A preparation device and method for low-pollution flat membrane

The low-pollution flat membrane is prepared by heating dissolution method and spin coating technology, which solves the pollution and stability problems in the preparation of titanium dioxide nanowire flat membranes in the existing technology, improves the mechanical properties and preparation efficiency, and forms a self-healing and self-cleaning function. material.

CN118491310BActive Publication Date: 2024-10-18福建省蓝深环保技术股份有限公司
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410959575.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-10-18
Estimated Expiration
2044-07-17

AI Technical Summary

Technical Problem

Existing titanium dioxide nanowire flat film preparation methods have problems such as high pollution, poor stability, low purity, and low processing efficiency, resulting in serious environmental pollution and poor mechanical properties.

Method used

The polyvinylidene fluoride casting film base liquid is prepared by a heating dissolution method, and the titanium dioxide nanowire casting film sol is evenly distributed on it. A low-pollution flat film is formed through spin coating and hot air drying technology to replace the ABS diversion layer to form a self-contained film. The support layer has self-healing and self-cleaning functions.

Benefits of technology

The degree of contamination is significantly reduced, the corrosion resistance, high strength, toughness and wear resistance of the flat membrane are improved, the mechanical properties are enhanced, and the preparation efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118491310B_ABST
    Figure CN118491310B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of nanowire flat membranes, specifically a method for preparing a low-pollution flat membrane, including step one: preparing a polyvinylidene fluoride casting base liquid; step two: preparing a titanium dioxide nanowire casting sol; step three: preparing a titanium dioxide nanowire casting film with a lining flat membrane; step four: preparing a low-pollution flat membrane; step five: rinsing and air-drying; step six: finished product. The present invention improves the hydrophilicity and antibacterial properties of the polyvinylidene fluoride flat membrane and the corrosion resistance, high strength, high toughness, and wear resistance of the flat membrane, thereby improving the stability of the flat membrane, greatly reducing the degree of pollution, and the substrate material improves the mechanical properties of the flat membrane and replaces the ABS guide layer to form a self-supporting layer with self-repairing and self-cleaning functions. The present device can sequentially perform stirring and dissolving, extrusion coating, hot air drying, and drying treatment processes, thereby greatly improving the efficiency of preparation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a preparation method and equipment thereof, in particular to a preparation equipment and method of a low-pollution flat membrane, belonging to the technical field of nanowire flat membranes. Background Art

[0002] The flat membrane has a wire diameter and length at the nanoscale. These nanowires are tightly arranged on the flat substrate to form a dense membrane structure. The material has excellent physical and chemical properties, such as high specific surface area, good chemical stability, excellent photocatalytic performance and mechanical strength. The flat membrane also has unique interface effects and quantum size effects, which make it show broad application potential in photocatalysis, environmental purification, energy conversion and other fields.

[0003] Flat membrane preparation mainly uses vinylidene fluoride PVDF, polysulfone PSF, polyacrylonitrile PAN, polyether sulfone PES, polyethylene PE, polypropylene PP and the like as raw materials, which are dissolved in a solvent to make a casting solution, and then spread into a thin layer on a glass plate or other substrate, and phase separation is carried out by evaporation of the solvent to form a film;

[0004] Existing titanium dioxide nanowires are prepared by dissolving titanium dioxide powder in a solution and reacting it through high-temperature hydrothermal reaction to generate nanowires. The nanowires need to be bonded to acrylonitrile-butadiene-styrene copolymer (ABS), and a hexagonal honeycomb or other similar structure with a hollow center is processed on the ABS board as a water channel. This results in a large flat membrane thickness, low packing density, and poor stability, thus causing a large amount of environmental pollution. The reaction conditions for preparing titanium dioxide nanowires by the hydrothermal method are strictly controlled, and the purity, stability, and processing efficiency are low.

[0005] Therefore, there is an urgent need to improve the preparation method of low-pollution flat membrane components to solve the above-mentioned problems. Summary of the invention

[0006] The purpose of the present invention is to provide a low-pollution flat membrane preparation device and method. The preparation method and preparation device of the present invention improve the hydrophilicity and antibacterial property of the polyvinylidene fluoride flat membrane, greatly reduce the pollution to the surrounding environment, and at the same time improve the corrosion resistance, high strength, high toughness and wear resistance of the flat membrane, reduce the solubility of the flat membrane, and greatly reduce the degree of pollution. The substrate material improves the mechanical properties of the flat membrane and replaces the ABS guide layer to form a self-supporting layer with self-repairing and self-cleaning functions.

