006] In the heating process, only the overall temperature of the preheating section, the first heating section, the second heating section, and the soaking section was regulated. When the billet is heated in the furnace, the furnace gas is affected by thermal expansion and contraction, and tends to accumulate in the upper half of the furnace, resulting in a higher temperature in the upper half and a lower temperature in the lower half. Although the overall temperature of the billet tends to be uniform after a certain period of furnace storage, there is still a temperature difference of 30 to 40°C between the upper and lower surfaces. During the subsequent rolling process, the plate shape will warp due to the temperature difference between the upper and lower surfaces, and the furnace storage time is too long. The cooling water supply for the work rolls is centrally supplied by a water tank on the mill stand. Cooling water nozzles are installed on the water tank, and the cooling water is sprayed onto the work rolls through the water supply pipeline from the water tank to the nozzles. The water pressure and flow rate of all nozzles are basically the same, so the cooling degree of the work rolls is almost the same during the rolling process. However, the area where the roll surface contacts the steel plate during the rolling process is often more severely worn, which causes steps to appear on the roll surface along the width direction. The steps on the roll surface will cause the thickness difference in the width direction of ordinary steel plates. When rolling thin steel plates with a thickness of 5-6mm, the steel plate cools down quickly and has greater deformation resistance. The steps on the work rolls will cause the roll convexity to be unbalanced during the rolling process. The steel plate cannot fully fit with the work roll, resulting in inconsistent deformation at the edges and the middle of the steel plate, and the problem of uncontrolled plate shape. To ensure rolling stability, rolling needs to be carried out for about 1 to 2 hours after the work rolls are put on the machine. During this period, the wear of the work rolls is small and the thermal expansion effect can keep the work rolls in a slightly flat state (camber 0 to -0.2 mm). At other times, the work roll step problem makes it impossible to roll thin steel plates, resulting in low production efficiency of thin steel plates and affecting contract delivery.
[0007] Among the existing technologies is a technology entitled "Hot Rolling Equipment and Hot Rolling Method for Steel Plates" with publication number "CN101253011A". This technology provides hot rolling equipment and hot rolling method for steel plates. The equipment has excellent cost and maintenance performance, and has good cooling capacity. Based on this, by properly controlling the temperature of the rolled steel, steel plates with excellent properties can be effectively manufactured. Specifically, a cooling device (20) is provided near the inlet and outlet sides of the rolling mill (12) to supply cooling water to the upper and lower surfaces of the steel plate (10) while it passes through. The cooling device (20) has an upper water tank (21) at a position where the residual cooling water (24) after being supplied to the upper surface of the steel plate (10) can be intercepted by the work roll (12a) of the rolling mill. The upper water tank (21) has an upper nozzle (22) that sprays rod-shaped cooling water (23) onto the upper surface of the steel plate (10) at a downward angle θU = 30° to 60°. A lower water tank (31) is provided between the work roll (12a) and the adjacent roller table roll (13a). The lower water tank (31) has a lower nozzle (32) that sprays rod-shaped cooling water (33) onto the lower surface of the steel plate (10) at an upward angle θL = 45° to 90°.
[0008] However, this technology does not address the technical issues and solutions of this application. Summary of the Invention
[0009] The technical problem to be solved by this invention is to provide a simple structure for a thin-gauge steel plate rolling mill, which adopts dynamic linear cooling technology for the work rolls and uses the principle of thermal expansion and contraction of the work rolls to compensate for roll surface wear. This ensures that the convexity of the work rolls is always in a slightly flat state, guaranteeing reliable contact between the rolled piece (steel plate) and the work rolls. This makes the deformation at the edges and in the middle of the rolled piece basically consistent, ensuring that the plate shape is controlled throughout the entire process of the work rolls running on the mill, without obvious waviness or warping problems. This improves the rolling quality and production efficiency of thin-gauge steel plates.
[0010] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows:
[0011] This invention relates to a thin-gauge steel plate rolling mill structure. A cooling component is located on the side of the work roll. The cooling component includes a main cooling pipe, which is connected to multiple branch cooling pipes. Each branch cooling pipe is connected to multiple cooling sub-pipes, and each sub-pipe is connected to a nozzle. A flow control valve is installed on each sub-pipe. A branch cooling pipe is located at the center of the work roll. Multiple branch cooling pipes are arranged at intervals from the center of the work roll to both sides. The water spray volume of the nozzles in the branch cooling pipes from the center of the work roll to the side of the work roll is arranged in a progressively decreasing structure. The work roll is a convex roll. When the roll profile convexity of the work roll wears down to below -0.1mm, a downward bending force is applied to the roll shaft at each end of the upper work roll, and an upward bending force is applied to the roll shaft at each end of the lower work roll.
[0012] The working roller includes an upper working roller and a lower working roller. An upper cooling component is arranged near the side of the upper working roller. The upper cooling component includes an upper cooling main pipe, which is connected to multiple upper cooling branch pipes. Each upper cooling branch pipe is connected to multiple upper cooling branch pipes, and each upper cooling branch pipe is connected to a nozzle at its end.
[0013] A lower cooling component is installed near the side of the lower work roller. The lower cooling component includes a lower cooling main pipe, which is connected to multiple lower cooling branch pipes. Each lower cooling branch pipe is connected to multiple lower cooling branch pipes, and each lower cooling branch pipe is connected to a nozzle at its end.
