A vacuum drying device and vacuum drying method thereof

By using a multi-stage reduced pressure drying method and a uniform air device in the crystallization film formation process of perovskite solar cells, the problem of uneven drying environment and rate is solved, uniform drying of the coating layer and high-quality film formation are achieved, improving improve battery performance and production efficiency.

CN118463512BActive Publication Date: 2024-10-11ZHEJIANG YUCHENDONG INTELLIGENT TECH CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410909808.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-10-11
Estimated Expiration
2044-07-09

AI Technical Summary

Technical Problem

In the existing technology, in the crystallization film forming process of perovskite solar cells, the drying environment and uneven speed lead to coating layer quality and performance problems, affecting the surface quality and performance of the battery.

Method used

Design a decompression drying device, including a vacuum chamber, a decompression device, an air supply device, an air pressure detector and a PLC control system. The air pressure is adjusted through a multi-stage decompression drying method to ensure the stability and consistency of the drying process and utilize uniformity. The uniform airflow of the wind device prevents surface defects of the coating layer.

Benefits of technology

It achieves uniform drying of the coating layer, improves product quality and performance, reduces defects such as uneven film thickness, flow marks, cracks, and dents, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118463512B_ABST
    Figure CN118463512B_ABST
Patent Text Reader

Abstract

The invention discloses a reduced pressure drying device and a reduced pressure drying method thereof, which are used to carry out reduced pressure drying on a substrate with a solvent coating layer, and include a vacuum chamber, a reduced pressure device, an air supply device, an air pressure detector and a PLC control system; the substrate is placed in the vacuum chamber, an exhaust port and an air supply port are provided at the bottom of the vacuum chamber, and are respectively connected to the reduced pressure device and the air supply device; the air pressure detector is used to detect the air pressure in the vacuum chamber, the PLC control system receives the air pressure value detected by the air pressure detector, and the reduced pressure device and the air supply device are connected to the PLC control system; the reduced pressure drying device has good preparation uniformity and high quality; the reduced pressure drying method is easy to operate, and can reduce defects such as uneven film thickness, flow marks, cracks, dents, wind spots, etc. that occur during the reduced pressure drying process through multi-stage reduced pressure drying.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery preparation devices, and in particular to a reduced pressure drying device and a reduced pressure drying method thereof. Background Art

[0002] At present, perovskite solar cells have become the most potential substitute for silicon-based solar cells due to their advantages such as high photoelectric conversion efficiency, low cost and simple process. The production of perovskite solar cells requires the preparation of a variety of transport layers or conductive layers on the surface of a transparent substrate. Conventional ones include transparent conductive oxides, electron transport layers, perovskite layers, hole transport layers and back electrodes. Dry or wet processes are used to prepare various transport layers. Among them, the commonly used film-forming methods of wet processes include slit coating, spin coating or vapor deposition. However, after the preparation is completed, crystallization film formation is required. Only after the process is completed can the transport layer be qualified for use. Common equipment for crystallization film formation process includes annealing furnace and vacuum drying device. According to the experience of semiconductor industry production lines and the characteristics of perovskite materials, vacuum drying devices are currently used for crystallization film formation. The principle is to reduce the pressure of the transport layer coated with solvent, so that the solvent inside the coating layer reaches the saturated vapor pressure and then evaporates the solvent gas until the coating layer is dry, achieving a high-quality, high-performance coating layer.

[0003] Since the drying is carried out in a wet film state, the environment and the drying effect have a direct impact on the quality and performance of the coating. The drying environment is carried out under negative pressure. If the environment contains impurities, oil mist, high oxygen content, harmful gases, etc., it will directly affect the purity of the solvent and affect the quality and performance of the coating. The drying effect will also directly affect the surface quality and performance of the coating. If the drying rate is low, uneven drying will occur, the internal density of the coating will be poor, and solvent agglomeration will occur. A high drying rate will affect the surface roughness of the coating, and there will be more pinhole defects under the microscopic level. If the existing technology only dries at the same rate throughout the entire drying process, it will affect the quality of the coating. Summary of the invention

[0004] In order to overcome the above-mentioned defects in the prior art, a reduced pressure drying device and a reduced pressure drying method capable of rapid reduced pressure drying are provided.

