A method for preparing bromine
By preparing superhydrophobic polyvinylidene fluoride hollow fiber membranes and modified activated carbon adsorbents, the problems of large equipment, high energy consumption, and reduced mass transfer performance in bromine preparation were solved, and efficient and low-energy bromine extraction was achieved. , extending the service life of the membrane and reducing absorbent liquid overflow.
Patent Information
- Application Number
- CN202410948921.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-07-16
AI Technical Summary
Among the existing bromine preparation methods, the air blowing method has the problems of large equipment footprint, high energy consumption and low extraction rate. The hydrophobic membrane of the hollow fiber gaseous membrane method is easily infiltrated by water, resulting in reduced mass transfer performance and increased absorption liquid volume. , the problem of overflowing containers.
By preparing a superhydrophobic polyvinylidene fluoride hollow fiber membrane, five soaking treatments are used to improve the hydrophobicity, and a modified activated carbon adsorbent is used, combined with high-temperature treatment and cross-linked resin, to improve the mass transfer performance and adsorption capacity of the membrane and avoid absorbing liquid overflow.
It extends the service life of the hollow fiber membrane, improves the mass transfer performance, reduces the problem of absorbent overflow, and achieves efficient bromine extraction. The bromine content is increased from 67mg/L to 22.0-22.7g/L, and the debromination rate reaches 86.9 -87.9%.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bromine preparation, and in particular to a method for preparing bromine. Background Art
[0002] Bromine is the only non-metallic element that is in liquid form at room temperature. It is a dark reddish brown liquid with a pungent odor. As an important chemical raw material, bromine is mainly used to prepare bromides. It can also be used in medicine, pesticides, dyes, spices, photographic materials, fire extinguishing agents, mineral processing, metallurgy, tanning, water purification and other departments as a common analytical reagent, oxidant, absorbent for ethylene and heavy hydrocarbons, and brominating agent for organic synthesis.
[0003] The main methods for preparing bromine include air blowing method, steam distillation method and absorption method. The air blowing method is to pass chlorine gas into seawater or brine containing bromide, oxidize the bromide into bromine element, then heat the bromine element with water vapor and blow it out, and then use an absorbent to absorb the bromine element. The steam distillation method is to co-distill the bromide in seawater or brine with water, extract the water vapor and bromine vapor, and then use an absorbent to absorb the bromine vapor. The absorption method is a method of using an absorbent to directly absorb the bromide in seawater or brine to obtain bromine. Among them, the air blowing method can extract bromine from low-concentration bromine-containing brine or seawater, is simple to operate, and is currently the most commonly used preparation method.
[0004] However, when preparing bromine by air blowing method, there are the following problems: the equipment of air blowing method occupies a large area; the main equipment of air blowing method is blowing tower, which is filled with fillers, but the bromine-containing brine or seawater contains impurities such as mud and sand, which can easily cause the fillers to be blocked; when the bromine content in bromine-containing brine or seawater is low, the amount of water vapor used is large, which will lead to high energy consumption; when the temperature of bromine-containing brine or seawater is low, the blowing effect will be poor, resulting in a decrease in extraction rate. Therefore, it is necessary to develop a new method for preparing bromine to solve the problems of air blowing method.
[0005] The hollow fiber gas membrane method uses brine as raw material, after acidification and oxidation, alkali solution is used as absorbent, and hydrophobic polyvinylidene fluoride hollow fiber membrane components are used to efficiently enrich bromine in bromine-containing liquid. The hollow fiber gas membrane method has the advantages of large specific surface area, high mass transfer rate, low energy consumption, small footprint, and simple operation, and has broad development prospects in the field of bromine preparation. However, when preparing bromine by the hollow fiber gas membrane method, there are still the following problems: hydrophobic polyvinylidene fluoride hollow fiber membranes are usually prepared by phase inversion method, and the water-soluble pore-forming agent in the hollow fiber membrane is difficult to completely remove, resulting in the hydrophobicity of the hollow fiber membrane gradually decreasing during use, further resulting in the hollow fiber membrane being easily infiltrated by water during operation, thereby causing a decrease in mass transfer performance and affecting the service life of the hollow fiber membrane. Although the hydrophobic modification method can be used to increase the service life of the hollow fiber membrane, the existing hydrophobic modification is mainly a method of coating hydrophobic nanoparticles on the surface of the hollow fiber membrane, and the hydrophobic nanoparticles are easy to clog the hollow fiber membrane. The membrane is thicker, which affects the mass transfer performance of the hollow fiber membrane. In the process of free bromine transfer through the hydrophobic polyvinylidene fluoride hollow fiber membrane, water will be transferred from the high vapor pressure side to the low vapor pressure side. Therefore, when using a high-concentration absorption liquid for absorption, the vapor pressure on the high-concentration absorption liquid side is small, and the water in the bromine-containing feed liquid will enter the absorption liquid under the action of the vapor pressure difference on both sides of the hollow fiber membrane, resulting in a decrease in the concentration of the absorption liquid and an increase in the volume. Moreover, as bromine reacts with the absorption liquid, the vapor pressure on the absorption liquid side is further reduced, further causing the water in the bromine-containing feed liquid to enter the absorption liquid. Therefore, after long-term operation, the volume of the absorption liquid will continue to increase and overflow from the container. Summary of the invention
[0006] In view of the shortcomings of the prior art, the present invention provides a method for preparing bromine, in which bromine is prepared by a hollow fiber gas membrane method. The hollow fiber gas membrane used has a long service life and can reduce the problem of absorption liquid overflow in long-term operation.