[0014] An upper support roll is provided above the upper work roll, and a lower support roll is provided below the lower work roll. When the workpiece passes through the upper and lower work rolls, the convexity bending of the roll surface of the upper work roll and the upper support roll is close to 0 mm, and the convexity bending of the contact surface between the upper work roll and the workpiece is -0.1 to -0.2 mm; the convexity bending of the roll surface of the lower work roll and the lower support roll is close to 0 mm, and the convexity bending of the contact surface between the lower work roll and the workpiece is -0.1 to -0.2 mm.
[0015] The initial roll profile convexity of the upper support roller is +0.2mm, and the initial roll profile convexity of the lower support roller is +0.2mm.
[0016] The upper cooling sub-pipes include a central upper cooling sub-pipe, a left first upper cooling sub-pipe, a left second upper cooling sub-pipe, a right first upper cooling sub-pipe, and a right second upper cooling sub-pipe; the lower cooling sub-pipes include a central lower cooling sub-pipe, a left first lower cooling sub-pipe, a left second lower cooling sub-pipe, a right first lower cooling sub-pipe, and a right second lower cooling sub-pipe.
[0017] When the thin-gauge steel plate rolling mill structure is rolling the workpiece, the cooling water flow rate of the nozzles of each group of upper cooling pipes on the upper work roll is controlled as follows: center upper cooling pipe < left first upper cooling pipe < left second upper cooling pipe, center upper cooling pipe < right first upper cooling pipe < right second upper cooling pipe; as the running time increases, the water spray volume of the nozzles of the center upper cooling pipe decreases sequentially at different time periods, the water spray volume of the left first upper cooling pipe and the left second upper cooling pipe decreases sequentially or remains unchanged, and the water spray volume of the right first upper cooling pipe and the right second upper cooling pipe decreases sequentially or remains unchanged.
[0018] When the thin-gauge steel plate rolling mill structure is rolling the workpiece, the cooling water flow rate of the nozzles of each group of lower cooling sub-pipes of the lower work roll is controlled as follows: center lower cooling sub-pipe < left first lower cooling sub-pipe < left second lower cooling sub-pipe, center lower cooling sub-pipe < right first lower cooling sub-pipe < right second lower cooling sub-pipe; as the machine time increases, the water spray volume of the nozzles of the center lower cooling sub-pipe decreases sequentially at different time periods, the water spray volume of the left first lower cooling sub-pipe and the left second lower cooling sub-pipe decreases sequentially or remains unchanged, and the water spray volume of the right first lower cooling sub-pipe and the right second lower cooling sub-pipe decreases sequentially or remains unchanged.
[0019] The flow control valves are solenoid valves, and each flow control valve is connected to a control component.
[0020] When the thin-gauge steel plate rolling mill structure is rolling the workpiece, during the same time period, each nozzle of the upper cooling component and the corresponding nozzles of the lower cooling component are symmetrically arranged. The water spray volume of each nozzle of the upper cooling component is less than the water spray volume of the nozzles symmetrically arranged in the lower cooling component.
[0021] The steel plate rolling mill structure for thin-gauge steel plates involves steel plate rolling processes including heating, rolling, post-rolling straightening, and cooling.
[0022] In the heating process, four temperature zones are used for upper and lower layer heating. The preheating zone temperature is as follows: upper layer temperature: 650~880℃, lower layer temperature: 690~920℃; the first heating zone temperature is as follows: upper layer temperature: 920~1150℃, lower layer temperature: 970~1200℃; the second heating zone temperature is as follows: upper layer temperature: 1150~1200℃, lower layer temperature: 1190~1250℃; and the soaking zone temperature is as follows: upper layer temperature: 1140~1250℃, lower layer temperature: 1190~1300℃.
[0023] The working principle and beneficial effects of the technical solution adopted in this invention are as follows:
[0024] The thin-gauge steel plate rolling mill structure of this invention adopts dynamic linear cooling technology for the work rolls. This involves eliminating the centralized cooling method of supplying cooling water to the work rolls from a central water tank. Instead, multiple cooling branch pipes are connected to the main cooling pipe, and each branch pipe is connected to multiple cooling sub-pipes. Each sub-pipe is connected to a nozzle, and a flow control valve is installed on each sub-pipe. Each nozzle is controlled by a separate water supply pipe and flow valve. The cooling water volume is linearly controlled based on the work roll's running time (longer running time results in more severe wear and a more hollow roll profile). This is coordinated with the rolling sequence of the steel plate from wide to narrow. The principle of thermal expansion and contraction of the work rolls compensates for roll surface wear, maintaining the work roll's convexity in a slightly flat state (convexity 0 to -0.2 mm). This ensures reliable contact between the rolled piece and the work roll, keeping the deformation at the edges and center of the steel plate (rolled piece) essentially consistent. This ensures that the plate shape is controlled throughout the work roll's running time, preventing significant waviness and warping, and improving the production efficiency of thin-gauge steel plates. Meanwhile, based on the dynamic linear cooling technology of the work roll, the present invention ensures that the roll profile of the work roll is always maintained at 0 to -0.2 mm, so that the support roll is subjected to uniform force and the wear on the support roll is less than that of the rolling method with step-type integral cooling work roll. Under the linear cooling method adopted in this invention, it takes about 12 days for the support roll to wear down by 0.2mm. Therefore, the initial roll profile of the support roll can be adjusted from +0.4mm to +0.2mm. In the early stage of the support roll's use, it can be matched with the work roll with a roll profile of 0 to -0.2mm to roll thin steel plates. During the period of 0 to 12 days after the support roll is put on the mill, it can roll thin steel plates with a thickness of 5 to 6mm. In the last 3 days of the support roll's use, the roll profile crown wears down to about -0.1mm. At this time, the work roll can be bent during the finishing rolling process. The bending force of the work roll can be used to bend the work roll to a certain extent, changing the crown of the contact surface with the workpiece and the contact surface with the support roll respectively. The crown of the roll surface in contact with the support roll is bent to about 0mm, and the crown of the contact surface between the work roll and the workpiece is bent to -0.1 to -0.2mm, so that it meets the conditions for rolling thin steel plates. This enables the rolling of thin steel plates with a thickness of 5 to 6mm throughout the 15 days of the support roll's use on the mill. The thin-gauge steel plate rolling mill structure of the present invention can realize the rolling of thin-gauge steel plates in the early, middle and late stages of the use of the support rolls and work rolls, thereby increasing the rolling output of thin-gauge steel plates, shortening the production cycle and improving the delivery capability of this product. Attached Figure Description
[0025] The following is a brief explanation of the contents depicted in the accompanying drawings and the markings therein:
[0026] Figure 1 This is a front view schematic diagram of the thin-gauge steel plate rolling mill structure described in this invention;
[0027] Figure 2This is a side view of the thin-gauge steel plate rolling mill structure described in this invention.