[0005] The technical solution of the present invention is as follows: a reduced-pressure drying device for performing reduced-pressure drying on a substrate with a solvent coating layer, comprising a vacuum chamber, a reduced-pressure device, an air supply device, an air pressure detector and a PLC control system; the substrate is placed in the vacuum chamber, and an exhaust port and an air supply port are provided at the bottom of the vacuum chamber, which are respectively connected to the reduced-pressure device and the air supply device; the air pressure detector is used to detect the air pressure in the vacuum chamber, the PLC control system receives the air pressure value detected by the air pressure detector, and the reduced-pressure device and the air supply device are connected to the PLC control system.

[0006] Preferably, a substrate tray and a slide rail are provided in the vacuum chamber; the slide rail is mounted on both sides of the inner wall of the vacuum chamber, the substrate tray is used to connect the substrate and the slide rail, and the substrate tray is slidably connected on the slide rail.

[0007] Preferably, a uniform air flow device for uniform air pressure is also provided in the vacuum chamber.

[0008] Preferably, the uniform air flow device comprises an upper uniform air flow device and a lower uniform air flow device; the upper uniform air flow device is mounted above the substrate tray; and the lower uniform air flow device is mounted above the bottom of the vacuum chamber.

[0009] Preferably, the pressure reducing device comprises a vacuum pump and an exhaust regulating valve, and the exhaust regulating valve is assembled on a stainless steel hose provided between the vacuum pump and the exhaust port.

[0010] Preferably, the gas supply device includes a gas supply source and a gas supply regulating valve, and the gas supply regulating valve is assembled on a stainless steel hose provided between the gas supply source and the gas supply port.

[0011] Preferably, a signal communication line for transmitting instructions is provided between the PLC control system and the air pressure detector, the pressure reducing device and the air supply device.

[0012] Preferably, a chamber door panel and a door lock assembly are provided on the side of the vacuum chamber, and the door lock assembly is used to fasten the chamber door panel and the vacuum chamber.

[0013] Preferably, a vacuum observation window is provided above the vacuum chamber.

[0014] Part 2, a reduced pressure drying method of a reduced pressure drying device, comprising the following steps:

[0015] S1. Assemble the reduced pressure drying device: place the substrate with the solvent coating layer on the fixed position of the substrate tray, with the side with the solvent coating layer facing upward, install the uniform air device, push the substrate tray into the vacuum chamber and fix it, close the chamber door to make the vacuum chamber sealed, and the initial atmospheric pressure is point P1;

[0016] S2, implement the first stage of reduced pressure drying: start the decompression device, adjust the exhaust regulating valve, and exhaust the internal environment of the vacuum chamber to the pressure of point a at the decompression speed V1, and extract the gas containing moisture in the vacuum chamber; close the decompression device, open the gas supply device, and adjust the gas supply regulating valve to restore the inside of the vacuum chamber to the atmospheric pressure point P1; close the gas supply device, open the decompression device, and adjust the exhaust regulating valve, and the gas pressure of the vacuum chamber is reduced to point P2 at the decompression speed V1 for the second time; close the decompression device, open the gas supply device, and adjust the gas supply regulating valve to restore the inside of the vacuum chamber to the atmospheric pressure point P1;

[0017] S3, implement the second stage of reduced pressure drying: close the gas supply device, open the pressure reducing device, adjust the exhaust regulating valve, and reduce the pressure of the vacuum chamber to point P3 at the pressure reducing speed V2;

[0018] S4, implement the third stage of reduced pressure drying: adjust the exhaust regulating valve, reduce pressure and exhaust gas at the reduced pressure speed V3, and reduce pressure to point P4;

[0019] S5, implement the fourth stage of decompression drying: adjust the exhaust regulating valve to decompress and evacuate the vacuum chamber at a decompression speed V4 until the air pressure drops to point P5;

[0020] S6. Close the pressure reducing device, open the air supply regulating valve, and take out the dried substrate.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] A decompression drying device, through the cooperation of the decompression device and the air supply device, adjusts the air pressure of the vacuum chamber, thereby changing the drying rate of the solvent coating layer on the substrate, making it dry evenly and improving the product quality; the PLC control system detects the air pressure through the air pressure detector. The air pressure in the vacuum chamber is adjusted as needed. The PLC control system automatically controls the decompression device and the air supply device to ensure the stability and consistency of the drying process and improve production efficiency.