[0007] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows:
[0008] A method for preparing bromine, comprising the following steps: preparing a super-hydrophobic polyvinylidene fluoride hollow fiber membrane, preparing an adsorbent, pre-treatment, separation, and post-treatment;
[0009] The preparation of the super-hydrophobic polyvinylidene fluoride hollow fiber membrane comprises the following steps: one soaking, two soakings, three soakings, four soakings, and five soakings;
[0010] The primary immersion comprises completely immersing the polytetrafluoroethylene hollow fiber membrane in the primary immersion solution, standing at 40-50° C. for 1.5-2 hours, taking it out, and drying it at 70-80° C. for 2-3 hours to obtain the primary immersion hollow fiber membrane;
[0011] The inner diameter of the polytetrafluoroethylene hollow fiber membrane is 0.8 mm, the outer diameter is 1.6 mm, the average pore size is 1 μm, and the porosity is 85%;
[0012] The preparation method of the primary soaking liquid is as follows: after mixing tridecafluorooctyl triethoxysilane, anhydrous ethanol and deionized water, stirring at room temperature for 30-40 minutes, and standing for 30-40 minutes to obtain the primary soaking liquid;
[0013] In the preparation of the primary immersion solution, the mass volume ratio of tridecafluorooctyltriethoxysilane, anhydrous ethanol and deionized water is 20-21 g: 1400-1500 mL: 800-900 mL;
[0014] The secondary soaking is to completely soak the primary soaked hollow fiber membrane in the secondary soaking solution, stand at 40-50° C. for 30-40 minutes, take it out, and dry it at 70-80° C. for 2-3 hours to obtain the secondary soaked hollow fiber membrane;
[0015] The preparation method of the secondary soaking solution is as follows: 2-phenylbenzothiazole and anhydrous ethanol are mixed, and the mixture is stirred at room temperature for 30-40 minutes to obtain the secondary soaking solution;
[0016] In the preparation of the secondary soaking solution, the mass volume ratio of 2-phenylbenzothiazole to anhydrous ethanol is 30-35g:900-1000mL;
[0017] The three-time soaking is to completely soak the second-time soaking hollow fiber membrane in the three-time soaking solution, stand at 40-50° C. for 1.5-2 hours, take it out, and dry it at 70-80° C. for 2-3 hours to obtain the three-time soaking hollow fiber membrane;
[0018] The preparation method of the three-time soaking solution is the same as the preparation method of the one-time soaking solution;
[0019] The four-time soaking is to completely soak the three-time soaking hollow fiber membrane in the four-time soaking solution, stand at 40-50° C. for 20-30 minutes, take out, and dry at 70-80° C. for 2-3 hours to obtain the four-time soaking hollow fiber membrane;
[0020] The preparation method of the four-time soaking solution is as follows: n-butyl titanate is added dropwise to nitric acid, the nitric acid is continuously stirred during the dropping process, stirring is continued for 10-20 minutes after the dropping is completed, and then stirring is stopped, and the mixture is allowed to stand at 80-90° C. for 3.5-4 hours to obtain the four-time soaking solution;
[0021] In the preparation of the four immersion solutions, the volume ratio of n-butyl titanate drops to nitric acid is 80-90:1200-1300;
[0022] The volume concentration of the nitric acid is 0.7%;
[0023] The five-time soaking is to completely soak the four-time soaking hollow fiber membrane in the five-time soaking solution, stand at 40-50° C. for 4-5 hours, take it out, and dry it at 70-80° C. for 9-10 hours to obtain the five-time soaking hollow fiber membrane;
[0024] The preparation method of the five-time soaking solution is as follows: hexadecyltrimethoxysilane and anhydrous ethanol are mixed, and stirred at room temperature for 1-1.5 hours to obtain the five-time soaking solution;
[0025] In the preparation of the five immersion solutions, the volume ratio of hexadecyltrimethoxysilane to anhydrous ethanol is 40-45:1000-1300;
[0026] The preparation of the adsorbent comprises the following steps: primary modification, secondary modification, mixing, high temperature treatment, and crushing;
[0027] The primary modification comprises mixing large-particle activated carbon and small-particle activated carbon uniformly, drying at 105-115° C. for 12-15 hours, mixing with nitric acid, reflux stirring at 70-80° C. for 2.5-3 hours, filtering, washing the filter residue with deionized water for 4-5 times, and drying at 110-120° C. for 6-7 hours to obtain primary modified activated carbon;
[0028] In the primary modification, the mass volume ratio of large particle size activated carbon, small particle size activated carbon and nitric acid is 90-100g:90-120g:3200-3500mL;
[0029] The average particle size of large-size activated carbon is 200 μm;
[0030] The average particle size of small-size activated carbon is 10 μm;
[0031] The mass concentration of the nitric acid is 20%;
[0032] The secondary modification comprises mixing 3-(2,3-oxypropoxy)propyltrimethoxysilane, primary modified activated carbon, deionized water and anhydrous ethanol, stirring and refluxing at 75-80° C. for 3.5-4 hours, filtering, washing the filter residue with anhydrous ethanol for 3-4 times, and drying at 110-120° C. for 6-7 hours to obtain secondary modified activated carbon;
[0033] In the secondary modification, the mass volume ratio of 3-(2,3-oxypropoxy)propyltrimethoxysilane, primary modified activated carbon, deionized water, and anhydrous ethanol is 120-130 mL: 180-220 g: 250-300 mL: 3400-3500 mL;
[0034] The mixing is to mix 2-aminobenzothiazole and N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane, and then ball milling is performed at room temperature for 20-30 minutes, the rotation speed in the ball milling is 300-400 rpm, and the ball-to-material ratio is 10-12:1, and then the secondary modified activated carbon is added, and the ball milling is continued for 40-50 minutes to obtain a mixture;
[0035] In the mixture, the mass ratio of 2-aminobenzothiazole, N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane, and secondary modified activated carbon is 80-85:210-230:130-140;
[0036] The high temperature treatment comprises heating the mixture to 170-190° C. at a heating rate of 6-8° C. / min under the protection of nitrogen, standing at 170-190° C. for 80-100 minutes, and then naturally returning to room temperature to obtain a mixture after high temperature treatment;
[0037] The pulverizing is to pulverize the mixture after high temperature treatment to an average particle size of 100-150 μm to obtain an adsorbent;
[0038] The pre-treatment is to adjust the pH of the brine to 3-3.5, and then introduce chlorine gas to oxidize until there is no bromide ion in the brine, thereby obtaining the pre-treated brine;
[0039] The chlorine gas introduction rate is 450-500 mL / min;
[0040] The separation comprises passing the pre-treated brine into the tube side of a hollow fiber membrane assembly equipped with a super-hydrophobic polyvinylidene fluoride hollow fiber membrane, passing the absorption liquid into the shell side of a hollow fiber membrane assembly equipped with a super-hydrophobic polyvinylidene fluoride hollow fiber membrane, the pre-treated brine and the absorption liquid flow in a countercurrent manner, collecting the pre-treated brine flowing out of the hollow fiber membrane assembly equipped with the super-hydrophobic polyvinylidene fluoride hollow fiber membrane and then centrally treating it, detecting the pH of the absorption liquid flowing out of the hollow fiber membrane assembly equipped with the super-hydrophobic polyvinylidene fluoride hollow fiber membrane, and if the pH is higher than 4.5, continuing to pass the absorption liquid into the shell side of the hollow fiber membrane assembly equipped with the super-hydrophobic polyvinylidene fluoride hollow fiber membrane for recycling, and if the pH is lower than 4.5, collecting the absorption liquid;
[0041] The preparation method of the absorption liquid is as follows: adding the adsorbent to a sodium formate aqueous solution, and ultrasonically oscillating for 8-10 minutes to obtain the absorption liquid;
[0042] In the preparation of the absorption liquid, the mass volume ratio of the adsorbent and the sodium formate aqueous solution is 28-30 g:950-1000 mL;
[0043] The mass concentration of the sodium formate aqueous solution is 5%;
[0044] The temperature of the pre-treated brine is 20-25°C, and the flow rate is 19-21.5L / h;
[0045] The temperature of the absorption liquid is 20-25°C and the flow rate is 4.5-5L / h;
[0046] The effective membrane area of the hollow fiber membrane module is 2m 2 ;
[0047] The post-treatment comprises filtering the absorption liquid collected in the separation step to obtain a first filter residue and a first filtrate, adding the first filter residue to deionized water with a mass of 5-5.5 times that of the first filter residue, stirring at 90-95° C. for 2.5-3 hours, filtering to obtain a second filter residue and a second filtrate, drying the second filter residue at 110-120° C. for 8-9 hours, and reusing it as a recovered adsorbent, combining the first filtrate with the second filtrate to obtain a concentrated solution, adjusting the pH of the concentrated solution to 2.5-3, introducing chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distilling at 60-70° C. to collect the distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine;
[0048] The chlorine gas is introduced at a rate of 400-450 mL / min.