[0028] Figure 3 This is a partial structural schematic diagram of the thin-gauge steel plate rolling mill structure described in this invention;
[0029] Figure 4 The water flow control parameters of each nozzle during the cooling of the work roll in a specific embodiment of the cooling system of the thin-gauge steel plate rolling mill structure of the present invention;
[0030] Figure 5 The parameters of Embodiment 1 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 3.
[0031] Figure 6 The parameters of Embodiment 1 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 4.
[0032] Figure 7 The parameters of Embodiment 2 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 5.
[0033] Figure 8 The parameters of Embodiment 2 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 6.
[0034] Figure 9 The parameters of Embodiment 3 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 7.
[0035] Figure 10 The parameters of Embodiment 3 of the thin-gauge steel plate rolling mill structure of the present invention are shown in Table 8.
[0036] The labels in the attached diagram are as follows: 1. Cooling component; 2. Work roller; 3. Main cooling pipe; 4. Sub-cooling pipe; 5. Cooling branch pipe; 6. Nozzle; 7. Flow control valve; 8. Roller shaft;
[0037] 11. Center upper cooling branch pipe; 12. Left first upper cooling branch pipe; 13. Left second upper cooling branch pipe; 14. Right first upper cooling branch pipe; 15. Right second upper cooling branch pipe;
[0038] 21. Upper work roll; 22. Lower work roll; 23. Upper cooling unit; 24. Lower cooling unit; 25. Upper support roll; 26. Lower support roll; 27. Rolled workpiece;
[0039] 31. Center lower cooling branch pipe; 32. Left first lower cooling branch pipe; 33. Left second lower cooling branch pipe; 34. Right first lower cooling branch pipe; 35. Right second lower cooling branch pipe. Detailed Implementation
[0040] The following description, with reference to the accompanying drawings, provides a more detailed explanation of the specific embodiments of the present invention, including the shape and structure of each component, the relative positions and connections between the parts, the functions and working principles of each part:
[0041] As attached Figure 1 - Appendix Figure 3 As shown, this invention relates to a thin-gauge steel plate rolling mill structure. A cooling component 1 is located on the side of the work roll 2. The cooling component 1 includes a main cooling pipe 3, which is connected to multiple cooling branch pipes 4. Each cooling branch pipe 4 is connected to multiple cooling branch pipes 5, and each cooling branch pipe 5 has a nozzle 6 connected to its end. A flow control valve 7 is installed on each cooling branch pipe 5. A cooling branch pipe 4 is located in the middle of the work roll 2, and multiple cooling branch pipes 4 are arranged at intervals from the middle of the work roll 2 outwards to both sides. The water spray volume of the nozzles 6 in the cooling branch pipes 4 from the middle of the work roll 2 to the side of the work roll 2 is arranged in a progressively decreasing structure. The work roll 2 is a convex roll. When the roll profile convexity of the work roll 2 wears to below -0.1mm, the roller shaft 8 at each end of the upper work roll 2 is subjected to a downward bending force, and the roller shaft 8 at each end of the lower work roll 2 is subjected to an upward bending force. This structure addresses the shortcomings of the prior art by proposing an improved technical solution. The thin-gauge steel plate rolling mill structure of this invention employs dynamic linear cooling technology for the work rolls. Specifically, it eliminates the centralized cooling method of supplying cooling water to the work rolls from a central water tank. Instead, multiple cooling branch pipes 4 are connected to the main cooling pipe 3, and each branch pipe 4 is connected to multiple cooling branch pipes 5. Each cooling branch pipe 5 is connected to a nozzle 6 at its end, and a flow control valve 7 is installed on each branch pipe 5. Thus, each nozzle is controlled by a separate water supply pipe and flow valve. The cooling water volume is linearly controlled based on the working time of the work roll 2 (the longer the working time, the more severe the wear of the work roll and the more hollow the roll profile). Figure 1 and Figure 2 ,See Figure 4(Table 1) By arranging the rolling sequence of the steel plate from wide to narrow, the principle of thermal expansion and contraction of the work rolls is used to compensate for roll surface wear, maintaining the convexity of the work rolls in a slightly flat state (convexity 0 to -0.2 mm). This ensures reliable contact between the rolled piece 27 and the work roll 2, making the deformation at the edges and center of the steel plate (rolled piece) basically consistent. This ensures that the plate shape is controlled throughout the work roll's operation, preventing obvious waviness and warping problems, and improving the production efficiency of thin-gauge steel plates. Simultaneously, based on the dynamic linear cooling technology of the work rolls, this invention maintains the work roll profile at 0 to -0.2 mm, resulting in uniform stress on the support rolls. The wear on the support rolls is less than that of the integral cooling work roll method with stepped sections. In the existing integral cooling method, it takes about 7 days for the support roll to wear 0.2 mm, about 12 days for 0.4 mm wear, and about 15 days for the entire operation. In the last 3 days, the roll profile convexity is about -0.2 mm. Under the linear cooling method adopted in this invention, it