[0007] In order to achieve the above object, the main technical solutions adopted by the present invention include:

[0008] A method for preparing a low-pollution flat membrane comprises the following steps:

[0009] Step 1: Prepare polyvinylidene fluoride film casting base liquid, put polyvinylidene fluoride PDVF powder into a raw material heating and dissolving box, add water and heat to dissolve, heat the raw material heating and dissolving box through a heating ring, the heating temperature is: 40±5°C, adjust the speed of the stirring and pressurizing mechanism to 50r / min, the reaction time is 5min, and then add a solvent to prepare the polyvinylidene fluoride film casting base liquid;

[0010] Step 2: preparing titanium dioxide nanowire casting sol, adding titanium dioxide powder to the casting base liquid, adjusting the speed of the stirring and pressurizing mechanism (2) to 75r / min, adding 10 mol / L sodium hydroxide solution, heating the temperature to 180±5°C, reacting for 24h, washing with 0.1 mol / L hydrochloric acid solution until neutral, washing with 50% ethanol solution for 2min, placing in an oven and heating the temperature to 60±5°C, reacting for 20min, and preparing titanium dioxide nanowire casting sol;

[0011] Step 3: preparing a titanium dioxide nanowire cast film with a backing flat plate membrane, wherein the raw material is heated and dissolved in the box (1) by a stirring and pressurizing mechanism (2) and the titanium dioxide cast film sol is evenly distributed on both sides of the substrate material by a spin coating method to prepare a titanium dioxide cast film with a backing flat plate membrane;

[0012] Step 4: preparing a low-pollution flat membrane, placing the titanium dioxide nanowire cast membrane with a liner flat membrane into a hot air drying mechanism (4), heating it to a temperature of 60±5° C. by a heating plate (403) for evaporation temperature treatment for 120 min;

[0013] Titanium dioxide nanowires will be grown on polyvinylidene fluoride to form high-purity, uniform-sized nanowire crystals;

[0014] Then it is pulled into the drying mechanism (5) and treated at a spiral heating plate (501) at a temperature of 120±5°C for 60 minutes to cause the polyvinylidene fluoride to undergo phase transformation and prepare a low-pollution flat membrane;

[0015] Step 5: Rinse and air-dry. Place the titanium dioxide nanowire plate in clean water and rinse for 120 minutes, then take it out and air-dry it naturally.

[0016] Step 6: Finished product: cutting the membrane, welding the edges to seal, connecting the water pipe, and forming a membrane assembly according to a certain filling density.

[0017] A low-pollution flat-plate mold preparation device, comprising symmetrically distributed raw material heating and dissolving boxes, wherein a heating ring is fixedly arranged on the outer side of the raw material heating and dissolving boxes, a backing material is arranged between two of the raw material heating and dissolving boxes, a stirring and pressurizing mechanism corresponding to the raw material heating and dissolving boxes is arranged above the raw material heating and dissolving boxes, and a coating mechanism is connected to the bottom of the raw material heating and dissolving boxes, wherein the coating mechanism comprises a first connecting pipe and a coating box, wherein one end of the first connecting pipe is connected to the interior of the raw material heating and dissolving boxes, and the other end of the first connecting pipe is connected to the interior of the coating box through a second connecting pipe, and a coating roller is rotatably arranged inside the coating box, and the coating roller abuts against the backing material;

[0018] A hot air drying mechanism is fixedly arranged on one side of the coating mechanism, and a drying mechanism is fixedly arranged on one side of the hot air drying mechanism. The drying mechanism includes a spiral heating plate and a winding roller fixedly arranged at the bottom of the spiral heating plate, and a winding roller motor is arranged at the output end of the winding roller, and the winding roller motor is used to wind up the substrate material.

[0019] Preferably, one side of the raw material heating and dissolving box is fixedly connected to the stirring and pressurizing mechanism through a stirring mechanism support frame, the stirring and pressurizing mechanism is arranged just above the raw material heating and dissolving box, the stirring and pressurizing mechanism comprises a stirring motor and an electric telescopic rod, the stirring motor is fixedly arranged at the output end of the electric telescopic rod, the output end of the stirring motor is provided with a stirring rod, and the stirring rod is fixedly provided with a plurality of evenly distributed stirring teeth;

[0020] The bottom of the stirring rod is connected with a piston joint, and the piston joint is connected with a piston through threads.

[0021] Preferably, a buffer bin connected to the first connecting pipe is fixedly provided on the first connecting pipe, the buffer bin is connected to the interior of the coating box through the second connecting pipe, and a brush is fixedly provided on the outer side surface of the coating roller.

[0022] Preferably, the hot air drying mechanism comprises a fan box and a hot air drying box arranged above the fan box, the hot air drying box is fixedly provided with symmetrically distributed heating plates inside, and the substrate material is arranged between the heating plates;

[0023] A fan is fixedly arranged inside the fan box, and a substrate material through hole corresponding to the substrate material is opened on the outer side of the hot air drying box. The substrate material passes through the substrate material through hole and extends to the outside of the substrate material through hole.

[0024] Preferably, a heating plate top cover is fixedly arranged on the upper part of the spiral heating plate, a heating plate bottom cover is fixedly arranged on the bottom of the spiral heating plate, the winding roller motor is rotatably arranged inside the spiral heating plate, and one end of the substrate material is fixedly arranged on the winding roller motor;

[0025] The top cover of the heating plate is connected with a third connecting pipe, and the third connecting pipe is connected with the interior of the hot air drying mechanism;

[0026] The bottom of the heating plate bottom cover is fixedly provided with a heating plate bottom cover supporting foot, the bottom of the heating plate bottom cover supporting foot is fixedly connected with a fixed bottom plate, and the raw material heating and dissolving box is fixedly provided on the fixed bottom plate through a second supporting foot.