[0049] Compared with the prior art, the present invention has the following beneficial effects:
[0050] (1) The present invention uses a hollow fiber gas membrane method to prepare bromine, and the polytetrafluoroethylene hollow fiber membrane used is soaked five times, wherein the first soaking is to treat the polytetrafluoroethylene hollow fiber membrane with tridecafluorooctyl triethoxysilane, and adsorb it on the surface of the polytetrafluoroethylene hollow fiber membrane through hydrophobic interaction, the second soaking is to treat the polytetrafluoroethylene hollow fiber membrane with 2-phenylbenzothiazole, and adsorb it on the surface of the polytetrafluoroethylene hollow fiber membrane through sulfur-fluorine non-covalent interaction, the third soaking is to treat the polytetrafluoroethylene hollow fiber membrane with tridecafluorooctyl triethoxysilane, and adsorb it on the surface of the polytetrafluoroethylene hollow fiber membrane through sulfur-fluorine non-covalent interaction, and the fourth soaking is to treat the polytetrafluoroethylene hollow fiber membrane with titanium sol. The polytetrafluoroethylene hollow fiber membrane was treated, and titanium dioxide was adsorbed on the surface of the polytetrafluoroethylene hollow fiber membrane through liquid phase deposition. The titanium dioxide was hydrophobically modified with hexadecyltrimethoxysilane for five times of immersion. The use of 2-phenylbenzothiazole can improve the binding force of tridecafluorooctyltriethoxysilane on the surface of the polytetrafluoroethylene hollow fiber membrane. The use of titanium sol and hexadecyltrimethoxysilane can improve the hydrophobicity of the polytetrafluoroethylene hollow fiber membrane. Compared with only using tridecafluorooctyltriethoxysilane and 2-phenylbenzothiazole for two modifications, the use of titanium dioxide and hexadecyltrimethoxysilane can improve the hydrophobicity of the polytetrafluoroethylene hollow fiber membrane. The pore structure of titanium dioxide can also be used to improve the hydrophobicity of the polytetrafluoroethylene hollow fiber membrane. The mass transfer performance of polytetrafluoroethylene hollow fiber membrane, compared with the double modification using only tridecafluorooctyltriethoxysilane and titanium sol, the use of 2-phenylbenzothiazole can improve the binding force between tridecafluorooctyltriethoxysilane and titanium dioxide and polytetrafluoroethylene hollow fiber membrane, avoid the loss of tridecafluorooctyltriethoxysilane and titanium dioxide causing the hydrophobicity of polytetrafluoroethylene hollow fiber membrane to decrease, and avoid the pore blockage of polytetrafluoroethylene hollow fiber membrane caused by excessive use of titanium sol, affecting the mass transfer performance; the adsorbent used in the absorption liquid in the separation is to activate two activated carbons with different particle sizes using nitric acid, and the activated carbons with different particle sizes can improve the adsorption capacity after being composited, and then use 3-(2,3-oxypropoxy)propyltrimethoxy Silane is used for surface modification to introduce epoxy groups on the surface of activated carbon, and then 2-aminobenzothiazole, N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane and activated carbon with epoxy groups are mixed to obtain a mixture, and then high-temperature treatment is performed to cross-link the amino groups and epoxy groups in the mixture at 170-190° C. to obtain a mixture of cross-linked resin and activated carbon. After the cross-linked resin and activated carbon are mixed, the cross-linked resin plays a role in fixing the activated carbon and can also improve the adsorption of the activated carbon, thereby avoiding agglomeration of the activated carbon and increasing the adsorption amount of the activated carbon. In addition, the cross-linked resin has good heat resistance, which can avoid damage to the cross-linked resin during the desorption process and is also conducive to improving the desorption speed and desorption rate of the activated carbon;
[0051] (2) The method for preparing bromine of the present invention extracts bromine from brine having a bromine content of 67 mg / L, wherein the bromine content of the brine flowing out of the hollow fiber membrane module in the separation step is 8.1-8.8 mg / L, the debromination rate is 86.9-87.9%, and the bromine content of the concentrated solution obtained in the post-treatment step is 22.0-22.7 g / L;
[0052] (3) The hollow fiber gas membrane used in the bromine preparation method of the present invention has a long service life, and the total mass transfer coefficient decrease rate is 2.2-2.5% after continuous operation for one month;
[0053] (4) The method for preparing bromine of the present invention can reduce the problem of absorption liquid overflow during long-term operation. DETAILED DESCRIPTION
[0054] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific implementation methods of the present invention are now described.