takes approximately 12 days for the support roll to wear down by 0.2mm. Therefore, the initial roll profile of the support roll can be adjusted from +0.4mm to +0.2mm. In the initial stage of operation, the support roll can be matched with the work roll (0 to -0.2mm profile) to roll thin steel plates. For approximately 12 days after operation, it can roll thin steel plates with a thickness of 5-6mm. In the last 3 days of use, the roll crown wears down to approximately -0.1mm. At this point, bending operations on the work roll can be used during the finishing rolling process. Figure 3 As shown, the work roll is bent to a certain extent using bending force, thereby changing the convexity of the contact surface with the workpiece and the contact surface with the support roll. The convexity of the work roll contacting the support roll is bent to approximately 0 mm, and the convexity of the work roll contacting the workpiece is bent to -0.1 to -0.2 mm, meeting the conditions for rolling thin-gauge steel plates. This allows for the rolling of 5-6 mm thick thin-gauge steel plates throughout the 15-day period of the support roll's operation. Through this improvement, thin-gauge steel plates can be rolled in the early, middle, and late stages of the support roll and work roll's operation, increasing the rolling output of thin-gauge steel plates, shortening the production cycle, and improving the delivery capacity of this product. In summary, the thin-gauge steel plate rolling mill structure described in this invention is simple in structure and employs dynamic linear cooling technology for the work rolls. It utilizes the principle of thermal expansion and contraction of the work rolls to compensate for roll surface wear, maintaining the convexity of the work rolls in a slightly flat state at all times. This ensures reliable contact between the rolled piece (steel plate) and the work rolls, making the deformation at the edges and in the middle of the rolled piece basically consistent. It also ensures that the plate shape is controlled throughout the entire process of the work rolls running on the mill, without obvious waviness or warping problems, thereby improving the rolling quality and production efficiency of thin-gauge rolled pieces.
[0042] The working roller 2 includes an upper working roller 21 and a lower working roller 22. An upper cooling component 23 is provided near the side of the upper working roller 21. The upper cooling component 23 includes an upper cooling main pipe, which is connected to multiple upper cooling branch pipes. Each upper cooling branch pipe is connected to multiple upper cooling branch pipes, and each upper cooling branch pipe is connected to a nozzle 6 at its end.
[0043] A lower cooling component 24 is provided near the side of the lower working roller 22. The lower cooling component 24 includes a lower cooling main pipe, which is connected to multiple lower cooling branch pipes. Each lower cooling branch pipe is connected to multiple lower cooling branch pipes, and each lower cooling branch pipe is connected to a nozzle 6 at its end.
[0044] An upper support roll 25 is positioned above the upper work roll 21, and a lower support roll 26 is positioned below the lower work roll 22. When the workpiece 27 passes through the upper work roll 21 and the lower work roll 22, the roll surface convexity of the upper work roll 21 and the upper support roll 25 is close to 0 mm, and the convexity of the contact surface between the upper work roll 21 and the workpiece 27 is -0.1 to -0.2 mm. Similarly, the roll surface convexity of the lower work roll 22 and the lower support roll 26 is close to 0 mm, and the convexity of the contact surface between the lower work roll 22 and the workpiece 27 is -0.1 to -0.2 mm. The initial roll profile convexity of the upper support roll 25 and the lower support roll 26 is both +0.2 mm. This structure, with the upper work roll 21 and the upper support roll 25 cooperating, and the lower work roll 22 and the lower support roll 26 cooperating, satisfies the rolling requirements of the workpiece. Under the linear cooling method adopted in this invention, it takes approximately 12 days for the support roll to wear down by 0.2mm. Therefore, the initial roll profile of the support roll can be adjusted from +0.4mm to +0.2mm. This allows the support roll to be matched with the work roll (0 to -0.2mm profile) for rolling thin steel plates from the initial stage of operation. For approximately 0 to 12 days after operation, it can roll thin steel plates with a thickness of 5 to 6mm. In the last 3 days of use, the roll crown wears down to approximately -0.1mm. At this point, bending operations on the work roll can be used during the finishing rolling process. Figure 3 As shown, the work roll is bent by applying a bending force, which changes the convexity of the contact surface with the workpiece and the contact surface with the support roll. The convexity of the work roll contacting the support roll is bent to approximately 0 mm, while the convexity of the work roll contacting the workpiece is bent to -0.1 to -0.2 mm. This meets the requirements for rolling thin steel plates, enabling the rolling of 5-6 mm thick thin steel plates throughout the 15-day operation of the support roll. The work roll end shaft is mounted on a connecting seat, which is connected to a telescopic cylinder. When a bending force is required, the telescopic component extends, applying a specific magnitude and direction of bending force to the end shaft. Since the work roll and support roll are in contact, the bending force is applied to both sides of the work roll.