[0027] Preferably, a V-shaped support frame is fixedly provided on one side of the raw material heating and dissolving box, a limit frame is fixedly provided on the other side of the raw material heating and dissolving box, the limit frame corresponds to the V-shaped support frame, the hot air drying mechanism is fixedly provided on the V-shaped support frame, and the bottom of the V-shaped support frame is fixedly connected to the fixed bottom plate through a first supporting foot;

[0028] The V-shaped support frame comprises an upper support arm and a lower support arm, and symmetrically distributed first guide rollers are arranged on the upper support arm and the lower support arm, and the substrate material is arranged between the first guide rollers.

[0029] Preferably, the limiting frame is internally rotatably provided with symmetrically distributed second guide rollers, and the substrate material passes through between the second guide rollers and between the first guide rollers in sequence.

[0030] Preferably, one end of the stirring mechanism support frame is fixedly connected to a support frame fixing block, the support frame fixing block is fixedly connected to the upper end of the stirring and pressurizing mechanism, and a plurality of evenly distributed fixed connecting arms are fixedly arranged on the stirring mechanism support frame;

[0031] A heating coil fixing block is fixedly connected to the bottom of the outer side surface of the heating coil, and the bottom of the stirring mechanism support frame is fixedly connected to the heating coil fixing block.

[0032] Preferably, the solvent is one of N-methyl-2-pyrrolidone (NMP), dimethylacetamide (DMAc) or N,N-dimethylformamide (DMF), and the substrate material is one of non-woven fabric, polyester (PET) or polypropylene.

[0033] The present invention has at least the following beneficial effects:

[0034] 1. The preparation method and preparation equipment of the present invention improve the hydrophilicity and antibacterial property of the polyvinylidene fluoride flat membrane, greatly reduce the pollution to the surrounding environment, and at the same time improve the corrosion resistance, high strength, high toughness and wear resistance of the flat membrane, reduce the solubility of the flat membrane, and greatly reduce the degree of pollution. The substrate material improves the mechanical properties of the flat membrane and replaces the ABS guide layer to form a self-supporting layer with self-repairing and self-cleaning functions. The equipment can sequentially carry out stirring and dissolving, extrusion coating, hot air drying and drying treatment processes, greatly improving the preparation efficiency.

[0035] 2. After the raw materials are put into the raw material heating and dissolving box, the raw material heating and dissolving box can be directly heated by the heating ring to speed up the efficiency of raw material dissolution. A substrate material is arranged between the two raw material heating and dissolving boxes. The substrate material can be preheated in advance between the two raw material heating and dissolving boxes to speed up the coating efficiency. In the process of dissolving the raw materials, stirring is performed by the stirring and pressurizing mechanism.

[0036] 3. When it is necessary to heat and dissolve the raw materials inside the raw material heating and dissolving box, the stirring rod is extended into the raw material heating and dissolving box through the electric telescopic rod on the stirring and pressurizing mechanism, and the stirring rod on the stirring and pressurizing mechanism is started to rotate. Therefore, while the stirring rod rotates, the stirring teeth on the stirring rod stir the raw materials inside the raw material heating and dissolving box. At the same time, the temperature inside the raw material heating and dissolving box is controlled by the heating ring to improve the quality and efficiency of dissolution.

[0037] 4. During the extrusion process, the titanium dioxide casting film sol enters the interior of the buffer bin through the first connecting pipe, and then enters the interior of the coating box through the second connecting pipe. After the coating roller inside the coating box is started, the titanium dioxide casting film sol inside the coating box can be coated on the substrate material through a brush. Both raw material heating and dissolving boxes are connected with coating rollers, which can coat both sides of the substrate material at the same time, greatly improving the coating efficiency.

[0038] 5. After the substrate material enters the interior of the spiral heating plate, the substrate material is heated by the spiral heating plate. A heating plate top cover is fixedly provided on the spiral heating plate, and a heating plate bottom cover is fixedly provided below, which helps to reduce heat loss and improve drying efficiency. The spiral heating plate is connected to the interior of the hot air drying box through a third connecting pipe, so that the hot air flow in the hot air drying box can be guided to the interior of the spiral heating plate, thereby increasing the airflow to speed up the drying efficiency and helping to save electricity resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0040] Figure 1 is a preparation flow chart of the present invention;

[0041] Figure 2 The three-dimensional Figure 1 ;

[0042] Figure 3 The local structure of the present invention Figure 1 ;

[0043] Figure 4 It is a structural diagram of the coating mechanism of the present invention;

[0044] Figure 5 This is a structural diagram of the stirring and pressurizing mechanism of the present invention;

[0045] Figure 6 It is the structural diagram of the drying mechanism of the present invention;

[0046] Figure 7 is a cross-sectional view of the drying mechanism of the present invention;

[0047] Figure 8 The three-dimensional Figure 2 ;

[0048] Fig. 9 The local structure of the present invention Figure 2 ;

[0049] Fig.10 It is a partial cross-sectional view of the present invention;

[0050] Fig.11 It is a partial top view of the present invention.