[0055] Example 1
[0056] A method for preparing bromine, specifically:
[0057] 1. Preparation of super hydrophobic polyvinylidene fluoride hollow fiber membrane:
[0058] (1) Soaking once: completely soak the polytetrafluoroethylene hollow fiber membrane in the soaking solution, let it stand at 40°C for 1.5 hours, take it out, and dry it at 70°C for 2 hours to obtain a soaked hollow fiber membrane;
[0059] The inner diameter of the polytetrafluoroethylene hollow fiber membrane is 0.8 mm, the outer diameter is 1.6 mm, the average pore size is 1 μm, and the porosity is 85%;
[0060] The preparation method of the primary soaking liquid is as follows: 20 g of tridecafluorooctyl triethoxysilane, 1400 mL of anhydrous ethanol, and 800 mL of deionized water are mixed, stirred at room temperature for 30 minutes, and allowed to stand for 30 minutes to obtain a primary soaking liquid;
[0061] (2) Secondary soaking: The first soaked hollow fiber membrane is completely immersed in the secondary soaking solution, left to stand at 40°C for 30 min, taken out, and dried at 70°C for 2 h to obtain a secondary soaked hollow fiber membrane;
[0062] The preparation method of the secondary soaking solution is as follows: 30 g of 2-phenylbenzothiazole and 900 mL of anhydrous ethanol are mixed, and the mixture is stirred at room temperature for 30 minutes to obtain a secondary soaking solution;
[0063] (3) Three-time soaking: The two-time soaking hollow fiber membrane is completely immersed in the three-time soaking solution, and is allowed to stand at 40°C for 1.5 h. It is then taken out and dried at 70°C for 2 h to obtain a three-time soaking hollow fiber membrane.
[0064] The preparation method of the three-time soaking solution is the same as the preparation method of the one-time soaking solution;
[0065] (4) Four-time soaking: The three-time soaking hollow fiber membrane is completely immersed in the four-time soaking solution, allowed to stand at 40°C for 20 min, taken out, and dried at 70°C for 2 h to obtain a four-time soaking hollow fiber membrane;
[0066] The preparation method of the four-time soaking solution is as follows: 80 mL of n-butyl titanate is added dropwise to 1200 mL of nitric acid with a volume concentration of 0.7%, the nitric acid is continuously stirred during the dropping process, and the stirring is continued for 10 minutes after the dropping is completed, and then the stirring is stopped, and the mixture is allowed to stand at 80° C. for 3.5 hours to obtain the four-time soaking solution;
[0067] (5) Five-time soaking: The four-time soaking hollow fiber membrane is completely immersed in the five-time soaking solution, left to stand at 40°C for 4 h, taken out, and dried at 70°C for 9 h to obtain a five-time soaking hollow fiber membrane;
[0068] The preparation method of the five-time soaking solution is as follows: 40 mL of hexadecyltrimethoxysilane and 1000 mL of anhydrous ethanol are mixed, and the mixture is stirred at room temperature for 1 hour to obtain the five-time soaking solution;
[0069] 2. Preparation of adsorbent:
[0070] (1) Primary modification: 90 g of activated carbon with an average particle size of 200 μm and 90 g of activated carbon with an average particle size of 10 μm were mixed evenly, dried at 105 °C for 12 h, then mixed with 3200 mL of 20% nitric acid, refluxed and stirred at 70 °C for 2.5 h, filtered, and the filter residue was washed 4 times with deionized water, and dried at 110 °C for 6 h to obtain primary modified activated carbon;
[0071] (2) Secondary modification: 120 mL of 3-(2,3-oxypropoxy)propyltrimethoxysilane, 180 g of primary modified activated carbon, 250 mL of deionized water, and 3400 mL of anhydrous ethanol were mixed, stirred and refluxed at 75 °C for 3.5 h, filtered, and the filter residue was washed with anhydrous ethanol for 3 times, and dried at 110 °C for 6 h to obtain secondary modified activated carbon;
[0072] (3) Mixing: 80 g of 2-aminobenzothiazole and 210 g of N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane were mixed, and the mixture was ball-milled at room temperature for 20 min. The rotation speed of the ball mill was 300 rpm, and the ball-to-material ratio was 10:1. Then, 130 g of secondary modified activated carbon was added, and the ball milling was continued for 40 min to obtain a mixture.
[0073] (4) High temperature treatment: Under the protection of nitrogen, the mixture was heated to 170°C at a heating rate of 6°C / min, allowed to stand at 170°C for 80 min, and then naturally returned to room temperature to obtain a mixture after high temperature treatment;
[0074] (5) crushing: crushing the mixture after high temperature treatment to an average particle size of 100 μm to obtain an adsorbent;
[0075] 3. Pretreatment: adjust the pH of the brine to 3, then introduce chlorine gas to oxidize until there is no bromide ion in the brine, and obtain the pretreated brine;
[0076] The bromine content in the brine is 67 mg / L;
[0077] The chlorine gas introduction rate is 450 mL / min;
[0078] 4. Separation: the pre-treated brine is passed through the tube side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane, and the absorption liquid is passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane. The pre-treated brine and the absorption liquid flow in the reverse direction. The pre-treated brine flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is collected and then centrally processed. The pH of the absorption liquid flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is detected. If the pH is higher than 4.5, the absorption liquid is continuously passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane for recycling. If the pH is lower than 4.5, the absorption liquid is collected.
[0079] The preparation method of the absorption liquid is as follows: 28g of the adsorbent is added into 950mL of a sodium formate aqueous solution with a mass concentration of 5%, and ultrasonically vibrated for 8min to obtain the absorption liquid;
[0080] The temperature of the pre-treated brine is 20°C and the flow rate is 19L / h;
[0081] The temperature of the absorption liquid is 20°C and the flow rate is 4.5L / h;
[0082] The effective membrane area of the hollow fiber membrane module is 2m 2 ;
[0083] The bromine content of the pre-treated brine collected from the hollow fiber membrane module equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane was 8.4 mg / L, and the debromination rate was 87.5%;
[0084] 5. Post-treatment: Filter the absorption liquid collected in the separation step to obtain a first filter residue and a first filtrate, add the first filter residue to deionized water with a mass 5 times that of the first filter residue, stir at 90°C for 2.5 hours, filter to obtain a second filter residue and a second filtrate, dry the second filter residue at 110°C for 8 hours, and reuse it as a recovered adsorbent, combine the first filtrate with the second filtrate to obtain a concentrated solution, adjust the pH of the concentrated solution to 2.5, introduce chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distill at 60°C to collect the distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine;
[0085] The bromine content in the concentrate is 22.7 g / L;
[0086] The chlorine gas was introduced at a rate of 400 mL / min.