[0023] A reduced pressure drying method for a reduced pressure drying device is convenient to operate. Through multi-stage reduced pressure drying, it can reduce defects such as uneven film thickness, flow marks, cracks, dents, wind spots, etc. that occur during the reduced pressure drying process. In the first stage of reduced pressure drying, the air with water vapor is reduced in the vacuum chamber by multiple reduced pressure air supply, thereby improving the subsequent reduced pressure drying effect. The second stage of reduced pressure drying increases the pressure in the vacuum chamber by a higher reduced pressure rate. The increased negative pressure makes the evaporation rate of the coating layer solvent on the internal substrate faster, thereby improving the drying efficiency. However, an excessively fast evaporation rate will cause the solvent to evaporate and damage the overall quality of the coating layer. Therefore, the reduced pressure rate is reduced during the third stage of reduced pressure drying, and the reduced pressure rate is increased during the fourth stage of reduced pressure drying to completely dry the coating layer solvent. Finally, the air pressure in the vacuum chamber is restored to the actual atmospheric pressure to complete the reduced pressure work.

[0024] Other features and advantages of the present invention will be disclosed in detail in the following specific embodiments and drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] The present invention will be further described below in conjunction with the accompanying drawings:

[0026] Figure 1 It is a schematic diagram of the installation of a reduced pressure drying device of the present invention;

[0027] Figure 2It is a schematic diagram of the structure of the vacuum chamber of the present invention and a schematic diagram of the flow of gas molecules in the vacuum chamber;

[0028] Figure 3 It is a schematic diagram of the reduced pressure drying process curve of the present invention;

[0029] Figure 4 It is a process flow chart of reduced pressure drying of the present invention;

[0030] The following are the descriptions of the reference numerals:

[0031] Substrate 1, vacuum chamber 2, decompression device 3, air supply device 4, air pressure detector 5, PLC control system 6, exhaust port 21, air supply port 22, substrate tray 11, slide rail 12, uniform air device 7, upper uniform air device 71, lower uniform air device 72, vacuum pump 31, exhaust regulating valve 32, air supply source 41, air supply regulating valve 42, stainless steel hose 8, signal communication line 9, chamber door panel 23, door lock assembly 24, vacuum observation window 25. DETAILED DESCRIPTION

[0032] The technical solutions of the embodiments of the present invention are explained and described below in conjunction with the drawings of the embodiments of the present invention, but the following embodiments are only preferred embodiments of the present invention, not all. Based on the embodiments in the implementation mode, other embodiments obtained by those skilled in the art without creative work are all within the protection scope of the present invention.

[0033] In the following description, terms such as "inside", "outside", "up", "down", "left", "right", etc. that indicate directions or positional relationships are only used to facilitate the description of the embodiments and simplify the description, and do not indicate or imply that the referred device or element must have a specific direction, be constructed and operate in a specific direction. Therefore, it should not be understood as a limitation of the present invention.

[0034] like Figure 1 to Figure 2 As shown, a reduced pressure drying device is used to perform reduced pressure drying on a substrate 1 with a solvent coating layer. The substrate 1 is placed in a vacuum chamber 2. The reduced pressure drying device adjusts the air pressure through a reduced pressure device 3 and an air supply device 4 to uniformly dry the solvent coating layer on the substrate 1, thereby improving the nucleation crystallization quality of the coating layer and improving the performance of the substrate 1.

[0035] The vacuum chamber 2 is a closed space with a low air leakage rate. The vacuum pump 31 is used to evacuate air to reduce the pressure of the internal environment to the pressure value required by the process, which is beneficial to the reduced pressure drying process of the coating layer of the substrate 1.