[0051] In the figure, 1, raw material heating and dissolving box; 2, stirring and pressurizing mechanism; 201, stirring rod; 202, stirring motor; 203, electric telescopic rod; 204, piston joint; 205, piston; 206, stirring teeth; 3, coating mechanism; 301, coating box; 302, first connecting pipe; 303, buffer bin; 304, second connecting pipe; 305, coating roller; 4, hot air drying mechanism; 401, fan box; 402, fan; 403, heating plate; 404, hot air drying box; 405, substrate material through hole; 5, drying mechanism; 501, spiral pressurizing Hot plate; 502, heating plate top cover; 503, heating plate bottom cover; 504, heating plate bottom cover support foot; 505, third connecting pipe; 506, winding roller motor; 507, winding roller; 6, V-shaped support frame; 601, upper support arm; 602, lower support arm; 603, first guide roller; 7, limit frame; 701, second guide roller; 8, heating coil; 801, heating coil fixing block; 9, stirring mechanism support frame; 901, support frame fixing block; 902, fixed connecting arm; 10, first supporting foot; 11, second supporting foot; 12, fixed bottom plate. DETAILED DESCRIPTION

[0052] The following will describe the implementation methods of the present application in detail with the help of accompanying drawings and examples, so that the implementation process of how the present application uses technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.

[0053] like Figure 1-Figure 11 As shown, the method for preparing a low-pollution flat membrane provided in this embodiment comprises the following steps:

[0054] Step 1: prepare polyvinylidene fluoride film casting base liquid, put polyvinylidene fluoride PDVF powder into the raw material heating and dissolving box 1, add water and heat to dissolve, heat the raw material heating and dissolving box 1 through the heating ring 8, the heating temperature is: 40±5°C, adjust the speed of the stirring and pressurizing mechanism 2 to 50r / min, the reaction time is 5min, and then add the solvent to prepare the polyvinylidene fluoride film casting base liquid;

[0055] The solvent is one of N-methyl-2-pyrrolidone NMP solvent, dimethylacetamide DMAc solvent or N,N-dimethylformamide DMF solvent;

[0056] N-Methyl-2-pyrrolidone NMP solvent is a colorless to pale yellow liquid with low volatility, high boiling point and high polarity. It is an excellent solvent that can dissolve most organic and inorganic compounds.

[0057] Dimethylacetamide DMAc solvent is a colorless, transparent liquid with moderate volatility and good solubility. It is also a polar solvent that can dissolve many organic and inorganic compounds.

[0058] N,N-dimethylformamide DMF solvent is a colorless and transparent liquid with low volatility, high boiling point and good chemical stability. It is a polar solvent that can dissolve many organic and inorganic compounds.

[0059] Step 2: preparing titanium dioxide nanowire casting sol, adding titanium dioxide powder to the casting base liquid, adjusting the speed of the stirring and pressurizing mechanism (2) to 75r / min, adding 10 mol / L sodium hydroxide solution, heating the temperature to 180±5°C, reacting for 24h, washing with 0.1 mol / L hydrochloric acid solution until neutral, washing with 50% ethanol solution for 2min, placing in an oven and heating the temperature to 60±5°C, reacting for 20min, and preparing titanium dioxide nanowire casting sol;

[0060] Step 3: preparing a titanium dioxide nanowire cast film with a backing flat film, extruding the raw material heating and dissolving box 1 through the stirring and pressurizing mechanism 2, and evenly distributing the titanium dioxide cast film sol on both sides of the substrate material by spin coating, to prepare a titanium dioxide cast film with a backing flat film;

[0061] The substrate material is one of non-woven fabric, polyester PET or polypropylene PP;

[0062] Non-woven fabric is a kind of fabric that does not require spinning and weaving. It uses physical methods to directly bond fibers together to form a fiber mesh structure. It has superior performance and improved tensile strength.

[0063] Polyester mainly refers to polyethylene terephthalate (PET), which is a high molecular compound formed by the polycondensation of dibasic or polybasic acid and dibasic or polyol. It has good air tightness and fragrance retention, moderate moisture resistance, and excellent heat resistance, cold resistance and chemical resistance.

[0064] Polypropylene is a polymer formed by the addition polymerization of propylene. It is a thermoplastic synthetic resin with excellent performance, chemical resistance, heat resistance, electrical insulation, high-strength mechanical properties and good high-wear resistance processing performance;

[0065] Step 4: prepare a low-pollution flat membrane, put the titanium dioxide nanowire cast membrane with liner flat membrane into the hot air drying mechanism 4, and heat it to 60±5° C. by the heating plate 403 for evaporation temperature treatment for 120 min;

[0066] Titanium dioxide nanowires will be grown on polyvinylidene fluoride to form high-purity, uniform-sized nanowire crystals;

[0067] Then it is pulled into the drying mechanism 5, and the temperature of the spiral heating plate 501 is: 120±5℃ drying temperature treatment for 60min, the polyvinylidene fluoride undergoes phase transformation, and a low-pollution flat membrane is prepared;

[0068] Step 5: Rinse and air-dry. Place the titanium dioxide nanowire plate in clean water and rinse for 120 minutes, then take it out and air-dry it naturally.