[0087] Example 2
[0088] A method for preparing bromine, specifically:
[0089] 1. Preparation of super hydrophobic polyvinylidene fluoride hollow fiber membrane:
[0090] (1) Soaking once: completely soak the polytetrafluoroethylene hollow fiber membrane in the soaking solution, let it stand at 45°C for 1.5 hours, take it out, and dry it at 75°C for 2.5 hours to obtain a soaked hollow fiber membrane;
[0091] The inner diameter of the polytetrafluoroethylene hollow fiber membrane is 0.8 mm, the outer diameter is 1.6 mm, the average pore size is 1 μm, and the porosity is 85%;
[0092] The preparation method of the primary soaking liquid is as follows: 20.5 g of tridecafluorooctyl triethoxysilane, 1450 mL of anhydrous ethanol, and 850 mL of deionized water are mixed, stirred at room temperature for 35 minutes, and allowed to stand for 35 minutes to obtain a primary soaking liquid;
[0093] (2) Secondary immersion: The first-immersion hollow fiber membrane is completely immersed in the secondary immersion solution, and allowed to stand at 45°C for 305 min. The membrane is taken out and dried at 75°C for 2.5 h to obtain a secondary immersion hollow fiber membrane.
[0094] The secondary soaking solution is prepared by mixing 32 g of 2-phenylbenzothiazole and 950 mL of anhydrous ethanol, and stirring at room temperature for 35 minutes to obtain a secondary soaking solution;
[0095] (3) Three-time soaking: The two-time soaking hollow fiber membrane is completely immersed in the three-time soaking solution, and allowed to stand at 45°C for 1.5 h. Then, it is taken out and dried at 75°C for 2.5 h to obtain a three-time soaking hollow fiber membrane.
[0096] The preparation method of the three-time soaking solution is the same as the preparation method of the one-time soaking solution;
[0097] (4) Four-time immersion: The three-time immersion hollow fiber membrane is completely immersed in the four-time immersion solution, allowed to stand at 45°C for 25 min, taken out, and dried at 75°C for 2.5 h to obtain a four-time immersion hollow fiber membrane;
[0098] The preparation method of the four-time soaking solution is as follows: 85 mL of n-butyl titanate is added dropwise to 1250 mL of nitric acid with a volume concentration of 0.7%, the nitric acid is continuously stirred during the dropping process, and the stirring is continued for 15 minutes after the dropping is completed, and then the stirring is stopped, and the mixture is allowed to stand at 85° C. for 3.5 hours to obtain the four-time soaking solution;
[0099] (5) Five-time immersion: The four-time immersion hollow fiber membrane is completely immersed in the five-time immersion solution, allowed to stand at 45°C for 4.5 h, taken out, and dried at 75°C for 9.5 h to obtain a five-time immersion hollow fiber membrane;
[0100] The preparation method of the five-time soaking solution is as follows: 42 mL of hexadecyltrimethoxysilane and 1200 mL of anhydrous ethanol are mixed, and the mixture is stirred at room temperature for 1 hour to obtain the five-time soaking solution;
[0101] 2. Preparation of adsorbent:
[0102] (1) Primary modification: 95 g of activated carbon with an average particle size of 200 μm and 100 g of activated carbon with an average particle size of 10 μm were mixed evenly, dried at 110 °C for 13 h, then mixed with 3400 mL of 20% nitric acid, refluxed and stirred at 75 °C for 2.5 h, filtered, and the filter residue was washed with deionized water for 4 times, and dried at 115 °C for 6.5 h to obtain primary modified activated carbon;
[0103] (2) Secondary modification: 125 mL of 3-(2,3-oxypropoxy)propyltrimethoxysilane, 200 g of primary modified activated carbon, 280 mL of deionized water, and 3450 mL of anhydrous ethanol were mixed, stirred and refluxed at 78 ° C for 3.5 h, filtered, and the filter residue was washed with anhydrous ethanol for 3 times, and dried at 115 ° C for 6.5 h to obtain secondary modified activated carbon;
[0104] (3) Mixing: 82 g of 2-aminobenzothiazole and 220 g of N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane were mixed, and the mixture was ball-milled at room temperature for 25 min. The rotation speed of the ball mill was 350 rpm, and the ball-to-material ratio was 11:1. Then, 135 g of secondary modified activated carbon was added, and the ball milling was continued for 45 min to obtain a mixture.
[0105] (4) High temperature treatment: Under the protection of nitrogen, the mixture was heated to 180°C at a heating rate of 7°C / min, allowed to stand at 180°C for 90 min, and then naturally returned to room temperature to obtain a mixture after high temperature treatment;
[0106] (5) crushing: crushing the mixture after high temperature treatment to an average particle size of 100 μm to obtain an adsorbent;
[0107] 3. Pretreatment: adjust the pH of the brine to 3.2, then introduce chlorine gas to oxidize until there is no bromide ion in the brine, and obtain the pretreated brine;
[0108] The bromine content in the brine is 67 mg / L;
[0109] The chlorine gas introduction rate is 480 mL / min;
[0110] 4. Separation: the pre-treated brine is passed through the tube side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane, and the absorption liquid is passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane. The pre-treated brine and the absorption liquid flow in the reverse direction. The pre-treated brine flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is collected and then centrally processed. The pH of the absorption liquid flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is detected. If the pH is higher than 4.5, the absorption liquid is continuously passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane for recycling. If the pH is lower than 4.5, the absorption liquid is collected.
[0111] The preparation method of the absorption liquid is as follows: 29g of the adsorbent is added into 980mL of a sodium formate aqueous solution with a mass concentration of 5%, and ultrasonically vibrated for 9min to obtain the absorption liquid;
[0112] The temperature of the pre-treated brine is 22°C and the flow rate is 20.5L / h;
[0113] The temperature of the absorption liquid is 22°C and the flow rate is 4.8 L / h;
[0114] The effective membrane area of the hollow fiber membrane module is 2m 2 ;
[0115] The bromine content of the pre-treated brine collected from the hollow fiber membrane module equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane was 8.1 mg / L, and the debromination rate was 87.9%;
[0116] 5. Post-treatment: Filter the absorption liquid collected in the separation step to obtain a first filter residue and a first filtrate, add the first filter residue to deionized water 5.2 times the mass of the first filter residue, stir at 92°C for 2.5 hours, filter to obtain a second filter residue and a second filtrate, dry the second filter residue at 115°C for 8.5 hours, and reuse it as a recovered adsorbent, combine the first filtrate with the second filtrate to obtain a concentrated solution, adjust the pH of the concentrated solution to 2.8, introduce chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distill at 65°C to collect the distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine;
[0117] The bromine content in the concentrate is 22.4 g / L;
[0118] The chlorine gas was introduced at a rate of 430 mL / min.