[0045] The upper cooling sub-pipes include a central upper cooling sub-pipe 11, a left first upper cooling sub-pipe 12, a left second upper cooling sub-pipe 13, a right first upper cooling sub-pipe 14, and a right second upper cooling sub-pipe 15; the lower cooling sub-pipes include a central lower cooling sub-pipe 31, a left first lower cooling sub-pipe 32, a left second lower cooling sub-pipe 33, a right first lower cooling sub-pipe 34, and a right second lower cooling sub-pipe 35. In this structure, the central upper cooling sub-pipe 11, the left first upper cooling sub-pipe 12, the left second upper cooling sub-pipe 13, the right first upper cooling sub-pipe 14, and the right second upper cooling sub-pipe 15 are each equipped with multiple upper nozzles, thus forming multiple sets of upper nozzles. Each set of upper nozzles can be controlled independently, and the flow rate of each nozzle within a set can also be controlled independently. The central lower cooling sub-pipe 31, the left first lower cooling sub-pipe 32, the left second lower cooling sub-pipe 33, the right first lower cooling sub-pipe 34, and the right second lower cooling sub-pipe 35 are each equipped with multiple lower nozzles, thus forming multiple sets of lower nozzles. In this way, each group of lower nozzles can be controlled individually, and the flow rate of each lower nozzle within a group can also be controlled individually, achieving linear dynamic and differentiated control of cooling water.
[0046] When the thin-gauge steel plate rolling mill structure is rolling the workpiece, the cooling water flow rate of the nozzles 6 of each group of upper cooling sub-pipes of the upper work roll 21 is controlled as follows: center upper cooling sub-pipe 11 < left first upper cooling sub-pipe 12 < left second upper cooling sub-pipe 13, center upper cooling sub-pipe 11 < right first upper cooling sub-pipe 14 < right second upper cooling sub-pipe 15; as the machine time increases, the spray water volume of the nozzles 6 of the center upper cooling sub-pipe decreases sequentially at different time periods, the spray water volume of the left first upper cooling sub-pipe 12 and left second upper cooling sub-pipe 13 decreases sequentially or remains unchanged, and the spray water volume of the right first upper cooling sub-pipe 14 and right second upper cooling sub-pipe 15 decreases sequentially or remains unchanged. When the thin-gauge steel plate rolling mill structure is rolling the workpiece, the cooling water flow rate of the nozzles 6 of each group of lower cooling sub-pipes of the lower work roll 22 is controlled as follows: center lower cooling sub-pipe 31 < left first lower cooling sub-pipe 32 < left second lower cooling sub-pipe 33, center lower cooling sub-pipe 31 < right first lower cooling sub-pipe 34 < right second lower cooling sub-pipe 35; as the machine time increases, the water spray volume of the nozzles 6 of the center lower cooling sub-pipe 31 decreases sequentially at different time periods, the water spray volume of the left first lower cooling sub-pipe 32 and the left second lower cooling sub-pipe 33 decreases sequentially or remains unchanged, and the water spray volume of the right first lower cooling sub-pipe 34 and the right second lower cooling sub-pipe 35 decreases sequentially or remains unchanged. The above settings differentiate and dynamically adjust the water flow rates for different groups of nozzles in the upper cooling component and the lower cooling component. Each nozzle is controlled by a separate water supply pipe and flow valve, and the cooling water flow is linearly controlled based on the working roller's operating time (longer operating time results in more severe roller wear and a more hollow roller profile). Figure 1 and Figure 2 ,See Figure 4 (Table 1, the unit of water flow rate data for each nozzle in Table 1 is: m) 3 / h), in conjunction with the rolling sequence of steel plates from wide to narrow, the principle of thermal expansion and contraction of the work rolls is used to compensate for the wear of the roll surface, and the convexity of the work rolls is always kept in a slightly flat state (convexity 0 to -0.2mm), ensuring that the rolled piece 27 and the work roll 2 are reliably attached, so that the deformation of the edge and the middle of the steel plate is basically consistent, ensuring that the plate shape is controlled throughout the process of the work rolls on the machine, without obvious waviness and warping problems, and improving the production efficiency of thin-gauge steel plates.
[0047] The flow control valve 7 is a solenoid valve, and each flow control valve 7 is connected to a control component. In this structure, each flow control valve's opening degree and start / stop are controlled by the control component, thereby enabling each nozzle to be supplied with cooling water independently. This improves the control accuracy of the cooling water flow, creates a dynamic linear cooling water supply, enhances cooling reliability, and improves rolling performance.
[0048] When the thin-gauge steel plate rolling mill structure described above rolls the workpiece, within the same on-machine time period, each nozzle 6 of the upper cooling component 23 and the corresponding nozzle 6 of the lower cooling component 24 are symmetrically arranged. The water spray volume of each nozzle 6 of the upper cooling component 23 is less than the water spray volume of the nozzles 6 symmetrically arranged in the lower cooling component 24. In the above structure, the upper cooling component includes multiple nozzles, which are called upper nozzles, and the lower cooling component includes multiple nozzles, which are called lower nozzles. The upper cooling component is set at the front and rear of the upper work roll, and each upper nozzle is aligned with the joint of the upper work roll and the upper support roll. Similarly, the lower cooling component is set at the front and rear of the lower work roll, and each upper nozzle is aligned with the joint of the upper work roll and the upper support roll, thus achieving precise and reliable cooling.