[0069] Step 6: Finished product: cutting the membrane, welding the edges to seal, connecting the water pipe, and forming a membrane module according to a certain packing density;

[0070] The polyvinylidene fluoride PDVF powder is heated and dissolved to prepare a polyvinylidene fluoride casting base liquid, and then titanium dioxide powder is added to prepare a titanium dioxide casting sol, and a titanium dioxide casting film with a liner flat membrane is prepared by spin coating, and finally the low-pollution flat membrane is dried twice, so that the mechanical strength of the low-pollution flat membrane can be greatly enhanced, and a hexagonal honeycomb or other similar structures with a hollow middle are processed on an acrylonitrile-butadiene-styrene copolymer ABS plate as a water channel, which does not increase the thickness of the flat membrane, has a high packing density and a high space utilization rate, and the aeration volume required for cleaning will also be reduced accordingly. Compared with the traditional hydrothermal method for preparing titanium dioxide nanowires, the reaction conditions are more relaxed, the purity is higher, and the size uniformity is also higher;

[0071] The preparation method and the preparation equipment of the present invention improve the hydrophilicity and antibacterial property of the polyvinylidene fluoride flat membrane, greatly reduce the pollution to the surrounding environment, and at the same time improve the corrosion resistance, high strength, high toughness and wear resistance of the flat membrane, reduce the solubility of the flat membrane, and greatly reduce the pollution degree. The substrate material improves the mechanical properties of the flat membrane and replaces the ABS guide layer to form a self-supporting layer with the functions of self-repair and self-cleaning.

[0072] like Figure 1-Figure 11 As shown, the low-pollution flat mold preparation equipment provided in this embodiment includes symmetrically distributed raw material heating and dissolving boxes 1, and the outer side of the raw material heating and dissolving box 1 is fixedly provided with a heating ring 8. After the raw material is put into the raw material heating and dissolving box 1, the raw material heating and dissolving box 1 can be directly heated by the heating ring 8 to accelerate the efficiency of raw material dissolution. A substrate material is arranged between the two raw material heating and dissolving boxes 1. The substrate material can be preheated in advance between the two raw material heating and dissolving boxes 1 to accelerate the coating efficiency. A stirring and pressurizing mechanism 2 corresponding to the raw material heating and dissolving box 1 is arranged above the raw material heating and dissolving box 1. In the process of dissolving the raw material, stirring is performed by the stirring and pressurizing mechanism 2, specifically:

[0073] Stirring and dissolving, one side of the raw material heating and dissolving box 1 is fixedly connected to the stirring and pressurizing mechanism 2 through the stirring mechanism support frame 9, the stirring and pressurizing mechanism 2 is arranged just above the raw material heating and dissolving box 1, the stirring and pressurizing mechanism 2 fixed just above the raw material heating and dissolving box 1 is arranged on the stirring mechanism support frame 9, the stirring and pressurizing mechanism 2 includes a stirring motor 202 and an electric telescopic rod 203, the stirring motor 202 is fixedly arranged at the output end of the electric telescopic rod 203, the output end of the stirring motor 202 is provided with a stirring rod 201, and the stirring rod 201 is fixedly provided with a plurality of evenly distributed The stirring teeth 206, when it is necessary to heat and dissolve the raw materials in the raw material heating and dissolving box 1, extend the stirring rod 201 into the raw material heating and dissolving box 1 through the electric telescopic rod 203 on the stirring and pressurizing mechanism 2, and start the stirring motor 202 on the stirring and pressurizing mechanism 2 to drive the stirring rod 201 to rotate. Therefore, when the stirring rod 201 rotates, the stirring teeth 206 on the stirring rod 201 stir the raw materials in the raw material heating and dissolving box 1. At the same time, the temperature inside the raw material heating and dissolving box 1 is controlled by the heating ring 8, thereby improving the quality and efficiency of dissolution;

[0074] The bottom of the stirring rod 201 is connected with a piston joint 204, and a piston 205 is connected to the piston joint 204 through a thread. After the piston 205 is threadedly connected to the piston joint 204 on the stirring rod 201, the piston 205 is squeezed into the inside of the raw material heating and dissolving box 1 through the electric telescopic rod 203, and the titanium dioxide casting film sol inside the raw material heating and dissolving box 1 is squeezed;

[0075] Extrusion coating, when the stirring rod 201 squeezes the piston 205 into the interior of the raw material heating and dissolving box 1, the titanium dioxide casting film sol enters the interior of the coating mechanism 3 under the action of the piston 205, and the bottom of the raw material heating and dissolving box 1 is connected with the coating mechanism 3, and the coating mechanism 3 includes a first connecting pipe 302 and a coating box 301, one end of the first connecting pipe 302 is connected to the interior of the raw material heating and dissolving box 1, and the other end of the first connecting pipe 302 is connected to the interior of the coating box 301 through the second connecting pipe 304, and a coating roller 305 is rotatably arranged inside the coating box 301, and the coating roller 305 is against the substrate material, and a coating roller 305 is fixedly arranged on the first connecting pipe 302. The buffer bin 303 is connected to the coating box 301 through the second connecting pipe 304, and the outer side of the coating roller 305 is fixedly provided with a brush. During the extrusion process, the titanium dioxide casting film sol enters the buffer bin 303 through the first connecting pipe 302, and then enters the coating box 301 through the second connecting pipe 304. After the coating roller 305 inside the coating box 301 is started, the titanium dioxide casting film sol inside the coating box 301 can be coated on the substrate material through the brush. The two raw material heating and dissolving boxes 1 are both connected with the coating roller 305, which can coat both sides of the substrate material at the same time, greatly improving the coating efficiency;