[0119] Example 3
[0120] A method for preparing bromine, specifically:
[0121] 1. Preparation of super hydrophobic polyvinylidene fluoride hollow fiber membrane:
[0122] (1) One-time immersion: The polytetrafluoroethylene hollow fiber membrane is completely immersed in the one-time immersion solution, left to stand at 50°C for 2 h, taken out, and dried at 80°C for 3 h to obtain a one-time immersion hollow fiber membrane;
[0123] The inner diameter of the polytetrafluoroethylene hollow fiber membrane is 0.8 mm, the outer diameter is 1.6 mm, the average pore size is 1 μm, and the porosity is 85%;
[0124] The preparation method of the primary soaking liquid is as follows: 21 g of tridecafluorooctyl triethoxysilane, 1500 mL of anhydrous ethanol, and 900 mL of deionized water are mixed, stirred at room temperature for 40 minutes, and allowed to stand for 40 minutes to obtain a primary soaking liquid;
[0125] (2) Secondary soaking: The primary soaked hollow fiber membrane is completely immersed in the secondary soaking solution, left to stand at 50°C for 40 min, taken out, and dried at 80°C for 3 h to obtain a secondary soaked hollow fiber membrane;
[0126] The secondary soaking solution is prepared by mixing 35 g of 2-phenylbenzothiazole and 1000 mL of anhydrous ethanol, and stirring at room temperature for 40 minutes to obtain a secondary soaking solution;
[0127] (3) Three-time soaking: The two-time soaking hollow fiber membrane is completely immersed in the three-time soaking solution, and allowed to stand at 50°C for 2 h. Then, it is taken out and dried at 80°C for 3 h to obtain the three-time soaking hollow fiber membrane.
[0128] The preparation method of the three-time soaking solution is the same as the preparation method of the one-time soaking solution;
[0129] (4) Four-time immersion: The three-time immersion hollow fiber membrane is completely immersed in the four-time immersion solution, allowed to stand at 50°C for 30 min, taken out, and dried at 80°C for 3 h to obtain a four-time immersion hollow fiber membrane;
[0130] The preparation method of the four-time soaking solution is as follows: 90 mL of n-butyl titanate is added dropwise to 1300 mL of nitric acid with a volume concentration of 0.7%, the nitric acid is continuously stirred during the dropping process, and the stirring is continued for 20 minutes after the dropping is completed, and then the stirring is stopped, and the mixture is allowed to stand at 90° C. for 4 hours to obtain the four-time soaking solution;
[0131] (5) Five-time immersion: The four-time immersion hollow fiber membrane is completely immersed in the five-time immersion solution, left to stand at 50°C for 5 h, taken out, and dried at 80°C for 10 h to obtain a five-time immersion hollow fiber membrane;
[0132] The preparation method of the five-time soaking solution is as follows: 45 mL of hexadecyltrimethoxysilane and 1300 mL of anhydrous ethanol are mixed, and the mixture is stirred at room temperature for 1.5 hours to obtain the five-time soaking solution;
[0133] 2. Preparation of adsorbent:
[0134] (1) Primary modification: 100 g of activated carbon with an average particle size of 200 μm and 120 g of activated carbon with an average particle size of 10 μm were mixed evenly, dried at 115 °C for 15 h, then mixed with 3500 mL of 20% nitric acid, refluxed and stirred at 80 °C for 3 h, filtered, and the filter residue was washed with deionized water for 5 times, and dried at 120 °C for 7 h to obtain primary modified activated carbon;
[0135] (2) Secondary modification: 130 mL of 3-(2,3-oxypropoxy)propyltrimethoxysilane, 220 g of primary modified activated carbon, 300 mL of deionized water, and 3500 mL of anhydrous ethanol were mixed, stirred and refluxed at 80 °C for 4 h, filtered, and the filter residue was washed with anhydrous ethanol for 4 times, and dried at 120 °C for 7 h to obtain secondary modified activated carbon;
[0136] (3) Mixing: 85 g of 2-aminobenzothiazole and 230 g of N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane were mixed, and the mixture was ball-milled at room temperature for 30 min at a rotation speed of 400 rpm and a ball-to-material ratio of 12:1. Then, 140 g of secondary modified activated carbon was added, and the ball-milling was continued for 50 min to obtain a mixture.
[0137] (4) High temperature treatment: Under the protection of nitrogen, the mixture was heated to 190°C at a heating rate of 8°C / min, allowed to stand at 190°C for 100 min, and then naturally returned to room temperature to obtain a mixture after high temperature treatment;
[0138] (5) crushing: crushing the mixture after high temperature treatment to an average particle size of 150 μm to obtain an adsorbent;
[0139] 3. Pretreatment: adjust the pH of the brine to 3.5, then introduce chlorine gas to oxidize until there is no bromide ion in the brine, and obtain the pretreated brine;
[0140] The bromine content in the brine is 67 mg / L;
[0141] The chlorine gas introduction rate is 500mL / min;
[0142] 4. Separation: the pre-treated brine is passed through the tube side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane, and the absorption liquid is passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane. The pre-treated brine and the absorption liquid flow in the reverse direction. The pre-treated brine flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is collected and then centrally processed. The pH of the absorption liquid flowing out of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane is detected. If the pH is higher than 4.5, the absorption liquid is continuously passed through the shell side of the hollow fiber membrane assembly equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane for recycling. If the pH is lower than 4.5, the absorption liquid is collected.
[0143] The preparation method of the absorption liquid is as follows: 30g of the adsorbent is added into 1000mL of a sodium formate aqueous solution with a mass concentration of 5%, and ultrasonically vibrated for 10min to obtain the absorption liquid;
[0144] The temperature of the pre-treated brine is 25°C and the flow rate is 21.5L / h;
[0145] The temperature of the absorption liquid is 25°C and the flow rate is 5L / h;
[0146] The effective membrane area of the hollow fiber membrane module is 2m 2 ;
[0147] The bromine content of the pre-treated brine collected from the hollow fiber membrane module equipped with super-hydrophobic polyvinylidene fluoride hollow fiber membrane was 8.8 mg / L, and the debromination rate was 86.9%;
[0148] 5. Post-treatment: Filter the absorption liquid collected in the separation step to obtain a first filter residue and a first filtrate, add the first filter residue to deionized water with a mass 5.5 times that of the first filter residue, stir at 95°C for 3 hours, filter to obtain a second filter residue and a second filtrate, dry the second filter residue at 120°C for 9 hours, and reuse it as a recovered adsorbent, combine the first filtrate with the second filtrate to obtain a concentrated solution, adjust the pH of the concentrated solution to 3, introduce chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distill at 70°C to collect the distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine;
[0149] The bromine content in the concentrated solution is 22.0 g / L;
[0150] The chlorine gas was introduced at a rate of 450 mL / min.