[0036] The vacuum chamber 2 is provided with a substrate tray 11, a slide rail 12, a chamber door panel 23, a door lock assembly 24 and a vacuum observation window 25; the slide rail 12 is mounted on both sides of the inner wall of the vacuum chamber 2, and the substrate tray 11 is used to connect the substrate 1 and the slide rail 12. The substrate tray 11 is slidably connected on the slide rail 12, and the substrate tray 11 can be pulled out of the vacuum chamber 2, which is convenient for operators to operate the substrate 1 with a coating layer and improve the operating efficiency. Among them, the chamber door panel 23 and the door lock assembly 24 are mounted on the side of the vacuum chamber, and the chamber door panel 23 connects the inside of the vacuum chamber 2 with the atmosphere, which can facilitate the removal of the substrate 1 after drying, and can form a closed space in the vacuum chamber 2. The door lock assembly 24 fastens the chamber door panel 23 and the vacuum chamber 2, so that it reaches a preliminary sealing state to prevent air leakage. The vacuum observation window 25 is mounted above the vacuum chamber 2, which is convenient for operators to intuitively view the coating drying effect and drying rate of the substrate inside the vacuum chamber 2.

[0037] Furthermore, a uniform wind device 7 for uniform air pressure is also provided in the vacuum chamber 2. The uniform wind device 7 includes an upper uniform wind device 71 and a lower uniform wind device 72; the upper uniform wind device 71 is mounted above the substrate tray 11; the lower uniform wind device 72 is mounted above the bottom of the vacuum chamber 2. When the pressure reducing device 3 or the air supply device 4 is working, the upper uniform wind device 71 protects the surface quality of the coating layer on the substrate, avoids the reduction of the quality of the coating layer due to the air flow velocity or impact nearby, and can achieve the effect of uniform wind speed; the lower uniform wind device 72 is installed at the bottom of the vacuum chamber 2, covers the bottom of the vacuum chamber 2, and is provided with an exhaust port 21 and an air supply port 22, protects the surface quality of the coating layer on the substrate and maintains the uniform pressure and wind speed inside the vacuum chamber 2.

[0038] The exhaust port 21 and the pressure reducing device 3 are connected by a stainless steel hose 8, and the air supply port 22 and the air supply device 4 are connected by a stainless steel hose 8; the pressure reducing device 3 includes a vacuum pump 31 and an exhaust regulating valve 32, and the exhaust regulating valve 32 is mounted on the stainless steel hose 8 provided between the vacuum pump 31 and the exhaust port 21, so as to realize the function of exhausting and reducing pressure inside the vacuum chamber 2; the air supply device 4 includes an air supply source 41 and an air supply regulating valve 42, and the air supply regulating valve 42 is mounted on the stainless steel hose 8 provided between the air supply source 41 and the air supply port 22, so as to realize the function of restoring the air supply inside the vacuum chamber 2 to atmospheric pressure.

[0039] Among them, the vacuum chamber 2 is also connected to a device for detecting the air pressure inside the vacuum chamber 2. The detected air pressure value is output to the PLC control system 6 through the signal communication line 9. The PLC control system is an electronic device used for industrial automation control, which is intended to replace the traditional relay sequence control, perform logic, timing, counting and other sequence control functions, and establish a flexible remote control system. The PLC control system has the characteristics of strong versatility, easy use, wide adaptability, high reliability, strong anti-interference ability, and simple programming. The PLC control system 6 can integrate various functions on the control panel for easy operation. In this embodiment, it is used to control devices such as the pressure reducing device 3 and the air supply device 4, which is convenient for operators to adjust the pressure and dry. The signal communication line 9 communicates with various electrical accessories, allowing them to receive the output instructions of the PLC control system 6 and complete the required functions. In this embodiment, instructions such as equipment startup, flow adjustment and recording of process parameters can be output.

[0040] The exhaust regulating valve 32 or the air supply regulating valve 42 receives the signal of the PLC control system 6, adjusts its opening angle, completes the exhaust flow and speed control, and completes the uniform and reasonable decompression drying. The vacuum pump 31 is connected to the vacuum chamber 2 through the stainless steel hose 8 to achieve the purpose of decompression. After the air supply source 41 is decompressed to a certain pressure, it returns to atmospheric pressure, making it convenient to take out the dried coating layer inside.

[0041] like Figure 3 to Figure 4 As shown, in the reduced pressure drying method, the substrate 1 coated with the solvent slurry is directly placed on the fixed position of the substrate tray 11, with the side with the solvent facing upward, and the uniform air flow device 7 is installed to prepare for the subsequent uniform air flow movement. The substrate tray 11 is pushed into the vacuum chamber 2 and fixed, and the chamber door panel 23 is closed and locked with the door lock assembly 24 to make the interior of the vacuum chamber 2 sealed.