[0076] Hot air drying, after coating, the substrate material will enter the interior of the hot air drying mechanism 4, one side of the coating mechanism 3 is fixedly provided with a hot air drying mechanism 4, the hot air drying mechanism 4 includes a fan box 401 and a hot air drying box 404 arranged above the fan box 401, the interior of the hot air drying box 404 is fixedly provided with symmetrically distributed heating plates 403, the substrate material is arranged between the heating plates 403, the outer side of the hot air drying box 404 is provided with a substrate material through hole 405 corresponding to the substrate material, the substrate material passes through the substrate material through hole 405 and extends to the outside of the substrate material through hole 405, the substrate material is coated in the coating mechanism 3 After coating, the substrate material passes through the substrate material through hole 405 on the hot air drying box 404 and enters the interior of the hot air drying box 404, passes between the two heating plates 403, and is dried under the action of the heating plates 403. The substrate material is dried by the two heating plates 403 at the same time, which greatly improves the drying efficiency. At the same time, a fan 402 is fixedly arranged inside the fan box 401, and a fan box 401 is fixedly arranged at the bottom of the hot air drying box 404. The fan 402 inside the fan box 401 is used to blow air into the interior of the hot air drying box 404 to increase the airflow inside the hot air drying box 404, so as to achieve the purpose of hot air drying;

[0077] Drying treatment: A drying mechanism 5 is fixedly arranged on one side of the hot air drying mechanism 4. The drying mechanism 5 includes a spiral heating plate 501 and a winding roller 507 fixedly arranged at the bottom of the spiral heating plate 501. A winding roller motor 506 is arranged at the output end of the winding roller 507. The winding roller motor 506 is used to wind up the substrate material. One end of the substrate material is fixed on the winding roller 507 of the winding roller motor 506. The winding roller 507 pulls the substrate material into the interior of the spiral heating plate 501, which is convenient for winding up the substrate material and improves the winding efficiency.

[0078] A heating plate top cover 502 is fixedly provided on the upper part of the spiral heating plate 501, a heating plate bottom cover 503 is fixedly provided on the bottom of the spiral heating plate 501, a winding roller motor 506 is rotatably provided inside the spiral heating plate 501, and one end of the substrate material is fixedly provided on the winding roller motor 506. After the substrate material enters the interior of the spiral heating plate 501, the substrate material is heated by the spiral heating plate 501. A heating plate top cover 502 is fixedly provided on the spiral heating plate 501, and a heating plate bottom cover 503 is fixedly provided at the bottom, which helps to reduce heat loss and improve drying efficiency. At the same time, a third connecting pipe 505 is connected to the heating plate top cover 502, and the third connecting pipe 505 is connected to the interior of the hot air drying mechanism 4. The spiral heating plate 501 is connected to the interior of the hot air drying box 404 through the third connecting pipe 505, so that the hot air flow in the hot air drying box 404 can be guided to the interior of the spiral heating plate 501, thereby accelerating the drying efficiency by increasing the airflow and helping to save electricity resources.

[0079] Further, such as Figure 2 , Figure 6 as well as Figure 7 As shown, a heating plate bottom cover supporting foot 504 is fixedly provided at the bottom of the heating plate bottom cover 503, and a fixed bottom plate 12 is fixedly connected to the bottom of the heating plate bottom cover supporting foot 504. The heating plate bottom cover 503 is fixedly provided on the fixed bottom plate 12 through the heating plate bottom cover supporting foot 504, thereby improving the overall stability of the drying mechanism 5. The raw material heating and dissolving box 1 is fixedly provided on the fixed bottom plate 12 through the second supporting foot 11, and the raw material heating and dissolving box 1 is fixedly provided on the fixed bottom plate 12 through the second supporting foot 11, thereby improving the overall stability of the raw material heating and dissolving box 1.

[0080] One end of the stirring mechanism support frame 9 is fixedly connected to a support frame fixing block 901, and the support frame fixing block 901 is fixedly connected to the upper end of the stirring and pressurizing mechanism 2. A number of evenly distributed fixed connecting arms 902 are fixedly arranged on the stirring mechanism support frame 9. One end of the stirring mechanism support frame 9 is fixedly connected to the stirring and pressurizing mechanism 2, and a heating ring fixing block 801 is fixedly connected to the bottom of the outer side of the heating ring 8. The bottom of the stirring mechanism support frame 9 is fixedly connected to the heating ring fixing block 801, and the other end is fixedly connected to the heating ring 8 through the heating ring fixing block 801, thereby improving the stability of the stirring and pressurizing mechanism 2. At the same time, the stirring mechanism support frames 9 are connected through the fixed connecting arms 902 to improve the overall structural strength of the stirring mechanism support frame 9.