[0151] Comparative Example 1
[0152] Adjustments were made to the preparation method of Example 1. Specifically, the second soaking liquid in the second soaking step (2) in the first step of preparing the super-hydrophobic polyvinylidene fluoride hollow fiber membrane was changed to be the same as the fourth soaking liquid in the fourth soaking, that is, the preparation method of the second soaking liquid was changed to:
[0153] 80 mL of n-butyl titanate was added dropwise to 1200 mL of 0.7% nitric acid, and the nitric acid was continuously stirred during the dropping process. After the dropping was completed, stirring was continued for 10 minutes, and then stirring was stopped. The mixture was allowed to stand at 80°C for 3.5 hours to obtain four soaking solutions.
[0154] The remaining operations are the same as those in Example 1.
[0155] In this comparative example, the bromine content of the pre-treated brine flowing out of the hollow fiber membrane module equipped with the super-hydrophobic polyvinylidene fluoride hollow fiber membrane collected in the separation step was 11.4 mg / L, and the debromination rate was 87.0%;
[0156] The bromine content of the concentrated liquid obtained in the post-treatment step was 22.8 g / L.
[0157] Comparative Example 2
[0158] The preparation method of Example 1 is adjusted. Specifically, the four soaking liquids in the four soaking steps in step (4) of the step of preparing the super-hydrophobic polyvinylidene fluoride hollow fiber membrane in step 1 are changed to be the same as the second soaking liquid in the second soaking, that is, the preparation method of the four soaking liquids is changed to:
[0159] Mix 30 g of 2-phenylbenzothiazole and 900 mL of anhydrous ethanol, and stir at room temperature for 30 min to obtain a secondary soaking solution;
[0160] The remaining operations are the same as those in Example 1.
[0161] In this comparative example, the bromine content of the pre-treated brine flowing out of the hollow fiber membrane module equipped with the super-hydrophobic polyvinylidene fluoride hollow fiber membrane collected in the separation step was 8.7 mg / L, and the debromination rate was 83.0%;
[0162] The bromine content of the concentrated liquid obtained in the post-treatment step was 22.7 g / L.
[0163] Comparative Example 3
[0164] The preparation method of Example 1 was adjusted, and the specific adjustments were as follows: the preparation of the adsorbent in step 2 was omitted, and the absorption liquid in the separation step in step 4 was changed to a sodium formate aqueous solution with a mass concentration of 5%;
[0165] And accordingly change the post-processing step 5 to:
[0166] Add 140 mL of deionized water to the absorption liquid collected in the separation step to obtain a concentrated solution, adjust the pH of the concentrated solution to 2.5, introduce chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distill at 60° C. to collect the distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine;
[0167] The remaining operations are the same as those in Example 1.
[0168] The bromine content in the concentrate in the post-treatment step was 24.5 g / L.
[0169] From the bromine content and debromination rate of the pre-treated brine flowing out from the hollow fiber membrane assembly equipped with superhydrophobic polyvinylidene fluoride hollow fiber membrane collected in the separation step in Examples 1-3 and Comparative Examples 1-3, and the bromine content in the concentrated solution obtained in the post-treatment step in Examples 1-3 and Comparative Examples 1-3, it can be seen that the bromine content and debromination rate of the pre-treated brine flowing out from the hollow fiber membrane assembly equipped with superhydrophobic polyvinylidene fluoride hollow fiber membrane in Comparative Example 1 are relatively low, indicating that the superhydrophobic polyvinylidene fluoride hollow fiber membrane prepared according to the method of Comparative Example 1 has poor mass transfer performance; the bromine content in the concentrated solution obtained in the post-treatment step of Comparative Example 3 is relatively high, indicating that after the adsorbent is added to the absorption liquid, the bromine in the absorption liquid will be adsorbed, and then when desorbed in the post-treatment step, the bromine content in the concentrated solution obtained in the post-treatment step will be affected by the desorption rate.
[0170] Test Example 1
[0171] The preparation methods of bromine according to Examples 1-3 and Comparative Examples 1-2 were run continuously for 30 days, and the total mass transfer coefficient of the hollow fiber membrane assembly equipped with the super hydrophobic polyvinylidene fluoride hollow fiber membrane was tested on the first and 30th days of continuous operation, and the total mass transfer coefficient reduction rate was calculated. The calculation formula and the calculation results are as follows:
[0172] Total mass transfer coefficient reduction rate = (total mass transfer coefficient on the first day of continuous operation - total mass transfer coefficient on the 30th day of continuous operation) / total mass transfer coefficient on the first day of continuous operation × 100%
[0173]
[0174] Test Example 2
[0175] According to the preparation methods of bromine of Examples 1-3 and Comparative Examples 1-3, respectively, in the separation step, 50 L of absorption liquid was used for cyclic absorption until the pH was lower than 4.5 to obtain the absorption liquid after cyclic absorption. The volume of the absorption liquid after cyclic absorption was recorded, and the recording results were as follows:
[0176]
[0177] It can be seen from the results of Experimental Examples 1 and 2 that the preparation method of bromine of Examples 1-3 can reduce the overall mass transfer coefficient reduction rate, and in the separation step, the volume change of the absorption liquid before and after absorption is small.
[0178] Unless otherwise specified, all percentages used in the present invention are by mass.