[0049] The aforementioned thin-gauge steel plate rolling mill structure involves steel plate rolling processes including heating, rolling, post-rolling straightening, and cooling. In the heating process, four temperature zones are used for upper and lower layer partitioning. The preheating zone temperatures are: upper layer: 650–880℃, lower layer: 690–920℃; first heating zone temperatures: upper layer: 920–1150℃, lower layer: 970–1200℃; second heating zone temperatures: upper layer: 1150–1200℃, lower layer: 1190–1250℃; and soaking zone temperatures: upper layer: 1140–1250℃, lower layer: 1190–1300℃. This configuration, by partitioning the four temperature zones of the heating furnace for upper and lower layer partitioning, achieves differentiated heating between the upper and lower layers, i.e., differentiated heating between different sections. The upper heating temperature is controlled 40-50°C lower than the lower temperature, fully utilizing the upward tendency of high-temperature flue gas. This enhances the heating capacity of the lower part while ensuring uniform heating of the billet as a whole. It avoids the problem of prolonged residence time in the soaking zone to achieve uniform billet temperature, effectively shortening the batch storage time in the furnace. This reduces the temperature difference between the upper and lower surfaces of the billet to approximately 10-20°C when tapped, providing conditions for subsequent shape control of thin-gauge steel plates. These improvements enhance the processing quality of the rolled products.
[0050] The following is a further description through specific embodiments of the device of the present invention.
[0051] (1) Example 1:
[0052] This embodiment of the double-stand heavy plate rolling mill efficiently produces thin-gauge steel plates with a thickness of 5mm and a width of 2900mm. The steel plate grade is Q345R. The steel plate production method of this embodiment includes heating, rolling, post-rolling straightening, and cooling processes. The specific process steps are as follows: Heating process: The billet thickness is 180mm. Four temperature sections are used for upper and lower layer heating. Preheating section temperature: upper layer temperature: 650~880℃, lower layer temperature: 690~920℃; First heating section temperature: upper layer temperature: 920~1150℃, lower layer temperature: 970~1200℃; Second heating section temperature: upper layer temperature: 1150~1200℃, lower layer temperature: 1190~1250℃; Soaking section temperature: upper layer temperature: 1140~1250℃, lower layer temperature: 1190~1300℃; Furnace holding time: 270 minutes.
[0053] Rolling process: The initial roll profile crown of the finishing mill support rolls is +0.2mm. Thin-gauge steel plates can be rolled within the 0-12 day period after the support rolls are installed. Simultaneously, the initial roll profile crown of the work rolls is -0.1mm. Dynamic linear cooling technology is used for the work roll cooling water, and the cooling water flow rate is controlled according to Table 2. During work roll rolling, the steel plate rolling width is arranged from widest to narrowest. Since the finished width of this billet is 2900mm, which is the widest dimension that the mill can roll, it is scheduled for rolling within 0-0.5 hours after the work rolls are installed.
[0054] The roughing rolling process begins at 1159℃ and ends at 1053℃, producing an intermediate billet thickness of 68mm. Five rolling passes are used. High-pressure water descaling is applied in the first and third passes, while widening is performed in the second and fourth passes to ensure the intermediate billet width matches the finished steel plate width. The intermediate billet is then rapidly conveyed to the finishing mill via a conveyor roller conveyor. The finishing rolling process begins at 1013℃ and ends at 843℃, with five rolling passes completed. High-pressure water descaling is only applied in the first pass. The entire process is longitudinal rolling, followed by air cooling. The hot straightening process uses an eleven-roll online hot straightener. The initial straightening temperature is 733℃, with a first straightening force of 23000KN, a second straightening force of 18000KN, and a third straightening force of 15000KN. The final straightening temperature is 565℃. The cooling process involves natural cooling on a cooling bed. Steel plates are prohibited from being stacked, and the spacing between each row of plates should be at least 300mm to ensure uniform cooling. The properties and straightness of the steel plate in this embodiment are shown in Tables 3 and 4, respectively.
[0055] Figure 5 Table 3 shows the performance data of the 5mm Q345R steel plate in Example 1.
[0056] Figure 6 Table 4 shows the unevenness data of the 5mm Q345R steel plate in Example 1.
[0057] As can be seen from the performance test results and flatness measurement results in Tables 3 and 4, the 5mm Q345R steel plate has good performance and flatness indicators, which fully meet the delivery requirements of Q345R.
[0058] (2) Example 2:
[0059] This embodiment describes a dual-stand heavy plate rolling mill for the efficient production of thin-gauge steel plates with a thickness of 5mm and a width of 2200mm. The steel plate grade is Q345R. The steel plate production method in this embodiment includes heating, rolling, post-rolling straightening, and cooling processes. The specific process steps are as follows:
[0060] Heating process: The billet thickness is 180mm. Four temperature zones are used for upper and lower layer heating. Preheating zone temperature: upper layer temperature: 630~870℃, lower layer temperature: 680~915℃; first heating zone temperature: upper layer temperature: 915~1140℃, lower layer temperature: 955~1190℃; second heating zone temperature: upper layer temperature: 1140~1200℃, lower layer temperature: 1190~1250℃; soaking zone temperature: upper layer temperature: 1150~1250℃, lower layer temperature: 1190~1300℃; furnace holding time: 250 minutes.
[0061] Rolling process: The initial roll profile crown of the finishing mill support rolls is +0.2mm. Thin-gauge steel plates can be rolled within the 0-12 day period after the support rolls are installed. Simultaneously, the initial roll profile crown of the work rolls is -0.1mm. Dynamic linear cooling technology is used for the work roll cooling water, and the cooling water flow rate is controlled according to Table 2. During work roll rolling, the steel plate rolling width is arranged from widest to narrowest. Since the finished width of this billet is 2200mm, which is an intermediate dimension for the mill, it is scheduled for rolling within 2-5 hours after the work rolls are installed.