[0081] Furthermore, Figure 3 , Figure 6 as well as Figure 7 As shown, a V-shaped support frame 6 is fixedly arranged on one side of the raw material heating and dissolving box 1, and a limit frame 7 is fixedly arranged on the other side of the raw material heating and dissolving box 1. The inner part of the limit frame 7 is rotatably provided with symmetrically distributed second guide rollers 701. The substrate material sequentially passes through the second guide rollers 701 and the first guide rollers 603. The V-shaped support frame 6 includes an upper support arm 601 and a lower support arm 602. The upper support arm 601 and the lower support arm 602 are provided with symmetrically distributed first guide rollers 603. The substrate material is arranged between the first guide rollers 603, and the substrate material is arranged between the second guide rollers 701 and the first guide rollers 603. On the roller 603, the second guide roller 701 and the first guide roller 603 play a certain guiding and supporting role for the substrate material. The limit frame 7 corresponds to the V-shaped support frame 6 and is on the same vertical plane, which is convenient for guiding and supporting the substrate material to prevent wrinkles. It is also convenient for the heating plate 403 to dry it. The hot air drying mechanism 4 is fixedly arranged on the V-shaped support frame 6. The bottom of the V-shaped support frame 6 is fixedly connected to the fixed bottom plate 12 through the first supporting foot 10. The bottom of the V-shaped support frame 6 is fixedly connected to the fixed bottom plate 12 through the first supporting foot 10, so as to improve the structural strength of the V-shaped support frame 6.

[0082] For example, certain words are used in the specification and claims to refer to specific components. Those skilled in the art should understand that hardware manufacturers may use different terms to refer to the same component. This specification and claims do not use differences in names as a way to distinguish components, but use differences in the functions of components as the criteria for distinction. For example, "including" mentioned throughout the specification and claims is an open term, so it should be interpreted as "including but not limited to". "Approximately" means that within an acceptable error range, those skilled in the art can solve technical problems within a certain error range and basically achieve technical effects.

[0083] It should be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a product or system including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such product or system. In the absence of more restrictions, the elements defined by the sentence "comprises a ..." do not exclude the existence of other identical elements in the product or system including the elements.

[0084] The above description shows and describes several preferred embodiments of the present invention, but as mentioned above, it should be understood that the present invention is not limited to the form disclosed herein, and should not be regarded as excluding other embodiments, but can be used in various other combinations, modifications and environments, and can be modified within the scope of the invention concept described herein through the above teachings or the technology or knowledge of the relevant field. Changes and variations made by those skilled in the art do not depart from the spirit and scope of the present invention, and should be within the scope of protection of the claims attached to the present invention.

Claims

1. A method for preparing a low-pollution flat membrane, characterized in that: The following steps are involved: Step 1: preparing a polyvinylidene fluoride film casting base liquid, putting polyvinylidene fluoride PDVF powder into a raw material heating and dissolving box (1) and adding water to heat and dissolve it, heating the raw material heating and dissolving box (1) through a heating ring (8), the heating temperature is: 40±5°C, the speed of the stirring and pressurizing mechanism (2) is adjusted to 50r / min, the reaction time is 5min, and then a solvent is added to prepare a polyvinylidene fluoride film casting base liquid, the solvent is one of N-methyl-2-pyrrolidone NMP solvent, dimethylacetamide DMAc solvent or N,N-dimethylformamide DMF solvent; Step 2: preparing titanium dioxide nanowire casting sol, adding titanium dioxide powder to the casting base liquid, adjusting the speed of the stirring and pressurizing mechanism (2) to 75r / min, adding 10 mol / L sodium hydroxide solution, heating the temperature to 180±5°C, reacting for 24h, washing with 0.1 mol / L hydrochloric acid solution until neutral, washing with 50% ethanol solution for 2min, placing in an oven and heating the temperature to 60±5°C, reacting for 20min, and preparing titanium dioxide nanowire casting sol; Step 3: preparing a titanium dioxide nanowire cast film with a backing flat film, wherein the raw material is heated and dissolved in a box (1) by a stirring and pressurizing mechanism (2) and the titanium dioxide cast film sol is evenly distributed on both sides of the substrate material by a rotary coating method to prepare a titanium dioxide cast film with a backing flat film, wherein the substrate material is one of non-woven fabric, polyester PET or polypropylene (PP); Step 4: preparing a low-pollution flat membrane, placing the titanium dioxide nanowire cast membrane with a liner flat membrane into a hot air drying mechanism (4), heating it to a temperature of 60±5° C. by a heating plate (403) for evaporation temperature treatment for 120 min; Titanium dioxide nanowires will be grown on polyvinylidene fluoride to form high-purity, uniform-sized nanowire crystals; Then it is pulled into the drying mechanism (5) and treated at a spiral heating plate (501) at a temperature of 120±5°C for 60 minutes to cause the polyvinylidene fluoride to undergo phase transformation and prepare a low-pollution flat membrane; Step 5: Rinse and air-dry. Place the titanium dioxide nanowire plate in clean water and rinse for 120 minutes, then take it out and air-dry it naturally. Step 6: Finished product: cutting the membrane, welding the edges to seal, connecting the water pipe, and forming a membrane assembly according to a certain filling density.