[0179] Finally, it should be noted that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing bromine, characterized in that: The method comprises the following steps: preparing a super-hydrophobic polytetrafluoroethylene hollow fiber membrane, preparing an adsorbent, pre-treatment, separation, and post-treatment; The preparation of the super-hydrophobic polytetrafluoroethylene hollow fiber membrane comprises the following steps: soaking once, soaking twice, soaking three times, soaking four times, and soaking five times; The primary immersion comprises completely immersing the polytetrafluoroethylene hollow fiber membrane in the primary immersion solution, standing at 40-50° C., taking out, and drying to obtain the primary immersion hollow fiber membrane; The preparation method of the primary soaking liquid is as follows: after mixing tridecafluorooctyl triethoxysilane, anhydrous ethanol and deionized water, stirring at room temperature and standing to obtain the primary soaking liquid; The secondary soaking is to completely soak the primary soaked hollow fiber membrane in the secondary soaking solution, let it stand at 40-50° C., take it out, and dry it to obtain the secondary soaked hollow fiber membrane; The preparation method of the secondary soaking liquid is as follows: 2-phenylbenzothiazole and anhydrous ethanol are mixed, and then stirred at room temperature to obtain the secondary soaking liquid; The three-time soaking is to completely soak the second-time soaking hollow fiber membrane in the three-time soaking solution, stand at 40-50° C., take out, and dry to obtain the three-time soaking hollow fiber membrane; The preparation method of the three-time soaking solution is the same as the preparation method of the one-time soaking solution; The four-time soaking comprises completely soaking the three-time soaking hollow fiber membrane in the four-time soaking solution, standing at 40-50° C., taking out, and drying to obtain the four-time soaking hollow fiber membrane; The preparation method of the four-time soaking solution is as follows: n-butyl titanate is added dropwise to nitric acid, the nitric acid is continuously stirred during the dropping process, the stirring is continued after the dropping is completed, and then the solution is allowed to stand at 80-90° C. to obtain the four-time soaking solution; The five soakings are to completely soak the four-immersion hollow fiber membrane in the five-immersion solution, stand at 40-50° C., take out, and dry to obtain a super-hydrophobic polytetrafluoroethylene hollow fiber membrane; The preparation method of the five-time soaking solution is as follows: hexadecyltrimethoxysilane and anhydrous ethanol are mixed, and stirred at room temperature to obtain the five-time soaking solution; The preparation of the adsorbent comprises the following steps: primary modification, secondary modification, mixing, high temperature treatment, and crushing; The primary modification comprises mixing large-size activated carbon and small-size activated carbon uniformly, drying, mixing with nitric acid, stirring under reflux at 70-80° C., filtering, washing and drying the filter residue to obtain the primary modified activated carbon; The secondary modification comprises mixing 3-(2,3-epoxypropoxy)propyltrimethoxysilane, primary modified activated carbon, deionized water and anhydrous ethanol, stirring and refluxing at 75-80° C., filtering, washing and drying the filter residue to obtain the secondary modified activated carbon; The mixing comprises mixing 2-aminobenzothiazole and N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane, ball milling, adding the secondary modified activated carbon, and continuing the ball milling to obtain a mixture; The high temperature treatment is to heat the mixture to 170-190° C. under the protection of nitrogen, keep the temperature and let it stand, and then naturally return to room temperature to obtain a mixture after high temperature treatment.
2. The method for preparing bromine according to claim 1, characterized in that: In the preparation of the primary immersion solution, the mass volume ratio of tridecafluorooctyltriethoxysilane, anhydrous ethanol and deionized water is 20-21 g: 1400-1500 mL: 800-900 mL.
3. The method for preparing bromine according to claim 1, characterized in that: In the preparation of the secondary soaking solution, the mass volume ratio of 2-phenylbenzothiazole to anhydrous ethanol is 30-35g:900-1000mL.
4. The method for preparing bromine according to claim 1, characterized in that: In the preparation of the four immersion solutions, the volume ratio of n-butyl titanate drops to nitric acid is 80-90:1200-1300; The volume concentration of the nitric acid is 0.7%.
5. The method for preparing bromine according to claim 1, characterized in that: In the preparation of the five immersion solutions, the volume ratio of hexadecyltrimethoxysilane to anhydrous ethanol is 40-45:1000-1300.
6. The method for preparing bromine according to claim 1, characterized in that: In the primary modification, the mass volume ratio of large particle size activated carbon, small particle size activated carbon and nitric acid is 90-100g:90-120g:3200-3500mL; The average particle size of large-size activated carbon is 200 μm; The average particle size of small-size activated carbon is 10 μm; The mass concentration of the nitric acid is 20%.
7. The method for preparing bromine according to claim 1, characterized in that: In the secondary modification, the mass volume ratio of 3-(2,3-epoxypropoxy)propyltrimethoxysilane, primary modified activated carbon, deionized water and anhydrous ethanol is 120-130 mL: 180-220 g: 250-300 mL: 3400-3500 mL.
8. The method for preparing bromine according to claim 1, characterized in that: In the mixture, the mass ratio of 2-aminobenzothiazole, N,N,N',N'-tetraglycidyl-4,4'-diaminodiphenylmethane, and secondary modified activated carbon is 80-85:210-230:130-140; The pulverizing is to pulverize the mixture after high temperature treatment to obtain an adsorbent.
9. The method for preparing bromine according to claim 1, characterized in that: The pre-treatment is to adjust the pH of the brine to 3-3.5, and then introduce chlorine gas to oxidize until there is no bromide ion in the brine, thereby obtaining the pre-treated brine; The separation comprises passing the pre-treated brine into the tube side of a hollow fiber membrane assembly equipped with a super-hydrophobic polytetrafluoroethylene hollow fiber membrane, passing the absorption liquid into the shell side of a hollow fiber membrane assembly equipped with a super-hydrophobic polytetrafluoroethylene hollow fiber membrane, the pre-treated brine and the absorption liquid flow in a countercurrent direction, collecting the pre-treated brine flowing out of the hollow fiber membrane assembly equipped with the super-hydrophobic polytetrafluoroethylene hollow fiber membrane and then centrally treating it, detecting the pH of the absorption liquid flowing out of the hollow fiber membrane assembly equipped with the super-hydrophobic polytetrafluoroethylene hollow fiber membrane, and if the pH is higher than 4.5, continuing to pass the absorption liquid into the shell side of the hollow fiber membrane assembly equipped with the super-hydrophobic polytetrafluoroethylene hollow fiber membrane for recycling, and if the pH is lower than 4.5, collecting the absorption liquid; The preparation method of the absorption liquid is as follows: adding the adsorbent to a sodium formate aqueous solution, and ultrasonically oscillating for 8-10 minutes to obtain the absorption liquid; In the preparation of the absorption liquid, the mass volume ratio of the adsorbent and the sodium formate aqueous solution is 28-30 g:950-1000 mL; The mass concentration of the sodium formate aqueous solution is 5%; The temperature of the pre-treated brine is 20-25 ° C, and the flow rate is 19-21.5L / h; The temperature of the absorption liquid is 20-25°C and the flow rate is 4.5-5L / h; The effective membrane area of the hollow fiber membrane module is 2m 2 .
10. The method for preparing bromine according to claim 1, characterized in that: The post-treatment comprises filtering the absorption liquid collected in the separation step to obtain a first filter residue and a first filtrate, adding the first filter residue into deionized water with a mass of 5-5.5 times that of the first filter residue, stirring at 90-95° C., filtering to obtain a second filter residue and a second filtrate, combining the first filtrate with the second filtrate to obtain a concentrated solution, adjusting the pH of the concentrated solution to 2.5-3, introducing chlorine gas to oxidize until there is no bromide ion in the concentrated solution, and then distilling at 60-70° C. to collect a distillate, and after the distillate is allowed to stand for stratification, the lower layer is bromine.