[0062] The roughing rolling temperature is 1160℃, the finishing rolling temperature is 1056℃, the thickness of the intermediate billet after rolling is 65mm, and there are 5 rolling passes. The first and third passes are descaled with high-pressure water, and the second and fourth passes are used to widen the billet so that the width of the intermediate billet is consistent with the width of the finished steel plate. After rolling, the intermediate billet is quickly transported to the front of the finishing mill by the conveyor rollers. The finishing rolling temperature is 1015℃, the finishing rolling temperature is 841℃, and the rolling passes are controlled to be completed in 5 passes. High-pressure water descaling is only used in the first pass. The entire process is longitudinal rolling, and the billet is air-cooled after rolling.
[0063] The hot straightening process uses an eleven-roll online hot straightener. The initial straightening temperature is 743℃, the first straightening force is 23300KN, the second straightening force is 19300KN, the third straightening force is 14600KN, and the final straightening temperature is 535℃. In the cooling process, the steel plates are allowed to cool naturally on a cooling bed. Stacking is prohibited, and the spacing between each row of steel plates should be at least 300mm to ensure uniform cooling.
[0064] The steel plate properties and straightness in this embodiment are shown in [the original text]. Figure 7 (Table 5) and Figure 8 (Table 6)
[0065] Table 5 shows the performance of the 5mm Q345R steel plate in Example 2.
[0066] Table 6. Unevenness of 5mm Q345R steel plate in Example 2 (Table 6)
[0067] As can be seen from the performance test results and flatness measurement results in Tables 5 and 6, the various performance indicators and flatness indicators of the 5mm Q345R steel plate are good, and fully meet the delivery requirements of Q345R.
[0068] (3) Example 3:
[0069] This embodiment describes a dual-stand heavy plate rolling mill for the efficient production of thin-gauge steel plates with a thickness of 6mm and a width of 1800mm. The steel plate is made of Q345C. The steel plate production method in this embodiment includes heating, rolling, post-rolling straightening, and cooling processes. The specific process steps are as follows:
[0070] Heating process: The billet thickness is 210mm. Four temperature zones are used for upper and lower layer heating. Preheating zone temperature: upper layer temperature: 650~900℃, lower layer temperature: 700~950℃; first heating zone temperature: upper layer temperature: 915~1150℃, lower layer temperature: 965~1200℃; second heating zone temperature: upper layer temperature: 1160~1200℃, lower layer temperature: 1210~1250℃; soaking zone temperature: upper layer temperature: 1160~1250℃, lower layer temperature: 1200~1300℃; furnace holding time: 280 minutes.
[0071] Rolling process: The initial roll profile crown of the finishing mill support rolls is +0.2mm. Thin-gauge steel plates can be rolled within the 0-12 day period after the support rolls are installed. Simultaneously, the initial roll profile crown of the work rolls is -0.1mm. Dynamic linear cooling technology is used for the work roll cooling water, and the cooling water flow rate is controlled according to Table 2. During work roll rolling, the steel plate rolling width is arranged from widest to narrowest. Since the finished width of this billet is 1800mm, which is a narrow dimension for the mill, it is scheduled for rolling within 5-7 hours after the work rolls are installed.
[0072] The roughing rolling temperature is 1157℃, the finishing rolling temperature is 1059℃, the thickness of the intermediate billet after rolling is 70mm, and there are 5 rolling passes. The first and third passes are descaled with high-pressure water, and the second and fourth passes are used to widen the billet so that the width of the intermediate billet is consistent with the width of the finished steel plate. After rolling, the intermediate billet is quickly transported to the front of the finishing mill by the conveyor rollers. The finishing rolling temperature is 1021℃, the finishing rolling temperature is 846℃, and the rolling passes are controlled to be completed in 5 passes. High-pressure water descaling is only used in the first pass. The entire process is longitudinal rolling, and the billet is air-cooled after rolling.
[0073] The hot straightening process uses an eleven-roll online hot straightener. The initial straightening temperature is 748℃, the first straightening force is 23900KN, the second straightening force is 20100KN, the third straightening force is 15300KN, and the final straightening temperature is 515℃.
[0074] During the cooling process, the steel plates are allowed to cool naturally on a cooling bed. Stacking of steel plates is prohibited, and the spacing between each row of steel plates should be more than 300mm to ensure uniform cooling.
[0075] The steel plate properties and straightness in this embodiment are shown in [the original text]. Figure 9 (Table 7) and Figure 10 (Table 8)
[0076] Table 7 shows the performance of 6mm Q345R steel plate in Example 3.
[0077] Table 8. Unevenness of 6mm Q345R steel plate in Example 3.
[0078] As can be seen from the performance test results and flatness measurement results in Tables 7 and 8, the various performance indicators and flatness indicators of the 6mm Q345R steel plate are good, and fully meet the delivery requirements of Q345R.
[0079] The present invention has been described above by way of example with reference to the accompanying drawings. Obviously, the specific implementation of the present invention is not limited to the above-described manner. Any improvements made by adopting the inventive concept and technical solution of the present invention, or the direct application of the inventive concept and technical solution of the present invention to other occasions without modification, are all within the protection scope of the present invention.