[0042] According to the vacuum drying process Figure 4 Execute the T0 process, start the vacuum pump 31, and perform the first stage of reduced pressure drying S1. The internal environment of the vacuum chamber 2 is evacuated to the pressure of point a at a reduced pressure speed V1 to extract part of the gas containing moisture in the space.

[0043] Then open the gas supply regulating valve 42, close the exhaust regulating valve 32, and execute the T1 process. The valve opening size can be controlled to provide dry gas to enter the vacuum chamber 2. After the gas is evenly circulated once through the lower uniform air device 72, the clean dry gas evenly flows through the dead corners inside the chamber. After the interior of the lower uniform air device 72 returns to the atmospheric pressure P1 point, according to Figure 2 As shown, on the surface of the reverse gas reflow chamber, most of the fast airflow will flow close to the inner wall. Since the coating layer is protected by the upper uniform air device 71 on all sides, the flowing gas passing through the surface of the coating layer is secondary uniformized, which is not easy to affect the coating layer.

[0044] Then execute the T2 process, and reduce the pressure to point P2 at the decompression speed V1. The internal pressure of the vacuum chamber 2 drops sharply, and the gas with air moisture in the vacuum chamber 2 is basically discharged outside the chamber. At this time, there will be slight condensation on the surface of the coating layer. Then open the air supply regulating valve 42 for the second time, close the exhaust regulating valve 32, and execute the T3 process to restore the atmospheric pressure point P1, so that the vacuum chamber 2 is filled with clean and dry gas to avoid the retention of water vapor in dead corners. Multiple decompression and air supply can quickly clean the air with water vapor in the internal dead corners, and the impact of dry air on the interior can also reduce the condensation of water on the surface, which can easily improve the decompression and drying effect.

[0045] The second stage of vacuum drying S2 is performed, and the T4 process is executed. The opening size of the exhaust regulating valve 32 is controlled, and the pressure of the vacuum chamber 2 is sharply reduced to point P3 at the decompression speed V2. The solvent inside the coating layer on the surface of the substrate 1 begins to actively migrate to the surface. When the saturated vapor pressure of the solvent is reached, it evaporates on the surface to form a vapor flow, such as Figure 2 As shown, the vapor above the surface of the substrate 1 flows toward the exhaust port 21. Since the upper uniform wind device 71 protects the coating layer around, the high-speed airflow nearby has little effect on the coating layer, which can suppress the uneven drying defects caused by the high-speed airflow on the coating layer. The vapor is affected by the upper uniform wind device 71 and flows evenly on the surface of the coating layer, reducing the occurrence of flow marks or wind spot defects and improving the quality of the coating layer. When the reduced pressure is lower than point P3, the negative pressure increases, causing the internal coating layer solvent to evaporate too quickly, and the internal solvent movement becomes more active. In order to avoid excessive drying rate causing solvent evaporation to damage the overall quality of the coating layer, when performing the third stage of reduced pressure drying S3, it is necessary to suppress the activity of the solvent and slow down the solvent evaporation rate.

[0046] Execute the T5 process, control the opening size of the exhaust regulating valve 32, slowly reduce pressure and evacuate at a pressure reduction rate of V3, and the solvent components in the coating layer are uniformly vaporized and evaporated. After a long period of pressure reduction to point P4, the evaporation of the coating layer is basically completed; however, there will still be solvents that are difficult to evaporate inside. According to the vacuum drying process curve description, execute the T6 process, start the fourth vacuum drying S4, and quickly reduce pressure and evacuate the vacuum chamber 2 at a pressure reduction rate of V4 until the pressure drops to point P5. At this time, the solvent inside the coating layer is not active in evaporation because there is not much solvent left after the third vacuum drying, and the effect on the drying quality of the coating layer is very small. At this time, the drying is basically completed.

[0047] Start to execute the T7 process, close the exhaust regulating valve 32, turn off the vacuum pump 31 and stop working, open the air supply regulating valve 42, and open the valve to the maximum to restore the atmospheric pressure inside the vacuum chamber 2 to facilitate the removal of the dried coating layer. During the execution of the T7 process, since the pressure inside the chamber is several orders of magnitude lower than the external atmospheric pressure, although the restoration of atmospheric pressure will produce a very fast and strong airflow, the coating layer has been fully dried and crystallized after reduced pressure drying, and the uniform wind speed and pressure of the upper uniform wind device 71 and the lower uniform wind device 72 well protect the quality of the coating layer and improve the service life and performance of the coating layer.