2. A low-pollution flat plate mold preparation device, using the low-pollution flat plate mold preparation method according to claim 1, characterized in that: The invention comprises symmetrically distributed raw material heating and dissolving boxes (1), wherein a heating ring (8) is fixedly arranged on the outer side of the raw material heating and dissolving boxes (1), a substrate material is arranged between two of the raw material heating and dissolving boxes (1), and a stirring and pressurizing mechanism (2) corresponding to the raw material heating and dissolving boxes (1) is arranged above the raw material heating and dissolving boxes (1). The bottom of the raw material heating and dissolving boxes (1) is connected with a coating mechanism (3), and the coating mechanism (3) comprises a first connecting pipe (302) and a coating box (301), one end of the first connecting pipe (302) is connected to the inside of the raw material heating and dissolving boxes (1), and the other end of the first connecting pipe (302) is connected to the inside of the coating box (301) through a second connecting pipe (304), and a coating roller (305) is rotatably arranged inside the coating box (301), and the coating roller (305) abuts against the substrate material; A hot air drying mechanism (4) is fixedly arranged on one side of the coating mechanism (3); a drying mechanism (5) is fixedly arranged on one side of the hot air drying mechanism (4); the drying mechanism (5) comprises a spiral heating plate (501) and a winding roller (507) fixedly arranged at the bottom of the spiral heating plate (501); a winding roller motor (506) is arranged at the output end of the winding roller (507); the winding roller motor (506) is used to wind up the substrate material; A heating plate top cover (502) is fixedly arranged on the upper part of the spiral heating plate (501), a heating plate bottom cover (503) is fixedly arranged on the bottom of the spiral heating plate (501), the winding roller motor (506) is rotatably arranged inside the spiral heating plate (501), and one end of the substrate material is fixedly arranged on the winding roller motor (506); The heating plate top cover (502) is connected to a third connecting pipe (505), and the third connecting pipe (505) is connected to the interior of the hot air drying mechanism (4); A heating plate bottom cover supporting foot (504) is fixedly arranged at the bottom of the heating plate bottom cover (503); a fixed bottom plate (12) is fixedly connected to the bottom of the heating plate bottom cover supporting foot (504); and the raw material heating and dissolving box (1) is fixedly arranged on the fixed bottom plate (12) via a second supporting foot (11); A V-shaped support frame (6) is fixedly arranged on one side of the raw material heating and dissolving box (1), and a limit frame (7) is fixedly arranged on the other side of the raw material heating and dissolving box (1), wherein the limit frame (7) corresponds to the V-shaped support frame (6), and the hot air drying mechanism (4) is fixedly arranged on the V-shaped support frame (6), and the bottom of the V-shaped support frame (6) is fixedly connected to the fixed bottom plate (12) via a first supporting foot (10); The V-shaped support frame (6) comprises an upper support arm (601) and a lower support arm (602), the upper support arm (601) and the lower support arm (602) being provided with symmetrically distributed first guide rollers (603), and the substrate material being provided between the first guide rollers (603); The limiting frame (7) is internally rotatably provided with symmetrically distributed second guide rollers (701), and the substrate material sequentially passes through between the second guide rollers (701) and between the first guide rollers (603).

3. The low-pollution flat plate mold preparation device according to claim 2, characterized in that: One side of the raw material heating and dissolving box (1) is fixedly connected to the stirring and pressurizing mechanism (2) via a stirring mechanism support frame (9); the stirring and pressurizing mechanism (2) is arranged directly above the raw material heating and dissolving box (1); the stirring and pressurizing mechanism (2) comprises a stirring motor (202) and an electric telescopic rod (203); the stirring motor (202) is fixedly arranged at the output end of the electric telescopic rod (203); a stirring rod (201) is arranged at the output end of the stirring motor (202); and a plurality of evenly distributed stirring teeth (206) are fixedly arranged on the stirring rod (201); The bottom of the stirring rod (201) is connected to a piston joint (204), and a piston (205) is threadedly connected to the piston joint (204).

4. The low-pollution flat plate mold preparation device according to claim 2, characterized in that: A buffer bin (303) connected to the first connecting tube (302) is fixedly arranged on the first connecting tube (302); the buffer bin (303) is connected to the interior of the coating box (301) via the second connecting tube (304); and a brush is fixedly arranged on the outer side surface of the coating roller (305).

5. The low-pollution flat plate mold preparation device according to claim 2, characterized in that: The hot air drying mechanism (4) comprises a fan box (401) and a hot air drying box (404) arranged above the fan box (401); symmetrically distributed heating plates (403) are fixedly arranged inside the hot air drying box (404); and the substrate material is arranged between the heating plates (403); A fan (402) is fixedly arranged inside the fan box (401), and a substrate material through hole (405) corresponding to the substrate material is opened on the outer side surface of the hot air drying box (404), and the substrate material passes through the substrate material through hole (405) and extends to the outside of the substrate material through hole (405).

6. The low-pollution flat plate mold preparation device according to claim 3, characterized in that: One end of the stirring mechanism support frame (9) is fixedly connected to a support frame fixing block (901), the support frame fixing block (901) is fixedly connected to the upper end of the stirring and pressurizing mechanism (2), and a plurality of evenly distributed fixed connection arms (902) are fixedly provided on the stirring mechanism support frame (9); A heating coil fixing block (801) is fixedly connected to the bottom of the outer side surface of the heating coil (8), and the bottom of the stirring mechanism support frame (9) is fixedly connected to the heating coil fixing block (801).

Citation Information

Patent Citations

  • Novel polyvinylidene fluoride film as well as preparation method and application thereof

    CN102728240A

  • Coating system, nanometer silver wire conductive thin film and preparation method therefor

    CN106847411A

  • Composite membrane and preparation method thereof

    CN107537320A