Claims
1. A method of using a thin-gauge steel plate rolling mill structure, characterized in that: The cooling component (1) is located on the side of the working roller (2). The cooling component (1) includes a cooling main pipe (3), which is connected to multiple cooling branch pipes (4). Each cooling branch pipe (4) is connected to multiple cooling branch pipes (5). Each cooling branch pipe (5) is connected to a nozzle (6) at its end. Each cooling branch pipe (5) is equipped with a flow control valve (7). A cooling branch pipe (4) is located in the middle of the working roller (2). Multiple cooling branch pipes (4) are set at intervals from the middle of the working roller (2) to both sides. The water spray volume of the nozzles (6) of the cooling branch pipes (4) from the middle of the working roller (2) to the side of the working roller (2) is set to decrease sequentially. The working roller (2) is a convex roller. When the convexity of the working roller (2) is worn to below -0.1mm, the roller shafts (8) at each end of the upper working roller (2) are subjected to a downward bending force, and the roller shafts (8) at each end of the lower working roller (2) are subjected to an upward bending force. An upper cooling component (23) is provided near the side of the upper working roller (21). The upper cooling component (23) includes an upper cooling main pipe, and multiple upper cooling sub-pipes are connected to the upper cooling main pipe. A lower cooling component (24) is provided near the side of the lower working roller (22). The lower cooling component (24) includes a lower cooling main pipe and multiple lower cooling sub-pipes are connected to the lower cooling main pipe. The upper cooling sub-pipes include a central upper cooling sub-pipe (11), a left first upper cooling sub-pipe (12), a left second upper cooling sub-pipe (13), a right first upper cooling sub-pipe (14), and a right second upper cooling sub-pipe (15); the lower cooling sub-pipes include a central lower cooling sub-pipe (31), a left first lower cooling sub-pipe (32), a left second lower cooling sub-pipe (33), a right first lower cooling sub-pipe (34), and a right second lower cooling sub-pipe (35). During the rolling of the workpiece, as the time on the machine increases, the amount of water sprayed by the nozzles (6) of the center upper cooling sub-pipe (11) and the center lower cooling sub-pipe (31) decreases sequentially at different time periods. The amount of water sprayed by the left first upper cooling sub-pipe (12) and the left second upper cooling sub-pipe (13) decreases sequentially or remains unchanged. The amount of water sprayed by the right first upper cooling sub-pipe (14) and the right second upper cooling sub-pipe (15) decreases sequentially or remains unchanged. The amount of water sprayed by the left first lower cooling sub-pipe (32) and the left second lower cooling sub-pipe (33) decreases sequentially or remains unchanged. The amount of water sprayed by the right first lower cooling sub-pipe (34) and the right second lower cooling sub-pipe (35) decreases sequentially or remains unchanged. An upper support roller (25) is provided above the upper working roller (21), and a lower support roller (26) is provided below the lower working roller (22). The initial roll profile convexity of the upper support roller (25) is +0.2mm, and the initial roll profile convexity of the lower support roller (26) is +0.2mm; In the initial stage of the support rolls' use, they are matched with work rolls with a roll profile convexity of 0 to -0.2 mm to roll thin steel plates. During the first 0 to 12 days after the support rolls are put on the mill, thin steel plates with a thickness of 5 to 6 mm are rolled. During the 13th to 15th day of the support rolls' use, the work rolls are bent during the finishing rolling process. The work rolls are bent by the applied bending force, which changes the convexity of the contact surface with the workpiece and the contact surface with the support rolls. The convexity of the roll surface in contact with the support rolls is close to 0 mm, and the convexity of the contact surface between the work rolls and the workpiece is -0.1 to -0.2 mm. This allows for the rolling of thin steel plates with a thickness of 5 to 6 mm throughout the 15 days of the support rolls' use on the mill.
2. The method of using the thin-gauge steel plate rolling mill structure according to claim 1, characterized in that: Each upper cooling branch pipe connects to multiple upper cooling branch pipes, and each upper cooling branch pipe end is connected to a nozzle (6).
3. The method of using the thin-gauge steel plate rolling mill structure according to claim 1, characterized in that: Each lower cooling branch pipe connects to multiple lower cooling sub-pipes, and each lower cooling sub-pipe is connected to a nozzle (6) at its end.
4. The method of using the thin-gauge steel plate rolling mill structure according to claim 1, characterized in that: When the thin-gauge steel plate rolling mill structure is rolling the workpiece, during the same time period, each nozzle (6) of the upper cooling component (23) and the corresponding nozzle (6) of the lower cooling component (24) are symmetrically arranged. The water spray volume of each nozzle (6) of the upper cooling component (23) is less than the water spray volume of the nozzle (6) symmetrically arranged in the lower cooling component (24).
5. The method of using the thin-gauge steel plate rolling mill structure according to claim 1 or 2, characterized in that: The steel plate rolling mill structure for thin-gauge steel plates involves steel plate rolling processes including heating, rolling, post-rolling straightening, and cooling. In the heating process, four temperature zones are used for upper and lower layer heating. The preheating zone temperature is as follows: upper layer temperature: 650~880℃, lower layer temperature: 690~920℃; the first heating zone temperature is as follows: upper layer temperature: 920~1150℃, lower layer temperature: 970~1200℃; the second heating zone temperature is as follows: upper layer temperature: 1150~1200℃, lower layer temperature: 1190~1250℃; and the soaking zone temperature is as follows: upper layer temperature: 1140~1250℃, lower layer temperature: 1190~1300℃.
Citation Information
Patent Citations
Hot rolling facility of steel plate and hot rolling method
CN101253011A
Segmented heating device
CN110153188A
Segmented cooling device for hot-rolling working roll
CN112264466A
Four-roller system with large-offset slab to control working-roller
CN1169342A