[0048] Finally, the chamber door 23 is opened, the substrate tray 11 is pulled out, and the substrate 1 is taken out, and the decompression drying work is completed.

[0049] Combined with the above reduced pressure drying method, according to Figure 2 As shown, in the first stage of vacuum drying S1, the internal environment of the vacuum chamber 2 is evacuated and decompressed to point P2 through two decompressions, wherein the decompression is performed twice at the same decompression rate V1, so as to remove the condensed water vapor in the vacuum chamber 2 and provide a better vacuum drying environment; in the second stage of vacuum drying S2, the pressure of the vacuum chamber 2 is sharply reduced to point P3 at the decompression rate V2, and the decompression rate V2 is greater than the decompression rate V1, so that the solvent inside the coating layer on the surface of the substrate 1 starts to actively migrate to the surface, evaporates quickly to form a vapor flow, and improves the drying efficiency; in the third stage of vacuum drying S3, the pressure of the vacuum chamber 2 is slowly reduced to point P4 at the decompression rate V3, and the decompression rate V3 is less than the decompression rate V1. 1. If the pressure is too low at this time, the solvent will evaporate and the overall quality of the coating layer will be damaged. Therefore, the decompression rate is reduced. In the fourth stage of decompression drying S4, the vacuum chamber 2 is decompressed and evacuated quickly at the decompression rate V4 until the pressure drops to point P5. The decompression rate V4 is greater than the decompression rate V2. After the above-mentioned decompression in several stages, the drying of the coating layer has been basically completed. At this moment, the use of a larger decompression rate has little effect on the drying quality of the coating layer. The residual solvent that is difficult to evaporate is dried at the decompression rate V4. The air pressure in the vacuum chamber is adjusted by the above-mentioned multiple stages of different decompression rates to reduce the defects such as uneven film thickness, flow marks, cracks, dents, wind spots, etc. that occur during the decompression drying process, thereby improving the product quality. Finally, the pressure is increased to atmospheric pressure, the vacuum chamber is opened, and the substrate is taken out.

[0050] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that the present invention includes but is not limited to the contents described in the drawings and the above specific embodiments. Any modification that does not deviate from the functional and structural principles of the present invention will be included in the scope of the claims.

Claims

1. A vacuum drying method of a vacuum drying device, characterized in that: The following steps are involved: S1. Assemble the reduced pressure drying device: place the substrate (1) with the solvent coating layer on a fixed position of the substrate tray (11), with the side with the solvent coating layer facing upward, install the uniform air flow device (7), push the substrate tray (11) into the vacuum chamber (2) and fix it, close the chamber door (23) so that the interior of the vacuum chamber (2) is in a sealed state, and the initial atmospheric pressure is point P1; S2, implement the first stage of reduced pressure drying: start the pressure reducing device (3), adjust the exhaust regulating valve (32), and exhaust the internal environment of the vacuum chamber (2) to the pressure point a at the pressure reducing speed V1, thereby extracting some of the gas containing moisture in the vacuum chamber (2); close the pressure reducing device (3), open the gas supply device (4), and adjust the gas supply regulating valve (42) to restore the inside of the vacuum chamber (2) to the atmospheric pressure point P1; close the gas supply device (4), open the pressure reducing device (3), adjust the exhaust regulating valve (32), and reduce the gas pressure of the vacuum chamber (2) to the atmospheric pressure point P2 at the pressure reducing speed V1 for the second time; close the pressure reducing device (3), open the gas supply device (4), and adjust the gas supply regulating valve (42) to restore the inside of the vacuum chamber (2) to the atmospheric pressure point P1; fill the vacuum chamber (2) with clean dry gas to avoid the retention of water vapor in dead corners; S3, implementing the second stage of reduced pressure drying: closing the gas supply device (4), opening the reduced pressure device (3), adjusting the exhaust regulating valve (32), and reducing the pressure of the vacuum chamber (2) to point P3 at a reduced pressure rate V2; the reduced pressure rate V2 is greater than the reduced pressure rate V1, so that the solvent inside the coating layer on the surface of the substrate (1) begins to actively migrate to the surface, evaporates quickly to form a vapor flow, and improves the drying efficiency; S4, implementing the third stage of reduced pressure drying: adjusting the exhaust regulating valve (32), reducing pressure and exhausting air at a reduced pressure rate V3, and reducing pressure to point P4; the reduced pressure rate V3 is less than the reduced pressure rate V1; S5, implementing the fourth stage of reduced pressure drying: adjusting the exhaust regulating valve (32) to reduce pressure and evacuate the vacuum chamber (2) at a reduced pressure rate V4 until the pressure drops to point P5; the reduced pressure rate V4 is greater than the reduced pressure rate V2; S6, close the pressure reducing device (3), open the air supply regulating valve (42), and take out the dried substrate (1); A reduced pressure drying device used in a reduced pressure drying method, for performing reduced pressure drying on a substrate (1) with a solvent coating layer, comprising a vacuum chamber (2), a reduced pressure device (3), an air supply device (4), an air pressure detector (5) and a PLC control system (6); the substrate (1) is placed in the vacuum chamber (2); an exhaust port (21) and an air supply port (22) are provided at the bottom of the vacuum chamber (2), which are respectively connected to the reduced pressure device (3) and the air supply device (4); the air pressure detector (5) is used to detect the air pressure in the vacuum chamber (2); the PLC control system (6) receives the air pressure value detected by the air pressure detector (5); the reduced pressure device (3) and the air supply device (4) are connected to the PLC control system (6); The vacuum chamber (2) is also provided with a uniform air pressure device (7); the uniform air device (7) comprises an upper uniform air device (71) and a lower uniform air device (72); the upper uniform air device (71) is mounted above the substrate tray (11); the lower uniform air device (72) is mounted above the bottom of the vacuum chamber (2); the lower uniform air device (72) is installed at the bottom of the vacuum chamber (2), and covers the bottom of the vacuum chamber (2) provided with an exhaust port (21) and an air supply port (22), so as to protect the surface quality of the coating layer on the substrate and maintain uniform pressure and wind speed inside the vacuum chamber (2); after the gas is uniformly circulated once through the lower uniform air device (72), the clean dry gas flows evenly through the dead corners inside the chamber.

2. The reduced pressure drying method of the reduced pressure drying device according to claim 1, characterized in that: A substrate tray (11) and a slide rail (12) are provided in the vacuum chamber (2); the slide rail (12) is mounted on both sides of the inner wall of the vacuum chamber (2); the substrate tray (11) is used to connect the substrate (1) and the slide rail (12); the substrate tray (11) is slidably connected on the slide rail (12).

3. The reduced pressure drying method of the reduced pressure drying device according to claim 1, characterized in that: The decompression device (3) comprises a vacuum pump (31) and an exhaust regulating valve (32), wherein the exhaust regulating valve (32) is mounted on a stainless steel hose (8) provided between the vacuum pump (31) and the exhaust port (21).

4. The reduced pressure drying method of the reduced pressure drying device according to claim 1, characterized in that: The gas supply device (4) comprises a gas supply source (41) and a gas supply regulating valve (42), wherein the gas supply regulating valve (42) is mounted on a stainless steel hose (8) provided between the gas supply source (41) and the gas supply port (22).

5. The reduced pressure drying method of the reduced pressure drying device according to claim 1, characterized in that: Signal communication lines (9) for transmitting instructions are provided between the PLC control system (6) and the air pressure detector (5), the pressure reducing device (3) and the air supply device (4).

6. The reduced pressure drying method of a reduced pressure drying device according to claim 1, characterized in that: A chamber door panel (23) and a door lock assembly (24) are provided on the side of the vacuum chamber (2); the door lock assembly (24) is used to fasten the chamber door panel (23) and the vacuum chamber (2).

7. The reduced pressure drying method of the reduced pressure drying device according to claim 1, characterized in that: A vacuum observation window (25) is provided above the vacuum chamber (2).

Citation Information

Patent Citations

  • Frequency conversion type natural gas long-distance pipeline vacuum dry unit suitable for high temperature environment

    CN102620529A

  • Vacuum drying device and vacuum drying method

    CN110039915A

  • Reduced-pressure drying device and reduced-pressure drying method

    CN115532558A

  • Negative pressure drying box

    CN117570657A

  • Drying equipment

    CN209833004U